METHOD FOR PRODUCING PLASTIC INJECTION-MOLDED COMPONENTS AND PLASTIC INJECTION-MOLDED COMPONENT
Patent Information
- Application Number
- DE502022001801
- Authority / Receiving Office
- DE · DE
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2021-09-16
- Filing Date
- 2022-08-31
- Publication Date
- 2024-10-17
- Estimated Expiration
- 2042-08-31
AI Technical Summary
Existing methods for producing plastic injection molded components with sensor holders, such as two-component injection molding, result in visible sensors and inadequate heat conduction, leading to surface disturbances and inefficient temperature management.
A method involving a temperature-controlled stamp forming a bead on the surface of the plastic injection molded component, where the stamp is pressed into the component to create a recess for the sensor, with precise temperature control and limited melting zone to maintain surface integrity and secure sensor holding.
This method allows for secure sensor holding without disturbing the visible surface and achieves a localized, short-term temperature increase, enhancing the production of plastic components with embedded sensors.
Description
[0001] The invention relates to a method for producing plastic injection-molded components with at least one holder for sensors and plastic injection-molded component. State of the art
[0002] In motor vehicles, sensors are installed in body parts for distance measurement, for example. Such sensors can be installed in a front and / or rear bumper and measure the distance to an obstacle or another vehicle while parking. Such systems are known as PDC sensors.
[0003] Common sensors of this type are embedded in bumper openings and painted in the same color as the vehicle or bumper. DE 103 14 862 A1 shows an example of a PDC sensor embedded in a body panel, bumper strip, or bumper.
[0004] The disadvantage of such a solution is the visibility of the sensors, even if their visible surface is painted in the color of the bumper strip.
[0005] DE 200 10 478 U1 discloses a vehicle component comprising a fastening element for a parking sensor on a bumper. The fastening element comprises a connecting part and an installation housing, which are manufactured from different plastic materials, e.g., using a two-component injection molding process, and are positively connected to one another. The connecting part has the task of fastening the entire fastening element, including the installed parking sensor, to the bumper of a motor vehicle, in particular via a welded connection. The connecting part has a substantially cylindrical receiving part, on the upper edge of which a welding flange enclosing an opening is provided. The parking sensor is arranged in this opening when it is received in the cylindrical installation housing and secured thereto.
[0006] DE 10 2006 022 925 B4 discloses a component used to accommodate sensors. The first component of the component is made of polycarbonate and forms a continuous, flat outer part of the component. The holder mounts the sensor on the inside of the first component. In this case, both the first component and the second component of the component, which forms the holder for the sensor, are formed in the 2K injection molding process, eliminating the need for an additional mounting part.
[0007] Hot staking is a process for joining two components, at least one of which is made of thermoplastic. Hot staking takes advantage of the fact that thermoplastics assume a doughy state when heat is applied. Examples of thermoplastics include polyethylene (PE), polypropylene (PP), polyvinyl chloride (PVC), and polycarbonate (PC). The process is also suitable for thermoplastics with a high glass fiber content. When heated, the material becomes soft and malleable. In this state, it can be welded to the adjacent area or formed with a stamp. This creates a permanent form- and force-fitting, sometimes also material-fitting, connection that allows the transmission of forces and torques. Since plastics are poor heat conductors and the process only requires short periods of time (a few seconds), the temperature increase is limited to a small spatial area.
[0008] DE 199 20 941 A1 shows a method for producing plastic parts with an embossed structure for three-dimensional injection-molded circuit carriers by hot-stamping a conductor track structure from a film onto an injection-molded substrate.
[0009] The operation of the injection molding machine is such that the plastic part is injected in cycle 1 and the embossing step is carried out simultaneously in cycle 2.
[0010] DE 198 19 791 A1 discloses a device for separating a formed substrate from an embossing tool, comprising a pair of mutually adjustable chamber parts of a closable chamber, of which a first chamber part serves as a support for the embossing tool, and a second chamber part serves as a support for the formable substrate. The chamber contains a substrate holder that, when the chamber is closed, fixes the substrate to its support outside the embossing area, whereby, when the chamber is opened, the substrate is detached from the embossing tool. The second chamber part is formed by an annular projection of the substrate holder and not by the embossing die itself. The annular second chamber part is pressurized with compressed air to allow easier demolding of the substrate.
[0011] US 5 681 556 A1 discloses a method for producing a plastic injection-molded component from a plastic with at least one recess suitable for receiving sensors by forming a bead on the surface of the plastic injection-molded component with the following steps: producing the plastic injection-molded component in a tool with upper and lower tool halves, introducing a temperature-controlled punch which is guided in a sleeve, placing the sleeve with integrated annular space on the surface of the plastic injection-molded component, pressing the temperature-controlled punch into the surface of the plastic injection-molded component to form an annular bead in the annular space by displacing molten material of the plastic injection-molded component in the direction of the annular space and cooling the punch and lifting it off the surface.
[0012] DE 196 07 855 C1 describes a process for producing molded parts with a surface covered with a facing or decorative material by back-injection molding and subsequent folding. In this process, one end of the facing or decorative material is bent by pressing it into the still plastically deformable molded part using three slide tools.
[0013] The object of the invention is to produce a component which dispenses with two-component injection molding and nevertheless allows a sensor to be held securely, whereby the externally visible surface of the component remains undisturbed and whereby a spatially limited temperature increase is generated for short time intervals of a few seconds in a poor heat conductor. Description of the invention
[0014] The object is achieved by a method for producing a plastic injection-molded component from a plastic with at least one recess for receiving sensors by forming a bead on the surface (8) of the plastic injection-molded component, comprising the following steps: Manufacturing the plastic injection-molded component in a tool with upper and lower tool halves, lifting the upper tool half and inserting a temperature-controlled punch which is guided in a sleeve, placing the sleeve with integrated annular space on the surface of the plastic injection-molded component, pressing the temperature-controlled punch into the surface of the plastic injection-molded component to form an annular bead in the annular space by displacing molten material of the plastic injection-molded component in the direction of the annular space, cooling the punch (3) and lifting it off the surface.
[0015] The annular space is limited by the surface of the injection-molded component, the outer surface of the sleeve, the boundary of the sleeve, and the outer surface of the punch.
[0016] The problem is also solved by a method in which the insertion depth of the punch is greater than or equal to half the thickness of the plastic injection-molded component. Description of the characters
[0017] Figure 1a, 1b, 1c shows schematically the manufacturing steps of a bracket in a plastic injection molding plant, Figure 2 shows details of the stamp.
[0018] Figure 1aschematically shows an injection molding tool consisting of a lower tool half 5 and an upper tool half 9. The two tool halves 5, 9 form a cavity that determines the shape of the plastic injection-molded component 2. The plastic injection-molded component 2 is defined by the two inner surfaces of the two tool halves 5 and 9, whereby the edges are not further shown as boundaries in the diagram shown.
[0019] After the plastic injection-molded component 2 has been produced, the upper mold half 9 is lifted off. The plastic injection-molded component 2 remains on the lower mold half 5 and can be tempered via the support surface. For example, it can be cooled more slowly than after complete demolding.
[0020] In order to create a recess for the installation of a sensor, a temperature-controlled stamp 3 is placed on the surface 8 of the injection-molded component 2.
[0021] Surface 8 is the side facing inward in the vehicle. The temperature-controlled die 3 is located in a sleeve 6, which is inserted into the injection molding machine by a tool holder (not shown).
[0022] The exact design of the punch 3 and the sleeve 6 is shown in Figure 2 explained in more detail. The sleeve 6 consists of a cylinder with an outer surface 6A and an inner surface 6B. The sleeve 6 has a horizontal boundary 6C that connects the inner surface 6B to the outer surface 6A. The inner surface 6B is shorter than the outer surface 6A. The outer surface 6A sits flush with the injection-molded component 2, while the inner surface 6A is spaced a certain height h from the surface of the plastic injection-molded component 2.
[0023] This creates a space 4 that forms a ring in a cylindrical punch 3. This annular space 4 is initially bounded by the surface 8 of the injection-molded component 2, the outer surface 6A of the sleeve 6, the boundary 6C of the sleeve 6, and the outer surface of the punch 3.
[0024] In the next process step, the punch 3 is heated and pressed under pressure into the injection-molded component 2. The pressing takes place to a depth that does not penetrate the total thickness D of the injection-molded component 2. However, the penetration depth is greater than half the thickness D / 2 of the plastic injection-molded component 2. As a result, the punch 3 penetrates the plastic injection-molded component 2 and penetrates the central axis 7 of the plastic injection-molded component 2.
[0025] Due to the heat input of the stamping die 3, the material of the plastic injection-molded component 2 melts and is displaced primarily upwards by the pressure of the stamping die 3 and the limited melting zone within the plastic injection-molded component 2. The melting zone forms only a narrow ring around the heated stamping die and does not extend far into the plastic injection-molded component 2. As a result, the material enters the designated annular space 4.
[0026] In the next process step, the stamp 3 is no longer heated; it may even be cooled. The stamp 3 is then removed upwards from the plastic injection-molded component 2.
[0027] Since the forming takes place with the punch 3 in the lower tool half 5, the outer surface 10 of the plastic injection-molded component 2 always remains in contact with the lower tool half 5. This minimizes the effects of minimal temperature input and the surface is cooled and stabilized by the lower tool half in order to maintain an optimal surface on the surface facing the outside of the vehicle.
[0028] The plastic injection-molded component 2 can then be removed from the mold. It now has the shape specified by the injection mold and a recess adapted to the shape of a sensor to be installed. An annular bead is created by the treatment with the stamp and serves as a frame and for securing a sensor to be installed.
[0029] The shape of each recess in the plastic injection-molded component 2 is determined by the used punch 3 and sleeve 6. The punches 3 and sleeve 6 are coated with materials that easily detach from the material. This prevents the pulling out of material threads during removal.
[0030] The temperature profile, the speed at which the stamp sinks, the force of the stamp and the optimal times for dwell and cooling are precisely adapted to each specific application.
Claims
1. Method for producing an injection-moulded plastic component (2) made of a plastic having at least one recess for accommodating sensors by forming a bead on the surface (8) of the injection-moulded plastic component (2), having the following steps: producing the injection-moulded plastic component (2) in a mould having top and bottom mould halves (5, 9), raising the top mould half (9) and introducing a thermoregulatable ram (3) which is guided in a sleeve (6), placing the sleeve (6) with integrated annular space (4) on the surface of the injection-moulded plastic component (2), pressing the thermoregulated ram (3) into the surface (8) of the injection-moulded plastic component (2) to form an annular bead in the annular space (4) by displacing melted material of the injection-moulded plastic component (2) in the direction of the annular space (4), cooling the ram (3) and raising it from the surface (8), characterized in that the annular space (4) is bounded by the surface (8) of the injection-moulded plastic component (2), the outer face (6A) of the sleeve (6), the boundary (6C) of the sleeve (6), and the outer casing of the ram (3).
2. Method according to Claim 1, characterized in that the press-in depth of the ram (3) is not less than half the thickness D of the injection-moulded plastic component (2).
3. Method according to either of the preceding claims, where the annular space (4) and the sleeve (6) and the ram (3) exhibit any desired contour of the annular space (4).