Device for preventing the agglomeration of ceramsite sand in a kiln
By introducing disturbance and cooling mechanisms into the ceramsite calcination device, the material movement trajectory is changed and the local temperature is reduced, which solves the problems of agglomeration and kiln blockage during the high-temperature calcination of ceramsite and achieves stability of material flowability and product quality in the kiln.
Patent Information
- Application Number
- CN202620104625.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2026-01-26
- Publication Date
- 2026-11-24
- Estimated Expiration
- 2036-01-26
AI Technical Summary
In the high-temperature calcination process of ceramsite sand, the existing technology is prone to uneven heating of the material or excessively high local temperature, which can easily lead to melting and adhesion between particles, forming agglomerates or kiln blockage, affecting the flowability of materials in the kiln and the stability of product quality. Moreover, the overall control method is difficult to achieve targeted intervention.
The design combines a disturbance mechanism and a cooling mechanism. The disturbance mechanism changes the material movement trajectory through an adjustable-angle disturbance plate, while the cooling mechanism reduces the temperature of the kiln-prone area through a cooling medium. The disturbance and cooling work together to achieve real-time directional intervention in specific areas of the kiln.
It effectively reduced the probability of ceramsite sand agglomeration in the kiln, improved the continuity of kiln operation and the consistency of product quality, and enhanced the ability to respond to sudden agglomeration trends.
Smart Images

Figure CN225017138U_ABST
Abstract
Description
Technical Field
[0001] This utility model relates to the field of sintering equipment technology, and in particular to a device for preventing ceramsite sand from caking in a kiln. Background Technology
[0002] During high-temperature calcination, ceramsite sand is prone to melting and agglomeration due to uneven heating or excessively high local temperatures, leading to clumping and even kiln blockage. This affects the flowability of materials within the kiln and the stability of product quality. To mitigate this problem, existing rotary kiln or vertical kiln systems typically intervene by controlling the kiln speed, adjusting fuel supply, or optimizing the feeding method. However, these methods primarily affect the overall thermal regime or material conveying rhythm. When dealing with local hot spots or sudden agglomeration trends, their response speed and control precision are limited, making it difficult to achieve targeted intervention on the state of ceramsite sand in specific areas of the kiln. Consequently, the risk of localized kiln blockage may still exist in continuous production, affecting the continuity of equipment operation and product consistency. Utility Model Content
[0003] The purpose of this utility model is to provide a device for preventing ceramsite sand from caking in a kiln, thus solving the problems mentioned in the background art.
[0004] This utility model is implemented as follows: a kiln device for preventing ceramsite sand agglomeration includes a kiln body, a disturbance mechanism, and a cooling mechanism, wherein: The disturbance mechanism is installed on the inner wall of the kiln. The disturbance mechanism includes a support ring, a disturbance plate, a rotating shaft, and a drive rod. The support ring is fixedly connected to the circumferential position of the inner wall of the kiln. Multiple disturbance plates are equidistantly distributed along the circumference of the support ring. One end of the disturbance plate is rotatably connected to the support ring through the rotating shaft. The other end of the disturbance plate extends towards the center of the kiln and is curved in an arc. One end of the drive rod is fixedly connected to the middle of the disturbance plate. The other end of the drive rod passes through the side wall of the kiln and is connected to an external operating component. By pushing and pulling the drive rod, the tilt angle of the disturbance plate is changed, thereby adjusting the tumbling trajectory and residence time of the material in the kiln.
[0005] The cooling mechanism is embedded in the inner wall of the kiln and located below the disturbance mechanism. The cooling mechanism includes a cooling chamber, an inlet pipe, an outlet pipe, and a flow guide baffle. The cooling chamber is formed by the inner wall of the kiln and the inner lining plate. The inlet pipe and the outlet pipe are respectively connected to both ends of the cooling chamber. The flow guide baffle is fixedly connected to the inside of the cooling chamber and divides the cooling chamber into multiple serpentine flow channels. The cooling medium flows in from the inlet pipe and flows along the serpentine flow channels, and is discharged through the outlet pipe, carrying away the heat of the local area of the kiln body, reducing the surface temperature of the ceramsite sand in that area, and inhibiting its melting tendency.
[0006] Optionally, the surface of the disturbance plate is provided with a number of raised stripes, which extend along the length of the disturbance plate and form a guide groove between adjacent raised stripes to guide the ceramsite sand to slide in a specific direction and avoid the material from accumulating on the surface of the disturbance plate.
[0007] Optionally, a sealing sleeve is provided at the position where the drive rod passes through the side wall of the kiln body. The inner wall of the sealing sleeve is tightly fitted with the outer wall of the drive rod. The two ends of the sealing sleeve are fixedly connected to the outer wall of the kiln body and the inner lining plate, respectively, to prevent high-temperature gas from leaking out of the kiln.
[0008] Optionally, the inner lining of the cooling chamber is made of high-temperature resistant alloy material, and its side facing the kiln cavity is sprayed with a heat-insulating coating to reduce the interference of the cooling medium on the overall temperature field inside the kiln and ensure that cooling is only applied to the target area.
[0009] Optionally, the inlet pipe and outlet pipe are externally connected to a flow regulating valve, which controls the local cooling intensity by adjusting the flow rate of the cooling medium to adapt to the process requirements of different calcination stages.
[0010] Optionally, multiple sets of disturbance mechanisms are arranged along the axial direction on the inner wall of the kiln. Each set of disturbance mechanisms corresponds to an independent cooling mechanism. The drive rods of each set of disturbance mechanisms are connected to different operating handles. Operators can adjust the disturbance angle and cooling intensity of a certain area individually according to the kiln temperature monitoring data to achieve precise intervention in different zones.
[0011] Optionally, the operating handle is equipped with an angle indicator disk, which is fixedly connected to the outer wall of the kiln. The outer end of the drive rod is fixedly connected to the pointer of the angle indicator disk. The pointer rotates with the drive rod and indicates the current tilt angle of the disturbance plate on the angle indicator disk, which facilitates precise control by the operator.
[0012] Optionally, the flow guide baffles of the cooling mechanism are arranged in a wave-like pattern, so that the cooling medium forms a continuous zigzag flow path in the cooling chamber, prolonging the heat exchange time and improving the local heat dissipation efficiency.
[0013] Optionally, the free end edge of the disturbance plate is provided with a wear-resistant trim, which is made of silicon carbide ceramic material to enhance the service life of the disturbance plate in a high-temperature abrasive environment.
[0014] The present invention provides a device for preventing ceramsite sand from caking in a kiln, which has the following beneficial effects: This device uses adjustable-angle disturbance plates in its disturbance mechanism to alter the movement trajectory and tumbling frequency of ceramsite sand within the kiln, breaking up localized material accumulation and promoting uniform heat transfer. Simultaneously, a cooling mechanism creates a controllable low-temperature zone below the disturbance area, directly reducing the surface temperature of materials in areas prone to clumping and inhibiting particle melting and adhesion. The synergistic effect of disturbance and cooling not only alleviates the problem of overall thermal regime control lag but also enables real-time, targeted intervention in specific high-risk areas within the kiln. Multiple disturbance and cooling units are distributed along the kiln's axial direction, coupled with independent operating handles and flow control valves, allowing operators to flexibly adjust the disturbance intensity and cooling depth of each area according to actual operating conditions, significantly improving the response capability to sudden clumping trends. The design of raised stripes and guide channels further optimizes material flow characteristics, preventing secondary accumulation; wear-resistant edging and heat-insulating coatings ensure long-term stable operation of the device in high-temperature environments. In summary, this invention effectively reduces the probability of ceramsite sand clumping, improving the continuity of kiln operation and the consistency of product quality. Attached Figure Description
[0015] Figure 1 This is a schematic diagram of the overall structure of a kiln device for preventing ceramsite sand caking according to the present invention; Figure 2 This is a partial cross-sectional view of the disturbance mechanism and cooling mechanism according to an embodiment of this application; Figure 3 This is a partially enlarged structural diagram of the connection between the disturbance plate and the drive rod of this utility model; Explanation of reference numerals in the attached figures: 1. Kiln body; 2. Agitator; 3. Cooling mechanism; 4. Support ring; 5. Agitator plate; 6. Rotating shaft; 7. Drive rod; 8. Operating handle; 9. Cooling chamber; 10. Inlet pipe; 11. Outlet pipe; 12. Flow guide baffle; 13. Inner lining plate; 14. Raised stripes; 15. Material guide chute; 16. Sealing sleeve; 17. Heat insulation coating; 18. Flow regulating valve; 19. Angle indicator; 20. Pointer; 21. Wear-resistant edging; 22. Inner wall of the kiln; 23. External operating components; 24. Serpentine flow channel; 25. Silicon carbide ceramic material. Detailed Implementation
[0016] The technical solutions of the present utility model will be clearly and completely described below with reference to the accompanying drawings of the embodiments. Obviously, the described embodiments are only some embodiments of the present utility model, and not all embodiments. Based on the embodiments of the present utility model, all other embodiments obtained by those of ordinary skill in the art without creative effort are within the protection scope of the present utility model.
[0017] Please see Figures 1 to 3This utility model provides a device for preventing ceramsite sand from caking in a kiln. This device is suitable for industrial scenarios where ceramsite sand is subjected to local melting and adhesion during high-temperature calcination, preventing the formation of lumps or kiln caking. The device includes a kiln body 1, a disturbance mechanism 2, and a cooling mechanism 3, wherein the disturbance mechanism 2 and the cooling mechanism 3 are arranged alternately along the axial direction of the kiln body 1, together forming an active intervention system for the flow state of materials and the local temperature field inside the kiln.
[0018] Reference Figure 1 The kiln body 1 has a cylindrical structure, with an internal chamber for containing ceramsite sand and firing it at high temperatures. At least two sets of agitation mechanisms 2 are axially arranged on the inner wall 22 of the kiln body 1, with a cooling mechanism 3 correspondingly located below each set of agitation mechanisms 2. Each agitation mechanism 2 is independently configured and connected to a different operating handle 8, allowing the operator to individually adjust the operating status of the corresponding agitation mechanism 2 according to the temperature distribution in different areas of the kiln.
[0019] Reference Figure 2 The disturbance mechanism 2 includes a support ring 4, disturbance plates 5, a rotating shaft 6, and a drive rod 7. The support ring 4 is an annular component, and its outer circumference is fixedly connected to the inner wall 22 of the kiln body 1. The axis of the support ring 4 coincides with the axis of the kiln body 1. Multiple disturbance plates 5 are equidistantly distributed along the circumference of the support ring 4, and the included angle between adjacent disturbance plates 5 is equal. One end of each disturbance plate 5 is rotatably connected to the support ring 4 through the rotating shaft 6, which is perpendicular to the radial direction of the support ring 4. The disturbance plate 5 can swing around the rotating shaft 6 within a certain angle range. The other end of the disturbance plate 5 extends towards the center of the kiln body 1 and is curved in an arc shape. Its curvature direction is consistent with the rotation direction of the kiln body 1 to adapt to the movement trend of the material as the kiln body 1 rotates.
[0020] One end of the drive rod 7 is fixedly connected to the middle of the disturbance plate 5, and the other end of the drive rod 7 passes through the side wall of the kiln body 1 and extends outward to connect with the external operating component 23. The operating component 23 is the operating handle 8, which is fixedly connected to the outer end of the drive rod 7. When the operator moves the operating handle 8, the drive rod 7 drives the disturbance plate 5 to rotate around the rotating shaft 6, thereby changing the tilt angle of the disturbance plate 5 relative to the horizontal plane. The change in the tilt angle of the disturbance plate 5 directly affects the tumbling trajectory, sliding speed, and residence time of the ceramsite sand in the kiln body 1, breaking the local accumulation state and promoting the uniform transfer of heat in the material layer.
[0021] Reference Figure 3The surface of the disturbance plate 5 is provided with several raised stripes 14, which extend along the length of the disturbance plate 5, and a guide groove 15 is formed between adjacent raised stripes 14. The cross-section of the guide groove 15 is V-shaped or U-shaped, and its depth and width are set according to the particle size range of the ceramsite sand, to ensure that the ceramsite sand flows directionally along the guide groove 15 during the sliding process on the surface of the disturbance plate 5, and to avoid material retention or accumulation on the surface of the disturbance plate 5. The free end edge of the disturbance plate 5 is provided with a wear-resistant inlay 21, which is made of silicon carbide ceramic material 25 and is fixed to the end of the disturbance plate 5 by high-temperature sintering or mechanical fitting, so as to resist the continuous scouring and abrasion of the edge of the disturbance plate 5 by the ceramsite sand under high temperature environment, and extend the service life of the disturbance plate 5.
[0022] A sealing sleeve 16 is provided at the position where the drive rod 7 passes through the side wall of the kiln body 1. The sealing sleeve 16 is a hollow cylindrical structure, with one end welded and fixed to the outer wall of the kiln body 1, and the other end fixedly connected to the inner lining plate 13. The drive rod 7 passes through the central hole of the sealing sleeve 16, and the inner wall of the sealing sleeve 16 is tightly fitted with the outer wall of the drive rod 7, with no gap between them, to prevent high-temperature gas in the kiln from leaking out through the gap between the drive rod 7 and the kiln body 1, thus ensuring the sealing performance and thermal efficiency of the kiln body 1.
[0023] The cooling mechanism 3 is embedded in the inner wall 22 of the kiln body 1 and located directly below the disturbance mechanism 2. The cooling mechanism 3 includes a cooling chamber 9, an inlet pipe 10, an outlet pipe 11, and a flow guide baffle 12. The cooling chamber 9 is formed by the inner wall 22 of the kiln body 1 and the inner lining plate 13. The inner lining plate 13 is an arc-shaped plate with its inner side facing the kiln cavity and its outer side forming a closed cooling chamber 9 with the inner wall 22 of the kiln body 1. The inlet pipe 10 and the outlet pipe 11 are respectively connected to both ends of the cooling chamber 9. The inlet pipe 10 is located at the bottom of one end of the cooling chamber 9, and the outlet pipe 11 is located at the top of the other end. After the cooling medium flows in from the inlet pipe 10, it completes the heat exchange process in the cooling chamber 9 and is finally discharged from the outlet pipe 11.
[0024] The flow guide baffle 12 is fixedly connected inside the cooling chamber 9, dividing the cooling chamber 9 into multiple continuous serpentine flow channels 24. The flow guide baffle 12 is arranged in a wave shape, with its crests and troughs alternately connecting between the inner lining plate 13 and the inner wall 22 of the kiln body 1, forcing the cooling medium to flow along a serpentine path in the cooling chamber 9, prolonging the residence time of the cooling medium in the cooling chamber 9, and enhancing the heat exchange effect. The cooling medium can be water, heat transfer oil, or other liquids with high specific heat capacity. When it flows through the serpentine flow channel 24, it absorbs heat from local areas of the kiln body 1, reduces the surface temperature of the ceramsite sand in that area, and inhibits the melting and adhesion of particles due to overheating.
[0025] The inner lining plate 13 is made of high-temperature resistant alloy material, and its side facing the kiln cavity is sprayed with a heat insulation coating 17. The heat insulation coating 17 is made of zirconium oxide or alumina-based ceramic material with a thickness of 0.5 mm to 2 mm. It effectively blocks the low temperature in the cooling chamber 9 from interfering with the overall temperature field of the kiln cavity, ensuring that the cooling effect is limited to the target area and avoiding affecting the normal firing process in other areas of the kiln.
[0026] A flow regulating valve 18 is externally connected to the inlet pipe 10 and the outlet pipe 11. The flow regulating valve 18 is a manual or electric regulating valve, installed on the exposed section of the inlet pipe 10 or the outlet pipe 11. The operator adjusts the flow cross-sectional area of the cooling medium by rotating the handwheel or actuator of the flow regulating valve 18, thereby controlling the flow rate and volume of the cooling medium and achieving precise control of the local cooling intensity. In the early stage of ceramsite sand calcination or in a stage with low risk of kiln clumping, the flow rate of the cooling medium can be reduced; when an abnormal increase in local temperature or a tendency to agglomerate is detected, the flow rate can be increased to enhance the cooling effect.
[0027] An angle indicator dial 19 is provided on the operating handle 8. The angle indicator dial 19 is a circular graduated dial, with its back fixedly connected to the outer wall of the kiln body 1, and its surface facing outward. The outer end of the drive rod 7 is fixedly connected to the pointer 20, which is perpendicular to the surface of the angle indicator dial 19 and points to the scale line. When the operating handle 8 drives the drive rod 7 to rotate, the pointer 20 rotates synchronously and indicates the current tilt angle of the disturbance plate 5 on the angle indicator dial 19. The scale range of the angle indicator dial 19 covers the adjustable angle range of the disturbance plate 5, typically from -30 degrees to +60 degrees, making it easy for operators to intuitively read and accurately reproduce the required disturbance angle.
[0028] Multiple sets of disturbance mechanisms 2 are arranged axially along the inner wall 22 of the kiln body 1, each set of disturbance mechanisms 2 corresponding to an independent cooling mechanism 3. The drive rods 7 of each set of disturbance mechanisms 2 are connected to different operating handles 8, and the inlet pipes 10 and outlet pipes 11 of each cooling mechanism 3 are connected to independent flow regulating valves 18. The operator can adjust the operating handles 8 and flow regulating valves 18 of a certain area individually according to the infrared temperature measurement data or thermocouple feedback information at different axial positions in the kiln body 1, so as to achieve precise intervention in the disturbance intensity and cooling depth of that area. For example, when the temperature in the middle area of the kiln body 1 is too high, only the operating handle 8 of the middle area is adjusted to increase the inclination angle of the disturbance plate 5 to enhance the material turning, and at the same time the flow regulating valve 18 of that area is opened to enhance cooling, while the original operating conditions of other areas remain unchanged.
[0029] In actual operation, the ceramsite sand enters from the high end of the kiln body 1 and moves axially towards the low end under the slow rotation of the kiln body 1. When the material passes through the area where the disturbance mechanism 2 is located, the disturbance plate 5 applies disturbance force to it, changing the rolling path of the material and breaking up any agglomerates that may form. Subsequently, the material falls into the area above the cooling mechanism 3. At this time, the cooling medium in the cooling chamber 9 has already lowered the kiln wall temperature in this area. The surface temperature of the ceramsite sand drops during its brief stay here, and the melting tendency is effectively suppressed. Through the synergistic effect of disturbance and cooling, the risk of kiln clogging in the hot spot area inside the kiln is significantly reduced.
[0030] The arc-shaped structure of the disturbance plate 5 matches the rotation direction of the kiln body 1, allowing it to apply moderate lateral disturbance to the material without hindering its normal movement. The combination of raised stripes 14 and the guide chute 15 further optimizes the flow behavior of the material on the surface of the disturbance plate 5, preventing fine powder or wet material from accumulating on the disturbance plate 5 and forming a hard shell. The sealing sleeve 16 ensures that the drive rod 7 can maintain the airtightness of the kiln body 1 during frequent push-pull operations, avoiding energy waste or safety hazards caused by high-temperature flue gas leakage.
[0031] In summary, this invention, through the cooperation of the structured disturbance mechanism 2 and the cooling mechanism 3, achieves active and directional control of the material state and temperature field in local areas of the kiln without altering the overall thermal regime of the kiln body 1. All structural components are made of high-temperature resistant and wear-resistant materials, and are supplemented with heat insulation and sealing designs to ensure the reliability and stability of the device under long-term high-temperature operating conditions.
[0032] The above description is only a preferred embodiment of the present utility model and is not intended to limit the present utility model. Any modifications, equivalent substitutions and improvements made within the spirit and principles of the present utility model should be included within the protection scope of the present utility model.
Claims
1. A device for preventing ceramsite sand caking in a kiln, characterized in that, It includes a kiln body (1), a disturbance mechanism (2), and a cooling mechanism (3), wherein: The disturbance mechanism (2) is installed on the inner wall (22) of the kiln body (1) and includes a support ring (4), a disturbance plate (5), a rotating shaft (6) and a drive rod (7). The support ring (4) is fixedly connected to the circumferential position of the inner wall (22) of the kiln body (1). Multiple disturbance plates (5) are equidistantly distributed along the circumferential direction of the support ring (4). One end of the disturbance plate (5) is rotatably connected to the support ring (4) through the rotating shaft (6), and the other end extends toward the center of the kiln body (1) and is curved in an arc. One end of the drive rod (7) is fixedly connected to the middle of the disturbance plate (5), and the other end passes through the side wall of the kiln body (1) and is connected to the operating handle (8). The cooling mechanism (3) is embedded in the inner wall (22) of the kiln body (1) and located below the disturbance mechanism (2). It includes a cooling chamber (9), an inlet pipe (10), an outlet pipe (11), and a flow guide baffle (12). The cooling chamber (9) is formed by the inner wall (22) of the kiln body (1) and the inner lining plate (13). The inlet pipe (10) and the outlet pipe (11) are respectively connected to both ends of the cooling chamber (9). The flow guide baffle (12) is fixed inside the cooling chamber (9) and divides the cooling chamber (9) into multiple serpentine flow channels (24).
2. The kiln device for preventing ceramsite sand caking according to claim 1, characterized in that: The surface of the disturbance plate (5) is provided with a plurality of raised stripes (14), the raised stripes (14) extend along the length direction of the disturbance plate (5), and a guide groove (15) is formed between adjacent raised stripes (14).
3. The kiln device for preventing ceramsite sand caking according to claim 1, characterized in that: A sealing sleeve (16) is provided at the position where the drive rod (7) passes through the side wall of the kiln body (1). The inner wall of the sealing sleeve (16) is tightly fitted with the outer wall of the drive rod (7). The two ends of the sealing sleeve (16) are fixedly connected to the outer wall of the kiln body (1) and the inner lining plate (13), respectively.
4. The kiln device for preventing ceramsite sand caking according to claim 1, characterized in that: The inner lining plate (13) of the cooling chamber (9) is made of high-temperature resistant alloy material, and a heat insulation coating (17) is sprayed on the side facing the kiln cavity.
5. The kiln device for preventing ceramsite sand caking according to claim 1, characterized in that: The inlet pipe (10) and outlet pipe (11) are externally connected by a flow regulating valve (18).
6. The kiln device for preventing ceramsite sand caking according to claim 1, characterized in that: The inner wall (22) of the kiln body (1) is provided with multiple sets of disturbance mechanisms (2) along the axial direction. Each set of disturbance mechanisms (2) corresponds to an independent cooling mechanism (3). The drive rod (7) of each set of disturbance mechanisms (2) is connected to different operating handles (8).
7. The kiln device for preventing ceramsite sand caking according to claim 6, characterized in that: The operating handle (8) is provided with an angle indicator (19), which is fixedly connected to the outer wall of the kiln body (1). The outer end of the drive rod (7) is fixedly connected to the pointer (20). The pointer (20) rotates with the drive rod (7) and indicates the tilt angle of the current disturbance plate (5) on the angle indicator (19).