Multi-stage shielding device for edge portion of anode plate of surface treatment machine
By designing a multi-level shielding device in the copper foil surface treatment machine, the problem of copper foil edge curling caused by uneven current density of the anode plate was solved. This enabled flexible adjustment of the shielding range and electroplating uniformity, ensuring smooth copper foil winding, improving the stability of the device and reducing costs.
Patent Information
- Application Number
- CN202522671146.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2025-12-17
- Publication Date
- 2026-11-24
- Estimated Expiration
- 2035-12-17
AI Technical Summary
During the copper foil surface treatment process, the uneven current density on both sides of the anode plate leads to uneven electroplating layer thickness, causing copper foil to curl at the edges and making it difficult to rewind. Furthermore, the shielding range is difficult to adjust conveniently according to changes in width and process.
Design a multi-level shielding device, including titanium-clad copper and an anode plate. The mounting plate is equipped with a shielding plate and a side shielding mechanism. The shielding range can be flexibly adjusted through detachable bolt connections and threaded hole adjustments. Countersunk holes are provided on the shielding plate to prevent bolt protrusion from affecting copper foil processing.
It effectively prevents copper foil edge warping, ensures smooth copper foil winding, has an adjustable shielding range, avoids uneven electroplating, improves the stability and reliability of the device, and reduces costs.
Smart Images

Figure CN225020903U_ABST
Abstract
Description
Technical Field
[0001] This utility model relates to the technical field of copper foil post-processing equipment, specifically to a multi-level shielding device for the edge of the anode plate of a surface treatment machine. Background Technology
[0002] The copper foil surface treatment machine mainly consists of an unwinding device, 17 process tanks from pickling to silane treatment (pickling, roughening, curing, roughening, curing, roughening, curing, water washing, blackening, water washing, ashing, water washing, passivation, water washing, water washing, silane treatment), tension control device, speed control device, transmission system, conductive system, spray washing system, drying device, winding device, roller system and submersible roller sealing device, safety / protection device, electrical control cabinet, and frame.
[0003] During the copper foil post-processing, the current density on both sides of the anode plate is greater than that on the inner side, resulting in a thicker electroplated layer on the sides of the copper foil than on the inner side. This causes the edges to curl up during collection on the rollers, affecting the normal winding and slitting of the copper foil. Furthermore, the width of the copper foil and the processing technology may vary from production batch to batch, leading to some differences in the shielding range of the anode plate.
[0004] Therefore, there is an urgent need for a multi-stage shielding device for anode plates that can enhance the shielding effect and be easily adjustable according to different widths. Summary of the Invention
[0005] The purpose of this invention is to overcome the shortcomings of the prior art and provide a multi-level shielding device for the edge of the anode plate of a surface treatment machine.
[0006] The objective of this utility model is achieved through the following technical solution: This utility model provides a multi-level shielding device for the edge of an anode plate of a surface treatment machine, including a titanium-clad copper plate and an anode plate connected to its bottom edge. A mounting plate is connected to one side of the anode plate. Shielding plates are installed along the length of the mounting plate, at its top and bottom. Side shielding mechanisms are detachably installed on both sides of the two shielding plates along the width of the mounting plate, and the installation position of the side shielding mechanisms can be adjusted along the length of the shielding plates.
[0007] Furthermore, each of the shielding plates has countersunk holes at both ends along its length. The mounting plate and the shielding plate are connected and fixed by passing the connecting bolts through the countersunk holes and tightening them into the threaded holes of the mounting plate.
[0008] Furthermore, each of the shielding plates has multiple threaded holes evenly spaced between the countersunk holes at both ends. When the shielding range needs to be adjusted, the side shielding mechanism is moved to the corresponding threaded hole as required and connected and fixed to the anode plate by connecting bolts.
[0009] Furthermore, the side shielding mechanism includes a base plate with a mountain-shaped structure. The base plate has dovetail grooves symmetrically formed on both sides with the central boss as the center. A lip seal is provided in the dovetail groove. A PTFE strip is provided on the top of the boss, and the upper end of the lip seal passes through the PTFE strip. A clamping strip is provided on the top of the PTFE strip, which coincides with the position of the boss. The clamping strip has multiple countersunk holes, and the clamping strip is connected and fixed to the boss by multiple connecting bolts.
[0010] Furthermore, the boss is provided with through holes corresponding to the countersunk holes at both ends of the clamping strip, and the connecting bolts are connected to the threaded holes on the shielding plate by passing through the countersunk holes and through holes.
[0011] Furthermore, the multi-level shielding device also includes an upper clip and a lower clip with the same structure. The upper clip has a U-shaped structure and a threaded hole on one side. The upper clip is used to clamp the titanium-clad copper and the top shielding plate and fix them through the connector. The lower clamp is used to hold the anode plate and the bottom shielding plate and is fixed by the connector.
[0012] Compared with the prior art, the technical solution provided by this utility model has the following beneficial effects: 1. The device of this utility model is used to prevent the edges of the surface-treated copper foil from warping and affecting the winding, and to shield the copper foil according to the surface treatment process. This device is a purely mechanical structure, which is simpler in structure, easier to install, and more stable and reliable while saving costs.
[0013] 2. By installing shielding plates at the top and bottom of the anode plate and opening uniformly threaded holes on the shielding plates, and installing side shielding mechanisms on the left and right sides of the anode plate, when the width of the copper foil or the process changes and the shielding area needs to be adjusted, the side shielding mechanism is moved to the corresponding threaded hole and the installation position is changed by using hexagonal screws or titanium hexagonal screws. Additionally, a top shielding plate is installed because the anode plate and titanium-clad copper are assembled at the top using titanium bolts. The presence of these bolts can cause uneven surface composition on the anode plate in this area. Therefore, the top shielding plate is used to prevent uneven electroplating when the copper foil passes through this area. The inlet for the electroplating solution is located at the bottom of the tank. The ion concentration of the newly added electroplating solution differs from that of other areas in the tank. Therefore, a shielding plate is installed at the bottom of the anode plate to ensure that the newly added solution is fully mixed with the tank solution before initiating the electrochemical reaction.
[0014] 3. Countersunk holes are made at both ends of the top and bottom shielding plates, as well as on the top of the side shielding mechanism. The countersunk holes are designed so that the surface will not protrude after the screws or bolts are installed, thus avoiding contact with the copper foil during processing and affecting the processing quality. Attached Figure Description
[0015] The accompanying drawings are incorporated in and form part of this specification, and together with the description, serve to explain the principles of this invention.
[0016] To more clearly illustrate the technical solutions in the embodiments of this utility model or the prior art, the drawings used in the description of the embodiments or the prior art will be briefly introduced below. Obviously, for those skilled in the art, other drawings can be obtained based on these drawings without creative effort.
[0017] Figure 1 This is a schematic diagram of the overall structure of the multi-level shielding device of this utility model; Figure 2 This is a front view of the multi-level shielding device of this utility model; Figure 3 This is a right view of the multi-level shielding device of this utility model; Figure 4 This is a schematic diagram of the side shielding mechanism of the multi-level shielding device of this utility model; Figure 5 This is a side view of the side shielding mechanism of this utility model.
[0018] Wherein: 1 is titanium-clad copper; 2 is anode plate; 3 is shielding plate; 4 is side shielding mechanism; 41 is base plate; 411 is boss; 412 is dovetail groove; 42 is lip seal; 43 is PTFE strip; 44 is clamping strip; 5 is mounting plate; 6 is upper clamp; 7 is lower clamp. Detailed Implementation
[0019] Exemplary embodiments will now be described in detail, examples of which are illustrated in the accompanying drawings. When the following description relates to the drawings, unless otherwise indicated, the same numerals in different drawings denote the same or similar elements. The embodiments described in the following exemplary embodiments do not represent all embodiments consistent with this invention. Rather, they are merely examples of apparatuses consistent with some aspects of this invention as detailed in the appended claims.
[0020] To enable those skilled in the art to better understand the technical solution of this utility model, the present utility model will be further described in detail below with reference to the accompanying drawings and embodiments.
[0021] See Figures 1-5This embodiment provides a multi-level shielding device for the edge of an anode plate of a surface treatment machine, including a titanium-clad copper 1 and an anode plate 2 connected to its bottom edge. A mounting plate 5 is connected to the front of the anode plate 2. UPVC shielding plates 3 are installed along the length of the mounting plate 5, at its top and bottom. Side shielding mechanisms 4 are detachably installed on both sides of the two shielding plates 3 along the width of the mounting plate 5, and the installation position of the side shielding mechanisms 4 can be adjusted along the length of the shielding plates 3.
[0022] Among them, the titanium-clad copper 1 has a U-shaped structure with both ends of the top extending outwards. The anode plate 2 is attached to the lower surface of the titanium-clad copper 1. The anode plate 2 is connected and fixed to the titanium-clad copper 1 by the cooperation of the anode stud and the anode fastening nut.
[0023] like Figure 1 As shown, each of the shielding plates 3 has countersunk holes at both ends along its length. Titanium bolts pass through the countersunk holes and are inserted into the threaded holes of the mounting plate 5 to tighten them, thereby connecting and fixing the mounting plate 5 and the shielding plate 3.
[0024] Optionally, the titanium bolt passes through the countersunk hole, the threaded hole of the mounting plate 5, and is threadedly connected to the anode plate 2 for fixation; or the titanium bolt passes through the countersunk hole, the threaded hole of the mounting plate 5, and the through hole on the anode plate 2 and is then locked with a nut.
[0025] like Figure 1 As shown, each of the shielding plates 3 has multiple threaded holes evenly distributed between the countersunk holes at both ends. When the shielding range needs to be adjusted (such as adjusting the shielding area according to the changes in the copper foil width or the copper foil post-processing process), the side shielding mechanism 4 is moved to the corresponding threaded hole as required and connected and fixed to the anode plate 2 by internal hexagonal titanium bolts or internal hexagonal titanium screws.
[0026] like Figure 4 and 5 As shown, the side shielding mechanism 4 includes a UPVC substrate 41 with a mountain-shaped structure. Dovetail grooves 412 are symmetrically formed on both sides of the central boss 411 on the substrate 41. A lip seal 42 made of EPDM rubber is provided in the dovetail groove 412. A PTFE strip 43 (polytetrafluoroethylene) is provided on the top of the boss 411, and the upper end of the lip seal 42 passes through the PTFE strip 43. A clamping strip 44 is provided on the top of the PTFE strip 43, which coincides with the position of the boss 411. The clamping strip 44 has multiple countersunk holes and is connected and fixed to the boss 411 by multiple hexagonal titanium screws.
[0027] Furthermore, the boss 411 has through holes corresponding to the countersunk holes at both ends of the clamping strip 44. An internal hexagon bolt is passed through the countersunk hole and the through hole to be threaded into the threaded hole on the shielding plate 3. The internal hexagon bolt is installed in the countersunk hole to prevent the bolt head from protruding and contacting the copper foil, which could then damage the copper foil. In addition, the side shielding mechanism 4 can be installed and fixed on the threaded hole corresponding to the width of the copper foil that needs to be shielded.
[0028] In this embodiment, the clamping strip 44 is made of UPVC material.
[0029] The multi-level shielding device also includes an upper clip 6 and a lower clip 7 with the same structure. The upper clip 6 has a U-shaped structure and a threaded hole on its back. The upper clip 6 is used to clamp the titanium-clad copper 2 and the top shielding plate 3 and fix them with external hexagonal screws. Specifically, the external hexagonal screws are passed through the threaded hole and inserted into the threaded hole of the titanium-clad copper 1, so that the back of the upper clip 6 is connected and fixed to the titanium-clad copper 2. The lower clamp 7 is used to clamp the anode plate 2 and the bottom shielding plate 3 and is fixed by external hexagonal screws. The connection method is the same as that of the upper clamp 7.
[0030] The installation method of this utility model is as follows: Place the anode plate 2 and the titanium-clad copper 1 according to the corresponding holes, and tighten the anode bolts through the holes and the anode nuts to complete the connection and fixation. Connect the PVC plate (mounting plate) to the front of the anode plate 2 with hexagonal titanium screws. Place the top and bottom shielding plates 3 on the PVC plate according to the corresponding holes, and install the hexagonal titanium screws in the threaded holes of the PVC plate and tighten them. Insert the lip seal 42 into the dovetail groove 412 of the substrate 41, and then place the PTFE strip 43 and the clamping strip 44 on the upper surface of the substrate 41 according to the corresponding holes. Then install the countersunk hexagonal screws in the multiple threaded holes of the substrate 41 and tighten them in sequence to connect and fix the PTFE strip 43 and the clamping strip 44 to the substrate 41. The upper clamp 6 holds the titanium cladding cylinder 2 and the top shielding plate 3; the lower clamp 7 holds the anode plate 2 and the bottom shielding plate 3, and connect the upper clamp 6 to the back of the titanium cladding cylinder 2 with hexagonal screws; connect the lower clamp 7 to the anode plate 2.
[0031] The above description is merely a specific embodiment of this utility model, enabling those skilled in the art to understand or implement it. Various modifications to these embodiments will be readily apparent to those skilled in the art, and the general principles defined herein may be implemented in other embodiments without departing from the spirit or scope of this utility model.
[0032] It should be understood that this utility model is not limited to the content already described above, and various modifications and changes can be made without departing from its scope. The scope of this utility model is limited only by the appended claims.
Claims
1. A multi-stage shielding device for the edge of an anode plate in a surface treatment machine, comprising a titanium-clad copper plate (1) and an anode plate (2) connected to its bottom edge, characterized in that, A mounting plate (5) is connected to one side of the anode plate (2). Shielding plates (3) are installed along the length of the mounting plate (5), at its top and bottom. Side shielding mechanisms (4) are detachably installed on both sides of the two shielding plates (3) along the width of the mounting plate (5). The installation position of the side shielding mechanisms (4) can be adjusted along the length of the shielding plates (3).
2. The multi-stage shielding device for the edge of the anode plate of the surface treatment machine according to claim 1, characterized in that, Each of the shielding plates (3) has countersunk holes at both ends along its length. The mounting plate (5) and the shielding plate (3) are connected and fixed by passing the connecting bolts through the countersunk holes and tightening them into the threaded holes of the mounting plate (5).
3. The multi-stage shielding device for the edge of the anode plate of the surface treatment machine according to claim 2, characterized in that, On each of the shielding plates (3), multiple threaded holes are evenly provided between the countersunk holes at both ends. When the shielding range needs to be adjusted, the side shielding mechanism (4) is moved to the corresponding threaded hole as required and connected and fixed to the anode plate (2) by connecting bolts.
4. The multi-stage shielding device for the edge of the anode plate of the surface treatment machine according to claim 1, characterized in that, The side shielding mechanism (4) includes a base plate (41) with a mountain-shaped structure. The base plate (41) has dovetail grooves (412) symmetrically opened on both sides with the boss (411) in the middle as the center. The dovetail groove (412) is provided with a lip seal (42). The top of the boss (411) is provided with a PTFE strip (43), and the upper end of the lip seal (42) passes through the PTFE strip (43). The top of the PTFE strip (43) is provided with a pressing strip (44) that coincides with the position of the boss (411). The pressing strip (44) is provided with multiple countersunk holes. The pressing strip (44) is connected and fixed to the boss (411) by multiple connecting bolts.
5. The multi-stage shielding device for the edge of the anode plate of the surface treatment machine according to claim 4, characterized in that, The boss (411) has through holes corresponding to the countersunk holes at both ends of the clamping strip (44), and the connecting bolts are connected to the threaded holes on the shielding plate (3) by passing through the countersunk holes and through holes.
6. The multi-stage shielding device for the edge of the anode plate of the surface treatment machine according to claim 1, characterized in that, The multi-level shielding device also includes an upper clip (6) and a lower clip (7) with the same structure. The upper clip (6) has a U-shaped structure and a threaded hole on one side. The upper clip (6) is used to hold the titanium-clad copper (1) and the top shielding plate (3) and fix them by connectors. The lower clamp (7) is used to clamp the anode plate (2) and the bottom shielding plate (3) and is fixed by the connector.