A dual-sided handwriting pad with auxiliary line patterns

By adopting a flexible substrate layer and a magnetic adsorption base layer design on the handwriting tablet, the problems of high processing difficulty of pattern layer and single-sided writing are solved, realizing double-sided writing and magnetic adsorption functions, improving the production efficiency and space utilization of the handwriting tablet, and adapting to the needs of diverse scenarios.

CN225018729UActive Publication Date: 2026-11-24DONGGUAN BAOLICHUANG OPTOELECTRONICS CO LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202522648143.X
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2025-12-15
Publication Date
2026-11-24
Estimated Expiration
2035-12-15

AI Technical Summary

Technical Problem

The existing handwriting tablet pattern layer is difficult to process and cannot be used on both sides, resulting in low space utilization. It is especially unable to meet the needs of simultaneous display of multiple contents in small scenarios.

Method used

The pattern is set on a flexible substrate layer, which is bonded to the writing film and back panel through an adhesive layer. The pattern is printed on the flexible substrate layer, and the back panel is bonded to the magnetic adsorption base layer to realize the double-sided writing function. The magnetic adsorption base layer and the magnetic adsorption back panel enhance convenience.

Benefits of technology

It reduces production costs and error losses, improves product yield, expands application scenarios, enhances space utilization, ensures smooth writing and abrasion resistance, and adapts to diverse scenario needs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN225018729U_ABST
    Figure CN225018729U_ABST
Patent Text Reader

Abstract

This utility model provides a double-sided writing tablet with auxiliary line patterns, relating to the field of liquid crystal writing tablet technology. A double-sided writing tablet with auxiliary line patterns includes a writing film, a back plate, and a pattern, and also includes a flexible substrate layer. The pattern is disposed on the flexible substrate layer, which is positioned between the writing film and the back plate. The flexible substrate layer is bonded to the writing film via a first adhesive layer and to the back plate via a second adhesive layer. The writing film is a transparent liquid crystal writing film. This utility model aims to solve the technical problems of existing writing tablets not being able to be used on both sides and the difficulty in processing the pattern layer printed on a rigid substrate, enabling simpler implementation of auxiliary patterns on the writing tablet.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This utility model relates to the field of liquid crystal writing tablet technology, and in particular to a double-sided writing tablet with auxiliary line patterns. Background Technology

[0002] Handwriting tablets are commonly used auxiliary tools in teaching, office work, and sports training. Their reusable writing and easy-to-clean features make them widely applicable for explaining knowledge points, tactical simulations, and temporary note-taking. However, traditional handwriting tablets suffer from the following technical drawbacks: Firstly, the writing surface is often printed on a rigid substrate. The printing, cutting, and edge processing of rigid substrates require higher precision, leading to issues such as printing misalignment and edge damage. This results in a lower yield rate compared to flexible substrates and higher printing costs. Secondly, most handwriting tablets only have writing functionality on one side, with the other side being non-functional. This results in low space utilization, especially in small classrooms and training grounds with limited space, making it difficult to meet the need for simultaneous display of multiple contents.

[0003] Furthermore, existing writing tablets with double-sided writing capabilities mostly use the same material and structure for both writing surfaces, without differentiated design for different usage needs.

[0004] For example, patent document CN202020142851.0, entitled "A Liquid Crystal Writing Film, Writing Board and Blackboard with Auxiliary Lines", discloses a liquid crystal writing film, writing board and blackboard with auxiliary lines, including: a first conductive layer, a liquid crystal layer and a second conductive layer; a plurality of closed regions are etched on one of the conductive layers, the closed regions are spliced ​​to form auxiliary lines, and the auxiliary lines are combined to form a predetermined pattern; or, a plurality of closed regions are etched on the first conductive layer and the second conductive layer respectively, the closed regions are spliced ​​to form auxiliary lines; the auxiliary lines on the first conductive layer and the second conductive layer together constitute a predetermined pattern; a predetermined distance is spaced between two adjacent closed regions.

[0005] The patterns in the aforementioned patent documents are set on the conductive layer or substrate of the writing film. When set on the conductive layer of the writing film, the pattern cannot be displayed if the conductive layer fails to conduct. Moreover, the process of etching auxiliary lines on the conductive layer to form patterns is complex and costly. When set on the substrate, ink screen printing, inkjet printing, laser printing, or laser etching are used. Since the substrate is made of rigid plastic, there are two disadvantages when printing patterns: 1. The substrate surface is porous and has a granular texture, which is uneven and affects the smoothness of writing; 2. The substrate is a rigid board. Printing on small-sized boards is relatively easy, but printing on large-sized boards is very difficult. First, it requires customized large-scale printing equipment. Second, the printed products of large-sized boards need to undergo post-processing such as lamination, die-cutting, bending, and assembly. Lamination is prone to bubbles and delamination (caused by poor board flatness), and die-cutting is prone to dimensional deviations (caused by board expansion and contraction).

[0006] Therefore, this utility model will describe a technical solution for more easily implementing auxiliary patterns on a handwriting tablet. Utility Model Content

[0007] Therefore, it is necessary to provide a double-sided handwriting tablet with auxiliary line patterns to address the existing technical problems, in order to solve the problems of high processing difficulty of pattern layers and the inability of handwriting tablets to be used on both sides.

[0008] To solve the problems of the existing technology, the present invention adopts the following technical solution:

[0009] A double-sided writing tablet with auxiliary line patterns includes a writing film, a back plate, and a pattern, and also includes a flexible substrate layer. The pattern is disposed on the flexible substrate layer, and the flexible substrate layer is disposed between the writing film and the back plate. The flexible substrate layer is bonded to the writing film through a first adhesive layer, and the flexible substrate layer is bonded to the back plate through a second adhesive layer. The writing film is a transparent liquid crystal writing film.

[0010] Furthermore, the flexible substrate layer is made of flexible materials, including but not limited to paper, PET plastic, non-woven fabric or soft PVC sheet.

[0011] Furthermore, the flexible substrate layer is printed with a pattern, and the printing process is one of inkjet printing, laser printing, screen printing and UV printing, which can print different patterns as required.

[0012] Furthermore, the pattern is an independent pattern layer, attached to the flexible substrate layer.

[0013] Furthermore, the first and second adhesive layers are double-sided adhesives, and the thickness of the adhesive layers is 10-70 μm.

[0014] Furthermore: the first adhesive layer and the second adhesive layer are formed by brushing or spraying adhesive, and the thickness of the adhesive layer is 10-70μm.

[0015] Furthermore: a magnetically conductive adsorption base layer A is provided between the back plate and the second adhesive layer, and the magnetically conductive adsorption base layer A is adhesively bonded to the back plate.

[0016] Furthermore, the outer surface of the backplate, i.e. the side away from the writing membrane, is a writable whiteboard surface.

[0017] Furthermore, the side of the back plate away from the writing film is provided with a magnetic adsorption base layer B, which is adhesively bonded to the back plate. The outer surface layer of the magnetic adsorption base layer B is coated, film-coated or physically modified to form a writing layer with low friction coefficient, high hardness, anti-adhesion and easy cleaning on the substrate surface.

[0018] Furthermore, both the magnetic adsorption base layer A and the magnetic adsorption base layer B are magnetically conductive materials, including but not limited to sheet metal and galvanized steel sheets.

[0019] The beneficial effects of this utility model are as follows:

[0020] This invention prints patterns onto a flexible substrate layer. Compared to traditional printing on rigid substrates, this method offers a more mature production process, effectively reducing manufacturing costs while improving product yield and minimizing errors and losses during production. It also boasts superior adaptability for industrial production. The flexible substrate layer allows for flexible customization of patterns to suit diverse scenarios such as teaching, sports training, and office work, meeting users' personalized needs and expanding the application range of the writing tablet. Secondly, the writing tablet is double-sided, with the writing film and the back writing layer forming two independent writing surfaces, allowing for simultaneous display of different content and significantly improving space utilization, especially suitable for small classrooms, training grounds, and other spaces with limited space. The LC film layer has high light transmittance and excellent surface hardness, clearly displaying the content of the underlying pattern layer while ensuring smooth writing and abrasion resistance. The metallic paint layer is a white matte material with low reflectivity and good long-distance visibility, suitable for repeated writing and erasing with whiteboard markers without leaving any residue. Finally, the writing tablet has magnetic attraction on both sides, enhancing ease of use. Attached Figure Description

[0021] Figure 1 This is a schematic diagram of the front structure of this utility model;

[0022] Figure 2 This is a structural diagram of the back of the present invention;

[0023] Figure 3 This is a cross-sectional view of the present invention;

[0024] Figure 4This is a schematic diagram of a football field as the design of this utility model;

[0025] Figure 5 This is a schematic diagram of the writing grid pattern of this utility model.

[0026] The meanings of the markings in the diagram are as follows: 1. Handwriting tablet; 2. Stylus; 3. Clear button; 4. Marker; 101. Handwriting film; 102. First adhesive layer; 103. Flexible substrate layer; 104. Second adhesive layer; 105. Magnetic adsorption base layer A; 108. Back panel; 106. Magnetic adsorption base layer B; 107. Writing layer. Detailed Implementation

[0027] To further understand the features, technical means, and specific objectives and functions achieved by this utility model, the following detailed description of this utility model is provided in conjunction with the accompanying drawings and specific embodiments.

[0028] Please see Figures 1 to 5 As shown, this utility model discloses a double-sided handwriting board 1 with auxiliary line patterns. The layer structure of the handwriting board from the front to the back is as follows: handwriting film 101, first adhesive layer 102, flexible substrate layer 103, second adhesive layer 104, magnetic adsorption base layer A105, back plate 108, and whiteboard surface.

[0029] The handwriting film 101 is an LC film, specifically a transparent liquid crystal handwriting film. The liquid crystal molecules in this film can change their arrangement under external pressure (such as from a stylus or finger pressing), creating localized optical scattering / refraction differences. This allows for a direct presentation of handwriting and accurately captures details such as writing pressure and pen stroke angle, achieving a damping feel and variations in pen thickness similar to paper writing, thus meeting the core requirements of handwriting input. Furthermore, it is compatible with the overlay display scenario described in this case, without obstructing the pattern on the underlying flexible substrate layer, ensuring clear display of the pattern content.

[0030] The handwriting film 101 is bonded to the flexible substrate layer 103 through the first adhesive layer 102. The LC film is made of a flexible polymer substrate, and its flexibility is compatible with the deformation characteristics of the flexible substrate layer (paper, non-woven fabric, PET plastic, etc.). This can avoid warping and adhesive layer peeling caused by excessive hardness difference between the interlayer materials. At the same time, the LC film has a high surface flatness, which can ensure the uniformity of adhesive layer bonding and prevent assembly defects such as bubbles and incomplete bonding.

[0031] Furthermore, by simplifying the production process of the pattern layer and reducing production costs, this invention replaces the previous printing on rigid substrates and conductive layers with a flexible substrate layer 103 as the pattern layer. The flexible substrate layer is adhered to the inside of the LC film by a first adhesive layer. The flexible substrate layer includes, but is not limited to, paper, non-woven fabric, PET plastic, and soft PVC. The pattern required by the user is printed on the flexible substrate layer to form the pattern layer. From the perspective of raw material costs, paper, non-woven fabric, and soft PVC are all basic materials for mass production, and their costs are far lower than those of rigid substrates. From the perspective of processing costs, the flexible substrate layer does not require complex secondary processing such as cutting and polishing after printing, and the energy consumption during processing is low. In addition, they can easily meet small-batch customization needs, such as printing knowledge point patterns in teaching scenarios and printing table patterns in office scenarios. These materials can quickly switch printing templates without the need to readjust high-precision processing equipment like rigid substrates, reducing the additional costs of customized production.

[0032] Meanwhile, the flexible material can adapt to the surface flatness of the adhesive layer and adjacent layers. During lamination, air between layers can be expelled by rolling with pressure rollers, avoiding the air pockets and edge lifting problems that are prone to occur with rigid materials. This ensures a tight bond between the pattern layer and the writing film and the magnetic adsorption base layer, allowing the pattern details to be clearly visible from the LC film side, such as the lines of a football field tactical diagram and the borders of a grid (e.g., Figure 4 , Figure 5 (As shown). Furthermore, the flexible material has slight elasticity, which can cushion the pressure of the stylus during writing, preventing the pressure from being directly transmitted to the magnetic adsorption base layer and causing deformation of the board surface. At the same time, it reduces wear on the hardened coating of the writing film and extends the overall lifespan of the writing tablet. For the previous hard base layer, there was no such cushioning effect. Long-term pressing can easily lead to aging of the underlying adhesive layer and local damage to the LC film, affecting the writing effect.

[0033] Meanwhile, different flexible materials are suitable for different usage environments. Paper is non-reflective and does not easily leave fingerprints, which can avoid the glare problem when viewing patterns under strong light, making it suitable for use in bright environments such as teaching and office. PET plastic and non-woven fabric have good toughness, tear resistance and wear resistance, and are not easily damaged by slight impacts, making them suitable for outdoor use.

[0034] Furthermore, to enable the stylus 2 to be magnetically attracted to one side of the LC film, a magnetically conductive adsorption base layer A105 is provided on the side of the flexible substrate layer away from the writing film. The magnetically conductive adsorption base layer A105 is bonded to the flexible substrate layer 103 through a second adhesive layer 104. The magnetically conductive adsorption base layer A105 is made of a magnetically conductive material, including but not limited to sheet metal and galvanized steel. This material ensures a stable magnetic attraction effect and avoids oxidation and rust affecting the overall structure of the writing tablet during long-term use. It is also easy to process and suitable for the mass production needs of writing tablets.

[0035] Meanwhile, the LC film is a non-metallic flexible substrate layer that does not shield the magnetic properties of the magnetic adsorption base layer. Users can attach magnets, magnetic nails, and styluses to one side of the LC film.

[0036] Furthermore, in order to enhance the adhesion of the adhesive layer, the side of the magnetically conductive adsorption base layer A105 that contacts the second adhesive layer 104 needs to be sandblasted to control the surface roughness Ra=0.8-1.6μm. This roughness will cause the metal surface to form a uniform micro-uneven structure. When the adhesive layer is cured, it will penetrate into these micro-gaps, increase the actual contact area, and significantly enhance the adhesion of the adhesive layer.

[0037] Furthermore, to achieve the double-sided handwriting function, a back plate 108 is adhesively attached to the side of the magnetic adsorption base layer A away from the writing film. The back plate 108, as a rigid substrate, provides mechanical strength and morphological stability to the overall structure, preventing bending, deformation, and interlayer delamination of the multi-layer structure due to its own weight or external pressure. Simultaneously, the rigidity of the back plate allows for more even pressure distribution on the writing film side, improving the clarity and consistency of the LC film's display, while also preventing damage to the interlayer structure due to excessive pressure, thus extending the service life of the writing film 101 and the overall device.

[0038] Furthermore, to enable the back of the writing tablet to also have a magnetic attraction function, a magnetically conductive adsorption base layer B106 is provided on the side of the back panel away from the writing film. The magnetically conductive adsorption base layer B106 is a magnetically conductive material, including but not limited to sheet metal and galvanized sheet. The magnetically conductive adsorption base layer B106 is adhesively bonded to the back panel 108. To fix the magnetically conductive adsorption base layer B106 and the back panel 108, structural adhesive needs to be evenly applied to the bonding surfaces of the back panel and the magnetically conductive adsorption base layer B106, with a coating thickness of 50-100μm. After alignment and bonding, pressure is applied to form a rigid composite support layer.

[0039] The magnetically conductive adsorption base layer A and magnetically conductive adsorption base layer B are layered structures with magnetic properties and adsorption function, including but not limited to sheet metal and galvanized sheet, which can be adsorbed by magnetic items such as magnetic pens.

[0040] Furthermore, in order to complete the writing function of the whiteboard surface, a writing layer 107 with low friction coefficient, high hardness, anti-adhesion and easy cleaning is formed on the outer surface of the magnetic adsorption base layer B by coating, film or physical modification.

[0041] The coating process is the most common implementation path. First, the side of the magnetic adsorption base layer B away from the writing film is pretreated. The surface of the sheet metal layer is degreased, derusted, and passivated to remove surface impurities and oxide layers, forming a dense conversion film that improves the adhesion between the coating and the substrate, preventing subsequent coating peeling. Then, the coating, consisting of a resin matrix, white pigments and fillers, and functional additives, is evenly applied to the surface of the magnetic adsorption base layer B. Finally, UV curing, low-temperature baking (60-100℃), or room-temperature air drying processes are used to form a dense white film layer with a thickness of 10-30μm on the sheet metal surface, which is the writing layer. Users can write smoothly on it with a marker 4, and it can be erased without leaving a streak. The marker 4 can also be magnetically attached to the writing layer 107.

[0042] The coating process adopts a modular production method, which has higher production efficiency. This process involves prefabricating a white functional film and attaching it to the surface of the magnetic adsorption base layer B, and sealing the edges to prevent moisture from seeping in and causing the film to fall off.

[0043] The physical modification process enhances the physical properties of the magnetic adsorption base layer B, providing a stable substrate for subsequent coatings, and is suitable for high-end customized scenarios.

[0044] Furthermore, in order to ensure adhesive strength without affecting the writing experience, the thickness of the first adhesive layer 102 and the second adhesive layer 104 is 10-70μm. If the adhesive layer thickness is <10μm, the adhesive layer is prone to breakage and insufficient adhesion. The pressure applied during writing will cause the pattern layer to shift and lift, especially in the edge area of ​​large-size writing tablets where the risk is higher. If the adhesive layer thickness is too thick, >70μm, the adhesive layer is easily pressed and dented during writing, resulting in pen tip jamming and poor writing feel.

[0045] Preferably, when the first and second adhesive layers use double-sided adhesive, the construction process is simple. It only requires peeling off the release paper, accurately attaching the double-sided adhesive to the designated position of the layer to be bonded, and then achieving tight bonding through roller pressing. This is a cold bonding process that does not require curing time and can be quickly completed. Moreover, the uniformity of the adhesive layer thickness is guaranteed by the prefabricated specifications, with almost no construction error.

[0046] Preferably, when the first and second adhesive layers are formed by brushing or spraying adhesive, it is suitable for customized production. The thickness and coating range of the adhesive layer can be flexibly adjusted. The advantage is that the final bonding strength is high, the liquid adhesive can penetrate and fill the tiny gaps between the layers, and the formed adhesive layer is bonded to the substrate at the molecular level. It has better temperature resistance and weather resistance and is suitable for long-term use scenarios.

[0047] Furthermore, in order to clear the writing content on the surface, a clear button 3 is provided in the lower right corner of the front of the handwriting pad. The clear button is electrically connected to the handwriting film 101. After pressing, it can instantly reset the arrangement of all liquid crystal molecules, realize one-click clearing of the content on the LC film, and improve the efficiency of use.

[0048] The embodiments described above are merely illustrative of several implementations of this utility model, and while the descriptions are relatively specific and detailed, they should not be construed as limiting the scope of this utility model patent. It should be noted that those skilled in the art can make various modifications and improvements without departing from the concept of this utility model, and these all fall within the protection scope of this utility model. Therefore, the protection scope of this utility model patent should be determined by the appended claims.

Claims

1. A double-sided writing board with auxiliary line patterns, comprising a writing film, a backing plate, and patterns, characterized in that: It also includes a flexible substrate layer, the pattern is disposed on the flexible substrate layer, the flexible substrate layer is disposed between the handwriting film and the back plate, a first adhesive layer is disposed between the flexible substrate layer and the handwriting film, a second adhesive layer is disposed between the flexible substrate layer and the back plate, and the handwriting film is a transparent liquid crystal handwriting film.

2. The double-sided handwriting tablet with auxiliary line patterns according to claim 1, characterized in that: The flexible substrate layer is made of flexible materials, including but not limited to paper, PET plastic, non-woven fabric or soft PVC sheet.

3. A double-sided handwriting tablet with auxiliary line patterns according to claim 1, characterized in that: The flexible substrate layer is printed with patterns, and the printing process is one of inkjet printing, laser printing, screen printing and UV printing, which can print different patterns as required.

4. A double-sided handwriting tablet with auxiliary line patterns according to claim 1, characterized in that: The pattern is an independent pattern layer, which is attached to the flexible substrate layer.

5. A double-sided handwriting tablet with auxiliary line patterns according to claim 1, characterized in that: The first and second adhesive layers are double-sided adhesives, and the thickness of the adhesive layers is 10-70 μm.

6. A double-sided handwriting tablet with auxiliary line patterns according to claim 1, characterized in that: The first and second adhesive layers are formed by brushing or spraying adhesive, and the thickness of the adhesive layers is 10-70 μm.

7. A double-sided handwriting tablet with auxiliary line patterns according to claim 1, characterized in that: A magnetically conductive adsorption base layer A is provided between the back plate and the second adhesive layer, and the magnetically conductive adsorption base layer A is adhesively bonded to the back plate.

8. A double-sided handwriting tablet with auxiliary line patterns according to claim 1, characterized in that: The outer surface of the back panel, i.e. the side away from the writing membrane, is a writable whiteboard surface.

9. A double-sided writing tablet with auxiliary line patterns according to claim 1, characterized in that: The side of the back panel away from the writing film is provided with a magnetic adsorption base layer B, which is adhesively bonded to the back panel. The outer surface of the magnetic adsorption base layer B is coated, film-coated or physically modified to form a writing layer with low friction coefficient, high hardness, anti-adhesion and easy cleaning on the substrate surface.

10. A double-sided writing tablet with auxiliary line patterns according to claim 7 or 9, characterized in that: Both the magnetic adsorption base layer A and the magnetic adsorption base layer B are magnetically conductive materials, including but not limited to sheet metal and galvanized steel.

Citation Information

Patent Citations

  • Liquid crystal writing film with auxiliary lines, writing board and blackboard

    CN211426977U