Anti-corrosion structure for rotary kiln hood
By installing graphite refractory bricks and an anti-corrosion layer on the rotary kiln hood and fixing them with bolts and leak-proof washers, the corrosion problem of the hood was solved, achieving effective corrosion prevention and cost savings.
Patent Information
- Application Number
- CN202522787583.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2025-12-29
- Publication Date
- 2026-11-24
- Estimated Expiration
- 2035-12-29
AI Technical Summary
Rotary kiln hoods are susceptible to corrosion in high-humidity flue gas, and existing acid-resistant refractory bricks are easily damaged and difficult to repair.
The system combines refractory bricks with an anti-corrosion layer. The refractory bricks are made of graphite and are fixed with bolts and leak-proof washers to prevent corrosive slurry from coming into contact with and leaking.
It achieves excellent corrosion resistance, reduces maintenance costs, and ensures the long-term normal operation of the rotary kiln.
Smart Images

Figure CN225017073U_ABST
Abstract
Description
Technical Field
[0001] This utility model relates to the field of rotary kiln technology, specifically to an anti-corrosion structure for the rotary kiln hood. Background Technology
[0002] A rotary kiln is a common industrial heating furnace used for drying, heating, or roasting materials. During operation, the kiln rotates at a certain speed. It typically has hoods at both ends for feeding and discharging materials. During operation, the hoods (2) remain stationary while the kiln body (1) rotates. Figure 4 As shown, in a wet process kiln, the material is a slurry that is fed into the calcining kiln through the kiln tail feed pipe. High-humidity flue gas flows counter-currently through the tail hood and is discharged into the tail washing device. When the material reacts with acid, the high-humidity flue gas contains a large amount of high-concentration acid gas, and the condensed acid often causes significant corrosion to equipment such as the kiln tail hood. To prevent corrosion, acid-resistant refractory bricks with a certain strength are often used as the lining of the kiln tail hood. However, the kiln tail hood is an irregularly shaped component, which is extremely prone to falling off and being damaged during thermal expansion and vibration, making its maintenance and construction quite difficult. Summary of the Invention
[0003] The purpose of this utility model is to solve the technical problems existing in the prior art and to provide an anti-corrosion structure for rotary kiln hoods.
[0004] The specific solution of this utility model is as follows: a corrosion-resistant structure for a rotary kiln hood, including a hood shell, with a plurality of refractory bricks arranged on the inner wall of the hood shell, the refractory bricks being arranged according to the shape of the hood shell, a corrosion-resistant layer being provided between the refractory bricks and the inner wall of the hood shell, a through hole being provided in the middle of the refractory bricks, a bolt being installed in the through hole, a countersunk hole A being provided on the side of the refractory brick facing the corrosion-resistant layer, the countersunk hole A being arranged coaxially with the through hole, a leak-proof washer being installed in the countersunk hole A, the thickness of the leak-proof washer being greater than the thickness of the countersunk hole A, one end of the bolt passing through the leak-proof washer, the corrosion-resistant layer and the hood shell, and a locking nut being installed on the outer end.
[0005] Furthermore, a countersunk hole B is provided at the end of the through hole away from the cover. The depth of the countersunk hole B is greater than the thickness of the bolt head. The countersunk hole B is used to allow the bolt head to retract into the countersunk hole B.
[0006] Furthermore, the leak-proof gasket is made of polytetrafluoroethylene.
[0007] Optionally, the refractory brick has a trapezoidal cross-section, and two adjacent refractory bricks are installed in opposite directions, so that the refractory bricks press against each other through the inclined surface.
[0008] Furthermore, the refractory bricks are made of graphite.
[0009] This invention has the following advantages: by setting refractory bricks and an anti-corrosion layer, the refractory bricks, made of graphite, are inherently corrosion-resistant. The anti-corrosion layer prevents the corrosive slurry flowing into the gaps of the refractory bricks from corroding the casing. The refractory bricks are fixed with bolts and leak-proof washers are installed. The refractory bricks are pressed together, preventing the corrosive slurry that has seeped into the gaps of the refractory bricks from contacting the bolts and from leaking to the outside from the bolt holes. This achieves good anti-corrosion performance and saves on anti-corrosion costs. Attached Figure Description
[0010] Figure 1 This is a structural schematic diagram of Embodiment 1 of the present utility model;
[0011] Figure 2 yes Figure 1 AA view;
[0012] Figure 3 This is a schematic diagram of the structure of Embodiment 2 of this utility model;
[0013] Figure 4 This is a three-dimensional schematic diagram of a rotary kiln;
[0014] In the diagram: 1. Kiln body; 2. Cover; 3. Shell; 4. Refractory brick; 5. Anti-corrosion layer; 6. Countersunk hole B; 7. Bolt; 8. Leak-proof washer; 9. Locking nut. Detailed Implementation
[0015] Example 1
[0016] See Figure 1-2 This embodiment is an anti-corrosion structure for a rotary kiln hood 2, including a hood 3. The inner wall of the hood 3 is provided with several graphite refractory bricks 4. The refractory bricks 4 are arranged according to the shape of the hood 3. An anti-corrosion layer 5 is provided between the refractory bricks 4 and the inner wall of the hood 3. A through hole is provided in the middle of the refractory brick 4. A bolt 7 is installed in the through hole. A countersunk hole A is provided on the side of the refractory brick 4 facing the anti-corrosion layer 5. The countersunk hole A is arranged coaxially with the through hole. A leak-proof washer 8 is installed in the countersunk hole A. The thickness of the leak-proof washer 8 is greater than the thickness of the countersunk hole A. One end of the bolt 7 passes through the leak-proof washer 8, the anti-corrosion layer 5 and the hood 3, and a locking nut 9 is installed on the outer end.
[0017] Furthermore, a countersunk hole B6 is provided at the end of the through hole away from the cover 3. The depth of the countersunk hole B6 is greater than the thickness of the bolt 7 head. The countersunk hole B6 is used to allow the bolt 7 head to retract into the countersunk hole B6.
[0018] Furthermore, the leak-proof washer 8 is made of polytetrafluoroethylene. In this embodiment, the surface of the bolt 7 cap is provided with an anti-corrosion coating.
[0019] In this embodiment, during construction, several holes are first drilled at designed intervals on the surface of the casing 3. Then, an anti-corrosion layer 5 is applied to the inner wall of the casing 3. Finally, pre-made refractory bricks 4 and leak-proof washers 8 are attached one by one to the anti-corrosion layer 5, and bolts 7 are used to pass through the refractory bricks 4, leak-proof washers 8, and casing 3 and are then connected and tightened with locking nuts 9. Pressure is applied to the refractory bricks 4 by the bolts 7, and the refractory bricks 4 transmit the pressure to the leak-proof washers 8, thereby pressing the leak-proof washers 8 onto the anti-corrosion layer 5 to achieve the leak-proof function.
[0020] Example 2
[0021] See Figure 3 The structure of this embodiment is basically the same as that of embodiment one. The difference is in the splicing method of the refractory bricks 4. The cross section of the refractory bricks 4 in this embodiment is trapezoidal. Two adjacent refractory bricks 4 are installed in opposite directions, so that the refractory bricks 4 are pressed tightly against the adjacent refractory bricks 4 by the inclined surface. The advantage of this setting is that it can save some of the material cost of bolts 7 and anti-leakage washers 8 as well as the corresponding construction cost.
[0022] In this embodiment, because trapezoidal refractory bricks 4 are used, during construction, such as Figure 3 As shown, the middle refractory brick 4 can be pressed together by two adjacent refractory bricks 4, thereby saving the cost of fasteners for the middle refractory brick 4 and the corresponding construction cost.
[0023] This invention fixes the refractory bricks 4 with bolts 7, making them less likely to fall off and ensuring the long-term normal operation of the rotary kiln when used with corrosive materials.
Claims
1. A corrosion-resistant structure for rotary kiln hoods, characterized by: The device includes a casing, the inner wall of which is provided with several refractory bricks arranged according to the shape of the casing. A corrosion-resistant layer is provided between the refractory bricks and the inner wall of the casing. A through hole is provided in the middle of the refractory brick, and a bolt is installed in the through hole. A countersunk hole A is provided on the side of the refractory brick facing the corrosion-resistant layer. The countersunk hole A is arranged coaxially with the through hole. A leak-proof washer is installed in the countersunk hole A. The thickness of the leak-proof washer is greater than the thickness of the countersunk hole A. One end of the bolt passes through the leak-proof washer, the corrosion-resistant layer and the casing, and a lock nut is installed on the outer end.
2. The anti-corrosion structure for a rotary kiln hood according to claim 1, characterized in that: The end of the through hole away from the cover is provided with a countersunk hole B. The depth of the countersunk hole B is greater than the thickness of the bolt head. The countersunk hole B is used to allow the bolt head to retract into the countersunk hole B.
3. The anti-corrosion structure for a rotary kiln hood according to claim 1, characterized in that: The leak-proof gasket is made of polytetrafluoroethylene.
4. The anti-corrosion structure for a rotary kiln hood according to claim 1, characterized in that: The refractory brick has a trapezoidal cross-section, and two adjacent refractory bricks are installed in opposite directions, so that the refractory bricks press against each other through the inclined surface.
5. The anti-corrosion structure for a rotary kiln hood according to any one of claims 1-4, characterized in that: The refractory bricks are made of graphite.