A flexible heat-conducting insulating gasket structure
By introducing a sandwich structure of a vertical graphene composite thermal conductive layer and an insulating encapsulation layer into a flexible thermal conductive pad, the problems of poor thermal conductivity and long-term stability in the thickness direction of traditional flexible thermal conductive pads are solved, achieving efficient thermal conductivity and mechanical stability.
Patent Information
- Application Number
- CN202522750367.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2025-12-25
- Publication Date
- 2026-11-24
- Estimated Expiration
- 2035-12-25
AI Technical Summary
Traditional flexible thermal pads have poor thermal conductivity in the thickness direction. Under long-term high temperature and high pressure, the polymer matrix is prone to plastic deformation, resulting in a decrease in contact pressure and an increase in thermal resistance.
The structure employs upper and lower elastic buffer layers composed of silicone rubber layers filled with thermally conductive fillers, with a vertical graphene composite thermally conductive layer in the middle. Vertical graphene sheets are grown on a flexible porous support substrate by chemical vapor deposition and encapsulated with an insulating adhesive layer to form a sandwich structure. Combined with the upper and lower thermally conductive and insulating encapsulation layers, a seamless whole is formed by direct hot pressing.
It significantly reduces thermal resistance in the thickness direction, provides excellent compressibility and elasticity, ensures tight interface adhesion, protects the integrity of the core thermal conductive layer, absorbs and disperses mechanical loads, and improves interface peel strength and long-term performance stability.
Smart Images

Figure CN225020897U_ABST
Abstract
Description
Technical Field
[0001] This utility model relates to the field of thermally conductive insulating pad technology, and in particular to a flexible thermally conductive insulating pad structure. Background Technology
[0002] Thermal pads are high-performance gap-filling thermally conductive materials, mainly used as the interface between electronic devices and heat sinks or product housings. Traditional flexible thermal pads are mostly homogeneous silicone filled with randomly distributed thermally conductive fillers, which have inherent defects; the filler interface has high thermal resistance, and the disordered arrangement of the filler results in poor thermal conductivity in the thickness direction. Under long-term high temperature and high pressure, the polymer matrix is prone to plastic deformation, which leads to a decrease in contact pressure and an increase in thermal resistance over time. Utility Model Content
[0003] To overcome the technical defects of the existing technology, this utility model provides a flexible thermally conductive insulating pad structure.
[0004] The technical solution adopted in this utility model is: a flexible thermally conductive insulating pad structure, including an upper elastic buffer layer and a lower elastic buffer layer composed of a silicone rubber layer filled with thermally conductive filler, a vertical graphene composite thermally conductive layer disposed between the upper elastic buffer layer and the lower elastic buffer layer, the vertical graphene composite thermally conductive layer including a flexible porous support substrate; a graphene sheet perpendicular to its plane is formed in situ grown on the surface of the flexible porous support substrate by chemical vapor deposition; and the porous support substrate and the graphene sheet are encapsulated by an insulating adhesive layer.
[0005] Preferably, the upper surface of the upper elastic buffer layer is provided with an upper thermally conductive insulating encapsulation layer; the lower surface of the lower elastic buffer layer is provided with a lower thermally conductive insulating encapsulation layer.
[0006] Preferably, the lower surface of the upper elastic buffer layer and the upper surface of the lower elastic buffer layer are both provided with an array of three-dimensional protrusions facing downwards.
[0007] Preferably, the height of the three-dimensional protrusion is 50 μm to 200 μm.
[0008] Preferably, the three-dimensional protrusion is hemispherical, truncated conical, or quadrangular pyramidal in shape.
[0009] Preferably, the flexible porous support substrate is one of polyimide nonwoven fabric, electrospun polymer nanofiber membrane, or ceramic fiber paper.
[0010] Preferably, the insulating adhesive layer is a silicone resin filled with thermally conductive filler.
[0011] Preferably, the top ends of the three-dimensional protrusions of the upper and lower elastic buffer layers are bonded to the surface of the vertical graphene composite thermal conductive layer by direct hot pressing.
[0012] The beneficial effects of this utility model are as follows: 1. This utility model uses an upper elastic buffer layer, a lower elastic buffer layer, and a vertical graphene composite thermal conductive layer as the main body to form a pad body, and the three form a sandwich structure. The vertical graphene composite thermal conductive layer constructs a super-high-speed thermal conductive channel from the chip to the heat sink through the graphene sheet, which greatly reduces the thermal resistance in the thickness direction, so that the pad has an ultra-high thermal conductivity in the thickness direction. In addition, by setting the upper elastic buffer layer and the lower elastic buffer layer, the soft silicone rubber matrix and the array-type three-dimensional protrusions provide excellent compressibility and elasticity, ensuring that the interface is tightly fitted, effectively absorbing and dispersing installation stress, vibration and thermal expansion stress, avoiding these mechanical loads from acting directly on the precision vertical graphene structure, and protecting the integrity and long-term effectiveness of the core thermal conductive layer. Attached Figure Description
[0013] One or more embodiments are illustrated by way of example with reference numerals in the accompanying drawings. These illustrations do not constitute a limitation on the embodiments. Elements with the same reference numerals in the drawings are denoted as similar elements. Unless otherwise stated, the figures in the drawings are not to be limited by scale.
[0014] Figure 1 This is a schematic diagram of the overall structure of this utility model; Figure 2 This is a partial structural schematic diagram of the present invention; Figure 3 This is a schematic diagram showing the distribution of the three-dimensional protrusions of this utility model.
[0015] Explanation of reference numerals in the attached figures: 1. Upper elastic buffer layer; 2. Lower elastic buffer layer; 3. Vertical graphene composite thermally conductive layer; 301. Flexible porous support substrate; 302. Graphene sheet; 4. Upper thermally conductive insulating encapsulation layer; 5. Lower thermally conductive insulating encapsulation layer; 6. Three-dimensional protrusion. Detailed Implementation
[0016] To make the objectives, technical solutions, and advantages of this utility model clearer, the various embodiments of this utility model will be described in detail below with reference to the accompanying drawings. However, those skilled in the art will understand that many technical details have been provided in the various embodiments of this utility model to facilitate a better understanding of this application. However, the technical solutions claimed in the claims of this application can be implemented even without these technical details and with various variations and modifications based on the following embodiments.
[0017] like Figures 1 to 3As shown, this embodiment provides a flexible thermally conductive insulating pad structure, with an upper elastic buffer layer 1, a lower elastic buffer layer 2, and a vertical graphene composite thermally conductive layer 3 forming the main body of the pad. The thickness range of the upper elastic buffer layer 1 and the lower elastic buffer layer 2 is 0.3 mm - 1.0 mm (this thickness includes the height of the three-dimensional protrusions), and the thickness range of the vertical graphene composite thermally conductive layer (3) is 0.05 mm - 0.3 mm.
[0018] Both the upper elastic buffer layer 1 and the lower elastic buffer layer 2 use a two-component addition-type thermally conductive silicone rubber as the matrix. High thermal conductivity insulating fillers are incorporated into the silicone rubber matrix, specifically a mixture of spherical alumina (average particle size 5 μm) and lamellar boron nitride (particle size 10-15 μm) in a mass ratio of 7:3. The total volumetric filling rate of the fillers is 60%.
[0019] The vertical graphene composite thermally conductive layer 3 uses a polyimide nonwoven fabric with a thickness of approximately 0.1 mm as a flexible porous support substrate 301, which is arranged in a chemical vapor deposition (CVD) reaction chamber. Methane is used as the carbon source, and hydrogen is used as the carrier gas and etchant, with growth occurring at a reaction temperature of 1050℃. By controlling the growth parameters, vertically oriented graphene sheets (302) are grown in situ on the surface of the three-dimensional fiber network of the nonwoven fabric. The graphene sheets are approximately 25 μm high, with a morphology of few-layer graphene flakes, and are essentially perpendicular to the substrate plane.
[0020] An addition-type liquid silicone resin filled with boron nitride nanosheets is used as the insulating adhesive layer. A vacuum impregnation process is employed to fully impregnate the graphene-grown polyimide nonwoven fabric with the insulating adhesive, ensuring that the gaps between the graphene sheets are completely filled and all exposed graphene tips are covered.
[0021] Curing and shaping: The impregnated composite material was pre-cured in an 80℃ oven for 1 hour, followed by flatbed hot pressing at 150℃ for 10 minutes under a pressure of 0.5 MPa. This process not only fully cured the insulating adhesive, but also flattened the composite layer to a total thickness of approximately 0.25 mm, forming a smooth surface and a vertical graphene composite thermally conductive layer 3 with vertical graphene channels running through it.
[0022] The upper thermally conductive insulating encapsulation layer 4 and the lower thermally conductive insulating encapsulation layer 5 are commercially available polyimide films (PI films) coated on one side with silicone adhesive. The film itself is 0.05 mm thick, and the silicone adhesive layer is approximately 0.01 mm thick. This layer combines high insulation (PI film), high thermal conductivity (which can be achieved by selecting a high thermal conductivity model), and adhesive properties.
[0023] The entire structure is directly thermo-pressed and solidified, removing the semi-cured vertical graphene composite thermally conductive layer 3. Without the need for additional liquid adhesives or coupling agents, the raised surfaces of the fully cured upper elastic buffer layer 1 and lower elastic buffer layer 2 are directly bonded to the upper and lower surfaces of the semi-cured vertical graphene composite thermally conductive layer 3. Similarly, the adhesive surfaces of the upper and lower thermally conductive insulating encapsulation layers 4 and 5 are bonded to the opposite sides of the corresponding buffer layers. The entire five-layer stack is then placed in a thermo-press mold for a one-time final co-curing and solidification. The process parameters are: pressure 1.0 MPa, temperature 160℃, and time 90 minutes. During this process, the semi-cured insulating adhesive 7 and the silicone rubber material undergo interdiffusion and co-crosslinking under high temperature and pressure, forming molecular-level mixing and strong chemical bonds at the interface. Simultaneously, the adhesives of the upper and lower encapsulation insulating layers 4 and 5 also complete their final curing. This method completely eliminates the additional thermal resistance interface caused by the use of separate adhesives between layers, making the internal layers of the gasket a truly seamless whole. Tests show that the interfacial peel strength of this gasket is about 40% higher than that of gaskets using post-bonding processes, and its performance stability under long-term thermal cycling is better.
[0024] Furthermore, any content not described in detail in this specification is existing technology known to those skilled in the art.
[0025] Those skilled in the art will understand that the above embodiments are specific examples of implementing the present invention, and in practical applications, various changes can be made to them in form and detail without departing from the spirit and scope of the present invention.
Claims
1. A flexible thermally conductive insulating pad structure, characterized in that: The system includes an upper elastic buffer layer (1) and a lower elastic buffer layer (2) composed of a silicone rubber layer filled with thermally conductive filler. A vertical graphene composite thermally conductive layer (3) is disposed between the upper elastic buffer layer (1) and the lower elastic buffer layer (2). The vertical graphene composite thermally conductive layer (3) includes a flexible porous support substrate (301). A graphene sheet (302) perpendicular to the plane of the flexible porous support substrate (301) is formed in situ by chemical vapor deposition on the surface of the flexible porous support substrate (301). The porous support substrate (301) and the graphene sheet (302) are encapsulated by an insulating adhesive layer.
2. The flexible thermally conductive insulating pad structure according to claim 1, characterized in that: The upper surface of the upper elastic buffer layer (1) is provided with an upper thermally conductive insulating encapsulation layer (4); the lower surface of the lower elastic buffer layer (2) is provided with a lower thermally conductive insulating encapsulation layer (5).
3. The flexible thermally conductive insulating pad structure according to claim 1, characterized in that: The lower surface of the upper elastic buffer layer (1) and the upper surface of the lower elastic buffer layer (2) are provided with an array of three-dimensional protrusions (6) facing downwards.
4. The flexible thermally conductive insulating pad structure according to claim 3, characterized in that: The height of the three-dimensional protrusion (6) is 50 μm to 200 μm.
5. The flexible thermally conductive insulating pad structure according to claim 3, characterized in that: The three-dimensional protrusion (6) is hemispherical, truncated cone or quadrangular pyramid.
6. The flexible thermally conductive insulating pad structure according to claim 1, characterized in that: The flexible porous support substrate (301) is one of polyimide nonwoven fabric, electrospun polymer nanofiber membrane or ceramic fiber paper.
7. The flexible thermally conductive insulating pad structure according to claim 3, characterized in that: The top of the three-dimensional protrusions (6) of the upper elastic buffer layer (1) and the lower elastic buffer layer (2) are bonded to the surface of the vertical graphene composite thermal conductive layer (3) by direct hot pressing.