Corrosion-resistant PVC coiled floor
By employing a composite structure of anti-corrosion surface and inner layers in PVC roll flooring, and utilizing a combination of fluorocarbon resin-modified PVC with nano-silicon carbide, PVDF with nano-montmorillonite, and an interlocking structure of hook-type interlocking protrusions and interlocking grooves, the problem of insufficient corrosion resistance of PVC roll flooring in highly corrosive environments is solved, achieving a multi-dimensional anti-corrosion effect.
Patent Information
- Application Number
- CN202522823697.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2025-12-31
- Publication Date
- 2026-11-24
- Estimated Expiration
- 2035-12-31
AI Technical Summary
Existing PVC roll flooring has poor resistance to acid, alkali and organic solvent corrosion in highly corrosive environments such as chemical workshops and laboratories, and cannot adapt to highly corrosive environments.
It adopts a composite structure of anti-corrosion surface layer and anti-corrosion inner layer. The anti-corrosion surface layer is composed of fluorocarbon resin modified PVC and nano silicon carbide blend material, and the inner layer is composed of PVDF and nano montmorillonite composite flexible film. Combined with the interlocking structure of hook-shaped interlocking protrusions and interlocking grooves, and with the edge sealing coating, it forms multi-dimensional protection.
It significantly improves the acid and alkali resistance and organic solvent corrosion resistance of PVC roll flooring, enabling it to be used for a long time in highly corrosive environments without surface damage, internal penetration, or edge corrosion, thus improving the stability and practicality of the flooring.
Smart Images

Figure CN225014529U_ABST
Abstract
Description
Technical Field
[0001] This utility model relates to the field of waterproof building materials, and in particular to a corrosion-resistant PVC roll flooring. Background Technology
[0002] Currently, with the increasing demands for corrosion resistance in special fields such as chemical, electronic, and laboratory industries, PVC roll flooring is gradually becoming a candidate material for such scenarios due to its advantages of convenient installation and moderate cost.
[0003] Regarding the aforementioned technologies, the inventors believe that the following defects exist: In actual use, PVC roll flooring has poor resistance to acid and alkali corrosion and organic solvent corrosion, and cannot adapt to highly corrosive environments such as chemical workshops and laboratories. Utility Model Content
[0004] In order to improve the problem that existing PVC roll flooring has poor resistance to acid, alkali and organic solvent corrosion and cannot adapt to highly corrosive environments such as chemical workshops and laboratories, this application provides a corrosion-resistant PVC roll flooring.
[0005] This application provides a corrosion-resistant PVC roll flooring with the following technical solution: A corrosion-resistant PVC roll flooring includes a roll flooring body. The roll flooring body is provided with an anti-corrosion surface layer, an anti-corrosion inner layer, a PVC substrate layer, and an absorbent bottom layer from top to bottom. The layers are fixedly connected by an adhesive structure. The lower surface of the anti-corrosion surface layer has an array of barbed interlocking protrusions. The upper surface of the anti-corrosion inner layer has corresponding matching interlocking grooves. The barbed interlocking protrusions and the interlocking grooves are engaged to form an interlayer mechanical fixing structure. The roll flooring body has soft concave-convex interlocking edges on both sides. The soft concave-convex interlocking edges include an integrally formed flexible ridge and a flexible groove. The top of the flexible ridge has a cylindrical positioning pin. The bottom of the flexible groove has a corresponding positioning hole. The cylindrical positioning pin and the positioning hole form an interference fit structure. The lower surface of the absorbent bottom layer has an array of hemispherical absorbent protrusions.
[0006] By adopting the above technical solution, the anti-corrosion surface layer is a blend of fluorocarbon resin modified PVC and nano silicon carbide. PVC resin ensures the flexibility and formability required for the roll material, fluorocarbon resin provides core chemical corrosion resistance, and nano silicon carbide fills the internal pores of the material and enhances the surface hardness and wear resistance. The three work together to form a wear-resistant and corrosion-resistant surface protection. The anti-corrosion inner layer is a PVDF and nano montmorillonite composite flexible membrane. PVDF material itself has excellent acid and alkali resistance and organic solvent resistance. Nano montmorillonite forms a labyrinthine penetration barrier in a layered dispersion form, which greatly reduces the penetration rate of corrosive media.
[0007] Furthermore, the anti-corrosion outer layer and the anti-corrosion inner layer are a double-layer superimposed structure, with the anti-corrosion outer layer completely covering the upper surface of the anti-corrosion inner layer and its edges flush with the edges of the anti-corrosion inner layer.
[0008] By adopting the above technical solution, the superposition of the anti-corrosion surface layer and the anti-corrosion inner layer improves the anti-corrosion effect of the main body of the roll flooring and extends its actual service life.
[0009] Furthermore, the hook-shaped bite protrusion has an inverted conical structure, and the groove shape of the bite tooth groove is perfectly matched with the shape of the hook-shaped bite protrusion. After fitting, the side wall of the hook-shaped bite protrusion fits tightly with the groove wall of the bite tooth groove.
[0010] By adopting the above technical solution, the barbed interlocking protrusions and interlocking grooves are fitted and fixed, eliminating the gaps between layers, forming a surface anti-corrosion and inner barrier effect, thus improving the corrosion resistance of the main body of the roll flooring.
[0011] Furthermore, the soft, interlocking edges extend continuously along the length of the roll floor body, and the cross-sections of the flexible protrusions and flexible grooves are semi-circular, and they are symmetrically distributed on both sides of the roll floor body.
[0012] By adopting the above technical solution, the flexible protrusions and flexible grooves are used in combination to facilitate the fitting of multiple roll flooring bodies. At the same time, the cylindrical positioning pins and positioning holes further improve the fitting effect of multiple roll flooring bodies and enhance practicality.
[0013] Furthermore, the adsorption substrate has a sheet-like structure, and the hemispherical adsorption protrusions are integrally formed with the adsorption substrate and are evenly distributed on the entire lower surface of the adsorption substrate.
[0014] By adopting the above technical solution, hemispherical adsorption protrusions are evenly distributed on the adsorption bottom layer, which improves the adsorption effect between the main body of the roll flooring and the ground and enhances its stability.
[0015] Furthermore, the edge end face of the main body of the roll flooring is provided with an edge sealing coating. The edge sealing coating covers the edge end face of the anti-corrosion surface layer, the anti-corrosion inner layer, the PVC substrate layer and the absorbent bottom layer, forming a closed structure.
[0016] By adopting the above technical solution, the edge sealing coating is used to seal the edge surfaces of the anti-corrosion surface layer, the anti-corrosion inner layer, the PVC substrate layer, and the adsorption bottom layer, which effectively prevents edge corrosion and improves the actual use effect.
[0017] Furthermore, the cylindrical positioning pin is coaxially arranged with the flexible protrusion, and the depth of the positioning hole is adapted to the length of the cylindrical positioning pin, so that the cylindrical positioning pin is completely embedded in the positioning hole after assembly.
[0018] By adopting the above technical solution, the cylindrical positioning pin and the positioning hole are fully engaged, making the flexible protrusion and the flexible groove more securely engaged, thus improving the splicing effect of multiple roll flooring bodies.
[0019] Compared with related technologies, the corrosion-resistant PVC roll flooring provided by this utility model has the following beneficial effects: This utility model provides a corrosion-resistant PVC roll flooring. By using a unique combination of materials for the anti-corrosion surface layer and the anti-corrosion inner layer, it not only ensures the required flexibility and adaptability for roll installation, but also significantly improves the resistance to acid and alkali corrosion and organic solvent corrosion through the synergistic design of fluorocarbon resin, nano-silicon carbide, PVDF and nano-montmorillonite. It avoids the shortcomings of insufficient protection by a single material. The anti-corrosion surface material can be integrally molded with inverted conical hook-like interlocking protrusions, and the anti-corrosion inner layer material has slight elasticity to ensure a tight fit with the interlocking grooves. Combined with the sealing effect of the edge sealing coating, it blocks the penetration path of corrosive media from multiple dimensions such as the surface, inner layer, interlayer, and end face, resulting in better corrosion resistance and durability. It significantly improves the corrosion resistance of the substrate and is suitable for use in highly corrosive environments. Attached Figure Description
[0020] Figure 1 This is a schematic diagram of a preferred embodiment of a corrosion-resistant PVC roll floor provided by this utility model.
[0021] The following are the labeling elements in the diagram: 1. Main body of roll flooring; 2. Anti-corrosion surface layer; 21. Hook-type interlocking protrusions; 3. Anti-corrosion inner layer; 31. Interlocking grooves; 4. PVC substrate layer; 5. Adsorption bottom layer; 51. Hemispherical adsorption protrusions; 6. Soft concave-convex interlocking edge; 7. Flexible ridge; 71. Cylindrical positioning pin; 8. Flexible groove; 81. Positioning hole; 9. Edge sealing coating. Detailed Implementation
[0022] To facilitate understanding of this utility model, a more comprehensive description will be provided below with reference to the accompanying drawings. The drawings show typical embodiments of this utility model.
[0023] Example 1: like Figure 1As shown, this utility model discloses a corrosion-resistant PVC roll flooring, comprising a roll flooring body 1. The roll flooring body 1 is provided with an anti-corrosion surface layer 2, an anti-corrosion inner layer 3, a PVC substrate layer 4, and an adsorption bottom layer 5 from top to bottom. The layers are fixedly connected by an adhesive structure. The lower surface of the anti-corrosion surface layer 2 is integrally formed with an array of barbed interlocking protrusions 21. The upper surface of the anti-corrosion inner layer 3 is provided with corresponding matching interlocking grooves 31. The barbed interlocking protrusions 21 and the interlocking grooves 31 are fitted together to form an interlayer mechanical fixing structure. The roll flooring body 1 is provided with soft concave-convex interlocking edges 6 on both sides. The soft concave-convex interlocking edges 6 include an integrally formed flexible protrusion 7 and a flexible groove 8. The top of the flexible protrusion 7 is provided with a cylindrical positioning pin 71. The bottom of the flexible groove 8 is provided with a corresponding positioning hole 81. The cylindrical positioning pin 71 and the positioning hole 81 form an interference fit structure. The lower surface of the adsorption bottom layer 5 is distributed with an array of hemispherical adsorption protrusions 51.
[0024] like Figure 1 As shown, the anti-corrosion surface layer 2 is formed by twin-screw extrusion calendering process. PVC resin, fluorocarbon resin, nano silicon carbide and flexible toughening agent are mixed in a specific ratio and then melt-blended in an extruder. During calendering, inverted conical hook-type interlocking protrusions 21 are integrally formed to ensure the integrity of the protrusion structure and its integration with the surface material. The anti-corrosion inner layer 3 is formed by casting process. PVDF resin and nano montmorillonite are mixed and cast into a film. Then, interlocking grooves 31 that match the hook-type interlocking protrusions 21 are opened on the film through molding process to ensure precise fitting between the grooves and the protrusions. Subsequently, the anti-corrosion surface layer 2, the anti-corrosion inner layer 3, the PVC substrate layer 4, and the adsorption bottom layer 5 are bonded and fixed with adhesive. Finally, an edge sealing coating 9 is applied to the edge face of the roll material to form a complete corrosion-resistant structure. After long-term use in a highly corrosive environment, the roll floor body 1 has no problems such as surface damage, inner layer penetration, or edge corrosion, and its corrosion resistance is stable.
[0025] like Figure 1 As shown, the anti-corrosion surface layer 2 and the anti-corrosion inner layer 3 are a double-layer superimposed structure. The anti-corrosion surface layer 2 completely covers the upper surface of the anti-corrosion inner layer 3, and its edge is flush with the edge of the anti-corrosion inner layer 3.
[0026] like Figure 1 As shown, the hook-shaped occlusal protrusion 21 has an inverted conical structure. The groove shape of the occlusal tooth groove 31 is perfectly matched with the shape of the hook-shaped occlusal protrusion 21. After fitting, the side wall of the hook-shaped occlusal protrusion 21 fits tightly with the groove wall of the occlusal tooth groove 31.
[0027] like Figure 1 As shown, the soft, concave-convex interlocking edge 6 extends continuously along the length of the roll floor body 1, and the cross-sections of the flexible convex ridge 7 and the flexible groove 8 are semi-circular, and the two are symmetrically distributed on both sides of the roll floor body 1.
[0028] like Figure 1As shown, the adsorption bottom layer 5 has a sheet-like structure, and the hemispherical adsorption protrusions 51 are integrally formed with the adsorption bottom layer 5 and are evenly distributed on the entire lower surface of the adsorption bottom layer 5.
[0029] like Figure 1 As shown, the edge end face of the roll flooring body 1 is provided with an edge sealing coating 9, which covers the edge end face of the anti-corrosion surface layer 2, the anti-corrosion inner layer 3, the PVC substrate layer 4 and the adsorption bottom layer 5, forming a closed structure.
[0030] like Figure 1 As shown, the cylindrical positioning pin 71 is coaxially arranged with the flexible protrusion 7, and the depth of the positioning hole 81 is adapted to the length of the cylindrical positioning pin 71. After assembly, the cylindrical positioning pin 71 is completely embedded in the positioning hole 81.
[0031] In practice, the corrosion-resistant PVC roll flooring of this utility model includes a roll flooring body 1, and its molding and assembly process is as follows: Anti-corrosion surface layer 2: A blend of fluorocarbon resin modified PVC and nano silicon carbide is mixed in a specific ratio and fed into a twin-screw extruder. After melt blending, it is formed by calendering. During the calendering process, an array of inverted conical hook-type interlocking protrusions 21 are integrally formed. The surface layer thickness is adapted to the overall design of the roll material. Anti-corrosion inner layer 3: PVDF and nano montmorillonite composite flexible film is used. After the film is made by casting process, the interlocking grooves 31 that are adapted to the barbed interlocking protrusions 21 are opened by molding process. PVC substrate layer 4: A conventional flexible PVC substrate is selected and formed into a sheet structure through an extrusion process; Adsorption bottom layer 5: Made of modified EVA foam adsorption material, produced by foaming molding process, with hemispherical adsorption protrusions 51 arranged in an array during molding. Stack the layers in the following order: "anti-corrosion surface layer 2 → anti-corrosion inner layer 3 → PVC substrate layer 4 → adsorption bottom layer 5". Align the barbed interlocking protrusions 21 of the anti-corrosion surface layer 2 with the interlocking grooves 31 of the anti-corrosion inner layer 3 to form a mechanical fixation. Then, apply water-based adhesive to the contact surfaces of each layer and use a hot-pressing bonding process to firmly bond each layer together. The hot-pressing temperature and time are adapted to the conventional flexible roll material process to ensure the bonding strength without damaging the structure of each layer. Edge sealing coating 9: Select an anti-corrosion coating material that is compatible with the material of the anti-corrosion inner layer 3, apply it to the edge end face of the main body 1 of the roll flooring through a scraping process, cover the end face of all layers, and cure it with ultraviolet light to form a closed structure. Soft concave-convex interlocking edge 6: During the extrusion molding of the roll floor body 1, a flexible convex ridge 7, a flexible groove 8, a cylindrical positioning pin 71 at the top of the convex ridge, and a positioning hole 81 at the bottom of the groove are integrally formed to ensure that the cylindrical positioning pin 71 is coaxial with the flexible convex ridge 7 and that the positioning hole 81 is adapted to the cylindrical positioning pin 71.
[0032] In this technical solution, the main body 1 of the roll flooring achieves highly efficient corrosion resistance through the synergistic effect of its various layers, components, and processes. The anti-corrosion surface layer 2 is a blend of fluorocarbon resin-modified PVC and nano-silicon carbide. The PVC resin ensures the required flexibility and formability of the roll, the fluorocarbon resin provides core chemical corrosion resistance, and the nano-silicon carbide fills the internal pores of the material and enhances the surface hardness and wear resistance. The three work together to form a wear-resistant and corrosion-resistant surface protection. The anti-corrosion inner layer 3 uses a flexible composite film of PVDF and nano-montmorillonite. PVDF material itself has excellent corrosion resistance. With its acid and alkali resistant and organic solvent resistant properties, nano-montmorillonite forms a labyrinthine penetration barrier in a layered dispersion form, significantly reducing the penetration rate of corrosive media. Combined with the inverted conical hook-shaped interlocking protrusions 21 on the lower surface of the anti-corrosion surface layer 2 and the interlocking grooves 31 on the upper surface of the anti-corrosion inner layer 3, it eliminates the gaps between layers. At the same time, the edge sealing coating 9 of the roll material seals the end faces of each layer, forming a multi-dimensional corrosion-resistant system with surface anti-corrosion, inner layer barrier, and structural sealing. This effectively solves the problem of insufficient corrosion resistance of existing PVC roll flooring and is suitable for use in highly corrosive environments such as chemical workshops and laboratories.
[0033] The above are merely exemplary embodiments of this disclosure and should not be construed as limiting the scope of this disclosure. Any equivalent changes and modifications made in accordance with the teachings of this disclosure shall still fall within the scope of this disclosure. This application is intended to cover any variations, uses, or adaptations of this disclosure that follow the general principles of this disclosure and include common knowledge or customary techniques in the art not described in this disclosure.
Claims
1. A corrosion-resistant PVC roll flooring, characterized in that: The roll flooring includes a main body (1), which is provided with an anti-corrosion surface layer (2), an anti-corrosion inner layer (3), a PVC substrate layer (4), and an absorbent bottom layer (5) from top to bottom. The layers are fixedly connected by an adhesive structure. The lower surface of the anti-corrosion surface layer (2) is integrally formed with an array of barbed interlocking protrusions (21). The upper surface of the anti-corrosion inner layer (3) is provided with corresponding matching interlocking grooves (31). The barbed interlocking protrusions (21) and the interlocking grooves (31) fit together to form a mechanical fixation between the layers. The structure includes a soft, concave-convex interlocking edge (6) on both sides of the main body (1) of the roll flooring. The soft, concave-convex interlocking edge (6) includes an integrally formed flexible protrusion (7) and a flexible groove (8). The top of the flexible protrusion (7) is provided with a cylindrical positioning pin (71), and the bottom of the flexible groove (8) is provided with a corresponding positioning hole (81). The cylindrical positioning pin (71) and the positioning hole (81) form an interference fit structure. The lower surface of the adsorption bottom layer (5) is distributed with an array of hemispherical adsorption protrusions (51).
2. The corrosion-resistant PVC roll flooring according to claim 1, characterized in that, The anti-corrosion surface layer (2) and the anti-corrosion inner layer (3) are a double-layer superimposed structure. The anti-corrosion surface layer (2) completely covers the upper surface of the anti-corrosion inner layer (3), and its edge is flush with the edge of the anti-corrosion inner layer (3).
3. The corrosion-resistant PVC roll flooring according to claim 1, characterized in that, The hook-shaped bite protrusion (21) has an inverted conical structure. The groove shape of the bite groove (31) is perfectly matched with the shape of the hook-shaped bite protrusion (21). After fitting, the side wall of the hook-shaped bite protrusion (21) fits tightly with the groove wall of the bite groove (31).
4. The corrosion-resistant PVC roll flooring according to claim 1, characterized in that, The soft, concave-convex interlocking edge (6) extends continuously along the length of the roll floor body (1), and the cross-section of the flexible convex edge (7) and the flexible groove (8) is semi-circular, and the two are symmetrically distributed on both sides of the roll floor body (1).
5. The corrosion-resistant PVC roll flooring according to claim 1, characterized in that, The adsorption bottom layer (5) has a sheet-like structure, and the hemispherical adsorption protrusions (51) are integrally formed with the adsorption bottom layer (5) and are evenly distributed on the entire lower surface of the adsorption bottom layer (5).
6. The corrosion-resistant PVC roll flooring according to claim 1, characterized in that, The edge end face of the roll floor body (1) is provided with an edge sealing coating (9), which covers the edge end face of the anti-corrosion surface layer (2), the anti-corrosion inner layer (3), the PVC substrate layer (4) and the adsorption bottom layer (5) to form a closed structure.
7. The corrosion-resistant PVC roll flooring according to claim 1, characterized in that, The cylindrical positioning pin (71) is coaxially arranged with the flexible protrusion (7), and the depth of the positioning hole (81) is adapted to the length of the cylindrical positioning pin (71). After assembly, the cylindrical positioning pin (71) is completely embedded in the positioning hole (81).