Flat plate solid oxide cell electrolyte layer densification detection apparatus

The highly integrated planar solid oxide battery electrolyte layer density testing equipment solves the problems of complex equipment and difficulty in quantitative detection in existing technologies, and realizes rapid and safe electrolyte layer density testing, supporting the battery industrialization process.

CN225017975UActive Publication Date: 2026-11-24JIANGSU JINGCI INTELLIGENT SENSING TECH RES INST CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202522424751.2
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2025-11-15
Publication Date
2026-11-24
Estimated Expiration
2035-11-15

AI Technical Summary

Technical Problem

In the existing technology, the plate-type solid oxide battery electrolyte layer density detection equipment has a complex structure and low integration, cannot achieve quantitative detection at room temperature, and poses safety hazards.

Method used

A highly integrated planar solid oxide battery electrolyte layer density testing device was designed, including a gas cylinder, pressure reducing valve, rubber ring, pressurization component, test platform, and metering component. Through integrated design and rolling cooperation, quantitative testing at room temperature is achieved.

Benefits of technology

It achieves small equipment footprint, low connection loss, and low energy consumption, enabling rapid and quantitative detection of electrolyte layer density, reducing battery damage risk, and supporting the optimization of stack assembly and manufacturing processes.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN225017975U_ABST
    Figure CN225017975U_ABST
Patent Text Reader

Abstract

This utility model relates to the field of solid oxide battery testing technology, and in particular to a planar solid oxide battery electrolyte layer density testing device, comprising a mounting frame, a gas cylinder, a pressure reducing valve, a rubber ring, and a pressurizing component, a testing platform, a first metering component, a second metering component, and a third metering component mounted on the mounting frame. The gas cylinder's outlet is connected to the pressure reducing valve's inlet. The pressurizing component and the testing platform are arranged vertically opposite each other. The rubber ring is placed on the testing platform's surface. The testing platform has a hollow structure, with an air hole at the center of the platform surface. The first outlet of the pressure reducing valve is connected to a cylinder in the pressurizing component through the first metering component, and its second outlet is connected to the testing platform through the second metering component. The third metering component is connected to the testing platform. This utility model has a simple structural design, high integration, small footprint, and can achieve quantitative detection at room temperature.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This utility model relates to the field of solid oxide battery testing technology, and in particular to a flat-plate solid oxide battery electrolyte layer density testing device. Background Technology

[0002] Solid oxide batteries (SOCs) are a highly efficient and environmentally friendly electrochemical energy conversion technology. Among them, the planar single-cell structure has been widely studied due to its excellent mechanical and electrochemical properties. A single cell uses a porous anode as a support layer, with a dense electrolyte film on its surface, approximately 8 to 10 micrometers thick. The density of the electrolyte layer is closely related to the performance of the single cell. During the mass production of single cells, the electrolyte layer of large-area single cells is prone to various defects, such as microcracks and pores. These defects may cause structural damage under the high-temperature operation (700-800℃) of solid oxide batteries, thus posing safety hazards.

[0003] Defect identification in the electrolyte layer of a single cell is mainly achieved through high-temperature in-situ testing. During testing, the single cell is heated to its operating temperature and hydrogen and air are introduced. Changes in the open-circuit voltage or exhaust gas composition are observed to determine the presence of electrolyte layer defects. While this method allows for in-situ detection at high temperatures, if the electrolyte layer density is insufficient, oxygen from the air electrode side will diffuse to the fuel electrode, causing oxidation and combustion, resulting in permanent damage to the single cell. Furthermore, the testing process is lengthy and lacks quantitative detection capabilities, directly limiting the industrialization of solid oxide batteries.

[0004] Currently, although there are testing devices on the market that can identify defects in the electrolyte layer of a single cell at room temperature, most of these devices have complex structural designs, many parts, and adopt a split design, resulting in large connection losses between components, low integration, and a large footprint. Utility Model Content

[0005] The technical problem to be solved by this utility model is: in order to solve the problems existing in the prior art mentioned above, to provide a flat-plate solid oxide battery electrolyte layer density detection device with simple structural design, high integration, small footprint, and the ability to achieve quantitative detection at room temperature.

[0006] The technical solution adopted by this utility model to solve its technical problem is: a flat-plate solid oxide battery electrolyte layer density testing device, including a mounting frame, a gas cylinder, a pressure reducing valve, a rubber ring, and a pressurizing component, a testing platform, a first metering component, a second metering component, and a third metering component mounted on the mounting frame; the gas cylinder's outlet is connected to the pressure reducing valve's inlet, the pressurizing component and the testing platform are arranged vertically opposite each other, the rubber ring is set on the testing platform's surface, the testing platform has a hollow structure, and an air hole is opened in the center of the testing platform's surface; the first outlet of the pressure reducing valve is connected to a cylinder in the pressurizing component through the first metering component, and its second outlet is connected to the testing platform through the second metering component; the third metering component is connected to the testing platform.

[0007] Furthermore, the pressurization assembly includes a cylinder, a pressurization column, a pressurization plate, and a pressure sensor. The cylinder is mounted on the top of the mounting bracket with its drive end facing downwards. The pressurization column is mounted on the drive end of the cylinder. The top center of the pressurization plate is connected to the bottom end of the pressurization column via a pressure sensor. The pressurization plate is arranged vertically opposite to the test platform.

[0008] Furthermore, the pressurizing assembly also includes guide shafts, which are respectively installed at the four corners of the pressurizing plate and pass through the shaft holes opened at the top of the mounting bracket.

[0009] Furthermore, the guide shaft is slidably fitted with the shaft hole.

[0010] Furthermore, the guide shaft is clearance-fitted with the shaft hole, and the inner wall of the shaft hole is fitted with balls, which abut against the guide shaft.

[0011] Furthermore, the test platform has limiting protrusions at each of the four corners of its surface.

[0012] Furthermore, the first metering component includes a first pipeline, a first gas mass flow meter, and a first solenoid valve. The first pipeline connects the first outlet of the pressure reducing valve to the cylinder. The first gas mass flow meter is installed on the top of the mounting bracket and is located on the first pipeline. The first solenoid valve is installed on the first gas mass flow meter.

[0013] Furthermore, the second metering component includes a second pipeline, a second gas mass flow meter, and a second solenoid valve. The second pipeline connects the second outlet of the pressure reducing valve to the test platform. The second gas mass flow meter is installed at the bottom of the mounting bracket and is located on the second pipeline. The second solenoid valve is installed on the second gas mass flow meter.

[0014] Furthermore, the third metering component includes a third pipeline, a pressure sensor, and a third solenoid valve. The pressure sensor is installed at the bottom of the mounting bracket and is connected to the test platform through the third pipeline; the third solenoid valve is installed on the pressure sensor.

[0015] Furthermore, the mounting bracket includes a top cover, a base, and a support column, wherein the top cover and the base are arranged opposite each other vertically and are connected by the support column.

[0016] The beneficial effects of this utility model are:

[0017] (1) This utility model integrates the rubber ring, the pressure component, the test platform, the first metering component, the second metering component and the third metering component on the mounting frame. The structure is simple, the integration is high, and the integrated design significantly reduces the floor space and the connection loss between components. It can also achieve quantitative detection at room temperature.

[0018] (2) By setting the ball bearings, the guide shaft and the shaft hole form a rolling fit, which reduces the coefficient of friction, thereby extending the service life and reducing energy consumption.

[0019] (3) By setting the limiting protrusion, the present invention mechanically limits the end of the stroke of the pressure plate, thereby avoiding overpressure due to pressure sensor failure or malfunction, and thus avoiding damage to the battery due to overpressure. Attached Figure Description

[0020] The present invention will be further described below with reference to the accompanying drawings and embodiments.

[0021] Figure 1 This is a schematic diagram of the structure of this utility model;

[0022] Figure 2 This is a front view of the present invention;

[0023] Figure 3 This is the right view of this utility model;

[0024] Figure 4 This is a cross-sectional view of the ball bearing in this utility model;

[0025] Figure 5 This is a schematic diagram of the limiting protrusion in this utility model.

[0026] In the diagram: 100, mounting bracket; 110, top cover; 120, base; 130, support column; 200, gas cylinder; 300, pressure reducing valve; 400, rubber ring; 500, pressurizing assembly; 510, cylinder; 520, pressurizing column; 530, pressure plate; 540, pressure sensor; 550, guide shaft; 560, ball bearing; 600, test platform; 610, air port; 700, first metering assembly; 710, first pipeline; 720, first gas mass flow meter; 730, first solenoid valve; 800, second metering assembly; 810, second pipeline; 820, second gas mass flow meter; 830, second solenoid valve; 900, third metering assembly; 910, third pipeline; 920, air pressure sensor; 930, third solenoid valve; 1000, limit protrusion. Detailed Implementation

[0027] The present invention will now be described in further detail with reference to the accompanying drawings. These drawings are simplified schematic diagrams, illustrating only the basic structure of the present invention, and therefore only show the components relevant to the present invention.

[0028] Example 1

[0029] like Figure 1 As shown, a flat-plate solid oxide battery electrolyte layer density testing device includes a mounting frame 100, a gas cylinder 200, a pressure reducing valve 300, a rubber ring 400, and a pressurizing component 500, a testing platform 600, a first metering component 700, a second metering component 800, and a third metering component 900 mounted on the mounting frame 100. The gas outlet of the gas cylinder 200 is connected to the gas inlet of the pressure reducing valve 300. The pressurizing component 500 and the testing platform 600 are arranged vertically opposite each other. The rubber ring 400 is set on the table surface of the testing platform 600. The testing platform 600 has a hollow structure, and an air hole 610 is opened in the center of the table surface of the testing platform 600. The first outlet of the pressure reducing valve 300 is connected to the cylinder 510 in the pressurizing component 500 through the first metering component 700, and its second outlet is connected to the testing platform 600 through the second metering component 800. The third metering component 900 is connected to the testing platform 600.

[0030] Specifically, the gas cylinder 200 stores a detection gas, such as helium; the outlet of the gas cylinder 200 is connected to the inlet of the pressure reducing valve 300 through a main pipe; the pressure reducing valve 300 has two switches for controlling the start and stop of the instrument; a fourth solenoid valve is installed on the pressure reducing valve 300; the entire device can be controlled by a control system (not shown in the figure).

[0031] The rubber ring 400, pressure assembly 500, test platform 600, first metering assembly 700, second metering assembly 800 and third metering assembly 900 are integrated on the mounting frame 100. The structure is simple, highly integrated and integrated, which significantly reduces the floor space, reduces the connection loss between components, and enables quantitative detection at room temperature.

[0032] like Figure 1 and Figure 2 As shown, the mounting bracket 100 includes a top cover 110, a base 120, and a support column 130. The top cover 110 and the base 120 are arranged vertically opposite each other and connected by the support column 130. Specifically, the test platform 600 is installed at the top center of the base 120.

[0033] like Figure 1 and Figure 2 As shown, the pressurization assembly 500 includes a cylinder 510, a pressurization column 520, a pressurization plate 530, and a pressure sensor 540. The cylinder 510 is mounted on the top of the mounting bracket 100 with its drive end facing downwards. The pressurization column 520 is mounted on the drive end of the cylinder 510. The top center of the pressurization plate 530 is connected to the bottom end of the pressurization column 520 via the pressure sensor 540. The pressurization plate 530 is vertically opposite to the test platform 600. Specifically, the cylinder 510 is mounted in the center of the top cover 110.

[0034] Cylinder 510 drives pressure plate 530 to press down, squeezing the battery placed on rubber ring 400 until the pressure value displayed by pressure sensor 540 reaches the loading pressure of normal assembly of solid oxide battery stack, such as 200-300 kgf. At this time, a sealed cavity is formed between the battery, rubber ring 400 and test platform 600.

[0035] like Figure 1 and Figure 2 As shown, the pressurizing assembly 500 also includes guide shafts 550, which are respectively installed at the four corners of the pressurizing plate 530. The guide shafts 550 pass through the shaft holes opened at the top of the mounting bracket 100. Specifically, the shaft holes are opened on the top cover 110; the guide shafts 550 slide with the shaft holes to guide the movement of the pressurizing plate 530, ensuring the stable and precise lifting and lowering of the pressurizing plate 530.

[0036] like Figure 1 and Figure 2As shown, the first metering component 700 includes a first pipeline 710, a first gas mass flow meter 720, and a first solenoid valve 730. The first pipeline 710 connects the first outlet of the pressure reducing valve 300 to the cylinder 510. The first gas mass flow meter 720 is mounted on the top of the mounting bracket 100 and is positioned on the first pipeline 710. The first solenoid valve 730 is mounted on the first gas mass flow meter 720. Specifically, the first gas mass flow meter 720 is mounted on the top cover 110 and has an accuracy of at least 0.01 ml / min. Two switches are arranged on the first gas mass flow meter 720 for controlling the start and stop of the instrument.

[0037] like Figure 1 and Figure 2 As shown, the second metering component 800 includes a second pipeline 810, a second gas mass flow meter 820, and a second solenoid valve 830. The second pipeline 810 connects the second outlet of the pressure reducing valve 300 to the test platform 600. The second gas mass flow meter 820 is mounted on the bottom of the mounting bracket 100 and is positioned on the second pipeline 810. The second solenoid valve 830 is mounted on the second gas mass flow meter 820. Specifically, the second gas mass flow meter 820 is mounted on the base 120.

[0038] When the gas being detected passes through the pressure reducing valve 300 and is output from the first metering component 700 and the second metering component 800 respectively, the gas pressure can be controlled to different pressure values ​​as needed.

[0039] like Figure 1 and Figure 3 As shown, the third metering component 900 includes a third pipeline 910, a pressure sensor 920, and a third solenoid valve 930. The pressure sensor 920 is mounted on the bottom of the mounting bracket 100 and is connected to the test platform 600 through the third pipeline 910; the third solenoid valve 930 is mounted on the pressure sensor 920. Specifically, the pressure sensor 920 is mounted on the base 120.

[0040] The settings of the first solenoid valve 730, the second solenoid valve 830, the third solenoid valve 930, and the fourth solenoid valve can respectively control the instrument's values ​​and transmit and record data.

[0041] During testing, the flat single-cell battery is placed with the electrolyte side facing down on the rubber ring 400. The gas cylinder 200 and the pressure reducing valve 300 are opened. The gas detected in the gas cylinder 200 enters the pressure reducing valve 300 through the main pipe, and then enters the first metering component 700 and the second metering component 800 respectively. The first gas mass flow meter 720 is opened, and the gas detected enters the cylinder 510 through the first pipeline 710, driving the pressure plate 530 to press down. The reading of the pressure sensor 540 is observed. The gas intake stops when the loading pressure for normal assembly of the solid oxide battery stack is reached. The second gas mass flow meter 820 is opened, and the gas detected enters the inner cavity of the test platform 600 through the second pipeline 810, and then enters the sealed cavity formed by the battery, the rubber ring 400 and the test platform 600 through the air hole 610. The reading of the pressure sensor 920 is observed. The gas intake stops when the maximum gas pressure value of the solid oxide battery in actual testing is reached. Let the test stand for a few seconds (e.g., 10 seconds) and observe the pressure sensor 920. If there is leakage in the electrolyte layer of the battery, the detection gas in the cavity will pass through the electrolyte layer to the other side of the battery, causing the detection gas to leak from the side of the battery. The reading of the pressure sensor 920 will drop. At this time, the third solenoid valve 930 sends a signal to the second gas mass flow meter 820, controlling the second gas mass flow meter 820 to continuously fill the battery with gas at a small flow rate until the pressure reaches the maximum value. The gas flow rate is controlled. When the filling and leakage rates are balanced and the pressure remains stable, the reading of the second gas mass flow meter 820 is the amount of electrolyte leakage. After the test, release the detection gas in the cavity of the test platform 600, and the pressure plate 530 rises and resets.

[0042] Using this application to test the electrolyte layer density of a single battery cell, the test time from start to finish is less than one minute, enabling rapid and large-scale testing of the electrolyte layer density of planar solid oxide batteries. This not only provides a rapid screening solution for qualified batteries in battery stack assembly, but also guides the optimization of the manufacturing process through the correlation analysis between leakage data and electrolyte microstructure, which is of great significance for promoting the industrialization of solid oxide batteries.

[0043] It should be noted that the rubber ring 400 and the pressure plate 530 in this application are replaceable to accommodate testing of flat single cells of different sizes. At the same time, by conducting zone testing (such as dividing the battery surface into multiple areas and testing each area separately), the location of defects can be accurately located by combining the differences in leakage.

[0044] Example 2

[0045] This embodiment improves upon embodiment 1, such as... Figure 4As shown, in this embodiment, the guide shaft 550 is clearance-fitted with the shaft hole, and the inner wall of the shaft hole is embedded with ball bearings 560. The ball bearings 560 abut against the guide shaft 550, so that the guide shaft 550 and the shaft hole form a rolling fit, which reduces the coefficient of friction, thereby extending the service life and reducing energy consumption.

[0046] Example 3

[0047] This embodiment adds a limiting protrusion 1000 to the basis of embodiment 1 or 2, such as Figure 5 As shown, the limiting protrusions 1000 are respectively set at the four corners of the test platform 600. Specifically, the highest point of the limiting protrusion 1000 is roughly flush with the top surface of the rubber ring 400 when it is subjected to maximum pressure.

[0048] The setting of the limit protrusion 1000 mechanically limits the end of the stroke of the pressure plate 530, avoiding overpressure due to malfunction or failure of the pressure sensor 540, thereby preventing damage to the battery due to overpressure.

[0049] Based on the above-described preferred embodiments of this utility model, and through the foregoing description, those skilled in the art can make various changes and modifications without departing from the technical concept of this utility model. The technical scope of this utility model is not limited to the contents of the specification, but must be determined according to the scope of the claims.

Claims

1. A flat plate solid oxide cell electrolyte layer densification detection apparatus comprising a mounting frame (100), characterised in that: It also includes a gas cylinder (200), a pressure reducing valve (300), a rubber ring (400), and a pressurizing assembly (500), a test platform (600), a first metering assembly (700), a second metering assembly (800), and a third metering assembly (900) mounted on a mounting bracket (100); the outlet of the gas cylinder (200) is connected to the inlet of the pressure reducing valve (300), the pressurizing assembly (500) and the test platform (600) are arranged vertically opposite each other, and the rubber ring (400) is set... On the test platform (600), the test platform (600) has a hollow structure. An air hole (610) is opened in the center of the test platform (600). The first air outlet of the pressure reducing valve (300) is connected to the cylinder (510) in the pressure increasing component (500) through the first metering component (700), and its second air outlet is connected to the test platform (600) through the second metering component (800). The third metering component (900) is connected to the test platform (600).

2. The flat-plate solid oxide battery electrolyte layer compactness testing device according to claim 1, characterized in that: The pressurization assembly (500) includes a cylinder (510), a pressurization column (520), a pressurization plate (530), and a pressure sensor (540). The cylinder (510) is mounted on the top of the mounting bracket (100) with its drive end facing downwards. The pressurization column (520) is mounted on the drive end of the cylinder (510). The top center of the pressurization plate (530) is connected to the bottom end of the pressurization column (520) through the pressure sensor (540). The pressurization plate (530) is arranged vertically opposite to the test platform (600).

3. The flat-plate solid oxide battery electrolyte layer compactness testing device according to claim 2, characterized in that: The pressurizing assembly (500) also includes a guide shaft (550), which is installed at the four corners of the pressurizing plate (530) and passes through the shaft hole opened at the top of the mounting bracket (100).

4. The flat-plate solid oxide battery electrolyte layer compactness testing device according to claim 3, characterized in that: The guide shaft (550) is in sliding fit with the shaft hole.

5. The flat-plate solid oxide battery electrolyte layer compactness testing device according to claim 3, characterized in that: The guide shaft (550) is clearance-fitted with the shaft hole, and the inner wall of the shaft hole is fitted with a ball (560), which abuts against the guide shaft (550).

6. The flat-plate solid oxide battery electrolyte layer compactness testing device according to claim 1, characterized in that: The test platform (600) has limiting protrusions (1000) at the four corners of its surface.

7. The flat-plate solid oxide battery electrolyte layer compactness testing device according to claim 1, characterized in that: The first metering component (700) includes a first pipeline (710), a first gas mass flow meter (720), and a first solenoid valve (730). The first pipeline (710) connects the first outlet of the pressure reducing valve (300) to the cylinder (510). The first gas mass flow meter (720) is mounted on the top of the mounting bracket (100) and is located on the first pipeline (710). The first solenoid valve (730) is mounted on the first gas mass flow meter (720).

8. The flat-plate solid oxide battery electrolyte layer compactness testing device according to claim 1, characterized in that: The second metering component (800) includes a second pipeline (810), a second gas mass flow meter (820), and a second solenoid valve (830). The second pipeline (810) is connected to the second outlet of the pressure reducing valve (300) and the test platform (600). The second gas mass flow meter (820) is installed at the bottom of the mounting bracket (100) and is located on the second pipeline (810). The second solenoid valve (830) is installed on the second gas mass flow meter (820).

9. The flat-plate solid oxide battery electrolyte layer compactness testing device according to claim 1, characterized in that: The third metering component (900) includes a third pipeline (910), a pressure sensor (920), and a third solenoid valve (930). The pressure sensor (920) is installed at the bottom of the mounting bracket (100) and is connected to the test platform (600) through the third pipeline (910). The third solenoid valve (930) is installed on the pressure sensor (920).

10. The flat-plate solid oxide battery electrolyte layer compactness testing device according to claim 1, characterized in that: The mounting bracket (100) includes a top cover (110), a base (120) and a support column (130). The top cover (110) and the base (120) are arranged opposite each other and connected by the support column (130).