METHOD FOR MANUFACTURING A HOSE NIPPLE
Patent Information
- Application Number
- DE502020009484
- Authority / Receiving Office
- DE · DE
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2019-07-05
- Filing Date
- 2020-06-05
- Publication Date
- 2024-10-31
- Estimated Expiration
- 2040-06-05
AI Technical Summary
Existing manufacturing processes for profiled hose nipples often result in imprecise dimensions, material weakening, and the risk of leaks, with methods like machining producing chips and rolling/hammering not ensuring sufficient accuracy or strength, while cold-forming reduces diameter and creates burrs.
A method involving a pre-tool with a forming die and compression sleeve to compress and radially reduce the pipe section's diameter, followed by expansion and hammering to form a high-precision outer contour without cutting, ensuring strength and precision without diameter reduction or burrs.
This method enables high-precision, high-strength hose nipple production with enhanced pressure resistance and tightness, eliminating the need for welding or soldering and minimizing material waste.
Description
[0001] The invention relates to a manufacturing method for profiled hose nipples.
[0002] Hose nipples are primarily used in fluid technology for attaching flexible fluid lines, such as rubber hoses. Because the fluid line must be secured to the hose nipple, these nipples have an external profile. This profile is designed so that, for example, when the fluid line is crimped onto the nipple, the profile is pressed into the fluid line material, ensuring a tight connection that prevents the fluid line from slipping off the nipple.
[0003] Due to ever-increasing demands on the tightness of the connections between hose and nipple, high accuracy and strength of the nipples are required.
[0004] Hose nipples can be manufactured in various ways. For example, the nipple profile can be created by turning, grinding, rolling, hammering, or pressing. Pre-fabricated nipples can also be welded onto pipes, but this is relatively complex and carries the risk of leaks.
[0005] Machining has the disadvantage that it can produce chips which must be carefully removed or the parts must be disposed of. While rolling and hammering are chipless processes, the result is not always precise enough. Furthermore, the associated reduction in diameter is not always acceptable.
[0006] WO 1986 00 68 13 A1 discloses a method in which a pipe end is deformed into a predetermined profiled shape by cold forming and diameter reduction. Besides the risk of burrs forming during this process, a further disadvantage is that the diameter of the pipe is reduced in the area of the nipple. This leads to a lower flow rate in the nipple area, so that the entire pipe may need to be designed with a larger diameter. Further manufacturing methods for profiled hose nipples are disclosed in JP2016022490A, US4330142A, and FR2332476A.
[0007] The invention was based on the objective of creating a method by which hose nipples of the type described above can be easily manufactured while avoiding the aforementioned disadvantages and without reducing the diameter.
[0008] This task is solved by the fact that the procedure comprises the following steps, namely Provision of a pre-tool comprising a forming punch, a crushing sleeve, and a pipe holder; insertion of a pipe section into the pipe holder; insertion of the forming punch into the interior of the pipe section; sliding the crushing sleeve onto the pipe section with the forming punch inserted, wherein the crushing sleeve has a predetermined smaller inner diameter than the pipe section, wherein, upon sliding the crushing sleeve onto the pipe section, the pipe section is axially crushed on the one hand and radially reduced in diameter to a predetermined dimension on the other, thereby forming a flange on the pipe section; retraction of the forming punch through the part of the pipe section located in the crushing sleeve, thereby widening the inner diameter of the pipe section by a predetermined amount, given by a preselected ratio of the original inner diameter of the pipe section and the outer diameter of the forming punch.which reduces the wall thickness of the pipe section in the area of the compression sleeve, removal of the pipe section from the compression sleeve, sliding the pipe section onto a support mandrel with a predetermined diameter, provision of a hammering tool and hammering of the pipe section, thereby forming a predetermined outer contour of the pipe section, removal of the finished part from the tool.
[0009] This process enables the high-precision production of hose nipples of the type described. By reducing the wall thickness of the pipe section while simultaneously pre-calibrating the inner and outer diameters, a strengthening of the pipe section material can be achieved. Thus, high-strength hose nipples can be produced using the process according to the invention.
[0010] The entire process, except for deburring at the nipple tip, is virtually chip-free. No burrs are present on the critical outer surfaces of the nipple. Hose nipples produced in this way have proven their high pressure resistance and leak-tightness, along with high fatigue strength, in corresponding test runs.
[0011] An example of the invention is explained in more detail below with reference to the drawing. It shows Fig. 1 a pre-formed pipe section in a partial longitudinal section, Fig. 2 a pre-formed hose nipple.
[0012] The Fig. 1Figure 1 shows a pre-formed pipe section 1 in a partial longitudinal section. At its first end 2, the pipe section 1 has a region 3 in which, by a prior insertion of a compression sleeve (not shown here), the outer diameter 4 of the pipe section 1 is reduced compared to the outer diameter 5 of the remaining pipe section, and the wall thickness 6 in section 3 is reduced compared to the wall thickness 7 of the remaining pipe section 1.
[0013] Furthermore, the insertion of the sleeve (not shown) has caused a compression ring 9 to be dented.
[0014] The inner diameter 8 of pipe section 1 was initially reduced in area 3 by the compression sleeve (not shown), and then expanded again to a predetermined dimension after calibrating with a forming die (not shown) after passing through the compression chamber. Through the interaction of the compression sleeve and the forming tool (both not shown), the geometry of pipe section 1 shown in section 3, with a defined inner diameter 8, outer diameter 4, and wall thickness 6, can be produced with high precision. This fulfills the requirements for a subsequent hammering process.
[0015] In Fig. 2 A fully formed hose nipple 10, produced using the inventive method, is shown. It is based on a prefabricated blank, such as the one described in Fig. 1 is shown.
[0016] The hose nipple 10 has a shape approximately like that of the one from the Fig. 1A profile 12, which has profile grooves 12 A and profile webs 12 B, is formed in the already prefabricated area 3 corresponding to area 11. This profile 12 was produced by a hammering process, which is known per se and is not shown here.
[0017] To ensure that the inner diameter 13 in area 11 does not fall below a predetermined value during hammering, the hammering process takes place on a mandrel, not shown here, inserted into the interior of the hose nipple 10.
[0018] The manufacturing process according to the invention produces a high-precision hose nipple with very good strength, which can be manufactured directly from a pipe section without soldering or welding. Reference symbol list (Part of the description)
[0019] 1 Pre-formed pipe section 2 First end of pre-formed pipe section 1 3 Formed area of pipe section 1 4 Outer diameter of pipe section 1 in area 3 5 Outer diameter of pipe section 1 outside area 3 6 Wall thickness of pipe section 1 in area 3 7 Wall thickness of pipe section 1 outside area 3 8 Inner diameter of pipe section 1 9 Fitting collar of pipe section 1 10 Hose nipple 11 Profiled area of hose nipple 10 12 In area 11 of hose nipple 10 12A Profile grooves of profile 12 12B Profile webs of profile 12 13 Inner diameter of hose nipple in area 11
Claims
1. Production method for profiled hose nipples (10), characterized in that the method comprises the following operative steps: - providing a preliminary tool having a forming die, a compression sleeve and a tube holder; - placing a tubular portion (1) into the tube holder; - introducing the forming die into the interior of the tubular portion (1); - pushing the compression sleeve onto the tubular portion (1) having the inserted forming die, wherein the compression sleeve has a predetermined smaller internal diameter (4) than the tubular portion (1), wherein - when pushing on the compression sleeve - the tubular portion (1) is axially compressed, on the one hand, and in terms of the diameter is radially reduced to a predetermined dimension (4), on the other hand, while forming an enclosure collar (9) on the tubular portion (1); - retracting the forming die through that part (3) of the tubular portion (1) that is located in the compression sleeve, while enlarging the internal diameter (8) of the tubular portion (1) by a predetermined dimension which is defined by a preselected ratio of original internal diameter (8) of the tubular portion (1) and external diameter of the forming die, as a result of which the wall thickness (6) of the tubular portion (1) in the region (3) of the compression sleeve is reduced; - retrieving the tubular portion (1) from the compression sleeve; - pushing the tubular portion (1) onto a supporting mandrel having a predetermined diameter; - providing a hammering tool and hammering the tubular portion (1) while forming a predetermined external contour (12) of the tubular portion (1); and - retrieving the finished part (10) from the tool.