Package substrate

By setting mounting grooves and embedding buffer protection structures at the edges of the glass substrate, the problem of glass substrate fragility is solved, and the mechanical force is effectively dispersed and the process is compatible during the packaging process, thereby improving product yield and high-frequency performance.

CN225021038UActive Publication Date: 2026-11-24SUZHOU GUOXIAN INNOVATION TECHNOLOGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202522760483.1
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2025-12-25
Publication Date
2026-11-24
Estimated Expiration
2035-12-25

AI Technical Summary

Technical Problem

Glass substrates are susceptible to cracks due to mechanical impact during the packaging process, and traditional protection methods affect the overall planarity and high-frequency performance of the packaging process.

Method used

A mounting groove is provided at the edge of the substrate and a buffer protection structure is embedded therein, including an embedded part and an extension part. The extension part forms a load-bearing area outside the substrate to avoid direct contact and disperse mechanical force. The material of the buffer protection structure can be optimized independently.

Benefits of technology

It reduces the risk of cracks in the glass substrate during manufacturing, maintains the global planarity and high-frequency performance of the packaging process, and improves product yield.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN225021038U_ABST
    Figure CN225021038U_ABST
Patent Text Reader

Abstract

This application provides a packaging carrier board, comprising: a substrate with a mounting groove surrounding its edge; and a buffer protection structure including an insert and an extension. The insert is disposed within the mounting groove, and the extension extends from the insert in a direction parallel to the substrate surface and away from the substrate center, extending beyond the edge of the substrate. By embedding the insert of the buffer protection structure within the mounting groove at the edge of the substrate, this application reduces the vertical height difference introduced by conventional surface mount technology (SMT) methods, thus mitigating the impact on subsequent critical processes that rely on global planarity. Furthermore, the extension of the buffer protection structure forms a load-bearing area outside the substrate edge. Throughout the manufacturing process, clamping, handling, and other mechanical forces are designed to act on this extension and are dispersed to the substrate body through the insert, thereby covering the substrate edge, preventing crack formation, and improving product yield.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This application relates to the field of semiconductor packaging technology, and more particularly to a packaging substrate. Background Technology

[0002] Compared to silicon substrates, glass substrates have advantages such as low loss, high mechanical stability, low cost, and the ability to achieve large-size and ultra-thin designs. Therefore, they have attracted widespread attention and have broad application prospects, and are used in fields such as optical communication, radio frequency modules, optoelectronic system integration, consumer electronics, electronic power amplifiers, and medical devices.

[0003] Currently, the risk of chip cracking is high and the yield is low when the packaging substrate is clamped. Utility Model Content

[0004] Based on this, this application provides a packaging substrate that reduces the risk of crack formation and improves yield.

[0005] This application provides a packaging carrier board, including: The substrate has mounting grooves arranged around its edges. The buffer protection structure includes an embedded part and an extension part. The embedded part is disposed in a mounting groove, and the extension part extends from the embedded part in a direction parallel to the surface of the substrate and away from the center of the substrate, and extends beyond the edge of the substrate.

[0006] In one embodiment, the extension extends beyond the edge of the substrate by a distance greater than or equal to 0.01 mm and less than or equal to 0.2 mm.

[0007] In one embodiment, in the extension direction of the extension, the width of the mounting groove is greater than or equal to 8 mm and less than or equal to 10 mm; in the thickness direction of the substrate, the depth of the mounting groove is greater than or equal to 50 μm and less than or equal to 150 μm.

[0008] In one embodiment, the mounting groove is a stepped groove formed by recessing from the substrate surface; and the minimum distance between the surface of the embedded part away from the bottom wall of the mounting groove and the surface of the substrate is less than or equal to 10 μm.

[0009] In one embodiment, the buffer protection structure includes a layer of buffer material and an adhesive layer stacked together, with the adhesive layer located between the buffer material layer and the mounting groove.

[0010] In one embodiment, the cushioning material layer includes at least one of copper-clad laminate, metal layer, and organic polymer.

[0011] In one embodiment, the buffer material layer is spaced apart from the sidewall of the mounting groove in the extending direction of the extension.

[0012] In one embodiment, the packaging carrier further includes: A redistribution layer is disposed on at least one side of a substrate, including a trace layer and a dielectric layer. The dielectric layer is at least partially located on the side of the buffer protection structure away from the substrate, and the orthographic projection of the dielectric layer on the substrate at least partially overlaps with the orthographic projection of the buffer protection structure on the substrate; and the orthographic projection of the edge of the extension on the substrate is located outside the orthographic projection of the edge of the dielectric layer on the substrate.

[0013] In one embodiment, the dielectric layer fills the gap between the buffer material layer and the sidewall of the mounting groove.

[0014] In one embodiment, the substrate is a glass substrate, the glass substrate includes glass through holes, and the packaging carrier further includes a seed layer and a conductive structure disposed in the glass through holes. The conductive structure fills the glass through holes, and the seed layer covers the hole walls of the glass through holes and part of the surface of the glass substrate.

[0015] The packaging substrate provided in this application offers edge protection for the substrate during manufacturing through a buffer protection structure. The embedded portion of the buffer protection structure is integrated into the mounting groove at the edge of the substrate, reducing the vertical height difference introduced by traditional surface mount solutions and minimizing the impact on subsequent critical processes that rely on global planarity. Furthermore, the extension of the buffer protection structure forms a load-bearing area outside the substrate edge. Throughout the manufacturing process, clamping, handling, and other mechanical forces are designed to act on this extension and are dispersed to the substrate body through the embedded portion, thereby covering the substrate edge, preventing crack formation, and improving product yield.

[0016] Meanwhile, the buffer protection structure can use optimized materials different from those on the substrate, achieving independent design and performance improvement of the protection function. Attached Figure Description

[0017] To more clearly illustrate the technical solutions in this application or related technologies, the drawings used in the description of the embodiments or related technologies will be briefly introduced below. Obviously, the drawings described below are only embodiments of this application. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.

[0018] Figure 1 This is a schematic diagram of the packaging carrier board in one embodiment of this application; Figure 2 yes Figure 1 A magnified view of a section at point A in the middle; Figure 3 yes Figure 1 Top view of the intermediate packaging carrier board; Figure 4 This is a schematic diagram of the packaging carrier board in another embodiment of this application; Figure 5 This is a schematic diagram of the packaging carrier board in another embodiment of this application; Figure 6 This is a schematic diagram of the packaging carrier board in another embodiment of this application; Figure 7 This is a flowchart illustrating a method for manufacturing a packaging carrier board according to another embodiment of this application; Figure 8 This is a schematic diagram of the process steps for manufacturing a packaging substrate according to another embodiment of this application.

[0019] Marker explanation: 100. Packaging carrier; 10. Substrate; 101. Glass via; 11. Edge; 12. Mounting slot; 20. Buffer protection structure; 201. Embedded part; 202. Extension part; 21. Buffer material layer; 22. Adhesive layer; 30. Conductive structure; 31. Seed layer; 40. Redundancy layer; 41. Trajectory layer; 42. Dielectric layer; D. Extension distance; W. Slot width. Detailed Implementation

[0020] To make the objectives, technical solutions, and advantages of this application clearer, the following detailed description is provided in conjunction with specific embodiments and the accompanying drawings.

[0021] It should be noted that, unless otherwise defined, the technical or scientific terms used in the embodiments of this application should have the ordinary meaning understood by one of ordinary skill in the art to which this application pertains. The terms "first," "second," and similar terms used in the embodiments of this application do not indicate any order, quantity, or importance, but are merely used to distinguish different components. Terms such as "comprising" or "including" mean that the element or object preceding the word encompasses the elements or objects listed after the word and their equivalents, without excluding other elements or objects. Terms such as "connected" or "linked" are not limited to physical or mechanical connections, but can include electrical connections, whether direct or indirect. Terms such as "upper," "lower," "left," and "right" are only used to indicate relative positional relationships; when the absolute position of the described object changes, the relative positional relationship may also change accordingly.

[0022] With the rapid development of information technology, the demands on chip computing power, bandwidth, energy efficiency, and integration density are increasing exponentially. Traditional organic packaging substrates face bottlenecks in handling ultra-high frequency signal transmission (e.g., >100GHz) and high-density interconnects due to their high dielectric loss and limited dimensional stability. Against this backdrop, glass core substrates stand out with their unique material properties and are considered the preferred substrate material for next-generation advanced packaging. Their core advantages include: extremely low dielectric constant and loss factor, which can significantly reduce signal transmission delay and attenuation, meeting the stringent requirements of AI chips for ultra-high bandwidth and low-power interconnects; ultra-high surface flatness and dimensional stability, supporting the fabrication of submicron-level fine lines and multi-layer stacking alignment; excellent insulation resistivity, which can effectively isolate high-frequency signals and reduce crosstalk; adjustable coefficient of thermal expansion, which can achieve good matching with chip materials such as silicon and compound semiconductors, improving thermomechanical reliability; and optical transparency and compatibility with optical waveguide processes, which provide possibilities for optoelectronic co-packaging and embedding passive devices.

[0023] However, while glass materials possess excellent electrical and physical properties, several inherent key characteristics also pose fundamental challenges to industrialization: (a) high brittleness and low fracture toughness: glass is extremely sensitive to surface and edge defects. Minor scratches or impact stress concentrations can easily lead to catastrophic crack propagation and overall shattering, posing a significant threat to mechanical operations (such as clamping, handling, and testing) during production; (b) softening at high temperatures: although glass has a high transition temperature, its rigidity decreases in certain encapsulation processes (such as high-temperature reflow soldering and thermoforming bonding). Traditional surface-mount protective structures may fail or shift at high temperatures due to adhesive softening or material creep; (c) surface chemical inertness: compared to silicon and organic materials, glass surfaces have weaker adhesion to certain metals or polymers, requiring special interface treatments to ensure interlayer bonding strength.

[0024] To address the issue of fragile glass substrate edges, related technologies typically employ a polymer or metal protective frame attached to the substrate edge surface. Through in-depth process testing and failure analysis, the inventors of this application discovered the following drawbacks of this approach: First, the attached protective frame introduces a vertical height difference on the substrate surface. This height difference can disrupt subsequent critical processes that rely on global planarity. For example, it can cause uneven photoresist thickness during spin coating; focal plane shift and pattern distortion during exposure; interface voids during vacuum lamination of multilayer dielectric films; and dish-shaped indentations or erosion during chemical mechanical polishing (CMP). Second, the adhesive interface of the attached structure is prone to aging and debonding after experiencing high temperatures, humidity, and stress cycles during the packaging process, leading to a decrease in protective reliability over time. Furthermore, the protective frame itself may introduce unwanted parasitic capacitance or electromagnetic interference, affecting high-frequency performance.

[0025] In view of this, this application provides a packaging substrate to solve the problem of cracks in glass substrates caused by mechanical impact at the edges, while maintaining surface flatness.

[0026] This application provides a packaging carrier board 100. For example... Figures 1 to 3 As shown, the packaging carrier 100 includes a substrate 10 and a buffer protection structure 20. A mounting groove 12 is provided on the edge 11 of the substrate 10. The buffer protection structure 20 includes an insert portion 201 and an extension portion 202. The insert portion 201 is disposed within the mounting groove 12, and the extension portion 202 extends from the insert portion 201 in a direction parallel to the surface of the substrate 10 and away from the center of the substrate 10, extending beyond the edge 11 of the substrate 10 to form a load-bearing area for external clamping.

[0027] Specifically, the encapsulation carrier 100 includes a substrate 10, which is typically a plate-like structure with a highly flat main surface, and its material can be glass, silicon, or an organic insulating material. In the main application scenarios addressed in this application, the substrate 10 is preferably a glass substrate, which has excellent electrical properties and dimensional stability, but also exhibits inherent brittleness. The edge 11 of the substrate 10, i.e., its outer contour perimeter, is a structural weak point.

[0028] To address the issue of edge 11 being prone to breakage during manufacturing due to clamping and handling, this application forms a surrounding mounting groove 12 in the edge 11 region of the substrate 10. Specifically, the mounting groove 12 is a closed-loop groove that surrounds the substrate edge 11, with its enclosed area defining the core functional area of ​​the substrate 10. The mounting groove 12 is a cavity structure formed by recessing inwards (i.e., towards the center of the substrate) from the main working surface (e.g., the upper surface) of the substrate 10.

[0029] The packaging substrate 100 also includes a separate buffer protection structure 20, which comprises two physically and functionally related parts: an insert 201 and an extension 202. The insert 201 is shaped and sized to match the cavity of the mounting groove 12, allowing it to be received and disposed within the groove, typically secured by adhesive or other fastening methods. The extension 202 is integrally connected to the insert 201 and extends outward from one end of the insert 201 near the edge 11 of the substrate 10 (i.e., the outer end), in a direction parallel to the surface of the substrate 10 (as shown in the X or Y direction). As a result of this extension, the extension 202 is at least partially suspended beyond the edge 11 of the substrate 10 in the horizontal direction.

[0030] The packaging substrate 100 provided in this application embodiment integrates the embedded portion 201 of the buffer protection structure 20 into the mounting groove 12 of the substrate 10, enabling the exposed surface of the buffer protection structure 20 to be coplanar or nearly coplanar with the surface of the substrate 10. This avoids introducing additional protrusions and height differences on the substrate surface, thereby reducing potential interference to subsequent critical processes that are sensitive to surface topology, such as photolithography, lamination, and thin film deposition.

[0031] Furthermore, the extension 202 forms a platform outside the substrate edge 11 specifically designed to withstand external mechanical forces. During production, the clamping force of the mechanical fixture is designed to act on the extension 202. The mechanical force is transmitted through the extension 202 to the insert 201, and then dispersed to the body of the substrate 10. Throughout the stress process, the fragile substrate edge 11 is covered from above by the extension 202, avoiding direct contact with hard tools and stress concentration, thus reducing the risk of crack formation from a physical structural perspective.

[0032] Meanwhile, the buffer protection structure 20, as an independent component, can be made of a different material than the substrate 10, allowing for optimization based on requirements such as mechanical buffering and thermal expansion matching, without being limited by the performance of the substrate material itself.

[0033] Specifically, the substrate 10 is made of glass.

[0034] The glass substrate in this embodiment provides a platform for realizing ultra-short-pitch, low-loss silicon bridges or high-density redistribution layers between chips, shortening the signal transmission path, reducing power consumption, and improving computing power and bandwidth. The low-loss characteristics of the glass substrate are suitable for millimeter-wave antenna arrays.

[0035] Specifically, the packaging substrate 100 of this application embodiment can be widely used in advanced packaging fields where the integrity of the substrate edge is highly critical. For example, in the manufacturing of large-panel MEMS (microelectromechanical systems) that requires multiple clamping, alignment and dicing, it can effectively prevent substrate breakage caused by edge stress concentration. In the packaging of high-frequency, high-density glass-based chips for AI and 6G, it provides edge protection while ensuring the global planarity required for subsequent key processes such as photolithography and thin film deposition, thus ensuring the processing yield of the circuit.

[0036] In some embodiments, such as Figure 2 As shown, the extension distance D of the extension 202 beyond the edge 11 of the substrate 10 is 0.01 mm to 0.2 mm.

[0037] The extension distance D is defined as the minimum horizontal distance between the outer edge of the extension 202 and the edge 11 of the substrate 10 in a direction parallel to the main surface of the substrate 10 and perpendicular to the edge 11 of the substrate. The buffer protection structure 20 is fabricated using a high-precision process and mounted in the mounting groove 12 using precision equipment with visual alignment. Through the above process control, it can be ensured that the extension distance D satisfies: 0.01mm ≤ D ≤ 0.2mm. In specific implementations, the extension distance D can be any value within this range, such as 0.01mm, 0.05mm, 0.08mm, 0.12mm, 0.15mm, 0.18mm, or 0.2mm.

[0038] The range of the extension distance D is determined based on a comprehensive consideration of protection reliability, process compatibility, and structural mechanical performance. Firstly, the extension distance D must be able to accommodate various tolerances present in industrial production systems, including the repeatability of the robotic arm, the dimensional tolerances of the substrate 10, and the mounting alignment errors of the buffer protection structure 20 itself. Setting the lower limit of D to 0.01 mm ensures that under any expected production conditions, the contact surface of the external fixture can completely fall on the extension 202, thereby maintaining a defined safety gap between the substrate edge 11 and the fixture to prevent accidental scratches. If D is less than this value, for example, 0.005 mm, the protection function becomes unreliable and there is a risk of failure. Secondly, the extension 202 is an additional structure that extends beyond the substrate design boundary. In high-efficiency production methods such as panel-level packaging, an excessively large extension distance will excessively encroach on the cutting space between adjacent device units, affecting layout density and material utilization. Setting the upper limit to 0.2 mm balances the contradiction between protection function and production efficiency while providing sufficient protection margin. Thirdly, if D is too large (e.g., >0.2mm), a deep gap will form below the extension 202, which may lead to chemical residues during wet cleaning or electroplating processes, potentially causing subsequent contamination or corrosion. Furthermore, from a mechanical perspective, the extension 202 can be considered a cantilever beam. Preferably, controlling the extension distance D to 0.08mm helps maintain sufficient rigidity and stability in the extension 202, minimizing deformation during clamping and providing stable support.

[0039] Therefore, limiting the extension distance D to the range of 0.01mm to 0.2mm helps to achieve reliable protection, good process compatibility, and reasonable layout density.

[0040] In one embodiment, in the extending direction of the extension 202, the width W of the mounting groove 12 is greater than or equal to 8 mm and less than or equal to 10 mm. In the thickness direction of the substrate 10, the depth H of the mounting groove 12 is greater than or equal to 50 μm and less than or equal to 150 μm.

[0041] Specifically, in the same horizontal direction as the extension 202 extending outward, the mounting groove 12 has a groove width W. This groove width W is defined as the maximum distance between the sidewall of the mounting groove 12 near the center of the substrate and the corresponding edge of the substrate at the opening of the mounting groove, and satisfies: 8mm ≤ W ≤ 10mm. The groove width W can be any value within this range, such as 8mm, 9mm, or 10mm.

[0042] In the thickness direction of the substrate 10, the groove depth H of the mounting groove 12 satisfies: 50μm≤H≤150μm. The groove depth H can be any value within this range, such as 50μm, 100μm, 150μm, etc.

[0043] The width and depth design of the mounting slot 12 allows the buffer protection structure 20 to form a surrounding reinforcement frame with a certain cross-sectional area. This reinforcement frame structure can effectively suppress edge stress concentration generated in the substrate during subsequent thinning, lamination and other processes, reduce the risk of overall board warping, and improve its transmission and processing stability in the production line. At the same time, the ample space allows for the integration of a wider functional metal layer within the buffer material layer 21, such as forming a large-board-level ring ground layer or power busbar.

[0044] If the slot width W is too narrow (e.g., <3mm), both structural strength and functional integration will be insufficient; if the slot width W is too wide (e.g., >10mm), it will unnecessarily erode the core area of ​​the chip wiring and may weaken the overall rigidity of the substrate, increasing the risk of warping. Therefore, using a width range of 8mm to 10mm and a depth range of 50μm to 150μm can balance strength and wiring space.

[0045] In some embodiments, the mounting groove 12 is a stepped groove recessed from the surface of the substrate 10. Meanwhile, the height difference between the surface of the embedding portion 201 away from the bottom wall of the mounting groove 12 and the surface of the substrate is less than or equal to 10 μm.

[0046] Specifically, through precision machining and mounting process control, the height difference between the surface of the embedded part 201 and the same-side surface of the substrate 10 is less than or equal to 10 μm. When buffer protection structures 20 are provided on both sides of the substrate 10, the upper surface of the buffer protection structure 20 is coplanar or nearly coplanar with the upper surface of the substrate 10. The lower surface of the buffer protection structure 20 is coplanar or nearly coplanar with the lower surface of the substrate 10.

[0047] To eliminate the vertical height difference introduced by traditional surface mount technology (SMT) methods, the mounting groove 12 is preferably a stepped groove recessed from the surface of the substrate 10. Through precision machining and mounting control, the height difference between the surface of the embedded part 201 and the surface of the substrate 10 is less than or equal to 10 μm. This not only achieves functional "zero height difference" but also avoids interference with subsequent critical processes such as photolithography and CMP.

[0048] In some embodiments, the buffer protection structure 20 includes a buffer material layer 21 and an adhesive layer 22 stacked together, with the adhesive layer 22 located between the buffer material layer 21 and the mounting groove 12.

[0049] like Figure 4 As shown, the buffer protection structure 20 includes a buffer material layer 21 and an adhesive layer 22 stacked together. The adhesive layer 22 is located between the buffer material layer 21 and the bottom wall of the mounting groove 12, serving as a fixed connection.

[0050] Furthermore, the cushioning material layer 21 includes at least one of copper-clad laminate, metal layer and organic polymer.

[0051] Specifically, the adhesive layer 22 is located between the buffer material layer 21 and the bottom wall of the mounting groove 12, and is used for primary fixation. The material of the buffer material layer 21 can be selected according to specific needs. For example, the buffer material layer 21 can be made of copper clad laminate (CCL), a composite electronic material made by laminating conductive copper foil on one or both sides of an insulating substrate, which serves as a substrate for structural support, electrical insulation, and circuit conduction. The insulating substrate portion of the CCL can be, for example, a glass fiber reinforced epoxy resin laminate. Using CCL as the buffer material layer 21 provides high strength and high process compatibility. Alternatively, the buffer material layer 21 can be made of a metal layer, such as copper or stainless steel, providing extremely high rigidity and excellent thermal and electrical conductivity. Alternatively, the buffer material layer 21 can be made of an organic polymer, such as polyimide, providing high elasticity and fatigue resistance.

[0052] For example, the buffer material layer 21 can be designed to include a ground layer and / or a power layer. This means that the buffer structure is not only a mechanical protector, but also an integrated edge electrical function module for electromagnetic shielding, noise filtering, or auxiliary power supply. When the buffer material layer 21 needs to be integrated with the conductive structure in the substrate 10, a conductive seed layer (not shown) can be pre-fabricated on the inner surface of the mounting groove 12 and on the buffer material layer 21 so that the metal layer in the buffer protection structure 20 can be electrically integrated with the redistribution layer or grounding network on the substrate 10 by electroplating.

[0053] In some embodiments, the buffer material layer 21 is spaced apart from the sidewall of the mounting groove 12 in the extending direction of the extension 202.

[0054] In some embodiments, the adhesive layer 22 is located only between the cushioning material layer 21 and the bottom wall of the mounting groove 12. In other embodiments, the adhesive layer 22 may simultaneously fill the space between the cushioning material layer 21 and the bottom and side walls of the mounting groove 12.

[0055] Specifically, when the cushioning material layer 21 is placed in the mounting groove 12, a circumferential gap is formed between the cushioning material layer 21 and the side wall of the mounting groove 12. This ensures that there is no direct contact between the cushioning material layer 21 and the groove wall (including the bottom wall and / or side wall) of the mounting groove 12.

[0056] The resulting spacing structure provides a buffer space for dimensional changes caused by the difference in thermal expansion coefficients between the buffer material layer 21 and the substrate 10 (especially the glass core board), thus avoiding interface stress concentration caused by rigid extrusion during thermal processing. It also reduces the requirements for the processing accuracy and mounting alignment accuracy of the buffer material layer 21, improving the process tolerance.

[0057] It should be noted that the spacing can be due to manufacturing tolerances, but is more preferably an active design feature. That is, the size of the embedding portion 201 of the cushioning material layer 21 is designed to be slightly smaller than the inner cavity size of the mounting groove 12 to allow space for stress buffering and thermal expansion. In this case, the adhesive layer 22 primarily provides fixation at the bottom (Z direction), while lateral (X / Y directions) fixation and cushioning can be achieved by the subsequently filled medium layer 42. In some embodiments, such as Figure 5 , Figure 6 As shown, the substrate 10 is a glass substrate, which includes a glass through-hole 101. The packaging carrier 100 also includes a conductive structure 30 and a seed layer 31 disposed in the glass through-hole 101. The conductive structure 30 fills the glass through-hole 101, and the seed layer 31 covers the hole wall of the glass through-hole 101 and part of the surface of the glass substrate.

[0058] Specifically, the conductive structure 30 penetrates the substrate 10 along the thickness direction (Z direction in the figure). The seed layer 31 is mainly located between the conductive structure 30 and the substrate 10. The seed layer 31 may include an adhesive sublayer and a conductive sublayer, with the adhesive sublayer located between the substrate 10 and the conductive sublayer.

[0059] To ensure excellent electrical connection reliability and long-term interface stability between the conductive structure 30 and the substrate 10, a seed layer 31 is provided between the filler metal of the conductive structure 30 and the via wall of the substrate 10. The seed layer 31 adopts a double-layer structure design, specifically including an adhesion sublayer and a conductive sublayer formed sequentially. The adhesion sublayer (such as a titanium, chromium, or tantalum thin film formed by sputtering) directly contacts and covers the glass via wall of the via. Its main function is to form a strong chemical bond with the glass surface through its high reactivity, providing excellent adhesion and preventing metal layer peeling during subsequent processes or use. The conductive sublayer (such as a sputtered copper layer) is deposited on the adhesion sublayer. Its function is to provide a continuous, uniform, and low-resistance conductive starting surface for subsequent large-scale filling of the via to form the main body of the conductive structure 30 by electroplating, ensuring that the electroplated metal can grow and fill the via without defects from the bottom to the top of the via. The dense seed layer 31 itself forms part of the vertical interconnect, which helps to reduce the series resistance of the entire via and improve the efficiency and signal transmission quality of the large board-level power distribution network.

[0060] Furthermore, the packaging substrate 100 also includes a redistribution layer 40, which is disposed on one side of the substrate 10, or on opposite sides of the substrate 10. The redistribution layer 40 includes a wiring layer 41 and a dielectric layer 42. The wiring layer 41 is electrically connected to the conductive structure 30. The orthographic projection of the dielectric layer 42 on the substrate 10 at least partially overlaps with the orthographic projection of the buffer protection structure 20 on the substrate 10. The orthographic projection of the edge 11 of the extension 202 on the substrate 10 is located outside the orthographic projection of the edge 11 of the dielectric layer 42 on the substrate 10.

[0061] Furthermore, the medium layer 42 fills the gap between the buffer material layer 21 and the sidewall of the mounting groove 12.

[0062] Specifically, a glass via 101 extending through the thickness of the substrate 10 is provided, and a conductive structure 30 is filled within the glass via 101. For example, the substrate 10 is a glass substrate, the glass via 101 is TGV, and the conductive structure 30 is a conductive pillar structure formed by filling the glass via 101 with metal (such as copper). A redistribution layer 40 is formed on one or both surfaces of the substrate 10. The redistribution layer 40 includes a wiring layer 41 for wiring and a dielectric layer 42 for insulation. The wiring layer 41 is electrically connected to the conductive structure 30, realizing vertical transmission and horizontal redistribution of signals. The orthographic projection of the dielectric layer 42 at least partially overlaps with the orthographic projection of the buffer protection structure 20, meaning that the dielectric layer 42 covers the buffer protection structure 20 during fabrication. The buffer protection structure 20 is installed first, followed by the redistribution layer 40. This ensures that the substrate edges are safe during the delicate circuit fabrication process. That is, edge protection is completed first, followed by wiring processing. Meanwhile, the edge projection of the extension 202 is outside the edge projection of the medium layer 42, which ensures that the extension 202, as a functional part of the mechanical clamping area, is not completely covered by the medium layer 42, thereby ensuring that the clamping tool can act directly and reliably on the extension 202.

[0063] In the process of forming the redistribution layer 40, the dielectric material constituting the dielectric layer 42 (such as polyimide or photosensitive dielectric material) naturally flows into and fills the gap between the buffer material layer 21 and the mounting groove 12 through spin coating, curing and other steps. After curing, the dielectric layer 42 firmly anchors the buffer material layer 21 in the mounting groove 12, realizing structural fixation; on the other hand, its own elastic modulus can act as an excellent stress buffer layer, further absorbing and dispersing the mechanical clamping force or thermal stress transmitted from the extension 202, thereby providing double protection for the brittle edges of the substrate 10.

[0064] This application also provides a method for manufacturing a packaging substrate, which is used to manufacture the packaging substrate 100 in any of the above embodiments.

[0065] like Figure 7 and Figure 8 As shown, the method for manufacturing the packaging substrate 100 includes the following steps: Step S10: Provide a substrate 10 and form a surrounding mounting groove 12 on the edge 11 of the substrate 10; Step S20: Fix the buffer protection structure 20 in the mounting groove 12, and make a part of the buffer protection structure 20 extend beyond the edge 11 of the substrate 10 in a direction parallel to the surface of the substrate 10 to form an extension 202.

[0066] Specifically, first, a substrate 10 is provided, and a surrounding mounting groove 12 is formed on the edge 11 of the substrate 10, for example, by processes such as laser ablation, photolithography, and etching. Second, a buffer protection structure 20 is fixed within the mounting groove 12. During this process, by controlling process parameters, a portion of the buffer protection structure 20 extends beyond the edge 11 of the substrate 10 in a direction parallel to the surface of the substrate 10, thereby forming an extension 202. Specifically, a surrounding mounting groove is formed on the edge of the substrate; the prefabricated buffer protection structure 20 is fixed within the groove, and the formation of the horizontal extension is controlled. This can be achieved by applying an adhesive, bonding a buffer material layer, and then curing.

[0067] In this case, by forming a mounting groove 12 at the edge 11 of the substrate 10, the buffer protection structure 20 is fixed in the mounting groove 12 and a horizontal extension 202 is formed, which enables the buffer protection structure 20 to be embedded and to bear force externally.

[0068] Furthermore, in step S20, the buffer protection structure 20 is fixed in the mounting groove 12, including the following sub-steps: Step S21: Apply adhesive to the mounting groove 12; Step S22: Attach the buffer material layer 21 into the mounting groove 12 coated with adhesive.

[0069] The fixing step may specifically include: applying adhesive to the mounting groove 12; then attaching a pre-made buffer material layer 21 (such as a cut copper-clad laminate) to the mounting groove 12 with adhesive; and then curing the adhesive to form an adhesive layer 22, thus completing the fixing process, thereby forming a complete process flow of "grooving-applying adhesive-attaching-curing".

[0070] In some embodiments, after step S20, the manufacturing method further includes the following steps: Step S30: A redistribution layer 40 is formed on at least one side of the substrate 10; wherein, forming the redistribution layer 40 includes forming a dielectric layer 42 and a wiring layer 41 located in the dielectric layer 42, the wiring layer 41 being electrically connected to the conductive structure 30 in the substrate 10; and, the patterning process of the dielectric layer 42 is controlled such that the orthographic projection of the dielectric layer 42 on the substrate 10 at least partially overlaps with the orthographic projection of the buffer protection structure 20 on the substrate 10, while the orthographic projection of the edge of the extension 202 on the substrate 10 is located outside the orthographic projection of the edge of the dielectric layer 42 on the substrate 10.

[0071] The process involves first installing the edge protection structure 20, followed by the fine redistribution layer 40, ensuring that the edge 11 of the substrate 10 remains protected throughout the entire manufacturing cycle.

[0072] It should be noted that the above description describes some embodiments of this application. Other embodiments are within the scope of the appended claims. In some cases, the actions or steps recorded in the claims can be performed in a different order than that shown in the above embodiments and still achieve the desired result. Furthermore, the processes depicted in the drawings do not necessarily require a specific or sequential order to achieve the desired result. In some embodiments, multitasking and parallel processing are also possible or may be advantageous.

[0073] The embodiments described above are merely illustrative of several implementation methods of this application, and while the descriptions are specific and detailed, they should not be construed as limiting the scope of this application. It should be noted that those skilled in the art can make various modifications and improvements without departing from the technical concept of this application, and these all fall within the protection scope of this application. Therefore, the protection scope of this patent application should be determined by the appended claims.

Claims

1. A packaging carrier board, characterized in that, include: A substrate, wherein a mounting groove is provided around the edge of the substrate; A buffer protection structure includes an embedded portion and an extension portion. The embedded portion is disposed within the mounting groove, and the extension portion extends from the embedded portion in a direction parallel to the surface of the substrate and away from the center of the substrate, and extends beyond the edge of the substrate.

2. The packaging carrier board according to claim 1, characterized in that, The extension beyond the edge of the substrate extends by a distance greater than or equal to 0.01 mm and less than or equal to 0.2 mm.

3. The packaging carrier board according to claim 1, characterized in that, In the extension direction of the extension portion, the width of the mounting groove is greater than or equal to 8 mm and less than or equal to 10 mm; in the thickness direction of the substrate, the depth of the mounting groove is greater than or equal to 50 μm and less than or equal to 150 μm.

4. The packaging carrier board according to claim 1, characterized in that, The mounting groove is a stepped groove formed by recessing from the surface of the substrate; the minimum distance between the surface of the embedded part away from the bottom wall of the mounting groove and the surface of the substrate is less than or equal to 10 μm.

5. The packaging carrier board according to claim 1, characterized in that, The buffer protection structure includes a layer of buffer material and an adhesive layer stacked together, with the adhesive layer located between the buffer material layer and the mounting groove.

6. The packaging carrier board according to claim 5, characterized in that, The cushioning material layer includes at least one of copper-clad laminate, metal layer and organic polymer.

7. The packaging carrier board according to claim 5, characterized in that, In the extending direction of the extension, the buffer material layer is spaced apart from the sidewall of the mounting groove.

8. The packaging carrier board according to claim 7, characterized in that, The packaging carrier also includes: A redistribution layer is disposed on at least one side of the substrate, comprising a trace layer and a dielectric layer, wherein the dielectric layer is at least partially located on the side of the buffer protection structure away from the substrate, and the orthographic projection of the dielectric layer on the substrate at least partially overlaps with the orthographic projection of the buffer protection structure on the substrate; and the orthographic projection of the edge of the extension on the substrate is located outside the orthographic projection of the edge of the dielectric layer on the substrate.

9. The packaging carrier board according to claim 8, characterized in that, The medium layer fills the gap between the buffer material layer and the sidewall of the mounting groove.

10. The packaging carrier board according to claim 1, characterized in that, The substrate is a glass substrate, the glass substrate includes glass through holes, the packaging carrier further includes a seed layer and a conductive structure disposed in the glass through holes, the conductive structure fills the glass through holes, and the seed layer covers the hole wall of the glass through holes and part of the surface of the glass substrate.