Hot melt head assembly and hot melt device

By introducing a shaping component into the hot-melt head assembly, the problem of protrusion after hot melting was solved, improving the safety performance and production efficiency of the battery cell.

CN225010563UActive Publication Date: 2026-11-24SUNWODA MOBILITY ENERGY TECHNOLOGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202522569584.0
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2025-12-02
Publication Date
2026-11-24
Estimated Expiration
2035-12-02

AI Technical Summary

Technical Problem

Traditional hot-melt head designs are prone to forming protrusions after hot melting, leading to decreased cell performance and insulation failure.

Method used

A hot melt head assembly is used, including a hot melt column and a shaping component. The hot melt point is shaped by the movement of the shaping component after hot melting, which reduces the protrusion height and improves the peel strength.

Benefits of technology

It effectively reduces the protrusion around the hot melting point, improves the safety performance and peel strength of the battery cell, shortens the production cycle, and improves the automation level of the production line.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN225010563U_ABST
    Figure CN225010563U_ABST
Patent Text Reader

Abstract

This application provides a hot-melt head assembly and a hot-melt device, relating to the field of battery cell manufacturing technology. The hot-melt head assembly includes: a hot-melt column, with a first end face disposed at one axial end; a shaping member, movable axially relative to the hot-melt column; a second end face disposed on the side of the shaping member near the first end face; the shaping member has a first position and a second position; when the shaping member is in the first position, there is an axial gap between the second end face and the first end face; when the shaping member is in the second position, the second end face coincides with the first end face. The hot-melt head assembly of this application can achieve a shaping effect on the hot-melt point, reduce the protrusion around the hot-melt point, improve the peel strength of the hot-melt point, and improve the safety performance of the battery cell.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This application relates to the field of battery cell manufacturing technology, and in particular to a hot melt head assembly and a hot melt device. Background Technology

[0002] During the battery cell manufacturing process, an insulating film is usually wrapped around the outside of the bare battery cell. The insulating film is first heat-fused to the bottom plate and then heat-fused to the plastic under the top cover.

[0003] Traditional hot-melt head designs typically use independent hot-melt heads. After hot-melt, a 0.3 mm to 0.7 mm protrusion is easily formed around the hot-melt point. When the internal space of the battery cell is compact, the protrusion will compress the bottom of the battery cell, forming an indentation, which will lead to a decrease in battery cell performance. At the same time, the stress concentration at the protrusion will reduce the peel strength at the hot-melt point, causing the insulation film to fall off and resulting in insulation failure. Utility Model Content

[0004] In view of the above problems, this application provides a hot melt head assembly and a hot melt device to solve the problem that after the hot melt head in the prior art is hot melted, it is easy to form a protrusion around the hot melt point, which leads to the degradation of cell performance and insulation failure.

[0005] To achieve the above objectives, the embodiments of this application provide the following technical solutions:

[0006] A first aspect of this application provides a hot melt head assembly, comprising:

[0007] A hot melt column, with a first end face provided at one axial end;

[0008] The shaping component is capable of moving axially relative to the hot melt column; a second end face is provided on the side of the shaping component near the first end face; the shaping component has a first position and a second position; when the shaping component is in the first position, there is an axial gap between the second end face and the first end face; when the shaping component is in the second position, the second end face coincides with the first end face.

[0009] In one possible implementation, there are multiple hot melt pillars, which are spaced apart; the pillars are projected axially onto the plane of the forming part, and the projection of any hot melt pillar is located within the projection area of ​​the forming part.

[0010] In one possible implementation, projections are made along the axial direction onto the plane where the forming part is located, and the projections of multiple hot melt pillars are arranged in a rectangular, circular, racetrack-shaped, or elliptical array.

[0011] The second end face is a continuous plane that matches the array arrangement.

[0012] In one possible implementation, the forming part is provided with distribution holes, and the hot melt column is clearance-fitted with the distribution holes.

[0013] In one possible implementation, the hot melt head assembly further includes a housing, the housing including a first wall connected to the end of the hot melt column away from the first end face, the first wall being used to drive the hot melt column to move axially.

[0014] In one possible implementation, the outer shell further includes a second wall that is circumferentially disposed around the edge of the first wall, and the second wall and the first wall together enclose the first cavity; the hot-melt column and the shaping component are built into the first cavity.

[0015] In one possible implementation, the hot melt head assembly further includes a connecting rod connected to the shaping part, the connecting rod being used to drive the shaping part to move axially.

[0016] In one possible implementation, the housing further includes a third wall body connected to the first wall body;

[0017] The third wall ring is assembled to form a second cavity, which is connected to the first cavity; the connecting rod is coaxially arranged with the second cavity;

[0018] One axial end of the connecting rod passes through the second cavity and extends into the first cavity to connect with the shaping component.

[0019] In one possible implementation, the housing further includes a fourth wall, which is angled to the third wall;

[0020] A limiting element is provided at the end of the connecting rod away from the shaping part along the axial direction. When the shaping part is in the second position, the limiting element abuts against the fourth wall.

[0021] A second aspect of this application provides a hot-melt apparatus, including the hot-melt head assembly as described above.

[0022] The hot-melt head assembly provided in this application mainly includes a hot-melt column and a shaping component. The hot-melt column has a hot-melt function, and the shaping component has a shaping function. When the hot-melt column hot-melts and fixes the insulating film and the base plate, the first end face of the hot-melt column contacts the insulating film. At this time, the shaping component is in the first position, and there is a gap between the second end face and the first end face along the axial direction Y. After the hot-melt column completes the hot-melt process of the insulating film, the first end face of the hot-melt column remains in contact with the insulating film, and the shaping component moves along the axial direction to the second position, where the second end face coincides with the first end face. This achieves the shaping effect of the hot-melt point, reduces the protrusion around the hot-melt point, and improves the peel strength of the hot-melt point while enhancing the safety performance of the battery cell.

[0023] In addition to the technical problems solved by the embodiments of this application, the technical features constituting the technical solutions, and the beneficial effects brought about by the technical features of these technical solutions described above, other technical problems that can be solved by the hot melt head assembly and hot melt device provided by the embodiments of this application, other technical features included in the technical solutions, and the beneficial effects brought about by these technical features will be further explained in detail in the specific implementation. Attached Figure Description

[0024] To more clearly illustrate the technical solutions in the embodiments of this application or the prior art, the drawings used in the description of the embodiments or the prior art will be briefly introduced below. Obviously, the drawings described below are some embodiments of this application. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.

[0025] Figure 1 This is a schematic diagram of the assembly structure of the hot melt head assembly provided in the first embodiment of this application, wherein the shaping component is in the first position;

[0026] Figure 2 for Figure 1 A magnified view of a portion of point A in the middle;

[0027] Figure 3 for Figure 1 A schematic diagram of the arrangement of the hot melt columns in the hot melt head assembly shown;

[0028] Figure 4 A schematic diagram showing the arrangement of the hot melt columns in the hot melt head assembly provided in the second embodiment of this application;

[0029] Figure 5 A schematic diagram showing the arrangement of the hot melt columns in the hot melt head assembly provided in the third embodiment of this application;

[0030] Figure 6 This is a schematic diagram showing the arrangement of the hot melt columns in the hot melt head assembly provided in the fourth embodiment of this application;

[0031] Figure 7 A schematic diagram of the axial projection shape of the first wall of the hot melt head assembly provided in the fifth embodiment of this application;

[0032] Figure 8 A schematic diagram of the axial projection shape of the first wall of the hot melt head assembly provided in the sixth embodiment of this application;

[0033] Figure 9 A schematic diagram of the axial projection shape of the first wall of the hot melt head assembly provided in the seventh embodiment of this application;

[0034] Figure 10This is a schematic diagram of the assembly structure of the hot melt head assembly provided in the first embodiment of this application, wherein the shaping component is located in the second position.

[0035] Explanation of reference numerals in the attached figures:

[0036] 10. Hot melt column; 11. First end face; 20. Shaping part; 201. Distribution hole; 21. Second end face; 30. Outer shell; 301. First cavity; 302. Second cavity; 31. First wall; 32. Second wall; 33. Third wall; 34. Fourth wall; 40. Connecting rod; 50. Limiting part; Y, Axial direction. Detailed Implementation

[0037] First, those skilled in the art should understand that these embodiments are merely for explaining the technical principles of this application and are not intended to limit the scope of protection of this application. Those skilled in the art can make adjustments as needed to adapt to specific application scenarios.

[0038] Secondly, it should be noted that, in the description of the embodiments of this application, unless otherwise explicitly specified and limited, the terms "connected" and "linked" should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral connection; they can refer to a mechanical connection or an electrical connection; they can refer to a direct connection or an indirect connection through an intermediate medium; and they can refer to the internal connection of two components. Those skilled in the art can understand the specific meaning of the above terms in the embodiments of this application according to the specific circumstances.

[0039] As described in the background section, the hot melt head in the related technology is prone to forming protrusions around the hot melt point after hot melting, which leads to a decrease in cell performance and insulation failure. The inventors have found that the reason for this problem is that the hot melt head design in the related technology is usually an independent hot melt head, which is fixed only by hot melting and lacks subsequent shaping steps, resulting in an uneven welding area.

[0040] To address the aforementioned technical problems, this application provides a hot melt head assembly and a hot melt device. The hot melt head assembly includes: a hot melt column, with a first end face provided at one axial end; a shaping member, capable of moving axially relative to the hot melt column; a second end face provided on the side of the shaping member close to the first end face; the shaping member having a first position and a second position; when the shaping member is in the first position, there is an axial gap between the second end face and the first end face; when the shaping member is in the second position, the second end face coincides with the first end face.

[0041] The hot-melt head assembly provided in this application mainly includes a hot-melt column and a shaping component. The hot-melt column has a hot-melt function, and the shaping component has a shaping function. When the hot-melt column hot-melts and fixes the insulating film and the base plate, the first end face of the hot-melt column contacts the insulating film. At this time, the shaping component is in the first position, and there is a gap between the second end face and the first end face along the axial direction Y. After the hot-melt column completes the hot-melt process of the insulating film, the first end face of the hot-melt column remains in contact with the insulating film, and the shaping component moves along the axial direction to the second position, where the second end face coincides with the first end face. This achieves the shaping effect of the hot-melt point, reduces the protrusion around the hot-melt point, and improves the peel strength of the hot-melt point while enhancing the safety performance of the battery cell.

[0042] To make the above-mentioned objectives, features, and advantages of the embodiments of this application more apparent and understandable, the technical solutions of the embodiments of this application will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only a part of the embodiments of this application, and not all of them. All other embodiments obtained by those skilled in the art based on the embodiments of this application without creative effort are within the scope of protection of this application.

[0043] Please refer to Figure 1-10 The first aspect of this application provides a hot melt head assembly, including:

[0044] A hot melt column 10, with a first end face 11 provided at one end of the axial Y direction;

[0045] The shaping component 20 is movable relative to the hot melt column 10 along the axial direction Y; the shaping component 20 is provided with a second end face 21 on the side near the first end face 11; the shaping component 20 has a first position and a second position; when the shaping component 20 is in the first position, there is a gap between the second end face 21 and the first end face 11 along the axial direction Y; when the shaping component 20 is in the second position, the second end face 21 coincides with the first end face 11.

[0046] The hot-melt head assembly provided in this application mainly includes a hot-melt column 10 and a shaping component 20. The hot-melt column 10 has a hot-melt function, and the shaping component 20 has a shaping function. When the hot-melt column 10 hot-melts and fixes the insulating film and the base plate, the first end face 11 of the hot-melt column 10 contacts the insulating film. At this time, the shaping component 20 is in the first position, and there is a gap between the second end face 21 and the first end face 11 along the axial direction Y. After the hot-melt column 10 completes the hot-melt process of the insulating film, the first end face 11 of the hot-melt column 10 remains in contact with the insulating film, and the shaping component 20 moves along the axial direction Y to the second position, where the second end face 21 coincides with the first end face 11, thereby achieving the shaping effect of the hot-melt point, reducing the protrusion around the hot-melt point, improving the peel strength of the hot-melt point, and improving the safety performance of the battery cell.

[0047] Furthermore, the hot melt column 10 can be a cylinder or frustum with an outer diameter φ of 0.1 mm to 1 mm and a height of 0.2 mm to 2 mm. The outer diameter and height of the hot melt column 10 can be flexibly adjusted within the range to adapt to the hot melt requirements of different models of micro cells. The material of the hot melt column 10 can be selected from tungsten copper or other copper alloys, taking into account both thermal conductivity and strength, thereby shortening the hot melt time, improving production efficiency, and ensuring the mechanical stability of the hot melt column 10.

[0048] Furthermore, the thickness of the shaping part 20 can be 0.1 mm to 1.9 mm, so as to match the height of the hot melt column 10 and ensure the shaping effect.

[0049] In one possible implementation, when the shaping part 20 is in the first position, the first end face 11 contacts the insulating film, and the hot melt column 10 begins to heat up;

[0050] When the forming part 20 is in the second position, the hot melt column 10 stops heating;

[0051] The first end face 11 and the second end face 21 remain in contact with the insulating film for a period of time, and the residual heat of the hot melt column 10 is used to reshape the hot melt point.

[0052] In this embodiment, the hot-melt column 10's hot-melt and shaping process mainly includes three stages: The first stage is the hot-melt stage, where the shaping component 20 is in the first position, and there is a gap between the second end face 21 and the first end face 11 along the axial direction Y. The hot-melt column 10 contacts the insulating film and begins to heat, completing the hot-melt process; The second stage is the transition stage, where the shaping component 20 moves along the axial direction Y to the second position, and the second end face 21 coincides with the first end face 11, and the hot-melt column 10 stops heating; The third stage is the shaping stage, where the second end face 21 and the first end face 11 remain in contact with the insulating film for a period of time, using residual heat to shape the hot-melt point, thereby achieving the shaping effect of the hot-melt point. This not only improves the hot-melt effect, reduces the risk of insulating film detachment, and improves the yield, but also reduces the height of the hot-melt point protrusion, improving the cell safety performance.

[0053] In addition, the integrated design of the three-stage process (hot melting-transition-shaping) eliminates the need for additional shaping steps, thereby shortening the production cycle, reducing manual intervention, improving the automation level of the production line, and reducing energy consumption through waste heat shaping.

[0054] In one possible implementation, please see Figure 1 As shown, there are multiple hot melt columns 10, which are spaced apart; please refer to [link / reference]. Figure 2 As shown, projections are made along the axial direction Y onto the plane where the forming part 20 is located, and the projection of any hot melt column 10 is located within the projection area of ​​the forming part 20.

[0055] In this embodiment, the projection of any hot melt pillar 10 is located within the projection area of ​​the shaping component 20, thereby ensuring that the position of the hot melt pillar 10 in the axial Y direction is completely covered by the shaping component 20, ensuring that the shaping component 20 can shape all hot melt points, improving the hot melt point peel strength, and improving the battery cell safety performance.

[0056] In one possible implementation, the projection along the axial direction onto the plane where the forming part 20 is located is arranged in a rectangular, circular, racetrack-shaped or elliptical array.

[0057] The second end face 21 is a continuous plane that matches the array arrangement.

[0058] In this embodiment, the hot-melt pillars 10 are arranged in an array according to a shape profile that matches the shape and structure of the battery cell. For example, this allows the hot-melt action point to closely match the area to be fixed, helping to achieve a more uniform stress distribution and avoiding local stress concentration. The second end face 21 is a continuous plane that matches the array arrangement. This not only ensures that the pressure acting on the entire hot-melt area of ​​the insulating film is evenly distributed, allowing all hot-melt points to be shaped simultaneously under the same pressure, thereby obtaining a highly consistent, flat, and smooth shaped surface and avoiding uneven protrusions caused by uneven pressure, but also that the continuous plane can form a strong constraint zone for the insulating film around the hot-melt point. When the material softens due to heat, this constraint can effectively inhibit the uncontrolled flow and accumulation of material to the periphery, forcing excess material to fill and flatten more evenly inward under pressure, thereby effectively reducing or even eliminating the protrusion height around the hot-melt point.

[0059] In one possible implementation, please see Figure 2 and Figure 3 As shown, the forming part 20 is provided with a distribution hole 201, and the hot melt column 10 is clearance-fitted with the distribution hole 201.

[0060] In this embodiment, by providing a distribution hole 201 on the shaping component 20, the hot melt column 10 is fitted with the distribution hole 201 with a clearance, thereby providing guidance for the hot melt column 10 through the distribution hole 201, preventing the hot melt column 10 from deviating during movement, ensuring that the first end face 11 of the hot melt column 10 is always in contact with the insulating film at a set angle, and improving the accuracy of hot melting of the insulating film and shaping of the hot melt point.

[0061] In one possible implementation, please see Figure 1 As shown, the hot melt head assembly also includes a housing 30, which includes a first wall 31. The first wall 31 is connected to the end of the hot melt column 10 away from the first end face 11. The first wall 31 is used to drive the hot melt column 10 to move along the axial direction Y.

[0062] In this embodiment, the outer shell 30 serves as the carrier for the movement of the hot melt column 10. The hot melt column 10 is fixed to the first wall 31 of the outer shell 30. Through the rigid constraint of the first wall 31, the hot melt column 10 is ensured to move linearly along the axial Y direction, preventing the hot melt column 10 from tilting or deviating during movement. This ensures that the first end face 11 of the hot melt column 10 is always in contact with the insulating film at a set angle, and maintains the synchronicity of the movement of multiple hot melt columns 10. This ensures that the hot melting of the insulating film and the shaping of the hot melt point are regular and consistent in depth, which is beneficial to improving the product yield.

[0063] In one possible implementation, please see Figure 1 As shown, the outer shell 30 also includes a second wall 32, which is circumferentially arranged around the edge of the first wall 31. The second wall 32 and the first wall 31 together enclose the first cavity 301; the hot melt column 10 and the shaping part 20 are built into the first cavity 301.

[0064] In this embodiment, the outer shell 30 is enclosed by the second wall 32 and the first wall 31 to form the first cavity 301. The second wall 32 and the first wall 31 form a physical barrier to isolate the hot melt column 10 and the shaping part 20 from the external environment, which can protect the hot melt column 10 and the shaping part 20 and prevent other components from interfering with or damaging the hot melt column 10 and the shaping part 20, thus ensuring the reliability of the equipment operation. At the same time, it can prevent external foreign objects from contaminating the hot melt column 10 and the shaping part 20, ensuring the cleanliness of the hot melt column 10 and the shaping part 20 and ensuring the stability of the hot melt and shaping process.

[0065] In one possible implementation, please see Figure 1 As shown, the hot melt head assembly also includes a connecting rod 40, which is connected to the shaping part 20. The connecting rod 40 is used to drive the shaping part 20 to move along the axial direction Y.

[0066] In this embodiment, the connecting rod 40 serves as the carrier for the movement of the shaping component 20. The connecting rod 40 is fixed to the shaping component 20, and the rigid constraint ensures that the shaping component 20 moves linearly along the axial Y direction. On the one hand, this ensures that the second end face 21 of the shaping component 20 can simultaneously and uniformly contact all the hot melt points to achieve flat pressing. On the other hand, it ensures that the guiding and pressing effects of the distribution holes 201 on all the hot melt pillars 10 occur simultaneously, making the shaping force on the entire insulating film surface highly consistent, thereby obtaining a uniform and flat welding surface, achieving synchronous shaping, and thus ensuring the absolute flatness and synchronicity of the shaping action.

[0067] In this embodiment, the connecting rod 40 is controlled by an independent drive source (such as another cylinder or electric cylinder), so that its movement is completely decoupled from the movement of the outer shell 30 of the hot melt column 10. In the "hot melt-transition-shaping" process, specifically: Hot melt stage: The connecting rod 40 is raised to keep the shaping part 20 in a high position; the first wall 31 drives the hot melt column 10 to descend to complete the hot melt; Transition stage: The connecting rod 40 independently drives the shaping part 20 to descend precisely to a position flush with the end face of the hot melt column 10; Shaping stage: The connecting rod 40 and the first wall 31 together maintain pressure as a whole and use residual heat for shaping, so that the three-stage process of "hot melt-transition-shaping" can be accurately realized. Moreover, the independent control of the connecting rod 40 allows the pressing speed, pressure and action time of the shaping part 20 to be individually adjusted and optimized to adapt to insulating films of different materials and thicknesses and obtain better shaping effect.

[0068] Furthermore, the rigid design of the connecting rod 40 provides a strong reaction force fulcrum for the shaping stage, avoiding pressure loss or unevenness caused by the flexible deformation of the rod itself, and ensuring that the design pressure is accurately and completely transmitted to the shaping part 20.

[0069] In one possible implementation, please see Figure 1 As shown, the outer casing 30 also includes a third wall 33, which is connected to the first wall 31;

[0070] The third wall 33 surrounds the second cavity 302, which is connected to the first cavity 301; the connecting rod 40 is coaxially arranged with the second cavity 302.

[0071] One end of the connecting rod 40 passes through the second cavity 302 and extends into the first cavity 301 to connect with the shaping component 20.

[0072] It should be noted that during the three-stage process of "hot melting-transition-shaping", even a slight deviation can cause the distribution holes of the shaping part 20 to misalign with the hot melting column 10, resulting in wear of the column body of the friction hot melting column 10, or failure to accurately press onto the hot melting point, leading to uneven shaping pressure and thus damaging the shaping effect.

[0073] In this embodiment, the connecting rod 40 and the second cavity 302 are coaxially arranged. The inner wall of the second cavity 302 and the outer diameter of the connecting rod 40 can form a sliding pair, thereby guiding the connecting rod 40 through the second cavity 302. On the one hand, this ensures that the connecting rod 40 moves strictly and uniquely along the axial Y direction, preventing the shaping component 20 from shaking, shifting, or twisting during movement. It also ensures the precise alignment of the distribution holes 201 of the shaping component 20 with the hot melt column 10, thereby improving the accuracy of hot melting of the insulating film and shaping of the hot melt point. On the other hand, during the shaping stage, when the shaping component 20 presses against the insulating film, a small lateral force may be generated due to the unevenness of the insulating film surface. The cooperation between the second cavity 302 and the connecting rod 40 provides a strong radial support for the connecting rod 40, thereby enhancing the system's resistance to lateral loads, avoiding jamming and wear, and helping to ensure the service life of the system.

[0074] In one possible implementation, please see Figure 10 As shown, the outer casing 30 also includes a fourth wall 34, which is angled to the third wall 33;

[0075] A limiting member 50 is provided at one end of the connecting rod 40 away from the shaping member 20 along the axial direction. When the shaping member 20 is in the second position, the limiting member 50 abuts against the fourth wall 34.

[0076] In this embodiment, the limiting member 50 abuts against the fourth wall 34, thereby providing a forced and reliable limit for the movement endpoint of the shaping member 20. This not only avoids damage to the shaping member 20 caused by direct limiting, ensuring the shaping accuracy of the shaping member 20, but also ensures the repeatability of the positioning accuracy for each shaping action. No matter how many times the equipment runs, when the limiting member 50 abuts against the fourth wall 34, the shaping member 20 is in the same second position, thereby providing completely consistent shaping pressure and flatness for each product, effectively improving the consistency of product yield.

[0077] In one possible implementation, projection is performed along the Y-axis; see [link to relevant documentation]. Figure 3 , Figure 7 , Figure 8 and Figure 9 As shown, the projected shape profile of the first wall 31 is adjustable; the projected shape profile of the first wall 31 can be... Figure 3 The rectangle shown can also be Figure 7 The circle shown can also be Figure 8 The ellipse shown can also be Figure 9The track shape shown; the projection shape contour of the shaping component 20 is adjustable. The projection shape contour of the shaping component 20 and the arrangement of the hot melt pillars 10 are adjusted with the projection shape contour of the first wall 31, so that the hot melt head assembly can adapt to a variety of battery cell shapes without customized design, improve the versatility of the hot melt head assembly, and help reduce production costs.

[0078] A second aspect of this application also provides a hot-melting apparatus, including the hot-melt head assembly as described above.

[0079] In this embodiment of the hot-melt device, by employing the aforementioned hot-melt head assembly, when the hot-melt column 10 hot-melts and fixes the insulating film and the base plate, the first end face 11 of the hot-melt column 10 contacts the insulating film. At this time, the shaping component 20 is in the first position, and there is a gap between the second end face 21 and the first end face 11 along the axial direction Y. After the hot-melt column 10 completes the hot-melt process on the insulating film, the first end face 11 of the hot-melt column 10 remains in contact with the insulating film, and the shaping component 20 moves along the axial direction Y to the second position, where the second end face 21 coincides with the first end face 11. This achieves the shaping effect of the hot-melt point, reduces the protrusion around the hot-melt point, and improves the peel strength of the hot-melt point while enhancing the safety performance of the battery cell.

[0080] The various embodiments or implementation methods described in this specification are presented in a progressive manner. Each embodiment focuses on the differences from other embodiments, and the same or similar parts between the embodiments can be referred to each other.

[0081] It should be noted that the terms "one embodiment," "embodiment," "exemplary embodiment," "some embodiments," etc., mentioned in the specification indicate that the described embodiment may include a specific feature, structure, or characteristic, but not every embodiment necessarily includes that specific feature, structure, or characteristic. Furthermore, such phrases do not necessarily refer to the same embodiment. Moreover, when a specific feature, structure, or characteristic is described in connection with an embodiment, implementing such a feature, structure, or characteristic in conjunction with other embodiments, whether explicitly described or not, is within the knowledge scope of those skilled in the art.

[0082] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of this application, and are not intended to limit them. Although this application has been described in detail with reference to the foregoing embodiments, those skilled in the art should understand that modifications can still be made to the technical solutions described in the foregoing embodiments, or equivalent substitutions can be made to some or all of the technical features therein. Such modifications or substitutions do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of this application.

Claims

1. A hot melt head assembly, characterized in that, include: A hot melt column, wherein a first end face is provided at one axial end of the hot melt column; The shaping component is capable of moving axially relative to the hot melt column; The shaping component has a second end face on the side near the first end face; the shaping component has a first position and a second position; when the shaping component is in the first position, there is an axial gap between the second end face and the first end face; When the shaping component is in the second position, the second end face coincides with the first end face.

2. The hot melt head assembly according to claim 1, characterized in that, The number of hot melt columns is multiple, and the multiple hot melt columns are arranged at intervals; they are projected along the axial direction onto the plane where the forming part is located, and the projection of any one of the hot melt columns is located within the projection area of ​​the forming part.

3. The hot melt head assembly according to claim 2, characterized in that, Projecting along the axial direction onto the plane where the forming part is located, the projections of the multiple hot melt columns are arranged in a rectangular, circular, racetrack-shaped, or elliptical array; The second end face is a continuous plane that matches the array arrangement.

4. The hot melt head assembly according to claim 1, characterized in that, The forming part is provided with distribution holes, and the hot melt column is clearance-fitted with the distribution holes.

5. The hot melt head assembly according to any one of claims 1-4, characterized in that, The hot melt head assembly also includes a housing, the housing including a first wall, the first wall being connected to the end of the hot melt column away from the first end face, the first wall being used to drive the hot melt column to move axially.

6. The hot melt head assembly according to claim 5, characterized in that, The outer shell also includes a second wall, which is circumferentially arranged around the edge of the first wall, and the second wall and the first wall together form a first cavity; the hot melt column and the shaping component are built into the first cavity.

7. The hot melt head assembly according to claim 6, characterized in that, The hot melt head assembly also includes a connecting rod, which is connected to the shaping part and is used to drive the shaping part to move axially.

8. The hot melt head assembly according to claim 7, characterized in that, The outer casing also includes a third wall, which is connected to the first wall; The third wall body surrounds and forms a second cavity, which is connected to the first cavity; the connecting rod is coaxially arranged with the second cavity; One axial end of the connecting rod passes through the second cavity and extends into the first cavity to connect with the shaping component.

9. The hot melt head assembly according to claim 8, characterized in that, The outer casing also includes a fourth wall, which is angled to the third wall; A limiting member is provided at one end of the connecting rod away from the shaping member along the axial direction. When the shaping member is in the second position, the limiting member abuts against the fourth wall.

10. A hot-melt device, characterized in that, Includes the hot melt head assembly as described in any one of claims 1 to 9 above.