Multilayer composite food preservation film with low water vapor transmission rate
The multi-layered composite structure of the preservation film solves the problems of inconvenient tearing and moisture loss, enabling quick tearing, reducing water vapor permeability, inhibiting bacterial growth, and extending the shelf life of food.
Patent Information
- Application Number
- CN202522765250.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2025-12-26
- Publication Date
- 2026-11-24
- Estimated Expiration
- 2035-12-26
AI Technical Summary
Existing plastic wrap is prone to tilting, stretching or breaking when torn, which cannot effectively prevent food from losing moisture. Furthermore, the water vapor in the food condenses into mist-like droplets, affecting the eating experience and potentially causing the food to spoil prematurely.
It adopts a multi-layer composite structure, including a support layer, a barrier layer and a contact layer. The barrier layer has horizontal grooves and limiting grooves, and the contact layer has through holes. Combined with a hydrophilic layer and an antibacterial layer, it is designed to guide tearing and reduce water vapor transmission rate, blocking moisture loss and bacterial growth.
It enables quick and precise tearing of food to the required size, reduces water vapor transmission rate, minimizes food moisture loss, prevents water droplet condensation, extends shelf life, prevents bacterial growth, and improves food preservation.
Smart Images

Figure CN225010754U_ABST
Abstract
Description
Technical Field
[0001] This utility model relates to the field of food preservation film technology, and in particular to a multi-layer composite food preservation film with low water vapor permeability. Background Technology
[0002] Plastic wrap is used to wrap and seal food (such as fresh fruits and vegetables, cooked food, and leftovers) to temporarily preserve freshness and prevent contamination, and it is widely used in daily life. However, plastic wrap currently faces the following technical problems: First, the tearing process lacks defined boundaries, making it prone to skewing, stretching, or breaking during tearing, thus making it difficult to quickly obtain the required size. Secondly, existing plastic wrap cannot effectively prevent food from losing moisture, and its poor moisture retention leads to food drying out and spoiling faster.
[0003] Third, during use, the water vapor released by the food will condense into mist-like water droplets on the inner surface of the membrane, which will not only affect the taste of the food but may also cause bacteria to grow and spoil the food prematurely. Summary of the Invention
[0004] To address the above problems, this utility model provides a multi-layer composite food preservation film with low water vapor permeability.
[0005] To achieve the above objectives, the present invention adopts the following technical solution: A multi-layer composite food preservation film with low water vapor permeability includes a support layer, a barrier layer, and a contact layer. The support layer, barrier layer, and contact layer are arranged sequentially from the outside to the inside. The barrier layer has a horizontal groove on its side facing the contact layer. The contact layer has a through hole, which is arranged along the length of the horizontal groove and is located inside the horizontal groove.
[0006] Furthermore, the barrier layer includes a first barrier layer and a second barrier layer. The first barrier layer is disposed facing the contact layer. A plurality of horizontal grooves are disposed parallel and equidistantly on the first barrier layer. The second barrier layer has a limiting groove on its side facing the support layer. The position of the limiting groove corresponds to the position of the horizontal groove. The limiting groove is horizontally disposed, and the length of the limiting groove is the same as the width of the second barrier layer.
[0007] Furthermore, the distance between the two ends of the horizontal groove and the two side edges of the barrier layer is at least 0.5cm, and the spacing between two adjacent horizontal grooves is 4-8cm.
[0008] Furthermore, the horizontal groove includes at least one row of arrayed through holes within its range.
[0009] Furthermore, the support layer is a PET layer, the first barrier layer is a vacuum-metallized polyester film layer, the second barrier layer is a polyvinylidene chloride layer, and the contact layer is a PE layer.
[0010] Furthermore, the horizontal groove is coated with a hydrophilic layer, and the side of the contact layer away from the barrier layer is coated with an antibacterial layer.
[0011] Furthermore, the hydrophilic layer is a chitosan layer, a sodium alginate layer, or a polyvinylpyrrolidone layer, and the antibacterial layer is a nano-SiO2 layer or a quaternary ammonium salt compound layer.
[0012] Furthermore, the support layer, barrier layer, and contact layer are co-extruded together.
[0013] Compared with the prior art, the beneficial effects of this utility model are as follows: (1) This utility model provides a clear tearing guide by designing a horizontal groove in the barrier layer, and the tearing force is evenly transmitted with the limiting groove, which completely avoids skewing, stretching or breaking during tearing, and can quickly obtain the required size without additional cutting. (2) This utility model is designed with a first barrier layer and a second barrier layer to form double protection, which greatly reduces the water vapor transmission rate, reduces the loss of food moisture, prevents the food from drying out, and extends the shelf life. (3) The hydrophilic layer in the horizontal groove of this utility model actively adsorbs water vapor, and the through holes in the contact layer assist the flow of water vapor, maintaining the microenvironment inside the membrane moist and preventing water accumulation. This not only locks in the moisture of the food and prevents the food from drying out, but also extends the moisture retention period of the food and reduces bacterial growth. In addition, the antibacterial layer directly inhibits the growth of bacteria and mold, preventing the food from spoiling prematurely due to moisture or bacterial contamination. Attached Figure Description
[0014] Figure 1 This is a schematic diagram of the structure of the multilayer composite food preservation film with low water vapor permeability of this utility model. Figure 2 This is a schematic diagram of the three-dimensional structure of each layer of the multilayer composite food preservation film with low water vapor permeability of this utility model. Figure 3 This is a three-dimensional structural diagram of the first barrier layer and the contact layer of the multilayer composite food preservation film with low water vapor permeability of this utility model. Detailed Implementation
[0015] To provide a better understanding of the purpose, structure, features, and functions of this utility model, detailed descriptions are provided below with reference to specific embodiments.
[0016] Please refer to the reference. Figure 1 , Figure 2 , Figure 3This invention discloses a multi-layer composite food preservation film with low water vapor permeability, comprising a support layer 100, a barrier layer 200, and a contact layer 300. The support layer 100, barrier layer 200, and contact layer 300 are arranged sequentially from the outside in, forming a multi-layer structure. The support layer 100 ensures strength, the barrier layer 200 reduces water vapor permeability, and the contact layer 300 securely adheres to the food. This ensures the preservation film has good sealing properties, reduces water vapor permeability, retains moisture, and extends the food's shelf life.
[0017] The barrier layer 200 has a horizontal groove 210 on its side facing the contact layer 300, and the contact layer 300 has a through hole 310. The through hole 310 is arranged along the length of the horizontal groove 210 and is located inside the horizontal groove 210. During the manufacturing process of the cling film, a flow channel corresponding to the barrier layer is designed in the flow divider block within the co-extrusion die. When the melt passes through this flow channel, a preset horizontal groove 210 is formed on the barrier layer 200. This horizontal groove 210 provides guidance for tearing the cling film, facilitating tearing. The horizontal groove limits the tearing range, preventing skewed tearing and ensuring quick tearing of the desired size of cling film. The position of the through hole 310 corresponds to the position of the horizontal groove 210. The diameter of the through-hole 310 is much smaller than the width of the horizontal groove 210. This through-hole 310 can be formed by punching holes in the contact layer 300 of the co-extruded composite cling film using a needle roller or laser, or by pre-setting tiny needle-like protrusions corresponding to the horizontal groove on the die head of the co-extruded contact layer during co-extrusion. When the raw material is extruded from the die head, the through-hole is directly pressed into the contact layer. The design of the through-hole 310 ensures that water vapor released from the food can pass through the through-hole 310 and condense into water droplets within the horizontal groove 210 of the barrier layer 200, reducing the amount of water droplets in contact with the food and preventing bacterial growth that could lead to premature spoilage.
[0018] Furthermore, the barrier layer 200 includes a first barrier layer 201 and a second barrier layer 202. The first barrier layer 201 is disposed facing the contact layer 300. A plurality of horizontal grooves 210 are disposed parallel and equidistantly on the first barrier layer 201. The second barrier layer 202 has a limiting groove 220 on its side facing the support layer 100. The position of the limiting groove 220 corresponds to the position of the horizontal grooves 210. The limiting groove 220 is horizontally disposed, and its length is the same as the width of the second barrier layer 202. The limiting groove 220 is formed and prepared in the same manner as the horizontal groove 210. Through the two barrier layers, superimposed protection is ensured, significantly reducing the water vapor permeability and preventing food from drying out. The synchronously designed limiting groove 220 further provides tearing guidance, allowing the tearing force to be evenly transmitted in the horizontal direction, avoiding stretching of the film due to uneven force, ensuring accurate tearing size, and enabling quick acquisition of the required size. On the other hand, the setting of the limiting groove 220 ensures that the support layer 100 of the co-extruded plastic wrap is firmly bonded to the first barrier layer 202, restricting the interlayer displacement of the two layers, and at the same time, it can identify the tear point for easy tearing and use.
[0019] Furthermore, the distance between the two ends of the horizontal groove 210 and the two side edges of the barrier layer 200 is at least 0.5cm, and the spacing between two adjacent horizontal grooves 210 is 4-8cm. This ensures the strength of the cling film, prevents insufficient strength at the edges due to grooving, prevents tearing or peeling between layers during removal, and ensures the overall structural stability of the film. The 4-8cm spacing is suitable for everyday use, facilitating quick and easy cutting to the required length; the uniform and reasonable spacing avoids that being too dense will affect the barrier effect, while being too sparse will make removal inconvenient.
[0020] Furthermore, the contact layer within the range of the horizontal groove 210 includes at least one row of arrayed through holes 310. The through hole density within the range of the horizontal groove 210 is 2-5 holes / cm². 2 The multi-row through-hole 310 design increases the ventilation area, which can quickly remove water vapor released from food, reducing the amount of water vapor condensing and forming water droplets on the contact layer. This prevents more water droplets from coming into contact with food, affecting the eating experience and accelerating spoilage.
[0021] Furthermore, the support layer 100 is a PET layer, the first barrier layer 201 is a vacuum-metallized polyester film layer, the second barrier layer 202 is a polyvinylidene chloride layer, and the contact layer 300 is a PE layer. The outer layer uses a PET layer to provide high-strength support and ensure the stability of the film shape; the vacuum-metallized polyester film layer significantly reduces the permeability of water vapor and oxygen, enhancing the preservation barrier effect. This layer has good compatibility with the contact layer 300 and the second barrier layer 202, and the co-extrusion process results in a tight bond between the layers, preventing delamination, blocking ultraviolet rays, and reducing food oxidation and spoilage. The second barrier layer of polyvinylidene chloride has strong barrier performance, capable of blocking water vapor and odors, forming a double protection with the first barrier layer, further reducing water vapor permeability and preventing odors from affecting the food's usability.
[0022] Furthermore, a hydrophilic layer 211 is coated inside the horizontal groove 210. The hydrophilic layer 211 is a chitosan layer, a sodium alginate layer, or a polyvinylpyrrolidone layer. Each layer is pre-prepared, and the hydrophilic layer 211 is coated inside the horizontal groove 210 of the first barrier layer 201 and cured at low temperature. Then, each layer is fed into a co-extrusion device, where multiple layers are tightly bonded together through a co-extrusion mold to form a food preservation film. The hydrophilic layer 211 actively adsorbs water vapor released from the food, preventing the formation of mist-like water droplets on the inner surface of the film, thus not affecting the appearance of the food and reducing the risk of food spoilage due to water droplets. The contact layer 300 also has through-holes 310, through which the adsorbed water vapor can slowly dissipate, maintaining a moist microenvironment inside the film without water accumulation. This locks in the moisture of the food, preventing it from drying out and extending its shelf life, while also reducing bacterial growth. An antibacterial layer 400 is coated on the side of the contact layer 300 away from the barrier layer 200. The antibacterial layer 400 is made of nano-SiO₂. 2 A layer of quaternary ammonium compounds. This inhibits the growth of bacteria, mold, and other microorganisms, slows down the spoilage of food, and is suitable for the temporary storage of fresh fruits and vegetables and cooked food, extending their shelf life.
[0023] Furthermore, the support layer 100, barrier layer 200, and contact layer 300 are co-extruded together. This co-extrusion process ensures a strong interlayer bond, prevents delamination, and guarantees superior barrier performance.
[0024] This utility model has been described by the above-described embodiments; however, these embodiments are merely examples for implementing this utility model. It must be noted that the disclosed embodiments do not limit the scope of this utility model. Conversely, any modifications and refinements made without departing from the spirit and scope of this utility model are within the scope of patent protection of this utility model.
Claims
1. A multi-layer composite food preservation film with low water vapor permeability, characterized in that: It includes a support layer, a barrier layer, and a contact layer, which are arranged sequentially from the outside to the inside. The barrier layer has a horizontal groove on its side facing the contact layer, and the contact layer has a through hole. The through hole is arranged along the length of the horizontal groove and is located inside the horizontal groove.
2. The multilayer composite food preservation film with low water vapor permeability as described in claim 1, characterized in that: The barrier layer includes a first barrier layer and a second barrier layer. The first barrier layer is disposed facing the contact layer. A plurality of horizontal grooves are disposed parallel and equidistantly on the first barrier layer. The second barrier layer has a limiting groove on its side facing the support layer. The position of the limiting groove corresponds to the position of the horizontal groove. The limiting groove is horizontally disposed, and the length of the limiting groove is the same as the width of the second barrier layer.
3. The multilayer composite food preservation film with low water vapor permeability as described in claim 1, characterized in that: The distance between the two ends of the horizontal groove and the two sides of the barrier layer is at least 0.5cm, and the distance between two adjacent horizontal grooves is 4-8cm.
4. The multilayer composite food preservation film with low water vapor permeability as described in claim 1, characterized in that: The horizontal groove contains at least one row of arrayed through holes.
5. The multilayer composite food preservation film with low water vapor permeability as described in claim 2, characterized in that: The support layer is a PET layer, the first barrier layer is a vacuum-metallized polyester film layer, the second barrier layer is a polyvinylidene chloride layer, and the contact layer is a PE layer.
6. The multilayer composite food preservation film with low water vapor permeability as described in claim 1, characterized in that: The horizontal groove is coated with a hydrophilic layer, and the side of the contact layer away from the barrier layer is coated with an antibacterial layer.
7. The multilayer composite food preservation film with low water vapor permeability as described in claim 6, characterized in that: The hydrophilic layer is a chitosan layer, a sodium alginate layer, or a polyvinylpyrrolidone layer, and the antibacterial layer is a nano-SiO2 layer or a quaternary ammonium salt compound layer.
8. The multilayer composite food preservation film with low water vapor permeability as described in claim 1, characterized in that: The support layer, barrier layer, and contact layer are co-extruded together.