Mould for producing autoclaved ceramsite board
By setting raised and recessed arrays on the mold for autoclaved alumina board production, combined with baffles and lifting cylinders, the problems of molds being unable to directly form patterns and uneven demolding force are solved, improving production efficiency and yield, and making it suitable for industrial production.
Patent Information
- Application Number
- CN202522767777.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2025-12-26
- Publication Date
- 2026-11-24
- Estimated Expiration
- 2035-12-26
AI Technical Summary
Existing autoclaved aerated concrete (AAC) board production molds cannot directly form surface textures, resulting in low production efficiency. Uneven stress during demolding can easily lead to board breakage, making it difficult to meet the needs of large-scale production.
A side mold frame with a raised array and a recessed array was designed, which, combined with baffles and lifting cylinders, enables automated demolding. Equipped with a vibrator and sealing gaskets, it ensures the slurry is dense and the texture is formed, avoiding hard friction.
It enables the formation of patterns without additional processing, improving yield and production efficiency, preventing board breakage, and making it suitable for industrial production.
Smart Images

Figure CN225010108U_ABST
Abstract
Description
Technical Field
[0001] This utility model relates to the field of building material production equipment technology, and in particular to a mold for producing autoclaved aerated concrete (AAC) boards. Background Technology
[0002] Autoclaved aerated concrete (AAC) boards, as a lightweight, high-strength, heat-insulating, and sound-insulating new type of environmentally friendly building material, are widely used in interior and exterior walls, floors, and other parts of buildings. In the production process, molds are one of the core pieces of equipment that determine the quality of the board forming and the production efficiency.
[0003] Currently, existing molds for producing autoclaved aerated concrete (AAC) boards have several shortcomings: First, most molds cannot directly form functional patterns on the surface of the AAC board, requiring additional milling, embossing, and other processing steps after the board is formed. This not only increases the production process and cost but also easily leads to board breakage and reduces the yield rate. Second, traditional molds are mostly integral structures, producing only one AAC board at a time, resulting in low production efficiency and difficulty in meeting the needs of large-scale production. Third, the mold closing and demolding processes mostly rely on manual or simple mechanical operations, which can easily lead to uneven stress during demolding, causing the edges of the AAC board to crack and the surface to be damaged, affecting product quality. Utility Model Content
[0004] To address the problems mentioned above, this utility model provides a mold for producing autoclaved aerated concrete (AAC) boards, which effectively solves the problems of traditional molds being unable to directly form functional textures on the surface of AAC boards, resulting in low production efficiency and uneven stress during demolding.
[0005] This utility model adopts the following technical solution: a mold for producing autoclaved aerated concrete (AAC) boards, including a base, a bottom mold frame fixedly connected to the top of the base, a side mold frame provided on the top of the bottom mold frame, and two opposing inner sidewalls of the side mold frame respectively provided with a raised array and a recessed array for forming the surface texture of the AAC board. The two inner sides of the side mold frame facing the mold cavity are fitted with evenly distributed baffles for dividing the mold cavity into multiple sub-mold cavities. Horizontal plates are provided on both outer sidewalls of the side mold frame. A lifting cylinder is installed on the top of the base below the horizontal plates. The output end of the lifting cylinder acts below the horizontal plates to drive the side mold frame to rise vertically and separate from the bottom mold frame. Vibrators are installed on both outer sidewalls of the side mold frame. Lifting ear plates are installed on the top of the outer sidewalls of the side mold frame. A top cover plate is provided on the top of the side mold frame, and multiple pre-embedded part insertion holes are opened on the top cover plate.
[0006] Furthermore, a sealing gasket is provided on the contact surface between the bottom mold frame and the side mold frame.
[0007] Furthermore, the vibrator is an attached flat plate vibrator, and is symmetrically distributed on both sides of the side mold frame.
[0008] Furthermore, the pre-embedded holes of the upper cover plate are fitted with replaceable wear-resistant bushings.
[0009] Furthermore, the surface of the baffle is coated with a release agent layer.
[0010] The advantages of this invention are as follows: By setting protrusion arrays and recessed arrays on the two opposing inner sidewalls of the side mold frame, the required texture can be directly pressed onto the surface of the ceramsite board during the molding process, eliminating the need for subsequent processing steps. This not only shortens the production cycle but also reduces the breakage rate of the boards during processing, increases the yield, and lowers the overall production cost. The side mold frame has evenly distributed grid plates inserted into the inner side facing the mold cavity, which can divide the mold cavity into multiple independent sub-cavities. Multiple ceramsite boards of the same specifications can be produced simultaneously with a single slurry injection, significantly improving production efficiency per unit time and adapting to industrial-scale production scenarios. The output end of the lifting cylinder acts on the horizontal plate, driving the side mold frame to rise vertically and smoothly and separate from the bottom mold frame, achieving automated demolding. Compared to traditional manual or simple mechanical demolding methods, this structure avoids hard friction and uneven stress between the mold and the board during demolding, effectively preventing edge cracking and surface scratches of the ceramsite board, ensuring the appearance quality and structural integrity of the finished board. Attached Figure Description
[0011] Figure 1 This is a schematic diagram of the structure of this utility model; Figure 2 This is a schematic diagram of the structure of this utility model.
[0012] In the figure, 1-base, 11-bottom mold frame, 2-side mold frame, 21-protrusion array, 22-recessed array, 3-grid plate, 4-horizontal plate, 5-lifting cylinder, 6-vibrator, 7-lifting ear plate, 8-top cover plate, 81-embedded part insertion hole. Detailed Implementation
[0013] To enable those skilled in the art to better understand the present invention, the technical solutions of the present invention will be clearly and completely described below with reference to the accompanying drawings of the embodiments. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort should fall within the protection scope of the present invention.
[0014] In the description of this utility model, it should be understood that the terms "longitudinal", "lateral", "length", "width", "thickness", "upper", "lower", "front", "rear", "left", "right", "vertical", "horizontal", "top", "bottom", "inner", and "outer" indicate the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings. They are only for the convenience of describing this utility model and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation. Therefore, they should not be construed as limitations on this utility model.
[0015] See Figure 1-2 As shown, a mold for producing autoclaved aerated concrete (AAC) boards includes a base 1, a bottom mold frame 11 fixedly connected to the top of the base 1, a side mold frame 2 on the top of the bottom mold frame 11, and two opposing inner side walls of the side mold frame 2 respectively provided with a raised array 21 and a recessed array 22 for forming the surface texture of the AAC board. The two inner sides of the side mold frame 2 facing the mold cavity are fitted with evenly distributed grid plates 3 for dividing the mold cavity into multiple sub-mold cavities. Horizontal plates 4 are provided on both outer side walls of the side mold frame 2. A lifting cylinder 5 is installed on the top of the base 1 below the horizontal plates 4. The output end of the lifting cylinder 5 acts below the horizontal plates 4 to drive the side mold frame 2 to rise vertically and separate from the bottom mold frame 11. Vibrators 6 are installed on both outer side walls of the side mold frame 2. Lifting ear plates 7 are installed on the top of the outer side walls of the side mold frame 2. An upper cover plate 8 is provided on the top of the side mold frame 2, and multiple embedded part insertion holes 81 are opened on the upper cover plate 8.
[0016] A sealing gasket is provided on the contact surface between the bottom mold frame 11 and the side mold frame 2 to prevent grout leakage and ensure product quality.
[0017] Vibrator 6 is an attached plate vibrator, symmetrically distributed on both sides of the side formwork frame 2. The attached plate vibrator can directly and extensively transmit vibration force to the side formwork frame 2, thereby efficiently acting on the concrete inside the formwork cavity. The symmetrical distribution ensures that the vibration force is transmitted synchronously and evenly from both sides of the plate, effectively avoiding problems such as uneven internal density and air bubbles concentrated on one side due to uneven vibration.
[0018] The embedded part insertion hole 81 of the upper cover plate 8 is fitted with a replaceable wear-resistant bushing. Frequent insertion and removal of the embedded part will cause serious wear to the inner wall of the insertion hole, resulting in the hole becoming larger and the positioning inaccurate. The wear-resistant bushing avoids this situation.
[0019] The surface of the baffle plate 3 is coated with a release agent layer to ensure smooth demolding and protect the slab.
[0020] Working principle: First, the bottom mold frame 11 is fixedly installed on the top of the base 1 to ensure that the bottom mold frame 11 is firmly connected to the base 1; a sealing gasket is laid on the contact surface between the bottom mold frame 11 and the side mold frame 2, and then the side mold frame 2 is precisely placed on top of the bottom mold frame 11 so that the side mold frame 2 and the bottom mold frame 11 fit tightly together, and the sealing gasket ensures the sealing performance between the two; according to the required specifications of the ceramsite board, the grid plate 3 coated with the release agent layer is evenly inserted into the inner side of the side mold frame 2 facing the mold cavity, dividing the mold cavity into multiple sub-mold cavities of the same specifications; finally, the top cover plate 8 is placed on top of the side mold frame 2 to complete the mold assembly. Autoclaved alumina slurry is evenly poured into each sub-mold cavity through the corresponding positions of the upper cover plate 8. Simultaneously, according to product design requirements, embedded parts are precisely inserted into the slurry through embedded part insertion holes 81 on the upper cover plate 8, achieving precise positioning and installation of the embedded parts. The wear-resistant bushings embedded in the embedded part insertion holes 81 prevent wear on the insertion holes during insertion and removal. The attached flat vibrators 6, installed on the outer side walls of the side mold frame 2, are activated. The vibration force generated by the vibrators 6 is transmitted to the slurry in the mold cavity through the side mold frame 2. Due to the symmetrical distribution of the vibrators 6, the vibration force is evenly applied to the slurry in each sub-mold cavity, ensuring thorough compaction of the slurry and expelling internal air bubbles. At the same time, the slurry fully adheres to the raised array 21 and recessed array 22 on the inner side of the side mold frame 2, forming the required texture on the surface of the board. After vibration is completed, the mold is kept closed, and the slurry is allowed to initially solidify and form. After the ceramsite slab has initially solidified, first remove the top cover plate 8, then activate the lifting cylinder 5 at the top of the base 1. The output end of the lifting cylinder 5 acts upward on the horizontal plates 4 on the outer side walls of the side mold frame 2, driving the side mold frame 2 to rise vertically and smoothly, separating the side mold frame 2 from the bottom mold frame 11 and the formed ceramsite slab. Subsequently, pull out the partition plates 3 separating the sub-mold cavities one by one. Since the surface of the partition plates 3 is coated with a release agent layer, they can be easily separated from the ceramsite slab. Finally, the formed autoclaved ceramsite slabs are removed from the bottom mold frame 11 by hoisting equipment or manually, completing a single production cycle. If the next round of production is required, simply repeat the above assembly, pouring, vibration, and demolding steps.
[0021] It will be apparent to those skilled in the art that this invention is not limited to the details of the exemplary embodiments described above, and that it can be implemented in other specific forms without departing from the spirit or essential characteristics of this invention. Therefore, the embodiments should be considered illustrative and non-limiting in all respects, and the scope of this invention is defined by the appended claims rather than the foregoing description. Thus, it is intended that all variations falling within the meaning and scope of equivalents of the claims be included within this invention. No reference numerals in the claims should be construed as limiting the scope of the claims.
[0022] Furthermore, it should be understood that although this specification describes embodiments, not every embodiment contains only one independent technical solution. This narrative style is merely for clarity. Those skilled in the art should consider the specification as a whole, and the technical solutions in each embodiment can also be appropriately combined to form other embodiments that can be understood by those skilled in the art.
Claims
1. A mold for the production of autoclaved ceramic granulate boards, comprising a base (1), characterized in that: The base (1) is fixedly connected to the top of a bottom mold frame (11), and a side mold frame (2) is provided on the top of the bottom mold frame (11). The two opposite inner sidewalls of the side mold frame (2) are respectively provided with a raised array (21) and a recessed array (22) for forming the surface texture of the ceramsite board. The two inner sides of the side mold frame (2) facing the mold cavity are fitted with evenly distributed baffles (3) for dividing the mold cavity into multiple sub-mold cavities. The outer two sidewalls of the side mold frame (2) are each provided with a horizontal plate (4). The base (1) is top... A lifting cylinder (5) is installed below the horizontal plate (4). The output end of the lifting cylinder (5) acts on the lower part of the horizontal plate (4) to drive the side mold frame (2) to rise vertically and separate from the bottom mold frame (11). Vibrators (6) are installed on both outer side walls of the side mold frame (2). Lifting ear plates (7) are installed on the top of the outer side walls of the side mold frame (2). An upper cover plate (8) is provided on the top of the side mold frame (2). Multiple pre-embedded part insertion holes (81) are opened on the upper cover plate (8).
2. The mold for producing autoclaved alumina boards according to claim 1, characterized in that: A sealing gasket is provided on the contact surface between the bottom mold frame (11) and the side mold frame (2).
3. The mold for producing autoclaved alumina boards according to claim 2, characterized in that: The vibrator (6) is an attached plate vibrator and is symmetrically distributed on both sides of the side mold frame (2).
4. The mold for producing autoclaved alumina boards according to claim 3, characterized in that: The pre-embedded insertion hole (81) of the upper cover plate (8) is fitted with a replaceable wear-resistant bushing.