A solar cell and photovoltaic module

By designing a first textured structure with a width ratio of less than 3% and an overlapping recessed structure on the side of the semiconductor substrate of the solar cell, combined with a wave shape and a specific angle, the problem of low efficiency of existing solar cells is solved, and higher photoelectric conversion efficiency is achieved.

CN225020934UActive Publication Date: 2026-11-24LONGI PHOTOVOLTAIC TECHNOLOGY (ORDOS) CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202522758721.5
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2025-12-25
Publication Date
2026-11-24
Estimated Expiration
2035-12-25

AI Technical Summary

Technical Problem

The low efficiency of existing solar cells is mainly due to the non-uniformity of the side textured structure and the high recombination rate, which leads to poor passivation effect of the passivation layer and affects the photoelectric conversion efficiency.

Method used

The side of the semiconductor substrate is designed as a first textured structure region and a second textured structure region. The first textured structure region has a width ratio of less than 3%, and the second textured structure region is a recessed structure. The overlapping recessed structures have better surface flatness and passivation layer deposition thickness. Combined with the wave shape and specific angle design, the carrier recombination rate is reduced.

Benefits of technology

This improved the passivation quality and uniformity of the passivation layer, reduced the carrier recombination rate, enhanced photoelectric conversion efficiency, and improved the cell efficiency of solar cells.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN225020934U_ABST
    Figure CN225020934U_ABST
Patent Text Reader

Abstract

This utility model discloses a solar cell and a photovoltaic module, relating to the field of solar cell technology, to solve the problem of how to improve the cell efficiency of solar cells. The solar cell includes a semiconductor substrate and a passivation layer. The semiconductor substrate includes a first surface and a second surface opposite to each other, and a plurality of side surfaces connecting the first surface and the second surface. Along the direction from the first surface to the second surface, the side surfaces include a first textured structure region and a second textured structure region, the first textured structure region being close to the first surface. The first textured structure region has a first textured structure, and the second textured structure region includes a plurality of recessed structures. The size of the first textured structure is smaller than the size of the recessed structures, and the ratio of the width of the first textured structure region to the total width of the side surfaces is less than or equal to 3%. The passivation layer is formed at least on the side surfaces.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This utility model relates to the field of solar cell technology, and in particular to a solar cell and a photovoltaic module. Background Technology

[0002] A solar cell is a device that utilizes solar energy to directly convert light energy into electrical energy through the photoelectric effect or photochemical effect.

[0003] Current solar cells mainly include IBC cells (Interdigitated Back Contact), TOPCon (Tunnel Oxide Passivated Contact) cells, PERC cells (Passivated emitter and real cell), hybrid HBC (Hybrid Back Contact) cells, heterojunction cells, and bifacial solar cells.

[0004] Currently, improving the efficiency of solar cells is a pressing technical problem that the industry needs to solve. Utility Model Content

[0005] The purpose of this invention is to provide a solar cell and a photovoltaic module for improving the cell efficiency of solar cells.

[0006] To achieve the above objectives, in a first aspect, the present invention provides a solar cell. The solar cell includes a semiconductor substrate and a passivation layer. The semiconductor substrate includes a first surface and a second surface opposite to each other, and a plurality of side surfaces connecting the first surface and the second surface. Along the direction from the first surface to the second surface, the side surfaces include a first textured structure region and a second textured structure region, the first textured structure region being close to the first surface. The first textured structure region has a first textured structure, and the second textured structure region includes a plurality of recessed structures. The size of the first textured structure is smaller than the size of the recessed structures, and the ratio of the width of the first textured structure region to the total width of the side surfaces is less than or equal to 3%. The passivation layer is formed at least on the side surfaces.

[0007] In the solar cell provided by this invention, compared with the first textured structure, the recessed structure has better surface smoothness, which is beneficial to improving the passivation quality of the passivation layer. The rough surface of the first textured structure leads to a poorer passivation effect and a higher surface recombination rate, while the recessed structure ensures a higher passivation effect. Furthermore, the deposition thickness of the film is inversely proportional to the specific surface area of ​​the surface on which it is deposited. Therefore, compared with the first textured structure, the passivation layer formed on the recessed structure is thicker and more uniform, which is beneficial to enhancing the passivation effect of the passivation layer at the recessed structure, further reducing the carrier recombination rate in the region where the recessed structure is located, and improving the photoelectric conversion efficiency of the solar cell. Furthermore, the ratio of the width of the first textured structure region to the total width of the side surface is less than or equal to 3%, and the proportion of the first textured structure region is relatively small. This is more conducive to the formation of the passivation layer, improving the passivation effect, and thus improving the cell efficiency of the solar cell.

[0008] In one implementation, at least some of the recessed structures are overlapped, and the height difference between the bottom surfaces of adjacent recessed structures at the overlap position is less than 2 μm.

[0009] The overlapping arrangement of at least some of the recessed structures makes the passivation layer formed on the surface of the recessed structure more uniform, the film quality of the passivation layer is better, and the density of the passivation layer is better, thereby improving the passivation effect of the solar cell.

[0010] In one implementation, the side of the first texture structure region closest to the second surface is wavy; the distance between the crests and troughs of the wavy shape along the direction from the first surface to the second surface is 0.5 μm to 2 μm.

[0011] Therefore, the regularity of the wave shape leads to better film formation quality at the interface between the first and second textured structure regions, resulting in a more uniform and orderly film. Furthermore, edge recombination of charge carriers occurs on the side of the first textured structure region closer to the second surface, and the magnitude of the recombination current is directly related to the edge length. Smooth edges and low roughness can reduce the length of the edge region, decrease charge carrier recombination, and improve battery performance. Therefore, when the distance between the peaks and troughs of the wave shape meets the above-mentioned value range, the length of the edge region can be reduced, charge carrier recombination can be decreased, and battery performance can be improved.

[0012] In one implementation, along the direction from the first surface to the second surface, the second textured structure region includes a central region and two edge regions, with multiple recessed structures arranged along a first straight line. Within the central region, the angle between the first straight line and the side edge of the side surface is less than or equal to 30°. Within the edge regions, the angle between the first straight line and the side edge of the side surface is between 30° and 60°, and the side edge of the side surface is parallel to the first surface.

[0013] When the aforementioned two included angles are within the specified range, the capillary effect can be reduced or eliminated. This reduces or eliminates the probability that water sprayed on the front of the solar cell during cleaning is drawn to the back of the solar cell, thereby reducing the proportion of the first textured structure region. Based on this, it is more conducive to the formation of the passivation layer, improving the passivation effect and thus increasing the cell efficiency of the solar cell.

[0014] In one implementation, the solar cell further includes: A first doped conductive layer is formed on the first surface and the first textured structure region; The second doped conductive layer is formed at least on a portion of the second surface and a portion of the second textured structure region; the first doped conductive layer and the second doped conductive layer have opposite conductivity types. The passivation layer located on the side is formed on the side of the first doped conductive layer and the second doped conductive layer that is away from the semiconductor substrate.

[0015] At this point, the first texture structure region and the second texture structure region do not overlap, thus preventing leakage caused by doped conductive layers with opposite polarities overlapping on the side of the semiconductor substrate.

[0016] In one implementation, the second surface includes a non-electrode region having a third texture structure, the third texture structure including a recessed structure, the size of the recessed structure located in the second texture structure region being larger than the size of the recessed structure located in the non-electrode region.

[0017] Because the side of the battery retains either a first or second doped conductive layer, as well as a first and second textured structure region, the surface morphology of the side is quite complex. Therefore, designing a recessed structure on the side of the solar cell with a surface size larger than that of the third textured structure can improve the quality of the passivation layer film formation on the side, enhance its passivation effect, and thus increase the power on the back of the solar cell and improve the bifaciality of the solar cell by reducing the carrier recombination probability.

[0018] In one implementation, the one-dimensional size of the orthographic projection of the recessed structure located in the second textured structure region onto the semiconductor substrate is 15 μm to 40 μm; the one-dimensional size of the orthographic projection of the recessed structure located in the non-electrode region onto the semiconductor substrate is 8 μm to 20 μm.

[0019] When adopting the technical solution, if the surface size of the recessed structure located in the second texture structure region and the recessed structure located in the non-electrode region is too large, the surface undulation will be too gentle, which is not conducive to the coating quality. For example, the passivation layer is prone to cracking. By setting the surface size of the recessed structure within the above range, it is possible to reduce the cracking phenomenon and increase the coating area of ​​the passivation layer to improve the passivation performance.

[0020] In one implementation, the depth of the recessed structure located in the second texture structure region is 0.1 μm to 3 μm.

[0021] When the depth of the recessed structure in the second textured structure region exceeds 3 μm, the roughness of the recessed structure is too large. This results in a larger thickness and poorer uniformity of the doped conductive and passivation layers formed on the recessed structure, which is detrimental to the formation of high-density and high-uniformity doped conductive and passivation layers. However, setting the depth of the recessed structure within the aforementioned range can prevent excessively thick local film layers caused by the doped conductive and passivation layers, thereby improving the open-circuit voltage of the solar cell and enhancing the fill factor and photoelectric conversion efficiency.

[0022] In one implementation, the solar cell further includes a tunneling layer located between the semiconductor substrate and the second doped conductive layer; the second doped conductive layer is a doped polycrystalline silicon layer.

[0023] In this technical solution, the tunneling layer is located between the semiconductor substrate and the second doped conductive layer, and the second doped conductive layer is formed at least on the second surface and the second textured structure region. This allows for passivation of the sides corresponding to the second surface and the second textured structure region of the semiconductor substrate, reducing the carrier recombination rate. Furthermore, all other factors being equal, compared to textured structures with large undulations such as pyramidal velvet structures, the undulations of the recessed structure without a pyramidal tip are relatively smaller, which is beneficial for improving the formation quality and film thickness of the tunneling layer, thereby enhancing the passivation effect of the tunneling layer on the semiconductor substrate and improving the conversion efficiency of the solar cell. In addition, the recessed structure with a certain depth on the second textured structure region increases the specific surface area of ​​the semiconductor substrate, thereby increasing the contact area between the sides and the tunneling layer. This helps to saturate the dangling bonds of the semiconductor substrate, reducing recombination losses, thus improving the passivation effect of the solar cell and further improving the cell efficiency. Furthermore, the tunneling layer and the second doped conductive layer together form a tunneling passivation contact structure, which, while achieving efficient carrier transport, further enhances the passivation effect on the semiconductor substrate surface.

[0024] In one implementation, the first texture structure includes one or more of the following: a prismatic structure, an inverted pyramid structure, a frustum structure, or a pyramidal structure.

[0025] When employing the technical solution, if the first texture structure includes a pyramid structure or an inverted pyramid structure, compared to a recessed texture structure that predominates on a larger planar proportion (typically 100 crystal planes), the pyramid or inverted pyramid will expose more slopes of the 111 crystal planes. Therefore, the pyramid or inverted pyramid structure not only increases the contact area between the tunneling layer and different crystal planes of the semiconductor substrate, providing more transport paths for charge carriers, but the apex of the inverted pyramid is also more conducive to enhancing the electron tunneling effect.

[0026] In one implementation, a first surface of the semiconductor substrate has a first edge, and a first isolation region is formed between the boundary of the first doped conductive layer adjacent to the first edge and the first edge.

[0027] In the case of the adopted technical solution, the first isolation region separates the boundary of the first doped conductive layer adjacent to the first edge from the first edge, so as to help suppress leakage current.

[0028] In one implementation, the first isolation region has a fourth texture structure, which includes a recessed structure.

[0029] When the technical solution is adopted, a recessed structure is formed on the surface of the first isolation region, which makes the coating quality of the subsequent passivation layer better. While ensuring edge passivation, the insulating properties of the passivation layer can guarantee the electrical isolation between the first doped conductive layer and the second doped conductive layer.

[0030] In one implementation, the second surface includes a non-electrode region having a third texture structure, the third texture structure including a recessed structure, the size of the recessed structure located in the first isolation region being smaller than the size of the recessed structure located in the non-electrode region.

[0031] With the adoption of the technical solution, the size of the recessed structure in the first isolation region is small. While ensuring flatness and improving the passivation effect when the passivation layer is grown subsequently, it can reduce the reflectivity of the first isolation region and reduce the current drop caused by changes in surface state. The insulating properties of the passivation layer can ensure electrical isolation between the first doped conductive layer and the second doped conductive layer.

[0032] In one implementation, the ratio of the size of the recessed structure located in the first isolation region to the size of the recessed structure located in the non-electrode region is 0.5:1 to 1:1. The bottom surface dimension of the recessed structure located in the first isolation region is 4 μm to 10 μm.

[0033] With the adoption of the technical solution, the smaller size of the recessed structure in the first isolation area can reduce the surface reflectivity and reduce the impact on the current while ensuring the passivation effect. At the same time, the smaller recess means lower laser energy, which can use a lower power laser or increase the laser power output. The complete removal of the PN junction and the non-conductive passivation film ensure electrical isolation between the front and back sides.

[0034] In one implementation, the second surface of the semiconductor substrate has a second edge, and a second isolation region is formed between the boundary of the second doped conductive layer adjacent to the second edge and the second edge.

[0035] In the case of the adopted technical solution, the second isolation region separates the boundary of the second doped conductive layer adjacent to the second edge from the second edge, so as to help suppress leakage current.

[0036] It should be noted that, as described above, the so-called isolation regions (first isolation region and second isolation region) are areas where electron / hole collection does not occur. These regions do not contribute current, or there are no doped conductive layers (first doped conductive layer and second doped conductive layer) in these regions, and therefore no photocurrent is generated or collected. These isolation regions separate the boundaries of the doped conductive layers from the edges of the semiconductor substrate to ensure electrical insulation.

[0037] In one implementation, the second doped conductive layer is also formed on the first doped conductive layer located in the first texture structure region and on the first doped conductive layer located in the edge region of the first surface.

[0038] With the adopted technical solution, in the case of forming an isolation zone at the edge of the battery cell, the second doped conductive layer is formed in the first textured structure region or even the edge region of the first surface. This achieves good passivation of the battery side while ensuring no leakage. The first doped conductive layer remains on the surface of the first textured region, and the second doped conductive layer can form a partial field passivation effect in the first textured structure region. Combined with subsequent passivation layers, this can achieve good passivation near the side edge.

[0039] In one implementation, each corner in the bottom surface of the recessed structure includes at least one or more of the following: a rounded corner, a sharp corner, a rounded corner, or a sharp corner.

[0040] When employing the technical solution, if all corners are rounded or semi-rounded, the transition of the rounded or semi-rounded corners on the bottom surface is smoother and flatter compared to when all corners are sharp or semi-sharp. This makes the boundary transition of the recessed structure at the rounded or semi-rounded corners more gradual and blurred, resulting in a relatively flat surface on the side of the passivation layer facing away from the semiconductor substrate from a macroscopic perspective. This is beneficial for improving the formation quality and film thickness of the passivation layer, thereby enhancing the passivation effect of the passivation layer on the semiconductor substrate and improving the conversion efficiency of the solar cell.

[0041] When all corners are sharp or pointed, compared to when all corners are rounded or rounded, the transition of sharp or pointed corners is more obvious and the degree of undulation is greater. This is beneficial to increase the specific surface area of ​​the side of the second doped conductive layer away from the semiconductor substrate, thereby increasing the contact area between the subsequent second doped conductive layer and the electrode, improving the contact performance between the second doped conductive layer and the electrode, as well as the adhesion and shaping of the electrode on the second doped conductive layer, which is beneficial to improving the conversion efficiency of the solar cell.

[0042] Secondly, this utility model also provides a photovoltaic module, including a battery string and an encapsulation layer. The battery string includes multiple interconnecting elements and multiple solar cells as described in the above technical solution; the interconnecting elements are used to connect multiple solar cells in series to form a battery string, and the encapsulation layer is used to cover the surface of the battery string.

[0043] The beneficial effects of the photovoltaic module provided by this utility model are the same as those of the solar cell described in the above technical solution, and will not be repeated here. Attached Figure Description

[0044] The accompanying drawings, which are included to provide a further understanding of the present invention and constitute a part of this invention, illustrate exemplary embodiments of the present invention and, together with the description thereof, serve to explain the present invention and do not constitute an undue limitation thereof. In the drawings: Figure 1 This is a SEM image of the side of a solar cell in the prior art; Figure 2 This is a SEM image of the side of the solar cell in an embodiment of this utility model; Figure 3 This is a cross-sectional view of the solar cell in an embodiment of the present invention; Figure 4 This is a cross-sectional view of the first type of solar cell in this embodiment of the present invention; Figure 5 This is a cross-sectional view of the second type of solar cell in this embodiment of the present invention; Figure 6 This is a cross-sectional view of the recessed structure in an embodiment of the present invention. Figure 1 ; Figure 7 This is a cross-sectional view of the recessed structure in an embodiment of the present invention. Figure 2 ; Figure 8 This is a cross-sectional view of the recessed structure in an embodiment of the present invention. Figure 3 .

[0045] Figure label: 1-Semiconductor substrate, 10-First surface, 11-Second surface, 110-Non-electrode region, 12-Side surface; 2-Second doped conductive layer, 3-Passivation layer, 30-Alumina passivation layer, 31-Silicon nitride passivation layer; 4-First textured structure region, 40-First textured structure; 5-Second textured structure region, 51-Recessed structure, 52-Top opening, 53-Bottom surface, 54-Sidewall; 6-Tunneling layer, 7-First isolation region, 8-Second isolation region, 90-First electrode, 91-Second electrode, 92-Textured structure, 93-First doped conductive layer. Detailed Implementation

[0046] To facilitate a clear description of the technical solutions of the embodiments of this utility model, the terms "first" and "second" are used in the embodiments of this utility model to distinguish identical or similar items with essentially the same function and effect. For example, the first threshold and the second threshold are only used to distinguish different thresholds and do not limit their order. Those skilled in the art will understand that the terms "first" and "second" do not limit the quantity or execution order, and the terms "first" and "second" are not necessarily different.

[0047] It should be noted that in this utility model, the terms "exemplary" or "for example" are used to indicate examples, illustrations, or descriptions. Any embodiment or design scheme described as "exemplary" or "for example" in this utility model should not be construed as being more preferred or advantageous than other embodiments or design schemes. Specifically, the use of terms such as "exemplary" or "for example" is intended to present the relevant concepts in a specific manner.

[0048] In this invention, "at least one" refers to one or more, and "more than one" refers to two or more. "And / or" describes the relationship between related objects, indicating that three relationships can exist. For example, A and / or B can represent: A alone, A and B simultaneously, or B alone, where A and B can be singular or plural. The character " / " generally indicates that the preceding and following related objects are in an "or" relationship. "At least one of the following" or similar expressions refer to any combination of these items, including any combination of single or plural items. For example, at least one of a, b, or c can represent: a, b, c, a combination of a and b, a combination of a and c, a combination of b and c, or a, b, and c, where a, b, and c can be single or multiple.

[0049] See the background section for more details. Figure 1Currently, in conventional TOPCon battery manufacturing processes, the sides of the battery still retain a textured structure 92, and the area of ​​the textured structure 92 is relatively large. Furthermore, due to the severe influence of side line marks, different areas exhibit different residual morphologies and residual proportions. At the same time, the PN junctions at the textured residual locations are not removed, resulting in a significant decrease in passivation performance. The side of the battery has a low degree of optical response, requiring better passivation to reduce surface recombination on the side.

[0050] The above problem may be caused by the following: During the manufacturing process of solar cells, when processing the sides of the solar cells, an abrasive wheel is used to polish the sides, resulting in abrasion marks. Subsequently, during chain cleaning, a water film (a non-reactive solution that protects the front structure) is sprayed downwards from the front of the solar cell. Due to the capillary action of the abrasion marks, the liquid has surface tension, causing the water film to move towards the back of the solar cell, resulting in the black area shown in the image (e.g., [image of a black area]). Figure 1 Region A in the diagram is protected by a water film, and the textured surface structure 92 in this region was not removed, and there may even be residual PN junctions. Alternatively, when cleaning the side of the solar cell, the cleaning solution did not come into contact with the black area in the diagram, resulting in the textured surface structure 92 in this region not being removed, and there may even be residual PN junctions.

[0051] To address the aforementioned technical problems, in a first aspect, this utility model provides a solar cell. The solar cell can be a back-contact solar cell, a bifacial solar cell, a hybrid HBC (Hybrid BackContact) cell, a hybrid back-contact cell, or a tunneling oxide passivation back-contact cell, etc. HBC stands for back-contact heterojunction solar cell, wherein one electrode of the hybrid HBC cell is a heterojunction passivation structure, and the other electrode is a tunneling oxide passivation structure.

[0052] See Figures 2 to 7 The solar cell includes a semiconductor substrate 1 and a passivation layer 3. The semiconductor substrate 1 includes a first surface 10 and a second surface 11 opposite to each other, and a plurality of side surfaces 12 connecting the first surface 10 and the second surface 11. Along direction B from the first surface 10 to the second surface 11, the side surfaces 12 include a first textured structure region 4 and a second textured structure region 5, the first textured structure region 4 being close to the first surface 10. The first textured structure region 4 has a first textured structure 40, and the second textured structure region 5 includes a plurality of recessed structures 51. The size of the first textured structure 40 is smaller than the size of the recessed structures 51, and the ratio of the width W1 of the first textured structure region 4 to the total width W2 of the side surfaces 12 is less than or equal to 3%. For example, the ratio of the width W1 of the first textured structure region 4 to the total width W2 of the side surfaces 12 can be 3%, 2.8%, 2.5%, 2%, 1.8%, 1.5%, 1.3%, 1%, 0.8%, 0.5%, or 0.1%, etc.

[0053] See Figures 1 to 7 In the solar cell provided by this embodiment, compared with the first textured structure 40, the recessed structure 51 has better surface smoothness, which is beneficial to improving the passivation quality of the passivation layer 3. The rough surface of the first textured structure 40 leads to a poor passivation effect of the passivation layer 3 and causes higher surface recombination, while the recessed structure 51 can ensure that the passivation layer has a higher passivation effect. Furthermore, the deposition thickness of the film layer is inversely proportional to the specific surface area of ​​the surface on which it is deposited. Therefore, compared with the first textured structure 40, the passivation layer 3 formed on the recessed structure 51 is thicker and more uniform, which is beneficial to enhance the passivation effect of the passivation layer 3 at the recessed structure 51, further reducing the carrier recombination rate in the region where the recessed structure 51 is located, and improving the photoelectric conversion efficiency of the solar cell. In addition, the ratio of the width of the first textured structure region 4 to the total width of the side 12 is less than or equal to 3%, and the proportion of the first textured structure region 4 is relatively small. At this time, it is more conducive to the formation of the passivation layer 3, improving the passivation effect, thereby improving the cell efficiency of the solar cell. Furthermore, the ratio of the width of the first texture structure region 4 to the total width of the side 12 cannot be 0, because at this time the reaction solution on the side will overflow to the edge of the first surface, destroying the velvet structure of the edge of the first surface and damaging the light trapping effect on the first surface.

[0054] In terms of shape, the first surface 10 and the second surface 11 of the semiconductor substrate 1 may have the same shape or different shapes. In this embodiment of the present invention, the first surface 10 and the second surface 11 have the same shape. For example, the shape of the first surface 10 or the second surface 11 may be a square, a rectangle, a rounded square, a circle, etc.

[0055] In terms of materials, a semiconductor substrate can be any semiconductor material such as a silicon substrate, a germanium-silicon substrate, a germanium substrate, or a gallium arsenide substrate.

[0056] In terms of conductivity type, the semiconductor substrate can be an intrinsically conductive substrate, an N-type conductive substrate, or a P-type conductive substrate. Preferably, the semiconductor substrate is a P-type conductive substrate or an N-type conductive substrate. Compared with an intrinsically conductive substrate, a P-type conductive substrate or an N-type conductive substrate has better conductivity, resulting in a lower bulk resistivity in the final solar cell, thereby improving the efficiency of the solar cell. For example, the semiconductor substrate is an N-type silicon substrate. Compared with a P-type conductive substrate, an N-type silicon substrate has advantages such as higher minority carrier lifetime, no light decay, and better performance in low-light conditions.

[0057] In terms of light reception, when the first surface 10 is the light-facing surface, the second surface 11 is the shadow-facing surface. Alternatively, when the first surface 10 is the shadow-facing surface, the second surface 11 is the light-facing surface.

[0058] The light-facing surface of the semiconductor substrate 1 can be a plane, or the light-facing surface of the semiconductor substrate 1 (e.g., the first surface 10) can be a textured surface. Since a textured surface has a light-trapping effect, when the light-facing surface of the semiconductor substrate 1 is textured, the reflectivity of the light-facing surface can be reduced, allowing more light to be refracted from the light-facing surface into the semiconductor substrate 1 and absorbed and utilized by the semiconductor substrate 1, thereby improving the photoelectric conversion efficiency of the solar cell. In this invention, the first surface 10 of the semiconductor substrate 1 is textured.

[0059] Combination Figure 2 , Figure 6 and Figure 7 The aforementioned recessed structure 51 can be understood as the plane on which most of the surface, excluding the recessed structure 51, lies, being horizontal, and the recessed structure 51 is recessed relative to the horizontal plane. It should be noted that the "horizontal plane" in the above "most of the surface, excluding the recessed structure 51, lies, being horizontal" refers to the plane on which most of the surface of the semiconductor substrate 1, excluding the recessed structure 51, lies, for the semiconductor substrate 1 as a whole.

[0060] Compared to the horizontal surface corresponding to the second textured structure region 5, the surface area of ​​the recessed structures 51 in this application, which are concave relative to the horizontal surface, is larger. This not only enhances the adhesion of the passivation layer 3 formed later on this surface, improving the passivation effect of the solar cell, but also increases light refraction, allowing more light to be transmitted into the semiconductor substrate 1 of the solar cell, improving light trapping effect, and thus improving the photoelectric conversion efficiency of the solar cell.

[0061] As one possible implementation, see Figure 2 and Figure 8 The recessed structure 51 includes at least partially overlapping recessed structures 51 and non-overlapping recessed structures 51.

[0062] See Figure 8 Only some of the recessed structures 51 are stacked, which makes the passivation layer 3 formed on the surface of the recessed structure 51 more uniform, the film quality of the passivation layer 3 is better, and the density of the passivation layer 3 is better, thereby improving the passivation effect of the solar cell.

[0063] As one possible implementation, see Figure 8 The height difference between the bottom surfaces of adjacent recessed structures 51 at overlapping locations is less than 2 μm. For example, the height difference can be 1.9 μm, 1.8 μm, 1.7 μm, 1.5 μm, 1 μm, 0.5 μm, or 0 μm. Controlling the height difference between the bottom surfaces of the overlapping recessed structures 51 within an ideal range ensures that the roughness of the side surface 12 is within a suitable range, which is beneficial to improving the uniformity of the passivation layer formed on the recessed structure 51.

[0064] The above-mentioned "the size of the first texture structure 40 is smaller than the size of the recessed structure 51" can be understood as the tower height of the first texture structure 40 being smaller than the distance between the bottom surface and the top opening of the recessed structure 51, and / or the one-dimensional size of the orthographic projection of the first texture structure 40 on the semiconductor substrate 1 being smaller than the one-dimensional size of the orthographic projection of the recessed structure 51 on the semiconductor substrate 1.

[0065] The height of the first texture structure can be the height of a single first texture structure or the average height of the first texture structures within a certain area. When the cross-section of the first texture structure is a regular quadrilateral, the one-dimensional dimension can refer to the length, width, or diagonal of the first texture structure, etc. When the cross-section of the first texture structure is circular, the one-dimensional dimension can refer to the diameter of the first texture structure. When the cross-section of the first texture structure is elliptical, the one-dimensional dimension can refer to the major axis or minor axis of the first texture structure, etc. The same applies to recessed structures, and will not be elaborated here.

[0066] The material and thickness of the passivation layer can be set according to the actual situation and are not specifically limited here. For example, the material of the passivation layer may include one or more of silicon nitride, hydrogen-containing silicon nitride, silicon oxide, silicon oxynitride, aluminum oxide, zinc oxide, and hafnium dioxide.

[0067] As one possible implementation, see Figure 4 and Figure 5 The passivation layer 3 can be a single-layer film, such as a single layer of silicon nitride. It can also be a stack of multiple films, such as a stack of aluminum oxide and silicon nitride layers, or a stack of silicon nitride layers alone.

[0068] In one alternative approach, see Figure 2 The first textured structure region 4 has a wavy shape on the side closest to the second surface 11. Along the direction from the first surface 10 to the second surface 11, the distance between the crests and troughs of the wavy shape is 0.5 μm to 2 μm. For example, the distance can be 0.5 μm, 1 μm, 1.3 μm, 1.5 μm, 1.7 μm, 1.8 μm, or 2 μm, etc.

[0069] Therefore, the regularity of the wave shape results in better film formation quality at the junction of the first textured structure region 4 and the second textured structure region 5, leading to a more uniform and orderly film. Furthermore, in the first textured structure region 4, near the second surface 11, edge recombination of charge carriers occurs, and the magnitude of the recombination current is directly related to the edge length. A smooth edge and low roughness can reduce the length of the edge region, decrease charge carrier recombination, and improve battery performance. Therefore, when the distance between the peaks and troughs of the wave shape meets the above-mentioned value range, the length of the edge region can be reduced, charge carrier recombination can be decreased, and battery performance can be improved.

[0070] As one possible implementation, see Figure 2 Along the direction from the first surface 10 to the second surface 11, the second textured structure region 5 includes a central region and two edge regions, with multiple recessed structures 51 arranged along a first straight line. Within the central region, the angle between the first straight line and the side edge of the side surface 12 is less than or equal to 30° (not shown in the figure). Within the edge regions, the angle β between the first straight line and the side edge of the side surface 12 is between 30° and 60°, and the side edge of the side surface 12 is parallel to the first surface 10. For example, the angle within the central region can be 30°, 28°, 25°, 20°, 18°, 15°, 13°, 11°, or 10°, etc. The angle within the edge regions can be 31°, 32°, 35°, 38°, 40°, 42°, 45°, 48°, 50°, 52°, 55°, 58°, or 60°, etc.

[0071] When the two included angles are within the aforementioned range, the capillary effect can be reduced or eliminated, thereby reducing or eliminating the probability that the water film sprayed on the front of the solar cell during cleaning of the solar cell side 12 is absorbed to the back of the solar cell, thus reducing the proportion of the first textured structure region 4. Based on this, it is more conducive to the formation of the passivation layer 3, improving the passivation effect and thus improving the cell efficiency of the solar cell.

[0072] In some embodiments, the shape of the orthographic projection of the recessed structure 51 onto the semiconductor substrate 1 can be a triangle, a quadrilateral (e.g., a rectangle, a square, a rhombus, a parallelogram, or a trapezoid), a pentagon, or other polygons. It should be noted that the aforementioned "orthographic projection of the recessed structure 51 onto the semiconductor substrate 1" includes the orthographic projection of the top opening 52 of the recessed structure 51 onto the semiconductor substrate 1, and / or the orthographic projection of the bottom surface 53 of the recessed structure 51 onto the semiconductor substrate 1.

[0073] As one possible implementation, the solar cell further includes a first doped conductive layer 93 and a second doped conductive layer 2. The first doped conductive layer 93 is formed on the first surface 10 and the first textured structure region 4, and the second doped conductive layer 2 is formed on at least a portion of the second surface 11 and a portion of the second textured structure region 5. The first doped conductive layer 93 and the second doped conductive layer 2 have opposite conductivity types. The passivation layer 3 located on the side surface 12 and the passivation layer 3 located on the first surface 10 and the second surface 11 are formed on the side of the first doped conductive layer 93 and the second doped conductive layer 2 that faces away from the semiconductor substrate 1.

[0074] See Figure 3Since the first doped conductive layer 93 is formed on the first surface 10 and the first textured structure region 4, and the second doped conductive layer 2 is formed on at least part of the second surface 11 and part of the second textured structure region 5, the first textured structure region 4 and the second textured structure region 5 do not overlap. That is, there is a gap between the edge of the second doped conductive layer 2 and the edge of the first surface 10 (the position of the dashed box) shown in the figure. Therefore, it is possible to avoid leakage of current by doped conductive layers with opposite polarities overlapping on the side 12 of the semiconductor substrate 1.

[0075] As one possible implementation, the first doped conductive layer can be an additional film layer formed on the semiconductor substrate. Alternatively, the first doped conductive layer can be formed by diffusion treatment on a first surface of the semiconductor substrate, in which case the top surface of the first doped conductive layer is coplanar with the first surface of the semiconductor substrate.

[0076] In some embodiments, regarding the first doped conductive layer and the second doped conductive layer, in terms of doping type, the first doped conductive layer is N-type, and the second doped conductive layer is P-type. Alternatively, the first doped conductive layer is P-type, and the second doped conductive layer is N-type. This embodiment of the invention does not specifically limit the doping type of the first and second doped conductive layers, as long as their doping types are opposite. When the doping type is P-type, it is generally doped with a Group III element. When the doping type is N-type, it is generally doped with a Group V or Group VI element.

[0077] From a material perspective, the materials of the first doped conductive layer and / or the second doped conductive layer can include any semiconductor material such as silicon, germanium-silicon, or germanium. From the perspective of the arrangement of matter, the crystal phase of the first doped conductive layer and / or the second doped conductive layer can be amorphous, microcrystalline, nanocrystalline, single-crystal, or polycrystalline. For example, the first doped conductive layer and / or the second doped conductive layer can be composed of one or more of polycrystalline silicon, amorphous silicon, and microcrystalline silicon. For instance, when the first doped conductive layer is an additional film layer formed on the semiconductor substrate, the first doped conductive layer includes a first doped polycrystalline silicon layer. In this case, compared with a doped amorphous silicon layer, the doped polycrystalline silicon layer has higher carrier transport characteristics. Therefore, when the first doped conductive layer is a doped polycrystalline silicon layer, the carrier recombination rate can be further reduced, which is beneficial to improving the photoelectric conversion efficiency of the solar cell. The second doped conductive layer includes a doped amorphous silicon layer and / or a doped microcrystalline silicon layer. It should be noted that the term "microcrystalline" in the above-mentioned doped microcrystalline silicon layer refers to the grain size of the silicon material. Specifically, microcrystalline silicon materials refer to silicon materials with a grain size at the nanometer level.

[0078] In some embodiments, the semiconductor substrate and the first doped conductive layer form a PN junction. The semiconductor substrate is an N-type silicon substrate, the first doped conductive layer is a P-type doped conductive layer, and the first doped conductive layer is a diffusion layer on the surface of the semiconductor substrate.

[0079] As one possible implementation, see Figure 4 and Figure 5 The second surface 11 includes a non-electrode region 110, which has a third texture structure. The third texture structure includes a recessed structure, and the size of the recessed structure 51 located in the second texture structure region 5 is larger than the size of the recessed structure located in the non-electrode region 110.

[0080] Because the side of the battery retains either the first doped conductive layer 93 or the second doped conductive layer 2, as well as the first textured structure region 4 and the second textured structure region 5, the surface morphology of the side is relatively complex. Therefore, designing a recessed structure on the side of the solar cell with a surface size larger than that of the third textured structure can improve the quality of the passivation layer on the side, enhance its passivation effect, and thereby increase the power on the back of the solar cell and improve the bifaciality of the solar cell by reducing the carrier recombination probability.

[0081] In one alternative embodiment, the one-dimensional dimension of the orthographic projection of the recessed structure located in the second textured structure region 5 onto the semiconductor substrate is 15 μm to 40 μm. For example, the one-dimensional dimension of the orthographic projection of the recessed structure located in the second textured structure region 5 onto the semiconductor substrate can be 15 μm, 18 μm, 20 μm, 22 μm, 25 μm, 28 μm, 30 μm, 32 μm, 35 μm, 38 μm, or 40 μm, etc.

[0082] The one-dimensional dimension of the orthographic projection of a recessed structure located in a non-electrode region onto a semiconductor substrate ranges from 8 μm to 20 μm. For example, the one-dimensional dimension of the orthographic projection of a recessed structure located in a non-electrode region onto a semiconductor substrate can be 8 μm, 9 μm, 10 μm, 11 μm, 12 μm, 13 μm, 14 μm, 15 μm, 16 μm, 17 μm, 18 μm, 19 μm, or 20 μm, etc. Please refer to the previous description for the definition of one-dimensional dimension.

[0083] If the surface size of the recessed structure in the second textured structure region 5 and the recessed structure in the non-electrode region is too large when adopting the technical solution, the surface undulation will be too gentle, which is not conducive to the coating quality. For example, the passivation layer is prone to cracking. By setting the surface size of the recessed structure within the above range, it is possible to reduce the cracking phenomenon and increase the coating area of ​​the passivation layer to improve the passivation performance.

[0084] See Figure 6 and Figure 7As described above, along the direction extending into the semiconductor substrate 1, the recessed structure 51 has a top opening 52 and a bottom surface 53 disposed opposite to each other, and a sidewall 54 located between the bottom surface 53 and the top opening 52. Therefore, the "one-dimensional dimension of the orthographic projection of the recessed structure 51 onto the semiconductor substrate 1" can refer to the one-dimensional dimension of the top opening 52, the one-dimensional dimension of the bottom surface 53, or both. When the orthographic projection of the top opening 52 onto the semiconductor substrate 1 is completely consistent with and overlaps the orthographic projection of the bottom surface 53 onto the semiconductor substrate 1, the one-dimensional dimension of the top opening 52 and the one-dimensional dimension of the bottom surface 53 are the same value.

[0085] As one possible implementation, see Figure 6 and Figure 7 The depth D of the recessed structure 51 located in the second textured structure region 5 is 0.1 μm to 3 μm. For example, the depth D of the recessed structure 51 located in the second textured structure region 5 can be 0.1 μm, 0.5 μm, 0.8 μm, 1 μm, 1.2 μm, 1.5 μm, 1.8 μm, 2 μm, 2.5 μm, 2.8 μm or 3 μm, etc.

[0086] When the depth of the recessed structure 51 located in the second textured structure region 5 exceeds 3 μm, the roughness of the recessed structure 51 is too large. This results in a larger thickness and poorer uniformity of the doped conductive layer and passivation layer 3 formed on the recessed structure 51, which is detrimental to the formation of high-density and high-uniformity doped conductive and passivation layers. However, by setting the depth of the recessed structure 51 within the aforementioned range, it is possible to prevent excessively large local film thickness caused by the doped conductive and passivation layers 3, thereby improving the open-circuit voltage of the solar cell and enhancing the fill factor and photoelectric conversion efficiency.

[0087] As one possible implementation, the first texture structure includes one or more of the following: a prismatic structure, an inverted pyramid structure, a frustum structure, or a pyramidal structure.

[0088] When the first texture structure includes a pyramidal or inverted pyramidal structure, compared to a recessed texture structure with a predominantly planar proportion (typically 100 crystal planes), the pyramidal or inverted pyramidal structure exposes more of the sloping surfaces of the 111 crystal planes. Therefore, the pyramidal or inverted pyramidal structure not only increases the contact area between the tunneling layer 6 or the first doped conductive layer 93 and different crystal planes of the semiconductor substrate 1, providing more transport paths for charge carriers, but the apex of the inverted pyramid is also more conducive to enhancing the electron tunneling effect.

[0089] In some embodiments, the bottom surface of the first texture structure is square, rhomboid, rectangular, parallelogram, approximately rhomboid, or approximately rectangular.

[0090] As one possible implementation, see Figures 3 to 5 The solar cell also includes a tunneling layer 6. The tunneling layer 6 is located between the semiconductor substrate 1 and the second doped conductive layer 2, which is a doped polycrystalline silicon layer.

[0091] The tunneling layer 6 is located between the semiconductor substrate 1 and the second doped conductive layer 2, and the second doped conductive layer 2 is formed at least on the second surface 11 and the second textured structure region 5. This allows for passivation of the side surfaces 12 corresponding to the second surface 11 and the second textured structure region 5 of the semiconductor substrate 1, reducing the carrier recombination rate. Furthermore, under the same conditions, compared to textured structures with large undulations such as pyramidal textured surfaces, the recessed structure 51 without a pyramidal tip has relatively smaller undulations, which is beneficial for improving the formation quality and film thickness of the tunneling layer 6, thereby improving the passivation effect of the tunneling layer 6 on the semiconductor substrate 1 and increasing the conversion efficiency of the solar cell. In addition, the recessed structure 51 with a certain depth on the second textured structure region 5 increases the specific surface area of ​​the semiconductor substrate 1, thereby increasing the contact area between the side surfaces 12 and the tunneling layer 6. This helps to saturate the dangling bonds of the semiconductor substrate 1, reducing recombination losses, thereby improving the passivation effect of the solar cell and further improving the cell efficiency. Furthermore, the tunneling layer 6 and the second doped conductive layer 2 together form a tunneling passivation contact structure, which not only achieves efficient carrier transport but also further enhances the passivation effect on the surface of the semiconductor substrate 1.

[0092] The material and thickness of the tunneling layer 6 can be set according to actual conditions and are not specifically limited here. For example, the material of the tunneling layer 6 may include one or more of silicon oxide, aluminum oxide, titanium oxide, hafnium dioxide, gallium oxide, tantalum pentoxide, niobium pentoxide, silicon nitride, silicon carbonitride, aluminum nitride, titanium nitride, and titanium carbonitride. The thickness of the tunneling layer 6 is greater than or equal to 1 nm and less than or equal to 2 nm. For example, the thickness of the tunneling layer 6 may be 1 nm, 1.2 nm, 1.5 nm, 1.7 nm, 1.8 nm, or 2 nm. Further, the second doped conductive layer 2 is a doped polycrystalline silicon layer. The doped polycrystalline silicon layer may be a phosphorus-doped polycrystalline silicon layer, or it may be doped with other substances, which are not specifically limited here. The thickness of the second doped conductive layer 2 is from 80 nm to 300 nm. For example, the thickness of the second doped conductive layer 2 can be 80 nm, 90 nm, 100 nm, 110 nm, 120 nm, 130 nm, 140 nm, 150 nm, 160 nm, 170 nm, 180 nm, 190 nm, 200 nm, 210 nm, 220 nm, 230 nm, 240 nm, 260 nm, 280 nm or 300 nm, etc.

[0093] As one possible implementation, see Figure 4The first surface 10 of the semiconductor substrate 1 has a first edge, and a first isolation region 7 is provided between the boundary of the first doped conductive layer adjacent to the first edge and the first edge. The first isolation region 7 separates the boundary of the first doped conductive layer adjacent to the first edge from the first edge to facilitate the suppression of leakage current.

[0094] In one alternative approach, see Figure 4 The first isolation zone 7 has a fourth texture structure, which includes a recessed structure.

[0095] When the technical solution is adopted, a recessed structure is formed on the surface of the first isolation region 7, which makes the coating quality of the subsequent passivation layer 3 better. While ensuring edge passivation, the insulating properties of the passivation layer 3 can guarantee the electrical isolation between the first doped conductive layer and the second doped conductive layer 2.

[0096] In one alternative approach, see Figure 4 The size of the recessed structure located in the first isolation region 7 is smaller than the size of the recessed structure located in the non-electrode region 110.

[0097] With the adoption of the technical solution, the size of the recessed structure in the first isolation region 7 is small. While ensuring flatness and improving the passivation effect when the passivation layer 3 is grown subsequently, it can reduce the reflectivity of the first isolation region 7 and reduce the current drop caused by changes in surface state. The insulating properties of the passivation layer 3 can ensure electrical isolation between the first doped conductive layer and the second doped conductive layer 2.

[0098] In one alternative embodiment, the ratio of the size of the recessed structure located in the first isolation region to the size of the recessed structure located in the non-electrode region is 0.5:1 to 1:1. For example, the ratio may be 0.5:1, 0.58:1, 0.6:1, 0.7:1, 0.8:1, 0.9:1, or 1:1, etc.

[0099] The bottom surface dimension of the recessed structure located within the first isolation region is 4μm to 10μm. For example, the bottom surface dimension of the recessed structure located within the first isolation region can be 4μm, 4.5μm, 4.8μm, 5μm, 5.4μm, 5.8μm, 6μm, 6.5μm, 6.8μm, 7μm, 7.5μm, 7.8μm, 8μm, 8.5μm, 8.8μm, 9μm, 9.5μm, 9.8μm, or 10μm, etc.

[0100] With this technical solution, the smaller recessed structure size of the first isolation region can reduce surface reflectivity and minimize the impact on current while ensuring passivation. Simultaneously, the smaller recess size means that lower laser energy is sufficient to completely remove the PN junction. Combined with a non-conductive passivation film, electrical isolation between the front and back sides is guaranteed. Using a lower-power laser or a faster laser processing time increases laser throughput and reduces production costs.

[0101] As one possible implementation, see Figure 5 The second surface 11 of the semiconductor substrate 1 has a second edge, and a second isolation region 8 is provided between the boundary of the second doped conductive layer 2 adjacent to the second edge and the second edge. The second isolation region 8 separates the boundary of the second doped conductive layer 2 adjacent to the second edge from the second edge to facilitate the suppression of leakage current.

[0102] It should be noted that, as described above, the so-called isolation regions (first isolation region 7 and second isolation region 8) are regions where electron / hole collection does not occur. They do not contribute current, or there are no doped conductive layers (first doped conductive layer 93 and second doped conductive layer 2) in these regions, and therefore no photocurrent is generated or collected. These isolation regions separate the boundaries of the doped conductive layers from the edges of the semiconductor substrate 1 to ensure electrical insulation.

[0103] As one possible implementation, the second doped conductive layer is also formed on the first doped conductive layer located in the first textured structure region and on the first doped conductive layer located in the edge region of the first surface.

[0104] With the adopted technical solution, in the case of forming an isolation zone at the edge of the battery cell, the second doped conductive layer is formed in the first textured structure region or even the edge region of the first surface. This achieves good passivation of the battery side while ensuring no leakage. The first doped conductive layer remains on the surface of the first textured region, and the second doped conductive layer can form a partial field passivation effect in the first textured structure region. Combined with subsequent passivation layers, this can achieve good passivation near the side edge.

[0105] As one possible implementation, each corner in the bottom surface of the recessed structure in all regions includes at least one or more of the following: rounded corners, sharp corners, rounded corners, or sharp corners.

[0106] Taking the recessed structure 51 located in the second texture structure region 5 as an example, see Figure 6 and Figure 7 Each corner in the bottom surface 53 located within the second texture structure region 5 includes at least one or more of the following: rounded corner, sharp corner, rounded corner, or sharp corner.

[0107] See Figure 6When all corners are rounded or semi-rounded, compared to when all corners are sharp or semi-sharp, the transition of the rounded or semi-rounded corners on the bottom surface 53 is smoother and flatter. This makes the boundary transition of the recessed structure 51 at the rounded or semi-rounded corners more gradual and blurred, thus making the surface of the passivation layer 3 facing away from the semiconductor substrate 1 relatively flat from a macroscopic perspective. In this case, it is beneficial to improve the formation quality and film thickness of the passivation layer 3, thereby improving the passivation effect of the passivation layer 3 on the semiconductor substrate 1 and improving the conversion efficiency of the solar cell.

[0108] See Figure 7 When all corners are sharp or pointed, compared to when all corners are rounded or rounded, the transition of sharp or pointed corners is more obvious and the degree of undulation is greater. This is beneficial to increase the specific surface area of ​​the second doped conductive layer 2 on the side away from the semiconductor substrate 1, thereby increasing the contact area between the second doped conductive layer 2 and the electrode, improving the contact performance between the second doped conductive layer 2 and the electrode, as well as the adhesion and shaping of the electrode on the second doped conductive layer 2, which is beneficial to improving the conversion efficiency of the solar cell.

[0109] To facilitate understanding, the following description of the above-mentioned solar cell manufacturing method is given as an example in one possible manner. It should be noted that the following description is for comprehension only and is not intended to limit the specific application.

[0110] Combination Figures 2 to 5 First, a semiconductor substrate 1 is provided. The semiconductor substrate 1 includes a first surface 10 and a second surface 11 facing each other, and a plurality of side surfaces 12 connecting the first surface 10 and the second surface 11. The first surface 10 and the second surface 11 are texturized to form a textured structure. The textured structure can trap light, reduce the reflection of sunlight by the solar cell, and improve the performance of the solar cell. The shape, material, conductivity type, and light-receiving properties of the semiconductor substrate 1 are described above and will not be repeated here.

[0111] In one alternative approach, an N-type single-crystal silicon wafer is used as the semiconductor substrate 1. It is first pre-cleaned with alkali and hydrogen peroxide, and then the pre-cleaned silicon wafer is texturized to form a double-sided pyramidal textured surface structure, which improves the light trapping effect on the silicon wafer surface.

[0112] In some embodiments, the minority carrier lifetime of the N-type monocrystalline silicon wafer is greater than 1 ms, and the resistivity is 0.3 Ω·cm to 2.1 Ω·cm. The volume ratio of alkali to hydrogen peroxide in the pre-cleaning tank is 1:1 to 1:6, the temperature is 60°C to 80°C, and the time is 1 min to 4 min. The volume ratio of alkali to texturing additive in the texturing tank is 2:1 to 8:1, the texturing temperature is 60°C to 85°C, and the time is 4 min to 8 min. The pyramid size is 0.5 μm to 6 μm, the height is 0.5 μm to 5 μm, and the specific surface area is 1 to 3.

[0113] Next, the first surface 10 of the texturized semiconductor substrate is subjected to a diffusion process to form a first doped conductive layer and a first doped oxide layer formed on the first doped conductive layer. At this time, the semiconductor substrate 1 and the first doped conductive layer form a PN junction.

[0114] For example, the doping source used in the diffusion process includes a group III source, such as a boron source, a gallium source, an indium source, etc.

[0115] In one alternative approach, the aforementioned group III source is a boron source, and the first doped oxide layer is a borosilicate glass layer. The borosilicate glass layer can provide protection during subsequent processing of the solar cell.

[0116] In some embodiments, the first surface 10 of the semiconductor substrate 1 is subjected to diffusion treatment to form a first doped conductive layer and a first doped oxide layer formed on the first doped conductive layer. This can be achieved by placing the semiconductor substrate 1 in a tube diffusion furnace and diffusing a boron source BCl3 or BBr3 in a nitrogen and oxygen atmosphere. The diffusion time and temperature can be set according to actual needs. In this process, a first doped conductive layer (e.g., a doped P+ layer) and a first doped oxide layer (e.g., a borosilicate glass layer) are formed.

[0117] For example, when depositing boron on the first surface 10 of the semiconductor substrate 1, the doping depth can be from 300 nm to 1000 nm, and the doping surface concentration is 2E18 atom / cm³. 3 Up to 5E19 atom / cm 3 The thickness of the borosilicate glass layer can be from 40nm to 120nm.

[0118] Next, the first doped conductive layer formed on the second surface 11 is removed to remove the PN junction of the second surface 11. It should be noted that during the diffusion process on the first surface 10 of the semiconductor substrate 1, the first doped conductive layer and the first doped oxide layer are inevitably formed on at least a portion of the side surface 12 and the second surface 11. The at least a portion of the second surface 11 can be understood as either the edge region of the second surface 11 near the side surface 12, or the entire second surface 11.

[0119] For example, a chain-type single-sided acid pickling device is first used to acid pickle the second surface 11 (back surface) where the first doped conductive layer is formed to remove the first doped oxide layer. Then, a tank-type machine is used for alkali and hydrogen peroxide pre-cleaning. Finally, the second surface 11 is polished to remove the PN junction on the second surface 11 of the semiconductor substrate 1. As for the specific processing procedures and the reagents used, existing technologies can be referenced, and no specific limitations are made here. The chain-type acid pickling ensures that the first doped oxide layer on the back side is completely removed, while the first doped oxide layer on the front side remains unaffected. This ensures that subsequent polishing only affects the back side, while the first doped oxide layer on the front side acts as a protective layer, and the surface morphology remains unaffected.

[0120] In some embodiments, chain pickling is carried out at room temperature using an aqueous HF solution, with an HF to water ratio of 1:0.3 to 1:3. During tank pre-cleaning, the volume ratio of alkali to hydrogen peroxide is 1:1 to 1:10, the temperature is 60°C to 80°C, and the time is 1 min to 5 min. In the alkali polishing tank, the volume ratio of alkali to additives is 3:1 to 10:1, the alkali polishing temperature is 60°C to 85°C, the time is 3 min to 8 min, and the width of the tower base is 5 μm to 40 μm.

[0121] In this step, to improve the edge characteristics of the semiconductor substrate 1, the following optimization methods can be used: 1) Adjust the acid pickling process on the back side of the borosilicate glass layer to increase the corrosion of the borosilicate glass layer on the side 12 of the semiconductor substrate 1 by HF. 2) Add additives to the water film to reduce the surface tension of the water film and reduce the probability of the water film wetting the side 12 of the semiconductor substrate 1. 3) Coat the side 12 of the semiconductor substrate 1 with a hydrophobic coating to reduce the probability of the water film wetting the side 12. 4) Improve the cutting morphology of the side 12 to reduce the capillary effect.

[0122] Next, a tunneling layer 6 and a second doped conductive layer 2 are deposited on the second surface 11 of the polished semiconductor substrate 1. Simultaneously, a second doped oxide layer is grown on the second doped conductive layer 2. During subsequent processing of the solar cell, the second doped oxide layer provides protection, and the tunneling layer 6 effectively separates minority and majority carriers, improving passivation. Furthermore, it reduces corrosion of the semiconductor substrate 1 during printing, improving contact performance.

[0123] For example, a tunneling layer 6 and a second doped conductive layer 2 are sequentially grown on the polished second surface 11, and the tunneling layer 6 and the second doped conductive layer 2 are deposited around the edge region of the first surface 10. Alternatively, the tunneling layer 6 and the second doped conductive layer 2 are sequentially grown on the edge region of the first surface 10 and on the polished second surface 11. At the same time, a second doped oxide layer is grown on the second doped conductive layer 2.

[0124] In some implementations, the thickness of the tunneling layer 6 is 1 nm to 2 nm, and the thickness of the second doped conductive layer 2 is 80 nm to 300 nm. The second doped conductive layer 2 can be a doped polysilicon layer, and the second doped oxide layer is a phosphosilicate glass layer. Further descriptions of the tunneling layer 6 and the second doped conductive layer 2 can be found above and will not be repeated here.

[0125] As one possible implementation method, there are three possible approaches to depositing the second doped conductive layer 2: double-sided deposition of the doped conductive layer using LPCVD (Low Pressure Chemical Vapor Deposition), single-sided deposition of the doped conductive layer using LPCVD, and deposition of the second doped conductive layer 2 using PECVD (Plasma Enhanced Chemical Vapor Deposition). The specific process for forming the second doped conductive layer 2 is not specifically limited here.

[0126] The above-described method for fabricating solar cells can be used to create tunneling oxide layer passivated contact cells to meet practical needs. Furthermore, the chemical passivation of the tunneling layer 6 and the field passivation of the second doped conductive layer 2 can significantly reduce the recombination degree on the surface of the semiconductor substrate 1. Simultaneously, the tunneling layer 6 ensures effective tunneling of majority carriers, and the second doped conductive layer 2 significantly improves the conductivity of photogenerated carriers, thereby increasing the open-circuit voltage and fill factor of the solar cell. When the second surface 11 is stacked with the tunneling layer 6 and the second doped conductive layer 2, a passivated contact structure is formed. The tunneling layer 6 allows majority carriers to tunnel into the second doped conductive layer 2 while blocking minority carrier recombination, allowing majority carriers to be laterally transported and collected by the metal in the second doped conductive layer 2. This greatly reduces the metal contact recombination current, increases the open-circuit voltage and short-circuit current of the cell, and thus improves the cell efficiency.

[0127] Next, the tunneling layer 6 and the second doped conductive layer 2 located on the non-electrode region 110 of the second surface 11 are irradiated with a first laser to etch the tunneling layer 6 and the second doped conductive layer 2 located on the non-electrode region 110.

[0128] For example, a first laser process is used to irradiate the second doped oxide layer located in the non-electrode region 110. That is, the second doped oxide layer is patterned using a first laser; the area irradiated by the first laser is the non-electrode region 110, and the area not irradiated by the first laser is the electrode region. Through high-energy first laser irradiation, the first laser acts on the phosphosilicate glass layer for a short time, causing the phosphosilicate glass layer to be modified, loosened, or vaporized, reducing the protective capability of the phosphosilicate glass layer located in the non-electrode region 110. This ensures that a reaction rate gradient is formed during subsequent alkaline etching, allowing the non-electrode region 110 to be etched as required, while the electrode region remains unaffected due to the protection of the phosphosilicate glass layer. During subsequent processing, the second doped conductive layer 2 located in the electrode region is protected by the phosphosilicate glass layer and will not be etched by the alkaline agent. Because the phosphosilicate glass layer in the non-electrode region 110 is damaged, the second doped conductive layer 2 in the non-electrode region 110 is etched by the alkaline agent, and the alkaline agent further etches downwards into the tunneling layer 6 and the semiconductor substrate 1. At this point, the tunneling layer 6 and the second doped conductive layer 2 located in the electrode region form a conductive contact layer, which corresponds one-to-one with the electrode. The second doped conductive layer 2 located in the non-electrode region 110 on the second surface 11 is removed, which effectively reduces parasitic absorption and increases the battery current, while the second doped conductive layer 2 in the electrode region is retained to prevent the paste from corroding the semiconductor substrate 1 during metallization and improve the battery fill factor.

[0129] For example, the first laser wavelength in the first laser process is greater than or equal to 300 nm and less than or equal to 600 nm. For instance, the first laser wavelength can be 300 nm, 350 nm, 400 nm, 500 nm, 550 nm, or 600 nm, etc. The width W3 of the non-electrode region 110 is greater than or equal to 250 μm and less than or equal to 800 μm. For instance, the width W3 of the non-electrode region 110 can be 250 μm, 300 μm, 350 μm, 400 μm, 450 μm, 500 μm, 550 μm, 600 μm, 650 μm, 700 μm, 750 μm, or 800 μm, etc.

[0130] It should be noted that if the second surface 11 of the solar cell does not need to form the conductive contact layer corresponding to the electrodes, then the second doped oxide layer does not need to be subjected to the first laser patterning process. In this case, the second surface 11 is covered by the tunneling layer 6 and the second doped conductive layer 2.

[0131] Next, the tunneling layer 6 and the second doped conductive layer 2 located on the edge region of the first surface 10 are removed.

[0132] For example, a chain-type single-sided cleaning device is first used to remove the phosphosilicate glass layer (i.e., the second doped oxide layer) deposited on the first surface 10 (light-receiving surface) of the semiconductor substrate 1. For instance, the chain-type acid washing uses an aqueous HF solution and removes the phosphosilicate glass layer at room temperature, with an HF to water ratio greater than or equal to 1:15 and less than or equal to 1:3; for example, the HF to water ratio can be 1:3, 2:15, 1:5, 4:15, or 1:15, etc. Further, an alkaline solution is used to remove the tunneling layer 6 and the second doped conductive layer 2 on the edge region of the first surface 10. For example, the volume ratio of alkali to additive in the alkaline texturing bath is 2:1 to 8:1, the alkaline polishing temperature is 60°C to 85°C, and the time is 3 min to 8 min. It should be noted that whether the semiconductor substrate 1 corresponding to the edge region of the first surface 10 is further etched downwards is not specifically limited here and can be operated according to the actual situation.

[0133] In this step, the second doped oxide layer plated around the first surface 10 is removed, while the second doped conductive layer 2 and the second doped oxide layer on the side surface 12 are retained. The following scheme can be adopted: The first method involves using a second laser process to treat the plating area around the first surface 10, destroying the second doped oxide layer on the surface of the plating area. This ensures that the second doped conductive layer 2 formed by plating around the first surface 10 can be completely removed during the subsequent alkaline cleaning process. Since there is a significant thickness difference between the first doped oxide layer (borosilicate glass layer) and the second doped oxide layer (phosphosilicate glass layer), by appropriately adjusting the laser energy density of the second laser, it is possible to ensure complete destruction of the phosphosilicate glass layer plating around the first surface 10, while also preventing complete destruction of the borosilicate glass layer even when the laser irradiates it, thus achieving selective polishing and cleaning. The second laser can be any one of a green nanosecond laser, a green picosecond laser, a green femtosecond laser, an ultraviolet picosecond laser, or an ultraviolet femtosecond laser.

[0134] The second method involves depositing masks on the first surface 10 and the side surface 12 of the semiconductor substrate 1. The first surface 10 is then acid-washed to remove the mask. Next, the second surface 11 and the first surface 10 are etched using alkaline washing to form the desired cell morphology. Finally, the mask and the phosphorus silicate glass layer on the side surface 12 are removed by acid washing, thus preserving the tunneling layer 6 and the second doped conductive layer 2 on the side surface 12. In this application, the mask can be alumina, silicon nitride, etc., and the deposition method can be ALD, PECVD, etc. The mask thickness is 30 nm to 80 nm.

[0135] Since the second doped conductive layer 2 is retained on side 12, the following measures can be used to ensure electrical isolation between the first side 10 and the second side 11: The first method involves using a laser to destroy the borosilicate glass layer at the edge of the semiconductor substrate 1 on the first surface 10 after boron expansion. In the next alkaline polishing step, the laser-treated area is polished to remove the PN junction at the edge of the first surface 10, forming the first isolation region 7. This achieves edge electrical isolation, ensuring low leakage current in the battery.

[0136] For example, the bottom surface dimension of the recessed structure located in the first isolation region 7 is 4 μm to 10 μm. The ratio of the size of the recessed structure located in the first isolation region 7 to the size of the recessed structure located in the non-electrode region 110 is 0.5:1 to 1:1.

[0137] The second method involves laser processing at the edge of the second surface 11 after phosphorus diffusion to destroy the phosphorus-silicon glass layer on the surface of the edge of the second surface 11. In the subsequent decoupling process, alkaline polishing is performed on the laser-treated edge area to remove the doping on the second surface 11 and simultaneously etch downwards to remove the inner diffusion layer formed in the semiconductor substrate 1, thereby forming the second isolation region 8. This achieves the purpose of isolating the edges of the first surface 10 and the second surface 11, reducing the possibility of short circuits occurring when doped conductive layers with opposite polarities come into contact.

[0138] For example, the bottom surface dimension of the recessed structure located in the second isolation region 8 is 13 μm to 30 μm. The ratio of the size of the recessed structure located in the second isolation region 8 to the size of the recessed structure located in the electrode region is 1:1 to 1:3.

[0139] It should be noted that the edge isolation can be the first isolation zone 7 and / or the second isolation zone 8.

[0140] Next, a passivation layer 3 is formed on the first doped conductive layer, the second doped conductive layer 2, and the first surface 10 and the second surface 11 of the semiconductor substrate 1.

[0141] As for the material and thickness of the passivation layer 3, these can be set according to actual conditions and are not specifically limited here. For example, the material of the passivation layer 3 may include one or more of silicon nitride, hydrogen-containing silicon nitride, silicon oxide, silicon oxynitride, aluminum oxide, zinc oxide, and hafnium dioxide.

[0142] As one possible implementation, the passivation layer 3 can be a single-layer film, such as a single layer of silicon nitride; or it can be a stack of multiple films, such as a stack of aluminum oxide and silicon nitride layers, or a stack of silicon nitride alone.

[0143] In some embodiments, an aluminum oxide passivation layer 30 is grown on the first doped conductive layer, the second doped conductive layer 2, and the first surface 10 and the second surface 11 of the semiconductor substrate 1 using atomic layer deposition. Then, a silicon nitride passivation layer 31 is deposited on the aluminum oxide passivation layer 30 located on the first doped conductive layer, the second doped conductive layer 2, and the first surface 10 and the second surface 11 of the semiconductor substrate 1 using plasma enhanced chemical vapor deposition (PECVD).

[0144] The aforementioned passivation layer 3 can passivate the surface of the semiconductor substrate 1, reduce surface recombination, and improve the open-circuit voltage and fill factor. At the same time, the silicon nitride passivation layer 31 can protect the semiconductor substrate 1 and reduce contamination and mechanical damage.

[0145] For example, the thickness of the aluminum oxide passivation layer 30 is 2 nm to 20 nm, the thickness of the silicon nitride passivation layer 31 on the first surface 10 is 65 nm to 85 nm, and the refractive index is 1.7 to 2.2. The thickness of the silicon nitride passivation layer 31 on the second surface 11 is 70 nm to 100 nm, and the refractive index is 2 to 2.4.

[0146] Next, an electrode is formed on the passivation layer 3, and a first electrode 90 is fabricated on the first surface 10 of the semiconductor substrate 1 by a printing device, and a second electrode 91 is fabricated on the second surface 11 of the semiconductor substrate 1.

[0147] For example, the semiconductor substrate 1 is metallized, and electrodes are formed by methods such as screen printing or electroplating. The pastes used to fabricate the first electrode 90 and the second electrode 91 can be silver paste, silver-copper paste, copper paste, nickel paste, etc. The pastes are solidified by a low-temperature sintering process, and then the hydrogen passivation effect is enhanced by light injection. Finally, a good ohmic contact is formed using laser-assisted sintering contact optimization (LECO) technology to complete the production of the solar cell.

[0148] In summary, the above-described solar cell fabrication method optimizes the morphology of the side surface 12 of the solar cell. By removing most of the borosilicate glass layer on the side surface 12, the subsequent polishing process removes most of the textured surface structure and PN junction of the side surface 12, thereby improving the passivation effect of the side surface 12. Furthermore, since the tunneling layer 6 and the second doped conductive layer 2 are retained on the side surface 12 after phosphorus diffusion, an even better passivation effect can be obtained. Further, the use of edge laser isolation technology (i.e., forming a first isolation region 7 and / or a second isolation region 8) improves the leakage problem caused by the retention of the second doped conductive layer 2 on the side surface 12, thereby increasing the cell efficiency of the solar cell.

[0149] Secondly, this utility model embodiment also provides a photovoltaic module, including a battery string and an encapsulation layer. The battery string includes multiple interconnecting elements and multiple solar cells as described in the above technical solution; the interconnecting elements are used to connect multiple solar cells in series to form a battery string, and the encapsulation layer is used to cover the surface of the battery string.

[0150] The beneficial effects of the photovoltaic module provided in this embodiment are the same as those of the solar cell described in the above technical solution, and will not be repeated here.

[0151] Although the present invention has been described in conjunction with specific features and embodiments, it is obvious that various modifications and combinations can be made therein without departing from the spirit and scope of the present invention. Accordingly, this specification and drawings are merely exemplary descriptions of the present invention as defined by the appended claims, and are considered to cover any and all modifications, variations, combinations, or equivalents within the scope of the present invention. Clearly, those skilled in the art can make various alterations and modifications to the present invention without departing from the spirit and scope of the present invention. Thus, if such modifications and modifications of the present invention fall within the scope of the claims of the present invention and their equivalents, the present invention also intends to include such modifications and modifications.

Claims

1. A solar cell, characterized in that, include: A semiconductor substrate, the semiconductor substrate including opposing first and second surfaces, and a plurality of side surfaces connecting the first and second surfaces; Along the direction from the first surface to the second surface, the side surface includes a first textured structure region and a second textured structure region, wherein the first textured structure region is close to the first surface; The first texture structure region has a first texture structure, and the second texture structure region includes multiple recessed structures; the size of the first texture structure is smaller than the size of the recessed structures. The ratio of the width of the first texture structure region to the total width of the side surface is less than or equal to 3%; A passivation layer is formed at least on the stated side.

2. The solar cell according to claim 1, characterized in that, At least some of the recessed structures are arranged in an overlapping manner, and the height difference between the bottom surfaces of adjacent recessed structures at the overlapping positions is less than 2 μm.

3. The solar cell according to claim 1, characterized in that, The first textured structure region has a wave-like shape on the side closest to the second surface; along the direction from the first surface to the second surface, the distance between the crests and troughs of the wave shape is 0.5 μm to 2 μm.

4. The solar cell according to claim 1, characterized in that, Along the direction from the first surface to the second surface, the second textured structure region includes a central region and two edge regions; the plurality of the recessed structures are arranged along a first straight line; Within the intermediate region, the angle between the first straight line and the side edge of the side is less than or equal to 30°. Within the edge region, the angle between the first straight line and the side edge of the side surface is 30° to 60°. The side surface has a side edge that is parallel to the first surface.

5. The solar cell according to claim 1, characterized in that, The solar cell also includes: A first doped conductive layer is formed on the first surface and the first textured structure region; A second doped conductive layer is formed at least on a portion of the second surface and a portion of the second textured structure region; the first doped conductive layer and the second doped conductive layer have opposite conductivity types; The passivation layer located on the side is formed on the side of the first doped conductive layer and the second doped conductive layer that is away from the semiconductor substrate.

6. The solar cell according to claim 1, characterized in that, The second surface includes a non-electrode region, which has a third texture structure, the third texture structure including a recessed structure; The size of the recessed structure located in the second textured structure region is larger than the size of the recessed structure located in the non-electrode region.

7. The solar cell according to claim 6, characterized in that, The one-dimensional dimension of the orthographic projection of the recessed structure located in the second textured structure region onto the semiconductor substrate is 15 μm to 40 μm. The one-dimensional dimension of the orthographic projection of the recessed structure located in the non-electrode region onto the semiconductor substrate is 8 μm to 20 μm.

8. The solar cell according to claim 1, characterized in that, The depth of the recessed structure located in the second textured structure region is 0.1 μm to 3 μm.

9. The solar cell according to claim 5, characterized in that, The solar cell further includes a tunneling layer located between the semiconductor substrate and the second doped conductive layer; the second doped conductive layer is a doped polycrystalline silicon layer.

10. The solar cell according to claim 1, characterized in that, The first texture structure includes one or more of the following: a prismatic structure, an inverted pyramid structure, a frustum structure, or a pyramidal structure.

11. The solar cell according to claim 5, characterized in that, The first surface of the semiconductor substrate has a first edge, and the boundary of the first doped conductive layer adjacent to the first edge has a first isolation region between the first edge and the first edge.

12. The solar cell according to claim 11, characterized in that, The first isolation region has a fourth texture structure, which includes a recessed structure.

13. The solar cell according to claim 12, characterized in that, The second surface includes a non-electrode region, which has a third texture structure, the third texture structure including a recessed structure; The size of the recessed structure located in the first isolation region is smaller than the size of the recessed structure located in the non-electrode region.

14. The solar cell according to claim 13, characterized in that, The ratio of the size of the recessed structure located in the first isolation region to the size of the recessed structure located in the non-electrode region is 0.5:1 to 1:1; The bottom surface dimension of the recessed structure located within the first isolation zone is 4μm to 10μm.

15. The solar cell according to claim 5, characterized in that, The second surface of the semiconductor substrate has a second edge, and a second isolation region is formed between the boundary of the second doped conductive layer adjacent to the second edge and the second edge.

16. The solar cell according to claim 15, characterized in that, The second doped conductive layer is also formed on the first doped conductive layer located in the first textured structure region and on the first doped conductive layer located in the edge region of the first surface.

17. The solar cell according to any one of claims 1 to 16, characterized in that, Each corner in the bottom surface of the recessed structure includes at least one or more of the following: a rounded corner, a sharp corner, a rounded corner, or a sharp corner.

18. A photovoltaic module, characterized in that, The photovoltaic module includes: A battery string, the battery string comprising a plurality of interconnecting elements and a plurality of solar cells as described in any one of claims 1 to 17; the interconnecting elements being used to connect the plurality of solar cells together in series to form the battery string; An encapsulation layer for covering the surface of the battery string.