Packaging structure

By changing the right angles of the wafer to chamfers and combining this with plasma etching to form periodic undulating ripples, the problem of easy breakage of the dielectric layer was solved, improving the yield and reliability of the packaging structure.

CN225021042UActive Publication Date: 2026-11-24ADVANCED SEMICON ENG INC
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202521789437.8
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2025-08-21
Publication Date
2026-11-24
Estimated Expiration
2035-08-21

AI Technical Summary

Technical Problem

In existing technologies, the dielectric layer of 3D packaging structures experiences excessive structural stress at right angles on the wafer, leading to easy breakage of the dielectric layer and affecting the yield and reliability of the packaging structure.

Method used

By changing the right angles of the wafer to chamfers, the structural stress at the wafer corners corresponding to the dielectric layer is reduced. An inorganic dielectric layer is formed by chemical vapor deposition to cover the wafer, and periodic undulating ripples are formed by plasma etching to enhance the bonding force.

Benefits of technology

This effectively prevents the dielectric layer from cracking at the corners of the wafer, improves the yield and reliability of the packaging structure, and reduces the risk of cracking in subsequent processes.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN225021042U_ABST
    Figure CN225021042U_ABST
Patent Text Reader

Abstract

This invention provides a packaging structure comprising: a substrate; a plurality of spaced-apart wafers, the active surfaces of which are co-bonded to the substrate, the sidewalls and back surfaces of which are connected by chamfering; and a dielectric layer covering the wafers, wherein the top surface of the dielectric layer has a recess corresponding to the gap between adjacent wafers. The purpose of this invention is to provide a packaging structure that at least improves the yield of the packaging structure.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This utility model relates to a packaging structure. Background Technology

[0002] With the development of modern technology, the previous 2.5D input / output (I / O) count can no longer meet market demands, leading to a higher demand for 3D stacking. This has given rise to Hybrid Bonding (HBI) technology. In this technology, a passivation oxide layer is deposited using chemical vapor deposition (CVD) to cover the inorganic substrate and fill the gaps between components. Compared to molding technology, using inorganic layers (such as SiO, SiN, etc.) to cover components reduces the filling of complex organic compounds, which is a major trend in advanced packaging. Utility Model Content

[0003] In view of the problems existing in the related technologies, the purpose of this utility model is to provide a packaging structure to at least improve the yield of the packaging structure.

[0004] To achieve the above objectives, the present invention provides a packaging structure comprising: a substrate; a plurality of spaced-apart wafers, wherein the active surfaces of the wafers are mixed and bonded to the substrate, and the sidewalls and back surfaces of the wafers are connected by chamfering; and a dielectric layer covering the wafers, wherein the top surface of the dielectric layer has a recess corresponding to the gap between adjacent wafers.

[0005] In some embodiments, the active surface of the wafer has a first pad, and the surface of the substrate has a second pad, wherein the first pad and the second pad are in direct contact and partially misaligned.

[0006] In some embodiments, the sidewalls and chamfered surfaces of the wafer have periodic undulating patterns.

[0007] In some embodiments, the sidewalls and the back surface of the wafer are perpendicular.

[0008] In some embodiments, the angle between the chamfer and the sidewall is different from the angle between the chamfer and the back face.

[0009] In some embodiments, the angle between the chamfer and the sidewall is greater than the angle between the chamfer and the back face.

[0010] In some embodiments, the packaging structure further includes a redistribution layer electrically connected to the surface of the substrate opposite to the wafer.

[0011] In some embodiments, the angle between the chamfer and the sidewall, and the angle between the chamfer and the back surface, are obtuse angles.

[0012] In some embodiments, the roughness of the chamfer is greater than the roughness of the back surface.

[0013] In some embodiments, the roughness of the chamfer is the same as the roughness of the sidewall.

[0014] The beneficial technical effects of this utility model are as follows:

[0015] The embodiments of this application change the included angle between the sidewall and the back surface of the wafer to a chamfer, which can solve or reduce the problem of cracking caused by excessive stress at the corner of the wafer corresponding to the dielectric layer, and avoid damage to the dielectric layer. Attached Figure Description

[0016] To more clearly illustrate the technical solutions in the embodiments of this application or the prior art, the drawings used in the embodiments will be briefly described below. Obviously, the drawings described below are only some embodiments of this application. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort. It is worth noting that, according to industry standard practice, the components are not drawn to scale and are only used for illustrative purposes. In fact, for clarity of discussion, the dimensions of the components can be arbitrarily increased or decreased.

[0017] Figure 1 The image shows a wafer being cut along the dashed line.

[0018] Figure 2 The image shows a single wafer obtained after cutting.

[0019] Figure 3 This illustrates bonding a wafer to a substrate.

[0020] Figure 4 The formation of the dielectric layer is shown.

[0021] Figure 5 It shows Figure 4 Electron micrograph of a portion of the structure shown.

[0022] Figure 6 and Figure 7A The back-end process is shown, in which Figure 7A A side view of the carrier, carrier film, and wafer is shown.

[0023] Figure 7B Electron micrographs of parts of the finished product, taken using a scanning electron microscope, are shown.

[0024] Figure 8 A top view of the incoming wafers is shown.

[0025] Figure 9 A side view of two adjacent wafers is shown.

[0026] Figure 10 The formation of a chamfer is shown.

[0027] Figure 11 A side view of the monolithic wafer 10 is shown.

[0028] Figure 12 This illustrates bonding wafer 10 onto substrate 20.

[0029] Figure 13 The formation of the dielectric layer is shown.

[0030] Figure 14 It shows Figure 13 Electron micrograph of a portion of the structure shown.

[0031] Figure 15 It shows Figure 14 A magnified view of region A in the middle.

[0032] Figure 16 It shows the corresponding Figure 12 Cross-sectional view of the steps shown.

[0033] Figure 17 It shows the corresponding Figure 13 Cross-sectional view of the steps shown.

[0034] Figure 18 It shows that Figure 17 The structure shown is bonded to the glass substrate via an adhesive layer.

[0035] Figure 19 The substrate thinning process is shown.

[0036] Figure 20 The formation of the interlayer dielectric layer is shown.

[0037] Figure 21 The formation of the redistribution layer and the molding layer is shown.

[0038] Figure 22 The formation of bumps and solder balls is shown.

[0039] Figure 23 The packaging structure according to an embodiment of this application is shown.

[0040] Figure 24 This demonstrates the use of a blade to directly slit a wafer.

[0041] Figure 25 This illustrates a monolithic chip.

[0042] Figure 26 It shows in Figure 25 After the steps shown, the right angle at the top of the wafer is cut into a chamfer. Detailed Implementation

[0043] To better understand the spirit of the embodiments of this application, the following description is based on some preferred embodiments of this application.

[0044] Embodiments of this application will be described in detail below. Throughout this specification, identical or similar components and components having identical or similar functions are indicated by similar reference numerals. The embodiments described herein with reference to the accompanying drawings are illustrative and diagrammatic in nature and are intended to provide a basic understanding of this application. The embodiments of this application should not be construed as limiting this application.

[0045] The terms “approximately,” “generally,” “substantial,” “substantial,” “about,” and “approximately” used herein are used to indicate and explain minor variations. For example, when used in conjunction with numerical values, the above terms may refer to a range of variation less than or equal to ±10% of the corresponding numerical value, such as less than or equal to ±5%, less than or equal to ±4%, less than or equal to ±3%, less than or equal to ±2%, less than or equal to ±1%, less than or equal to ±0.5%, less than or equal to ±0.1%, or less than or equal to ±0.05%. As another embodiment, the thickness of a film or layer being “substantially uniform” may refer to the average thickness of the film or layer being less than or equal to ±10% of the standard deviation, such as less than or equal to ±5%, less than or equal to ±4%, less than or equal to ±3%, less than or equal to ±2%, less than or equal to ±1%, less than or equal to ±0.5%, less than or equal to ±0.1%, or less than or equal to ±0.05%. The term "substantially coplanar" can refer to two surfaces that are within 50 μm along the same plane (such as within 40 μm, 30 μm, 20 μm, 10 μm, or 1 μm along the same plane). If, for example, two components overlap or overlap within 200 μm, 150 μm, 100 μm, 50 μm, 40 μm, 30 μm, 20 μm, 10 μm, or 1 μm, then the two components can be considered "substantially aligned." If the angle between two surfaces or components is, for example, 90° ± 10° (such as ± 5°, ± 4°, ± 3°, ± 2°, ± 1°, ± 0.5°, ± 0.1°, or ± 0.05°), then the two surfaces or components can be considered "substantially perpendicular." When used in conjunction with an event or situation, the terms "approximately," "generally," "substantially," "materially," "about," and "approximately" can refer to the exact occurrence of the event or situation as well as the very close approximation of its occurrence.

[0046] In this specification, unless otherwise specified or limited, relative terms such as “central,” “longitudinal,” “lateral,” “front,” “rear,” “right,” “left,” “inner,” “outer,” “lower,” “higher,” “horizontal,” “vertical,” “above,” “below,” “above,” “below,” “top,” “bottom,” and their derivatives (e.g., “horizontally,” “downward,” “upward,” etc.) should be interpreted as referring to the directions described in the discussion or depicted in the accompanying drawings. These relative terms are used for descriptive convenience only and do not require that this application be constructed or operated in a particular orientation.

[0047] For ease of description, "first," "second," "third," etc., can be used in this article to distinguish different components of a figure or a series of figures. "First," "second," "third," etc., are not intended to describe the corresponding components.

[0048] As described in the background art, in 3D packaged integrated circuits (ICs), gap fill technology is often used instead of molding technology. A uniform inorganic dielectric layer (such as silicon oxide, SiO) is filled by chemical vapor deposition to protect the wafer and thicken it so that subsequent processing can be carried out. Figures 1 to 4 The packaging structure process of the prior art is shown.

[0049] Figure 1 The image shows a wafer being cut along the dashed line.

[0050] Figure 2 The single wafer 10 obtained after dicing is shown.

[0051] Figure 3 The image shows the bonding of wafer 10 to substrate 20.

[0052] Figure 4 A dielectric layer 40 covering wafer 10 is shown formed by performing a chemical vapor deposition process. The thickness of the dielectric layer 40 is, for example, 50 μm. The dielectric layer 40 is a passivation layer / oxide layer.

[0053] Figure 5 The image shown was taken using a scanning electron microscope (SEM). Figure 4 The electron microscope image of the structure shown shows that the dielectric layer (dielectric film) 40 has a delamination / crack 44 at the corner corresponding to the wafer 10.

[0054] Figure 6 and Figure 7A The diagram illustrates back-end processes, such as performing chemical mechanical polishing (CMP) on the resulting wafer 88, where... Figure 7A A side view of a carrier 82, a carrier film 84, and a wafer 88 is shown. The wafer 88 is ground on a polishing pad 80 using the carrier 82. The polishing pad 80 is rotated in the direction indicated by the arrow, and slurry 86 is applied to the polishing pad 80.

[0055] Figure 7B The image shows a partial electron microscope (SEM) image of the finished product taken using a scanning electron microscope. Due to structural issues with wafer 10, the dielectric layer 40 forms a thick film with high structural stress at the right angle (90°) of the covered wafer. This stress cannot be eliminated by chemical vapor deposition, resulting in weak structural strength of the dielectric layer 40 at this location, which can lead to cracking, delamination, and damage. This also increases the risk of breakage in subsequent processing steps. It is not possible to specifically adjust the structural stress of the dielectric layer 40 at the right angle of wafer 10.

[0056] In view of the problems existing in the prior art, the embodiments of this application modify the structure of the chip 10. Figures 8 to 23 The manufacturing process of the packaging structure 100 according to an embodiment of this application is shown.

[0057] Figure 8 A top view of the incoming wafer is shown, including a plurality of interconnected wafers 10. The material of the wafers 10 includes, for example, Si.

[0058] Figure 9 A side view of two adjacent wafers 10 is shown.

[0059] Figure 10 The process of performing plasma etching is shown, in which the angle between the back surface (passive surface / active surface) 18 and the sidewall 16 of the wafer 10 is changed from a right angle to a chamfer 30. The chamfer 30 is an angled angle with the extended surface of the back surface 18 and the sidewall 16 that is less than 90°, in order to reduce structural stress.

[0060] Figure 11 A side view of the monolithic wafer 10 obtained after wafer dicing is shown.

[0061] Figure 12 The diagram illustrates, for example, bonding a wafer 10 onto a substrate 20 using a hybrid bonding process. The substrate 20 may be made of materials such as Si.

[0062] Figure 13 The diagram illustrates a dielectric layer 40 covering a wafer 10, formed by depositing a passivation oxide layer (e.g., SiO, SiO2, etc.) using a chemical vapor deposition process, which serves as a protective layer for the wafer 10 to prevent it from cracking.

[0063] Figure 14The image shown was taken using a scanning electron microscope (SEM). Figure 13 The image shows a partial electron microscope image of the structure, with a magnification of 300x, an imaging mode of BSD Full, and an accelerating voltage of 15kV. Figure 15 It shows Figure 14 Enlarged view of region A. In this embodiment, the corners of wafer 10 are changed to chamfers 30 to reduce structural stress in this area, thereby reducing the risk of dielectric layer 40 cracking and preventing damage to the bonding area. This also reduces the risk of dielectric layer 40 cracking and damage during subsequent reliability testing.

[0064] Figure 16 It shows the corresponding Figure 12 The cross-sectional view of the steps shown. The active surface 14 of the wafer 10 is hybrid-bonded (i.e., metal-to-metal bonding, dielectric-to-dielectric bonding) to the substrate 20. The active surface 14 of the wafer 10 has a first pad 12, and the surface of the substrate 20 has a second pad 22. The first pad 12 and the second pad 22 are in direct contact and partially misaligned. The substrate 20 also includes a through-hole 24.

[0065] Figure 17 It shows the corresponding Figure 13 The cross-sectional view of the steps shown is compared to Figure 16 The steps shown simplify the number of the first pad 12, the second pad 22, and the through-hole 24. It is understood that the number of components in the accompanying drawings is merely illustrative and can be adjusted and designed according to actual conditions.

[0066] Figure 18 It shows that Figure 17 The structure shown is bonded to the glass carrier 70 via an adhesive layer 72.

[0067] Figure 19 Showing flip Figure 18 The structure shown is used, and the substrate 20 is thinned, for example by grinding or deep reactive ion etching (DRIE) processes, to expose the through-hole 24.

[0068] Figure 20 It shows in Figure 19 An interlayer dielectric layer 52 is formed on the top as shown.

[0069] Figure 21 It shows in Figure 20 The structure shown has a redistribution layer 50 and a molding layer 54, and holes 56 are formed in the molding layer 54 to expose the redistribution layer 50. The material of the molding layer 54 is, for example, polyimide (PI).

[0070] Figure 22The diagram shows a hole filled with bumps / pads 62, and solder balls 60 formed on the bumps 62.

[0071] Figure 23 The removal of the glass carrier 70 and the adhesive layer 72 is shown to obtain the encapsulation structure 100 according to an embodiment of this application.

[0072] Figure 24 It shows the use of blades (Blade 90) to form a shape that was not pre-formed. Figure 9 The wafer 96 of the groove 94 shown is directly cut (2.5D) to obtain the following: Figure 25 The monolithic wafer 10 shown has a wafer mounted on tape 92. Blade 90 is substantially perpendicular to the upper surface of wafer 96. A plasma etching process can then be performed to chamfer the right angle at the top of wafer 10.

[0073] It can also be done in Figure 25 After the steps shown, tilt the blade 90 degrees to cut the top of the wafer 10 at a right angle. Figure 26 The chamfered angle shown is 30°, replacing the plasma etching process.

[0074] See also Figure 23 and Figure 15 This application provides a packaging structure 100, including: a substrate 20; a plurality of spaced-apart wafers 10, the active surfaces 14 of the wafers 10 being bonded to the substrate 20, and the sidewalls 16 and back surfaces 18 of the wafers 10 being connected by a chamfer 30; and a dielectric layer 40 covering the wafers 10, wherein the top surface of the dielectric layer 40 has a recess 42 at the gap corresponding to the gap between adjacent wafers 10. This application's embodiment changes the included angle between the sidewalls 16 and back surfaces 18 of the wafers 10 to a chamfer 30, which can solve or reduce the problem of cracking caused by excessive stress at the corners of the dielectric layer 40 corresponding to the wafers 10, and avoid damage to the dielectric layer 40.

[0075] In some embodiments, due to the formation of the chamfer 30 by plasma etching and the scalloping effect of plasma etching, the sidewalls 16 and the surface of the chamfer 30 of the wafer 10 have periodic undulating ripples 32. The back surface 18 is planar, the roughness of the chamfer 30 is greater than that of the back surface 18, and the roughness of the chamfer 30 is the same as that of the sidewall 16. The microstructure produced by plasma etching can increase the adhesion between the wafer 10 and the dielectric layer 40.

[0076] In some embodiments, the sidewalls 16 and the back surface 18 of the wafer 10 are perpendicular.

[0077] In some embodiments, the included angle α1 between the chamfer 30 and the sidewall 16 is different from the included angle α2 between the chamfer 30 and the back surface 18.

[0078] In some embodiments, the included angle α1 between the chamfer 30 and the sidewall 16 is greater than the included angle α2 between the chamfer 30 and the back surface 18.

[0079] In some embodiments, the package structure 100 further includes a redistribution layer 50 that electrically connects the surface of the substrate 20 opposite to the wafer 10.

[0080] In some embodiments, the angle α1 between the chamfer 30 and the sidewall 16, and the angle α2 between the chamfer 30 and the back surface 18 are obtuse angles.

[0081] In some embodiments, the sidewalls 16 and active surfaces 14 of the wafer 10 are perpendicular.

[0082] In some embodiments, the substrate 20 is a semiconductor wafer, the dielectric layer 40 is an inorganic layer, and the material of the dielectric layer 40 is silicon oxide or silicon nitride.

[0083] In some embodiments, the dielectric layer 40 has a uniform thickness.

[0084] The above description is merely a preferred embodiment of this utility model and is not intended to limit the utility model. Various modifications and variations can be made to this utility model by those skilled in the art. Any modifications, equivalent substitutions, improvements, etc., made within the spirit and principles of this utility model should be included within the protection scope of this utility model.

Claims

1. A packaging structure, characterized in that, include: Substrate; A plurality of spaced-apart wafers, the active surfaces of which are mixed and bonded to the substrate, the sidewalls of which are connected to the back surface of which are chamfered; A dielectric layer covering the wafer. The top surface of the dielectric layer has a recess corresponding to the gap between adjacent wafers.

2. The packaging structure according to claim 1, characterized in that, The active surface of the wafer has a first pad, and the surface of the substrate has a second pad. The first pad and the second pad are in direct contact and partially misaligned.

3. The packaging structure according to claim 1, characterized in that, The wafer has periodic undulating patterns on the sidewalls and chamfered surfaces.

4. The packaging structure according to claim 1, characterized in that, The sidewalls and back surface of the wafer are perpendicular.

5. The packaging structure according to claim 1, characterized in that, The angle between the chamfer and the sidewall is different from the angle between the chamfer and the back face.

6. The packaging structure according to claim 5, characterized in that, The angle between the chamfer and the sidewall is greater than the angle between the chamfer and the back face.

7. The packaging structure according to claim 1, characterized in that, Also includes: A redistribution layer electrically connects the substrate to the surface opposite to the wafer.

8. The packaging structure according to claim 1, characterized in that, The angle between the chamfer and the sidewall, and the angle between the chamfer and the back surface, are obtuse angles.

9. The packaging structure according to claim 1, characterized in that, The roughness of the chamfer is greater than the roughness of the back surface.

10. The packaging structure according to claim 9, characterized in that, The roughness of the chamfer is the same as the roughness of the sidewall.