METHOD FOR OPERATING A SMOKING-OFF KERNEL
Patent Information
- Application Number
- DE502023005303
- Authority / Receiving Office
- DE · DE
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2022-11-07
- Filing Date
- 2023-11-06
- Publication Date
- 2026-11-05
- Estimated Expiration
- 2043-11-06
AI Technical Summary
The reductive environment in the staged combustion process of cement clinker production is not sufficiently reactive, requiring a high excess of carbon monoxide to effectively reduce nitrogen oxides, leading to undesirable carbon monoxide slip.
Operate the carbon monoxide reactor with precise process parameters, including an air-fuel ratio between 0.05 and 0.3, controlled temperature between 800°C to 1200°C, and adjusted rotational speed of the carbonization reactor, along with specific fuel preparation and residence time, to enhance the reactivity of pyrolysis gases for effective NOx reduction.
Achieves efficient NOx reduction with reduced carbon monoxide excess, producing a high yield of short-lived hydrocarbons that enhance the reactivity of exhaust gases for stable NOx conversion.
Description
[0001] The invention relates to a method for operating a carbonization furnace in a plant for the production of cement clinker, comprising at least one rotary kiln for sintering cement clinker, at least one clinker cooler downstream of the rotary kiln in the material flow and at least one carbonization reactor in which solid secondary fuels are carbonized in a co-current process to produce carbon monoxide (CO).
[0002] To produce cement clinker using the so-called dry process, a meal of silicate-bearing rock and carbonate-bearing rock is first heated in a heat exchanger and then subjected to heat treatment in a calciner to thermally drive off carbon dioxide (CO₂) from the carbonate-bearing rock, producing quicklime or calcium oxide (CaO). The heat-treated rock meal is then sintered into cement clinker in a rotary kiln at approximately 1,450°C in an oxidizing gas environment. Nitrogen oxides (NOₓ) are produced in both the rotary kiln and the calciner by the combustion of so-called fuel nitrogen, namely nitrogen chemically bound in the fuel, usually as an amine (R-NH₂), and by the combustion of so-called atmospheric nitrogen, namely the elemental nitrogen (N₂) present in the atmosphere.To reduce these nitrogen oxides (NOx) back to elemental nitrogen (N2) in the cement clinker production plant, carbon monoxide (CO) is introduced into the calciner, thus implementing staged combustion. The stages are created by an oxidative environment in the rotary kiln, near the kiln head, and in parts of the calciner. This is followed by a reducing environment due to the introduction of carbon monoxide (CO). Here, the nitrogen oxides (NOx) generated in the oxidative environment of the rotary kiln are given the opportunity to react with carbon monoxide (CO), ideally producing carbon dioxide (CO2) and elemental nitrogen (N2). Controlling the staged combustion process in the calciner, which itself is a fluidized bed reactor for the rock flour being deacidified, is not straightforward. Gas streams do not form stably in the calciner, and turbulence can occur.A stable, laminar flow is repeatedly disrupted by the suspended rock flour. Consequently, it is necessary to operate with a high excess of carbon monoxide to reliably and quantitatively reduce the nitrogen oxides (NOx). This, in turn, results in undesirable carbon monoxide slip. It would be desirable if the reductive environment in the staged combustion process were more reactive, so that the combustion of nitrogen oxides (NOx) could occur with a lower excess of carbon monoxide (CO).
[0003] Document WO 2021 / 104766 A1 discloses a plant for the production of cement clinker in which a rotary kiln for sintering is combined with a separate rotary drum reactor for the carbonization of secondary fuels. The rotary drum reactor is designed such that gas and solid streams are conducted countercurrently. This process is intended to carbonize unsorted secondary fuels in particular and to eliminate the need for a pilot burner.
[0004] US Patent 6,626,662 B2 discloses a process for producing cement clinker with an additional rotary drum reactor in which secondary fuels are processed in co-current flow together with a partial flow of tertiary air and a partial flow of raw meal. The raw meal serves for uniform heat transfer and temperature stabilization in the reactor, while the supplied tertiary air supports the combustion of the secondary fuels.
[0005] US Patent 6,468,075 B2 describes a device with a so-called strand calcinator in which a DeNOx burner is used to create a CO-containing reduction zone. A variable supply of tertiary air is provided to control the gas composition in the calciner, with the oxygen content and thus the effectiveness of the NOx reduction being regulated via a throttle valve in the rotary kiln exhaust gas stream.
[0006] The object of the invention is to make the reductive environment in the staged combustion process more reactive.
[0007] The problem according to the invention is solved by a method according to claim 1. Further advantageous embodiments are specified in the dependent claims to claim 1.
[0008] According to the invention, it is intended that the carbon monoxide (CO) reactor used for the production of carbon monoxide is operated with a narrow set of process parameters.
[0009] An important process parameter is the air-fuel ratio λ and the allothermic operation. Depending on the process conditions, different types of carbonization occur simultaneously in the carbonization reactor. When the secondary fuel is combusted with oxygen (O₂), carbon dioxide (CO₂) is produced from a generally exothermic combustion reaction, and carbon monoxide (CO) is also produced in a generally weakly exothermic to endothermic combustion reaction. In substoichiometric carbonization operation, where less oxygen (O₂) is supplied than is required for the complete combustion of the available secondary fuel, both types of carbonization occur concurrently. The waste heat generated during the combustion to carbon dioxide (CO₂) supports the carbonization to carbon monoxide (CO) of further secondary fuel components.If the waste heat from the exothermic reaction to carbon dioxide (CO₂) and the more endothermic reaction to carbon monoxide (CO) balance each other, an autothermal process takes place. If the waste heat from the combustion to carbon dioxide (CO₂) is subject to the more endothermic reaction to carbon monoxide (CO), a transition to an allothermic process occurs. This latter process is known as "substoichiometric operation." The remaining combustion to carbon dioxide (CO₂) in this process leads to relatively unreactive pyrolysis gases. The observation made during the invention is that if the formation of carbon dioxide (CO₂) is avoided, the pyrolysis gases become more reactive, which could be explained by the formation of short-lived, radical gas components as well as short-lived hydrocarbons in the pyrolysis gases.There is a less precisely defined lower limit for the air-fuel ratio λ, below which pyrolysis to carbon monoxide (CO) only occurs with a considerable input of process heat. At this lower limit, the air-fuel ratio λ is very low, so that no combustion to CO₂ is observed. Pyrolysis with such a low air-fuel ratio λ requires significant thermal energy to maintain. Furthermore, the air-fuel ratio λ must not fall below a critical lower value, because with an excessive lack of atmospheric oxygen (O₂), further processes occur in the presence of significant waste heat, in which water (H₂O) and sulfur (S) are driven from the secondary fuels. Therefore, pyrolysis with a significant heat input and the exclusion of atmospheric oxygen (O₂) is more akin to carbonization or coking, which does not produce the desired reactive pyrolysis gases.
[0010] An ideal air-fuel ratio λ, also called "excess air ratio λ", has proven advantageous when this ratio λ is between 0.05 and 0.3, preferably between 0.1 and 0.2. In strongly substoichiometric operation of the carbonization reactor with an air-fuel ratio λ significantly less than 1, increased carbon monoxide (CO) formation is ensured. The air-fuel ratio λ is adjusted by mixing the oxygen-depleted exhaust air from a rotary kiln used for sintering cement clinker with the exhaust air from a clinker cooler, which has an atmospheric oxygen content. It is important that the temperature of the mixed exhaust air does not become too low during this process.
[0011] An ideal temperature range has been found to be approximately 800°C to 1200°C for the treatment temperature of the secondary fuels in the rotary kiln. Within this range, the treatment temperature can be adjusted by varying the amount of fuel supplied per unit of time. As the temperature increases, the fuel supply per unit of time is increased, and as the temperature decreases, the fuel supply per unit of time is decreased. This seemingly inverse control—lowering the temperature with more fuel—originates from the Boudouard reaction. However, in addition to the Boudouard reaction, the carbonization of secondary fuels according to the invention involves a multitude of other reactions, such as the formation of short-lived, radical gas components, the formation of reactive hydrocarbons, the formation of water, and the release of sulfur.If the pyrolysis temperature becomes too high, the released water (H₂O) can, for example, be undesirably split into hydrogen (H₂) and oxygen (O₂). The invention relates to determining, in this mixture of a multitude of parallel pyrolysis reactions, the process parameters within which the utilization of the pyrolysis gases for further use as a gas for denitrification becomes more effective. In order to control the temperature without interfering with the pyrolysis reaction itself, it can also be provided to feed raw meal into the pyrolysis reactor. Raw meal contains lime (CaCO₃), which, when heated, formally releases carbon dioxide (CO₂) and is itself converted to quicklime (CaO). This deacidification reaction is strongly endothermic and can be used to reduce the pyrolysis temperature if it increases too much.If the following process parameters are adhered to, the temperature can also be controlled by selecting the rotational speed of the carbonization reactor. To increase the temperature, the rotational speed can be varied within a range of 0.3 to 3 revolutions per minute, and vice versa. An increased rotational speed increases the surface area release of secondary fuel per unit of time, and vice versa. To ensure that slower and faster rotation has a reliable and predictable effect on the temperature in the carbonization furnace, it is advantageous to adhere to the following process parameters.
[0012] Another highly advantageous process parameter is therefore the particle size of the solid secondary fuel. If the secondary fuel is too fine-grained, it tends to burn rapidly. This results in less carbon monoxide and little to no pyrolysis gases, which contain a high proportion of short-lived hydrocarbons. The inventors' experience with the operation of carbonization reactors shows that high proportions of short-lived hydrocarbons in the exhaust gases of these reactors, which can be detected by gas analysis using Raman or IR probes, significantly reduce the plant's nitrogen oxide emissions in addition to carbon monoxide. If the particle size is too large, hot spots form in the carbonization reactor that burn only slowly. This also results in fewer pyrolysis gases.It has been observed that pyrolysis gas production reaches its maximum when secondary fuels, if flat, such as industrial cardboard, roofing felt, wooden boards, or sheet-like industrial waste, have an edge length of approximately 500 mm and are no larger. A lower limit is approximately 100 mm to 150 mm. For lumpy fuels, such as shredded wood waste, wood chips, solid organic waste, or crushed industrial waste, the particle size should be around 80 mm. If they are significantly smaller, combustion becomes excessive. If they are larger, embers will form. A lower limit is approximately 15 mm to 20 mm.
[0013] To control the combustion of secondary fuels intended for smoldering, ensuring that a high proportion of short-lived hydrocarbons is produced alongside carbon monoxide (CO), it has proven advantageous to condition the secondary fuels before use so that they have a moisture content of less than 40%. The secondary fuels should have a carbon content of at least 5% and no more than 80%. Lower carbon content leads to the formation of other substances during smoldering, but too little carbon monoxide (CO). A higher carbon content, for example in pre-charred wood, reduces the formation of short-lived hydrocarbons. The hydrogen content of the secondary fuel is also important. A hydrogen content of 1% to 15% has proven advantageous.Higher concentrations of hydrogen (H₂) in the secondary fuel lead to excessive water formation in the pyrolysis gases. The mineral raw material content should also be less than 70%. With agricultural waste, or with industrial waste such as the incineration of industrial waste containing rock fibers or glass fibers, the mineral content can be high. A high mineral content leads to significant slag formation, which ultimately finds its way into the cement clinker and can considerably affect its quality. The sum of the aforementioned constituents can reach up to 100%. If the sum is lower, other accompanying substances are present, such as sulfur compounds and nitrogen compounds.
[0014] The residence time of the secondary fuel in the carbonization reactor also influences the quality of the resulting exhaust gases. It has proven advantageous to set a residence time of 1 to 45 minutes for the secondary fuel in the carbonization reactor, adjustable via a feed mechanism. In a rotary kiln, the feed mechanism is the combination of the kiln's tilt angle and its rotational speed. It is therefore advantageous if the carbonization reactor has a rotary kiln with a tilt angle between 1° and 8° and an adjustable rotational speed.
[0015] The exhaust gases from the carbonization reactor are finally fed into the calcinator of the plant for the production of cement clinker, where they serve to reduce nitrogen oxides.
[0016] The treatment of mineral residues after carbonization can vary. It is possible that the mineral components remaining after the combustion of the secondary fuels fall into the rotary kiln inlet chamber. There, the mineral components combine with the cement clinker. Organic waste is usually calcareous or silicate-containing residue.
[0017] The invention is explained in more detail with reference to the following figures. They show: Fig. 1 a plant for the production of cement clinker with a carbonization reactor, Fig. 2 a plant for the production of cement clinker with a carbonization reactor, wherein a sluice gate for removing the mineral combustion residue is arranged between the carbonization reactor and the calcinator.
[0018] In Figure 1Figure 1000 depicts a plant for the production of cement clinker. In this plant, a gas stream begins with the cooling air L at the clinker cooler 130 and flows into a material stream beginning with the raw meal, which is fed into the plant 1000 at the upper end of a cyclone heat exchanger 160. The cooling air L cools the fresh cement clinker Z in the clinker cooler 130 and flows as tertiary air into a tertiary air line 131 and as secondary air into the rotary kiln 120. The hot tertiary air, containing atmospheric oxygen, flows into the calciner 140 to maintain fuel combustion. The secondary air leaves the rotary kiln 120 with a very low oxygen content of approximately 2%–4%. From the tertiary air line 131, a line leads to the pyrolysis reactor 100, which, controlled by a slide valve 122, directs a certain amount of tertiary air into the pyrolysis reactor.Furthermore, a line 123 leads from the rotary kiln inlet chamber 121 to the carbonization reactor 100. By mixing the tertiary air, which contains atmospheric oxygen, with the oxygen-depleted rotary kiln exhaust air in line 123, the oxygen content in the carbonization reactor 100 can be precisely adjusted. Secondary fuel 110, with a controlled particle size, is fed into the carbonization reactor 100 and carbonized there under controlled conditions. This process produces not only carbon monoxide but also pyrolysis gases in the form of short-lived hydrocarbons. These short-lived hydrocarbons, as carbonization exhaust gases, increase the reactivity of the gas, causing nitrous gases (nitrogen oxides) to combine with the exhaust gases from the carbonization reactor 100 in the calciner 140, thus reducing the nitrogen oxides.The exhaust gases from the carbonization reactor 100, which have reacted with the nitrogen oxides, follow the descending branch 141 of the calcinator 140 into the cyclone heat exchanger 160, where they leave the plant 1000 as exhaust gases A.
[0019] In Figure 2 is one to in Figure 1 The plant shown is comparable to the one for the production of cement clinker. In contrast to the plant from Figure 1 A lock 150 is arranged here between the carbonization reactor 100 and the calcinator 140, which, via a grate inside, removes the mineral components 151 remaining after carbonization, so that they do not find their way into the cement clinker Z to be sintered. REFERENCE MARK LIST
[0020] 100 Carbonization furnace 141 descending branch 110 Secondary fuel 150 sluice 120 rotary kiln 151 mineral components 121 rotary kiln inlet chamber 160 Cyclone heat exchanger 122 Slider 1000 Attachment 123 Connecting pipe rotary kiln inlet chamber - carbonization reactor A Exhaust air L Cooling air 124 Slider R Raw flour 130 clinker cooler Z Cement clinker 140 Calcinator
Claims
1. Method of operating a carbonizing furnace (100) in a plant for production of cement clinker (1000), comprising - at least one rotary kiln (120) for sintering cement clinker, - at least one clinker cooler (130) downstream of the rotary kiln (120) in the material flow and - at least one carbonizing reactor (100), in which carbonizing reactor (100) solid secondary fuels (110) are carbonized for production of carbon monoxide (CO) by the direct current method, characterized by - carbonizing of the solid secondary fuels (110) in the exhaust air from the rotary kiln (120), where - the air ratio λ has a value between λ = 0.05 and λ = 0.3, preferably a value between λ = 0.1 and λ = 0.2, and where - the air ratio λ is adjusted by mixing the low-oxygen exhaust air from the rotary kiln (120) for sintering of cement clinker with the exhaust air from the clinker cooler (130) having an atmospheric oxygen content.
2. Method of operating a carbonizing furnace according to Claim 1, characterized by - a particle size of secondary fuels (110) with an edge length of less than 500 mm in the case of planar secondary fuels (110), such as crushed boards, crushed wood pallets, bulky household waste, industrial waste or cardboard in shredded or sheet form, and / or - a particle size of secondary fuels (110) with an edge length of less than 80 mm in the case of granular particles, such as woodchips, solid organic waste, crushed industrial waste.
3. Method of operating a carbonizing furnace according to either of Claims 1 and 2, characterized by - a moisture content of the secondary fuels (110) of less than 40%, - a carbon content of the secondary fuels (110) of 5% to 80%, - a hydrogen content of the secondary fuels (110) of 1% to 15%, - a mineral residual fraction of the secondary fuels (110) of less than 70%, where the sum total of the aforementioned ingredients may be up to 100% if no other accompanying substances are present.
4. Method of operating a carbonizing furnace according to any of Claims 1 to 3, characterized by - a treatment temperature of 800°C to 1200°C, wherein the treatment temperature is adjustable by the supply of secondary fuel (110) per unit of time, wherein - in the case of an increase in temperature, the supply of secondary fuel (110) per unit of time is increased, and - in the case of a decrease in temperature, the supply of secondary fuel (110) per unit of time is reduced.
5. Method of operating a carbonizing furnace according to any of Claims 1 to 4, characterized by a dwell time of the secondary fuels (110) in the carbonizing reactor (100) of 1 min to 45 min, adjustable by a feed mechanism.
6. Method of operating a carbonizing furnace according to any of Claims 1 to 5, characterized in that the carbonizing reactor (100) is a rotary kiln with a setting angle of between 1° and 8° and has an adjustable speed of rotation.
7. Method of operating a carbonizing furnace according to any of Claims 1 to 6, characterized in that the carbonizing reactor (100) is immediately above the rotary kiln (120).
8. Method of operating a carbonizing furnace according to any of Claims 1 to 7, characterized in that the offgases from the carbonizing furnace (100) are introduced into a calciner (140) of the plant (1000) for production of cement clinker.
9. Method of operating a carbonizing furnace according to any of Claims 1 to 8, characterized in that the mineral components that remain after the secondary fuels (110) have burned to completion fall into the rotary kiln (120) through a rotary kiln inlet chamber (121).
10. Method of operating a carbonizing furnace according to any of Claims 1 to 9, characterized in that the mineral components (151) that remain after the secondary fuels (110) have burned to completion are discharged through a lock (150).