Method for manufacturing a self-sealing vehicle pneumatic tire

A coating of fatty acid salts on the sealing and inner layers of self-sealing tires addresses adherence and crystal issues, maintaining tire performance and integrity.

DE102015219295B4Active Publication Date: 2026-11-19CONTINENTAL REIFEN DEUTSCHLAND GMBH
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
DE102015219295
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Filing Date
2015-10-06
Publication Date
2026-11-19
Estimated Expiration
2035-10-06

AI Technical Summary

Technical Problem

Existing self-sealing vehicle tires face issues with foreign particles adhering to the sealing layer and undesirable crystal formation due to reactions between amines and peroxides, which degrade the tire's performance and integrity.

Method used

Applying a coating containing alkali and/or alkaline earth salts of fatty acids to the sealing layer and inner layer surfaces to reduce stickiness and inhibit crystal formation, while maintaining the tire's sealing performance.

Benefits of technology

Prevents foreign particle adherence and significantly reduces crystal formation, ensuring the tire's self-sealing effectiveness without adverse effects on rolling resistance or tire weight.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

Method for manufacturing a self-sealing pneumatic tire comprising a belt assembly (2), a tread (1) arranged radially above the belt assembly (2), and a radially inner airtight inner layer (4), wherein the self-sealing of the pneumatic tire is achieved by a sealing layer (5) subsequently applied radially inside the tire after vulcanization, wherein the sealing layer (5) has approximately the width of the belt assembly (2) and is arranged approximately in its projection and has a cross-section formed in the cross-sectional plane containing the tire axle with a surface (5a) extending substantially parallel to the belt assembly in the axial direction and a surface (5b) extending substantially in the radial direction, characterized in that the sealing layer (5) is coated by applying at least one suspension.wherein the suspension contains at least one alkali salt of at least one fatty acid and / or at least one alkaline earth salt of at least one fatty acid.
Need to check novelty before this filing date? Find Prior Art

Description

The invention relates to a method for manufacturing a self-sealing pneumatic tire for vehicles, comprising a belt assembly, a tread arranged radially above the belt assembly, and a radially inner airtight inner layer, wherein the self-sealing of the pneumatic tire is achieved by a sealing layer subsequently applied radially inside the vehicle after vulcanization, wherein the sealing layer has approximately the width of the belt assembly and is arranged approximately in its projection, and has a cross-section formed in the cross-sectional plane containing the tire axle, with a surface extending substantially parallel to the belt assembly in the axial direction and a surface extending substantially in the radial direction. Such self-sealing pneumatic tires are known, for example, from DE 10 2006 059 286 A1 of the applicant. In this design, standard tire constructions are subsequently provided with a sealant layer. The sealant is a self-adhesive, viscous sealant that is applied radially inwards in the projection area of ​​the belt pack to the radially innermost tire layer, the largely airtight inner layer. The sealant layer is capable of independently sealing punctures up to five millimeters in diameter. After a puncture through the tread and into the inner layer, the sealant completely surrounds the foreign object, seals the interior from the environment, and thus prevents a loss of air pressure in the tire. The driver of the vehicle is not required to immediately replace the defective tire with a full-size spare or a temporary spare. The sealant is used by the applicant under the name ContiSeal®. The sealant is characterized by airtightness, strong adhesion, and balanced flow behavior. Due to the strong adhesive properties of the sealant layer, unwanted foreign particles that enter the tire interior (e.g., during tire storage) adhere to the sealant layer, particularly to the radially inward-facing surface. The radially outward-facing surface adheres to the inner layer and is therefore not exposed. Furthermore, components, especially amines, can migrate from the rubber compounds surrounding the sealant layer, particularly the inner layer, and react with peroxide components from the sealant. This can lead to the formation of undesirable crystals that also adhere to the sealant layer. Furthermore, peroxides can also migrate from the sealant layer and, together with amines from the inner layer, form crystals on the radially inward-facing surface of the inner layer. These crystals represent the reaction product of the amines with the peroxides. Further prior art is cited in the documents DE 24 57 808 A1, DE 10 2008 003 554 A1 and US 2014-0174639 A1. The object of the present invention is to provide a method for manufacturing a self-sealing vehicle pneumatic tire such that no foreign bodies adhere to the sealing layer inside the tire and crystal formation on the free surface inside the tire is greatly reduced or even completely prevented. The problem is solved by coating the sealant layer with a suspension containing at least one alkali salt of at least one fatty acid and / or at least one alkaline earth salt of at least one fatty acid. Such a coating significantly reduces the stickiness of the radially inward-facing surface of the sealant layer to such an extent that (almost) no unwanted foreign matter adheres to the radially inward-facing surface of the sealant layer, which runs essentially parallel to the belt pack. Furthermore, the alkali salt and / or alkaline earth salt of at least one fatty acid on the sealant layer reduces the extent of the reaction between amines from adjacent rubber mixtures and peroxides or their radicals (their radical fission products) from the sealant, so that undesirable crystal formation on the coated sealant layer does not occur or only to an insignificant extent. Furthermore, the manufactured vehicle tire shows no negative impairment with regard to its self-sealing properties. The essential feature of the invention is that the coating contains one or more fatty acid salts. This significantly reduces the stickiness of the sealant layer's surface and minimizes crystal formation inside the tire. At the same time, the sealing performance of the self-sealing pneumatic tire is not negatively affected by such a coating. Fatty acids are known to experts and, according to Römpp Online ® 2015, represent "aliphatic, saturated and unsaturated carboxylic acids with, with few exceptions, an unbranched carbon chain". In the context of the present invention, it is particularly preferred if the fatty acid has 8 to 18 carbon atoms. This effectively prevents the reaction of amines with peroxides to form undesirable crystals, as described above. For carbon atoms of 8 to 18, linear, unbranched carbon chains are particularly preferred. Preferred fatty acids, or their salts as described below, include, for example, and especially... Octanoic acid (also called caprylic acid) with 8 carbon atoms and / or tetradecanoic acid (also called myristic acid) with 14 carbon atoms and / or hexadecanoic acid (also called palmitic acid) with 16 carbon atoms and / or octadecanoic acid (also called stearic acid) with 18 carbon atoms. According to a preferred embodiment of the invention, the fatty acid is selected from the group consisting of octanoic acid and / or tetradecanoic acid and / or hexadecanoic acid and / or octadecanoic acid. According to a particularly preferred embodiment of the invention, the fatty acid is at least octadecanoic acid. According to the invention, at least one fatty acid is contained in the coating in the form of at least one alkali and / or alkaline earth salt. In the context of the present invention, "alkali salt of at least one fatty acid" means the alkali metal salt of at least one fatty acid, wherein alkali metals in salts are formally simply positively charged, such as, for example, and in particular, the alkali metal ions of lithium (Li+), sodium (Na+), potassium (K+), rubidium (Rb+). Preferably, the alkali metal ion of the salt is lithium (Li+) and / or sodium (Na+) and / or potassium (K+). The ions of the fatty acid are formally singly negatively charged, so that in the alkali salt of the fatty acid, one alkali metal ion and one ion of the fatty acid (carboxylate ion) correspond to a formally neutral charge. The at least one alkali salt of at least one fatty acid can also be a mixture of different alkali salts in which the alkali metals and / or the fatty acids are the same or different from each other. The same applies to the at least one alkaline earth salt of at least one fatty acid. Here, too, it can be a mixture in which the alkaline earth metals and / or fatty acids are the same or different from each other. Within the scope of the present invention, "alkaline earth salt of at least one fatty acid" means the alkaline earth metal salt of at least one fatty acid, wherein the alkaline earth metals in salts are formally doubly positively charged, such as, for example, and in particular, the alkaline earth metal ions beryllium (Be2+), magnesium (Mg2+), calcium (Ca2+), etc. Preferably, the alkaline earth metal ion of the salt is magnesium (Mg2+) and / or calcium (Ca2+), particularly preferably calcium (Ca2+). In the alkaline earth salt of the fatty acid, one alkaline earth metal ion and two fatty acid ions correspond to a formally neutral charge. According to a preferred embodiment of the invention, the coating contains at least one alkali salt of at least one fatty acid and at least one alkaline earth salt of at least one fatty acid. According to a particularly preferred embodiment of the invention, the alkaline earth salt of at least one fatty acid is at least calcium stearate. The preferably aqueous suspension contains preferably 50 to 70 wt% water, particularly preferably 58 to 65 wt% water, before application. A suitable aqueous suspension containing calcium stearate and at least one alkali salt of at least one fatty acid is available, for example, under the trade name Rhenodiv® BO 7672-1 from the company Rheinchemie. Such a suspension contains, before application and drying, 58 to 65 wt% water, 10 to 20 wt% at least one alkali salt of at least one fatty acid, 10 to 20 wt% calcium stearate and less than 2 wt% additives or impurities. According to a preferred embodiment of the invention, the suspension is applied using a sponge. In the context of the present invention, the term "sponge" means a sponge body which preferably contains polyurethane and / or polyether, and particularly preferably at least polyurethane, and is particularly preferably composed of polyurethane and / or polyether. Such sponges are also known as commercially available household sponges. Household sponges can have a multi-layered structure, often consisting of a sponge body made of polyurethane and / or polyether and at least one abrasive layer containing inorganic solids. In the context of the present invention, however, application is preferably carried out with the surface of the polyurethane and / or polyether sponge body, particularly preferably polyurethane, and not with an abrasive surface, if present. Application with an abrasive surface would lead to unnecessary damage to the sealant surface, causing it to become unnecessarily roughened. Since an aqueous suspension is preferably applied, water preferably evaporates as a component of the resulting coating. The applied suspension is preferably dried for 4 to 8 hours, whereby a residual amount of water may remain in the coating. To ensure that the water to be evaporated escapes as quickly as possible, it is preferred that the temperature of the self-sealing vehicle tire is 30 to 70 °C, preferably 30 to 50 °C, when the suspension is applied. A temperature above 70 °C is unnecessary and undesirable, as it would be too high for the operator, posing risks during application. Furthermore, excessively high temperatures can cause substances from the tire components, particularly the inner layer and sealant, to evaporate to an undesirable degree and subsequently redeposit on their surfaces. Therefore, application at 30 to 70 °C, preferably 30 to 50 °C, represents a good compromise between evaporation rate with minimized risks regarding hazards and the environment, as well as the lowest possible energy costs. The suspension is preferably applied in such a way that, after drying, a coating with a thickness of 0.01 to 1 mm, particularly preferably 0.05 to 0.15 mm, remains. Such a thickness ensures reduced stickiness even with minor irregularities on the surface of the sealant layer. At the same time, with such a thickness, a moderate amount of the coating (suspension) is applied, so that the tire weight and thus the rolling resistance of the vehicle tire according to the invention are not significantly negatively affected. The specified thickness of the coating represents the thickness measured in the radial direction perpendicular to the axial extent of the sealant layer. It is conceivable that the thickness of the coating varies by 0 to 0.005 mm in the axial direction. In the method according to the invention, it is preferred that the self-sealing pneumatic tire is rotated circumferentially during the application of the suspension. This ensures that the suspension is distributed evenly over the sealant layer. Within the scope of the present invention, the term "essentially" in the description of the arrangement of the individual components of the vehicle pneumatic tire according to the invention means that usual minor variations due to manufacturing are included. The sealant layer essentially has the same width as the belt package. The sealant layer is essentially arranged in its projection (the projection of the belt package), i.e., it runs radially within the belt package essentially parallel to it. The sealant layer has a cross-section formed in the cross-sectional plane containing the tire axle, with a surface extending substantially parallel to the belt package in the axial direction and a surface extending substantially in the radial direction. The sealant layer preferably has a substantially rectangular cross-section, and depending on the design of the tire dimensions, it may have a curvature, particularly in projection of the shoulder edges of the belt package. The sealing layer is bounded radially outwards by the inner layer and radially inwards by its radially inwards directed surface running in an axial direction, essentially parallel to the belt pack, and on both sides, preferably essentially symmetrically, by the surfaces running in a radial direction, essentially perpendicular to the belt pack. According to a preferred embodiment of the invention, the suspension is applied at least to the surface of the sealant layer that runs substantially parallel to the belt pack in the axial direction. This coats a large proportion of the exposed surface of the sealant layer, preventing foreign particles from adhering to this coated surface and thus preventing or minimizing undesirable crystal formation on this surface. According to a preferred embodiment of the invention, the suspension is additionally applied at least to the radially extending surface of the sealant layer. This prevents foreign particles from adhering to the lateral cross-sectional areas of the sealant layer and reduces or even completely prevents crystal formation in these areas as well. Preferably, the coating is applied to the radially extending surface of the sealant layer in such a way that there is an overlap with the inner layer on both sides in the axial direction. The axial width of the overlap is preferably 0.5 to 10 mm on each side, more preferably 0.5 to 2 mm, and particularly preferably 1 mm. In this embodiment, the coating is thus located on the entire surface of the sealant layer and on each side on a section of the inner layer that is 0.5 to 10 mm wide in the axial direction, more preferably 0.5 to 2 mm, and particularly preferably 1 mm, directly adjacent to the sealant layer. This ensures particularly effectively that no foreign matter adheres to the sides of the sealant layer and that no crystals form there. In particular, crystals can also form on the two inner lateral walls of the tires through evaporation and subsequent condensation of amines and peroxides or their radical fission products (as described above). According to a preferred embodiment of the invention, the suspension is therefore additionally applied to the radially inwardly directed surface of the inner layer. The radially outward-facing surface of the inner layer adheres to the tire components radially outside the inner layer and is therefore not exposed. Because the inner layer inside the tire is also coated with the coating described above, crystal growth is also prevented on both inner sidewalls of the tire. Preferably, the inner layer is coated on both sides from the sealant layer to the radially outer end of the bead core. Thus, the coating is preferably not applied where the vehicle tire according to the invention sits on or makes contact with the rim, in order to prevent slippage between the tire and rim in the contact area. According to this embodiment, when the tire is mounted on the rim, the entire inner surface of the vehicle tire is preferably coated without gaps around its circumference. Visually, this is recognizable, among other things, by the fact that the sealant layer and the inner surfaces of the tire are covered with a gray film. In order to achieve a simple manufacturing process for the vehicle pneumatic tire according to the invention, the coating is applied to the surface of the inner layer and the surface of the sealant layer with the same thickness. Further features, advantages and details of the invention are explained using the following example. A blank pneumatic tire was first prepared using processes known in the art and then vulcanized. The tire was cooled to 50 °C at room temperature. The tire was then placed on a device known to those skilled in the art, which rotates the tire around its axis in the direction of rotation. During this process, an aqueous suspension containing at least one alkali salt of at least one fatty acid and / or at least one alkaline earth salt of at least one fatty acid was applied using a polyurethane household sponge. The suspension used was Rhenodiv® BO 7672-1 from Rheinchemie. The suspension was applied to the surface of the sealant layer, which runs essentially parallel to the belt package in the axial direction, and dried for 6 hours, during which time water evaporated from the suspension. As can be seen in Fig. 1, in this example a coating 6 remains on the surface of the sealant layer 5a, which runs essentially parallel to the belt package in the axial direction. The coating density after 6 hours of drying was 0.1 mm. In another example, the suspension is additionally applied at least to the radially extending surface of the sealant layer 5b, with an overlap of 1 mm to the inner layer 4 on both sides (in the axial direction). Thus, the resulting pneumatic tire has the coating on the entire inwardly exposed surface of the sealant layer 5. In another example, the suspension is applied not only to the entire surface of the sealant layer but also to the radially inward-facing surface of the inner layer. Thus, the resulting pneumatic tire has the coating on its entire inner surface. The suspension is preferably applied only up to the radially outer end of the bead core to prevent slippage between the tire and rim. Reference symbol list (Part of the description) 1 Tread 2 Belt pack 2a Belt layer 2b Belt layer 3 Carcass 3a Carcass high edge 4 Inner layer 5 Sealant layer 5a Radially inward-facing surface, axially parallel to the belt pack, surface of the sealant layer 5b Radially perpendicular to the belt pack, surface of the sealant layer 6 Coating rR radial direction aR axial direction

Claims

Method for manufacturing a self-sealing pneumatic tire comprising a belt assembly (2), a tread (1) arranged radially above the belt assembly (2), and a radially inner airtight inner layer (4), wherein the self-sealing of the pneumatic tire is achieved by a sealing layer (5) subsequently applied radially inside the tire after vulcanization, wherein the sealing layer (5) has approximately the width of the belt assembly (2) and is arranged approximately in its projection and has a cross-section formed in the cross-sectional plane containing the tire axle with a surface (5a) extending substantially parallel to the belt assembly in the axial direction and a surface (5b) extending substantially in the radial direction, characterized in that the sealing layer (5) is coated by applying at least one suspension.wherein the suspension contains at least one alkali salt of at least one fatty acid and / or at least one alkaline earth salt of at least one fatty acid. Method according to one of the preceding claims, characterized in that the suspension contains 50 to 70 wt.% water. Method according to one of the preceding claims, characterized in that the fatty acid has 8 to 18 carbon atoms. Method according to one of the preceding claims, characterized in that the suspension contains at least calcium stearate as an alkaline earth salt of at least one fatty acid. Method according to one of the preceding claims, characterized in that the suspension is applied using a sponge. Method according to claim 5, characterized in that the surface of the sponge contains polyurethane. Method according to one of the preceding claims, characterized in that the temperature of the self-sealing vehicle pneumatic tire is 30 to 70 °C when the suspension is applied. Method according to one of the preceding claims, characterized in that the suspension is applied at least to the surface of the sealant layer (5a) which extends substantially parallel to the belt package in the axial direction. Method according to claim 8, characterized in that the suspension w is additionally applied at least to the radially extending surface of the sealant layer (5b). Method according to claim 9, characterized in that the suspension is additionally applied to the radially inwardly directed surface of the inner layer (4).

Citation Information

Patent Citations

  • Use of a polyurethane gel as a sealant for self-sealing pneumatic vehicle tires, method for producing a self-sealing pneumatic vehicle tire and self-sealing pneumatic vehicle tire

    DE102006059286A1

  • Pneumatic tire for vehicle, has two compact intermediate plies of different hardness are present for automatic sealing, in which each comprises viscoelastic material

    DE102008003554A1

  • Laminated puncture sealing strip for pneumatic tyres - with sealing compsn contained between barrier layers preventing migration of plasticising oil

    DE2457808A1

  • Tyre having a built-in self-sealing layer

    US20140174639A1