A high ductility concrete reinforced structure

By using high-ductility concrete to reinforce the structure, and utilizing reinforcement units composed of rough-surface grinding layers, reinforcing mesh layers, and steel bar inserts, the problem of insufficient interfacial bond strength and durability of concrete components is solved, achieving overall structural integrity and efficient reinforcement effect.

CN225014728UActive Publication Date: 2026-11-24HENAN ZHENGDA BUILDING MATERIALS CO LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202522793188.6
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2025-12-30
Publication Date
2026-11-24
Estimated Expiration
2035-12-30

AI Technical Summary

Technical Problem

The performance of concrete components in existing buildings deteriorates due to improved design standards, aging during service, increased loads, or environmental erosion. Existing reinforcement technologies are insufficient in terms of interfacial bond strength and durability, leading to risks of delamination, slippage, and peeling, making it difficult to meet engineering requirements.

Method used

The high-ductility concrete reinforcement structure, consisting of a rough-surface grinding layer, a reinforcing mesh layer, steel bar inserts, a conical elastic tension cylinder, and a water-absorbing and expanding outer layer, enhances the interfacial bonding strength and anchoring stability, disperses stress concentration, prevents slippage, and achieves overall structural integrity.

Benefits of technology

It improves the interfacial bond strength and anchorage stability of concrete components, avoids delamination and peeling, enhances the reliability and durability of reinforcement, and meets the engineering needs in complex environments.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN225014728U_ABST
    Figure CN225014728U_ABST
Patent Text Reader

Abstract

This utility model discloses a high-ductility concrete reinforcement structure, relating to the field of engineering construction technology. The high-ductility concrete reinforcement structure designed here uses a reinforcement unit to disperse stress through a reinforcing mesh layer to avoid localized stress concentration. The mesh layer has holes that allow the reinforced concrete surface layer to penetrate. Simultaneously, the external threads of the reinforcing bar inserts enhance mechanical engagement, and the conical elastic tension cylinder strengthens anchoring, achieving a dual improvement in overall tightness and anchoring stability, preventing slippage under stress. Furthermore, a water-absorbing expansion unit uses cylindrical horizontal blocks to fix protruding burrs. The water-absorbing expansion layer expands upon contact with water, pushing the burrs deeper into the concrete. Elastic connecting ropes then pull to prevent detachment, completely avoiding the risk of interface peeling. Ultimately, this ensures that the base surface to be constructed and the reinforcement layer are fully stressed, achieving the advantages of reliable reinforcement, high efficiency, and strong adaptability.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This utility model relates to the field of engineering construction technology, and in particular to a high-ductility concrete reinforcement structure. Background Technology

[0002] Concrete components in existing buildings often experience performance degradation due to improved design standards, aging during service, increased loads, or environmental erosion. They need to be restored and their load-bearing capacity improved through reinforcement technology. High ductility concrete (ECC) has become a research hotspot in the field of reinforcement because it combines high toughness and crack resistance.

[0003] A nano-carbonation-resistant concrete coating structure, patented in China (CN223061788U), is described. This invention features flexibility and low-temperature resistance, effectively sealing the further propagation of micro-cracks, resisting new cracking caused by the expansion and contraction of the concrete matrix, preventing moisture from penetrating the concrete interior, and exhibiting excellent hydrophobicity to prevent rainwater erosion. It also effectively prevents chloride ions, acids, alkalis, and salts from penetrating the concrete interior, thus preventing steel reinforcement corrosion. Furthermore, it improves the bond strength between different layers of concrete, making peeling and detachment less likely.

[0004] The interface between the old concrete base and the ECC reinforcement layer relies solely on simple grinding, resulting in insufficient mechanical interlocking and a lack of an effective anchoring system. This leads to poor synergistic stress distribution between the two, making them prone to delamination and slippage under load. Consequently, the durability and reinforcement reliability under complex environments such as humidity and vibration cannot meet engineering requirements. Utility Model Content

[0005] To address the shortcomings of existing technologies, this invention provides a high-ductility concrete reinforcement structure, which solves the problems mentioned in the background section.

[0006] To achieve the above objectives, this utility model provides the following technical solution: a high-ductility concrete reinforcement structure, comprising a base surface to be constructed, the outer side of which is sprayed with a concrete reinforcement surface layer, a reinforcement unit between the base surface and the concrete reinforcement surface layer, the reinforcement unit comprising a roughened grinding layer, the roughened grinding layer being disposed on the outer wall surface of the base surface to be constructed, a reinforcing mesh layer being disposed at the end of the roughened grinding layer away from the base surface to be constructed, a fiber composite material reinforcement layer being disposed at the end of the reinforcing mesh layer away from the roughened grinding layer, a plurality of steel bar inserts being fixedly connected at the end of the fiber composite material reinforcement layer near the reinforcing mesh layer, and a plurality of external threads being fixedly connected to the outer wall of the steel bar inserts, the plurality of external threads being equidistantly arranged.

[0007] As a further technical solution of this utility model, multiple internal holes and grooves are respectively opened on the outer side of the substrate to be constructed, the rough surface grinding layer, and the reinforcing mesh layer. A conical elastic tension cylinder is fixedly connected to one end of the multiple internal holes and grooves on the outer side of the reinforcing mesh layer near the rough surface grinding layer.

[0008] As a further technical solution of this utility model, the reinforcing bar rod extends into the conical elastic tension cylinder and penetrates into the base surface to be constructed, and the outer wall surface of the reinforcing mesh layer is provided with several evenly distributed holes.

[0009] As a further technical solution of this utility model, the end of the concrete reinforcement layer away from the fiber composite material reinforcement layer is uniformly covered with a polymer mortar protective layer, and the outer wall surface of the reinforcing mesh layer is provided with a plurality of uniformly and equidistantly arranged protruding burrs.

[0010] As a further technical solution of this utility model, a water absorption expansion unit is provided at the connection between the protruding burrs and the reinforcing mesh layer, and the water absorption expansion unit includes a cylindrical cross block.

[0011] As a further technical solution of this utility model, the cylindrical horizontal block is set at the root position of the protruding burrs and the reinforcing mesh layer, and the outer end of the cylindrical horizontal block is fixedly connected with a water-absorbing and expanding outer layer.

[0012] As a further technical solution of this utility model, the two sides of the water-absorbing and expanding outer layer are symmetrically fixedly connected with elastic connecting ropes, and the water-absorbing and expanding outer layer is fixedly connected to the reinforcing mesh layer and the protruding burrs by the two elastic connecting ropes respectively.

[0013] This utility model provides a high-ductility concrete reinforcement structure, which has the following advantages compared with the prior art: This design presents a high-ductility concrete reinforcement structure. The reinforcement unit disperses stress by laying a reinforcing mesh layer to avoid localized stress concentration. The mesh layer has holes that allow the reinforced concrete surface layer to penetrate. Simultaneously, the external threads of the steel bar inserts enhance mechanical interlocking, and the conical elastic tension cylinder strengthens the anchoring. This achieves a dual improvement in overall tightness and anchoring stability, preventing slippage under stress. Furthermore, a water-absorbing expansion unit uses cylindrical horizontal blocks to fix the protruding burrs. The water-absorbing expansion layer expands upon contact with water, pushing the burrs deeper into the concrete. Elastic connecting ropes then pull them to prevent detachment, completely avoiding the risk of interface peeling. Ultimately, this ensures that the base surface to be constructed and the reinforcement layer are fully stressed, achieving the advantages of reliable reinforcement, high efficiency, and strong adaptability. Attached Figure Description

[0014] Figure 1 This is a schematic diagram of the base surface structure to be constructed according to this utility model; Figure 2 This is a schematic diagram of the exploded structure of the substrate to be constructed according to this utility model; Figure 3 This is a schematic diagram of the reinforced mesh structure of this utility model; Figure 4 This is a side view cross-sectional diagram of the water-absorbing and swelling outer layer of this utility model.

[0015] In the picture: 1. Base surface to be constructed; 2. Rough surface grinding layer; 3. Reinforcing mesh layer; 4. Concrete reinforced surface layer; 5. Polymer mortar protective layer; 6. Fiber composite reinforcement layer; 7. Rebar insert; 8. External thread; 9. Internal groove; 10. External burr; 11. Hole; 12. Cylindrical cross block; 13. Water-absorbing and expanding outer layer; 14. Elastic connecting rope; 15. Conical elastic tension cylinder. Detailed Implementation

[0016] The technical solutions of the present utility model will be clearly and completely described below with reference to the accompanying drawings of the embodiments of the present utility model. Obviously, the described embodiments are only some embodiments of the present utility model, and not all embodiments. All other embodiments obtained by those skilled in the art based on the embodiments of the present utility model without creative effort are within the protection scope of the present utility model.

[0017] Please see Figures 1-4 This utility model provides a technical solution for a high-ductility concrete reinforcement structure: it includes a base surface 1 to be constructed, the outer side of the base surface 1 is sprayed and covered with a concrete reinforcement surface layer 4, a reinforcement unit is set between the base surface 1 and the concrete reinforcement surface layer 4, the reinforcement unit includes a rough surface grinding layer 2, the rough surface grinding layer 2 is set on the outer wall surface of the base surface 1, a reinforcing mesh layer 3 is set at the end of the rough surface grinding layer 2 away from the base surface 1, a fiber composite material reinforcement layer 6 is set at the end of the reinforcing mesh layer 3 away from the rough surface grinding layer 2, a plurality of steel bar inserts 7 are fixedly connected to the end of the fiber composite material reinforcement layer 6 near the reinforcing mesh layer 3, and a plurality of external threads 8 are fixedly connected to the outer wall of the steel bar inserts 7, and the plurality of external threads 8 are equidistant from each other.

[0018] Please see Figures 1-4 Multiple internal slots 9 are respectively opened on the outer side of the base surface 1 to be constructed, the rough surface grinding layer 2, and the reinforcing mesh layer 3. A conical elastic tension cylinder 15 is fixedly connected to one end of the multiple internal slots 9 on the outer side of the reinforcing mesh layer 3 near the rough surface grinding layer 2. The steel bar rod 7 extends into the conical elastic tension cylinder 15 and penetrates into the base surface 1 to be constructed. Several evenly distributed holes 11 are opened on the outer wall of the reinforcing mesh layer 3. The end of the concrete reinforcement surface layer 4 away from the fiber composite reinforcement layer 6 is evenly covered with a polymer mortar protective layer 5.

[0019] Please see Figures 1-4The outer wall of the reinforcing mesh layer 3 is provided with a plurality of uniformly spaced protruding burrs 10. A water-absorbing expansion unit is provided at the connection between the protruding burrs 10 and the reinforcing mesh layer 3. The water-absorbing expansion unit includes a cylindrical horizontal block 12. The cylindrical horizontal block 12 is located at the root position of the protruding burrs 10 and the reinforcing mesh layer 3. A water-absorbing expansion outer layer 13 is fixedly connected to the outer end of the cylindrical horizontal block 12. Elastic connecting ropes 14 are symmetrically fixedly connected to both sides of the water-absorbing expansion outer layer 13. The water-absorbing expansion outer layer 13 is fixedly connected to the reinforcing mesh layer 3 and the protruding burrs 10 respectively through two elastic connecting ropes 14.

[0020] The working principle of this utility model is as follows: First, the base surface 1 to be treated is ground to form a roughened grinding layer 2. The rough surface increases the contact area with subsequent structures, significantly improving the interfacial bonding strength. Then, a reinforcing mesh layer 3 is laid on the outside of the roughened grinding layer 2. The reinforcing mesh layer 3 can disperse stress and avoid localized stress concentration. Next, a steel bar 7 with external threads 8 is fixedly connected to the fiber composite reinforcement layer 6. The external threads 8 enhance the mechanical interlocking of the steel bar 7 with the surrounding materials, preventing slippage under stress. Then, internal slots 9 are made in the base surface 1, the roughened grinding layer 2, and the reinforcing mesh layer 3. A conical elastic tension cylinder 15 is installed at the end of the internal slot 9 on the side of the reinforcing mesh layer 3. The steel bar 7 is inserted through the conical elastic tension cylinder 15 into the base surface 1. The conical elastic tension cylinder 15 can... After the insertion of the reinforcing bar 7, it creates a wrapping effect, further enhancing the anchoring stability of the reinforcing bar 7. The holes 11 on the reinforced mesh layer 3 allow the subsequently poured concrete reinforcement layer 4 to penetrate into them, improving the overall tightness of the bond. The concrete reinforcement layer 4 is sprayed on the outside of the fiber composite reinforcement layer 6, utilizing its high ductility to absorb external load energy and reduce crack formation. The polymer mortar protective layer 5 covering the outside of the concrete reinforcement layer 4 can isolate external water and air erosion, extending the service life of the structure. The protruding burrs 10 on the outer wall of the reinforced mesh layer 3 can increase the contact points with the concrete reinforcement layer 4, while the protruding burrs 10 and the cylindrical horizontal block 12 at the root of the reinforced mesh layer 3 can ensure a stable connection. The water-absorbing and expanding outer layer 13 at the outer end of the cylindrical horizontal block 12 will expand when it encounters moisture in the concrete, causing the protruding burrs 10 to gradually protrude outward and penetrate into the uncured concrete reinforcement layer 4.

[0021] The inner part tightly fills the surrounding gaps, and with the pulling effect of the elastic connecting ropes 14 on both sides, it can effectively prevent the bulging burrs 10 from separating from the reinforcing mesh layer 3. Finally, through the synergistic effect of each structure, the base surface 1 to be constructed and the concrete reinforcement surface layer 4 form a complete force system, achieving a reliable reinforcement effect.

[0022] The above are merely preferred embodiments of this utility model. It should be noted that those skilled in the art can make various improvements and modifications without departing from the principles of this utility model, and these improvements and modifications should also be considered within the scope of protection of this utility model. Structures, devices, and operating methods not specifically described or explained in this utility model are implemented according to conventional methods in the art, unless otherwise specified or limited.

Claims

1. A high-ductility concrete reinforced structure, characterized in that, The system includes a substrate to be constructed, the outer side of which is coated with a reinforced concrete surface layer. A reinforcement unit is provided between the substrate and the reinforced concrete surface layer. The reinforcement unit includes a roughened grinding layer, which is disposed on the outer wall of the substrate. A reinforcing mesh layer is provided at the end of the roughened grinding layer away from the substrate. A fiber composite material reinforcement layer is provided at the end of the reinforcing mesh layer away from the roughened grinding layer. Multiple reinforcing bar rods are fixedly connected to the end of the fiber composite material reinforcement layer near the reinforcing mesh layer. Multiple external threads are fixedly connected to the outer wall of the reinforcing bar rods, and the multiple external threads are equidistant from each other.

2. The high-ductility concrete reinforcement structure according to claim 1, characterized in that, Multiple internal holes and slots are respectively opened on the outer side of the substrate to be constructed, the rough surface grinding layer, and the reinforcing mesh layer. A conical elastic tension cylinder is fixedly connected to one end of the multiple internal holes and slots on the outer side of the reinforcing mesh layer near the rough surface grinding layer.

3. The high-ductility concrete reinforcement structure according to claim 2, characterized in that, The reinforcing bar extends into the conical elastic tension cylinder and penetrates into the base surface to be constructed. The outer wall of the reinforcing mesh layer has several evenly distributed holes.

4. The high-ductility concrete reinforcement structure according to claim 1, characterized in that, The concrete reinforcement surface layer is uniformly covered with a polymer mortar protective layer at the end away from the fiber composite reinforcement layer, and the outer wall of the reinforcing mesh layer is provided with a plurality of uniformly and equidistantly arranged protruding burrs.

5. A high-ductility concrete reinforced structure according to claim 4, characterized in that, A water-absorbing expansion unit is provided at the connection between the protruding burrs and the reinforcing mesh layer, and the water-absorbing expansion unit includes a cylindrical cross block.

6. A high-ductility concrete reinforced structure according to claim 5, characterized in that, The cylindrical horizontal block is located at the root of the protruding burrs and the reinforcing mesh layer, and a water-absorbing and expanding outer layer is fixedly connected to the outer end of the cylindrical horizontal block.

7. A high-ductility concrete reinforced structure according to claim 6, characterized in that, The water-absorbing and expanding outer layer is symmetrically fixedly connected to two sides by elastic connecting ropes. The water-absorbing and expanding outer layer is fixedly connected to the reinforcing mesh layer and the protruding burrs by the two elastic connecting ropes respectively.

Citation Information

Patent Citations

  • Nano anti-carbonization concrete coating structure capable of being subjected to spraying construction