Buried oil pipeline integrated with electrochemiluminescence corrosion sensing structure
By integrating an electroluminescent corrosion sensing structure, real-time early warning of corrosion on the outer wall of buried oil pipelines is achieved, solving the problems of lag in corrosion monitoring and high operation and maintenance costs in existing technologies, and improving the corrosion resistance and adaptability of pipelines.
Patent Information
- Application Number
- CN202521621671.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2025-07-31
- Publication Date
- 2026-11-24
- Estimated Expiration
- 2035-07-31
AI Technical Summary
Existing buried oil pipelines are susceptible to electrochemical corrosion in complex environments such as high altitude and high humidity, leading to local perforation, thinning, or even rupture. Existing anti-corrosion measures, such as external anti-corrosion coatings, are prone to aging, and cathodic protection is greatly affected by soil resistivity. Furthermore, corrosion monitoring methods are lagging and have high operation and maintenance costs.
An integrated electroluminescent corrosion sensing structure, including an electroluminescent sensing layer, an optical fiber channel, and an intelligent monitoring device, is used to collect the optical response of the anti-corrosion structure through periodic electrical excitation, thereby achieving real-time early warning of corrosion on the outer wall of the pipeline.
It enables real-time early warning of corrosion on the outer wall of buried oil pipelines, improves corrosion resistance, reduces false alarm rate, adapts to various crude oil characteristics, and has good mechanical strength and thermal insulation properties, making it suitable for underground transportation scenarios such as oil, natural gas and chemical industries.
Smart Images

Figure CN225016300U_ABST
Abstract
Description
Technical Field
[0001] This utility model relates to the field of intelligent pipeline corrosion prevention, specifically to a buried oil pipeline with an integrated electroluminescent corrosion sensing structure. Background Technology
[0002] my country is a major energy consumer and has built a nationwide oil pipeline network covering over 180,000 kilometers, including transnational pipelines such as those between China and Russia and China and Myanmar, as well as backbone networks such as the "West-to-East Oil Transmission" project. Among these, buried oil pipelines are widely distributed in complex environments characterized by high altitude, high humidity, and high corrosion. Moisture, electrolytes, and stray currents in the underground medium can easily penetrate the protective layer, inducing electrochemical corrosion. This can lead to localized perforation, thinning, or even rupture of the pipeline's outer wall, causing severe economic losses and environmental pollution. External corrosion has become a key factor restricting the service life and safety of pipelines.
[0003] Current anti-corrosion measures mainly rely on external anti-corrosion coatings and cathodic protection systems. However, these methods have obvious drawbacks: the coatings are prone to aging and peeling, cathodic protection is greatly affected by soil resistivity, and corrosion monitoring methods such as ultrasonic thickness measurement, magnetic flux leakage detection, or corrosion probes are mostly offline detection, which has lag, local detection blind spots, and high operation and maintenance costs.
[0004] Therefore, there is an urgent need to develop a buried oil pipeline that is fast-responding, highly adaptable, easily identifiable, and suitable for underground environments. Utility Model Content
[0005] The purpose of this invention is to provide a buried oil pipeline with an integrated electroluminescent corrosion sensing structure. The electroluminescent sensing layer, optical fiber channel, and intelligent monitoring device are integrated with the pipeline's multi-layer protection structure. Under periodic electrical excitation conditions, the optical response caused by local anomalies in the anti-corrosion structure is collected, thereby providing early warning of corrosion risks on the pipeline's outer wall.
[0006] This utility model is implemented using the following technical solution: A buried oil pipeline with an integrated electroluminescent corrosion sensing structure includes, from the inside out, an anti-corrosion lining layer, a pressure-bearing base pipe layer, an electroluminescent anti-corrosion sensing layer, a heat insulation layer, and a composite protective layer, as well as an optical fiber channel and an intelligent monitoring device. The electroluminescent anti-corrosion sensing layer includes an electroluminescent sensing layer and a main anti-corrosion layer covering the outside of the electroluminescent sensing layer; the inner surface of the electroluminescent sensing layer is bonded to the outer surface of the pressure-bearing base pipe layer; the inner surface of the main anti-corrosion layer has axial microgrooves, and the optical fiber channel is embedded in the axial microgrooves; the intelligent monitoring device is disposed on the outer surface of the composite protective layer and is connected to both the electroluminescent sensing layer and the optical fiber channel.
[0007] Preferably, the electroluminescent sensing layer is made of electroluminescent particles and a polyurethane matrix, and has electrodes connected to a periodic power supply module. The periodic power supply module applies an excitation signal with a set frequency and voltage to the electroluminescent sensing layer. When the main anti-corrosion layer is intact, the optical response obtained by the photoelectric detection module is in a normal recognition state; when the main anti-corrosion layer is partially damaged, and media such as water and ions reach the electroluminescent sensing layer, the local electric field distribution changes, causing the local luminescence state of the periodically excited electroluminescent material to change and forming a recognizable abnormal light signal. This abnormal light signal is collected by the optical fiber channel and transmitted to the photoelectric detection module.
[0008] Preferably, the outer surface of the anti-corrosion lining layer is in close contact with the inner surface of the pressure-bearing base pipe layer, and the inner surface of the anti-corrosion lining layer is used to contact the conveying medium to reduce the risk of internal corrosion of the pipeline.
[0009] Preferably, both the inner and outer surfaces of the pressure-bearing base pipe layer are sandblasted to improve the adhesion performance with the adjacent protective layer.
[0010] Preferably, the optical fiber channel is made of flexible PMMA optical fiber, which is embedded in an axial micro-groove fixed on the inner surface of the main anti-corrosion layer. Its input end is attached to the electroluminescent sensing layer, and its output end is connected to the photoelectric detection module through a sealed connector.
[0011] Preferably, the inner and outer surfaces of the insulation layer are tightly bonded to the outer surface of the main anti-corrosion layer and the inner surface of the composite protective layer, respectively; the composite protective layer is used to withstand and disperse external mechanical forces and to protect the insulation layer, the main anti-corrosion layer and the optical fiber channel located inside it.
[0012] Preferably, the intelligent monitoring device includes a periodic power supply module, a photoelectric detection module, and an LED warning light; the periodic power supply module is connected to the electrodes of the electroluminescent sensing layer via wires, the photoelectric detection module is connected to the output end of the optical fiber channel, and the LED warning light is electrically connected to the photoelectric detection module. Upon receiving an abnormal light signal, the photoelectric detection module outputs a warning signal and can upload monitoring results to a remote monitoring platform.
[0013] This utility model has the following beneficial effects: 1. The electroluminescent sensing layer, optical fiber channel and pipeline protection structure are integrated, and the periodic power supply module provides the external electrical excitation required for electroluminescence; when the anti-corrosion structure is partially damaged and the medium invades, the risk of corrosion on the outer wall of the pipeline can be warned online by collecting the optical response that changes relative to the normal state. 2. Construct a multi-layered composite structure to improve overall corrosion resistance: Adopt a multi-functional structure from the inside out, including an epoxy zinc-rich anti-corrosion lining, a pressure-bearing base pipe, an electroluminescent layer, a fiber optic channel, a heat insulation layer, and a composite protective layer. This effectively isolates water vapor, acids, alkalis, electrolytes, etc., from penetrating and damaging the metal matrix, improving overall corrosion resistance and extending the service life of the pipeline. 3. Intelligent monitoring and SCADA system linkage: By combining with intelligent monitoring devices (periodic power supply module, photoelectric detection module, LED warning lights), the system can collect, record and remotely alarm luminous signals, and can be integrated into the SCADA system for centralized supervision and dispatch response. 4. Adjustable warning threshold and low false alarm rate: By utilizing the response characteristics of electroluminescent materials and the dynamic threshold adjustment capability of the SCADA system, early identification of minor corrosion and accurate alarm for severe corrosion are ensured, reducing resource waste caused by misjudgment; 5. Modular design, strong adaptability and wide range of applications: The designed pipeline structure is compatible with various crude oil characteristics such as high viscosity, low temperature and high sulfur, and has good mechanical strength and thermal insulation performance, which can be widely used in underground transportation scenarios such as oil, natural gas and chemical industries. 6. The optical fiber channel is embedded in the axial micro-groove on the inner surface of the main anti-corrosion layer and is located inside the insulation layer and the composite protective layer, which avoids the optical fiber being directly exposed to the backfill soil environment, and helps to reduce the risk of damage caused by mechanical action during construction backfilling and service. 7. Strong construction adaptability: The structure has high modular compatibility and can be industrialized through conventional construction processes such as standard winding, spraying, and film application, which facilitates promotion and deployment. Attached Figure Description
[0014] To more clearly illustrate the technical solutions in the embodiments of the present invention or the prior art, the drawings used in the description of the embodiments or the prior art will be briefly introduced below; obviously, the drawings described below are only some embodiments of the present utility model, and those skilled in the art can obtain other drawings based on these drawings without creative effort; Figure 1 A radial cross-sectional view of a buried oil pipeline with an integrated electroluminescent corrosion sensing structure; Figure 2 A radial cross-sectional view of the electroluminescent corrosion sensing layer; Figure 3 This is a diagram showing the modular structure of an intelligent monitoring device.
[0015] Icons: 1. Anti-corrosion lining layer; 2. Pressure-bearing base pipe layer; 3. Electroluminescent anti-corrosion sensing layer; 301. Main anti-corrosion layer; 302. Electroluminescent sensing layer; 4. Optical fiber channel; 5. Insulation layer; 6. Composite protective layer; 7. Intelligent detection device; 701. Periodic power supply module; 702. Photoelectric detection module; 703. LED warning light. Detailed Implementation
[0016] To more clearly describe the purpose, technical solution, and advantages of this utility model, the embodiments will be described in detail below. Please note that the embodiments described are only some embodiments of this utility model, not all embodiments. Based on these embodiments, those skilled in the art can obtain other embodiments without creative effort, and these embodiments also fall within the protection scope of this utility model. The technical solution of this utility model is shown in the accompanying drawings. According to the drawings, this embodiment relates to an improved pipeline structure, designed to solve problems existing in existing pipeline engineering.
[0017] This embodiment discloses a buried oil pipeline with an integrated electroluminescent corrosion sensing structure, comprising, from the inside out, an anti-corrosion lining layer 1, a pressure-bearing base pipe layer 2, an electroluminescent anti-corrosion sensing layer 3, an insulation layer 5, and a composite protective layer 6, as well as an optical fiber channel 4 and an intelligent monitoring device 7. The electroluminescent anti-corrosion sensing layer 3 includes an electroluminescent sensing layer 302 and a main anti-corrosion layer 301 covering its outer side. The optical fiber channel 4 is embedded in an axial micro-groove on the inner surface of the main anti-corrosion layer 301, and the intelligent monitoring device 7 is installed on the outer surface of the composite protective layer 6.
[0018] The anti-corrosion lining layer 1 consists of an epoxy zinc-rich primer layer, a glass flake epoxy resin intermediate layer, and a polyurethane surface layer. The epoxy zinc-rich primer layer is 0.4 mm thick, the glass flake epoxy resin intermediate layer is 0.8 mm thick, and the polyurethane surface layer is 0.5 mm thick, for a total thickness of 1.7 mm. The inner surface of the anti-corrosion lining layer 1 is in contact with the transported medium, and its outer surface is tightly bonded to the inner wall of the pressure-bearing base pipe layer 2.
[0019] The pressure-bearing base pipe layer 2 is made of seamless carbon steel pipe, such as 20# steel, with a thickness of 12mm. Both the inner and outer surfaces of the pressure-bearing base pipe layer 2 are sandblasted to improve the adhesion between it and the anti-corrosion lining layer 1 and the electroluminescent sensing layer 302.
[0020] The electroluminescent anti-corrosion sensing layer 3 includes a main anti-corrosion layer 301 and an electroluminescent sensing layer 302. The main anti-corrosion layer 301 has a three-layer structure: an inner layer of 0.8 mm thick epoxy powder coating, a middle layer of 0.5 mm thick adhesive layer, and an outer layer of 1.0 mm thick polyethylene layer, with a total thickness of approximately 2.3 mm. The electroluminescent sensing layer 302 is made of electroluminescent particles and a polyurethane matrix, and the electroluminescent particles can be ZnS:Cu particles. The electroluminescent sensing layer 302 is disposed between the outer surface of the pressure-bearing base pipe layer 2 and the inner surface of the main anti-corrosion layer 301, and its electrodes are connected to the periodic power supply module 701 through wires, and operate under periodic electrical excitation.
[0021] The optical fiber channel 4 is embedded in an axial micro-groove fixed on the inner surface of the main anti-corrosion layer 301, and uses flexible PMMA optical fiber. The input end of the optical fiber channel 4 is attached to the electroluminescent sensing layer 302, and the output end is connected to the photoelectric detection module 702 through an IP68-rated sealed connector. Since the optical fiber channel 4 is located in the groove of the main anti-corrosion layer 301 and is inside the insulation layer 5 and the composite protective layer 6, it is not directly exposed to the backfill soil environment. External mechanical forces are primarily borne and dispersed by the composite protective layer 6 and the insulation layer 5.
[0022] The insulation layer 5 is made of rigid polyurethane foam with a thickness of 80 mm, a density of 50 kg / m³, and a thermal conductivity of no more than 0.025 W / (m·K). The inner surface of the insulation layer 5 is tightly bonded to the outer surface of the main anti-corrosion layer 301, and the outer surface is tightly bonded to the inner surface of the composite protective layer 6.
[0023] The composite protective layer 6 includes a high-density polyethylene (HDPE) layer with a thickness of 3.0 mm, which is used to provide mechanical protection for the internal structure and reduce the direct impact of external environmental factors such as soil and water vapor on the internal structure. An intelligent monitoring device 7 is installed on its outer surface.
[0024] The intelligent monitoring device 7 includes a periodic power supply module 701, a photoelectric detection module 702, and an LED warning light 703. The installation spacing of the intelligent monitoring device 7 can be 12m. The periodic power supply module 701 is connected to the electrodes of the electroluminescent sensing layer 302 via wires and can output a square wave of 100V AC~500Hz, with the pulse time controlled between 0.5 and 1 second, and the excitation cycle is once every 30 to 60 minutes. The photoelectric detection module 702 is connected to the output end of the optical fiber channel 4 via a sealed connector, and the LED warning light 703 is electrically connected to the photoelectric detection module 702.
[0025] When the main anti-corrosion layer 301 is intact and in normal condition, the periodic power supply module 701 applies electrical excitation to the electroluminescent sensing layer 302 according to a set cycle, and the optical response received by the photoelectric detection module 702 is in a preset normal recognition state. When the external anti-corrosion structure of the pipeline is partially damaged, and water, ions, etc. in the underground medium reach the electroluminescent sensing layer 302, the local electric field distribution changes, causing the local luminescence state of the electroluminescent sensing layer 302 under the same periodic electrical excitation condition to change relative to the normal state, and forming an abnormal light signal that can be identified by the photoelectric detection module 702. This abnormal light signal is collected by the optical fiber channel 4 and transmitted to the photoelectric detection module 702. Based on this, the photoelectric detection module 702 outputs a warning signal, drives the LED warning light 703, and can upload the monitoring results to a remote monitoring platform.
[0026] Finally, the following points should be noted: First, in the description of this application, it should be noted that, unless otherwise specified and limited, the terms "support", "backfill", and "reverse filter" should be interpreted broadly, and "up", "down", "left", "right", etc. are only used to indicate relative positional relationships. When the absolute position of the described object changes, the relative positional relationship may change.
[0027] The above description is only a preferred embodiment of the present utility model and is not intended to limit the present utility model. Any modifications, equivalent substitutions, improvements, etc., made within the spirit and principles of the present utility model should be included within the protection scope of the present utility model.
Claims
1. A buried oil pipeline with an integrated electroluminescent corrosion sensing structure, characterized in that, The oil pipeline structure, from the inside out, includes an anti-corrosion lining layer (1), a pressure-bearing base pipe layer (2), an electroluminescent anti-corrosion sensing layer (3), an optical fiber channel (4), an insulation layer (5), a composite protective layer (6), and an intelligent monitoring device (7). The electroluminescent anti-corrosion sensing layer (3) includes an electroluminescent sensing layer (302) and a main anti-corrosion layer (301) covering the outside of the electroluminescent sensing layer (302). The inner surface of the electroluminescent sensing layer (302) is attached to the outer surface of the pressure-bearing base pipe layer (2). The inner surface of the main anti-corrosion layer (301) is provided with an axial micro-groove. The optical fiber channel (4) is embedded in the axial micro-groove and is arranged adjacent to the electroluminescent sensing layer (302). The intelligent monitoring device (7) is arranged on the outer surface of the composite protective layer (6) and is connected to the electroluminescent sensing layer (302) and the optical fiber channel (4) respectively.
2. The buried oil pipeline with an integrated electroluminescent corrosion sensing structure according to claim 1, characterized in that, The electroluminescent sensing layer (302) is made of electroluminescent particles and polyurethane matrix composite, and is disposed between the outer surface of the pressure-bearing base pipe layer (2) and the inner surface of the main anti-corrosion layer (301), and is provided with electrodes connected to the periodic power supply module (701).
3. A buried oil pipeline with an integrated electroluminescent corrosion sensing structure according to claim 1, characterized in that, The outer surface of the anti-corrosion lining (1) is closely attached to the inner surface of the pressure-bearing base pipe layer (2), and the inner surface of the anti-corrosion lining (1) is used to contact the conveying medium.
4. A buried oil pipeline with an integrated electroluminescent corrosion sensing structure according to claim 1, characterized in that, The inner and outer surfaces of the pressure-bearing base pipe layer (2) are both sandblasted, and its outer surface is closely attached to the inner surface of the electroluminescent sensing layer (302).
5. A buried oil pipeline with an integrated electroluminescent corrosion sensing structure according to claim 1, characterized in that, The optical fiber channel (4) is made of flexible PMMA optical fiber. Its input end is attached to the electroluminescent sensing layer (302), and its output end is connected to the photoelectric detection module (702) of the intelligent monitoring device (7) through a sealed connector.
6. A buried oil pipeline with an integrated electroluminescent corrosion sensing structure according to claim 1, characterized in that, The insulation layer (5) is made of rigid polyurethane foam, and its inner surface is closely attached to the outer surface of the main anti-corrosion layer (301), and its outer surface is closely attached to the inner surface of the composite protective layer (6).
7. A buried oil pipeline with an integrated electroluminescent corrosion sensing structure according to claim 1, characterized in that, The composite protective layer (6) includes a high-density polyethylene layer, and the intelligent monitoring device (7) is installed on the outer surface of the composite protective layer (6).
8. A buried oil pipeline with an integrated electroluminescent corrosion sensing structure according to claim 1, characterized in that, The main anti-corrosion layer (301) includes an epoxy powder coating, an adhesive layer and a polyethylene layer arranged sequentially from the inside to the outside.
9. A buried oil pipeline with an integrated electroluminescent corrosion sensing structure according to claim 1, characterized in that, The intelligent monitoring device (7) includes a periodic power supply module (701), a photoelectric detection module (702), and an LED warning light (703); the periodic power supply module (701) is connected to the electrode of the electroluminescent sensing layer (302) through a wire, the photoelectric detection module (702) is connected to the output end of the optical fiber channel (4), and the LED warning light (703) is electrically connected to the photoelectric detection module (702).