Device for inspecting quality of steel cord electroplating coating
By designing a steel cord electroplating layer inspection device, complex stress is applied by winding steel wire samples, which solves the problem that the existing technology cannot detect the coating adhesion. This enables reliable assessment and early warning of adhesion, avoids production accidents, and improves production efficiency and product quality.
Patent Information
- Application Number
- CN202522182668.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2025-10-15
- Publication Date
- 2026-11-24
- Estimated Expiration
- 2035-10-15
Smart Images

Figure CN225018001U_ABST
Abstract
Description
Technical Field
[0001] This utility model relates to the field of steel cord production technology, and more specifically to a device for inspecting the quality of electroplated coatings on steel cords. Background Technology
[0002] Steel cord, as a reinforcing material, is widely used in automobile tires, rubber conveyor belts, and other fields. Its reliability directly affects the safety and lifespan of the final product. The production of steel cord is a complex, multi-stage process, mainly including key steps such as dry drawing, electroplating, wet drawing, and twisting.
[0003] Among these processes, the electroplating of brass is crucial. This process involves plating a layer of copper-zinc alloy (brass) onto the surface of the steel wire. This brass film acts as a solid lubricant in the subsequent wet drawing process and forms a key adhesive with the rubber after twisting. Therefore, the stability of the product quality from the electroplating process, especially the bonding strength between the plating layer and the steel wire substrate, as well as the uniformity and density of the plating layer itself, directly determines the success or failure of the subsequent wet drawing and twisting processes.
[0004] In existing technologies, quality inspection of electroplated brass wire typically relies on visual inspection or compositional analysis. Visual inspection involves operators visually examining the wire surface for obvious defects such as color differences and scratches. However, many potential defects indicating insufficient adhesion cannot be identified visually when the wire is straight. Compositional analysis uses X-ray fluorescence spectrometry (XRF) to detect the copper-zinc ratio (copper-zinc ratio) of the plating. This method effectively monitors whether the chemical composition of the plating is within the process range.
[0005] Despite the aforementioned inspection methods, a persistent and thorny problem remains in production practice: some electroplated brass wires, while showing "normal" upon completion of their current process inspection (including visual and X-ray fluorescence detection), frequently exhibit abnormalities during the high-strength drawing process in wet drawing. For example, due to poor adhesion between the plating and the substrate, the plating peels off in flakes during drawing, quickly clogging and damaging expensive drawing dies. Another example is uneven lubrication caused by the peeling plating, leading to localized overheating and oxidation of the wire surface, resulting in blackening. Severe plating peeling can even directly expose the internal wire substrate to the environment.
[0006] Therefore, there is an urgent need in this field for a method or tool that can quickly, intuitively, and effectively detect the bonding quality between the plating layer and the steel wire substrate before the wet drawing process and after the electroplating process. This would fill the gap in the existing quality control system, identify and isolate semi-finished products with potential bonding problems in advance, thereby preventing defective brass wire from flowing into subsequent processes, causing unnecessary mold wear, product quality degradation, and production interruptions, and ultimately improving overall production efficiency and product qualification rate. Summary of the Invention
[0007] To address the technical problems existing in the inspection of electroplated coatings on steel wires in the prior art, the first aspect of this utility model proposes a technical solution: an inspection device for the quality of electroplated coatings on steel cords, comprising: The supporting structure has a channel extending in a linear direction; The wire winding structure has a first end extending into the channel and a second end extending outward from the channel. A drive component is connected to the channel and to the winding structure; The driving component is configured to drive the winding structure to perform a winding action. In the winding action, the winding structure rotates about a fixed axis and simultaneously generates axial displacement along the direction of the fixed axis, so that the steel wire fixed thereon bends around itself and spirally winds around the winding structure to form a spiral winding segment q.
[0008] Preferably, the wire winding structure includes a connecting rod, the connecting rod being aligned with the axis of the channel, and the ratio of the diameter of the connecting rod to the diameter of the wire to be tested is in the range of 0.8 to 1.2.
[0009] Preferably, the wire winding structure further includes a connector at one end of the connecting rod, and the connector has a positioning hole for fixing the end of the steel wire.
[0010] Preferably, the connector is constructed as a columnar structure.
[0011] Preferably, the positioning hole extends through the connector, and the position of the connector is at a predetermined distance from the extension direction of the connecting rod.
[0012] Preferably, the winding structure further includes a connecting structure that is detachably connected to the connecting rod.
[0013] Preferably, the driving component includes a handwheel and a transmission pair that converts the rotational motion into a combined rotational and axial displacement motion of the winding structure. The handwheel is connected to the transmission pair and is used to drive the transmission pair. The connection structure includes the transmission pair.
[0014] Preferably, the transmission pair is a threaded transmission pair, which includes a threaded section disposed on the winding structure and a threaded groove disposed on the support structure and cooperating with the threaded section.
[0015] Preferably, the support structure is further provided with a guide wheel set for guiding the direction of the steel wire. The guide wheel set includes a first wheel set and a second wheel set, which are used to guide the wire's path to extend above the winding structure.
[0016] Preferably, the support structure is further provided with a wire pressing structure for pressing the starting end of the steel wire.
[0017] Compared with the prior art, the advantages of this utility model are: The testing device proposed in this application, through the setting of a winding structure, can wind a steel wire sample in a standardized manner onto a connecting rod with a diameter equivalent to its own to form a winding segment. This actively introduces intense composite stress at the interface between the coating and the substrate of the steel wire sample, successfully achieving an intuitive and reliable assessment of the coating adhesion, a key quality indicator that cannot be effectively detected by existing technologies. This method can not only accurately warn of adhesion defects before the wet drawing process, effectively avoiding quality accidents such as mold bursting and wire breakage in subsequent production, as well as high mold wear, but also fills a key gap in the existing quality control system with its simple operation, intuitive results, and high reproducibility. Attached Figure Description
[0018] The accompanying drawings are not intended to be drawn to scale. In the drawings, each identical or nearly identical component shown in the various figures may be denoted by the same reference numeral. For clarity, not every component is labeled in each figure. Embodiments of various aspects of the present invention will now be described by way of example and with reference to the accompanying drawings, wherein: Figure 1 This is a schematic diagram of the structure of the inspection device for the quality of the electroplated coating of steel cord shown in this utility model; Figure 2 This is a schematic cross-sectional view of the inspection device for the quality of electroplated coating of steel cord shown in this utility model; Figure 3 This is a schematic diagram of the wire winding structure shown in this utility model being installed on the support structure; Figure 4 This is a schematic diagram of the wire winding structure shown in this utility model; Figure 5 This is a schematic diagram of the steel wire being installed onto the winding structure as shown in this utility model; Figure 6 This is a schematic diagram of the winding segment formed by the steel wire shown in this utility model. Detailed Implementation
[0019] To better understand the technical content of this utility model, specific embodiments are provided below in conjunction with the accompanying drawings.
[0020] It should be understood that current testing methods cannot effectively and conveniently assess the bonding or adhesion between the coating and the steel wire substrate. While X-ray fluorescence spectrometers can accurately analyze the chemical composition of the coating, they cannot reflect the physical bonding strength between the coating and the substrate. Visual inspection is even less effective at detecting such microscopic bonding defects.
[0021] Based on the above, this application aims to propose an inspection device that, by pre-bending a steel wire into a spirally wound section with one end spirally wound around its own diameter, actively applies a complex and intense stress far exceeding the conventional state at the interface between the coating and the substrate by tightly spirally winding the steel wire sample around its own diameter. This forcibly accelerates and amplifies defects such as weak adhesion between the coating and the substrate. When the coating and the substrate are well bonded, the coating can withstand the stress generated by this spiral deformation without being damaged. Conversely, if the adhesion is insufficient, the coating will peel, crack, or even flake off under stress.
[0022] Therefore, the surface condition of the wound steel wire sample is a direct and visual representation of the coating adhesion quality. The testing device proposed in this application is designed to achieve this standardized and repeatable stress application process.
[0023] {Example 1} Combination Figures 1 to 3 As shown, this utility model proposes an inspection device for the quality of electroplated coatings on steel cords, including a support structure 10, a winding structure 20, and a driving component 30.
[0024] The support structure 10 is provided with a channel 101 extending in a linear direction. At the first end of the channel 101, the support structure 10 is provided with a wire pressing structure 11 and a guide wheel assembly 12.
[0025] The wire pressing structure 11 is used to fix the starting end of the steel wire, ensuring that the steel wire will not loosen as a whole during the winding process, and ensuring the tightness and consistency of the winding. The guide wheel group 12 is used to precisely guide the direction of the steel wire, ensuring that the steel wire enters the winding area at a predetermined angle and position, and preventing unnecessary scratches or deformations before winding.
[0026] In an optional embodiment, the support structure 10 is constructed as a box structure with a drawer 14 at the bottom of the box, which can be used to place the steel wire to be tested.
[0027] In an optional embodiment, the wire pressing structure 11 includes two parts: a first part 111 is installed on the support structure 10, and a second part 112 is detachably connected to the first part 111. A gap is formed between the first part 111 and the second part 112, and a rubber material is provided between the first part 111 and the second part 112 to ensure that a certain damping is formed when the steel wire passes through the gap.
[0028] Furthermore, the first end of the winding structure 20 extends into the channel 101, and the second end extends outward from the channel 101. The steel wire can be connected to the winding structure 20 via the guide wheel group 12. The drive component 30 is connected to the channel 101 and to the winding structure 20, and can be operated to rotate the drive component 30 around the axis of the channel 101.
[0029] Thus, with the support structure 10 providing a reference and guidance, the wire winding structure 20 can realize the formation of winding segments of steel wire, and the drive component 30 can provide power for the rotation of the wire winding structure, which is conducive to forming standardized winding actions, that is, the steel wire forms standardized winding segments.
[0030] The wire winding structure 20 is configured such that after the driven component 30 rotates around the axis of the channel 101, the wire winding structure 20 rotates synchronously around the axis of the channel 101 and undergoes axial displacement along the axial direction of the channel 101, so that the steel wire connected to the wire winding structure 20 is spirally wound around the outer wall of the wire winding structure 20 and forms a winding segment q.
[0031] It should be understood that when the wire winding structure 20 rotates, it not only rotates around itself, but also generates axial displacement. This ensures that each coil of steel wire can be arranged tightly and at equal intervals. This combined rotational and forward motion can wind a straight steel wire into a tight spring, and this tight spring is the winding segment q. The winding segment q generates uniform and repeatable deformation stress on the surface of the steel wire, providing standardized stress conditions for bonding force testing.
[0032] In an optional embodiment, the support structure 10 is further provided with a blocking structure 13 at the end of the channel 101. The blocking structure 13 is a blocking block, which is intended to restrict the continuous movement of the winding structure 20 toward one end of the channel 101.
[0033] In an optional embodiment, the wire winding structure 20 includes a connector 21, a connecting rod 22, and a push rod structure. The push rod structure and the connector 21 are respectively connected to the two ends of the connecting rod 22. The connecting rod 21 coincides with the axis of the channel 101, and the push rod structure is connected to the drive component 30.
[0034] In this way, the connector 21 and the push rod structure are connected together by the connecting rod 22 to form a whole. The connecting rod 21 coincides with the axis of the channel 101, and the three can rotate together around the axis of the channel 101.
[0035] Furthermore, the connector 21 is provided with a positioning hole 211 for connecting the free end of the steel cord.
[0036] Thus, when the free end of the steel cord is installed into the positioning hole 211, the connector 21 rotates around the axis of the connecting rod 22, causing the steel cord to wrap around the outer wall of the connecting rod 21.
[0037] In an optional embodiment, the connector 21 and the connecting rod 22 are detachably connected by a threaded structure. When installing the steel wire, the connector 21 can be removed, the head of the steel wire can be inserted into the positioning hole 211, and then the connector 21 and the connecting rod 22 can be installed together.
[0038] In a preferred embodiment, the diameter of the connecting rod 22 is the same as the diameter of the steel wire to be tested.
[0039] Thus, when the diameter of the connecting rod is the same as the diameter of the steel wire, it means that the steel wire is wound around a very small radius (i.e., approximately equal to its own radius), which produces near-limit bending deformation, maximizing the excitation and bonding of defects with insufficient force. In addition, the connecting rod 22 can unify the center diameter of each winding, ensuring that tests conducted by different batches and different operators are carried out under equally stringent conditions, making the results comparable.
[0040] In other embodiments, the diameter of the connecting rod 22 is slightly different from the diameter of the wire to be tested, for example, 0.8 to 1.2 times the diameter of the wire to be tested, which can result in greater or less bending stress on the coating.
[0041] In a preferred embodiment, the connector 21 is configured as a columnar structure.
[0042] Thus, the columnar structure facilitates the machining of the positioning holes 211 and provides sufficient structural strength for fixing the ends of the steel wire, preventing it from coming undone due to stress concentration in the initial stage of winding.
[0043] In an optional embodiment, the positioning hole 211 penetrates the connector 21, and the position of the connector 21 is at a predetermined distance from the extending direction of the connecting rod 22. The through hole 211 is used for inserting and securing the steel wire.
[0044] Thus, before the steel wire begins to wrap around the connecting rod 22, it first forms a small angle bend after being inserted into the positioning hole 211. This initial bend helps the steel wire to wrap around the surface of the connecting rod 22 more smoothly, ensuring that the starting section of the wrapping is stable and neat, and avoiding slippage or skipping.
[0045] In an optional embodiment, combined with Figures 2 to 4 As shown, the push rod structure includes a connecting block 23 and a screw 24. The outer wall of the screw 24 is provided with a threaded section 242. The channel 101 is provided with a threaded groove 102 that matches the threaded section 242. The first end of the screw 24 is provided with a slot 241. The connecting block 23 is detachably connected to the slot 241, so that the connecting block 23 and the screw 24 are circumferentially fixed.
[0046] The screw 24 and the threaded groove 102 in the channel 101 form a threaded drive, which is a standard screw and nut pair.
[0047] Thus, when the drive component drives the screw 24 to rotate through the connecting block 23, due to the guiding effect of the thread, the screw 24 will inevitably generate axial displacement while rotating, realizing simultaneous rotation and axial displacement. This allows the rotational input of the drive component to be converted into a composite motion of rotation and axial movement required by the winding structure 20 without delay or deviation.
[0048] In an optional embodiment, the drive component 30 includes a handwheel 31, a gear set 32, and a drive shaft 33. The drive shaft 33 is connected to the gear set 32 for transmission. The drive shaft 33 is connected to the winding structure 20 and is used to drive the winding structure 20 to rotate around the axis of the channel 101.
[0049] The handwheel 31 provides a manual operation interface to suit workshop usage habits, while the gear set 32 can change speed and transmission direction, making operation more labor-saving and optimizing the overall structural layout of the device.
[0050] In an optional embodiment, the outer wall of the support structure 10 is further provided with a support structure 25, and the support structure 25 is provided with a support groove 251 for supporting the wire winding structure 20.
[0051] Thus, the support structure 25 can support the overhanging end of the winding structure 20, especially ensuring the concentricity when the long shaft rotates, extending the service life of the device and the consistency of the winding segment q formed by the steel wire.
[0052] In an optional embodiment, the guide wheel assembly 12 includes a first wheel assembly 121 and a second wheel assembly 122, which are used to guide the wire feeding path to extend above the winding structure 20.
[0053] In this way, the first set of wheels 121 and the second set of wheels 122 form a stable wire feeding channel, ensuring that the steel wire is accurately guided before entering the winding process and that the tension is consistent, thus avoiding loose or irregular winding caused by the fluctuating position of the steel wire.
[0054] {Example 2} A method for inspecting the electroplated coating of steel cord, using the aforementioned inspection device, includes the following steps: Step S1: Pre-bend the steel wire to form a first pre-bent section o, a second pre-bent section p, and a third pre-bent section r. The extension directions of the first pre-bent section o, the second pre-bent section p, and the third pre-bent section r are perpendicular to each other. Step S2: Connect the third pre-bent section r to the winding structure 20, and connect the first pre-bent section o and the second pre-bent section p to the guide wheel group 12. Press the end of the first pre-bent section o by the wire pressing structure 11. Step S3: Rotate the drive component 30 to make the wire winding structure 20 rotate, and the steel wire is wound around the outer wall of the wire winding structure 20 to form a winding section q between the second pre-bent section p and the third pre-bent section r; Step S4: Use pliers to cut the wire off the wound section q and observe the surface of the wound section q under a microscope; In step S2, the end of the third pre-bent section r is bent to form a fixed section s, so that the steel wire and the winding structure 20 are relatively fixed. In step S3, the winding segment q is a spiral structure formed by winding a steel wire around its own diameter.
[0055] As mentioned above, this application applies a standardized stress to the coating on the surface of the steel wire by pre-bending it into a winding segment q, forcing potential bonding defects to be exposed, thus achieving the function of detecting potential quality problems. The detection device proposed in this application replaces purely manual operation, ensuring the consistency of key parameters such as the curvature, speed, and number of turns of the winding, making the test results from different times and different personnel comparable, and truly becoming a reliable quality control method. Specifically, through the surface morphology that is clearly visible to the naked eye or microscope, from intact to peeling to detachment, the judgment criteria are direct, and ordinary workers can accurately judge after simple training, greatly reducing the detection threshold.
[0056] Furthermore, by simulating the severe plastic deformation experienced by the steel wire in the subsequent wet drawing process, this method can effectively predict the performance of the steel wire during the wet drawing process and achieve early warning of serious problems such as mold bursting.
[0057] Although the present invention has been disclosed above with reference to preferred embodiments, it is not intended to limit the present invention. Those skilled in the art to which this invention pertains can make various modifications and refinements without departing from the spirit and scope of the present invention. Therefore, the scope of protection of this invention shall be determined by the claims.
Claims
1. A device for inspecting the quality of electroplated coatings on steel cord, characterized in that, include: The support structure (10) has a channel (101) extending in a linear direction. The wire winding structure (20) has a first end extending into the channel (101) and a second end extending outward from the channel (101). The drive component (30) is connected to the channel (101) and to the winding structure (20); The driving component (30) is configured to drive the winding structure (20) to perform a winding action. In the winding action, the winding structure (20) rotates around a fixed axis and simultaneously generates an axial displacement along the direction of the fixed axis, so that the steel wire fixed thereon bends around itself and spirally winds around the winding structure (20) to form a spiral winding segment (q).
2. The device for inspecting the quality of electroplated coatings on steel cords according to claim 1, characterized in that, The winding structure (20) includes a connecting rod (22), which is aligned with the axis of the channel (101), and the ratio of the diameter of the connecting rod (22) to the diameter of the steel wire to be tested is in the range of 0.8 to 1.
2.
3. The device for inspecting the quality of electroplated coatings on steel cords according to claim 2, characterized in that, The winding structure (20) also includes a connector (21) disposed at one end of the connecting rod (22), and the connector (21) is provided with a positioning hole (211) for fixing the end of the steel wire.
4. The device for inspecting the quality of electroplated coatings on steel cords according to claim 3, characterized in that, The connector (21) is constructed as a columnar structure.
5. The inspection device for the quality of electroplated coating of steel cord according to claim 3, characterized in that, The positioning hole (211) passes through the connector (21), and the position of the connector (21) is at a predetermined distance from the extension direction of the connecting rod (22).
6. The device for inspecting the quality of electroplated coatings on steel cords according to claim 3, characterized in that, The winding structure (20) also includes a connection structure that is detachably connected to the connecting rod (22).
7. The device for inspecting the quality of electroplated coatings on steel cords according to claim 6, characterized in that, The drive component (30) includes a handwheel (31) and a transmission pair that converts rotational motion into a combined rotational and axial displacement motion of the winding structure (20). The handwheel (31) is connected to the transmission pair and is used to drive the transmission pair. The connection structure includes the transmission pair.
8. The device for inspecting the quality of electroplated coatings on steel cords according to claim 7, characterized in that, The transmission pair is a threaded transmission pair, which includes a threaded section (242) disposed on the winding structure (20) and a threaded groove (102) disposed on the support structure (10) and cooperating with the threaded section (242).
9. The device for inspecting the quality of electroplated coatings on steel cords according to claim 1, characterized in that, The support structure (10) is also provided with a guide wheel group (12) for guiding the direction of the steel wire. The guide wheel group (12) includes a first wheel group (121) and a second wheel group (122). The first wheel group (121) and the second wheel group (122) are used to guide the wire to extend above the winding structure (20).