Anti-aging glass microsphere reflective film
By introducing a composite structure of nano-tin oxide infrared reflective layer and modified benzotriazole ultraviolet blocking layer into the reflective film, combined with a wear-resistant surface layer of polycarbonate modified material, the problem of reflective film aging due to ultraviolet and infrared radiation is solved, product life is extended and wear-resistant and anti-slip performance is enhanced.
Patent Information
- Application Number
- CN202522757362.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2025-12-26
- Publication Date
- 2026-11-24
- Estimated Expiration
- 2035-12-26
AI Technical Summary
Existing reflective films are susceptible to ultraviolet and infrared radiation after long-term outdoor use, leading to accelerated aging, performance degradation, and shortened service life.
A heat-absorbing protective layer with a composite structure of nano-tin oxide infrared reflective layer and modified benzotriazole ultraviolet blocking layer, combined with a wear-resistant surface layer of polycarbonate modified material and micron-level anti-slip texture, forms a multi-layer protection mechanism.
It effectively prevents the accumulation of infrared heat and ultraviolet corrosion, extends the outdoor service life of the reflective film, and improves its wear resistance and anti-slip effect.
Smart Images

Figure CN225018474U_ABST
Abstract
Description
TECHNICAL FIELD
[0001] The utility model relates to the field of reflective film, especially in kind a kind of anti -aging glass bead reflective film. BACKGROUND
[0002] As the core retroreflective functional material commonly used in the field, the reflective film has irreplaceable application value in the field of traffic safety and outdoor protection, and is widely used in traffic duty reflective equipment, road sign facilities, construction safety protection appliances, outdoor warning devices and other scenes. Its high-efficiency retroreflective optical properties can effectively improve the visual recognition of users and signs in low-visibility environments such as night, rain and snow, and it is a key material to ensure public travel safety and outdoor work safety.
[0003] After long-term outdoor use, the existing reflective film is easily eroded by various complex environmental factors, and its performance has obvious short board: on the one hand, the ultraviolet radiation in sunlight can accelerate the degradation and aging of the high molecular matrix material in the reflective film, not only causing the appearance deterioration phenomenon such as embrittlement and yellowing of the film body, but also damaging the structural integrity of the reflective coating, and further causing the rapid attenuation of its retroreflective performance; on the other hand, the continuous irradiation of infrared rays will cause heat accumulation in the film body, which will further accelerate the aging rate of each functional layer and ultimately shorten the service life of the product. SUMMARY
[0004] The utility model provides a kind of anti-aging glass bead reflective film to overcome the problem of easy aging of the above reflective film.
[0005] The utility model adopts the following technical solutions: A kind of anti-aging glass bead reflective film, including abrasion-resistant surface layer, heat absorption protective layer, support layer, reflective layer and base layer compounded in sequence, the reflective layer is equipped with multiple glass beads, the lower hemisphere of the glass bead is plated with metal reflective coating, the above-mentioned heat absorption protective layer is compounded by infrared reflective layer and ultraviolet barrier layer, the above-mentioned infrared reflective layer is nano tin oxide coating, and the above-mentioned ultraviolet barrier layer is modified benzotriazole composite coating.
[0006] Further, the thickness of the above-mentioned infrared reflective layer and the above-mentioned ultraviolet barrier layer is 3-8 μm, preferably the thickness of the ultraviolet barrier layer is 5 μm, and the thickness of the infrared reflective layer is 6 μm.
[0007] Further, the abrasion-resistant surface layer is a film made of polycarbonate modified material, and the surface of the abrasion-resistant surface layer is provided with micron-level anti-slip texture.
[0008] Further, the above-mentioned metal reflective coating is an aluminum plating layer or a silver plating layer, preferably the metal reflective coating is a silver plating layer.
[0009] Further, the base layer is composed of a bonding layer and a release paper, and the bonding layer is bonded to the reflective layer on the side away from the release paper.
[0010] From the above description of the structure of the utility model, compared with the prior art, the utility model has the following advantages: 1. The heat-absorbing protective layer of the glass bead reflective film of the utility model is configured with a composite structure of a nano-tin oxide infrared reflective layer and a modified benzotriazole ultraviolet barrier layer, which can achieve precise protection against outdoor core aging factors. The nano-tin oxide coating has excellent infrared reflective performance, which can reduce the penetration of infrared rays and block the accumulation of heat, avoiding the accelerated aging problem caused by high temperature inside the film body. The modified benzotriazole composite coating has high ultraviolet barrier efficiency, which can isolate the erosion of ultraviolet rays on the high molecular substrate and reflective plating layer. The two form a synergistic protection mechanism to delay the deterioration process of the film body from the aging factor level and significantly improve the outdoor service life of the product.
[0011] 2. The wear-resistant surface layer of the utility model is made of a polycarbonate modified substrate, which has high strength and high wear resistance, and can effectively resist external damage such as friction and scratching in outdoor environments. At the same time, the surface layer is additionally provided with a micron-level anti-slip texture structure, which not only further enhances its wear resistance but also improves the anti-slip effect during use. This design is particularly suitable for application scenarios that frequently contact or are in harsh outdoor environments, ensuring the long-term stability of the appearance and core performance of the film body. BRIEF DESCRIPTION OF DRAWINGS
[0012] Figure 1 The figure is a structural schematic diagram of the glass bead reflective film of the utility model. DETAILED DESCRIPTION
[0013] The specific implementation manner of the utility model will be described below with reference to the drawings.
[0014] Referring to Figure 1 An anti-aging glass bead 10 reflective film includes a wear-resistant surface layer 6, a heat-absorbing protective layer 3, a support layer 2, a reflective layer 1, and a base layer, which are sequentially compounded. The reflective layer 1 is provided with a plurality of glass beads 10, the lower half of the glass bead 10 is plated with a metal reflective plating layer 11, the heat-absorbing protective layer 3 is formed by compounding an infrared reflective layer 31 and an ultraviolet barrier layer 32, the infrared reflective layer 31 is a nano-tin oxide coating, and the ultraviolet barrier layer 32 is a modified benzotriazole composite coating.
[0015] The thickness of the infrared reflective layer 31 and the ultraviolet barrier layer 32 is 3-8 μm, preferably the thickness of the ultraviolet barrier layer 32 is 5 μm, and the thickness of the infrared reflective layer 31 is 6 μm.
[0016] The aforementioned wear-resistant surface layer 6 is a thin film made of polycarbonate modified material, and the surface of the wear-resistant surface layer 6 is provided with micron-level anti-slip texture.
[0017] The aforementioned metallic reflective coating 11 is an aluminum plating layer or a silver plating layer, preferably a silver plating layer.
[0018] The aforementioned base layer is composed of an adhesive layer 4 and a release paper 5, with the reflective layer 1 bonded to the side of the adhesive layer 4 facing away from the release paper 5.
[0019] The above are merely specific embodiments of this utility model, but the design concept of this utility model is not limited thereto. Any non-substantial modifications made to this utility model using this concept shall be considered as an infringement of the protection scope of this utility model.
Claims
1. An anti-aging glass microsphere reflective film, comprising a wear-resistant surface layer, a heat-absorbing protective layer, a support layer, a reflective layer, and a base layer sequentially laminated together, wherein the reflective layer contains a plurality of glass microspheres, the lower hemisphere of which is coated with a metallic reflective coating, characterized in that: The heat-absorbing protective layer is formed by combining an infrared reflective layer and an ultraviolet blocking layer. The infrared reflective layer is a nano-tin oxide coating, and the ultraviolet blocking layer is a modified benzotriazole composite coating.
2. The anti-aging glass microsphere reflective film as described in claim 1, characterized in that: The thickness of both the infrared reflective layer and the ultraviolet blocking layer is 3-8 μm.
3. The anti-aging glass microsphere reflective film as described in claim 1, characterized in that: The wear-resistant surface layer is a thin film made of polycarbonate modified material, and the surface of the wear-resistant surface layer has micron-level anti-slip texture.
4. The anti-aging glass microsphere reflective film as described in claim 1, characterized in that: The reflective metallic coating is either an aluminum plating layer or a silver plating layer.
5. The anti-aging glass microsphere reflective film as described in claim 1, characterized in that: The base layer is composed of an adhesive layer and a release paper, with the reflective layer bonded to the adhesive layer on the side facing away from the release paper.