Track chain cleat transition plate and manufacturing die therefor

By designing a structure in which the thickness and length of the transition strip of the track anti-skid chain are negatively correlated, and optimizing the molding process, the problem of high cost of track anti-skid chain molds has been solved, achieving lightweight and high rigidity, and improving user experience and vehicle safety.

CN225010932UActive Publication Date: 2026-11-24DEQING GENERAL IND CO LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202522738998.1
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2025-12-24
Publication Date
2026-11-24
Estimated Expiration
2035-12-24

AI Technical Summary

Technical Problem

In the existing technology, tracked anti-skid chains require multiple sets of molds due to the need for transition strips of different lengths, resulting in high mold costs. Furthermore, the metal chains are prone to slipping and are heavy during installation, affecting user experience and vehicle load.

Method used

Design a transition strip for track anti-skid chains. The design adopts a negative correlation between the thickness and length of the main body of the strip. Combined with the curvature adaptation of the inner and outer reinforcing ribs, strips of different lengths are produced using a set of molds. The forming process is optimized by the mold closing gap, guiding slope and rounded corner transition structure.

Benefits of technology

It achieves reduced mold costs, lighter weight, and increased rigidity under the same raw material conditions, ensuring high adhesion and durability of the slats under harsh road conditions, and avoiding localized tearing and abrupt changes in thickness.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN225010932U_ABST
    Figure CN225010932U_ABST
Patent Text Reader

Abstract

A track anti-skid chain transition strip and its manufacturing mold are disclosed, relating to the field of tire anti-skid technology. The anti-skid chain transition strip is disposed on the rolling surface of the tire and connects to the anti-skid chain on the tire sidewall. It includes: a main body adapted to the tire rolling surface curve; an inner reinforcing rib disposed on the inner side of the main body; and an outer reinforcing rib disposed on the outer side of the main body. The thickness of the main body is configured to be negatively correlated with the overall length of the transition strip, such that under the same raw material conditions, a longer transition strip has a smaller main body thickness, and a shorter transition strip has a larger main body thickness. This design allows a single mold to produce strips of various specifications by adjusting the mold closing gap, significantly reducing mold costs.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This utility model relates to the field of tire anti-skid technology, and in particular to a track anti-skid chain transition strip and its manufacturing mold. Background Technology

[0002] Tire anti-skid technology is a crucial component of automotive safety, especially in snowy, muddy, or slippery conditions. Snow chains effectively increase the friction between the tires and the road surface, preventing slippage and ensuring vehicle stability and driving safety. With the increasing prevalence of automobiles and climate change, the demand for snow chains is growing. Their design must balance ease of installation, wear resistance, and cost-effectiveness to adapt to diverse user scenarios.

[0003] In the prior art, application number 202222616921.3 discloses a removable self-locking wear-resistant automotive tire anti-skid chain. This anti-skid chain mainly includes an anti-skid chain body, an installation component, and a reinforcement component. The installation component is connected via an outer connecting strip and an inner connecting strip located on the inner and outer sides of the anti-skid chain body. The outer and inner connecting strips have a first connecting end and a second connecting end at both ends, respectively, and are fixed by an opening groove and bolts, thereby improving the ease of disassembly.

[0004] However, the existing technology uses metal anti-skid chains on the tire rolling surface, which is relatively expensive to manufacture. In addition, metal chains are prone to shrinking and slipping during installation due to their mobility, which makes connection inconvenient and affects the user experience. Moreover, the weight of metal chains is relatively large, which may increase vehicle load and fuel consumption.

[0005] Currently, some tracked anti-skid chains use plastic anti-skid strips instead of metal chains on the tire rolling surface to reduce costs. Although this design reduces weight, the original transition plates of different lengths need to be formed in one go through multiple sets of forging dies, resulting in high mold costs. Utility Model Content

[0006] The technical problem to be solved by this utility model is to reduce the high cost caused by the need for multiple sets of molds for strips of different lengths.

[0007] To achieve the above objectives, according to one aspect of the utility model, a track anti-skid chain transition strip is provided, disposed on the rolling surface of a tire and connected to the anti-skid chain on the side of the tire, comprising: a plate body adapted to the rolling surface curve of the tire; an inner reinforcing rib disposed on the inner side of the plate body; and an outer reinforcing rib disposed on the outer side of the plate body; wherein the thickness of the plate body is configured to be negatively correlated with the overall length of the transition strip, such that under the same material conditions, a longer transition strip has a smaller plate body thickness, and a shorter transition strip has a larger plate body thickness.

[0008] As a preferred embodiment of the above technical solution, the main body of the plate has a mirror-symmetrical structure, and the main body of the plate includes a flat part with a large radius of curvature and a curved part with a small radius of curvature disposed on both sides of the flat part. The distribution direction of the inner reinforcing rib and the outer reinforcing rib is adapted to the curvature changes of the inner and outer surfaces of the main body of the plate, respectively.

[0009] A mold for manufacturing track anti-skid chain transition strips, used to manufacture the track anti-skid chain transition strips as claimed in the claims, includes: an upper mold and a lower mold; the lower end face of the upper mold and the upper end face of the lower mold are provided with curved surfaces with adapted curvatures; the lower mold has a lower groove for forming the outer reinforcing rib; the upper mold has an upper groove for forming the inner reinforcing rib; a mold closing gap is formed between the pressing curved surfaces of the upper mold and the lower mold, the height of the mold closing gap being greater than zero and less than or equal to the thickness of a single layer of raw material.

[0010] As a preferred embodiment of the above technical solution, the lower groove is provided with guide slopes on both sides for preferentially guiding the raw material into the lower groove for shaping during the pressing process.

[0011] As a preferred embodiment of the above technical solution, after the upper and lower templates are closed, their mating surfaces form a gently sloping clamping section and a curved clamping section with uniform gaps in the thickness direction of the main body of the plate; the gently sloping clamping section corresponds to the central region of the main body of the plate, and the curved clamping section corresponds to the two side edge regions of the main body of the plate; the gently sloping clamping section and the curved clamping section transition naturally.

[0012] As a preferred embodiment of the above technical solution, the edge of the groove of the lower groove and the lower end face of the upper template are naturally transitioned by a first rounded corner; the edge of the groove of the upper groove and the top of the guide slope are naturally transitioned by a second rounded corner.

[0013] As a preferred embodiment of the above technical solution, the upper template and the lower template are provided with alignment guide grooves on their left and right sides, and are guided by guide posts.

[0014] As a preferred embodiment of the above technical solution, a slat positioning post is also provided on the rear side of the lower template.

[0015] As a preferred embodiment of the above technical solution, the groove walls of the upper groove and the lower groove are designed as inclined structures with an inclination angle of 3°-5°, and the groove walls of the upper groove and the lower groove are provided with a rounded corner structure between them and the bottom surface.

[0016] In summary, this utility model has the following advantages:

[0017] 1. This utility model achieves structural self-adaptation under the same raw materials by using a negative correlation design between the thickness and length of the main plate: longer strips have reduced thickness to reduce weight, while shorter strips have increased thickness to compensate for rigidity. This design allows a single mold to produce strips of various specifications by adjusting the mold closing gap, significantly reducing mold costs;

[0018] 2. Furthermore, by setting up a guiding slope and rounded corner transition structure, the mold prioritizes guiding the raw material into the lower groove and outer reinforcing ribs in the early stage of mold closing, reducing material flow resistance. At the same time, the natural transition between the smooth clamping section and the curved clamping section allows the slab to extend evenly during the pressing process, avoiding local tearing or sudden changes in thickness.

[0019] Further or other beneficial effects will be discussed in the embodiments. Attached Figure Description

[0020] Figure 1 This is a schematic diagram of the anti-skid chain transition strip structure of this utility model;

[0021] Figure 2 This is a schematic diagram of the mold and transition strip of this utility model;

[0022] Figure 3 This is a schematic diagram of the clamping state of the mold and the transition strip from another angle.

[0023] Figure 4 This is a schematic diagram of the bottom structure of the upper template after it has been flipped over.

[0024] Figure 5 This is a schematic diagram of the lower template structure of this utility model;

[0025] Among them, 11-plate body, 12-inner reinforcing rib, 13-outer reinforcing rib, 111-smooth section, 112-bent section, 2-upper template, 3-lower template, 21-upper groove, 22-second rounded corner, 31-lower groove, 32-guide slope, 33-first rounded corner, 4-guide groove, 5-guide post, 6-positioning post, a-membrane gap, b-smooth clamping section, c-bent clamping section. Detailed Implementation

[0026] The directional terms such as up, down, left, right, front, back, front, back, top, and bottom mentioned or possibly used in this specification are defined relative to the construction shown in the accompanying drawings. The terms "inner" and "outer" refer to directions toward or away from the geometric center of a specific component, respectively. These are relative concepts and may therefore vary depending on their location and usage. Therefore, these or other directional terms should not be interpreted as restrictive.

[0027] The present invention will be further explained below with reference to the embodiments:

[0028] Example 1:

[0029] A track anti-skid chain transition strip, as shown in the reference Figure 1 The transition strip is placed on the rolling surface of the tire to connect the anti-skid chain on the tire sidewall. Its core design lies in adapting the curvature of the main body 11 to the tire's rolling surface curve, and optimizing stress transfer through the distribution of inner and outer reinforcing ribs 13. Specifically, the thickness of the inner reinforcing rib 12 is negatively correlated with the overall length of the transition strip; that is, under the same raw material conditions, a longer transition strip has a thinner main body 11, and a shorter transition strip has a thicker main body 11. This design allows the same mold to adapt to different strip lengths by adjusting the forming parameters, avoiding the need for separate molds for each length and significantly reducing mold costs. The main body 11 adopts a mirror-symmetrical structure, including a flat section 111 with a large radius of curvature and curved sections 112 on both sides with smaller radii of curvature. The orientations of the inner and outer reinforcing ribs 12 and 13 are adapted to the curvature changes of the inner and outer surfaces of the main body 11, respectively, ensuring uniform stress distribution under pressure and reducing the risk of localized fatigue fracture.

[0030] Example 2:

[0031] A mold for manufacturing track anti-skid chain transition strips, referring to Figure 2 , Figure 3 , Figure 4 and Figure 5 This mold, used to manufacture the transition strip for the anti-skid chain of the track in Example 1, includes an upper mold plate 2 and a lower mold plate 3. The lower end face of the upper mold plate 2 and the upper end face of the lower mold plate 3 are provided with curved surfaces of matching curvature. The lower mold plate 3 has a lower groove 31 for forming the outer reinforcing rib 13, and the upper mold plate 2 has an upper groove 21 for forming the inner reinforcing rib 12. A mold closing gap is formed between the pressing curved surfaces of the upper mold plate 2 and the lower mold plate 3. The height of the mold closing gap is greater than zero and less than or equal to the thickness of a single layer of raw material. That is, when the upper mold plate 2 and the lower mold plate 3 are closed, their final mold closing gap is controlled by an external press. This gap value is adapted to the length of the transition strip to be formed and the thickness of the plate body 11, so that a set of molds can press out transition strips of different specifications through different mold closing gaps.

[0032] The lower groove 31 has guide slopes 32 on both sides, which preferentially guide the raw material into the lower groove 31 during the pressing process, promoting the rapid shaping of the outer reinforcing ribs 13. After the upper mold 2 and the lower mold 3 are closed, their mating surfaces form a gently sloping clamping section b and a bent clamping section c with uniform gaps in the thickness direction of the plate body 11. The gently sloping clamping section b corresponds to the middle area of ​​the plate body 11, and the bent clamping section c corresponds to the two side edge areas. The two are connected by a naturally transitioning curved surface to avoid cracks in the blank due to sudden changes in thickness during the pressing process. In addition, the groove edge of the lower groove 31 is naturally transitioned to the lower end face of the upper mold 2 by a first rounded corner 33, and the groove edge of the upper groove 21 is naturally transitioned to the top of the guide slope 32 by a second rounded corner 22, further optimizing the deformation path during material pressing.

[0033] The mold has alignment guide grooves 4 on both sides, and precise positioning is achieved by guide pillars. The lower mold plate 3 also has a strip positioning pillar 6 on the rear side to limit the position of the blank and prevent it from shifting backward during the forming process. The groove walls of the upper groove 21 and the lower groove 31 are designed with an inclination angle of 3°-5°, and the groove walls and the bottom surface adopt a rounded corner structure to facilitate demolding and reduce stress concentration.

[0034] The conventional method for forming both ends of a slab in this field is as follows: heat the upper template 2 and the lower template 3, and place the slab on the lower template 3; then press down the upper template 2, and guide the inclined surface 32 to make the raw material fill the lower groove 31 first to form the outer reinforcing rib 13, while the upper groove 21 forms the inner reinforcing rib 12; since the slab needs to be formed at both ends, the mold design allows the pressing process to be repeated after one clamping by shifting or rotating the slab to ensure the structural consistency of both ends of the slab.

[0035] This solution optimizes material distribution while ensuring the bending strength and wear resistance of the slats through a gap control mechanism. Longer slats reduce weight with a smaller thickness, while shorter slats compensate for stiffness with a larger thickness, thus achieving both high adhesion and durability in harsh road conditions such as snow and mud.

[0036] Although preferred embodiments of the present invention have been described, those skilled in the art, upon learning the basic inventive concept, can make other changes and modifications to these embodiments. Therefore, the appended claims are intended to be interpreted as including the preferred embodiments as well as all changes and modifications falling within the scope of the present invention.

[0037] Obviously, those skilled in the art can make various modifications and variations to this utility model without departing from its spirit and scope. Therefore, if these modifications and variations fall within the scope of the claims of this utility model and their equivalents, this utility model also intends to include these modifications and variations.

Claims

1. A track chain transition shingle disposed on a rolling surface of a tire connecting a tire side surface chain, characterized by, include: The main body of the plate adapted to the tire rolling surface curve (11). Inner reinforcing ribs (12) are provided on the inner side of the plate body (11). External reinforcing ribs (13) are provided on the outside of the main body of the plate (11); The thickness of the main body (11) is configured to be negatively correlated with the overall length of the transition strip, so that under the same raw material conditions, the longer transition strip has a smaller main body (11) thickness and the shorter transition strip has a larger main body (11) thickness.

2. A track shoe chain link transition strip according to claim 1, wherein: The main body of the plate (11) has a mirror-symmetrical structure as a whole, and the main body of the plate (11) includes a flat part (111) with a large radius of curvature and a curved part (112) with a small radius of curvature disposed on both sides of the flat part (111). The distribution direction of the inner reinforcing rib (12) and the outer reinforcing rib (13) is adapted to the curvature changes of the inner and outer surfaces of the main body of the plate (11).

3. A mold for manufacturing track anti-skid chain transition strips, used to manufacture the track anti-skid chain transition strips as described in claim 1 or 2, characterized in that, include: Upper template (2) and lower template (3); the lower end face of the upper template (2) and the upper end face of the lower template (3) are provided with curved surfaces with matching curvature; the lower template (3) is provided with a lower groove (31) for forming the outer reinforcing rib (13); the upper template (2) is provided with an upper groove (21) for forming the inner reinforcing rib (12); a mold closing gap is formed between the pressing curved surfaces of the upper template (2) and the lower template (3), and the height of the mold closing gap is greater than zero and less than or equal to the thickness of a single layer of raw material.

4. The mold for manufacturing a track anti-skid chain transition strip according to claim 3, characterized in that: The lower groove (31) is provided with guide slopes (32) on both sides for preferentially guiding the raw material into the lower groove (31) for shaping during the pressing process.

5. A mold for manufacturing a track anti-skid chain transition strip according to claim 3, characterized in that: After the upper template (2) and the lower template (3) are closed, their mating surfaces form a smooth clamping section (b) and a curved clamping section (c) with uniform gaps in the thickness direction of the plate body (11); the smooth clamping section (b) corresponds to the middle region of the plate body (11), and the curved clamping section (c) corresponds to the two side edge regions of the plate body (11); the smooth clamping section (b) and the curved clamping section (c) transition naturally.

6. The mold for manufacturing a track anti-skid chain transition strip according to claim 4, characterized in that: The groove edge of the lower groove (31) and the lower end face of the upper template (2) are naturally transitioned by a first rounded corner (33); the groove edge of the upper groove (21) and the top end of the guide slope (32) are naturally transitioned by a second rounded corner (22).

7. A mold for manufacturing a track anti-skid chain transition strip according to claim 3, characterized in that: The upper template (2) and the lower template (3) are provided with alignment guide grooves (4) on their left and right sides, and are guided by guide columns.

8. A mold for manufacturing a track anti-skid chain transition strip according to claim 3, characterized in that: The lower template (3) is also provided with a slat positioning post (6) on the rear side.

9. A mold for manufacturing a track anti-skid chain transition strip according to claim 3, characterized in that: The groove walls of the upper groove (21) and the lower groove (31) are designed as inclined structures with an inclination angle of 3°-5°, and the groove walls of the upper groove (21) and the lower groove (31) are provided with rounded corner structures between them and the bottom surface.

Citation Information

Patent Citations

  • Self-locking wear-resistant automobile tire antiskid chain convenient to disassemble

    CN218536231U