A kind of enamel scale burst instantaneous detection device based on conductive principle
By covering the surface of enamel steel samples with conductive mesh electrodes and monitoring changes in electrical signals in real time, the problems of real-time performance and accuracy in detecting enamel scale bursts were solved, providing reliable experimental data support and promoting the research and development of enamel steel.
Patent Information
- Application Number
- CN202522317294.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2025-10-31
- Publication Date
- 2026-11-24
- Estimated Expiration
- 2035-10-31
AI Technical Summary
Existing technologies cannot detect the occurrence time and process of enamel flaking in real time, accurately and quantitatively, which limits the development of high-performance anti-flaking enamel steel.
An instantaneous detection device for enamel scale bursting based on the principle of conductivity is adopted. By covering the surface of the enamel steel sample with a conductive mesh electrode, the changes in electrical signal are monitored in real time to locate the location and extent of scale bursting.
It enables real-time and accurate detection of scale bursts, provides reliable macroscopic experimental data support, and promotes microscopic research and process optimization.
Smart Images

Figure CN225018140U_ABST
Abstract
Description
Technical Field
[0001] This utility model belongs to the field of material performance testing and non-destructive testing technology, specifically relating to an instantaneous detection device for enamel scale bursts based on the principle of electrical conductivity. Background Technology
[0002] Fishscaling defects in enamel steel are caused by the accumulation and precipitation of hydrogen in the steel matrix during the enamel firing process, leading to the cracking and peeling of the enamel layer. Currently, the detection of fishscaling in industrial production and routine experiments mainly relies on macroscopic observation by the naked eye after a period of natural exposure (e.g., 24 hours). This method is highly subjective, has low precision, cannot record the exact time of fishscaling occurrence, and cannot quantify the initiation and propagation process of fishscaling.
[0003] In laboratory microscopic studies, to accurately establish the quantitative relationship between the microstructure of the steel matrix (such as the density, type, and distribution of irreversible hydrogen traps) and the susceptibility to scaling explosions, a detection method is needed that can capture the instantaneous occurrence and process of scaling explosions in real time, with precision and quantification. Existing visual observation methods cannot meet this requirement, severely restricting the research and development of high-performance anti-scaling enamel steel.
[0004] The principle of electrical conductivity has been applied in coating damage detection, but traditional methods are mostly used to monitor the integrity of coatings under static or room temperature conditions (such as pinhole detection of anti-corrosion coatings). There is no accurate quantitative detection scheme applicable to high-temperature, dynamic, and instantaneous scaling phenomena during enamel firing.
[0005] In view of the above factors, an instantaneous detection device for enamel blistering based on the principle of conductivity is provided. By using grid electrodes to locate the location of blistering within a specific grid area, it can detect the accurate time, specific location, and relative severity of enamel glaze blistering during heating in real time, providing reliable macroscopic experimental data support for laboratory microscopic research. Utility Model Content
[0006] The purpose of this invention is to provide an instantaneous detection device for enamel scale bursting based on the principle of electrical conductivity, so as to solve the problems mentioned in the background art.
[0007] The purpose of this utility model is achieved through the following technical solution: an instantaneous detection device for enamel scale bursting based on the principle of conductivity, including a sample stage, the bottom of which has an adjustable height telescopic column, and the bottom of which is fixed with a circular base.
[0008] The sample stage is provided with a conductive post, and an enamel steel sample is placed on the conductive post. The enamel steel sample includes a steel substrate and an enamel layer. The surface of the enamel layer of the enamel steel sample is covered with a conductive mesh electrode. The conductive mesh electrode is in physical contact with the enamel layer surface but is electrically insulated.
[0009] The steel substrate serves as one electrode, and the conductive mesh electrode serves as another electrode;
[0010] The steel substrate is electrically connected to the conductive mesh electrode, and an electrical signal detection unit is used to monitor the resistance, current, or voltage signals in the circuit in real time.
[0011] Furthermore, the conductive pillars are connected to the sample stage by bolts or welding.
[0012] Furthermore, an insulating layer is provided between the conductive mesh electrode and the glaze surface, and the insulating layer is a thin and flexible high-temperature resistant insulating material.
[0013] Furthermore, the conductive mesh electrode is a precision mesh structure woven from high-temperature resistant and highly conductive metal materials.
[0014] Furthermore, the mesh structure of the conductive mesh electrode adopts a honeycomb structure or a rectangular structure.
[0015] Furthermore, the high-temperature resistant and highly conductive metal material is platinum wire or nickel-chromium alloy wire, which is woven into 100 mesh using platinum wire or nickel-chromium alloy wire with a diameter of 0.05mm, that is, 100 wires per inch.
[0016] Furthermore, the insulating layer is a mica sheet or a ceramic coating, and the insulating layer is bonded to the surface of the enamel steel sample.
[0017] An implementation method for an instantaneous detection device for enamel scale bursting based on the principle of electrical conductivity includes the following steps;
[0018] The first step is to select a 50mm × 50mm enamel steel plate sample made in the laboratory.
[0019] The second step involves using platinum wire with a diameter of 0.05 mm to weave a 100-mesh mesh electrode, which is 100 wires per inch, and then flattening it over the sample surface.
[0020] The third step is to lay the enamel steel plate sample flat on the conductive column, and cover the enamel steel plate sample with the mesh electrode. The steel substrate serves as one electrode, and the conductive mesh electrode serves as another electrode, forming a loop with the external detection circuit.
[0021] The fourth step is to electrically connect the external wires of the mesh electrode to the electrical signal detection unit, and the steel substrate is electrically connected to the electrical signal detection unit through the wires.
[0022] Among them, an integrally formed smooth rod structure is formed on the end face of the conductive post to connect the high current power line, and the conductive post is used as a heating unit;
[0023] The fifth step is to connect the electrical signal detection unit to the external CP terminal, which is the computer terminal. The room temperature is heated to 300°C at a rate of 10°C / min. Data is recorded and analyzed by the computer, and the loop current value is recorded in real time. In the initial stage of heating, the current value is always zero or extremely low, which is regarded as the background noise.
[0024] Step 6: When the sample temperature reaches 215°C, the data logger captures an instantaneous current pulse with an amplitude of 5μA.
[0025] In the seventh step, during the subsequent heat preservation process, multiple pulse signals with amplitudes ranging from 2 to 10 μA were successively captured;
[0026] Step 8: After the experiment, analyze the data: the time of the first pulse occurrence, t=215°C, is the critical time for scale bursting of the sample under this heating condition. The number of pulses, such as 5, reflects the number of scale bursting points, and the amplitude of the pulses can approximately reflect the size of the crack or the amount of hydrogen evolution after calibration;
[0027] The correlation analysis between the "critical time" obtained from this macroscopic test and the microscopic parameters such as the "irreversible hydrogen trap density" measured by the hydrogen permeation experiment of the same batch of materials was conducted to evaluate the anti-scaling performance of different microstructure ratios.
[0028] Compared with the prior art, the beneficial effects of this utility model are as follows:
[0029] The device and method of this invention can detect in real time and accurately the precise time, specific location and relative severity of enamel glaze cracking during heating, providing reliable macroscopic experimental data support for laboratory microscopic research.
[0030] This invention features high precision and quantification, transforming subjective macroscopic observation into objective electrical signal measurement. It can record the occurrence time of scale bursts with millisecond accuracy and perform semi-quantitative assessment of the degree of scale bursts through signal amplitude.
[0031] This invention provides real-time and dynamic monitoring, enabling continuous monitoring throughout the entire heating process. It can not only capture the first scale burst point but also record the initiation and expansion sequence of scale bursts throughout the process, providing dynamic data.
[0032] This invention's positioning capability, through the design of a precise grid electrode, can pinpoint the location of scale eruption to a specific grid area.
[0033] This invention is strongly linked to microscopic research. The precise macroscopic data it provides (such as "hydrogen-induced cracking critical time") can be accurately correlated with the hydrogen storage capacity (hydrogen permeation curve) and precipitation phase parameters of microstructures, which greatly promotes the optimization of composition and process.
[0034] This invention has high sensitivity: even very small, barely perceptible initial microcracks can be detected, enabling the detection of the "budding" state of scale bursts. Attached Figure Description
[0035] Figure 1 This is a three-dimensional schematic diagram of the present invention;
[0036] Figure 2 This is a schematic diagram of the connection between this utility model and the CP end;
[0037] Figure 3 This is a utility model Figure 1 A cross-sectional schematic diagram;
[0038] Figure 4 This is a partially enlarged schematic diagram of a enamel steel sample placed on a conductive column of this utility model.
[0039] Figure 5 This is a schematic diagram of the structure of the first conductive mesh electrode of this utility model;
[0040] Figure 6 This is a schematic diagram of the structure of the second type of conductive mesh electrode of this utility model;
[0041] Figure 7 This is a schematic diagram of the first conductive mesh electrode covered enamel steel sample of this utility model;
[0042] Figure 8 This is a schematic diagram of the second type of conductive mesh electrode covering an enamel steel sample according to this utility model. Detailed Implementation
[0043] The technical solutions of the present utility model will be clearly and completely described below with reference to the accompanying drawings of the embodiments of the present utility model. Obviously, the described embodiments are only some embodiments of the present utility model, and not all embodiments. All other embodiments obtained by those skilled in the art based on the embodiments of the present utility model without creative effort are within the protection scope of the present utility model.
[0044] In the description of this utility model, it should be noted that, unless otherwise explicitly specified and limited, the terms "installation," "connection," and "joining" should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral connection; they can refer to a direct connection or an indirect connection through an intermediate medium. Those skilled in the art can understand the specific meaning of the above terms in this utility model based on the specific circumstances.
[0045] In the description of this utility model, it should be understood that the terms "upper", "lower", "front", "rear", "left", "right", "vertical", "horizontal", "top", "bottom", "inner", "outer", etc., indicate the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings. They are only for the convenience of describing this utility model and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation. Therefore, they should not be construed as limitations on this utility model.
[0046] like Figure 1-8 As shown, an instantaneous detection device for enamel scale bursting based on the principle of conductivity includes a sample stage 1, the bottom of which has an adjustable height telescopic column 2, and the bottom of the adjustable height telescopic column 2 is fixed with a circular base.
[0047] The adjustable height telescopic column 2 at the bottom of the above-mentioned sample stage can be extended and retracted to adjust the fixed height. The adjustable height telescopic column 2 is fixed to the bottom of the sample stage by means of threaded detachment or welding. A circular base is fixed to the bottom of the adjustable height telescopic column 2 (fixed by positioning holes / screws). When fixing the sample stage, the circular base on the adjustable height telescopic column 2 is inserted into the positioning hole (not shown in the figure) on the corresponding working base.
[0048] The sample stage 1 is provided with a conductive post 3, and an enamel steel sample 4 is placed on the conductive post 3. The enamel steel sample 4 includes a steel substrate 4a and an enamel layer 4b. A conductive mesh electrode 5 is covered on the surface of the enamel layer 4b of the enamel steel sample 4. The conductive mesh electrode 5 is in physical contact with the surface of the enamel layer 4b but is electrically insulated.
[0049] The steel substrate 4a serves as one electrode, and the conductive mesh electrode 5 serves as another electrode;
[0050] The steel substrate 4a (which is connected to the electrical signal detection unit via a conductive post) is electrically connected to the conductive mesh electrode 5. The electrical signal detection unit 6 is used to monitor the resistance, current, or voltage signals in the circuit in real time. The electrical signal detection unit 6 is set on the column at the rear end of the sample stage 1. The electrical signal detection unit is placed on a platform that is fixedly welded on the column.
[0051] The electrical signal detection unit uses a Keithley 2450 series digital source meter. The electrical signal detection unit is connected to an external CP terminal via a connecting cable. The CP terminal is a computer terminal, which contains a source meter programmable system that matches the Keithley 2450 digital source meter.
[0052] In order to facilitate the use of conductive columns as heating units to provide the required heating temperature for the sample during use, conductive columns 3 are connected to the sample stage 1 by bolts or welding.
[0053] To facilitate use and ensure electrical insulation between the two in the initial state, and to prevent the electrode and enamel layer from reacting at high temperatures, an insulating layer 7 is provided between the conductive mesh electrode 5 and the surface of the enamel layer 4b. The insulating layer 7 is a thin and soft high-temperature resistant insulating material, which may be a mica sheet or a ceramic coating. The insulating layer 7 is bonded to the surface of the enamel steel sample 4.
[0054] To facilitate the determination of the location of scale eruption during use and to provide reliable macroscopic experimental data support for laboratory microscopic research, the conductive mesh electrode is a precision mesh structure woven from high-temperature resistant and highly conductive metal materials. The mesh structure of the conductive mesh electrode adopts a honeycomb structure or a rectangular structure.
[0055] When the glaze layer develops microcracks or warps due to internal hydrogen pressure, the insulation performance of the aforementioned conductive mesh electrode is compromised. The steel substrate will then make instantaneous physical contact with the mesh electrode on the surface through the crack, causing a sharp drop in the circuit resistance between the two electrodes and generating a transient current or voltage pulse signal.
[0056] To improve the durability of the conductive mesh electrode during use, the high-temperature resistant and highly conductive metal material is platinum wire or nickel-chromium alloy wire, which is woven into 100 meshes using platinum wire or nickel-chromium alloy wire with a diameter of 0.05mm, i.e., 100 wires per inch.
[0057] The conductive mesh electrode has external wires fixedly connected to its four corners. The external wires are electrically connected to the electrical signal detection unit, and the steel substrate is also connected to the electrical signal detection unit through external wires.
[0058] An implementation method for an instantaneous detection device for enamel scale bursting based on the principle of electrical conductivity includes the following steps;
[0059] The first step is to select a 50mm × 50mm enamel steel plate sample made in the laboratory.
[0060] The second step involves using platinum wire with a diameter of 0.05 mm to weave a 100-mesh mesh electrode, which is 100 wires per inch, and then flattening it over the sample surface.
[0061] The third step is to lay the enamel steel plate sample flat on the conductive column, and cover the enamel steel plate sample with the mesh electrode. The steel substrate serves as one electrode, and the conductive mesh electrode serves as another electrode, forming a loop with the external detection circuit.
[0062] The fourth step is to electrically connect the external wires of the mesh electrode to the electrical signal detection unit, and the steel substrate is electrically connected to the electrical signal detection unit through the wires.
[0063] Among them, an integrally formed smooth rod structure is formed on the end face of the conductive post to connect the high current power line, and the conductive post is used as a heating unit;
[0064] The fifth step is to connect the electrical signal detection unit to the external CP terminal, which is the computer terminal. The enamel steel plate sample is heated to 300°C at a rate of 10°C / min at room temperature. Data is recorded and analyzed through the computer terminal. The loop current value is recorded in real time. In the initial stage of heating, the current value is always zero or extremely low, which is regarded as the background noise.
[0065] Step 6: When the sample temperature reaches 215°C, the data logger captures an instantaneous current pulse with an amplitude of 5μA.
[0066] In the seventh step, during the subsequent heat preservation process, multiple pulse signals with amplitudes ranging from 2 to 10 μA were successively captured;
[0067] Step 8: After the experiment, analyze the data: the time of the first pulse occurrence, t=215°C, is the critical time for scale bursting of the sample under this heating condition. The number of pulses, such as 5, reflects the number of scale bursting points, and the amplitude of the pulses can approximately reflect the size of the crack or the amount of hydrogen evolution after calibration;
[0068] The correlation analysis between the "critical time" obtained from this macroscopic test and the microscopic parameters such as the "irreversible hydrogen trap density" measured by the hydrogen permeation experiment of the same batch of materials was conducted to evaluate the anti-scaling performance of different microstructure ratios.
[0069] An application method for an instantaneous detection device for enamel glaze bursting based on the principle of electrical conductivity is described. This method is applied to a laboratory environment to detect the instantaneous time, location, and extent of enamel glaze bursting (peeling) during the heating process.
[0070] Sample preparation and circuit construction: A conductive mesh electrode is covered on the glaze surface of the enamel sample. The mesh electrode is in physical contact with the glaze surface but electrically insulated. The steel substrate is used as one electrode, and the conductive mesh electrode is used as another electrode, forming a loop with the external detection circuit.
[0071] Insulation status monitoring: In the initial state, due to the insulation characteristics of the glaze layer, the circuit between the steel substrate and the conductive mesh electrode presents a high resistance or no current flow.
[0072] Heating and Real-time Monitoring: The sample is heated in a programmed manner to simulate the enamel firing process or hydrogen evolution process, and the changes in electrical signal parameters between the two electrodes are monitored in real time through a detection circuit;
[0073] Instantaneous judgment of scale burst: When the glaze layer produces microcracks or peels due to scale burst caused by internal hydrogen pressure, its insulation performance is destroyed. The steel substrate will make instantaneous physical contact with the mesh electrode on the surface through the crack, causing the circuit resistance between the two electrodes to drop sharply, generating a transient current or voltage pulse signal.
[0074] Signal Acquisition and Analysis: Electrical signal pulses are acquired and recorded via a computer-based source meter control system that matches the Keithley 2450 digital source meter for electrical signal detection. The exact time of the scale burst is determined based on the timing of the pulse signal occurrence. The intensity or number of pulse signals is used to assess the severity of the scale burst or the number of burst points. The location of the scale burst can be determined based on the grid positioning information of the mesh electrodes.
[0075] It will be apparent to those skilled in the art that this invention is not limited to the details of the exemplary embodiments described above, and that it can be implemented in other specific forms without departing from the spirit or essential characteristics of this invention. Therefore, the embodiments should be considered illustrative and non-limiting in all respects, and the scope of this invention is defined by the appended claims rather than the foregoing description. Thus, it is intended that all variations falling within the meaning and scope of equivalents of the claims be included within this invention. No reference numerals in the claims should be construed as limiting the scope of the claims.
[0076] Furthermore, it should be understood that although this specification describes embodiments, not every embodiment contains only one independent technical solution. This narrative style is merely for clarity. Those skilled in the art should consider the specification as a whole, and the technical solutions in each embodiment can also be appropriately combined to form other embodiments that can be understood by those skilled in the art.
Claims
1. A device for instantaneous detection of enamel scale bursting based on the principle of electrical conductivity, characterized in that: Includes a sample stage (1), the bottom of which has an adjustable height telescopic column (2), and the bottom of the adjustable height telescopic column (2) is fixed with a circular base. The sample stage (1) is provided with a conductive column (3), and an enamel steel sample (4) is placed on the conductive column (3). The enamel steel sample (4) includes a steel substrate (4a) and an enamel layer (4b). A conductive mesh electrode (5) is covered on the surface of the enamel layer (4b) of the enamel steel sample (4). The conductive mesh electrode (5) is in physical contact with the surface of the enamel layer (4b) but is electrically insulated. The steel substrate (4a) serves as one electrode, and the conductive mesh electrode (5) serves as another electrode; The steel substrate (4a) and the conductive mesh electrode (5) are electrically connected to an electrical signal detection unit (6) for real-time monitoring of resistance, current or voltage signals in the circuit.
2. The instantaneous detection device for enamel scale bursting based on the principle of electrical conductivity according to claim 1, characterized in that: The test stage (1) is connected to a conductive column (3) by bolts or welding.
3. The instantaneous detection device for enamel scale bursting based on the principle of electrical conductivity according to claim 2, characterized in that: An insulating layer (7) is provided between the conductive mesh electrode (5) and the surface of the glaze layer (4b). The insulating layer (7) is a thin and soft high-temperature resistant insulating material.
4. The instantaneous detection device for enamel scale bursting based on the principle of electrical conductivity according to claim 3, characterized in that: The conductive mesh electrode (5) is a precision mesh structure woven from high-temperature resistant and highly conductive metal materials.
5. The instantaneous detection device for enamel scale bursting based on the principle of electrical conductivity according to claim 4, characterized in that: The conductive mesh electrode (5) has a honeycomb structure or a rectangular structure.
6. The instantaneous detection device for enamel scale bursting based on the principle of electrical conductivity according to claim 5, characterized in that: The high-temperature resistant and highly conductive metal material is platinum wire or nickel-chromium alloy wire, which is woven into 100 meshes using platinum wire or nickel-chromium alloy wire with a diameter of 0.05mm, that is, 100 wires per inch.
7. The instantaneous detection device for enamel scale bursting based on the principle of electrical conductivity according to claim 5, characterized in that: The insulating layer (7) is a mica sheet or a ceramic coating, and the insulating layer (7) is bonded to the surface of the enamel steel sample (4).