A sapphire wafer grinding and polishing fixture

By combining the fractal porous ceramic gas film disk and the partitioned vacuum adsorption structure, the problems of uneven film thickness, edge roll-off and contamination in the grinding and polishing process of sapphire wafers are solved, achieving a high-precision and damage-free clamping effect, which is suitable for the processing of large-size sapphire wafers.

CN225009435UActive Publication Date: 2026-11-24KUNMING TAIDING PRECISION MASCH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202522377726.3
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2025-11-10
Publication Date
2026-11-24
Estimated Expiration
2035-11-10

AI Technical Summary

Technical Problem

Sapphire wafers suffer from problems such as large in-plane thickness differences, edge roll-off, back scratches, and particle contamination during grinding and polishing. Traditional fixtures are difficult to balance floating and scratch prevention with stable positioning, and the uneven vacuum adsorption and gas film formation result in poor processing quality.

Method used

Employing a fractal porous ceramic air film disk and a zoned vacuum adsorption structure, an isobaric air film is constructed through a two-stage throttling component. Combined with a fractal microporous terminal plate and three shallow annular grooves for zoned vacuum, uniform airflow distribution and zoned gentle suction are achieved. In conjunction with electrostatic assisted initial bonding and a circumferential Coanda air curtain, the stability and cleanliness of the workpiece are improved.

Benefits of technology

It achieves high-precision clamping and improved processing quality of sapphire wafers, improves in-plane film thickness uniformity by 20%, reduces edge roll-off and back scratches, and controls contaminant diffusion during processing. It is suitable for grinding and polishing wafers with a diameter of 200mm and above.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN225009435U_ABST
    Figure CN225009435U_ABST
Patent Text Reader

Abstract

This utility model discloses a sapphire wafer grinding and polishing fixture, belonging to the field of grinding and polishing tooling technology. The fixture body is equipped with a distribution and stabilizing ring cavity and a two-stage throttling system to supply gas to a multi-layer porous ceramic gas film disk. The upper layer holes of the gas film disk are inclined inwards, and the lower layer holes are inclined outwards, forming an isobaric and uniform gas film with fractal multi-scale terminal micro-holes. The working surface is equipped with three shallow annular grooves (center, middle, and outer) flush with the terminal plate, each with independent vacuum channels for zoned gentle suction. The through holes at the bottom of the grooves are circumferentially staggered with the micro-holes to prevent leakage. The gas supply and vacuum channels are sealed and isolated within the fixture body and equipped with leakage monitoring. Optional features include an electrostatic assisted initial bonding component and a circumferential Coanda gas curtain nozzle ring. This fixture reduces TTV and edge roll-off, improves Ra uniformity, and suppresses contamination, and is suitable for sapphire wafers with a diameter of 200 mm and above.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This utility model relates to the field of grinding and polishing tooling technology, specifically a sapphire wafer grinding and polishing fixture. Background Technology

[0002] Sapphire wafers are characterized by high hardness, brittleness, and anisotropy, making them prone to problems such as large in-plane thickness variations, edge roll-off, minor scratches on the back side, and secondary contamination from particles during grinding and polishing. As wafer size increases, the difficulty of controlling the uniformity of the bearing film thickness and the edge-to-center pressure distribution rises significantly. Traditional fixtures relying on single vacuum adsorption or rigid support struggle to balance the conflict between floating support for scratch prevention and stable positioning. Current solutions often improve edge quality through universal self-leveling carrier heads, edge protection rings, zoned back pressure, or multi-cavity vacuum. Some solutions also incorporate porous air supply systems on the polishing platform side to create air cushions and reduce friction. However, directly forming an isobaric and anisotropic air film on the workpiece side and coordinating it with zoned vacuum is still insufficient. Furthermore, micro-slippage of the wafer can easily occur during the initial loading stage before vacuum is established, and droplets and abrasive particles from wet processing can easily infiltrate along the outer edge, causing contamination.

[0003] Existing technologies improve clamping stability by adding soft pads, increasing the stiffness of edge retaining rings, or refining the vacuum array, but they still have certain limitations. For example, the radial decay of the film thickness on the bearing surface leads to an imbalance in the center-edge removal rate; the vacuum opening is not flush with the bearing surface, causing local indentations or leaks on the film surface; the alignment of micropores and vacuum through-holes in the same direction forms a straight leakage path, weakening the gas film bearing capacity; gas supply pulsation is transmitted to the working surface, causing film thickness fluctuations; insufficient isolation between the gas path and the vacuum path leads to crossflow risk; there is a lack of active adsorption methods in the loading stage and a lack of effective shielding against edge contamination during the processing.

[0004] Therefore, there is an urgent need for a sapphire wafer grinding and polishing fixture that constructs an isobaric gas film on the workpiece side and works in conjunction with a flush, partitioned shallow groove vacuum. This fixture achieves consistent in-plane flow through the inward / outward tilting holes of a double-layer porous ceramic and fractal multi-scale terminal micropores. Simultaneously, three independent shallow annular grooves are introduced on the top surface to achieve partitioned light suction and staggered perforation to suppress leakage. Combined with channel sealing isolation and leakage monitoring, this fixture can solve problems such as film thickness uniformity, edge roll-off, back-side safety, and process cleanliness in grinding and polishing large-size sapphire wafers. Furthermore, electrostatic initiation bonding and circumferential Coanda air curtains can be superimposed as needed to further improve wafer loading stability and edge protection capabilities. Utility Model Content

[0005] The purpose of this invention is to overcome the shortcomings of the prior art and to propose a sapphire wafer grinding and polishing fixture to solve the above-mentioned problems.

[0006] The purpose of this utility model is achieved through the following technical solution: a sapphire wafer grinding and polishing fixture, including a fixture body substrate and a workpiece bearing surface disposed on the fixture body substrate, a distribution and stabilizing ring cavity is provided in the fixture body substrate, and a first-stage throttling core and a second-stage porous medium are sequentially disposed downstream of the distribution and stabilizing ring cavity, the first-stage throttling core and the second-stage porous medium together constitute a two-stage throttling component. Downstream of the two-stage throttling component is an upward connection to a multi-layer porous ceramic film film disk. The multi-layer porous ceramic film film disk includes an upper supply layer and a lower permeation layer. The relative radial inclination angle α1 of the hole axis of the upper supply layer is 10° to 30°, and the relative radial outclination angle α2 of the hole axis of the lower permeation layer is 5° to 20°. The thickness ratio of the upper supply layer to the lower permeation layer is 1:(0.5 to 1.5). The upper surface of the multi-layer porous ceramic air film disk is fully bonded with a fractal microporous terminal plate. The fractal microporous terminal plate is an annular thin plate and constitutes part of the workpiece bearing surface. A fractal multi-scale annular microporous array is set on the fractal microporous terminal plate. The fractal multi-scale annular microporous array is only distributed in the solid zone area of ​​the concentric annular zone. The fractal microporous terminal board is provided with a partitioned vacuum adsorption structure, which includes a central shallow annular groove, a middle shallow annular groove, and an outer shallow annular groove that are independent of each other and flush with the upper surface of the fractal microporous terminal board. Each shallow annular groove has a groove depth of 0.30-0.40 mm and a groove width of 6-8 mm. An isolation rib with a width of not less than 1.0 mm is provided between adjacent shallow annular grooves. Several through holes are uniformly provided at the bottom of each shallow annular groove. The central shallow annular groove, the middle shallow annular groove, and the outer shallow annular groove are connected to an external vacuum source through the first vacuum channel, the second vacuum channel, and the third vacuum channel inside the fixture body substrate, respectively. The opening surfaces of the fractal microporous terminal plate and the partitioned vacuum adsorption structure are on the same plane, with a flatness difference of no more than 0.01 mm. The micropores of the fractal microporous terminal plate are arranged in a staggered phase relative to the through holes in the circumferential direction. The gas supply channel is composed of a distribution and stabilizing ring cavity, a two-stage throttling component, a multi-layer porous ceramic gas film disk, and a fractal microporous terminal plate. The gas supply channel is isolated from the first vacuum channel, the second vacuum channel, and the third vacuum channel inside the fixture body substrate by a sealing ring. The closest net distance between the gas supply channel and any vacuum channel is not less than 1.0 mm. The fixture forms a uniform air film bearing on the workpiece side, and achieves zoned light suction and controllable edge-center pressure difference through the central shallow annular groove, middle shallow annular groove and outer shallow annular groove flush with the fractal micro-hole terminal plate.

[0007] The fractal microporous terminal plate has an outer diameter of 300 mm and an inner diameter of 180 mm; the central shallow annular groove is located at a radius of 185–205 mm, the middle shallow annular groove is located at a radius of 210–235 mm, and the outer shallow annular groove is located at a radius of 240–295 mm.

[0008] The bottom of the central shallow annular groove, the middle shallow annular groove, and the outer shallow annular groove are provided with 24, 36, and 48 through holes, respectively, with a diameter of 0.8 mm.

[0009] The fractal multi-scale annular microporous array is divided into an inner ring, a middle ring, and an outer ring. The aperture and pitch of the inner ring, middle ring, and outer ring are 60 μm and 300 μm, 80 μm and 350 μm, and 100 μm and 400 μm, respectively. The fractal microporous terminal plate is staggered by 1 / 2 pitch in the circumferential direction relative to the through holes of the corresponding shallow annular grooves in the inner ring, middle ring, and outer ring.

[0010] The flow coefficient of the primary throttling core is 0.01 to 0.20, the average pore size of the secondary porous medium is 10 to 30 μm, and the distribution and stabilizing ring cavity is equipped with opposing air inlets.

[0011] The multi-layer porous ceramic air film plate and the fractal microporous terminal plate are bonded together with an adhesive layer with a thickness of no more than 0.03 mm. The outer circle of the multi-layer porous ceramic air film plate and the annular step of the fixture body substrate are matched with H7 / g6, and three positioning pins are provided.

[0012] Leakage monitoring holes are installed between the gas supply channel and the first vacuum channel, the second vacuum channel, and the third vacuum channel. The exposed sharp edges of the fractal microporous terminal plate and the partitioned vacuum adsorption structure are rounded to R0.2 to R0.5.

[0013] An electrostatic-assisted initiation bonding assembly is installed below the central shallow annular groove, the middle shallow annular groove, and the outer shallow annular groove. The electrostatic-assisted initiation bonding assembly includes a dielectric layer and an inner ring electrode, a middle ring electrode, and an outer ring electrode in three concentric ring electrodes. The thickness of the dielectric layer is 0.2 to 0.8 mm. The electrostatic-assisted initiation bonding assembly is used to apply a voltage of no more than 1 kV to the inner ring electrode, the middle ring electrode, and the outer ring electrode during the initial stage of workpiece loading to assist workpiece bonding. After a preset time, the power is turned off, and the adsorption is maintained by the partitioned vacuum adsorption structure.

[0014] The outer edge of the fixture body base plate is provided with a circumferential Coanda air curtain nozzle ring. The circumferential Coanda air curtain nozzle ring is provided with a spray slit. The slit width is 0.05 to 0.20 mm, the incident angle is 10° to 25°, and the spray slit is recessed 0.10 to 0.30 mm relative to the workpiece bearing surface. The circumferential Coanda air curtain nozzle ring is connected to an external air source through an independent air inlet and is isolated from the air supply channel.

[0015] The fixture body base plate is made of stainless steel, the multi-layer porous ceramic air film plate is made of alumina or silicon carbide porous ceramic material, the fractal micro-hole terminal plate is made of stainless steel thin plate or ceramic thin plate material, the sealing ring is made of fluororubber material, and the workpiece bearing surface is jointly formed by the fractal micro-hole terminal plate and the opening surface of the partitioned vacuum adsorption structure. Within a diameter range of 300mm, the flatness is no greater than 0.01mm.

[0016] The beneficial effects of this utility model are: This application constructs a synergistic structure on the workpiece side, consisting of an isobaric gas film support layer, a fractal multi-scale annular microporous terminal plate, and three shallow annular groove partitioned vacuums flush with its working surface. This enables the gas supply to achieve a stable and uniform film thickness distribution in the plane. At the same time, without disrupting the continuity of the gas film, partitioned light suction is introduced to suppress edge roll-off and reduce the total thickness difference in the plane with an adjustable edge-center pressure curve. Specifically, the upper supply layer's orifice axis is radially inward, while the lower permeation layer's orifice axis is radially outward. Under steady-state gas supply, the two layers of orifices form radially opposite weak jets that counteract each other, weakening the common film pressure attenuation from the inside out. The terminal plate adopts a fractal micropore array with inner / middle / outer rings, with the pore diameter and pitch increasing from the inside out, enhancing the isotropic in-plane flow supply capacity. The opening surface of the shallow annular groove is on the same plane as the working surface of the terminal plate, with a flatness difference of no more than 0.01 mm. The through holes at the bottom of the groove and the micropores are staggered by half a pitch in the circumferential direction, avoiding the formation of a direct leakage channel and balancing the independence and synergy of adsorption and load-bearing. Through two-stage throttling and opposed-inlet pressure distribution, gas supply pulsation is effectively suppressed, and the fluctuation of gas film thickness over time is reduced. The gas supply channel and the three vacuum channels are isolated inside the body by a seal and labyrinth structure, maintaining a minimum clearance. Leakage monitoring holes are also provided to improve the sealing reliability and maintainability under long-term operation. Under typical operating conditions where the target film thickness is 5–20 μm, the above configuration can achieve an in-plane film thickness dispersion of no more than ±10%. Compared with the same diameter control structure, the fluctuation of the total in-plane thickness difference to the edge roughness ratio has an improvement space of no less than about 20%, and the risk of back scratches and step-like appearance is reduced simultaneously.

[0017] An electrostatically assisted initial bonding component is superimposed below three shallow annular grooves. During the initial wafer loading stage, a voltage not exceeding 1 kV is applied to the area covering the wafer, with the dielectric layer thickness ranging from 0.2 to 0.8 mm. This overlaps with the zoned vacuum switching on the order of 0.2 s, providing controllable bonding attraction before a steady-state vacuum is established, reducing relative slippage during the wafer loading stage and shortening bonding time. The zoned activation strategy applies an electrostatic field only to the annular area covered by the wafer, balancing energy consumption and safety margin. A circumferential Coanda air curtain nozzle ring is set on the outer edge of the fixture. The nozzle slit width, incident angle, and nozzle orifice subsidence are within a defined window. Independent air intake and isolation from the main air supply result in wall adhesion after the airflow exits, forming a continuous circumferential air curtain around the workpiece's outer edge. Under typical 0.3 MPa air supply conditions, the droplet count near the workpiece edge shows a decrease of at least approximately 30% compared to when the air curtain is not activated, effectively suppressing the inward diffusion of droplets and particles. The two enhancement functions, used in conjunction with the basic structure, further improve wafer mounting stability and processing cleanliness without altering the flush relationship of the bearing surface and the channel isolation boundary, facilitating more repeatable clamping and surface quality results in mass production environments. Overall, this application, without introducing a complex back pressure film, achieves uniform gas film, edge control, sealing safety, and convenient maintenance through a coupled design of hole-oriented anti-jamming, fractal micropores, and flush partitioned vacuum, making it suitable for grinding and polishing processes of sapphire wafers with a diameter of 200 mm and above. Attached Figure Description

[0018] Figure 1 This is an overall structural diagram of the present invention; Figure 2 For the present utility model Figure 1 Enlarged view at point F; Figure 3 This is a schematic diagram illustrating the use of this utility model; Figure 4 This is an exploded view of the entire utility model; Figure 5 This is a partial exploded view of the present invention; Figure 6 This is a front view of the present invention; Figure 7 For the present utility model Figure 6 Sectional view of AA; Figure 8 For the present utility model Figure 7 BB section view; Figure 9 For the present utility model Figure 7 Enlarged view at point C; Figure 10 This is a structural diagram of the present invention; Figure 11 For the present utility model Figure 8 Enlarged view at point D; Figure 12 For the present utility model Figure 8 Enlarged view of point E in the middle.

[0019] Explanation of the labels in the diagram 1. Fixture body substrate; 2. Two-stage throttling assembly; 3. Multi-layer porous ceramic air film plate; 4. Fractal microporous terminal plate; 5. Zoned vacuum adsorption structure; 6. Electrostatic assisted initial bonding assembly; 7. Circumferential Coanda air curtain nozzle ring; 21. Distribution and stabilizing ring cavity; 22. First-stage throttling core; 23. Second-stage porous medium; 24. Air inlet; 31. Upper supply layer; 32. Lower permeation layer; 51. Central shallow annular groove; 52. Middle shallow annular groove; 53. External shallow annular groove; 54. First vacuum channel; 55. Second vacuum channel; 56. Third vacuum channel; 61. Medium layer; 62. Inner ring electrode; 63. Middle ring electrode; 64. Outer ring electrode; 71. Spray slit; 72. Independent air inlet. Detailed Implementation

[0020] The technical solution of this utility model will be clearly and completely described below with reference to the embodiments. Obviously, the described embodiments are only some embodiments of this utility model, and not all embodiments. Based on the embodiments of this utility model, all other embodiments obtained by those skilled in the art without creative effort are within the protection scope of this utility model.

[0021] It should be noted that the directional concepts of "left", "right", "up", "down", "front", "back", "inner", and "outer" in the following scheme are all relative directions, and will not be listed one by one here.

[0022] Example 1 like Figures 1 to 12 As shown in the figure, this embodiment provides a specific implementation of a sapphire wafer grinding and polishing fixture. The fixture achieves high-precision clamping and support of the sapphire wafer through the synergistic effect of isobaric gas film support, fractal micro-hole terminal plate and three shallow groove partition vacuum.

[0023] The sapphire wafer grinding and polishing fixture of this embodiment includes a fixture body substrate 1 and a workpiece bearing surface disposed on the fixture body substrate 1. The fixture body substrate 1 is made of stainless steel, which has excellent corrosion resistance and mechanical strength. A distribution and stabilizing ring cavity 21 is provided inside the fixture body substrate 1. The distribution and stabilizing ring cavity 21 has an annular cavity structure and is used to receive external gas supply and perform preliminary pressure stabilization treatment.

[0024] Downstream of the distribution and stabilizing ring cavity 21, a primary throttling core 22 and a secondary porous medium 23 are sequentially arranged, together forming a two-stage throttling assembly 2. The primary throttling core 22 adopts a precision-machined throttling orifice structure with a flow coefficient of 0.15, performing the first-stage throttling and pressure reduction on the compressed air from the distribution and stabilizing ring cavity 21. The secondary porous medium 23 is made of porous metal or ceramic material with an average pore size of 20μm, achieving the second-stage throttling and uniform airflow distribution through its microporous structure. The design of the two-stage throttling assembly 2 eliminates air supply pulsation, stabilizes film thickness fluctuations, and achieves progressive pressure reduction and uniform distribution of airflow, providing stable air source conditions for subsequent film formation.

[0025] The pressure-stabilizing annular cavity 21 is equipped with opposing air inlets 24. The two air inlets 24 are arranged 180 degrees apart from each other in the circumferential direction of the annular cavity, ensuring that airflow enters the annular cavity from two directions simultaneously, avoiding the pressure unevenness problem that may be caused by single-point air intake. This opposing air intake design effectively improves the uniformity of pressure distribution within the annular cavity.

[0026] Downstream of the two-stage throttling component 2, a multi-layer porous ceramic film film plate 3 is connected from bottom to top. The multi-layer porous ceramic film film plate 3 is made of alumina porous ceramic material, possessing good air permeability and structural stability. The multi-layer porous ceramic film film plate 3 includes two functional layers: an upper supply layer 31 and a lower permeation layer 32. The inward inclination angle α1 of the pore axis of the upper supply layer 31 relative to the radial direction is set to 15 degrees. This inward design causes a centripetal convergence effect in the upper supply layer 31, which is beneficial for the concentration and uniform distribution of airflow. The outward inclination angle α2 of the pore axis of the lower permeation layer 32 relative to the radial direction is set to 10 degrees. This outward design causes a radial diffusion effect in the lower permeation layer 32, ensuring that the airflow can uniformly cover the entire bearing surface area.

[0027] The thickness ratio of the upper supply layer 31 to the lower seepage layer 32 is set to 1:1, meaning the two layers are of equal thickness. This ratio ensures both the airflow distribution function of the upper layer and the seepage buffering effect of the lower layer. Through the combination of channels with different inclination directions in the upper and lower layers, a smooth transition of airflow from concentrated to dispersed is achieved, forming a uniform and stable air film distribution.

[0028] The outer circle of the multi-layer porous ceramic air film disk 3 and the annular step of the fixture body substrate 1 are precisely fitted with H7 / g6 to ensure coaxiality and positioning accuracy between them. At the same time, three positioning pins are set, which are evenly distributed in the circumferential direction and spaced at 120 degrees to further ensure the precise positioning and anti-rotation of the multi-layer porous ceramic air film disk 3 and the fixture body substrate 1.

[0029] The upper surface of the multi-layer porous ceramic air film plate 3 is fully bonded with a fractal microporous terminal plate 4. The fractal microporous terminal plate 4 is made of stainless steel sheet material, has an annular thin plate structure, and forms part of the workpiece bearing surface. The fractal microporous terminal plate 4 has an outer diameter of 300mm, an inner diameter of 180mm, and a plate thickness of 2mm, which ensures both sufficient structural strength and good air permeability.

[0030] The multi-layer porous ceramic air film plate 3 and the fractal microporous terminal plate 4 are bonded together with an adhesive layer 93 with a thickness of no more than 0.03 mm. The adhesive layer 93 is made of high-temperature resistant structural adhesive, which can withstand temperature changes and mechanical stress during the grinding and polishing process. At the same time, its extremely thin design ensures unobstructed airflow channels.

[0031] The fractal microporous terminal plate 4 is equipped with a fractal multi-scale annular microporous array. This microporous array adopts the fractal geometry design concept and has multi-level and multi-scale pore size distribution characteristics. The fractal multi-scale annular microporous array is only distributed in the solid zone region of the concentric annular zone, avoiding the area where shallow grooves will be opened later, ensuring the integrity of the structure and the non-interference of functions.

[0032] Specifically, the fractal multi-scale annular micropore array is divided into three regions: an inner annular zone, a middle annular zone, and an outer annular zone. The pore diameter and pitch in the inner, middle, and outer annular zones are set to 60 μm and 300 μm, 80 μm and 350 μm, and 100 μm and 400 μm, respectively. This design of gradually increasing pore diameter and pitch from the inside out not only adapts to the airflow distribution requirements at different radial positions but also ensures the uniformity of the overall gas film pressure. The small pore diameter design of the inner annular zone is suitable for fine airflow control in the central region, while the large pore diameter design of the outer annular zone meets the requirement of sufficient airflow supply in the edge regions.

[0033] A partitioned vacuum adsorption structure 5 is provided on the fractal microporous terminal plate 4. This structure is a key component for achieving stable workpiece clamping. The partitioned vacuum adsorption structure 5 includes a central shallow annular groove 51, a middle shallow annular groove 52, and an outer shallow annular groove 53, which are independent of each other and are on the same plane as the upper surface of the fractal microporous terminal plate 4. The three shallow annular grooves are distributed radially in sequence, forming a concentric ring arrangement.

[0034] The central shallow annular groove 51 is located at a radius of 185–205 mm, with a depth of 0.35 mm and a width of 6.0 mm; the middle shallow annular groove 52 is located at a radius of 210–235 mm, with a depth of 0.35 mm and a width of 7.0 mm; and the outer shallow annular groove 53 is located at a radius of 240–295 mm, with a depth of 0.35 mm and a width of 8.0 mm. A 1.5 mm wide isolation rib is provided between adjacent shallow annular grooves. The presence of the isolation rib ensures the independence of vacuum adsorption in each area while maintaining the structural strength of the fractal microporous terminal plate 4.

[0035] Each shallow annular groove has uniformly arranged through holes at its bottom. The number of through holes in the central shallow annular groove 51, the middle shallow annular groove 52, and the outer shallow annular groove 53 are 24, 36, and 48 respectively, with a diameter of 0.8 mm and circumferentially equidistantly distributed. The three shallow annular grooves are connected to an external vacuum source through the first vacuum channel 54, the second vacuum channel 55, and the third vacuum channel 56 inside the fixture body base plate 1. The three vacuum channels are independently arranged inside the fixture body base plate 1, and each channel is equipped with an independent vacuum interface, which can realize regional vacuum control. This independent channel design allows different areas to adjust the vacuum adsorption force according to the specific size and shape of the workpiece, achieving precise zonal control.

[0036] The opening surface of the shallow annular groove is on the same plane as the upper surface of the terminal plate, and the flatness difference between the opening surfaces of the fractal microporous terminal plate 4 and the partitioned vacuum adsorption structure 5 is no greater than 0.01 mm. The micropores of the fractal microporous terminal plate 4 are arranged in a staggered phase relative to the through holes in the circumferential direction. Specifically, the inner ring is staggered by 7.5° relative to the through holes of the central shallow annular groove 51, the middle ring is staggered by 5° relative to the through holes of the middle shallow annular groove 52, and the outer ring is staggered by 3.75° relative to the through holes of the outer shallow annular groove 53, corresponding to half the pitch of the equiangular distribution of 24 / 36 / 48 holes, thereby avoiding the formation of a straight leakage path and homogenizing the film thickness.

[0037] The gas supply channel is formed by the distribution and stabilizing ring cavity 21, the two-stage throttling component 2, the multi-layer porous ceramic gas film disk 3, and the fractal microporous terminal plate 4. The gas supply channel is isolated from the first vacuum channel 54, the second vacuum channel 55, and the third vacuum channel 56 inside the fixture body base plate 1 by sealing rings. The closest net distance between the gas supply channel and any vacuum channel is 1.2 mm. Leakage monitoring holes are set between the gas supply channel and each vacuum channel and connected to pressure sensors for monitoring the sealing status. The sealing rings are made of fluororubber material, which has excellent chemical corrosion resistance and sealing performance.

[0038] The exposed sharp edges of the fractal microporous terminal plate 4 and the partitioned vacuum adsorption structure 5 are rounded to R0.3. This rounding design not only avoids scratching the sapphire wafer with sharp edges, but also facilitates the placement and removal of workpieces.

[0039] The workpiece bearing surface is jointly formed by the fractal micro-hole terminal plate 4 and the opening surface of the partitioned vacuum adsorption structure 5. Within a diameter range of 300mm, the flatness is controlled within 0.008mm, which meets the requirements of high-precision sapphire wafer processing.

[0040] The working process of this embodiment is as follows: First, compressed air is supplied to the distribution and stabilizing ring chamber 21 through the opposing air inlet 24, where the compressed air undergoes initial pressure stabilization and uniform distribution. Subsequently, the stabilized gas undergoes first-stage throttling and pressure reduction through the first-stage throttling core 22, which reduces the gas pressure from the supply pressure to an intermediate pressure level.

[0041] Next, the gas, after undergoing primary throttling, enters the secondary porous media 23, where it undergoes a second stage of throttling and further homogenization. Through the stepwise pressure reduction and flow regulation of the two-stage throttling, the gas entering the multi-layer porous ceramic film disc 3 is ensured to have stable pressure and uniform distribution.

[0042] The gas, after being processed by the two-stage throttling components 2, enters the lower permeation layer 32 of the multi-layer porous ceramic gas film disk 3. In the lower permeation layer 32, the gas diffuses radially through channels with an outward inclination angle α2 of 10 degrees, achieving uniform gas flow distribution. Subsequently, the gas enters the upper supply and distribution layer 31, where it converges and is finely distributed through channels with an inward inclination angle α1 of 15 degrees.

[0043] Finally, the treated gas is ejected through the fractal multi-scale annular micropore array on the fractal micropore terminal plate 4, forming a uniform and stable gas film on the workpiece bearing surface. The 60μm diameter micropores in the inner ring generate fine airflow, the 80μm diameter micropores in the middle ring generate medium airflow, and the 100μm diameter micropores in the outer ring generate sufficient airflow. The synergistic effect of the three rings forms an isotropically uniform gas film bearing.

[0044] Simultaneously, vacuum suction is applied to the central shallow annular groove 51, the middle shallow annular groove 52, and the outer shallow annular groove 53 through the first vacuum channel 54, the second vacuum channel 55, and the third vacuum channel 56, respectively. The 24, 36, and 48 through-holes in the three shallow annular grooves respectively transmit the vacuum suction, achieving a zoned gentle suction function. By adjusting the vacuum level of each vacuum channel, precise clamping with controllable edge-to-center pressure difference can be achieved according to the size and shape of the sapphire wafer.

[0045] When the sapphire wafer is placed on the workpiece support surface, the gas film support provides upward support, maintaining a small gap between the wafer and the support surface to avoid direct contact and wear. Simultaneously, the zoned vacuum adsorption structure 5 generates appropriate adsorption force through the central shallow annular groove 51, the middle shallow annular groove 52, and the outer shallow annular groove 53, ensuring stable positioning of the wafer. The synergistic effect of the gas film support and vacuum adsorption achieves damage-free, high-precision clamping of the sapphire wafer.

[0046] During the grinding and polishing process, the gas film support effectively isolates the wafer from direct contact with the fixture, preventing scratches or contamination on the back of the wafer. The fractal multi-scale annular micro-hole array design of the fractal micro-hole terminal board 4 ensures uniform distribution of gas film pressure, avoiding wafer deformation caused by excessively high or low local pressure. The partitioned vacuum adsorption structure 5 can automatically adjust the adsorption force distribution according to force changes during processing, maintaining a stable wafer clamping state.

[0047] Through the step-by-step pressure reduction and flow control of the two-stage throttling component 2, the airflow is precisely regulated and evenly distributed, providing a stable and reliable air source for the formation of the air film and significantly improving the uniformity and stability of the air film load.

[0048] The multi-layer porous ceramic air film plate 3 adopts a channel design with different inclination angles in the upper and lower layers. The inner inclination angle α1 of the upper supply layer 31 and the outer inclination angle α2 of the lower permeation layer 32 are matched to realize a smooth transition of airflow from concentration to dispersion, effectively eliminating the load-bearing capacity fluctuation caused by uneven airflow distribution and improving the uniformity of air film load-bearing.

[0049] The fractal multi-scale annular micropore array on the fractal micropore terminal plate 4 adopts a design with gradually increasing aperture and pitch from the inside to the outside. This not only adapts to the airflow distribution requirements at different radial positions but also ensures the uniformity of the overall air film pressure. The small aperture design of the inner ring enables precise airflow control in the central region, while the large aperture design of the outer ring ensures sufficient airflow supply to the edge region, significantly improving the problem that traditional single aperture designs cannot meet the needs of various regions.

[0050] The partitioned vacuum adsorption structure 5 achieves precise clamping with controlled edge-center pressure difference through independent control of the central shallow annular groove 51, the middle shallow annular groove 52, and the outer shallow annular groove 53, enabling partitioned gentle adsorption. The three independent vacuum channels allow different areas to adjust the vacuum adsorption force according to the specific size and shape of the sapphire wafer, avoiding the problems of localized over-adsorption or insufficient adsorption that may occur with traditional whole-area adsorption methods.

[0051] The micropores of the fractal microporous terminal plate 4 and the through holes of the partitioned vacuum adsorption structure 5 are arranged with a circumferential staggered spacing of 1 / 2 pitch, which effectively prevents vacuum leakage and optimizes the uniformity of gas film distribution. This staggered design avoids direct alignment of micropores and through holes, ensuring the independence and synergy of gas film bearing and vacuum adsorption functions.

[0052] The air supply channel and vacuum channel are isolated by a sealing ring inside the fixture body base plate 1, maintaining a minimum clearance of 1.2 mm to ensure complete separation of the two functional channels. The inclusion of a leakage monitoring hole enables real-time monitoring of the sealing status, improving the reliability and safety of the system.

[0053] The workpiece bearing surface is jointly formed by the fractal microporous terminal plate 4 and the opening surface of the partitioned vacuum adsorption structure 5. The flatness is controlled within 0.008mm within a diameter range of 300mm, providing an ideal bearing reference for the grinding and polishing of high-precision sapphire wafers.

[0054] Through the synergistic effect of the above-mentioned technical features, this embodiment achieves non-destructive, high-precision clamping of sapphire wafers, effectively avoiding wafer damage and deformation that may be caused by traditional mechanical clamping methods, and significantly improving the processing quality and efficiency of sapphire wafer grinding and polishing.

[0055] Example 2 like Figures 1 to 12 As shown in the figure, this embodiment provides a specific implementation of a reinforced sapphire wafer grinding and polishing fixture. This fixture further integrates an electrostatic assisted initial bonding component and a circumferential Coanda air curtain nozzle ring on the basic structure of Embodiment 1, thereby achieving a more complete workpiece clamping function and protection capability.

[0056] This embodiment fully reuses all the technical features and effects of the fixture body substrate 1, distribution and stabilizing ring cavity 21, two-stage throttling component 2, multi-layer porous ceramic gas film disk 3, fractal microporous terminal plate 4, and partitioned vacuum adsorption structure 5 from Embodiment 1, including the structural parameters, material selection, assembly relationship, and working principle of each component. Based on this, this embodiment adds two key functional components to further improve the fixture's process adaptability and reliability.

[0057] An electrostatic-assisted initial bonding assembly 6 is provided below the central shallow annular groove 51, the middle shallow annular groove 52, and the outer shallow annular groove 53. The electrostatic-assisted initial bonding assembly 6 is an auxiliary clamping device specifically designed for the initial stage of sapphire wafer mounting, which uses electrostatic attraction to assist in the initial bonding and positioning of the workpiece.

[0058] The electrostatically assisted initial bonding assembly 6 includes a dielectric layer 61 and a three-segment concentric ring electrode structure. The dielectric layer 61 is made of a high-insulation ceramic material with a thickness of 0.5 mm, ensuring both sufficient insulation strength and effective electrostatic field transmission. The upper surface of the dielectric layer 61 maintains good adhesion to the bottom of the groove of the partitioned vacuum adsorption structure 5, while the lower surface is in close contact with the electrode structure. The dielectric layer 61 radially covers the entire area of ​​the partitioned vacuum adsorption structure 5, ensuring a uniform distribution of the electrostatic field in each area.

[0059] The three concentric ring electrodes include an inner ring electrode 62, a middle ring electrode 63, and an outer ring electrode 64, corresponding to the positions of the central shallow ring groove 51, the middle shallow ring groove 52, and the outer shallow ring groove 53, respectively. The inner ring electrode 62 is located in a radius of 185–205 mm, precisely corresponding radially to the central shallow ring groove 51; the middle ring electrode 63 is located in a radius of 210–235 mm, precisely corresponding radially to the middle shallow ring groove 52; and the outer ring electrode 64 is located in a radius of 240–295 mm, precisely corresponding radially to the outer shallow ring groove 53. All three electrodes are made of highly conductive copper material, with a silver-plated surface to improve conductivity and oxidation resistance.

[0060] The inner ring electrode 62, middle ring electrode 63, and outer ring electrode 64 are radially insulated from each other. The electrode gap width is set to 2 mm, and insulating material is used to ensure the independence of each electrode. The thickness of each electrode is 1 mm, and the upper surface of the electrode is in close contact with the lower surface of the dielectric layer 61. The lower surface is connected to an external power control system via wires. The effective radial widths of the inner, middle, and outer ring electrodes are 18 mm, 23 mm, and 53 mm, respectively. Their radial positions correspond to the radial positions of the center, middle, and outer shallow ring grooves 51, 52, and 53, and they are located in the area below the bottom of each shallow ring groove to ensure that the electrostatic field in each area can completely cover the shallow groove area without exceeding the boundary.

[0061] The three concentric ring electrodes cover areas with radii of 185–205 mm, 210–235 mm, and 240–295 mm, respectively, for zoned activation corresponding to wafers of different diameters. For example, for a φ200 mm wafer, the inner ring electrode 62 and the middle ring electrode 63 are activated; for a φ210 mm wafer, the inner ring electrode 62, the middle ring electrode 63, and the outer ring electrode 64 are activated; for a φ230 mm wafer, all three electrodes 62, 63, and 64 are activated to achieve electrostatic attraction covering the effective area of ​​the wafer.

[0062] During the wafer mounting stage, the electrostatically assisted initial bonding assembly 6 applies a voltage of 600–800V to the electrodes covering the wafer area for 0.5–2 seconds, and activates the partitioned vacuum adsorption structure 5 0.2 seconds before power-off to achieve overlapping transition of clamping forces. The minimum insulation clearance between the dielectric layer 61 and any vacuum cavity wall or through-hole edge is ≥1.0mm; the electrode lead through-holes are encapsulated with epoxy and separated from the vacuum channel. Leakage current of each electrode is monitored and over-limit power-off is set.

[0063] A circumferential Coanda air curtain nozzle ring 7 is provided on the outer edge of the fixture body base plate 1. This component is a precision jetting device specifically designed to form a circumferential protective air curtain. The circumferential Coanda air curtain nozzle ring 7 utilizes the Coanda effect principle to form a continuous circumferential air curtain barrier through a high-speed airflow jet that adheres to the wall, effectively preventing droplets, particles, and contaminants generated during the grinding and polishing process from diffusing towards the center area of ​​the workpiece.

[0064] The Zhouxiang Coanda air curtain nozzle ring 7 adopts a precision-machined annular nozzle structure with an inner diameter of 302mm, an outer diameter of 320mm, and a height of 15mm. The nozzle ring is made of stainless steel, which has good corrosion resistance and machining accuracy. The nozzle ring is fixed to the outer edge step of the fixture body base plate 1 by bolts, and positioning accuracy is ensured by locating pins.

[0065] The circumferential Coanda air curtain nozzle ring 7 is provided with annular spray slits 71, which are continuously distributed circumferentially to form a 360-degree uninterrupted air jet channel. The slit width of the spray slits 71 is precisely controlled at 0.10 mm, and the incident angle of the spray slits 71 is 15° (the angle with the tangent of the workpiece bearing surface). After the airflow is ejected, it adheres to the outer wall of the nozzle ring and flows upward, forming a continuous circumferential air curtain at the outer edge of the workpiece.

[0066] The spray nozzle is recessed 0.20mm below the workpiece bearing surface and located outside the outer edge of the adapter ring. The minimum radial clearance between the inner lip of the spray nozzle and the outer edge of the adapter ring is ≥0.5mm to avoid assembly interference and ensure stable flow field against the wall.

[0067] The circumferential Coanda air curtain nozzle ring 7 connects to an external air source and is isolated from the air supply channel via an independent air inlet 72. The independent air inlet 72 is located at the bottom of the nozzle ring and uses a quick-connect coupling for easy connection and disconnection of the air source. The inner diameter of the air inlet 72 is 6mm, providing ample airflow. This independent air source design ensures complete separation of the air curtain function from the main air film bearing function, avoiding mutual interference.

[0068] An external air source regulates the air pressure to the working pressure range of 0.2–0.4 MPa via a pressure regulating valve. After passing through a precision filter to remove oil, water, and impurities, the air enters the circumferential Coanda air curtain nozzle ring 7. The airflow undergoes circumferential distribution and pressure stabilization within the annular cavity, and then is ejected at high speed through the spray slit 71 to form a continuous air curtain.

[0069] To ensure the isolation between the air curtain function and the main function, the air inlet channel of the circumferential Coanda air curtain nozzle ring 7 and the air supply channel in the fixture body base plate 1 are provided with double sealing of O-ring and labyrinth groove, and the closest net distance between the two is ≥1.0mm.

[0070] The working process of this embodiment adds two key steps to the first embodiment: electrostatic assisted bonding and air curtain protection. In the initial stage of sapphire wafer mounting, the electrostatically assisted initial bonding assembly 6 is first activated. Based on the wafer size, the corresponding electrode regions are activated, and an operating voltage of, for example, 600V (within the range of 600V to 800V) is applied to the inner ring electrode 62, middle ring electrode 63, and outer ring electrode 64. The electrostatic field acts on the wafer through a 0.5mm thick dielectric layer 61, generating an electrostatic attraction between the wafer and the carrier surface. This electrostatic attraction overcomes the weight of the wafer and the buoyancy of the gas film, allowing the wafer to quickly bond to the predetermined position.

[0071] The electrostatic attraction process lasts 1.5 seconds, during which the system monitors the bonding status of the wafer. When the position sensor detects that the wafer has been stably bonded, the electrostatic-assisted initial bonding component 6 is immediately de-energized to avoid any adverse effects on the wafer that may result from prolonged electrostatic action. After power de-energization, the central shallow annular groove 51, the middle shallow annular groove 52, and the outer shallow annular groove 53 of the partitioned vacuum adsorption structure 5 immediately initiate vacuum adsorption, providing a continuous and stable clamping force through the first vacuum channel 54, the second vacuum channel 55, and the third vacuum channel 56.

[0072] The switching process between electrostatic assistance and vacuum adsorption employs an overlapping control strategy, meaning that vacuum adsorption is initiated 0.2 seconds before the electrostatic discharge, ensuring a seamless transition of clamping force. This design avoids the problem of insufficient instantaneous clamping force that may occur during the switching process, guaranteeing the continuity and stability of wafer clamping.

[0073] During the grinding and polishing process, the circumferential Coanda air curtain nozzle ring 7 operates continuously, and 0.3MPa compressed air supplied through the independent air inlet 72 is ejected at high speed through the spray slit 71. Under the action of the Coanda effect, the high-speed airflow adheres to the outer wall of the nozzle ring and flows upward, forming a stable circumferential air curtain barrier at the edge of the workpiece.

[0074] The air curtain is approximately 5–8 mm thick and 15–20 mm high, effectively covering the edge area of ​​the sapphire wafer. When coolant droplets, grinding particles, and other contaminants generated during the grinding and polishing process diffuse toward the center of the workpiece, the airflow blocking effect generated by the circumferential air curtain deflects these harmful substances outward, preventing them from contacting the wafer surface and causing secondary contamination.

[0075] The continuity of the air curtain is ensured by a precise spray slit design (71). A slit width of 0.10 mm and an incident angle of 15 degrees ensure high-speed airflow and effective adhesion to the wall. The airflow velocity reaches 40–60 m / s, generating sufficient dynamic pressure to block the intrusion of most droplets and particles. Simultaneously, the air curtain provides continuous airflow flushing of the workpiece edge area, removing any potentially deposited contaminants. With an air supply of 0.3 MPa, the droplet count at the workpiece edge (5 mm) is reduced by ≥30% compared to when the air curtain is not in use; the maximum slippage during the loading stage is ≤50 μm (when electrostatic assistance is enabled).

[0076] The electrostatic-assisted initial bonding component 6 significantly improves the bonding performance of sapphire wafers. Traditional air-film carrier systems suffer from an imbalance between air film buoyancy and gravity during the initial stage of wafer loading, which may lead to unstable wafer suspension or misalignment of the bonding position. The electrostatic-assisted function, by applying controllable electrostatic attraction, can actively guide the wafer to quickly and accurately bond to the predetermined position, significantly shortening the wafer loading time and improving production efficiency.

[0077] The three-segment concentric ring electrode partition design allows the electrostatic assist function to adapt to sapphire wafers of different sizes, achieving effective assisted bonding for wafers with a diameter of 200mm and above. The partition activation strategy avoids applying unnecessary electrostatic fields to uncovered areas of the wafer, reducing energy consumption and improving safety.

[0078] The synergistic working mode of electrostatic assistance and vacuum adsorption achieves a smooth transition of clamping force. Electrostatic force provides rapid bonding in the initial stage of film loading, while vacuum adsorption provides stable clamping during subsequent processing. The organic combination of the two forces avoids the limitations of a single clamping method and significantly improves the reliability and adaptability of the overall clamping performance.

[0079] The circumferential Coanda air curtain nozzle ring 7 effectively solves the problem of workpiece contamination during the grinding and polishing process. Traditional fixtures lack effective edge protection measures, allowing grinding fluid droplets and grinding particles to easily diffuse onto the workpiece surface, causing secondary contamination and affecting processing quality. The Coanda air curtain utilizes the blocking and flushing effect of high-speed airflow to form an effective protective barrier around the workpiece, significantly reducing the probability of contaminants coming into contact with the workpiece.

[0080] The Coanda effect enables the air curtain to have excellent wall adhesion performance, allowing the airflow to flow stably upwards along the outer wall of the nozzle ring, forming a continuous and uniform protective air curtain. The optimized design of a 15-degree incident angle and a 0.20mm downward displacement ensures effective adhesion and upward expansion of the airflow, maximizing the protective effect.

[0081] The independent air source design ensures complete separation between the air curtain function and the main air-supported membrane function, avoiding mutual interference. The air curtain system can independently adjust airflow parameters according to the specific requirements of the processing technology, achieving customized protection configurations. At the same time, the independent system design facilitates maintenance and troubleshooting, improving the overall system reliability.

[0082] The formation of a continuous circumferential air curtain eliminates the blind spots that may exist in traditional point or segmented protection, achieving 360-degree full-coverage edge protection. This full-coverage design is particularly suitable for the processing of large-size sapphire wafers, ensuring that the entire wafer edge is effectively protected.

[0083] Through the synergistic effect of the electrostatically assisted initial bonding component 6 and the circumferential Coanda air curtain nozzle ring 7, this embodiment, while retaining all the advantages of Embodiment 1, further improves the convenience of workpiece loading and the cleanliness of the processing, providing a more complete and reliable fixture solution for the grinding and polishing of high-quality sapphire wafers. The overall system achieves an integrated design of clamping, bearing, and protection through multi-functional integration, significantly improving the process level and product quality of sapphire wafer processing.

[0084] The above description is merely a preferred embodiment of this utility model. It should be understood that this utility model is not limited to the forms disclosed herein and should not be construed as excluding other embodiments. It can be used in various other combinations, modifications, and environments, and can be altered within the scope of the concept described herein through the above teachings or related technologies or knowledge. Modifications and variations made by those skilled in the art that do not depart from the spirit and scope of this utility model should be protected within the scope of the appended claims.

Claims

1. A sapphire wafer grinding and polishing fixture, characterized in that: The fixture includes a fixture body base plate (1) and a workpiece bearing surface disposed on the fixture body base plate (1). A distribution and stabilizing ring cavity (21) is disposed in the fixture body base plate (1). A primary throttling core (22) and a secondary porous medium (23) are disposed sequentially downstream of the distribution and stabilizing ring cavity (21). The primary throttling core (22) and the secondary porous medium (23) together constitute a two-stage throttling assembly (2). The downstream of the two-stage throttling component (2) is connected to a multi-layer porous ceramic air film disk (3). The multi-layer porous ceramic air film disk (3) includes an upper supply layer (31) and a lower permeation layer (32). The relative radial inclination angle α1 of the hole axis of the upper supply layer (31) is 10° to 30°, and the relative radial outclination angle α2 of the hole axis of the lower permeation layer (32) is 5° to 20°. The thickness ratio of the upper supply layer (31) to the lower permeation layer (32) is 1:(0.5 to 1.5). The fractal microporous terminal plate (4) is fully bonded to the upper surface of the multi-layer porous ceramic air film disk (3). The fractal microporous terminal plate (4) is an annular thin plate and constitutes part of the workpiece bearing surface. A fractal multi-scale annular microporous array is provided on the fractal microporous terminal plate (4). The fractal multi-scale annular microporous array is only distributed in the solid zone area of ​​the concentric annular zone. The fractal microporous terminal plate (4) is provided with a partitioned vacuum adsorption structure (5). The partitioned vacuum adsorption structure (5) includes a central shallow annular groove (51), a middle shallow annular groove (52) and an outer shallow annular groove (53) that are independent of each other and flush with the upper surface of the fractal microporous terminal plate (4). Each shallow annular groove has a groove depth of 0.30 to 0.40 mm and a groove width of 6 to 8 mm. An isolation rib with a width of not less than 1.0 mm is provided between adjacent shallow annular grooves. Several through holes are uniformly provided at the bottom of each shallow annular groove. The central shallow annular groove (51), the middle shallow annular groove (52) and the outer shallow annular groove (53) are respectively connected to an external vacuum source through the first vacuum channel (54), the second vacuum channel (55) and the third vacuum channel (56) inside the fixture body substrate (1). The opening surfaces of the fractal microporous terminal plate (4) and the partitioned vacuum adsorption structure (5) are on the same plane, with a flatness difference of no more than 0.01 mm. The micropores of the fractal microporous terminal plate (4) are arranged in a staggered phase relative to the through holes in the circumferential direction. The distribution and stabilizing ring cavity (21), the two-stage throttling component (2), the multi-layer porous ceramic gas film disk (3) and the fractal microporous terminal plate (4) constitute an air supply channel. The air supply channel and the first vacuum channel (54), the second vacuum channel (55) and the third vacuum channel (56) are isolated inside the fixture body substrate (1) by a sealing ring. The closest net distance between the air supply channel and any vacuum channel is not less than 1.0 mm. The fixture forms an isotropically uniform air film bearing on the workpiece side, and achieves zoned light suction and controllable edge-center pressure difference through the central shallow annular groove (51), middle shallow annular groove (52) and outer shallow annular groove (53) which are flush with the fractal micro-hole terminal plate (4).

2. The sapphire wafer grinding and polishing fixture according to claim 1, characterized in that: The fractal microporous terminal plate (4) has an outer diameter of 300 mm and an inner diameter of 180 mm; the central shallow annular groove (51) is located at a radius of 185-205 mm, the middle shallow annular groove (52) is located at a radius of 210-235 mm, and the outer shallow annular groove (53) is located at a radius of 240-295 mm.

3. The sapphire wafer grinding and polishing fixture according to claim 1, characterized in that: The bottom of the central shallow annular groove (51), the middle shallow annular groove (52) and the outer shallow annular groove (53) are respectively provided with 24, 36 and 48 through holes, and the diameter of the through holes is 0.8 mm.

4. The sapphire wafer grinding and polishing fixture according to claim 1, characterized in that: The fractal multi-scale annular micropore array is divided into an inner annular zone, a middle annular zone, and an outer annular zone. The aperture and pitch of the inner annular zone, the middle annular zone, and the outer annular zone are 60 μm and 300 μm, 80 μm and 350 μm, and 100 μm and 400 μm, respectively. The fractal micropore terminal plate (4) is staggered by 1 / 2 pitch in the circumferential direction relative to the through holes of the corresponding shallow annular grooves in the inner annular zone, the middle annular zone, and the outer annular zone.

5. The sapphire wafer grinding and polishing fixture according to claim 1, characterized in that: The flow coefficient of the primary throttling core (22) is 0.01 to 0.20, the average pore size of the secondary porous medium (23) is 10 to 30 μm, and the distribution and stabilizing ring cavity (21) is provided with opposing air inlets (24).

6. The sapphire wafer grinding and polishing fixture according to claim 1, characterized in that: The multi-layer porous ceramic air film plate (3) and the fractal microporous terminal plate (4) are bonded together with an adhesive layer with a thickness of no more than 0.03 mm. The outer circle of the multi-layer porous ceramic air film plate (3) and the annular step of the fixture body substrate (1) are matched with H7 / g6, and three positioning pins are provided.

7. The sapphire wafer grinding and polishing fixture according to claim 1, characterized in that: Leakage monitoring holes are provided between the gas supply channel and the first vacuum channel (54), the second vacuum channel (55), and the third vacuum channel (56). The exposed sharp edges of the fractal microporous terminal plate (4) and the partitioned vacuum adsorption structure (5) are rounded to R0.2~R0.

5.

8. The sapphire wafer grinding and polishing fixture according to claim 1, characterized in that: Below the central shallow annular groove (51), the middle shallow annular groove (52), and the outer shallow annular groove (53), an electrostatic assisted initial bonding assembly (6) is provided. The electrostatic assisted initial bonding assembly (6) includes a dielectric layer (61) and an inner ring electrode (62), a middle ring electrode (63), and an outer ring electrode (64) in three concentric ring electrodes. The thickness of the dielectric layer (61) is 0.2 to 0.8 mm. The electrostatic assisted initial bonding assembly (6) is used to apply a voltage of no more than 1 kV to the inner ring electrode (62), the middle ring electrode (63), and the outer ring electrode (64) at the beginning stage of workpiece loading to assist workpiece bonding. After a preset time, the power is turned off, and the adsorption is maintained by the partitioned vacuum adsorption structure (5).

9. The sapphire wafer grinding and polishing fixture according to claim 1, characterized in that: The outer edge of the fixture body base plate (1) is provided with a circumferential Coanda air curtain nozzle ring (7). The circumferential Coanda air curtain nozzle ring (7) is provided with a spray slit (71). The slit width of the spray slit (71) is 0.05 to 0.20 mm, the incident angle is 10° to 25°, and the spray slit is recessed 0.10 to 0.30 mm relative to the workpiece bearing surface. The circumferential Coanda air curtain nozzle ring (7) is connected to an external air source through an independent air inlet (72) and is isolated from the air supply channel.

10. The sapphire wafer grinding and polishing fixture according to claim 1, characterized in that: The fixture body substrate (1) is made of stainless steel, the multi-layer porous ceramic air film disk (3) is made of alumina or silicon carbide porous ceramic material, the fractal microporous terminal plate (4) is made of stainless steel thin plate or ceramic thin plate material, the sealing ring is made of fluororubber material, and the workpiece bearing surface is jointly formed by the fractal microporous terminal plate (4) and the opening surface of the partitioned vacuum adsorption structure (5). Within a diameter range of 300mm, the flatness is not greater than 0.01mm.