Battery cover plate with electrode connecting block adopting composite copper layer structure and secondary battery
By employing a composite copper layer structure in the electrode connection block and welding the stepped protrusions of the aluminum block and copper layer, the problems of heavy weight and corrosion in the prior art are solved, achieving a lightweight and cost-effective battery cover design.
Patent Information
- Application Number
- CN202522593863.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2025-12-08
- Publication Date
- 2026-11-24
- Estimated Expiration
- 2035-12-08
AI Technical Summary
Existing lithium-ion battery electrode connectors typically use an integral copper block structure, resulting in greater weight and higher cost. Alternatively, aluminum materials can be used, requiring separate processing of the electrode posts, which increases process complexity and cost. Furthermore, aluminum is prone to corrosion in electrolytes.
The electrode connecting block adopts a composite copper layer structure, which utilizes the combination of aluminum block and copper layer, and is welded to the electrode base through stepped protrusion. During the stamping process, the depth of the stamping hole and the width of the annular band are optimized to reduce weight and avoid copper layer breakage.
This achieves lightweighting of the electrode connector, reducing weight and cost, while ensuring strong welding and preventing electrolyte corrosion, which aligns with the trend of battery lightweighting.
Smart Images

Figure CN225019429U_ABST
Abstract
Description
Technical Field
[0001] This utility model belongs to the field of secondary batteries, and in particular relates to a battery cover plate with an electrode connection block using a composite copper layer structure and a secondary battery. Background Technology
[0002] Rechargeable batteries are key components in modern energy storage. They utilize reversible chemical reactions to achieve the cyclical storage and release of electrical energy, overcoming the limitation of single-use batteries. Among various rechargeable batteries, lithium-ion batteries have become the most widely used energy storage option due to their superior overall performance. They offer three main advantages: high energy density (providing longer battery life within limited volume and weight, supporting thinner and lighter device designs), no memory effect (allowing users to charge and discharge at any time without affecting battery life, offering greater freedom of use), and low self-discharge rate (minimal power loss when idle, ensuring devices are ready to use immediately).
[0003] These characteristics make lithium-ion batteries a crucial support for modern technological society. Without lithium-ion batteries, portable devices such as smartphones and laptops would hardly be as thin, light, and ubiquitous as they are today. More importantly, rechargeable batteries are driving the energy transition in the transportation sector. In the field of new energy vehicles, large battery packs are not only the "power heart" of the vehicle, providing all the driving force, but also the "value core" of the entire vehicle, accounting for 30% to 40% of the total cost.
[0004] However, this core component also presents significant challenges. In electric vehicles, the heavy battery pack can account for 20% to 30% of the total vehicle weight, creating a "weight penalty" cycle: increasing the battery to improve range leads to increased weight, which in turn requires more energy to power the increased weight. Therefore, "battery lightweighting" has become an important direction for improving energy efficiency, range, and overall vehicle performance, and it is urgent to achieve more efficient structural lightweighting at the system level by optimizing the battery casing structure and reducing material weight. Utility Model Content
[0005] In view of the shortcomings of the prior art, the technical problem to be solved by this utility model is to provide a battery cover plate with an electrode connection block adopting a composite copper layer structure and a secondary battery.
[0006] To solve the above-mentioned technical problems, this utility model provides the following technical solution: A battery cover plate with an electrode connection block using a composite copper layer structure includes an electrode substrate, an electrode connection block disposed above the electrode substrate, and an electrode base disposed below the electrode substrate. The bottom surface of the electrode connection block is covered with a copper layer, and a downwardly protruding stepped protrusion is formed in the area of the electrode connection block corresponding to the copper layer. The stepped protrusion has at least three steps. A through electrode hole is provided on the electrode substrate at the position corresponding to the stepped protrusion, and a through welding hole is provided on the electrode base at the position corresponding to the stepped protrusion. The stepped protrusion passes downward through the electrode through hole and extends into the welding hole to be welded and fixed to the electrode base. The electrode connection block, the electrode base, and the electrode substrate are insulated and isolated by an isolation structure.
[0007] Furthermore, the electrode connection block is made of aluminum-copper composite material, including an aluminum block and a copper layer covering the middle of the bottom surface of the aluminum block; the copper layer covers 30% to 70% of the bottom surface of the aluminum block.
[0008] Furthermore, a step structure is formed at the junction of the aluminum block and the copper layer corresponding to the step protrusion, and the shape of the step structure matches the shape of the step protrusion; a downwardly recessed step hole is formed on the top surface of the aluminum block corresponding to the step protrusion, and the shape of the step hole matches the shape of the step protrusion.
[0009] Furthermore, the thickness of the copper layer is 0.6mm to 1.2mm; the depth of each of the punched holes is less than or equal to 60% of the thickness of the aluminum block in the copper layer region, and the minimum width of the annular band between two adjacent punched holes is greater than the thickness of the copper layer.
[0010] Furthermore, the stepped protrusion has three steps. The first step of the stepped protrusion is a first protrusion formed on the bottom surface of the electrode connecting block. The second step of the stepped protrusion is a second protrusion formed on the first protrusion. The third step of the stepped protrusion is a third protrusion formed on the second protrusion. Correspondingly, the stepped hole includes three punching holes, namely a first punching hole formed in the middle of the electrode connecting block, a second punching hole formed at the bottom of the first punching hole, and a third punching hole formed at the bottom of the second punching hole.
[0011] Furthermore, all the punched holes are either circular or elliptical.
[0012] Furthermore, the isolation structure includes an upper plastic, a lower plastic, and a sealing ring; the upper plastic is disposed between the electrode connecting block and the upper end face of the electrode substrate, and the lower plastic is disposed between the electrode base and the lower end face of the electrode substrate; the sealing ring is disposed at the position of the electrode through hole, thereby forming a sealing structure at the electrode through hole; the upper plastic is provided with a first clearance through hole at the position corresponding to the step protrusion, and the lower plastic is provided with a second clearance through hole at the position corresponding to the step protrusion; the step protrusion passes through the first clearance through hole, the electrode through hole, and the second clearance through hole in sequence, and extends into the welding through hole.
[0013] Furthermore, the upper plastic is provided with an annular isolation portion extending into the electrode through hole. The diameter of the second clearance through hole is larger than the diameter of the electrode through hole, thereby forming an annular mounting groove around the stepped protrusion in the second clearance through hole. The sealing ring is installed in the annular mounting groove and seals the gap between the electrode through hole and the stepped protrusion.
[0014] Furthermore, a first limiting groove is formed on the upper end face of the upper plastic corresponding to the position of the electrode connecting block. The shape of the first limiting groove is adapted to the shape of the electrode connecting block, and the electrode connecting block is disposed in the first limiting groove. At least two first positioning blind holes are formed on the upper end face of the electrode substrate by stamping. A first boss is formed on the upper plastic corresponding to the position of each first positioning blind hole. The shape of the first boss is adapted to the first positioning blind hole, and the first boss extends into the first positioning blind hole. A downwardly protruding second boss is formed on the lower end face of the electrode substrate corresponding to the position of each first positioning blind hole. A second positioning blind hole is formed, the shape of which is adapted to the shape of the second boss, and the second boss extends into the second positioning blind hole; a third boss protruding downward is formed on the lower end face of the lower plastic corresponding to the position of each second positioning blind hole; a positioning notch is formed on the upper end face of the electrode base corresponding to the position of the third boss, the shape of which is adapted to the shape of the third boss, and the third boss extends into the positioning notch; a ring of baffles is also formed on the lower end face of the lower plastic corresponding to the periphery of the electrode base, the baffles forming a second limiting groove, the shape of which is adapted to the shape of the electrode base, and the electrode base is disposed in the second limiting groove.
[0015] A secondary battery, the outer casing of which includes a battery cover plate with an electrode connection block employing a composite copper layer structure as described in any of the preceding claims.
[0016] In this invention, the electrode connecting block utilizes a copper-aluminum composite material in a composite copper layer structure. This satisfies the requirement for welding the electrode connecting block and the electrode base to the same metal while significantly reducing weight. By forming a stepped protrusion in the copper layer, which replaces the electrode post for welding to the electrode base, and by forming a corresponding stepped hole on the front of the electrode connecting block, the stepped protrusion does not add any extra weight to the electrode connecting block, thus further reducing the weight of the battery cover. Furthermore, by selecting appropriate dimensional parameters such as the depth of the stamping hole and the minimum width of the annular band between two adjacent stamping holes, the electrode connecting block can be easily formed by stamping, preventing the copper layer from breaking during stamping and ensuring the product's yield requirements are met. Attached Figure Description
[0017] The accompanying drawings, which are included to provide a further understanding of this application and form part of this application, illustrate exemplary embodiments and are used to explain this application, but do not constitute an undue limitation of this application. In the drawings: Figure 1 This is a schematic diagram of an embodiment of a battery cover plate with a composite copper layer structure for an electrode connection block according to the present invention.
[0018] Figure 2 This is a schematic diagram of the electrode connection block.
[0019] Figure 3 and Figure 4 This is an exploded view of the battery cover.
[0020] Figure 5 for Figure 1 Top view.
[0021] Figure 6 for Figure 5 Sectional view along the AA direction.
[0022] Figure 7 for Figure 6 Enlarged view of point B in the middle.
[0023] The diagrams in the instruction manual are labeled as follows: Electrode connecting block 100; aluminum block 101; copper layer 102; stepped hole 110; first punch hole 111; second punch hole 112; third punch hole 113; first annular band 114; second annular band 115; stepped protrusion 120; first protrusion 121; second protrusion 122; third protrusion 123; stepped structure 130; Upper plastic 200; First clearance through hole 210; First limiting groove 220; First boss 230; Annular isolation part 240; Electrode substrate 300; electrode through hole 310; first positioning blind hole - 320; second boss - 330; 400 sealing ring; 410 annular mounting groove; Lower plastic part 500; second clearance through hole 510; second positioning blind hole 520; third boss 530; stop strip 540; second limiting groove 550; Electrode base 600; welding through hole 610; positioning notch 620. Detailed Implementation
[0024] The following specific examples illustrate the implementation of this utility model. The illustrations provided in the following embodiments are only schematic representations of the basic concept of this utility model. Unless otherwise specified, the following embodiments and features can be combined with each other.
[0025] Please see Figure 1 , Figure 1 This is a schematic diagram of an embodiment of a battery cover plate with an electrode connection block employing a composite copper layer structure. The battery cover plate with an electrode connection block employing a composite copper layer structure in this embodiment includes an electrode substrate 300, an electrode connection block 100 disposed above the electrode substrate 300, and an electrode base 600 disposed below the electrode substrate 300. The electrode connection block 100 employs a composite copper layer structure, with a copper layer 102 covering the center of its bottom surface. In this embodiment, the electrode connection block 100 is made of an aluminum-copper composite material, including an aluminum block 101 and a copper layer 102 covering the center of the bottom surface of the aluminum block 101. Alternatively, an aluminum-copper composite material with a bottom surface entirely composed of copper layers 102 can also be used.
[0026] In existing technologies, the electrode connector 100 typically employs a monolithic copper block structure to achieve homogeneous metal welding with the electrode base 600. However, copper itself is expensive, and the overall weight is significant. Another approach is to use an aluminum electrode connector 100 with a separate copper electrode post for homogeneous metal welding with the electrode base 600. However, this dissimilar metal combination requires separate fabrication of the electrode post, increasing process complexity and consequently raising manufacturing costs.
[0027] This embodiment uses aluminum to leverage its low density and low cost, aiming to achieve lightweight components and control production costs. However, aluminum can react chemically with the electrolyte inside the battery casing, leading to severe corrosion, especially in the negative electrode environment. Therefore, this embodiment incorporates a copper layer 102 on the contact surface of the aluminum block 101, ensuring that all parts in contact with the electrolyte are made of corrosion-resistant copper, effectively preventing electrolyte corrosion of the electrode connection block 100.
[0028] The area of the copper layer 102 needs to strike a balance between machinability and cost: if the area of the copper layer 102 is too small, it will be difficult to form the stepped protrusion 120 by stamping; if the area of the copper layer 102 is too large, it will cause unnecessary material waste and increased costs. Therefore, the copper layer 102 generally covers 30% to 70% of the bottom surface of the aluminum block 101. For example, the copper layer 102 can cover 30%, 40%, 50%, 60%, 70%, etc. of the bottom surface of the aluminum block 101. In the electrode connecting block 100 of this embodiment, the length of the aluminum block 101 is preferably 40 mm, the length of the copper layer 102 is preferably 16 mm, and the width of the copper layer 102 is the same as the width of the aluminum block 101; therefore, the copper layer 102 covers 40% of the bottom surface of the aluminum block 101.
[0029] To facilitate manufacturing using a stamping process, the thickness (i.e., d1 + d2) of the electrode connecting block 100 should not be too thick. Of course, the thickness of the electrode connecting block 100 should also not be too thin; the thickness can be 0.25 mm to 0.5 mm. For example, the thickness of the electrode connecting block 100 can be 0.25 mm, 0.3 mm, 0.35 mm, 0.4 mm, 0.45 mm, 0.5 mm, etc. In this embodiment, the thickness of the electrode connecting block 100 is preferably 0.3 mm.
[0030] Since the copper layer 102 needs to be welded to the electrode base 600, if the thickness of the copper layer 102 is too thin, it is easy to weld through the copper layer 102 during the welding process, thus causing the copper layer 102 to lose its protective function; on the other hand, if the thickness of the copper layer 102 is too thick, it will undoubtedly increase the cost and the weight of the electrode connecting block 100. Therefore, the thickness d2 of the copper layer 102 is generally 0.6mm to 1.2mm; for example, the thickness d2 of the copper layer 102 can be 0.6mm, 0.65mm, 0.7mm, 0.75mm, 0.8mm, 0.85mm, 0.9mm, 0.95mm, 1mm, 1.1mm, 1.2mm, etc. In this embodiment, the thickness d2 of the copper layer 102 is preferably 0.8mm; that is, in this embodiment, the thickness d1 of the aluminum block 101 at the copper layer 102 is 2.4mm.
[0031] Please see Figure 2The electrode connecting block 100 has a downwardly protruding stepped protrusion 120 corresponding to the copper layer 102, and the stepped protrusion 120 has at least three steps. A stepped structure 130 is formed at the junction of the aluminum block 101 and the copper layer 102, corresponding to the stepped protrusion 120, and the shape of the stepped structure 130 matches the shape of the stepped protrusion 120. By forming the stepped structure 130 at the junction of the aluminum block 101 and the copper layer 102, the thickness of the copper layer in this area can be made relatively uniform, avoiding excessively thin copper layers in some areas. Where the stepped protrusion 120 is not formed, the lower end face of the copper layer 102 is generally flush with the bottom surface of the aluminum block 101, thus making the bottom surface of the electrode connecting block 100 a plane outside the stepped protrusion 120.
[0032] The top surface of the aluminum block 101 has a downwardly recessed stepped hole 110 corresponding to the stepped protrusion 120. The shape of the stepped hole 110 is adapted to the shape of the stepped protrusion 120. By forming the stepped hole 110, the weight of the electrode connecting block 100 can be further reduced.
[0033] The stepped hole 110, stepped protrusion 120, and stepped structure 130 can be formed on the front side of the electrode connecting block 100 in an order from the inside to the outside (i.e., from small to large) through at least three stamping processes. Alternatively, the stepped hole 110, stepped protrusion 120, and stepped structure 130 can also be formed on the front side of the electrode connecting block 100 in an order from the outside to the inside (i.e., from large to small) through at least three stamping processes. Each stamping process forms one stamped hole and one step. The stepped protrusion 120 can replace the original electrode post, realizing the connection between the electrode connecting block 100 and the electrode base 600. In this embodiment, the stamped hole is generally a circular or elliptical hole. Of course, the stamped hole can also be other shapes.
[0034] To reduce the weight of the battery cover and control costs, the copper layer 102 is typically designed to be thin and small. However, copper itself has poor fluidity, and during stamping, the instantaneous tensile force can easily cause the thin copper layer 102 to break, resulting in product scrap. Therefore, in this embodiment, the dimensions of the stepped hole 110 and the stepped protrusion 120 are optimized to avoid the copper layer 102 breaking during stamping.
[0035] The depth of the punched holes (i.e., the depth of each punch) is closely related to whether the copper layer 102 will fracture. When the punched holes are deep, there is a higher probability that the copper layer 102 will fracture; while when the punched holes are shallow, the copper layer 102 generally will not fracture. However, if the punched holes are too shallow, the number of punches will increase, thereby increasing the process flow; therefore, it is necessary to reasonably select the depth of each punched hole. In this embodiment, the depth of each punched hole is preferably no greater than 60% of the thickness of the aluminum block 101 in the copper layer 102 region. For example, the depth of each punched hole can be 30%, 35%, 40%, 45%, 50%, 55%, 60%, etc., of the thickness of the aluminum block 101 in the copper layer 102 region, and the average depth of all punched holes is preferably between 40% and 50% of the thickness of the aluminum block 101 in the copper layer 102 region.
[0036] Based on the aforementioned depth requirements for the stamping holes and the height requirements for the stepped protrusion 120 (the stepped protrusion 120 needs to be connected to the lower electrode base 600, thus requiring a certain height), in this embodiment, the stepped protrusion 120 and the stepped structure 130 preferably have three levels of steps. The first level of the stepped protrusion 120 is a first protrusion 121 formed on the bottom surface of the electrode connecting block 100; the second level of the stepped protrusion 120 is a second protrusion 122 formed on the first protrusion 121; and the third level of the stepped protrusion 120 is a third protrusion 123 formed on the second protrusion 122. That is, the diameter of the first protrusion 121 is larger than the diameter of the second protrusion 122, and the diameter of the second protrusion 122 is larger than the diameter of the third protrusion 123.
[0037] Accordingly, the stepped hole 110 includes three punched holes: a first punched hole 111 formed on the front side of the electrode connecting block 100, a second punched hole 112 formed at the bottom of the first punched hole 111, and a third punched hole 113 formed at the bottom of the second punched hole 112. That is, the diameter of the first punched hole 111 is larger than the diameter of the second punched hole 112, and the diameter of the second punched hole 112 is larger than the diameter of the third punched hole 113.
[0038] In this embodiment, the depth of the first punch hole 111 and the height h1 of the first protrusion 121 are both 1.3 mm; the depth of the second punch hole 112 and the height h2 of the second protrusion 122 are both 0.9 mm; and the depth of the third punch hole 113 and the height h3 of the third protrusion 123 are both 1.1 mm. The average depth of the first punch hole 111, the second punch hole 112, and the third punch hole 113 is 1.1 m, which is approximately 46% of the thickness of the aluminum block 101 in the copper layer 102 region.
[0039] Furthermore, if the minimum width of the annular band between two adjacent stamping holes is too small, the copper layer 102 at the stamped step will be too thin, making it prone to breakage. Therefore, the minimum width of the annular band between two adjacent stamping holes generally needs to be greater than the thickness of the copper layer 102. For example, the minimum width of the annular band between two adjacent stamping holes can be 1.1 times, 1.15 times, 1.2 times, 1.25 times, 1.3 times, 1.35 times, 1.4 times, 1.45 times, or 1.5 times the thickness of the copper layer 102.
[0040] On the other hand, when the width of the annular band between two adjacent punching holes is too large, it will result in the stepped protrusion 120 occupying an excessively large area. Therefore, the width of the annular band between two adjacent punching holes should not be too large, and the width of the annular band between two adjacent punching holes needs to be reasonably selected. In this embodiment, each punching hole is preferably a coaxially arranged circular hole, so that the width of the annular band between two adjacent punching holes is equal everywhere. Preferably, the width of the annular band between two adjacent punching holes is between 1.2 and 1.3 times the thickness of the copper layer 102. In this embodiment, the annular band includes a first annular band 114 formed between the first punching hole 111 and the second punching hole 112, and a second annular band 115 formed between the second punching hole 112 and the third punching hole 113; the width L1 of the first annular band 114 and the width L2 of the second annular band 115 are both about 1 mm, which is 1.25 times the thickness of the copper layer 102.
[0041] In this embodiment, by selecting dimensional parameters such as the depth of the stamping hole and the minimum width of the annular band between two adjacent stamping holes, it is convenient to form the electrode connecting block 100 through the stamping process, and the copper layer 102 can be prevented from breaking when the stepped protrusion 120 is formed by stamping, so as to meet the product qualification rate requirements.
[0042] Please see Figure 3 , Figure 4 , Figure 5 , Figure 6 and Figure 7 The electrode substrate 300 has a through electrode hole 310 at the position corresponding to the stepped protrusion 120, and the electrode base 600 has a through welding hole 610 at the position corresponding to the stepped protrusion 120. The lower end of the stepped protrusion 120 passes downward through the electrode hole 310 and extends into the welding hole 610 to be welded and fixed to the electrode base 600. The electrode connecting block 100, the electrode base 600 and the electrode substrate 300 are insulated and isolated by an isolation structure.
[0043] In this embodiment, the isolation structure includes an upper plastic 200, a lower plastic 500, and a sealing ring 400. The upper plastic 200 is disposed between the upper end face of the electrode connecting block 100 and the electrode substrate 300, and the lower plastic 500 is disposed between the lower end face of the electrode base 600 and the electrode substrate 300. The sealing ring 400 is disposed at the position of the electrode through hole 310, thereby forming a sealing structure at the electrode through hole 310. The upper plastic 200 is provided with a first clearance through hole 210 at the position corresponding to the stepped protrusion 120, and the lower plastic 500 is provided with a second clearance through hole 510 at the position corresponding to the stepped protrusion 120. The stepped protrusion 120 passes sequentially through the first clearance through hole 210, the electrode through hole 310, and the second clearance through hole 510, and the lower end of the stepped protrusion 120 (i.e., the third protrusion 123) extends into the welding through hole 610.
[0044] To improve the sealing effect of the sealing ring 400, in this embodiment, the upper plastic 200 is provided with an annular isolation portion 240 extending into the electrode through hole 310. The diameter of the second clearance through hole 510 is larger than the diameter of the electrode through hole 310, thereby forming an annular mounting groove 410 around the second protrusion 122 of the stepped protrusion 120 in the second clearance through hole 510 to facilitate the installation of the sealing ring 400. The sealing ring 400 is installed in the annular mounting groove 410 and seals the gap between the electrode through hole 310 and the stepped protrusion 120 to achieve a seal of the battery cover at the electrode through hole 310. Specifically, in this embodiment, two air passages are formed at the lower part of the battery cover plate, connecting the annular mounting groove 410 and the internal space of the battery casing. These are the first air passage formed along the side of the third protrusion 123, the wall of the welding through hole 610, the end face of the second protrusion 122, and the upper surface of the electrode base 600, and the second air passage formed along the gap between the lower plastic 500 and the electrode substrate 300. In this embodiment, by forming the annular mounting groove 410, the sealing ring 400 can simultaneously seal the first and second air passages.
[0045] To facilitate the positioning of the components of the battery cover during installation, in this embodiment, a first limiting groove-220 is formed on the upper end face of the upper plastic 200 at the position corresponding to the electrode connecting block 100; the shape of the first limiting groove-220 is adapted to the shape of the electrode connecting block 100, and the electrode connecting block 100 is disposed in the first limiting groove-220, thereby realizing the positioning between the electrode connecting block 100 and the upper plastic 200.
[0046] The upper surface of the electrode substrate 300 is formed with at least two first positioning blind holes -320 by stamping. A first boss -230 is formed on the upper plastic 200 at the position corresponding to each first positioning blind hole -320. The shape of the first boss -230 is adapted to the first positioning blind hole -320, and the first boss -230 extends into the first positioning blind hole -320, thereby achieving positioning between the upper plastic 200 and the electrode substrate 300.
[0047] A downwardly protruding second boss 330 is formed on the lower end face of the electrode substrate 300 at the position corresponding to each first positioning blind hole 320. A second positioning blind hole 520 is formed on the lower plastic 500 at the position corresponding to the second boss 330. The shape of the second positioning blind hole 520 is adapted to the shape of the second boss 330, and the second boss 330 extends into the second positioning blind hole 520, thereby enabling positioning between the electrode substrate 300 and the lower plastic 500.
[0048] The lower end face of the lower plastic 500 has a downwardly protruding third boss 530 at the position corresponding to each second positioning blind hole 520. The upper end face of the electrode base 600 has a positioning notch 620 at the position corresponding to the third boss 530. The shape of the positioning notch 620 is adapted to the third boss 530, and the third boss 530 extends into the positioning notch 620, thereby achieving positioning between the lower plastic 500 and the electrode base 600. In addition, in this embodiment, a retaining strip 540 is also formed around the lower end face of the lower plastic 500 corresponding to the electrode base 600. The retaining strip 540 surrounds and forms a second limiting groove 550. The shape of the second limiting groove 550 is adapted to the shape of the electrode base 600. The electrode base 600 is disposed in the second limiting groove 550, thereby further limiting the electrode base 600.
[0049] In this embodiment, the electrode connecting block 100 adopts a copper-aluminum composite material in a composite copper layer structure. This satisfies the requirement of welding the electrode connecting block 100 and the electrode base 600 with the same metal, while significantly reducing weight compared to a copper block. By forming a stepped protrusion 120 at the copper layer 102, the stepped protrusion 120 is used to replace the electrode post for welding to the electrode base 600. A corresponding stepped hole 110 is formed on the front side of the electrode connecting block 100. This means that the stepped protrusion 120 does not add any extra weight to the electrode connecting block 100 (the weight of the stepped protrusion 120 is offset by the weight reduction at the stepped hole 110), further reducing the weight of the battery cover. In addition, by selecting dimensional parameters such as the depth of the stamping hole and the minimum width of the annular band between two adjacent stamping holes, the electrode connecting block 100 can be easily formed by stamping, and the copper layer 102 can be prevented from breaking during stamping, thus meeting the product yield requirements.
[0050] This utility model also discloses a secondary battery, the outer casing of which includes a battery cover plate with an electrode connection block using a composite copper layer structure as described in any of the above embodiments.
[0051] In this embodiment, the electrode connecting block 100 and the electrode base 600 can meet the requirements for welding with the same metal, resulting in a more robust and reliable weld. Furthermore, the contact surfaces between the electrode connecting block 100 and the electrolyte inside the battery are both copper layers 102, which can prevent corrosion by the electrolyte. In addition, the use of copper-aluminum composite materials for the electrode connecting block 100 and the formation of stepped holes 110 in the electrode connecting block 100 significantly reduce its weight, aligning with the trend towards lightweight battery casings.
[0052] The above embodiments only illustrate preferred implementations of this utility model, and their descriptions are relatively specific and detailed, but they should not be construed as limiting the scope of the utility model patent. It should be noted that those skilled in the art can make various modifications and improvements without departing from the concept of this utility model, and these all fall within the protection scope of this utility model. Therefore, the protection scope of this utility model patent should be determined by the appended claims.
Claims
1. A battery cover plate with an electrode connection block employing a composite copper layer structure, characterized in that: The device includes an electrode substrate, an electrode connecting block disposed above the electrode substrate, and an electrode base disposed below the electrode substrate. The bottom surface of the electrode connecting block is covered with a copper layer. A downwardly protruding stepped protrusion is formed in the area of the electrode connecting block corresponding to the copper layer. The stepped protrusion has at least three steps. A through-hole electrode is provided on the electrode substrate at the position corresponding to the stepped protrusion. A through-hole welding is provided on the electrode base at the position corresponding to the stepped protrusion. The stepped protrusion passes downward through the electrode through-hole and extends into the welding through-hole to be welded and fixed to the electrode base. The electrode connecting block, the electrode base, and the electrode substrate are insulated from each other by an isolation structure.
2. The battery cover plate with a composite copper layer structure for the electrode connection block as described in claim 1, characterized in that: The electrode connection block is made of aluminum-copper composite material, including an aluminum block and a copper layer covering the middle of the bottom surface of the aluminum block; the copper layer covers 30% to 70% of the bottom surface of the aluminum block.
3. A battery cover plate with a composite copper layer structure for electrode connection blocks as described in claim 2, characterized in that: At the junction of the aluminum block and the copper layer, a step structure is formed at the position corresponding to the step protrusion, and the shape of the step structure matches the shape of the step protrusion; a downwardly recessed step hole is formed on the top surface of the aluminum block at the position corresponding to the step protrusion, and the shape of the step hole matches the shape of the step protrusion.
4. A battery cover plate with a composite copper layer structure for electrode connection blocks as described in claim 3, characterized in that: The stepped protrusion has three steps. The first step of the stepped protrusion is a first protrusion formed on the bottom surface of the electrode connecting block. The second step of the stepped protrusion is a second protrusion formed on the first protrusion. The third step of the stepped protrusion is a third protrusion formed on the second protrusion. Correspondingly, the stepped hole includes three punching holes, namely a first punching hole formed in the middle of the electrode connecting block, a second punching hole formed at the bottom of the first punching hole, and a third punching hole formed at the bottom of the second punching hole.
5. A battery cover plate with a composite copper layer structure for electrode connection blocks as described in claim 4, characterized in that: The thickness of the copper layer is 0.6mm to 1.2mm; the depth of each of the punched holes is less than or equal to 60% of the thickness of the aluminum block in the copper layer region, and the minimum width of the annular band between two adjacent punched holes is greater than the thickness of the copper layer.
6. A battery cover plate with a composite copper layer structure for electrode connection blocks as described in claim 4, characterized in that: All the punched holes are either circular or elliptical.
7. A battery cover plate with a composite copper layer structure for electrode connection blocks as described in claim 1, characterized in that, The isolation structure includes an upper plastic, a lower plastic, and a sealing ring; the upper plastic is disposed between the electrode connecting block and the upper end face of the electrode substrate, and the lower plastic is disposed between the electrode base and the lower end face of the electrode substrate; the sealing ring is disposed at the position of the electrode through hole, thereby forming a sealing structure at the electrode through hole; the upper plastic is provided with a first clearance through hole at the position corresponding to the step protrusion, and the lower plastic is provided with a second clearance through hole at the position corresponding to the step protrusion; the step protrusion passes through the first clearance through hole, the electrode through hole, and the second clearance through hole in sequence, and extends into the welding through hole.
8. A battery cover plate with a composite copper layer structure for electrode connection blocks as described in claim 7, characterized in that: The upper plastic is provided with an annular isolation part extending into the electrode through hole. The diameter of the second relief through hole is larger than the diameter of the electrode through hole, thereby forming an annular mounting groove around the stepped protrusion in the second relief through hole. The sealing ring is installed in the annular mounting groove and seals the gap between the electrode through hole and the stepped protrusion.
9. A battery cover plate with a composite copper layer structure for electrode connection blocks as described in claim 7, characterized in that: The upper end face of the upper plastic substrate has a first limiting groove formed at the position corresponding to the electrode connecting block. The shape of the first limiting groove is adapted to the shape of the electrode connecting block, and the electrode connecting block is disposed in the first limiting groove. The upper end face of the electrode substrate has at least two first positioning blind holes formed by stamping. A first boss is formed on the upper plastic substrate at the position corresponding to each first positioning blind hole. The shape of the first boss is adapted to the first positioning blind hole, and the first boss extends into the first positioning blind hole. The lower end face of the electrode substrate has a downwardly protruding second boss formed at the position corresponding to each first positioning blind hole. A second boss is formed on the lower plastic substrate at the position corresponding to the second boss. The electrode base has a second positioning blind hole, the shape of which is adapted to the shape of the second boss, and the second boss extends into the second positioning blind hole; the lower end face of the lower plastic has a downward protruding third boss at the position corresponding to each second positioning blind hole, and the upper end face of the electrode base has a positioning notch at the position corresponding to the third boss, the shape of which is adapted to the shape of the third boss, and the third boss extends into the positioning notch; the lower end face of the lower plastic also has a ring of baffles around the electrode base, the baffles forming a second limiting groove, the shape of which is adapted to the shape of the electrode base, and the electrode base is disposed in the second limiting groove.
10. A secondary battery, characterized in that: The outer casing of the secondary battery includes a battery cover plate with a composite copper layer structure for the electrode connection block as described in any one of claims 1 to 9.