Semiconductor structure
By using a carbon-based barrier layer to cover the redistribution layer in the semiconductor structure, the problems of copper migration and oxidation in the redistribution layer are solved, thereby improving the reliability and lifespan of the product.
Patent Information
- Application Number
- CN202522351418.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2025-11-05
- Publication Date
- 2026-11-24
- Estimated Expiration
- 2035-11-05
AI Technical Summary
Existing semiconductor structures are prone to copper migration and oxidation in redistribution layers, leading to open circuits or short circuits, which cannot meet the requirements of high-reliability packaging products.
A carbon-based barrier layer is applied to the surface of the redistribution layer to reduce electron migration and oxidation. A carbon-based barrier layer is placed between the dielectric layer and the redistribution layer to protect the redistribution layer.
It improves the reliability of semiconductor structures, prevents copper migration and oxidation in redistribution layers, and extends product lifespan.
Smart Images

Figure CN225021034U_ABST
Abstract
Description
Technical Field
[0001] This utility model relates to a semiconductor structure. Background Technology
[0002] With the continued development and increasing demand for advanced applications such as artificial intelligence and automotive, products need to undergo more stringent reliability testing to meet the requirements of end customers. In packaged products and fan-out / in products, the redistribution layer (RDL) is a common site of failure. During electromigration testing, copper atoms in the redistribution layer migrate under the influence of high-density electrons, gradually creating voids and eventually causing open circuits. In high-temperature and high-humidity testing (THB, uBHAST, BHAST), copper oxidation in the redistribution layer forms copper ions, which migrate to the cathode, are reduced, and precipitate as copper dendrites, causing short circuits and ultimately burning out the redistribution layer. Therefore, it is necessary to improve the materials or structure of the redistribution layer to meet the high reliability requirements of packaged products.
[0003] Figure 1 Electron micrographs of prior art products after high temperature and humidity testing (HAST conditions: 110°C / 85% RH / 1.2Vcc) are shown. Figure 2 It shows the corresponding Figure 1 The diagram shows that in the redistribution layer 10, copper migration occurs at the anode due to oxidation. This copper migration reaches and passes through the interface of the dielectric layer 30. Copper ions also move to the cathode due to voltage reduction, forming copper dendrites 1, which increases leakage current. In severe cases, this can cause a short circuit and burn out the redistribution layer 10. Copper in the redistribution layer 10 is easily oxidized; in the presence of oxygen or moisture (water) at room temperature, it easily forms a loose oxide layer. Even though the packaged product has a packaging layer and a dielectric layer 30 to protect the redistribution layer 10, the protection provided by the dielectric layer 30 is weak, and oxidation-reduction reactions cannot be avoided during high-temperature and high-humidity testing. Utility Model Content
[0004] In view of the problems existing in the related technologies, the purpose of this utility model is to provide a semiconductor structure to at least improve the reliability of the semiconductor structure.
[0005] To achieve the above objectives, this invention provides a semiconductor structure comprising: a redistribution layer; and a carbon-based barrier layer covering at least a portion of the surface of the redistribution layer and conformally thereof. The barrier layer is used to reduce electron migration and oxidation of the redistribution layer. The semiconductor structure further comprises: a dielectric layer covering the redistribution layer, with the barrier layer disposed between the dielectric layer and the redistribution layer.
[0006] In some embodiments, the barrier layer is a conductive layer.
[0007] In some embodiments, the dielectric layer is provided with an opening that exposes the barrier layer.
[0008] In some embodiments, the dielectric layer is provided with an opening that exposes the redistribution layer.
[0009] In some embodiments, the top surface of the redistribution layer faces the opening, and the barrier layer covers the side surface of the redistribution layer.
[0010] In some embodiments, the barrier layer is thinner than the redistribution layer.
[0011] In some embodiments, the semiconductor structure further includes a seed layer disposed beneath the redistribution layer, the barrier layer covering at least a portion of the surface of the redistribution layer exposed relative to the seed layer.
[0012] In some embodiments, the barrier layer covers the side of the seed layer.
[0013] In some embodiments, the barrier layer contacts the top surface of the seed layer, and the side surface of the barrier layer is aligned with the side surface of the seed layer.
[0014] In some embodiments, the portion of the barrier layer covering the side of the seed layer protrudes laterally compared to the portion of the barrier layer covering the redistribution layer.
[0015] In some embodiments, the barrier layer is made of copper-graphene.
[0016] In some embodiments, the barrier layer is made of copper-carbon nanotubes.
[0017] In some embodiments, the dielectric layer and the redistribution layer are completely separated.
[0018] In some embodiments, the redistribution plane contacts the dielectric layer with respect to the top surface of the opening.
[0019] A semiconductor structure includes: a redistribution layer; and a carbon-based barrier layer covering at least a portion of the surface of the redistribution layer, the barrier layer being used to reduce oxidation of the redistribution layer.
[0020] In some embodiments, the semiconductor structure further includes: a dielectric layer covering the redistribution layer, wherein the barrier layer isolates at least a portion of the redistribution layer from the dielectric layer.
[0021] In some embodiments, the barrier layer isolates the sides of the redistribution layer from the dielectric layer.
[0022] In some embodiments, the barrier layer isolates the sides and top of the redistribution layer from the dielectric layer.
[0023] The beneficial technical effects of this utility model are as follows:
[0024] Embodiments of this application provide a semiconductor structure in which a carbon-based barrier layer covers at least a portion of the surface of a redistribution layer to protect the redistribution layer and improve the reliability of the semiconductor structure. Attached Figure Description
[0025] To more clearly illustrate the technical solutions in the embodiments of this application or the prior art, the drawings used in the embodiments will be briefly described below. Obviously, the drawings described below are only some embodiments of this application. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort. It is worth noting that, according to industry standard practice, the components are not drawn to scale and are only used for illustrative purposes. In fact, for clarity of discussion, the dimensions of the components can be arbitrarily increased or decreased.
[0026] Figure 1 The image shows an electron microscope image of a product from the prior art after undergoing a high temperature and high humidity test.
[0027] Figure 2 It shows the corresponding Figure 1 The structural diagram.
[0028] Figure 3 The first dielectric layer is shown coated on the carrier.
[0029] Figure 4 The formation of a seed layer is shown.
[0030] Figure 5 The mask layer is shown.
[0031] Figure 6 The formation of the redistribution layer is shown.
[0032] Figure 7 The removal of the mask layer is shown.
[0033] Figure 8 The etched seed layer is shown.
[0034] Figure 9 The formation of the barrier layer is shown.
[0035] Figure 10 The second mask layer is shown.
[0036] Figure 11 An etch barrier layer is shown.
[0037] Figure 12 The removal of the second mask layer is shown.
[0038] Figure 13 A second dielectric layer is formed.
[0039] Figure 14 The formation of the barrier layer is shown.
[0040] Figure 15 The formation of the redistribution layer is shown.
[0041] Figure 16 The portion showing the etching process removes the barrier layer is illustrated.
[0042] Figure 17 The removal of the mask layer is shown.
[0043] Figure 18 The etched seed layer is shown.
[0044] Figure 19 The formation of the second dielectric layer is shown.
[0045] Figure 20 The formation of the redistribution layer is shown.
[0046] Figure 21 The removal of the mask layer is shown.
[0047] Figure 22 The etched seed layer is shown.
[0048] Figure 23 The formation of the second dielectric layer is shown. Detailed Implementation
[0049] To better understand the spirit of the embodiments of this application, the following description is based on some preferred embodiments of this application.
[0050] Embodiments of this application will be described in detail below. Throughout this specification, identical or similar components and components having identical or similar functions are indicated by similar reference numerals. The embodiments described herein with reference to the accompanying drawings are illustrative and diagrammatic in nature and are intended to provide a basic understanding of this application. The embodiments of this application should not be construed as limiting this application.
[0051] The terms “approximately,” “generally,” “substantial,” “substantial,” “about,” and “approximately” used herein are used to indicate and explain minor variations. For example, when used in conjunction with numerical values, the above terms may refer to a range of variation less than or equal to ±10% of the corresponding numerical value, such as less than or equal to ±5%, less than or equal to ±4%, less than or equal to ±3%, less than or equal to ±2%, less than or equal to ±1%, less than or equal to ±0.5%, less than or equal to ±0.1%, or less than or equal to ±0.05%. As another embodiment, the thickness of a film or layer being “substantially uniform” may refer to the average thickness of the film or layer being less than or equal to ±10% of the standard deviation, such as less than or equal to ±5%, less than or equal to ±4%, less than or equal to ±3%, less than or equal to ±2%, less than or equal to ±1%, less than or equal to ±0.5%, less than or equal to ±0.1%, or less than or equal to ±0.05%. The term "substantially coplanar" can refer to two surfaces that are within 50 μm along the same plane (such as within 40 μm, 30 μm, 20 μm, 10 μm, or 1 μm along the same plane). If, for example, two components overlap or overlap within 200 μm, 150 μm, 100 μm, 50 μm, 40 μm, 30 μm, 20 μm, 10 μm, or 1 μm, then the two components can be considered "substantially aligned." If the angle between two surfaces or components is, for example, 90° ± 10° (such as ± 5°, ± 4°, ± 3°, ± 2°, ± 1°, ± 0.5°, ± 0.1°, or ± 0.05°), then the two surfaces or components can be considered "substantially perpendicular." When used in conjunction with an event or situation, the terms "approximately," "generally," "substantially," "materially," "about," and "approximately" can refer to the exact occurrence of the event or situation as well as the very close approximation of its occurrence.
[0052] In this specification, unless otherwise specified or limited, relative terms such as “central,” “longitudinal,” “lateral,” “front,” “rear,” “right,” “left,” “inner,” “outer,” “lower,” “higher,” “horizontal,” “vertical,” “above,” “below,” “above,” “below,” “top,” “bottom,” and their derivatives (e.g., “horizontally,” “downward,” “upward,” etc.) should be interpreted as referring to the directions described in the discussion or depicted in the accompanying drawings. These relative terms are used for descriptive convenience only and do not require that this application be constructed or operated in a particular orientation.
[0053] For ease of description, "first," "second," "third," etc., can be used in this article to distinguish different components of a figure or a series of figures. "First," "second," "third," etc., are not intended to describe the corresponding components.
[0054] Figures 3 to 13 A semiconductor structure 100 and its manufacturing process according to a first embodiment of this application are shown.
[0055] Figure 3 A carrier 50 is provided, a first dielectric layer 31 is coated on the carrier 50, and the first dielectric layer 31 is cured. The material of the first dielectric layer 31 is, for example, polyimide.
[0056] Figure 4 The diagram shows a seed layer 40 formed on a first dielectric layer 31. The seed layer 40 includes a first seed layer 41 and a second seed layer 42. The material of the first seed layer 41 is, for example, Ti, and the material of the second seed layer 42 is, for example, Cu.
[0057] Figure 5 The diagram shows a mask layer 60 coated on a seed layer 40 and patterned thereon. The material of the mask layer 60 is, for example, a photoresist (PR).
[0058] Figure 6 The diagram illustrates the formation of a redistribution layer 10 within a patterned mask layer 60, for example, via an electroplating process. The material of the redistribution layer 10 is, for example, Cu.
[0059] Figure 7 The removal of the mask layer 60 is shown.
[0060] Figure 8 The etching of the seed layer 40 using the redistribution layer 10 as a mask is shown.
[0061] Figure 9 This demonstrates, for example, the application of physical vapor deposition (PVD) or sputtering processes in... Figure 8 A barrier layer 20 conformally formed to the redistribution layer 10 is formed on the structure shown. In some embodiments, the barrier layer 20 is a carbon-based material, such as the copper-graphene disclosed in prior art TW202006144A. In some embodiments, the material of the barrier layer 20 is, for example, the copper-carbon nanotube disclosed in prior art CN118385597A. Furthermore, since the barrier layer 20 is formed by a sputtering process, its thickness can be effectively controlled, and the barrier layer 20 is thinner than the redistribution layer 10. The barrier layer 20 covers the top surface 12 and the side surface 14 of the redistribution layer 10.
[0062] Figure 10 The diagram shows a second mask layer 70 coated on the barrier layer 20 and patterned such that the second mask layer 70 surrounds the redistribution layer 10. The material of the second mask layer 70 is, for example, a photoresist (PR).
[0063] Figure 11The diagram shows the etching of the barrier layer 20 using a patterned second mask layer 70 as a mask.
[0064] Figure 12 The removal of the second mask layer 70 is shown.
[0065] Figure 13 It shows in Figure 12 A second dielectric layer 32 is formed on the structure shown, and an opening for exposing the barrier layer 20 is formed in the second dielectric layer 32. The material of the second dielectric layer 32 is, for example, a dielectric polymer, and the dielectric layer 30 includes a first dielectric layer 31 and a second dielectric layer 32.
[0066] Figures 14 to 19 A semiconductor structure 100 and its manufacturing process according to a second embodiment of this application are shown.
[0067] Figure 14 The steps shown in the first embodiment Figure 5 Following the steps shown, a barrier layer 20 is formed on the mask layer 60, for example, by physical vapor deposition (PVD) or sputtering. In some embodiments, the material of the barrier layer 20 is, for example, copper-graphene disclosed in prior art TW202006144A. In some embodiments, the material of the barrier layer 20 is, for example, copper-carbon nanotubes disclosed in prior art CN118385597A. Furthermore, because the barrier layer 20 is formed by sputtering, the thickness of the barrier layer 20 can be effectively controlled.
[0068] Figure 15 The diagram illustrates the formation of a redistribution layer 10 within a mask layer 60 covering a barrier layer 20, for example, via an electroplating process. The material of the redistribution layer 10 is, for example, Cu. The barrier layer 20 covers and conforms to the side surfaces 14 of the redistribution layer 10, while the top surface 12 of the redistribution layer 10 is exposed.
[0069] Figure 16 The portion of the etch-removed barrier layer 20 other than the portion located between the redistribution layer 10 and the mask layer 60 is shown, that is, the portion of the etch-removed barrier layer 20 other than the portion located on the side 14 of the redistribution layer 10.
[0070] Figure 17 The removal of the mask layer 60 is shown.
[0071] Figure 18 The etching of the seed layer 40 using the redistribution layer 10 and the barrier layer 20 as masks is shown.
[0072] Figure 19 It shows in Figure 18A second dielectric layer 32 is formed on the structure shown, and an opening is formed in the second dielectric layer 32 to expose the redistribution layer 10. The material of the second dielectric layer 32 is, for example, a dielectric polymer. The dielectric layer 30 includes a first dielectric layer 31 and a second dielectric layer 32.
[0073] Figures 20 to 23 A semiconductor structure 100 and its manufacturing process according to a third embodiment of this application are shown.
[0074] Figure 20 The steps shown in the first embodiment Figure 5 Following the steps shown, a redistribution layer 10 is formed in a patterned mask layer 60, for example, using physical vapor deposition (PVD) or sputtering processes. In some embodiments, the material of the redistribution layer 10 is, for example, copper-graphene disclosed in prior art TW202006144A. In some embodiments, the material of the redistribution layer 10 is, for example, copper-carbon nanotubes disclosed in prior art CN118385597A. Furthermore, because the redistribution layer 10 is formed using a sputtering process, the thickness of the redistribution layer 10 can be effectively controlled, preventing uneven thickness from causing localized failures during qualification testing or use. Additionally, a thinner redistribution layer 10 can be formed, improving the utilization rate of circuitry per unit volume to meet the demands of advanced high-density circuit packaging.
[0075] Figure 21 The removal of the mask layer 60 is shown.
[0076] Figure 22 The etching of the seed layer 40 using the redistribution layer 10 as a mask is shown.
[0077] Figure 23 It shows in Figure 22 A second dielectric layer 32 is formed on the structure shown, and an opening is formed in the second dielectric layer 32 to expose the redistribution layer 10. The material of the second dielectric layer 32 is, for example, a dielectric polymer, and the dielectric layer 30 includes a first dielectric layer 31 and a second dielectric layer 32.
[0078] For example, see Figure 13 and Figure 19 The embodiments of this application provide a semiconductor structure 100 in which a carbon-based barrier layer 20 covers at least a portion of the surface of a redistribution layer 10 to protect the redistribution layer 10 and improve the reliability of the semiconductor structure 100.
[0079] In some embodiments, the barrier layer 20 bonded / attached to the surface of the redistribution layer 10 holds the copper of the redistribution layer 10, thereby suppressing / reducing the electron migration effect of the redistribution layer 10 and reducing the oxidation reaction of the redistribution layer 10, thus improving product lifespan.
[0080] In some embodiments, the barrier layer 20 is a conductive layer, which is a carbon-based material with high conductivity. The conductivity of the barrier layer 20 is substantially equal to or greater than that of the redistribution layer 10.
[0081] In some embodiments, the semiconductor structure 100 further includes: a dielectric layer 30 covering the redistribution layer 10, and a barrier layer 20 disposed between the dielectric layer 30 and the redistribution layer 10.
[0082] See Figure 13 In some embodiments, the dielectric layer 30 is provided with an opening 32 that exposes the barrier layer 20.
[0083] See Figure 19 In some embodiments, the dielectric layer 30 is provided with an opening 32 that exposes the redistribution layer 10.
[0084] In some embodiments, the top surface 12 of the redistribution layer 10 faces the opening 32, and the barrier layer 20 covers the side surface 14 of the redistribution layer 10.
[0085] In some embodiments, the semiconductor structure 100 further includes a seed layer 40 disposed below the redistribution layer 10, and a barrier layer 20 covering at least a portion of the surface of the redistribution layer 10 exposed relative to the seed layer 40.
[0086] See Figure 13 In some embodiments, the barrier layer 20 covers the side of the seed layer 40.
[0087] See Figure 19 In some embodiments, the barrier layer 20 contacts the top surface of the seed layer 40, and the side surface 14 of the barrier layer 20 is aligned with the side surface of the seed layer 40.
[0088] See Figure 13 In some embodiments, the portion of the barrier layer 20 covering the side of the seed layer 40 protrudes laterally compared to the portion of the barrier layer 20 covering the redistribution layer 10.
[0089] See Figure 13 In some embodiments, the dielectric layer 30 and the redistribution layer 10 are completely separated.
[0090] See Figure 19 In some embodiments, the redistribution layer 10 contacts the dielectric layer 30 on the top surface 12 facing the opening 32.
[0091] For example, see Figure 13 and Figure 19 Embodiments of this application also provide a semiconductor structure 100, including: a redistribution layer 10; and a carbon-based barrier layer 20 covering at least a portion of the surface of the redistribution layer 10, wherein the barrier layer 20 is used to reduce oxidation of the redistribution layer 10.
[0092] In some embodiments, the semiconductor structure 100 further includes: a dielectric layer 30 covering the redistribution layer 10, and a barrier layer 20 separating at least a portion of the redistribution layer 10 from the dielectric layer 30.
[0093] In some embodiments, the barrier layer 20 isolates the side 14 of the redistribution layer 10 from the dielectric layer 30.
[0094] For example, see Figure 13 In some embodiments, the barrier layer 20 isolates the side surface 14 and top surface 12 of the redistribution layer 10 from the dielectric layer 30.
[0095] The above description is merely a preferred embodiment of this utility model and is not intended to limit the utility model. Various modifications and variations can be made to this utility model by those skilled in the art. Any modifications, equivalent substitutions, improvements, etc., made within the spirit and principles of this utility model should be included within the protection scope of this utility model.
Claims
1. A semiconductor structure, characterized in that, include: Rewire layer; A carbon-based barrier layer covers at least a portion of the surface of the redistribution layer and is conformal to the redistribution layer, the barrier layer being used to reduce electron migration and oxidation of the redistribution layer; A dielectric layer covers the redistribution layer, and a barrier layer is disposed between the dielectric layer and the redistribution layer.
2. The semiconductor structure according to claim 1, characterized in that, The barrier layer is a conductive layer.
3. The semiconductor structure according to claim 1, characterized in that, The dielectric layer has an opening that exposes the barrier layer.
4. The semiconductor structure according to claim 1, characterized in that, The dielectric layer has an opening that exposes the redistribution layer.
5. The semiconductor structure according to claim 3 or 4, characterized in that, The top surface of the redistribution layer faces the opening, and the barrier layer covers the side surface of the redistribution layer.
6. The semiconductor structure according to claim 1, characterized in that, The barrier layer is thinner than the redistribution layer.
7. The semiconductor structure according to claim 1, characterized in that, Also includes: A seed layer is disposed below the redistribution layer, and the barrier layer covers at least a portion of the surface of the redistribution layer exposed relative to the seed layer.
8. The semiconductor structure according to claim 7, characterized in that, The barrier layer covers the side of the seed layer.
9. The semiconductor structure according to claim 7, characterized in that, The barrier layer contacts the top surface of the seed layer, and the side surface of the barrier layer is aligned with the side surface of the seed layer.
10. The semiconductor structure according to claim 1, characterized in that, The barrier layer is made of copper-carbon nanotubes.
Citation Information
Patent Citations
Preparation method for network interface design of copper-based carbon nanotube composite material