Zirconia corundum molybdenum composite brick
By embedding C-shaped molybdenum plates into the cover bricks of the zirconia-corundum flow channel and fixing them with T-shaped support plates, and coating them with zirconium silicate, the problems of easy corrosion of molybdenum plates and the entry of support plates into the glass melt are solved. This achieves better anti-corrosion effect and easy separation and recycling, thus improving the quality and economy of glass production.
Patent Information
- Application Number
- CN202522097324.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2025-09-29
- Publication Date
- 2026-11-24
- Estimated Expiration
- 2035-09-29
AI Technical Summary
Existing composite molybdenum plate flow hole cover bricks are easily corroded by molten glass at high temperatures. The support plate entering the molten glass affects the glass quality. The molybdenum plate is difficult to separate from the zirconium corundum and is easily damaged, which affects the quality and cost of glass production.
A zirconium-corundum-molybdenum composite brick is designed, which uses a C-shaped molybdenum plate and is fixed by a T-shaped support plate. The surface of the molybdenum plate is coated with a zirconium silicate coating. The support plate is reinforced with a sand mold to ensure the stability of the molybdenum plate and easy separation.
It effectively prevents molten glass from corroding the interior of the molybdenum plate, avoids the support plate from entering the molten glass, improves product stability and recycling efficiency, and reduces production costs.
Smart Images

Figure CN225013318U_ABST
Abstract
Description
Technical Field
[0001] This utility model relates to the field of refractory bricks, and in particular to cover bricks for liquid flow holes in glass melting furnaces. Background Technology
[0002] Glass furnaces are essential melting devices in the glass manufacturing industry, and the flow channel of a glass furnace is a crucial part, as well as the area with the fastest erosion rate. On the one hand, the molten glass around the flow channel has a strong corrosive effect on the traditional cover bricks; on the other hand, the refractory bricks around the flow channel, after being eroded, enter the molten glass, altering its composition and forming glass veins, streaks, or concretions on the surface of the glass substrate, severely impacting glass quality and yield.
[0003] Chinese patent CN215480512U discloses an improved flow channel structure for a glass electric melting furnace, comprising a flow channel cover brick, a melting pool wall, a reserved space, a first support, a second support, and a third support. The flow channel cover brick is positioned above the flow channel, and the melting pool wall is positioned above the flow channel cover brick and located on the right side of the melting pool. The first support is positioned above the flow channel cover brick and located on the right side of the melting pool wall. The second support is positioned directly above the first support, and the two ends of the third support overlap the melting pool wall. On the second support, the flow hole cover brick, the melting pool wall, the first support, and the third support form a reserved space. This utility model reduces the temperature of the contact point with the molten glass by air cooling and increases the thickness of the melting pool wall and the front end of the flow hole cover brick, thereby extending the service life of the flow hole and the glass electric melting furnace. Although it can reduce the erosion of the flow hole cover brick by the molten glass to a certain extent, the construction is cumbersome, consumes a lot of materials, and the air cooling treatment can easily affect the flow speed and state of the molten glass, affecting the quality of the glass products.
[0004] Molybdenum metal possesses advantages such as high strength, high melting point, corrosion resistance, and abrasion resistance, making it widely used as a heating and structural material in high-temperature electric furnaces. Experiments have demonstrated that molybdenum metal is essentially not corroded by molten glass in an oxygen-free environment, nor does it contaminate the molten glass. However, in an oxygen-rich environment, molybdenum metal begins to oxidize slowly at temperatures up to 520 degrees Celsius, and rapidly oxidizes into molybdenum trioxide at temperatures above 600 degrees Celsius. Since the operating temperature of glass furnaces is generally above 1400 degrees Celsius, this significantly limits the use of molybdenum metal.
[0005] Based on the advantages of molybdenum metal, such as high strength, high melting point, corrosion resistance, and abrasion resistance, and utilizing its property of not being corroded by glass molten metal in an oxygen-free environment, the preparation of a composite molybdenum plate molten metal duct cover brick is a technical problem that needs to be solved. For example, Chinese patent CN115446954B discloses a production method of composite molybdenum plate molten metal duct cover brick, belonging to the field of refractory material preparation technology. The steps are as follows: the first support plate, the second support plate, and the third support plate are placed in the slots inside the mold frame, and then the molybdenum plate is placed in. The molybdenum plate is fixedly connected to the first support plate, the second support plate, and the third support plate by bolts to obtain the casting mold frame; the following raw materials are prepared in the following mass percentages: zircon 3-4%, industrial alumina 34-43%, boron carbide 2-3%, heat-insulating reinforcing fiber 5-8%, zircon sand 35-44%, sodium carbonate 0.9-1.2%, and the balance is fused zirconium corundum; the raw materials are melted and mixed, cast, cooled and annealed, demolded and trimmed to obtain the composite molybdenum plate molten metal duct cover brick. This invention utilizes the advantage of molybdenum plates, which have excellent resistance to molten glass corrosion at high temperatures, by embedding molybdenum plates into the zirconium corundum brick.
[0006] However, existing composite molybdenum plate flow channel cover bricks still have the following problems: 1. The molybdenum plate embedded in the composite molybdenum plate flow channel cover brick adopts an L-shaped structure. While the L-shaped molybdenum plate can indeed slow down glass corrosion in the initial stage, once the zirconium corundum on the surface of the molybdenum plate is completely eroded, the molten glass will further erode the interior of the L-shaped molybdenum plate, at which point the molybdenum plate loses its protective function. 2. In addition, the support plate used to fix the molybdenum plate remains inside the composite molybdenum plate flow channel cover brick after casting. Therefore, when the molten glass erodes the composite molybdenum plate flow channel cover brick, it will be eroded immediately, entering the molten glass and changing its composition, forming glass veins, streaks, or stones on the surface of the glass substrate, seriously affecting glass quality and yield. 3. Due to the high price of molybdenum plates, they have great recycling value. However, existing molybdenum composite bricks are difficult to separate from zirconium corundum after use in the kiln. For cost considerations, a crushing method is generally used for separation, but this method easily causes structural damage to the molybdenum plate.
[0007] Therefore, manufacturing a cover brick for the flow channel of a glass melting furnace that can solve the above problems is a technical problem that needs to be solved. Summary of the Invention
[0008] The problem to be solved by this utility model is to provide a novel zirconium-corundum-molybdenum composite brick, which addresses the shortcomings of the prior art.
[0009] To solve the above problems, the present invention adopts the following solution: a zirconium-alumina-molybdenum composite brick, characterized in that a C-shaped molybdenum plate is embedded in the cover brick of the zirconium-alumina flow hole, and the two ends of the C-shaped molybdenum plate that are higher correspond to the inlet and outlet directions of the flow hole respectively.
[0010] Furthermore, the zirconium-alumina-molybdenum composite brick is characterized in that a T-shaped support plate is provided at the opening of the C-shaped molybdenum plate, and the T-shaped support plate is used to fix the C-shaped molybdenum plate in the sand mold for casting the zirconium-alumina-molybdenum composite brick.
[0011] Furthermore, the zirconium-corundum-molybdenum composite brick is characterized in that the surface of one side of the C-shaped molybdenum plate groove is coated with a zirconium silicate coating.
[0012] Furthermore, the zirconium-corundum-molybdenum composite brick is characterized in that the T-shaped support plate is fixedly connected to the C-shaped molybdenum plate by bolts, and the C-shaped molybdenum plate and the T-shaped support plate are provided with matching mounting holes.
[0013] Furthermore, the zirconium-corundum-molybdenum composite brick is characterized in that a reinforcing plate is provided at the position of the T-shaped support plate in the sand mold, the reinforcing plate is fixedly connected to the T-shaped support plate and is completely embedded in the sand mold, which is used to enhance the bonding strength between the T-shaped support plate and the sand mold and prevent the C-shaped molybdenum plate from being misaligned.
[0014] The technical effects of this utility model are as follows: 1. The zirconium-alumina-molybdenum composite brick of this application has a C-shaped molybdenum plate embedded inside. The molybdenum plate completely encloses the liquid flow hole of the glass furnace. Even if the zirconium-alumina on the surface of the molybdenum plate is completely eroded, the molten glass will not enter the interior of the molybdenum plate, thus preventing further erosion by the molten glass. Compared with the existing L-shaped molybdenum plate composite brick, it has a better anti-erosion effect. 2. When casting the zirconium-alumina-molybdenum composite brick, the molybdenum plate is fixed in the sand mold using a T-shaped support plate. Compared with the existing molybdenum plate composite bricks that are fixed in three directions, the fixing method of this design will not leave impurities (support plate) on the front of the liquid flow hole after the zirconium-alumina-molybdenum composite brick is formed, thus preventing the support plate from entering the molten glass after melting. 3. This design incorporates a reinforcing plate on the T-shaped support plate, which is vertically and fixedly connected to the T-shaped support plate. This part is entirely embedded in the sand mold, which greatly enhances the bonding strength between the T-shaped support plate and the sand mold, thereby improving the stability of the fixed C-shaped molybdenum plate. This ensures the C-shaped molybdenum plate remains stable during casting, improving product yield. 4. By applying a zirconium silicate coating to the inside of the molybdenum plate, the separation and recycling of the molybdenum plate from the zirconium corundum is greatly facilitated without causing structural damage to the molybdenum plate. Furthermore, the zirconium silicate coating has a high melting point of approximately 2500℃, thus not affecting the performance of the zirconium corundum molybdenum composite brick. Attached Figure Description
[0015] Figure 1 This is a schematic diagram of the zirconium-corundum-molybdenum composite brick structure of this application.
[0016] Figure 2 This is a schematic cross-sectional view of the zirconium-corundum-molybdenum composite brick of this application in a sand mold.
[0017] Figure 3A schematic diagram of a zirconium-corundum-molybdenum composite brick with a C-shaped molybdenum plate and a three-dimensional support plate in a sand mold.
[0018] Figure 4 for Figure 3 Schematic diagram of the GG cross section.
[0019] Figure 5 for Figure 3 Schematic diagram of the FF section.
[0020] Figure 6 A schematic diagram of the cross-sectional structure of a zirconium-corundum-molybdenum composite brick with an L-shaped molybdenum plate and a three-dimensional support plate in a sand mold.
[0021] Among them, 1 is a zirconium corundum molybdenum composite brick, 2 is a C-shaped molybdenum plate, 3 is a T-shaped support plate, 4 is a bolt, 5 is an L-shaped molybdenum plate, 6 is a three-way support plate, and 7 is a sand mold. Detailed Implementation
[0022] The present invention will now be described in further detail with reference to the accompanying drawings.
[0023] Example 1: Zirconium-corundum-molybdenum composite brick with C-shaped molybdenum plate and T-shaped support plate.
[0024] like Figure 1 , Figure 2 As shown, a zirconium-alumina-molybdenum composite brick includes a C-shaped molybdenum plate embedded within the cover brick of a zirconium-alumina flow channel. The two protruding ends of the C-shaped molybdenum plate correspond to the inlet and outlet directions of the flow channel. A T-shaped support plate is installed at the opening of the C-shaped molybdenum plate to fix it within the sand mold used for casting the zirconium-alumina-molybdenum composite brick. The surface of the grooved side of the C-shaped molybdenum plate is coated with a zirconium silicate coating. The T-shaped support plate is bolted to the C-shaped molybdenum plate, and both the C-shaped molybdenum plate and the T-shaped support plate have matching mounting holes. A reinforcing plate is installed at the position of the T-shaped support plate within the sand mold. This reinforcing plate is fixedly connected to the T-shaped support plate and fully embedded in the sand mold, enhancing the bonding strength between the T-shaped support plate and the sand mold and preventing misalignment of the C-shaped molybdenum plate.
[0025] Example 2: Zirconium-corundum-molybdenum composite brick with C-shaped molybdenum plate and three-way support plate.
[0026] like Figure 3 , Figure 4 , Figure 5 As shown, a zirconium-alumina-molybdenum composite brick has a C-shaped molybdenum plate embedded in the cover brick of the zirconium-alumina flow channel, with the two protruding ends of the C-shaped molybdenum plate corresponding to the inlet and outlet directions of the flow channel. The C-shaped molybdenum plate is provided with support plates in three directions, which are used to fix the C-shaped molybdenum plate in the sand mold for casting the zirconium-alumina-molybdenum composite brick. The support plates are fixedly connected to the C-shaped molybdenum plate with bolts.
[0027] Example 3: Zirconium-corundum-molybdenum composite brick with L-shaped molybdenum plate and three-way support plate.
[0028] like Figure 6 As shown, a zirconium-alumina-molybdenum composite brick has an L-shaped molybdenum plate embedded in the cover brick of the zirconium-alumina flow hole. The L-shaped molybdenum plate is provided with a three-way support plate. The L-shaped molybdenum plate is fixed in the sand mold for casting the zirconium-alumina-molybdenum composite brick by the support plate in three directions. The support plate is fixedly connected to the L-shaped molybdenum plate by bolts.
Claims
1. A zirconia corundum molybdenum composite brick, characterized by, A C-shaped molybdenum plate is embedded in the cover brick of the zirconia-corundum flow tunnel, and the two ends of the C-shaped molybdenum plate that are higher correspond to the inlet and outlet directions of the flow tunnel.
2. The zirconia corundum molybdenum composite brick according to claim 1, characterized in that, A T-shaped support plate is provided at the opening of the C-shaped molybdenum plate. The T-shaped support plate is used to fix the C-shaped molybdenum plate in the sand mold for casting zirconium-corundum-molybdenum composite bricks.
3. The zirconia corundum molybdenum composite brick according to claim 1, characterized in that, The surface of the groove side of the C-shaped molybdenum plate is coated with a zirconium silicate coating.
4. The zirconium-corundum-molybdenum composite brick according to claim 2, characterized in that, The T-shaped support plate is fixedly connected to the C-shaped molybdenum plate by bolts, and the C-shaped molybdenum plate and the T-shaped support plate are provided with matching mounting holes.
5. The zirconium-corundum-molybdenum composite brick according to claim 2, characterized in that, The T-shaped support plate is provided with a reinforcing plate at the position in the sand mold. The reinforcing plate is fixedly connected to the T-shaped support plate and is completely embedded in the sand mold. This is used to enhance the bonding strength between the T-shaped support plate and the sand mold and prevent the C-shaped molybdenum plate from misaligning.
Citation Information
Patent Citations
A production method for composite molybdenum plate flow hole cover brick
CN115446954B
Improved throat structure of glass electric melting furnace