MIXER DRUM, CONCRETE MIXER AND METHOD FOR MANUFACTURING A MIXER DRUM

DE502023005354D1Active Publication Date: 2026-11-05STETTER
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
DE502023005354
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Priority Date
2022-07-12
Filing Date
2023-07-10
Publication Date
2026-11-05
Estimated Expiration
2043-07-10

AI Technical Summary

Technical Problem

Existing mixer drums for truck mixers face issues with irregular and undesirable deformations during manufacturing due to the use of harder steels with increased hardness, which are difficult to process and result in non-uniform welds, leading to wear and increased manufacturing complexity.

Method used

The mixer drum design incorporates welds that intersect the axial plane of the rotating body at an oblique angle, allowing harder steels to be used without causing deformations, by orienting the welds at specific angles relative to the rolling direction, thereby facilitating uniform deformation and reducing welds required.

Benefits of technology

This approach enables the use of harder steels for the mixer drum, reducing wear, manufacturing costs, and increasing the concrete payload capacity while maintaining uniformity and durability.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader
Need to check novelty before this filing date? Find Prior Art

Description

[0001] The invention relates to a mixer drum for a concrete mixer, in particular for a truck mixer, wherein the mixer drum is a rotating body formed by several roll-formed sheet metal blanks welded together by weld seams. The invention further relates to a concrete mixer, in particular a truck mixer, with such a mixer drum, and to a method for manufacturing a mixer drum.

[0002] Such a mixer drum is known, for example, from EP 1 950 017 B1. Here, a mixer drum with an improved mixing spiral is proposed, the mixing spiral being made of a steel with increased hardness to reduce wear. As already mentioned in EP 1 950 017 B1, such steels are difficult to process by rolling and bending. For this reason, correspondingly hard steels have not previously been used for the sheet metal blanks of the rotating body of the mixer drum, which form the drum shell and are welded together. Consequently, the drum shells of previously known mixer drums are prone to wear.In addition to the springback resulting from the increased hardness of the sheet metal blanks, the lower hardness of the welds compared to the outer material is also problematic for rolling and bending, leading to irregular and therefore undesirable deformations of the rotating body during the manufacturing process.

[0003] US 3,929,321 A discloses a mixer drum for a truck mixer, wherein the mixer drum is a body of revolution formed by several roll-formed sheet metal blanks welded together by welds, wherein at least one of the welds intersects an axial plane of the body of revolution at an oblique angle along its course, and wherein the mixer drum comprises at least two cone-shaped sections of the body of revolution.

[0004] EP 1 950 017 B1 describes a spiral segment of a mixer drum for a truck mixer that can have a hardness of up to 600 HB.

[0005] It is therefore the object of the invention to provide an improved mixer drum.

[0006] This problem is solved by a mixer drum with the features of claim 1, by a concrete mixer with the features of claim 7 and by a method according to the features of claim 8.

[0007] Because at least one of the welds intersects an axial plane of the body of revolution at an oblique angle, specifically one other than 0° or integer multiples of 90°, even harder steels, with a hardness of at least 400 HB in some areas, can be easily rolled and bent from the sheet metal blanks welded together via the weld, without causing irregular and undesirable deformations of the body of revolution. The at least one weld preferably has an elongated path that intersects a plane of a generating curve of the at least one body of revolution forming the mixer drum only at specific points. Thus, the at least one weld intersects any axial plane of the body of revolution at an oblique angle, i.e., an angle other than 0° or integer multiples of 90°, along its path between the sheet metal blanks.The axial planes of the solid of revolution are those planes in which the longitudinal axis of the solid of revolution, i.e., the axis of rotation of the mixer drum, lies. The intersection of the solid of revolution with each of the axial planes represents the generating curve of the solid of revolution.

[0008] Intersecting an axial plane of the rotating body at an oblique angle through at least one weld seam facilitates the manufacturing of the mixer drum, as less irregular and undesirable deformation of the rotating body occurs during the bending and rolling of the sheet metal blanks welded together via this weld seam. The more of the required weld seams that intersect an axial plane of the rotating body at an oblique angle along their path, the better irregular and undesirable deformations at the weld seams can be avoided during the bending and rolling of the rotating body of the mixer drum. However, the fewer weld seams required, the more uniformly the rotating body of the mixer drum can still be bent.

[0009] According to the invention, the mixer drum comprises at least two cone-shaped sections of the rotating body, wherein at least one weld connecting the sheet metal blanks of at least one of the cones intersects an axial plane of the respective rotating body section at an oblique angle along its course. The production of cones forming rotating body sections is particularly difficult with harder steels for the sheet metal blanks, as irregular and undesirable deformations are especially prone to occurring during the bending and rolling of the rotating body sections. Even with an oblique course of a weld connecting the sheet metal blanks of the cones to an axial plane of the respective rotating body section, more regularly shaped cones, especially from harder steels, can be produced for the sheet metal blanks if the weld intersects an axial plane of the rotating body only at specific points.The more of the required welds intersect an axial plane of the conical sections of the rotating body at an oblique angle along their path, the better irregular and undesirable deformations at the welds can be avoided during the bending and rolling of the rotating body sections. Conversely, the fewer welds are required overall, the more uniformly the rotating body of the mixer drum can be bent.

[0010] The skewed cutting angle ensures uniform deformation of the welded sheet metal blanks during the bending and rolling process, forming the rotating body that constitutes the mixer drum. The rotating body of the mixer drum is thus formed by the drum shell, which is itself composed of several sheet metal blanks welded together.

[0011] The inclined cutting angle is preferably greater than 4 degrees and less than 90 degrees. The inclined path of the at least one weld seam simplifies the use of harder steels for the sheet metal blanks, since the orientation of the weld seam relative to an axial plane of the rotating body results in more uniform deformation of the sheet metal blanks and the weld seam during bending and rolling of the blanks joined by the at least one weld seam. Thus, the weld seam is automatically oriented at an angle to the rolling direction selected during the bending and rolling of the rotating body.The longitudinal extent of the at least one weld should therefore lie outside a plane orthogonal to the rolling direction, so that irregular and unwanted deformations of the rotating body of the mixer drum can be easily avoided when the sheet metal blanks connected to each other via the at least one weld are deformed into the rotating body in the rolling direction by bending rolls.

[0012] Advantageous embodiments and further developments of the invention are set forth in the dependent claims. It should be noted that the features listed individually in the claims can also be combined with one another in any technologically meaningful way, thus revealing further embodiments of the invention.

[0013] A particularly preferred embodiment provides that the mixer drum comprises at least one cylindrical section of the rotating body, wherein a weld connecting the sheet metal blanks of the cylinder intersects an axial plane of the respective rotating body section at an oblique angle along its path. The production of cylinders forming sections of the rotating body is also difficult with harder steels for the sheet metal blanks, as irregular and undesirable deformations easily occur during the bending and rolling of the rotating body sections. Even with an oblique angle of intersection of the weld connecting the sheet metal blanks of the cylinders with an axial plane of the respective rotating body section, more regularly shaped cylinders, especially from harder steels for the sheet metal blanks, can be produced.The more of the required welds intersect an axial plane of the cylindrical sections of the body of revolution at an oblique angle along their course, the better irregular and undesirable deformations at the welds can be avoided during the bending and rolling of the sections of the body of revolution.

[0014] A particularly advantageous embodiment of the invention relates to at least one of the weld seams intersecting an axial plane of the rotating body and / or a rotating body section of the rotating body at an angle of at least 4 degrees, preferably at least 12 degrees, more preferably at least 14 degrees, and at most 45 degrees, preferably at most 35 degrees, more preferably at most 30 degrees, and more preferably at most 25 degrees. Such an angle of intersection allows the course of the at least one weld seam to be optimally positioned with respect to the rolling direction, thus avoiding irregular and undesirable deformations during the bending rolling of the rotating body or the rotating body sections of the rotating body.

[0015] A particularly advantageous embodiment of the invention provides that the weld seams in the development of the body of revolution and / or a section thereof have a straight course. This straight course makes it particularly easy to weld the sheet metal blanks together before bending. Thus, the sheet metal blanks can be joined together in one plane by means of the straight weld seam before bending to form the body of revolution or a section thereof.

[0016] An advantageous embodiment of the invention provides that at least two welded and roll-formed sheet metal blanks have a hardness of at least 420 HB, more preferably at least 450 HB, more preferably at least 475 HB, more preferably at least 490 HB, and more preferably at least 500 HB, at least in certain areas. These hardness values ​​for the steel of the sheet metal blanks allow for the creation of a drum shell for the mixer drum that is particularly wear-resistant. The greater the hardness, the less susceptible the mixer drum is to abrasion from the concrete transported within it, even with a comparatively thin wall and thus low weight of the mixer drum.

[0017] A particularly advantageous embodiment provides that at least two welded and roll-formed sheet metal blanks have a thickness of at most 3 mm, preferably at most 2.7 mm, at least in certain areas. The potentially higher hardness of the sheet metal blanks allows for a reduction in their thickness, as the mixer drum is subjected to less abrasion from the concrete transported within it. This results in a significant weight reduction on the mixer drum, enabling a larger concrete payload. Thanks to the increased hardness of the sheet metal blanks, the reduction in thickness does not shorten the service life of the mixer drum, as it is less susceptible to abrasion from the transported concrete.

[0018] Furthermore, the invention relates to a concrete mixer, in particular a truck mixer, as described above and below, with a mixing drum as described above and below. Particularly in truck mixers, the improved mixing drum offers the advantage of reduced manufacturing costs, low wear, and a higher concrete payload.

[0019] Furthermore, the invention relates to a method for manufacturing a mixer drum, in particular a mixer drum as described above and below in more detail, comprising the following successive steps: Cutting flat sheet metal blanks, wherein the sheet metal blanks have a hardness of at least 400 HB in at least some areas; welding the cut sheet metal blanks together via straight welds; bending and rolling the welded sheet metal blanks to form a section of a rotating body, wherein the path of at least one of the welds intersects an axial plane of the rotating body section at an oblique angle; welding the bent and rolled and welded sheet metal blanks to form the rotating body section; and joining several rotating body sections to form a mixer drum. Cutting the sheet metal for the mixer drum can be very simple, since the development of the rotating body and / or a rotating body section is formed by flat sheet metal blanks. The cut sheet metal blanks are then simply welded together via straight welds.The welded sheet metal blanks thus form a flat development of a section of a rotating body, which can easily be fed into a bending and rolling machine. During the bending and rolling process, a rotating body section is created, whereby the path of at least one of the welds, as explained above, intersects an axial plane of the rotating body section at an oblique angle. After bending and rolling, the bent and welded sheet metal blanks are welded together to form the rotating body section. This is preferably done via a straight weld seam that runs in an axial plane of the rotating body section. Such a weld seam can be easily executed on the already bent and rolled rotating body section. Subsequently, several similarly manufactured rotating body sections are joined to form a rotating body of the mixer drum.This is preferably achieved via circumferential welds between the sections of the rotating body.

[0020] An advantageous embodiment of the method involves welding an auxiliary plate to the first sheet metal blank of each rotating body section during bending and rolling. This allows the first blank to be inserted at an angle, along with the auxiliary plate, into the bending and rolling device in the rolling direction. The auxiliary plate facilitates precise insertion of the first blank into the bending and rolling device, defining a rolling direction such that the longitudinal extent of the at least one weld seam lies outside a plane orthogonal to the rolling direction. This effectively prevents irregular and undesirable deformations of the rotating mixer drum.The sheet metal blanks, joined by at least one weld, are deformed into the body of revolution by the bending and rolling process in the rolling direction. The weld lines intersect the plane perpendicular to the rolling direction at an oblique angle. The auxiliary plate facilitates the correct insertion of the welded sheet metal blanks. It can be removed after the first welded sheet metal blanks have been bent and rolled into a section of the body of revolution, before the section is welded shut.

[0021] A preferred embodiment of the method involves welding an auxiliary plate to the last sheet blank of each rotating body section inserted into a bending die during bending rolling. This serves to guide the last sheet blank obliquely out of the bending die, together with the auxiliary plate, in the rolling direction. Since the last sheet blank, inserted obliquely into the bending die, no longer rests against the starting block of the bending die, this sheet blank can no longer be reliably guided within the bending die. Without a corresponding auxiliary plate on the last sheet blank of each rotating body section inserted into the bending die, undefined deformation can occur, which can be easily and effectively avoided with the auxiliary plate.

[0022] According to a preferred embodiment of the method, at least one of the welds runs at an oblique angle to the axis of one or more rollers of the bending machine during the bending roll process. The sheet metal blanks welded together via the weld are bent by the bending machine at this oblique angle, minimizing stress on the weld. The oblique angle of the weld, which is typically softer than the sheet metal blanks, effectively prevents irregular and therefore undesirable deformations of the rotating body, as the weld, oriented obliquely to the rolling direction, is continuously and uniformly loaded and deformed by the roller(s) of the bending machine. The sheet metal blanks running obliquely alongside the weld in the rolling direction stabilize the weld, which is bent section by section along its path.This makes it very easy to compensate for differences in hardness between the sheet metal blanks and the usually softer welds, and to avoid irregular and therefore undesirable deformations of the rotating body.

[0023] Further features, details, and advantages of the invention will become apparent from the following description and from the drawings, which show exemplary embodiments of the invention. Corresponding objects or elements are provided with the same reference numerals in all figures. The figures show: Figure 1 Truck mixer according to the prior art, Figure 2 Side view of the mixer drum according to the invention, Figure 3 Front view of the mixer drum according to the invention, Figure 4 Rear view of the mixer drum according to the invention, Figure 5 Welded sheet metal blanks and roller, Figure 6 Development of a section of a rotating body, Figure 7 Further development of a section of a rotating body, Figure 8 Bending rolling device and sheet metal blank, Figure 9 Further bending rolling device and sheet metal blank, Figure 10 Further development of a section of a rotating body, and Figure 11 Detail view of the development of the section of a rotating body.

[0024] In the Figure 1Reference numeral 1 denotes a mixer drum as known from the prior art. The mixer drum 1 is rotatably mounted on the chassis 15 of a truck mixer 2 in the usual manner. With such a truck mixer 2, fresh concrete can be easily transported to a construction site for use in the construction of buildings. The mixer drum 1 of the truck mixer 2 forms a rotating body about the axis of rotation 16, about which a drive 17 of the truck mixer 2 rotates the mixer drum for mixing and emptying the concrete. The rotating body 1 is formed by several rolled sheet metal blanks 4 welded together by welds 3, which form the drum shell of the mixer drum 1. The welds 3 all run in an axial plane 5 ( Fig. 3, 4) of the rotating body 1. Thus, the welds 3 shown each extend in a plane of a generating curve of the at least one rotating body forming the mixer drum 1. If the welds 3 are oriented accordingly to the rolling direction, larger differences in hardness between the sheet blanks 4 and the usually softer welds 3 lead to irregular and therefore undesirable deformations of the rotating body 1, since the welds 3, which are oriented parallel to the rollers of the bending machine, exhibit different deformation behavior during bending than the harder sheet blanks 4.

[0025] This is where the invention comes in and proposes a solution for a truck mixer 2, as it is a Figure 1 As can be seen, a mixer drum 1 is shown, as used, for example, in Figure 2 The mixer drum 1 according to Figure 2 is characterized by the fact that one or more weld seams 3 have an axial plane 5 along their course ( Fig. 3, 4 ) of the solid of revolution 1 at an oblique angle.

[0026] This makes it very easy to roll and bend even harder steels of the sheet metal blanks 4 welded together via the weld seam 3, without irregular and undesirable deformations of the rotating body 1 occurring. The mixer drum 1 shown has three rotating body sections 6, 7, 8 designed as cones 6, 7, 8 of the rotating body 1. A rotating body section 9 designed as a cylinder 9 is arranged between the front cone 6 and the two rear cones 7 and 8, with the interconnected rotating body sections 6, 7, 8 and 9 forming the rotating body of the mixer drum 1 as its drum shell. In the embodiment of the invention shown here, at least the sheet metal blanks 4 of the first cone 6 and the second cone 7 are connected by weld seams 3, which form an axial plane 5 along their course ( Fig. 3u. 4) of the respective section of the body of revolution 6, 7 cut at an oblique angle. The sheet metal blanks 4 of the further cone 8 or the cylinder 9 can also be joined by corresponding welds which form an axial plane 5 along their course ( Fig. 3) of the respective sections of the rotating body 8, 9 intersect at an oblique angle. However, this is not the case in the illustrated embodiment. Depending on the selected hardness of the sheet metal blanks 4, the rotating body section of the cylinder 9 can still be manufactured from sheet metal blanks 4 that are joined by welds 3 oriented parallel to the rollers of the bending machine, since irregular and undesired deformations occur less frequently during the bending rolling of the cylinder 9, or only with larger differences in hardness between the sheet metal blanks 4 and the welds 3, and are easier to control during the bending rolling of the cylinder 9. In the embodiment, the third cone 8, i.e., the one adjoining the drum opening 18, is also manufactured from sheet metal blanks 4 that are joined by welds 3 oriented along the generating curve of the rotating body section 8.This is possible, for example, by selecting a lower hardness for the sheet metal blanks 4 of the cone 8 adjoining the drum opening 18 than for the sheet metal blanks 4 of the other cones 6, 7. Since the wear on the cone 8 adjoining the drum opening 18 is usually lower, sheet metal blanks 4 with a lower hardness than in the other sections of the rotating body 6, 7, 9 can be used at this point without significant disadvantages for the service life of the rest of the mixer drum 1.

[0027] This allows material costs to be kept lower without compromising the service life of the improved mixer drum 1. However, the more welds 3 required due to the raw material, the more an axial plane 5 ( Fig. 3The more the rotating body 1 is cut at an oblique angle (see u. 4), the better irregular and undesirable deformations can be avoided during the bending rolling of the rotating body of the mixer drum 1.

[0028] The Figure 3 The mixer drum 1 is shown according to Figure 2 in a front view from the direction of the rotation axis 16 ( Fig. 2 Here it can be seen that the welds 3, which connect the sheet metal blanks 4 of the first cone 6, intersect an arbitrary axial plane 5 of the body of revolution 1 at an oblique angle during their course between the sheet metal blanks 4. The axial planes 5 are those planes in which the axis of rotation 16 runs.

[0029] Also from Figure 4 , which shows a rear view of the mixer drum 1 according to Figure 2 shows, from the perspective of the rotation axis 16 ( Fig. 2) recognizable that the welds 3, which connect the sheet metal blanks 4 of the second cone 7 together, intersect an arbitrary axial plane 5 of the body of revolution 1 at an oblique angle during their course between the sheet metal blanks 4.

[0030] In Figure 5 Two sheet metal blanks 4 welded together via a weld seam 3 are shown as an example. These are used for bending and rolling a section of a rotating body 6, 7, 8, 9 ( Fig. 2 ) in the rolling direction 12 by means of a roller 14 to a bending and rolling device 10. It can be seen that the weld seam 3 is oriented obliquely along its course to the rolling direction 12 selected during the bending and rolling of the rotating body. The longitudinal extent of the weld seam 3 lies outside a plane orthogonal to the rolling direction 12. This can lead to irregular and undesirable deformations of the rotating body of the mixer drum 1 ( Fig. 2) can be easily avoided, since the sheet metal blanks 4, which are joined together via the weld 3, are deformed into the body of revolution in the rolling direction 12 by bending rollers. The weld 3, which is oriented obliquely to the rolling direction 12, is formed by the roller 14 or the rollers 14a, 14b, 14c, 14d of the bending roller device 10 ( Fig. 9 ) thus continuously stressed and deformed one after the other. The sheet metal blanks 4 running diagonally alongside the weld seam 3 in the rolling direction 12 stabilize the weld seam 3, which is continuously bent and rolled along its course, during the deformation of the sheet metal blanks 4 towards a section of the body of revolution 6, 7, 8, 9 ( Fig. 2 ). Thus, differences in hardness between the weld seam 3, the edge areas 19 of the sheet metal blanks 4 at the weld seam 3 and the remaining sheet metal blanks 4 can be reduced during the bending rolling of the mixer drum 1 ( Fig. 2) can be easily compensated. Even if the material of the welds 3 has the same hardness as the sheet metal blanks 4, the hardness in the edge areas 19 is reduced by the heating of the sheet metal during welding of the blanks.

[0031] The Figure 6 shows a development of a cone-shaped section of a body of revolution 6, 7, 8 ( Fig. 2 ) of the mixer drum 1. It can be seen that the welds 3 in the development of the rotating body section 6, 7, 8 ( Fig. 2 ) the mixer drum has a straight path. This straight path makes it possible to easily weld the flat sheet metal blanks 4 together before bending. For this purpose, the plate-shaped sheet metal blanks 4 are simply positioned butt-jointed to each other. In the Figure 6 An angle α is also shown, which indicates the inclined course of the weld seams 3, which, after bending and rolling of the welded sheet metal blanks 4, form an axial plane ( Fig. 3) of the bent-rolled rotating body of the mixer drum 1 are cut at a corresponding angle. For this purpose, the sheet metal blanks 4 are cut to size. Preferably, the weld seams 3 intersect an axial plane 5 along their course ( Fig. 3, 4 ) of the rotating body of the mixer drum 1 or of a rotating body section 6, 7, 8, 9 ( Fig. 2 ) of the rotating body 1 at an angle of at least 4 degrees and at most 45 degrees. This allows the weld seams 3 to be optimally aligned with respect to the rolling direction 12 ( Fig. 5 ) position so that irregular and undesired deformations occur during the bending roll of the rotating body 1 ( Fig. 2 ) or the sections of the body of revolution 6, 7, 8, 9 ( Fig. 2 ) of the solid of revolution are avoided. Depending on the size of the solids of revolution 6, 7, 8, 9 ( Fig. 2 ) and the bending roller device results in a minimum angle to prevent irregular and undesired deformations during the bending roller operation of the rotating body 1 ( Fig. 2) can be effectively prevented. Further explanations follow to simplify the determination of this minimum angle. After the sheets have been cut to size for the mixer drum 1 ( Fig. 2 The cut sheet metal blanks 4 can be easily welded together using straight weld seams 3. The in Figure 6 The shown flat development of the revolution body section can be easily achieved using a bending rolling device 10 ( Fig. 9 ) are supplied. The body of revolution section 6, 7, 8, 9 ( Fig. 2 ) is thus created by bending the welded sheet metal blanks 4, whereby the course of the weld seams 3 forms an axial plane 5 ( Fig. 3, 4 ) of the body of revolution section 6, 7, 8, 9 ( Fig. 2 ) cuts at the oblique angle α. Subsequently, the bent and welded sheet metal blanks 4 are added to the section of the body of revolution 6, 7, 8, 9 ( Fig. 2) welded together. To manufacture the mixer drum 1, several correspondingly manufactured sections of rotating body 6, 7, 8, 9 ( Fig. 2 ) to form a body of revolution 1. This is preferably done via circumferentially extending welds between the body of revolution sections 6, 7, 8, 9 ( Fig. 2 ), which in Figure 2 can be recognized. From the Figure 6 Auxiliary plates 11 are also visible, which are attached to the bending rolling device 10 before bending rolling ( Fig. 8 ) the inserted sheet metal blanks 4 are attached. The first sheet metal blank 4 can be very easily attached at an angle together with the auxiliary sheet 11 in the rolling direction 12 via this auxiliary sheet 11 ( Fig. 8 ) into the bending roller device 10 ( Fig. 8 ) are introduced. This makes it particularly easy to ensure that the welds 4 are aligned with an axis 13 of one or more rollers 14, 14a, 14b, 14c, 14d of the bending rolling device 10 during bending rolling ( Fig. 9) run at an oblique angle (α). In this embodiment, the auxiliary plate 11 is formed in the shape of a triangle and can preferably consist of offcuts from the sheet metal blanks 4.

[0032] Out of Figure 7 A further unfolding of a cone-shaped section of revolution 6, 7, 8 ( Fig. 2 ) of the mixer drum 1. This development differs from the one in Figure 6 The development shown is due to the fact that the paths of the weld seams 3 between the sheet metal blanks 4 are not uniform to the rolling direction 12 ( Fig. 5 ) are oriented obliquely, but alternately with a positive and a negative angle α to the rolling direction 12 ( Fig. 5 The positive and negative angles α do not have to be equal. The sheet metal blanks 4 are cut accordingly. Furthermore, the auxiliary sheet metal 11 is not triangular, but preferably rectangular.

[0033] The Figure 8 schematically shows a bending rolling device 10 with three rollers for bending the rotating body sections 6, 7, 8, 9 ( Fig. 2 ) of the mixer drum 1 ( Fig. 2 ) and a sheet metal blank 4, which is fed to the bending rolling device 10. The deformation process during the bending rolling of the welded sheet metal blanks 4 is mainly carried out by three rollers of the bending rolling device 10, which form a feed roller 14a, an upper roller 14b and a lower roller 14c.

[0034] In Figure 9 is another schematic bending rolling device 10 with four rollers 14a, 14b, 14c, 14d for bending rolling the sections of the rotating bodies 6, 7, 8, 9 ( Fig. 2 ) the mixer drum 1 and a sheet metal blank, which is fed to the bending rolling device 10. The bending rolling process begins with the initial bending. Here, the feed roller 14a is initially positioned, as shown in Figure 9As can be seen below. The discharge roller 14d is moved upwards and the sheet blank 4 is inserted between the upper roller 14b and the lower roller 14c until it reaches the discharge roller 14d. During the bending roll forming of a cone 6, 7, 8 ( Fig. 2 ) should be a generatrix I ( Fig. 11 ) against the discharge roller 14d. This "precedence" is necessary to ensure the correct alignment of the welded sheet metal blanks 4. If the first sheet metal blank 4 has an angled cut, an alternative contact point must be provided. The previously mentioned auxiliary plate 11 ( Fig. 6 or 7 ) are used. An extension in the form of an auxiliary plate 11 is also used on the outlet side of the sheet metal blanks 4 ( Fig. 6 and 7This is advantageous because the sheet metal is no longer in contact with the starting block of the bending machine 10 and is therefore no longer guided within the bending machine 10. This easily prevents undefined deformation. The sheet metal blank 4 is retracted for bending until it is just barely resting on the lower roller 14c ( Fig. 8 ). The actual bending process then follows. In this process, the first sheet metal blank 4 is initially clamped between the upper roller 14b and the lower roller 14c with the feed roller 14a in the lower position, as shown in Figure 9 as can be seen. Subsequently, the feed roller 14a is used, as shown in Figure 8 shown, ramped up. The area of ​​the sheet metal blank 4 between points P2 and P3 ( Fig. 8) remains undeformed – a straight piece is obtained here. The actual deformation process takes place between point P1 and point P2, where P2 marks the contact point of the sheet blank 4 on the upper roll 14b. However, the exact position of point P2 is not known. Since the feed roll 14a is used during the bending roll of a cone 6, 7, 8 ( Fig. 2 Since the rollers are inclined, the distance d between points P1 and P2 or P3 cannot be precisely determined, or rather, it varies across the entire width of the rollers 14, 14a, 14b, 14c in the bending roller device 10. In order to determine which oblique angle α ( Fig. 6 , 7 , 10 , 11 ) for the course of the weld seams 3 is at least required to avoid irregular deformations during bending rolling, the projected length p ( Fig. 10 ) of the welds 3 ( Fig. 10) can be determined. For this purpose, one can start from the geometric conditions when inserting the sheet metal blank 4 into the bending rolling device 10. The feed roller 14a and the lower roller 14c are, as in Figure 9 as seen, at the same height and the distance between the lower roller 14c and the feed roller 14a is very small. Preferably, the distance between the feed roller 14a and the lower roller 14c is at most 10 mm. The simplified view yields a projection length p, which is in any case greater than the distance between points P1 and P3 ( Fig. 8 In the simplified view for determining the minimum angle α, the contact point between the feed roller 14a and the sheet blank 4 lies at 12 o'clock and during the actual rolling process (see Figure 8) clearly to the right of 12 o'clock, which in this case results in a shorter projection line. Thus, a minimum angle α is obtained for the intended course of the welds 3 connecting the sheet metal blanks 4. α = acrtan p L ä nge l der Mantellinie Konus

[0035] This also refers to the detailed view according to Figure 11 referenced, which shows the length l of the generatrix of the cone, which results from the appropriate sheet metal cutouts.

[0036] In Figure 10 is also a further development of a cone-shaped section of revolution 6, 7, 8 ( Fig. 2 ) of the mixer drum 1 is shown. In this development, the bent and welded sheet metal blanks are welded to the rotating body section 6, 7, 8 ( Fig. 2 ) via a straight weld seam that lies in an axial plane (5 ( Fig. 3, 4 ) of the body of revolution section 6, 7, 8 ( Fig. 2) runs. This eliminates the need for auxiliary plates and such a weld seam can be made on the bend-rolled section of the rotating body 6, 7, 8 ( Fig. 2 ) easier to execute than a weld seam running diagonally along the drum shell to close the rotating body section 6, 7, 8 ( Fig. 2 ). Reference list

[0037] 1 Mixer drum (rotating body) 2 Truck mixer 3 Welds 4 Sheet metal blanks 5 Axial plane 6 First cone (first rotating body section) 7 Second cone (second rotating body section) 8 Third cone (third rotating body section) 9 Cylinder (fourth rotating body section) 10 Bending rolling device 11 Auxiliary sheet 12 Rolling direction 13 Axis 14 Roll, 14a Infeed roll, 14b Top roll, 14c Bottom roll, 14d Outfeed roll 15 Chassis 16 Rotation axis 17 Drive 18 Drum opening 19 Edge area α Oblique angle d Distance P1 - P2 p Projection length l Length of the generatrix (cone) D Sheet thickness

Claims

1. A mixer drum (1) for a concrete mixer, in particular for a truck mixer (2), wherein the mixer drum (1) is a body of revolution formed by a plurality of roll-bent sheet-metal blanks (4) welded to one another via weld seams (3), wherein at least one of the weld seams (3), along its course, intersects an axial plane (5) of the body of revolution (1) at an oblique angle (α), wherein the mixer drum (1) comprises at least two body-of-revolution sections (6, 7, 8) of the body of revolution (1) configured as cones (6, 7, 8), characterised in that at least two sheet-metal blanks (4) welded to one another and roll-bent have, at least in regions, a hardness of at least 400 HB, wherein at least one weld seam (3) connecting the sheet-metal blanks (4) of at least one of the cones (6, 7, 8), along its course, intersects an axial plane (5) of the respective body-of-revolution section (6, 7, 8) at an oblique angle (α).

2. The mixer drum (1) according to claim 1, characterised in that the mixer drum (1) comprises at least one body-of-revolution section (9) configured as a cylinder (9), wherein a weld seam (3) connecting the sheet-metal blanks (4) of the cylinder (9), along its course, intersects an axial plane (5) of the respective body-of-revolution section (9) at an oblique angle (α).

3. The mixer drum (1) according to any one of the preceding claims, characterised in that at least one of the weld seams (3), along its course, intersects an axial plane (5) of the body of revolution (1) and / or of a body-of-revolution section (6, 7, 8, 9) of the body of revolution at an oblique angle of at least 4 degrees and at most 45 degrees.

4. The mixer drum (1) according to any one of the preceding claims, characterised in that the weld seams (3), in the development of the body of revolution (1) and / or of a body-of-revolution section (6, 7, 8, 9) of the body of revolution, have a rectilinear course.

5. The mixer drum (1) according to any one of the preceding claims, characterised in that at least two sheet-metal blanks (4) welded to one another and roll-bent have, at least in regions, a hardness of at least 420 HB, more preferably at least 450 HB, more preferably at least 475 HB, more preferably at least 490 HB, more preferably at least 500 HB.

6. The mixer drum (1) according to any one of the preceding claims, characterised in that at least two sheet-metal blanks (4) welded to one another and roll-bent have, at least in regions, a thickness (D) of at most 3 mm, preferably at most 2.7 mm.

7. A concrete mixer, in particular a truck mixer (2), having a mixer drum (1) according to any one of the preceding claims.

8. A method for producing a mixer drum (1), in particular a mixer drum (1) according to any one of the preceding claims 1 to 6, comprising the following successive steps: - cutting flat sheet-metal blanks (4), - characterised in that - the sheet-metal blanks (4) have, at least in regions, a hardness of at least 400 HB, - welding the cut sheet-metal blanks (4) to one another via weld seams (3) extending in straight lines, - roll-bending the welded sheet-metal blanks (4) into a body-of-revolution section (6, 7, 8, 9), wherein the course of at least one of the weld seams (3) intersects an axial plane (5) of the body-of-revolution section (6, 7, 8, 9) at an oblique angle (α), - welding the roll-bent and welded sheet-metal blanks (4) closed to form the body-of-revolution section (6, 7, 8, 9), and - joining a plurality of body-of-revolution sections (6, 7, 8, 9) to form a mixer drum (1).

9. The method according to claim 8, characterised in that, during roll-bending, an auxiliary sheet-metal piece (11) is welded to a first sheet-metal blank (4) of each body-of-revolution section (6, 7, 8, 9), said first sheet-metal blank being introduced into a roll-bending device (10), in order to introduce the first sheet-metal blank (4) obliquely and together with the auxiliary sheet-metal piece (11), in the rolling direction (12), into the roll-bending device (10).

10. The method according to claim 8 or 9, characterised in that, during roll-bending, an auxiliary sheet-metal piece (11) is welded to a last sheet-metal blank (4) of each body-of-revolution section (6, 7, 8, 9), said last sheet-metal blank being introduced into a roll-bending device (10), in order to guide the last sheet-metal blank (4) obliquely and together with the auxiliary sheet-metal piece (11), in the rolling direction (12), out of the roll-bending device (10).

11. The method according to any one of claims 8 to 10, characterised in that, during roll-bending, at least one of the weld seams (4) extends at an oblique angle (α) relative to an axis (13) of one or more rollers (14, 14a, 14b, 14c, 14d) of the roll-bending device (10).