Metallic tubular heater reinforced by filler-assisted synergism
By using a combination structure of mesh tubes and support components in a metal tubular heater, the insulation layer is densified, the problem of voids in the insulation layer is solved, the insulation performance and safety are improved, and the service life is extended.
Patent Information
- Application Number
- CN202522717621.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2025-12-23
- Publication Date
- 2026-11-24
- Estimated Expiration
- 2035-12-23
AI Technical Summary
The insulation layer of existing metal tubular electric heating elements has gaps, resulting in insufficient insulation performance, which affects heating efficiency and service life, and poses safety hazards.
The system employs a combination structure of mesh tube and support components. Through a high-temperature tube shrinking process, molten filler uniformly fills the voids of the main filler to form a dense insulator. The support component design ensures a stable connection between the mesh tube and the outer metal tube and uniform flow of the filler.
It significantly improves insulation performance and safety, ensures the structural stability and thermal conductivity of the heater, and extends its service life.
Smart Images

Figure CN225020685U_ABST
Abstract
Description
Technical Field
[0001] This utility model relates to a metal tubular heater that is synergistically enhanced by filler. Background Technology
[0002] Metal tubular heating elements, with their significant advantages such as compact structure, high heating efficiency, long service life, and strong adaptability, occupy an indispensable position in many fields, including industrial heating, household appliance heating, and temperature control in special environments, with extremely wide application scenarios. The core structure of this type of heating element mainly consists of a metal outer tube, an insulating layer, and an electrically conductive heating element. Among them, the insulating layer is a key component that achieves electrical isolation between the electrically conductive heating element and the metal outer tube, and its performance directly determines the safety, stability, and service life of the heating element.
[0003] Currently, the industry commonly uses granular insulating filler as the core material for the insulation layer. The filler is compacted using a tube-shrinking process to form an insulating structure. However, the physical properties of granular filler inevitably leave numerous tiny voids between the particles during compaction. These voids disrupt the overall structure of the insulation layer, resulting in insufficient density and ultimately leading to a critical defect: reduced insulation performance. This defect not only weakens the heating efficiency of heating elements and shortens their lifespan but also compromises the reliability of electrical isolation, posing serious safety hazards such as electrical leakage and directly threatening operational safety.
[0004] To address these issues, existing technologies have introduced improved solutions by doping molten materials into granular magnesium oxide fillers. These solutions attempt to fill the voids between magnesium oxide particles through high-temperature melting, thereby enhancing the density of the insulation layer. However, this approach has significant drawbacks: the molten material is difficult to disperse uniformly within the magnesium oxide particle system, tending to accumulate in localized areas and form blocky glassy substances. This not only fails to completely eliminate the voids but also disrupts the internal heat conduction path of the heating element, leading to a significant decrease in thermal conductivity and consequently affecting the stability of heating efficiency and the overall lifespan of the element. Utility Model Content
[0005] In view of the above-mentioned technical defects in the existing technology, the purpose of this utility model is to provide a metal tubular heater that is reinforced by filler assistance, so as to solve the problems of voids and insufficient insulation performance in the insulation layer of existing metal tubular electric heating elements.
[0006] A metal tubular heater with filler-assisted synergistic reinforcement includes a metal outer tube, a mesh tube, a support member, and a resistance wire; the mesh tube is disposed inside the metal outer tube, the mesh tube has a hollow structure, and its outer wall has a plurality of uniformly distributed through holes; a molten filler region is formed between the mesh tube and the metal outer tube, and a main filler region is formed inside the mesh tube.
[0007] The support members are provided in several parts, evenly distributed between the inner walls of the mesh tube and the outer metal tube, for connecting the mesh tube and the outer metal tube, realizing the partitioning and synergistic effect of the main filler and the molten filler, laying the structural foundation for the molten filler to uniformly fill the voids of the main filler during the subsequent high-temperature tube shrinking process, and ensuring the stability of the installation and positioning of the mesh tube inside the outer metal tube.
[0008] Furthermore, the support member includes an arc-shaped portion on the outer side and a square portion on the inner side. The inner wall of the square portion is fixedly connected to the outer wall of the mesh tube, and the outer wall of the square portion is fixedly connected to the inner side of the arc-shaped portion. The width of the square portion is less than the minimum width of the arc-shaped portion. This structural design ensures a tight fit between the support member and the inner wall of the metal outer tube, and allows for flexible deformation during high-temperature tube shrinkage, avoiding obstruction of the filler flow and enhancing the connection between the mesh tube and the metal outer tube.
[0009] Furthermore, the number of the support members is 3-18, with three support members arranged in a ring to form a group. Multiple groups of support members are distributed at equal intervals along the axial direction of the mesh tube. This distribution method ensures that the mesh tube is subjected to uniform force, avoids structural deformation caused by local stress concentration, and provides sufficient flow channels and space for the molten filler, ensuring that it diffuses evenly to the main filler area during the high-temperature tube shrinking process.
[0010] Furthermore, the curvature of the arc-shaped portion is adapted to the curvature of the inner wall of the outer metal tube, so that the support and the inner wall of the outer metal tube can be fully fitted, improving the connection stability and the overall structural integrity. At the same time, it can adaptively withstand pressure and deformation during the tube shrinking process, avoiding gaps between the support and the outer metal tube that would affect the compaction effect.
[0011] Furthermore, the through holes on the outer wall of the mesh pipe have a diameter larger than that of the molten filler but smaller than that of the main filler. This ensures that the molten filler, after being melted at high temperature, can flow smoothly through the through holes to fill the gaps in the main filler area, while also effectively preventing the main filler particles from entering the molten filler area and causing channel blockage. This ensures the reliable realization of the zoned filling function and the synergistic strengthening effect.
[0012] Furthermore, the metal tubular heater is formed by high-temperature tube shrinking, resulting in a final diameter smaller than that of the original metal outer tube. The tube shrinking process ensures that all components fit together tightly, further compacting the main packing and molten packing. This promotes the molten packing to fully fill the voids in the main packing, forming a dense composite insulation layer and improving the heater's insulation performance and mechanical strength.
[0013] Furthermore, the outer metal tube is made of stainless steel, copper, or nickel-chromium alloy, and the mesh tube is made of nickel-chromium alloy or iron-chromium-aluminum alloy. The selection of the above-mentioned high-temperature resistant and corrosion-resistant materials can ensure the structural stability and service life of the heater in high-temperature working environments, while also adapting to the high-temperature melting process requirements of the molten filler, avoiding material aging and deterioration that could affect insulation performance and thermal conductivity. Beneficial effects
[0014] This device divides the inner cavity of the outer metal tube into a main packing region and a molten packing region through a mesh tube. Combined with a high-temperature tube shrinking process, the molten packing melts and flows to fill the voids in the main packing. After cooling, it forms a dense insulator with the main packing, solving the problem of insufficient insulation performance caused by gaps between insulating packings in existing technologies. This significantly improves the insulation performance and safety of the heater. The overall structure is rationally designed, the assembly process is simple, and it is easy to carry out industrial production. Attached Figure Description
[0015] Figure 1 This is a schematic diagram of the main structure of a metal tubular heater that is synergistically enhanced by filler material. Figure 2 This is a cross-sectional view of the internal structure of this type of metal tubular heater; Figure 3 This is a diagram illustrating the connection between the network management system and the connectors; Figure 4 This is a schematic diagram of the network management system. In the diagram: 1. Metal outer tube, 2. Mesh tube, 3. Supporting component. Detailed Implementation
[0016] To enhance understanding of this utility model, the present utility model will be further described in detail below with reference to the embodiments and accompanying drawings. These embodiments are only used to explain the present utility model and do not constitute a limitation on the scope of protection of the present utility model.
[0017] Example 1: As Figure 1-4 As shown, a metal tubular heater with synergistic reinforcement through packing includes a metal outer tube 1, a mesh tube 2, a support 3, a resistance wire, a main packing, and molten packing. The mesh tube 2 is located inside the metal outer tube 1. The mesh tube 2 has a hollow structure and its outer wall has uniformly distributed through holes. The through holes are evenly distributed along the axial and circumferential directions of the mesh tube 2.
[0018] like Figure 2 As shown, region A contains molten filler, which is a mixture of borate and silicate compounds, while region B contains main filler, which is magnesium oxide particles.
[0019] Twelve support members 3 are evenly distributed between the inner walls of the mesh tube 2 and the outer metal tube 1, used to connect the mesh tube 2 and the outer metal tube 1. The support member 3 includes an arc-shaped portion on the outer side and a square portion on the inner side. The inner wall of the square portion is welded and fixed to the outer wall of the mesh tube 2, and the outer wall of the square portion is welded and fixed to the inner side of the arc-shaped portion. The width of the square portion is less than the minimum width of the arc-shaped portion. The curvature of the arc-shaped portion is adapted to the curvature of the inner wall of the outer metal tube 1.
[0020] The resistance wire is placed inside the mesh tube 2. The main packing material is filled in the main packing area B, and the main packing material is magnesium oxide particles. Molten packing material is filled in the molten packing area A, and the molten packing material is a mixture of borate and silicate compounds, wherein the mass ratio of borate to silicate compounds is 2:1.
[0021] After assembly, the overall metal tubular heater is subjected to tube shrinking treatment in a high-temperature environment. During the tube shrinking process, the support 3 deforms, and the molten filler melts and flows through the through hole to the main filler area B, filling the gaps between the magnesium oxide particles. After cooling, the molten filler vitrifies and forms a dense insulator with the magnesium oxide particles.
[0022] The above description is only a preferred embodiment of the present utility model and is not intended to limit the present utility model. Any modifications, equivalent substitutions, improvements, etc., made within the spirit and principles of the present utility model should be included within the protection scope of the present utility model.
Claims
1. A metal tubular heater with synergistic reinforcement through filler, characterized in that, Includes metal outer tube, mesh tube, support components and resistance wire; The mesh tube is disposed inside the outer metal tube. The mesh tube has a hollow structure and has several evenly distributed through holes on its outer wall. A molten filler region is formed between the mesh tube and the outer metal tube, and a main filler region is formed inside the mesh tube. Several support members are provided and are evenly distributed between the inner walls of the mesh tube and the outer metal tube for connecting the mesh tube and the outer metal tube.
2. A metal tubular heater with synergistic reinforcement through filler assistance according to claim 1, characterized in that, The support member includes an arc-shaped portion on the outer side and a square portion on the inner side. The inner wall of the square portion is fixedly connected to the outer wall of the mesh tube, and the outer wall of the square portion is fixedly connected to the inner side of the arc-shaped portion. The width of the square portion is less than the minimum width of the arc-shaped portion.
3. A metal tubular heater with synergistic reinforcement through filler assistance according to claim 2, characterized in that, The number of support members is 3-18, with three support members arranged in a ring to form a group, and multiple groups of support members are distributed at equal intervals along the axial direction of the mesh tube.
4. A metal tubular heater with synergistic reinforcement through filler assistance according to claim 3, characterized in that, The curvature of the arc-shaped portion is adapted to the curvature of the inner wall of the outer metal tube.
5. A metal tubular heater with synergistic reinforcement through filler assistance according to claim 1, characterized in that, The diameter of the through holes on the outer wall of the mesh pipe is larger than the diameter of the molten packing but smaller than the diameter of the main packing.
6. A metal tubular heater with synergistic reinforcement through filler assistance according to claim 1, characterized in that, The metal tubular heater is formed by high-temperature tube shrinking, and the final diameter of the metal tubular heater is smaller than the diameter of the original metal outer tube.
7. A metal tubular heater with synergistic reinforcement through filler assistance according to claim 1, characterized in that, The outer metal tube is made of stainless steel, copper, or nickel-chromium alloy, and the mesh tube is made of nickel-chromium alloy or iron-chromium-aluminum alloy.