SUBSTRATE FOR A REFLECTIVE OPTICAL ELEMENT
Patent Information
- Application Number
- DE502019012350
- Authority / Receiving Office
- DE · DE
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2018-07-06
- Filing Date
- 2019-07-05
- Publication Date
- 2024-11-14
- Estimated Expiration
- 2039-07-05
AI Technical Summary
Reflective optical elements for the extreme ultraviolet wavelength range face challenges in maintaining long-term stability of surface shape due to relaxation effects after compaction, which can negatively impact imaging properties over time.
A substrate made of titanium-doped quartz glass with a high proportion of Si-O-O-Si or Si-Si bonds, along with controlled hydrogen content, is used to enhance the glass matrix's stability, reducing the likelihood of relaxation after compaction by creating predetermined breaking points that are less likely to recombine.
The proposed substrate achieves improved long-term stability of the surface shape, minimizing relaxation effects over months and years, thus maintaining precise imaging properties in EUV lithography and other optical systems.
Description
[0001] The present invention relates to substrates for a reflective optical element for the extreme ultraviolet wavelength range made of titanium-doped quartz glass, which have a surface region to be coated. It also relates to reflective optical elements for the extreme ultraviolet wavelength range with such a substrate having a surface region with a reflective coating. Furthermore, the invention relates to an optical system with such reflective optical elements and to an EUV lithography device with such an optical system or such a reflective optical element. The present application claims priority from German application 10 2018 211 234.7 of July 6, 2018, the contents of which are incorporated by reference in their entirety.
[0002] In order to produce ever finer structures using lithographic methods, for example, in the production of semiconductor components, increasingly shorter wavelengths of light are being used. When working in the extreme ultraviolet (EUV) wavelength range, for example, at wavelengths between approximately 5 nm and 20 nm, lens-like elements in transmission mode are no longer possible. Instead, illumination and projection lenses are constructed from mirror elements with reflective coatings adapted to the respective operating wavelength.
[0003] So-called zero-expansion materials are used as substrate materials, particularly for reflective optical elements for EUV lithography. Their thermal expansion coefficient approaches zero at temperatures slightly above room temperature prevailing during lithography. Glass-ceramics and titanium-doped quartz glass are the primary materials. These materials can be manufactured in such a way that, at a temperature that depends on the specific material, the thermal expansion coefficient, defined here as the differential of the relative linear expansion as a function of temperature, becomes zero. In titanium-doped quartz glass, this effect can be influenced by the content of additives; in glass-ceramics, it can be influenced by recrystallization processes under strictly controlled post-heating cycles.
[0004] EUV lithography devices rely on the reflective optical elements used to image a mask into an image plane to have a high degree of surface shape accuracy. Likewise, masks as reflective optical elements for the EUV wavelength range should have a high degree of surface shape accuracy, as their replacement significantly increases the operating costs of an EUV lithography device.
[0005] Conventional methods for correcting surfaces are generally based on removing the substrate material of optical elements mechanically or by irradiating them with ions. Another approach to correcting surfaces involves locally densifying the substrate material of optical elements by irradiating them with electromagnetic radiation or, preferably, with electrons. This procedure is described, for example, in WO 2013 / 050199 A1 and has the advantage of being applicable even to already coated substrates, particularly reflective optical elements.
[0006] However, it has been found that the surface shape corrections achieved through densification by irradiation exhibit relaxation effects, particularly during storage and operation of the reflective optical elements, which can negatively impact the imaging properties. In particular, it cannot be ruled out that the corrections will disappear completely after a few years.
[0007] WO 2009 / 145288 A1 discloses a substrate for reflective optical elements for the EUV wavelength range made of titanium-doped quartz glass, which has a hydrogen content of at least 15*10 17 molecules / cm 3 . DE 10 2010 009 589 A1 describes a substrate for reflective optical elements for the EUV wavelength range made of titanium-doped quartz glass, which has an average hydrogen content of at least 1*10 16 molecules / cm 3 .
[0008] It is an object of the present invention to show a possibility of improving the long-term stability of the surface shape of a reflective optical element.
[0009] This object is achieved by a substrate for a reflective optical element for the extreme ultraviolet wavelength range made of titanium-doped quartz glass, which has a surface region to be coated, wherein the titanium-doped quartz glass has, at least in the vicinity of the surface region, a proportion of Si-OO-Si bonds of at least 1*10 16< / cm 3< or a proportion of Si-Si bonds of at least 1*10 16< / cm 3<.
[0010] The approach is based on trying to influence the relaxation after densification of the substrate material by deliberately changing the structure of the glass matrix.
[0011] It is assumed that both peroxy bonds in the glass matrix (Si-OO-Si) and Si-Si bonds (also called oxygen-deficient centers) form predetermined breaking points that break particularly easily under the influence of high-energy irradiation, particularly with electrons, as used for compaction, but cannot recombine as easily as normal matrix bonds. A substrate with such a non-stoichiometric matrix can be compacted easily. However, it relaxes less than a substrate with a stoichiometric matrix, in which, for example, tighter SiO2 rings form or normal Si-O bonds within the tetrahedral basic structure of quartz glass break. The surface shape of a substrate proposed here should therefore exhibit better long-term stability.
[0012] Preferably, the titanium-doped quartz glass has, at least in the vicinity of the surface region, a proportion of Si-OO-Si bonds of at least 1*10 17< / cm 3< or even at least 5*10 17< / cm 3< , preferably at least 1*10 18< / cm 3< or even at least 5*10 18< / cm 3< , particularly preferably at least 1*10 19< / cm 3< or even at least 5*10 19< / cm 3< , very particularly preferably at least 1*10 20< / cm 3< or a proportion of Si-Si bonds of at least 1*10 17< / cm 3< or even at least 5*10 17< / cm 3< , preferably at least 1*10 18< / cm 3< or even at least 5*10 18< / cm 3< , particularly preferably at least 1*10 19< / cm 3< or even at least 5*10 19< / cm 3< , most preferably at least 1*10 20< / cm 3<. The more predetermined breaking points in the form of Si-OO-Si bonds or Si-Si bonds are present in the matrix, the more likely it is that long-term relaxation of surface corrections caused by irradiation can be suppressed.
[0013] In a preferred embodiment, the titanium-doped quartz glass has an average hydroxyl content of at most 100 ppm by weight, at least near the surface region. It has been recognized that relaxation of densities in the matrix of, in particular, titanium-doped quartz glass can occur structurally through displacements in the glass matrix or through the recombination of broken bonds. The glass matrix is particularly capable of displacements when it is rich in matrix terminators. Matrix terminators are understood here to be disturbances that interrupt the strict tetrahedral structure of an ideal quartz glass matrix, in which each silicon or titanium atom is four-coordinated via one oxygen atom each. Apart from hydroxyl, matrix terminators include, for example, SiF, SiOH, SiH, TiF, TiOH, TiH, TiOs, and TiOz.The aim is to keep the number of hydroxyl groups as low as possible while ensuring the highest possible number of predetermined breaking points in order to further reduce the probability of relaxation after compaction over longer periods of time.
[0014] In such embodiments, the titanium-doped quartz glass may have a content of additional matrix terminators, other than those having a hydroxyl group, of a maximum of 20% of the hydroxyl content near the surface region in order to further enhance the effect of lower relaxation after densification.
[0015] Advantageously, the titanium-doped quartz glass has a hydrogen content of less than 1×10 16 molecules / cm 3 , at least near the surface region. It has been shown that, particularly at higher temperatures, hydrogen can lead to the formation of SiH and SiOH at weakened bonds, which in turn can act as matrix terminators.
[0016] Preferably, the titanium-doped quartz glass comprises silicon fluoride or silicon chloride at least near the surface region.
[0017] Advantageously, the titanium-doped quartz glass has a hydrogen content of more than 5×10 18< molecules / cm 3< along an imaginary line perpendicular to the surface area over a length of 500 nm or more.
[0018] This is based on the assumption that heavily hydrogen-loaded titanium-doped quartz glass can exhibit greater material densification upon irradiation than less hydrogen-loaded titanium-doped quartz glass. It is assumed that broken matrix bonds of the form Si-O-Si -> Si + Si-O react to form SiH and SiOH in the presence of an excess of hydrogen, while they partially recombine in the absence of hydrogen. It is assumed that if a hydrogen-poor and at least locally densified substrate is subjected to a high amount of hydrogen, for example by introducing it into a hydrogen-containing atmosphere or purging it with hydrogen-containing gas, rearranged but energetically unfavorable bonds can be attacked and saturated, which should suppress slow relaxation.If a large amount of hydrogen is added to the substrate before densification, densification presumably leads less to matrix rearrangement and more to permanently broken bonds. This should reduce the relaxation rate and thus achieve better long-term stability of the substrate surface. Preferably, the substrate has a region of at least 500 nm thickness with increased hydrogen content near the surface area before, during, and immediately after densification for corrective purposes.
[0019] In particular, the titanium-doped quartz glass can have a hydrogen content of more than 1×10 19 molecules / cm 3 , particularly preferably more than 1×10 20 molecules / cm 3 , along an imaginary line perpendicular to the surface region over a length of 500 nm or more, in order to be able to further reduce the relaxation rate. The titanium-doped quartz glass of the substrate proposed here particularly preferably has this high hydrogen content before, during, and / or immediately after irradiation.
[0020] The more predetermined breaking points in the form of Si-OO-Si bonds or Si-Si bonds are present in the matrix, the more likely it is that long-term relaxation of surface corrections caused by irradiation can be suppressed.
[0021] Furthermore, this object is achieved by a reflective optical element for the extreme ultraviolet wavelength range with a substrate as just described, which has a surface region with a reflective coating.
[0022] Due to the special substrate materials proposed here, these reflective optical elements are particularly well-suited for correcting their surface shape through irradiation and corresponding densification of the substrate material. This is because the relaxation of this densification has a smaller impact, especially over long periods of months and years, than with substrates made of conventional titanium-doped quartz glass. The desired surface contour of the substrate for the respective reflective optical element can essentially be formed even before the application of a reflective coating. For this purpose, irradiation can also be used, which can lead to densification, at least in the irradiated area, and thus to a change in the surface contour.After coating, the respective reflective optical element can be checked on its own or in combination with other optical elements as required and then finely corrected accordingly.
[0023] In preferred embodiments, the substrate has a hydrogen content of more than 5×10 18< molecules / cm 3<, preferably more than 1×10 19< molecules / cm 3<, particularly preferably more than 1×10 20< molecules / cm 3<, along an imaginary line perpendicular to the surface area with the reflective coating over a length of 500 nm or more, in order to be able to reduce the relaxation rate more significantly.
[0024] Particularly preferably, the length of 500 nm or more has a distance from the reflective coating of no more than 1 mm, preferably no more than 100 µm, particularly preferably no more than 20 µm, and most preferably no more than 5 µm. It has been found that it is sufficient if the desired high hydrogen content develops, in particular, in the region directly beneath the reflective coating, where the corrections are also carried out whose relaxation is to be minimized.
[0025] Particularly preferably, the substrate has a hydrogen content of less than 5×10 17< molecules / cm 3<, preferably less than 1×10 17< molecules / cm 3<, particularly preferably less than 1×10 16< molecules / cm 3< along the imaginary line perpendicular to the surface region with the reflective coating at a distance from the latter of at least 1 mm, preferably at least 1 cm. By having a lower hydrogen content in the interior of the substrate, i.e. in particular apart from the region immediately beneath the reflective coating, it can be ensured that other material properties of the titanium-doped quartz glass are not adversely affected by an excessively high hydrogen content.
[0026] Advantageously, the substrate has a hydrogen content of more than 5×10 18< molecules / cm 3< within a period of up to one month after application of the reflective coating along an imaginary line perpendicular to the surface area with the reflective coating over a length of 500 nm or more, and a hydrogen content of more than 1×10 18< molecules / cm 3< within a period of one month after application of the reflective coating up to seven years after application of the reflective coating. It is expected that this long-term behavior of the hydrogen content can lead to the lowest possible relaxation of corrections introduced into the reflective optical element, even over a period of several years.
[0027] In a reflective optical element whose substrate has a further surface region which is located on a side of the substrate facing away from the surface region with the reflective coating and which does not have a reflective coating, the substrate preferably has, along the imaginary line over a further length of 500 nm or more at a distance of not more than 2 mm from the surface of the further, uncoated surface region, a hydrogen content of not more than half and not less than one twentieth of the hydrogen content over the length at a distance of not more than 1 mm from the reflective coating.
[0028] Furthermore, the object is achieved by an optical system with a reflective optical element as described above, as well as by an EUV lithography device with such an optical system or with a reflective optical element as described above. In this way, optical systems or EUV lithography devices can be provided that can have good optical properties with good long-term stability. Further preferred applications of the reflective optical elements based on the substrates proposed here include optical systems for inspection systems, for example, for wafers or masks, or for spectroscopic applications, for example in astrophysics, in particular extraterrestrial physics.
[0029] The present invention will be explained in more detail with reference to preferred embodiments. Figure 1 schematically shows an embodiment of an EUV lithography device; Figure 2 shows a schematic diagram of a first embodiment of a proposed reflective optical element; Figure 3 shows a schematic diagram of a second embodiment of a proposed reflective optical element; Figure 4 shows the distribution of the hydrogen content across the width of the substrate of a reflective optical element at a first point in time; and Figure 5 shows the distribution of the hydrogen content across the width of the substrate of a reflective optical element at a second point in time.
[0030] In Figure 1 An EUV lithography device 10 is shown schematically. The essential components are the illumination system 14, the photomask 17, and the projection system 20. The EUV lithography device 10 is operated under vacuum conditions so that the EUV radiation is absorbed as little as possible within it.
[0031] A plasma source or a synchrotron, for example, can serve as the radiation source 12. In the example shown here, it is a plasma source. The emitted radiation in the wavelength range from approximately 5 nm to 20 nm is first focused by the collector mirror 13. The operating beam is then introduced into the illumination system 14. In the Figure 1In the example shown, the illumination system 14 has two mirrors 15, 16. The mirrors 15, 16 direct the beam onto the photomask 17, which has the structure to be imaged onto the wafer 21. The photomask 17 is also a reflective optical element for the EUV and soft X-ray wavelength range, which is replaced depending on the manufacturing process. With the help of the projection system 20, the beam reflected by the photomask 17 is projected onto the wafer 21, thereby imaging the structure of the photomask onto it. In the example shown, the projection system 20 has two mirrors 18, 19. It should be noted that both the projection system 20 and the illumination system 14 can each have just one mirror or three, four, five, or more.
[0032] In principle, all reflective optical elements 13, 15, 16, 17, 18, 19 of the EUV lithography device 10 can comprise a substrate made of titanium-doped quartz glass having a surface region to be coated, wherein the titanium-doped quartz glass has, at least in the vicinity of the surface region, a proportion of Si-OO-Si bonds of at least 1*10 16< / cm 3< and / or a proportion of Si-Si bonds of at least 1*10 16< / cm 3< or, along an imaginary line perpendicular to the surface region over a length of 500 nm or more, a hydrogen content of more than 5×10 18< molecules / cm 3<. The ability to perform long-term stable fine correction of the surface profile is particularly important for mirrors of the projection system 20, since the projection system should ideally have the most precise imaging properties possible.The reflective optical elements mentioned can have in their respective substrate at least along an imaginary line perpendicular to the surface region with the reflective coating over a length of 500 nm or more a hydrogen content of more than 5×10 18< molecules / cm 3< , preferably more than 1×10 19< molecules / cm 3< , particularly preferably more than 1×10 20< molecules / cm 3<.
[0033] In the example shown here, the illumination system mirrors 15, 16, the photomask 17 and the projection system mirrors 18, 19 are mirrors 50 for quasi-normal incidence, whose reflective coating is based on a multilayer system 54, as shown schematically in the Figures 2 and 3These are alternating layers of a material with a higher real part of the refractive index at the operating wavelength, at which, for example, lithographic exposure is carried out (also called spacer 57) and a material with a lower real part of the refractive index at the operating wavelength (also called absorber 56), with an absorber-spacer pair forming a stack 55. This simulates, to a certain extent, a crystal whose lattice planes correspond to the absorber layers at which Bragg reflection occurs. The thicknesses of the individual layers 56, 57 as well as the repeating stack 55 can be constant across the entire multilayer system 54 or can vary, depending on which spectral or angle-dependent reflection profile is to be achieved.The reflection profile can also be specifically influenced by supplementing the basic structure of absorber 56 and spacer 57 with additional, more or less absorbent materials in order to increase the possible maximum reflectivity at the respective operating wavelength. For this purpose, absorber and / or spacer materials can be interchanged in some stacks, or the stacks can be constructed from more than one absorber and / or spacer material. The absorber and spacer materials can have constant or varying thicknesses across all stacks to optimize reflectivity. Furthermore, additional layers can be provided as diffusion barriers between spacer and absorber layers 57, 56. For example, a typical material combination for an operating wavelength of 13.4 nm is molybdenum as the absorber and silicon as the spacer material. A stack 55 typically has a thickness of just under 7 nm, with spacer layer 57 usually being thicker than absorber layer 56.
[0034] In the example shown here, the coating 52 additionally has an optional protective layer 53, which can also consist of more than one layer. For example, in a molybdenum-silicon multilayer system, the protective layer 53 can be constructed, among other things, from a layer of silicon nitride and a layer of ruthenium as a seal against the vacuum, in order to be used at wavelengths around approximately 13.5 nm. Other suitable material combinations, including those for other wavelengths in the EUV wavelength range, are known to those skilled in the art.
[0035] In principle, the reflective optical elements proposed here can also be designed for grazing incidence. For this purpose, one or a few metallic layers can be provided on the substrate to reflect the EUV radiation based on the phenomenon of total internal reflection.
[0036] The coating 54 is arranged on a substrate 51 made of titanium-doped quartz glass. In a first variant, the substrate 51 of the reflective optical element for the extreme ultraviolet wavelength range, for example, a mirror from the projection system of an EUV lithography device, has a surface region 511 to be coated and already coated here as described. At least in the vicinity of the surface region 511, the substrate 51 has a proportion of Si-OO-Si bonds of at least 1*10 16 / cm 3 and / or a proportion of Si-Si bonds of at least 1*10 16 / cm 3 .It is particularly advantageous if the titanium-doped quartz glass has, at least in the vicinity of the surface region 511, a proportion of Si-OO-Si bonds of at least 1*10 17< / cm 3< or even at least 5*10 17< / cm 3< , preferably at least 1*10 18< / cm 3< or even at least 5*10 18< / cm 3< , particularly preferably at least 1*10 19< / cm 3< or even at least 5*10 19< / cm 3< , very particularly preferably at least 1*10 20< / cm 3< and / or a proportion of Si-Si bonds of at least 1*10 17< / cm 3< or even at least 5*10 17< / cm 3< , preferably at least 1*10 18< / cm 3< or even at least 5*10 18< / cm 3< , particularly preferably at least 1*10 19< / cm 3< or even at least 5*10 19< / cm 3< , very particularly preferably at least 1*10 20< / cm 3<.
[0037] The higher the proportion of these bonds in the quartz glass matrix, the more predetermined breaking points are present, which break particularly easily under high-energy irradiation. This makes the corresponding titanium-doped quartz glass particularly easy to compact, i.e., densify, under high-energy irradiation. Since these bonds do not recombine as easily as normal matrix bonds, i.e., do not return to their original state as easily after radiation-induced combination, such substrates exhibit less relaxation than conventional substrates based on titanium-doped quartz glass. Titanium-doped quartz glass with this composition can be obtained by flame hydrolysis or via a soot process under oxidizing conditions for an increased proportion of Si-OO-Si bonds, or under reducing conditions for an increased proportion of Si-Si bonds.In flame hydrolysis, the flame can be operated under either an excess of oxygen (oxidizing conditions) or an excess of hydrogen (reducing conditions). In the case of a soot process, the SiO2 powder can be treated in an oxygen, nitrous oxide, or steam atmosphere at elevated temperatures instead of or in addition to oxidizing conditions. To achieve reducing conditions, physical drying can be performed using elevated temperatures and / or applying a vacuum, or chemical drying with the addition of halogens can be used to form silicon chloride or silicon fluoride.
[0038] In variants, the substrate 51 additionally has an average hydroxyl content of at most 100 wt. ppm, at least in the vicinity of the surface region 511, in order to thereby provide a reduced number of matrix terminators and reduce the likelihood of relaxation after compaction. Particularly preferably, the substrate 51 has a matrix terminator content of at most 20% of the hydroxyl content, at least in the vicinity of the surface region 514, in order to further reduce the likelihood of relaxation. Other matrix terminators besides OH groups can be, for example, SiOH, SiF, SiH, TiOH, TiF, TiH, TiO2, TiO3. The blanks for such substrates are preferably produced using soot processes. The hydroxyl content can be reduced in particular by drying or by producing and storing in a particularly dry atmosphere.
[0039] In this variant, the substrate advantageously has a hydrogen content of less than 1×10 16 molecules / cm 3 near the surface region 511 or further inside the substrate 51, in order to avoid the risk of a slight increase in hydrogen-related matrix terminators such as SiOH and SiH reducing the effect achieved by the high purity of the titanium-doped quartz glass. The hydrogen content can be reduced, for example, by carrying out the direct deposition of quartz glass in a low-hydrogen, reducing atmosphere in the case of flame hydrolysis, for example by using natural gas or methane instead of oxyhydrogen as the fuel. Quartz glass deposited using soot processes a priori does not contain any hydrogen unless it is deliberately added.
[0040] In a second variant, which is shown schematically in Figure 3As shown, the substrate 51 has a hydrogen content of more than 5×10 18 molecules / cm 3 , preferably more than 1×10 19 molecules / cm 3 , particularly preferably more than 1×10 20 molecules / cm 3 , along an imaginary line 513 perpendicular to the surface region 511 over a length 517 of 500 nm or more. As a result, during compaction by high-energy irradiation, an increased number of permanently broken bonds can be generated, which can reduce relaxation of the compaction. In the example shown here, the region 515 with increased hydrogen content is located in the surface region 511 below the reflective coating 54.The length 517 of 500 nm, over which the substrate 51 has a particularly high hydrogen content, has a distance from the reflective coating 54 of no more than 1 mm, preferably no more than 100 µm, particularly preferably no more than 20 µm, and most preferably no more than 5 µm in the example shown here, so that the substrate 51 has a desired high hydrogen content as close as possible to the reflective coating 54. At a greater distance from the reflective coating 54 along the imaginary line 513 perpendicular to the surface region 511, the substrate 51 in the example shown here has a lower hydrogen content, as can also occur in conventional titanium-doped quartz glasses.In particular, the substrate 51 has, along the imaginary line 513 perpendicular to the surface region 511 with the reflective coating 54 at a distance therefrom of at least 1 mm, preferably at least 1 cm, a hydrogen content of less than 5×10 17< molecules / cm 3<, preferably less than 1×10 17< molecules / cm 3<, particularly preferably less than 1×10 16< molecules / cm 3<.
[0041] The titanium-doped quartz glass blank can be charged with a high hydrogen content prior to its processing into a substrate at temperatures above room temperature, approximately in the range up to 600°C, preferably at approximately 100°C to 200°C, particularly near the surface region 511. Higher temperatures, such as in the range of 400°C to 600°C, allow the desired hydrogen content to be reached more quickly, or particularly high hydrogen contents. However, at higher temperatures, increased Ti3+ formation can occur, which can lead to blackening of the quartz glass and also have an undesirable effect on the thermal expansion coefficient of the quartz glass.
[0042] The blank can also be initially machined largely or completely to its final shape, resulting in a substantially coatable substrate that is charged with hydrogen prior to coating. Both the blank and the substantially coatable substrate can be charged with hydrogen, preferably in an autoclave, at hydrogen partial pressures in the range of approximately 10 atm to 100 atm. Particularly at higher pressures, particularly narrow hydrogen gradients with high concentrations in the surface area can be achieved.
[0043] If material is removed from the surface by polishing after loading with hydrogen and before coating, the maximum hydrogen content distribution can be located particularly close to the subsequently applied reflective coating. Simulations suggest that even if, for example, the hydrogen content in the surface area, especially in the immediate vicinity below the reflective coating, is somewhat lower than desired shortly after coating due to longer storage times between loading and coating or targeted annealing, the hydrogen content will accumulate below the reflective coating over months and years.
[0044] After coating, any surface defects still present or which occurred during the coating process can be corrected by compacting irradiation. Alternatively, a surface compaction process can be carried out over at least the entire coated surface, optionally even before coating, in which bonds are broken in the irradiated substrate areas with a high hydrogen content and saturated as SiH or SiOH in order to further increase the long-term stability of the reflective optical element as a whole. During subsequent storage, the hydrogen can diffuse further into the substrate and also escape from the substrate, particularly at uncoated surfaces. For example, Mo / Si multilayer coatings are good diffusion barriers for hydrogen. Simulations suggest that substrates which are loaded with hydrogen on their surfaces before coating will retain their hydrogen content even after several years of storage.Surfaces coated with a Mo / Si multilayer system still exhibit very high hydrogen contents. On the uncoated surface areas, however, the hydrogen content can decrease significantly within months. In particular, reflective optical elements according to variant 2 and in conjunction with... Figure 3described, substrates 51 which, within a period of up to one month after application of the reflective coating 54, along an imaginary line 517 perpendicular to the surface region 511 with the reflective coating 54 over a length 517 of 500 nm or more, have a hydrogen content of more than 5×10 18< molecules / cm 3< and within a period of one month after application of the reflective coating 54 up to seven years after application of the reflective coating 54, still have a hydrogen content of more than 1×10 18< molecules / cm 3<. In the case of a reflective optical element whose substrate has a further surface region which is located on a side of the substrate facing away from the surface region with the reflective coating and which does not have a reflective coating, as is the case, for example, in Figure 3As is the case in the example shown, the substrate can have a hydrogen content of no more than half and no less than one twentieth of the hydrogen content over the length at a distance of no more than 1 mm from the reflective coating along the imaginary line 513 over a further length of 500 nm or more at a distance of no more than 2 mm from the surface of the further surface area over the said period of time. This is because on the side of the reflective optical element without a reflective coating, the hydrogen can diffuse out of the substrate over time. In the process, the maximum of the distribution of the hydrogen content slowly migrates into the interior of the substrate. The exact hydrogen content in the further surface area and its distribution at a specific time depend in particular on the specific hydrogen loading.
[0045] For example, the Figures 4 and 5which depicts a simulation based on loading titanium-doped quartz glass at a hydrogen partial pressure of 25 bar and a temperature of approximately 250°C for 5 hours. The resulting hydrogen content distribution is shown in Figure 4shown. The thickness of the substrate is plotted in mm on the x-axis. The substrate has a thickness of 4 cm and a reflective coating is assumed on the surface at 0 cm, which acts as a diffusion barrier for hydrogen, such as a molybdenum-silicon multilayer system. On the opposite surface at 4 cm, however, the surface is uncoated, so that the hydrogen present in the area of this surface can diffuse out of the substrate over time. After loading, both surfaces have a hydrogen content of 10×10 18< molecules / cm 3<, which is only just a tenth of this within a distance of one millimeter from the respective surface.
[0046] In Figure 5The simulated state after 7 years of storage at room temperature is shown. Adjacent to the reflective coating at 0 mm, the hydrogen content distribution has broadened slightly and decreased in amplitude by a factor of 4. On the uncoated, opposite side of the substrate at 4 mm, the distribution has decreased in amplitude by a factor of more than 20, and the hydrogen content distribution has also broadened slightly.
[0047] It should be noted that, for clarity, this effect is discussed here with reference to the surface with the reflective coating and the opposite surface without a coating. However, this effect is also expected for differently positioned surfaces, such as side surfaces. Here, too, a greater decrease in hydrogen content over time is to be expected if the respective surface is not coated after loading with hydrogen than if it is coated.
[0048] In a variation of the method used in conjunction with Figure 3 In the variant described, the substrate 51 can, in addition to the high hydrogen content, at least and preferably in the vicinity of the surface region 511, also have a proportion of Si-OO-Si bonds of at least 1*10 16< / cm 3< and / or a proportion of Si-Si bonds of at least 1*10 16< / cm 3< in order to more effectively reduce relaxation after compaction.
[0049] The hydroxyl and hydrogen contents, as well as the proportion of defects in the quartz glass matrix, such as Si-OO-Si bonds or Si-Si bonds, can be determined, for example, using Raman spectroscopy on the finished substrate or reflective optical element with resolutions down to the submillimeter range. Using confocal Raman spectroscopy, resolutions in the submicrometer range can also be achieved. Raman spectroscopy can also be used to determine the fictive glass transition temperature of different substrate regions, for example, via the ratio of three- to four-fold SiO2 rings. Depending on whether the region is uncorrected or compacted for correction by high-energy irradiation, different fictive glass transition temperatures and different defect densities can be expected.
[0050] In the Figures 2 or 3In the illustrated embodiments of a reflective optical element 50, the substrate 51 has a density variation of approximately 1 vol% at least along an imaginary surface 514 with a fixed distance between 1 µm and 100 µm from the surface 512. For the sake of clarity, this is only shown in Figure 2After coating the substrate, a fine correction of the surface profile was performed according to the procedure described in WO 2013 / 050199 A1. In particular, the correction was carried out by local compaction in area 516 of the substrate using an electron beam, with the electron energy being selected such that the electrons penetrate the reflective coating 54 with protective layer 53 and are completely deposited in the first few micrometers in the substrate 51 below the reflective coating 54. As a result, the titanium-doped quartz glass is compacted by up to approximately 1% for all substrate variants, which in the example shown here leads to a surface deformation of approximately 10 nm.
[0051] The reflective optical elements proposed here demonstrate improved long-term stability of the surface shape. In particular, the relaxation of the corrections inscribed by compaction is reduced. Even after, for example, seven years, the corrections can be expected to still exhibit an amplitude of more than two-thirds of their original amplitude.
[0052] In addition to EUV lithography, further preferred applications of the reflective optical elements based on the substrates proposed here include optical systems for inspection systems for, for example, wafers or masks or for spectroscopic applications, for example in astrophysics, in particular extraterrestrial physics. Reference symbol
[0053] 10EUV lithography device 12EUV radiation source 13Collector mirror 14Illumination system 15First mirror 16Second mirror 17Mask 18Third mirror 19Fourth mirror 20Projection system 21Wafer 50Collector mirror 51Substrate 511Surface area 512Surface 514Line 513Line 515Area 516Area 517Length 53Protective layer 54Multilayer system 55Layer pair 56Absorber 57Spacer
Claims
1. Substrate for a reflective optical element for the extreme ultraviolet wavelength range made of titanium-doped quartz glass that has a surface region that is to be coated, characterized in that the titanium-doped quartz glass has at least in the vicinity of the surface region (511) a proportion of Si-O-O-Si bonds of at least 1*1016 / cm3 or a proportion of Si-Si bonds of at least 1*1016 / cm3.
2. Substrate according to Claim 1, characterized in that the titanium-doped quartz glass has at least in the vicinity of the surface region (511) a proportion of Si-O-O-Si bonds of at least 1*1017 / cm3, preferably at least 1*1018 / cm3, with particular preference at least 1*1019 / cm3 or a proportion of Si-Si bonds of at least 1*1017 / cm3, preferably at least 1*1018 / cm3, with particular preference at least 1*1019 / cm3.
3. Substrate according to Claim 1 or 2, characterized in that the titanium-doped quartz glass has an average hydroxyl content of at most 100 ppm by weight at least in the vicinity of the surface region (511).
4. Substrate according to Claim 3, characterized in that the titanium-doped quartz glass has a hydrogen content of less than 1×1016 molecules / cm3 at least in the vicinity of the surface region (511).
5. Substrate according to one of Claims 1 to 4, characterized in that the titanium-doped quartz glass has silicon fluoride or silicon chloride at least in the vicinity of the surface region (511).
6. Substrate according to Claim 1 or 2, characterized in that the titanium-doped quartz glass has a hydrogen content of more than 5×1018 molecules / cm3 along an imaginary line (513) perpendicular to the surface region (511) over a length (517) of 500 nm or more.
7. Reflective optical element for the extreme ultraviolet wavelength range having a substrate according to one of Claims 1 to 6 that has a surface region with a reflective coating.
8. Reflective optical element according to Claim 7 when dependent on Claim 1 to 3, 5 or 6, characterized in that the substrate (51) has a hydrogen content of more than 5×1018 molecules / cm3, preferably more than 1×1019 molecules / cm3, with particular preference more than 1×1020 molecules / cm3, along an imaginary line (513) perpendicular to the surface region (511) with the reflective coating (54) over a length (517) of 500 nm or more.
9. Reflective optical element according to Claim 8, characterized in that the length (517) of 500 nm or more has a distance from the reflective coating (54) of no more than 1 mm, preferably no more than 100 µm, with particular preference no more than 20 µm, with very particular preference no more than 5 µm.
10. Reflective optical element according to Claim 8 or 9, characterized in that the substrate (51) has a hydrogen content of less than 5×1017 molecules / cm3, preferably less than 1×1017 molecules / cm3, with particular preference less than 1×1016 molecules / cm3, along the imaginary line (513) perpendicular to the surface region (511) with the reflective coating (54) at a distance therefrom of at least 1 mm, preferably at least 1 cm.
11. Reflective optical element according to one of Claims 8 to 10, characterized in that the substrate (51) has a hydrogen content of more than 5×1018 molecules / cm3 within a time period of up to one month after application of the reflective coating (54) along an imaginary line (513) perpendicular to the surface region (511) with the reflective coating (54) over a length (517) of 500 nm or more and has a hydrogen content of more than 1×1018 molecules / cm3 within a time period from one month after application of the reflective coating (54) up to seven years after application of the reflective coating (54).
12. Reflective optical element according to Claims 9 and 11, the substrate of which has a further surface region, which is located on a side of the substrate facing away from the surface region with the reflective coating and has no reflective coating, characterized in that the substrate (51) has, along the imaginary line (513) over a further length of 500 nm or more at a distance of no more than 2 mm from the surface of the further surface region, a hydrogen content of no more than half and no less than one twentieth of the hydrogen content over the length (517) at a distance of no more than 1 mm from the reflective coating.
13. Optical system having a reflective optical element according to one of Claims 7 to 12.
14. EUV lithography apparatus having an optical system according to Claim 13 or having a reflective optical element according to one of Claims 7 to 12.