Low-shrinkage PE-coated paper
By combining a composite anti-shrinkage structure with specific materials, the problems of high shrinkage and easy wrinkling and curling of PE coated paper have been solved, achieving the effects of low shrinkage and ease of industrial production.
Patent Information
- Application Number
- CN202522434881.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2025-11-17
- Publication Date
- 2026-11-24
- Estimated Expiration
- 2035-11-17
AI Technical Summary
Existing PE coated paper has a high shrinkage rate and is prone to wrinkling and curling, making it difficult to meet the stringent requirements of high-end packaging for low shrinkage rates. Furthermore, some solutions may affect coating uniformity or increase production costs.
A composite shrinkage-resistant structure is adopted, including a substrate layer, a composite layer and a surface treatment layer. A combination of a low-density solution flow layer, a vinyl acetate layer, an antioxidant layer, an adhesive layer, a protective layer, a base coating and a plasma layer is prepared through specific materials and processes to form a low-shrinkage PE coated paper.
It effectively reduces the shrinkage rate of PE coated paper, prevents wrinkling and curling, meets the needs of high-end packaging, and is easy to industrialize.
Smart Images

Figure CN225013877U_ABST
Abstract
Description
Technical Field
[0001] This utility model relates to the field of packaging materials technology, and in particular to a low-shrinkage PE coated paper. Background Technology
[0002] PE-coated paper is a composite packaging material formed by uniformly coating polyethylene (PE) plastic particles onto the surface of paper after heating and melting them through an extruder. It combines the stiffness and printability of paper with the waterproof, oil-proof, and barrier properties of PE film, and is widely used in food packaging (such as hamburger boxes, bread bags, and disposable lunch boxes), pharmaceutical packaging (such as drug packaging linings), and daily necessities packaging (such as sanitary napkin packaging and tissue packaging), among other fields.
[0003] To address the shrinkage issue of PE coated paper, existing technologies often employ methods such as increasing the molecular weight of the PE resin, adding small amounts of antioxidants, or adjusting the extrusion temperature. However, these methods have limited effectiveness in reducing shrinkage and are insufficient to meet the stringent requirements of high-end packaging applications for low shrinkage rates (typically below 5%). Furthermore, some methods can lead to decreased flowability of the PE coating layer, affecting coating uniformity or increasing production costs, which is detrimental to industrial production.
[0004] Therefore, developing a PE coated paper with low shrinkage, excellent overall performance, and easy industrial production is of great practical significance. Utility Model Content
[0005] The purpose of this invention is to provide a low-shrinkage PE coated paper, which solves the problems of high shrinkage and easy wrinkling and curling of existing PE coated paper.
[0006] To achieve the above objectives, this utility model employs a low-shrinkage PE coated paper, comprising a composite anti-shrinkage body. The composite anti-shrinkage body includes a substrate layer, a composite layer, and a surface treatment layer. The composite layer is fixedly connected to the substrate layer and is disposed below the substrate layer. The surface treatment layer is wrapped around the outer surfaces of the substrate layer and the composite layer.
[0007] The substrate layer includes a bleaching layer, a wood pulp layer, and a vulcanization layer. The bleaching layer is disposed on the outer surface of the wood pulp layer, and the vulcanization layers are interspersed and arrayed inside the wood pulp layer.
[0008] The composite layer includes a low-density solution flow layer, a vinyl acetate layer, an antioxidant layer, and an adhesive layer. The vinyl acetate layer is disposed inside the low-density solution flow layer, the antioxidant layer is disposed on the outer surface of the low-density solution flow layer, and the adhesive layer is inserted into the low-density solution flow layer and is also arrayed inside the vinyl acetate layer.
[0009] The surface treatment layer includes a protective layer, a base coating, and a plasma layer. The protective layer is disposed on the outer surface of the substrate layer and the composite layer. The base coating is disposed on the outer surface of the protective layer. The plasma layer is disposed on the outer surface of the base coating.
[0010] The sulfidation layer is made of sulfidated acetic acid.
[0011] The antioxidant layer is made of calcium carbonate.
[0012] The adhesive layer is made of stearamide.
[0013] The base coating is made of polyimide.
[0014] This invention discloses a low-shrinkage PE coated paper, comprising a composite anti-shrinkage body. The composite anti-shrinkage body includes a substrate layer, a composite layer, and a surface treatment layer. The composite layer is fixedly connected to the substrate layer and is disposed below the substrate layer. The surface treatment layer is wrapped around the outer surfaces of the substrate layer and the composite layer. By replacing the original formula structure with a composite anti-shrinkage body, the problems of high shrinkage rate and easy wrinkling and curling of PE coated paper in the prior art are effectively solved. Attached Figure Description
[0015] To more clearly illustrate the technical solutions in the embodiments of this utility model or the prior art, the drawings used in the description of the embodiments or the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of this utility model. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.
[0016] Figure 1 This is a schematic diagram of the overall structure of this utility model.
[0017] Figure 2 This is a front sectional view of the entire utility model.
[0018] Figure 3 This is a schematic diagram of the structure of the substrate layer of this utility model.
[0019] Figure 4 This is a schematic diagram of the composite layer structure of this utility model.
[0020] Figure 5 This is a schematic diagram of the surface treatment layer of this utility model.
[0021] 1-Substrate layer, 101-Bleaching layer, 102-Wood pulp layer, 103-Vulcanization layer, 2-Composite layer, 201-Low density solution layer, 202-Polyvinyl acetate layer, 203-Antioxidant layer, 204-Adhesive layer, 3-Surface treatment layer, 301-Protective layer, 302-Base coating, 303-Plasma layer. Detailed Implementation
[0022] The embodiments of this utility model are described in detail below. Examples of these embodiments are shown in the accompanying drawings, wherein the same or similar reference numerals denote the same or similar elements or elements having the same or similar functions throughout. The embodiments described below with reference to the accompanying drawings are exemplary and intended to explain this utility model, and should not be construed as limiting this utility model.
[0023] Please see Figures 1-5 , Figure 1 This is a schematic diagram of the overall structure of this utility model. Figure 2 This is a front sectional view of the entire utility model. Figure 3 This is a schematic diagram of the structure of the substrate layer of this utility model. Figure 4 This is a schematic diagram of the composite layer structure of this utility model. Figure 5 This is a schematic diagram of the surface treatment layer of this utility model.
[0024] This utility model provides a low-shrinkage PE coated paper, comprising a composite anti-shrinkage body. The composite anti-shrinkage body includes a substrate layer 1, a composite layer 2, and a surface treatment layer 3. The substrate layer 1 includes a bleaching layer 101, a wood pulp layer 102, and a vulcanization layer 103. The composite layer 2 includes a low-density melt flow layer 201, a vinyl acetate layer 202, an antioxidant layer 203, and an adhesive layer 204. The surface treatment layer 3 includes a protective layer 301, a base coating 302, and a plasma layer 303. This solution solves the problems of high shrinkage and easy wrinkling and curling of existing PE coated paper. It is understood that the aforementioned solution... During preparation, the wood pulp layer 102 raw material is fed into a pulper, an appropriate amount of water is added, and pulping is performed to a preset freeness. The pulp is then fed into the wire section of a paper machine for forming, initially creating a wet paper sheet. The bleached layer 101 pulp is evenly sprayed onto the surface of the wet paper sheet, which is then fed into a press. The vulcanized layer 103 particles are then interlaced within the semi-dry paper sheet using a needle-punching method. The paper sheet is then fed into a drying device and dried in three stages. The low-density solution flow layer 201, the vinyl acetate layer 202, the antioxidant layer 203, and the adhesive layer 204 raw materials are weighed according to a certain weight ratio and added to a high-speed mixer. The mixture is fed into a twin-screw extruder for melt extrusion, then cut into composite masterbatch by a pelletizer. The composite masterbatch is fed into a single-screw extruder for melt plasticization, and then extruded into a film through a T-die to obtain the composite layer 2. The raw material for the protective layer 301 is melted in an extruder and cast to form a protective film on the outer surface of the composite structure of the substrate layer 1 and the composite layer 2. A base coating 302 is then applied to the surface of the protective layer 301 using a doctor blade coating method. The coated semi-finished product is then sent to a plasma treatment machine to further treat the base coating 302. The plasma layer 303 is formed on the surface, thus completing the preparation of the surface treatment layer 3. The prepared substrate layer 1 and the composite layer 2 are bonded together using a hot press laminating machine. The protective layer 301 of the surface treatment layer 3 is wrapped around the outer surface of the composite structure of the substrate layer 1 and the composite layer 2 through an extrusion lamination process to ensure the integrity of the coating. The coated finished product is cooled and shaped, and the edges are trimmed and the width is adjusted according to the requirements. Finally, after quality inspection, it is rolled into a roll. This effectively solves the problems of high shrinkage rate and easy wrinkling and curling of PE coated paper in the prior art.
[0025] In this specific embodiment, the composite layer 2 is fixedly connected to the substrate layer 1, and the composite layer 2 is disposed below the substrate layer 1. The surface treatment layer 3 is wrapped around the outer surface of the substrate layer 1 and the composite layer 2. The prepared substrate layer 1 and the composite layer 2 are bonded together using a hot press laminating machine. The protective layer 301 of the surface treatment layer 3 is wrapped around the outer surface of the composite structure of the substrate layer 1 and the composite layer 2 through an extrusion lamination process to ensure the integrity of the coating. The finished product after coating is cooled and shaped, and the edges are trimmed and the width is adjusted according to the requirements. Finally, after quality inspection, it is rolled into a roll. This effectively solves the problems of high shrinkage rate and easy wrinkling and curling of PE coated paper in the prior art.
[0026] The bleaching layer 101 is disposed on the outer surface of the wood pulp layer 102, and the vulcanization layer 103 is interspersed and arrayed inside the wood pulp layer 102. The wood pulp layer 102 raw material is fed into a pulper, an appropriate amount of water is added, and pulping is carried out to a preset degree of freeness. The pulp is then fed into the wire section of a paper machine for forming, initially forming a wet paper sheet. The bleaching layer 101 pulp is evenly sprayed onto the surface of the wet paper sheet, and then the paper sheet enters the press equipment. The vulcanization layer 103 particles are interspersed and arrayed inside the semi-dry paper sheet using a needle punching method. The paper sheet is then fed into a drying equipment and dried in three stages.
[0027] The vinyl acetate layer 202 is disposed inside the low-density melt flow layer 201, the antioxidant layer 203 is disposed on the outer surface of the low-density melt flow layer 201, and the adhesive layer 204 is inserted inside the low-density melt flow layer 201 and is also arrayed inside the vinyl acetate layer 202. The raw materials of the low-density melt flow layer 201, the vinyl acetate layer 202, the antioxidant layer 203, and the adhesive layer 204 are weighed according to a certain weight ratio and put into a high-speed mixer to obtain a mixture. The mixture is fed into a twin-screw extruder, melt-extruded, and then cut into composite masterbatch by a pelletizer. The composite masterbatch is fed into a single-screw extruder, melt-plasticized, and then extruded into a film through a T-die to obtain the composite layer 2.
[0028] The protective layer 301 is disposed on the outer surface of the substrate layer 1 and the composite layer 2, the base coating 302 is disposed on the outer surface of the protective layer 301, and the plasma layer 303 is disposed on the outer surface of the base coating 302. A protective film is formed on the outer surface of the composite structure of the substrate layer 1 and the composite layer 2 by casting. The base coating 302 is coated on the surface of the protective layer 301 by blade coating. The coated semi-finished product is sent into a plasma treatment machine to form the plasma layer 303 on the surface of the base coating 302, thus completing the preparation of the surface treatment layer 3.
[0029] The vulcanized layer 103 is made of sulfided acetic acid, with sulfided acetic acid as the core raw material and low concentration of polyvinyl alcohol added as a binding agent to form a granular vulcanizing agent.
[0030] The antioxidant layer 203 is made of calcium carbonate, specifically nano-calcium carbonate, and is surface-modified with silane coupling agent KH-550.
[0031] The adhesive layer 204 is made of stearamide to assist the low-density melt flow layer 201 in fusing with the vinyl acetate layer 202.
[0032] The base coating 302 is made of polyimide resin, which helps to cover the subsequent plasma layer 303.
[0033] When using this utility model, the wood pulp layer 102 raw material is fed into a pulper, an appropriate amount of water is added, and pulping is performed to a preset degree of beating. The pulp is then fed into the wire section of a paper machine for forming, initially creating a wet paper sheet. The bleached layer 101 pulp is evenly sprayed onto the surface of the wet paper sheet, which is then fed into a press. The vulcanized layer 103 particles are then interlaced and arrayed within the semi-dry paper sheet using a needle-punching method. The paper sheet is then fed into a drying device, where a three-stage drying process is employed. The low-density melt flow layer 201, the vinyl acetate layer 202, the antioxidant layer 203, and the adhesive layer 204 raw materials are weighed according to a certain weight ratio and fed into a high-speed mixer to obtain a mixture. This mixture is then fed into a twin-screw extruder, melt-extruded, and cut into composite masterbatch by a pelletizer. The composite masterbatch is fed into a single-screw extruder, melt-plasticized, and then extruded into a film through a T-die, thus obtaining the composite layer 2. The protective layer 301 raw material is then processed... After melting in the extruder, a protective film is formed on the outer surface of the composite structure of the substrate layer 1 and the composite layer 2 by casting. The base coating 302 is then coated on the surface of the protective layer 301 by a doctor blade coating method. The coated semi-finished product is then fed into a plasma treatment machine to form the plasma layer 303 on the surface of the base coating 302, thus completing the preparation of the surface treatment layer 3. The prepared substrate layer 1 and the composite layer 2 are then bonded together by a hot press laminating machine. The protective layer 301 of the surface treatment layer 3 is then wrapped around the outer surface of the composite structure of the substrate layer 1 and the composite layer 2 by an extrusion lamination process to ensure the integrity of the coating. The wrapped finished product is then cooled and shaped, and the edges are trimmed and the width is adjusted according to requirements. Finally, after quality inspection, it is rolled into rolls. This effectively solves the problems of high shrinkage rate and easy wrinkling and curling of PE coated paper in the prior art.
[0034] The above-disclosed embodiments are merely preferred embodiments of the present utility model and should not be construed as limiting the scope of the present utility model. Those skilled in the art can understand that implementing all or part of the above-described embodiments and making equivalent changes in accordance with the claims of the present utility model are still within the scope of the utility model.
Claims
1. A low-shrinkage PE coated paper, characterized in that, The composite shrinkage protector includes a substrate layer (1), a composite layer (2) and a surface treatment layer (3). The composite layer (2) is fixedly connected to the substrate layer (1), and the composite layer (2) is disposed below the substrate layer (1). The surface treatment layer (3) is disposed on the outer surface of the substrate layer (1) and the composite layer (2).
2. The low-shrinkage PE coated paper as described in claim 1, characterized in that, The substrate layer (1) includes a bleaching layer (101), a wood pulp layer (102) and a vulcanization layer (103). The bleaching layer (101) is disposed on the outer surface of the wood pulp layer (102), and the vulcanization layer (103) is interspersed in the interior of the wood pulp layer (102).
3. The low-shrinkage PE coated paper as described in claim 1, characterized in that, The composite layer (2) includes a low-density melt flow layer (201), a vinyl acetate layer (202), an antioxidant layer (203), and an adhesive layer (204). The vinyl acetate layer (202) is disposed inside the low-density melt flow layer (201), the antioxidant layer (203) is disposed on the outer surface of the low-density melt flow layer (201), and the adhesive layer (204) is inserted inside the low-density melt flow layer (201) and is also arrayed inside the vinyl acetate layer (202).
4. The low-shrinkage PE coated paper as described in claim 1, characterized in that, The surface treatment layer (3) includes a protective layer (301), a base coating (302), and a plasma layer (303). The protective layer (301) is disposed on the outer surface of the substrate layer (1) and the composite layer (2). The base coating (302) is disposed on the outer surface of the protective layer (301). The plasma layer (303) is disposed on the outer surface of the base coating (302).
5. The low-shrinkage PE coated paper as described in claim 2, characterized in that, The sulfidation layer (103) is made of sulfidated acetic acid.
6. The low-shrinkage PE coated paper as described in claim 3, characterized in that, The antioxidant layer (203) is made of calcium carbonate.
7. The low-shrinkage PE coated paper as described in claim 3, characterized in that, The adhesive layer (204) is made of stearamide.