Polyamide compositions

ES2625006T5Active Publication Date: 2026-11-18ENVALIOR DEUTSCHLAND GMBH (100 00)
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
ES2015156682T
Authority / Receiving Office
ES · ES
Patent Type
Patents
Current Assignee / Owner
Priority Date
2014-03-26
Filing Date
2015-02-26
Publication Date
2026-11-18
Estimated Expiration
2035-02-26

AI Technical Summary

Technical Problem

Existing polyamide-based compositions for electrical components, such as FI switches and line protection switches, face challenges with poor thermoforming stability and anisotropic shrinkage, leading to deformation and inadequate self-extinguishing properties, particularly in thin wall thicknesses, due to the use of fiber-shaped fillers and halogen- or phosphorus-based flame retardants.

Method used

A composition comprising polyamide 6 or 66, non-fiber-shaped non-foamed ground glass, long chopped glass fibers, and melamine cyanurate, optimized for isotropic shrinkage and improved self-extinguishing properties, using additives like melamine cyanurate and silane-treated glass fibers to enhance thermoforming stability and flame resistance.

Benefits of technology

The composition achieves high thermoforming stability with low isotropic shrinkage and excellent self-extinguishing properties in the glow-wire test, even in thin wall thicknesses, ensuring reliable performance in electrical components.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

Compositions that contain A) polyamide 6 or polyamide 66, B) non-fiber-shaped and non-foamed ground glass with a d90 determined by laser diffractometry in the range of 5 to 250 mm, and a length in the range of 0.01 to 0.5 mm, C) long glass fibers cut with a starting length in the range of 1 to 50 mm, and D) melamine cyanurate.
Need to check novelty before this filing date? Find Prior Art

Description

Polyamide compositions The present invention relates to compositions containing polyamide 6 or polyamide 66, non-fiber and non-foamed ground glass, long fibers, and melamine cyanurate, as well as to the preparation and use of the compositions for the manufacture of products for the electrical industry, preferably electrical construction parts, especially preferably for the manufacture of FI switches and line protection switches. State of the art To modify their behavior during processing, transformation, and use, most plastics are treated with additives, fillers, and reinforcing agents. These latter substances improve properties such as stiffness, strength, thermal stability, and dimensional stability, and reduce the thermal expansion of plastic-based products. Mineral or glass fillers and reinforcing agents, particularly borosilicate or silicate glass, which are used in a wide variety of forms, are especially important for plastic compositions. These fillers and reinforcing agents have a significant influence on the thermoforming stability of plastics. For example, using fiber-based fillers with a correspondingly high length-to-diameter ratio results in very good thermoforming stability. However, the anisotropic geometry of a fiber leads to fiber alignment in the flow direction during processing, accompanied by anisotropic shrinkage, which consequently results in undesirable deformation of the finished product.Furthermore, the "wicking effect" associated with fibers leads to a deterioration of the self-extinguishing properties of these products, which are important, for example, in the glow wire test according to IEC 60695-2-12 (GWFI). To ensure sufficient flame resistance in plastic-based products, even with fiber-like fillers such as glass fibers, halogen or phosphorus-based flame retardants should generally be used. Halogen-based flame retardants are the subject of public debate due to their potential for environmental accumulation. Phosphorus-based flame retardants are frequently avoided because their preparation requires energy. Additionally, phosphorus-containing flame retardants pose a risk of corrosive deposits on electrical contacts, particularly in the case of electrical or electronic components. With the use of non-fiber fillers, in particular talc, clay minerals, mica, expanding or foaming glass, although isotropic shrinkage is obtained in products, these moldable masses and the products to be manufactured from them frequently exhibit insufficient thermoforming stability (<130 °C) or insufficient self-extinguishing properties in the GWFI test in the case of thinner wall thicknesses, in particular wall thicknesses < 1 mm. Document EP 1762592 A1 describes polymeric moldable masses based on thermoplastic polyamides and a phosphinic acid salt and / or a diphosphinic acid salt and / or their polymers. Document CN 103013104 A discloses nylon-6 compositions with halogen-free flame retardants, based on 53-70 parts by weight of nylon-6 resin, 7-15 parts by weight of melamine cyanurate, 20-30 parts by weight of an inorganic filler, 0-5 parts by weight of a flame protection synergist, and 1-5 parts by weight of a processing aid. Document EP 2468810 A1, example 3, describes a polyamide-based composition that, in addition to melamine cyanurate, contains ground glass and ground chopped glass fibers. According to EP 2468810 A1, this composition is disadvantageous due to its poor stability during thermoforming, resulting in very limited applicability in electrical components, such as line protection switches. Now, however, good thermoforming stability in the case of simultaneously isotropic shrinkage behavior and good self-extinguishing properties in the GWFI test is an important prerequisite for the application of polyamide-based compositions in complexly constructed electronic building parts, particularly in FI switches and line protection switches (FI = fault current protection switch). According to "http: / / de.wikipedia.org / wiki / Leitungsschutzschalter", a line protection switch, abbreviated LS switch, also colloquially called an automatic fuse or simply a fuse, is a device that protects against overcurrent in electrical installations and is used in low-voltage networks. The term FI switch refers to a fault current protection switch (see http: / / de.wikipedia.org / wiki / Fehlerstromschutzschalter). Therefore, the objective of the present invention was to provide polyamide-based compositions for use in FI circuit breakers and line protection switches, characterized by high thermoforming stability. with at the same time low isotropic shrinkage behavior and good self-extinguishing properties in the glow filament test according to IEC60695-2-12 also in the case of thin wall thicknesses, in particular in the case of wall thicknesses around 0.8 mm. According to "http: / / de.wikipedia.org / wiki / W%C3%A4rmeformbest%C3%A4ndigkeit", thermoforming stability is a measure of the temperature load-bearing capacity of plastics. Due to their viscoelastic behavior, there is no strictly defined upper service temperature for plastics; instead, a substitute quantity with a defined load is determined. Two standardized procedures are available for this purpose: the Thermoforming Stability Temperature (HDT) procedure and the Vicat Softening Temperature (VST) procedure. The procedure described in DIN EN ISO 75-1,-2,-3 (precursor: DIN 53461) for temperature stability in thermoforming uses standard test specimens with a rectangular cross-section, which are preferably subjected in a flat position to three-point bending with a constant load. Depending on the height of the specimen, a force is applied using weights and / or springs to obtain a so-called edge fiber stress Sf of 1.80 (procedure A), 0.45 (procedure B), or 8.00 N / mm² (procedure C). 2fff bh2 3 L b: sample width h: sample height L: distance from the support. The samples are then subjected to heating at a constant rate of 120 K / h (or 50 K / h). If, in this respect, the flexural strength of the sample reaches an elongation of the edge fiber of 0.2%, then the corresponding temperature is the heat deflection temperature (HDT) for thermoforming stability. The Vicat softening temperature (VST) according to DIN EN ISO 306 (predecessor: DIN 53460) is measured using a needle (with a round surface area of ​​1 mm²). This needle is loaded with a test force of 10 N (test force A) or 50 N (test force B). The test specimen, with a permissible thickness of 3 to 6.4 mm, is subjected to a defined heating rate of 50 or 120 K / h. The VST is reached when the penetrant achieves a penetration depth of 1 mm. According to the standard, the test can only be used for thermoplastics and provides information about the practical limit for continuous use, which is approximately 15 K below the Vicat temperature. By varying the boundary conditions, four parameter combinations result: VST / A50 VST / A120 VST / B50 (preferred procedure for comparative testing (ISO 10350-1) VST / B120. According to "http: / / de.wikipedia.org / wiki / Schwindung#Schwindung_bei_Gie.C3.9Fharzen," shrinkage is the change in volume of a material or workpiece without material removal or pressure being applied. Shrinkage occurs through drying, cooling, or chemical or physical reconstruction mechanisms within the material. Low shrinkage in thermoplastic-based molding resins is a quality criterion, as otherwise, modules with compressive strength may be introduced, and cracks may form in other areas that will become damp if adhesion is insufficient. In injection-molded products for electrical / electronic applications, shrinkage can lead to moisture ingress and reduced tensile strength. Isotropic shrinkage, as defined by experts, is shrinkage that is equal in all spatial directions.The shrinkage behavior test is performed in accordance with DIN EN ISO 294-4, as well as in the context of the present invention. It has now been surprisingly found that compositions based on PA 6 or PA 66, using ground glass not in fiber form and not foamed, as described in more detail below, in combination with long fibers and melamine cyanurate, lead to electrical or electronic articles with excellent properties with respect to the stability to thermoforming, resistance to ignition in the glow filament test according to IEC60695-2-12 and isotropic shrinkage behavior. Invention The invention involves compositions containing A) polyamide 6 or polyamide 66, B) non-fiber-formed, non-foamed ground glass with a d90 determined by laser diffractometry in the range of 5 to 250 mm, preferably in the range of 10 to 150 mm, especially preferably in the range of 15 to 80 mm, most preferably in the range of 16 to 25 mm, and a length in the range of 0.01 to 0.5 mm, C) long glass fibers cut to a starting length in the range of 1 to 50 mm, especially preferably in the range of 1 to 10 mm, and most preferably in the range of 2 to 7 mm, and D) melamine cyanurate. For clarification, it is added that the context of the present invention includes all the definitions and parameters set forth below, mentioned in general or in preferred ranges in discretionary combinations. The preferred subject of the invention is compositions containing A) from 5% to 92.9% by weight, preferably from 20% to 90% by weight, most preferably from 30% to 80% by weight of polyamide 6 or polyamide 66, B) from 5% to 80% by weight, preferably from 10% to 60% by weight, especially preferably from 15% to 50% by weight of a non-fiber-formed, non-foamed ground glass with a d90 determined by laser diffractometry in the range of 5 to 250 mm, preferably in the range of 10 to 150 mm, especially preferably in the range of 15 to 80 mm, most preferably in the range of 16 to 25 mm, and a length in the range of 0.01 to 0.5 mm, C) from 2% to 8% by weight, preferably from 3% to 7% by weight, most preferably from 4% to 6% by weight of long cut glass fibers with a starting length in the range of 1 to 50 mm, most preferably in the range of 1 to 10 mm, most preferably in the range of 2 to 7 mm, and D) from 0.1% to 40% by weight, preferably from 1% to 20% by weight of melamine cyanurate, on the condition that the sum of all the weight percentages always equals 100. The preparation of the compositions according to the invention for other uses is carried out by mixing the components A) to D), which are to be used as starting materials, in at least one mixing tool. This yields moldable masses as intermediate products based on the compositions according to the invention. These moldable masses may consist either exclusively of components A) to D), or they may also contain other components in addition to components A) to D). In this case, the quantities of components A) to D) may vary within the specified ranges, such that the sum of all the percentages by weight always equals 100%. Therefore, the invention also relates to moldable masses according to the invention intended for use in extrusion, blow molding or injection molding, preferably in granulated form, containing the compositions according to the invention, which constitute from 95% to 100% by weight, preferably from 98% to 100% by weight, and especially preferably from 99% to 100% by weight of the moldable masses according to the invention or to be used according to the invention for the manufacture of products in the electrical industry. Particle size determination in the context of the present invention is performed by laser diffractometry in accordance with ISO 13320. Indications of particle size distribution or particle sizes refer to so-called surface-based particle sizes, in each case prior to incorporation into the thermoplastic moldable mass. Regarding laser diffractometry, see C.M. Keck, Moderne Pharmazeutische Technologie 2009, Freie Universität Berlin, Chapter 3.1, or QuAnTACHROME PARTIKELWELT NO. 6, June 2007, pages 1 to 16. Preferred embodiments of the invention In a preferred embodiment, the non-fiber-formed, non-foamed ground glass is bonded with B') at least one aminoalkyltrialkoxysilane, preferably in quantities from 0.01% by weight to 1.5% by weight with respect to the amount of ground glass not in fiber form and not foamed. In one embodiment, the compositions contain, in addition to components A), B), C) and D) or A), B), B'), C), D) also E), from 0.01% to 5% by weight, most preferably from 0.05% to 3% by weight, particularly preferably from 0.1% to 2% by weight, in each case with respect to the total composition, at least one slip and / or release agent, the other components being reduced until the sum of all the percentages by weight is always 100. In one embodiment, the compositions contain, in addition to components A) to E) or instead of E) also F), from 0.01% to 10% by weight, preferably from 0.1% to 5% by weight, and especially preferably from 0.5% to 3.5% by weight, in each case with respect to the total composition, at least one laser absorber, preferably selected from the group of antimony trioxide, tin oxide, tin orthophosphate, barium titanate, aluminum oxide, copper hydroxyphosphate, copper orthophosphate, copper potassium diphosphate, copper hydroxide, antimony tin oxide, bismuth trioxide and anthraquinone, the other components being reduced so that the sum of all the percentages by weight always results in 100. In one embodiment, the compositions contain, in addition to components A) to F) or instead of E) and / or F) also G), from 0.01% to 60% by weight, preferably from 1% to 30% by weight, especially preferably from 5% to 25% by weight, most preferably from 0.01% to 60% by weight, in each case with respect to the total composition, at least one other flame retardant other than melamine cyanurate (= component D)), the other components being reduced until the sum of all the percentages by weight is always 100. According to the invention, halogen-free and / or phosphorus-free flame retardants are preferably used. In another embodiment, the compositions contain, in addition to components A) to G) or instead of E) and / or F) and / or G), also component H) from 0.01% to 50% by weight, preferably from 1% to 30% by weight, most preferably from 2% to 15% by weight, and in particular most preferably from 2% to 6% by weight, in each case with respect to the total composition, at least a different loading from components B) and C), the other components being reduced until the sum of all the percentages by weight is always 100. In one embodiment, the compositions contain, in addition to components A) to H) or instead of components E) and / or F) and / or G) and / or H) also K), from 0.01% to 20% by weight, preferably from 0.05% to 10% by weight, most preferably from 0.1% to 5% by weight, in each case with respect to the total composition, at least one other additive other than components D) to H), the other components being reduced until the sum of all the percentages by weight is always 100. Component A) As component A) they contain compositions PA 6 or PA 66. Copolyamides based on PA 6 and / or PA 66 are jointly comprised by the object of the present invention. The characterization of the polyamides used in the context of this application corresponds to the international standard, with the first digit(s) indicating the number of C atoms of the starting diamine and the last digit(s) indicating the number of C atoms of the dicarboxylic acid. If only one number is indicated, as in the case of PA 6, then this means that the starting material is an α,δ-aminocarboxylic acid or the lactam derived from it; in the case of PA 6, therefore, ε-caprolactam. For further information, see H. Domininghaus, Die Kunststoffe und ihre Eigenschaften, pages 272 et seq., VDI-Verlag, 1976. Preferably, the polyamide 6 or polyamide 66 to be used as component A) has a viscosity index determined in a 0.5% by weight solution in 96% by weight sulfuric acid at 25°C according to ISO 307 in the range of 80 to 180 ml / g. Polyamide 6, which is to be used as component A), according to the aforementioned standard and procedure, has a viscosity index in the range of 85 to 160 ml / g, and most preferably a viscosity index in the range of 90 to 140 ml / g. The polyamide 66 to be used as component A) has, according to the procedure mentioned above, preferably a viscosity index in the range of 110 to 170 ml / g, and most preferably a viscosity index in the range of 130 to 160 ml / g. According to Hans Domininghaus in "Die Kunststoffe und ihre Eigenschaften", 5th edition (1998), p. 14, thermoplastic polyamides are understood to be polyamides whose molecular chains do not have or have side branches that are also more or less long and different in number, which soften in heat and can be molded almost at will. The preferred polyamides according to the invention can be prepared by various methods and synthesized from very different modules. For specific applications, they can be combined with processing aids, stabilizers, or polymer alloys, preferably elastomers, to produce materials with specially tailored combinations of properties. Combinations with proportions of other polymers, preferably polyethylene, polypropylene, or ABS, are also suitable, and one or more compatibilizers may be used. The properties of the polyamides can be enhanced by the addition of elastomers, for example, with regard to impact resistance. The wide range of possible combinations allows for a very large number of products with diverse properties. A plurality of procedural modes have been known for the preparation of polyamides, in which, depending on the desired final product, different monomer modules are used, various chain regulating agents for the adjustment of a desired molecular weight, or also monomers with reactive groups for further treatments planned later. The technically relevant processes for the preparation of polyamides mostly involve polycondensation in the melt. In the context of the present invention, the hydrolytic polymerization of lactams is also understood as polycondensation. In the case of PA 6 and PA 66, which will be used as component A), these are partially crystalline polyamides. According to document DE 10 2011 084 519 A1, partially crystalline polyamides have an enthalpy of fusion in the range of 4 to 25 J / g, measured by the DSC procedure according to ISO 11357 during the second heating and integration of the melting peak. In contrast, amorphous polyamides have an enthalpy of fusion of less than 4 J / g, measured by the DSC procedure according to ISO 11357 during the second heating and integration of the melting peak. The polyamides or copolyamides that will preferably be used as component A) according to the invention are those prepared from diamines and dicarboxylic acids and / or lactams with at least five ring members or corresponding amino acids.The starting materials are preferably aliphatic dicarboxylic acids, especially adipic acid, aliphatic diamines, especially hexamethylenediamine, aminocarboxylic acids, in particular aminocapronic acid, or the corresponding lactams. Copolyamides of several of the aforementioned monomers are also included. The polyamide 6, which is to be used preferably as component A), can be obtained from ε-caprolactam. The polyamide 6, which is to be used preferably as component A), can be obtained from hexamethylenediamine and adipic acid. Composite materials are also preferred, which are based in most cases on PA 6, PA 66 or their copolyamides, in which one polyamide group in the polymer chain corresponds to 3 to 11 methylene groups, particularly and very preferably 4-6 methylene groups. Component B) As component B), the compositions contain non-fibrous and non-foamed ground glass with a particle size distribution having a d90 in the range of 5 to 250 pm, preferably in the range of 10 to 150 pm, most preferably in the range of 15 to 80 pm, and most preferably in the range of 16 to 25 pm, and a length in the range of 0.01 to 0.5 mm. Accordingly, non-fibrous and non-foamed ground glass is preferably used, which further has a d10 in the range of 0.3 to 10 pm, preferably in the range of 0.5 to 6 pm, and most preferably in the range of 0.7 to 3 pm. In this respect, ground glass that is not in the form of fiber and not foamed is highly preferred, and it also has a d50 in the range of 3 to 50 pm, preferably in the range of 4 to 40 pm, and especially preferably in the range of 5 to 30 pm. In addition to the bibliography cited above, reference is made with respect to the d10, d50 and d90 values, their determination and their importance also to Chemie Ingenieur Technik (72) pp. 273-276, 3 / 2000, Wiley-VCH Verlags GmbH, Weinheim, 2000, according to which the d10 value is that particle size below which 10% of the number of particles is found, the d50 value is that particle size below which 50% of the number of particles is found (median) and the d90 value is that particle size below which 90% of the number of particles is found. The particle size distribution or particle sizes referred to here are the so-called surface-based particle sizes, in each case before introduction into the thermoplastic moldable mass. This relates the surface diameters of the respective glass particles to the surface diameters of imaginary spherical particles (spheres). This is preferably done using a particle size analyzer that operates on the laser obscuration principle from Ankersmid (EyeTech® with the included EyeTech® software and ACM-104 measuring cell, Ankersmid Lab, Oosterhout, The Netherlands). Alternatively, the particle size distribution can also be determined by laser diffractometry, as described in the literature cited above.For this purpose, the glass to be used according to the invention is suspended in a 0.1% aqueous solution of sodium polyphosphate and then measured by laser diffractometry with a particle size analyzer of the type LS 13320 from Beckman Coulter GmbH, Krefeld, Germany. Preferably, the non-fiber and non-foamed ground glass is particle-shaped, non-cylindrical, and has a length-to-thickness ratio of less than 5, preferably less than 3, and most preferably less than 2. Logically, the value zero is included. For the purposes of this invention, foamed glass, often also called expanded glass, is understood to be glass in which gas vesicles, for example of air or carbon dioxide, are included. This gas inclusion, however, unlike the non-foamed glass to be used according to the invention, leads to a reduction in density. The non-fiber-formed, non-foamed ground glass to be used according to the invention therefore does not experience any reduction in density due to possible gas inclusions. For the purposes of the present invention, fiberglass is understood to mean a vitreous geometry with a cylindrical or oval cross-section having a length-to-diameter ratio (L / D ratio) greater than 5. The non-foamed, non-fiberglass ground glass to be used as component B) is therefore further characterized in that it does not have the typical vitreous geometry for fiberglass with a cylindrical or oval cross-section having a length-to-diameter ratio (L / D ratio) greater than 5. The non-foamed, non-fiber ground glass to be used according to the invention is preferably obtained by grinding glass with a mill, preferably a ball mill, and most preferably with subsequent separation or sieving. All geometric shapes of solidified glass are considered as starting material. The preferred starting materials for milling to obtain non-fiber, non-foamed ground glass for use according to the invention are also glass waste, as produced particularly in the manufacture of glass products as an unwanted byproduct and / or as a main product not conforming to specification (so-called Offspec-Ware). This includes, in particular, waste glass, recycled glass, and glass fragments, such as may be produced in the manufacture of window glass or bottle glass, as well as in the preparation of glass-containing fillers and reinforcing substances, particularly in the form of so-called melt cakes. The glass may be colored, although uncolored glass is preferred as a starting material. As starting glass for grinding, all types of glass as described, for example, in DIN 1259-1 are considered in principle. Lime-bicarbonate glass, float glass, quartz glass, lead glass, borosilicate glass, glass A, and glass E are preferred, with lime-bicarbonate glass, borosilicate glass, glass A, and glass E being particularly preferred, especially glass A and glass E. For physical data and composition of glass E, please refer to "http: / / wiki.r-g.de / index.php?title=Glasfasern". The non-fiber-formed, non-foamed ground glass E, which is to be used in accordance with the invention, is characterized by at least one of the features mentioned in Table 1 below: Table 1 E-glass properties Unit E-glass density g / cm2 at 20 °C 2.6 tensile strength MPa 3400 tensile modulus GPa elongation at break % 3.5-4 Chemical composition Unit Value SiO2 % 53-55 Al2O3 % 14-15 B2O3 % 6-8 CaO % 17-22 MgO % <5 K2O, Na2O % <1 other oxides % approx. 1 Similarly, for the preparation of the non-foamed, non-fiber glass to be used according to the invention, glass types in which the K₂O content is less than or equal to 2% by weight with respect to all glass components are particularly preferred. The non-foamed, non-fiber ground glass to be used according to the invention can be purchased, for example, from Vitro Minerals Inc., Covington, GA, USA. It is offered as CS Glass Powder in specifications CS-325, CS-500, and CS-600, or also as LA400 (see also www.glassfillers.com or Chris DeArmitt, Additives Feature, Mineral Fillers, COMPOUNDING WORLD, February 2011, pages 28-38 or www.compoundingworld.com). Vitro Minerals Inc. offers these glasses under CAS No. 65997-17-3 as glass oxide. Component B) preferably has a density (not apparent density!) according to ASTM C 693 in the range of 2400 to 2700 kg / m³, most preferably in the range of 2400 to 2600 kg / m³, and is thereby clearly distinct from foamed glass (density = 100–165 kg / m³), foamed glass granules (density = 130–170 kg / m³), and expanded glass (density = 110–360 kg / m³), see also AGY product brochure pub. no. LIT-2006-111 R2 (02 / 06). According to the invention, the non-foamed, non-fiber-formed ground glass to be used is provided with a surface modification or finish (component B') based on aminoalkyltryalkoxysilane.In alternative or preferred embodiments, the non-foamed and non-fiber-formed ground glass may be provided with additional surface modification or finishing based on silane or siloxane, preferably with glycidyl, carboxyl, alkenyl, acryloxyalkyl and / or methacryloxyalkyl functionalized trialkoxysilanes or their aqueous hydrolysates as well as combinations thereof. Surface modifications with aminoalkyltrialkoxysilanes are highly preferred as B'), in particular aminopropyltrimethoxysilane, aminobutyltrimethoxysilane, aminopropyltriethoxysilane, aminobutyltriethoxysilane or their aqueous hydrolysates, with aminopropyltriethoxysilane being particularly preferred. The aminoalkyltrialkoxysilanes of component B') are preferably used in amounts of 0.01% by weight to 1.5% by weight, especially preferably in amounts of 0.05% by weight to 1.0% by weight and most especially preferably in amounts of 0.1% by weight to 0.5% by weight, with respect to non-foamed and non-fiber ground glass B) for surface coating. The starting glass for grinding may already have been treated with a surface modification or finish. Similarly, the non-foamed, non-fiber ground glass to be used according to the invention may be treated after grinding with a surface modification or finish. In particular, MF7900 from Lanxess Deutschland GmbH, Cologne, can be used, a non-fiber-formed, non-foamed E-glass-based ground glass containing approximately 0.1% by weight with a d90 of 54 pm, a d50 of 14 pm, a d10 of 2.4 pm and an average particle size of 21 pm, in each case with respect to the particle surface, approximately 0.1% by weight of triethoxy(3-aminopropyl)silane finish. The non-foamed, non-fiber ground glass to be used according to the invention may, depending on the processing to obtain the composition according to the invention or to obtain molded bodies from the composition according to the invention or in the molded body, have a smaller d90 or d50 or d10 value or a smaller average particle size than the ground particles originally used. Component C) According to "http: / / de.wikipedia.org / wiki / Faser-Kunststoff-Verbund," fibers are classified as short fibers, also called staple fibers, with a length ranging from 0.1 to 1 mm; long fibers, with a length ranging from 1 to 50 mm; and endless fibers, with a length L > 50 mm. Short fibers are used in injection molding and can be processed directly in an extruder. Long fibers can be processed They are also used in extrusion presses. They are widely used in fiber injection molding. Long fibers are frequently mixed with thermosets as fillers. Endless fibers are used as roving or fabric in fiber-reinforced plastics. Products made with endless fibers achieve the highest values ​​of stiffness and strength. Ground glass fibers are also available, with a length after grinding typically ranging from 70 to 200 mm. According to the invention, long glass fibers cut to a starting length in the range of 1 to 50 mm, particularly preferably in the range of 1 to 10 mm, and even more preferably in the range of 2 to 7 mm, are used as component C). Depending on the processing to obtain the moldable mass or the final product, the glass fibers of component C) may have a smaller d97 or d50 value in the moldable mass or the final product than the glass fibers originally used. Thus, the arithmetic mean length of the glass fibers after processing is frequently only in the range of 150 mm to 300 mm. The glass fibers to be used as component C) preferably have a fiber diameter in the range of 7 to 18 mm, particularly preferably in the range of 9 to 15 mm. In a preferred embodiment, the glass fibers of component C) are provided with a suitable finishing system and a bonding agent or bonding agent system. A silane-based finishing system or bonding agent is preferred. The silane-based bonding agents especially preferred for pretreatment are silane compounds of general formula (I) ((X-(CH2)q)k-Si-(O-CrH2r+1)4-k (I) in which X represents NH2-, carboxyl, HO- or EITHER / \ H2C-CH-CHrO q represents an integer from 2 to 10, preferably from 3 to 4, r represents an integer from 1 to 5, preferably from 1 to 2 and k represents an integer from 1 to 3, preferably 1. The particularly preferred bonding agents are silane compounds of the aminopropyltrimethoxysilane, aminobutyltrimethoxysilane, aminopropyltriethoxysilane, aminobutyltriethoxysilane groups, as well as the corresponding silanes containing as a substituent X a glycidyl group or a carboxyl group, with carboxyl groups being particularly preferred. For the finishing of the glass fibers to be used as component C), the bonding agent is used, preferably silane compounds according to formula (I), preferably in quantities of 0.05% to 2% by weight, especially preferably in quantities of 0.25% to 1.5% by weight and most especially preferably in quantities of 0.5% to 1% by weight, in each case with respect to 100% by weight of component C). According to "http: / / www.rg.de / wiki / Glasfasern", glass fibers are prepared using the melt spinning process (continuous filament, rod drawing, and nozzle blowing). In the continuous filament process, the molten glass flows under the force of gravity through hundreds of nozzle holes in a platinum spinning plate. The individual fibers can be drawn to unlimited lengths at a speed of 3–4 km / minute. The expert differentiates between different types of fiberglass, some examples of which are listed in this document: E-glass, the material used in most cases with the optimal price-performance ratio (R&G E-glass) H glass, hollow glass fibers for reduced weight (R&G hollow glass fiber fabric 160 g / m2 and 216 g / m2) R, S glass, for high mechanical requirements (R&G S2 glass) D-glass, borosilicate glass for high electrical requirements C-glass, with high chemical resistance quartz glass, with high temperature stability Other examples can be found at "http: / / de.wikipedia.org / wiki / Glasfaser". E-glass fibers have achieved the greatest importance for reinforcing plastics. E stands for electrical glass, since it was originally used primarily in the electrical industry. E-glass is produced by preparing molten masses of pure quartz glass with additions of limestone, kaolin, and boric acid. These contain, in addition to silicon dioxide, varying amounts of different metal oxides. The composition determines the properties of the products. According to the invention, at least one type of glass fiber from the E-glass, H-glass, R-glass, S-glass, D-glass, C-glass, and quartz glass groups is preferably used, and E-glass fibers are particularly preferred. E-glass fibers are the most widely used reinforcing material. Their strength properties are comparable to those of metals (e.g., aluminum alloys), but the specific gravity of the laminates is lower. E-glass fibers are non-combustible, heat-resistant up to approximately 400 °C, and stable against most chemicals and weathering. Component D) As component D), the compositions according to the invention contain melamine cyanurate [CAS No. 37640-57-6]. Melamine cyanurate is understood to be the reaction product of preferably equimolar amounts of melamine and cyanuric acid or isocyanuric acid. This includes, among others, all commercially available and commonly used product grades. Examples include, among others, Melapur® MC 25 and Melapur® MC50 (BASF, Ludwigshafen, Germany). The melamine cyanurate to be used according to the invention preferably consists of particles with average particle diameters from 0.1 µm to 100 µm, more preferably from 0.1 µm to 30 µm, and most preferably from 0.1 µm to 7 µm, and may be surface-treated or coated or bonded with known agents.This category primarily includes organic compounds that can be applied in monomeric, oligomeric, and / or polymeric form to melamine cyanurate. In particular, coating systems based on silicon-containing compounds, especially organofunctional silanes or organosiloxanes, are preferred. Coatings with inorganic components are also possible. Component E) The slip and / or release agents to be used as component E) in a preferred embodiment of the compositions according to the invention are preferably long-chain fatty acids, in particular stearic acid or behenic acid, their salts, in particular Ca or Zn stearate, as well as their ester derivatives or amide derivatives, in particular ethylene-bis-stearylamide, montana wax as well as low molecular weight polyethylene or polypropylene waxes. The montan wax, according to the present invention, consists of mixtures of saturated, straight-chain carboxylic acids with chain lengths of 28 to 32 carbon atoms. According to the invention, slip and / or release agents from the ester or amide group of saturated or unsaturated aliphatic carboxylic acids with 8 to 40 carbon atoms, saturated aliphatic alcohols, or amines with 2 to 40 carbon atoms, as well as metal salts of saturated or unsaturated aliphatic carboxylic acids with 8 to 40 carbon atoms, are used in a particularly preferential manner. At least one slip and / or release agent from the ethylene-bis-stearylamide, calcium stearate, and ethylene glycol dimontanate group is used in a particularly preferential manner. Particularly preferably calcium stearate [CAS No. 1592-23-0] or ethylene-bis-stearylamide [CAS No. 110-30-5] is used. Ethylene-bis-stearylamide (Loxiol® EBS from Emery Oleochemicals) is particularly preferably used. Component F) At least one laser absorber is used as component F). According to Kunststoffe 8, 2008, 119-121, this refers to a laser light absorber, preferably for labeling plastic products. The laser absorber to be used as component F) is preferably selected from the group of antimony trioxide, tin oxide, tin orthophosphate, barium titanate, aluminum oxide, copper hydroxyphosphate, copper orthophosphate, copper potassium diphosphate, copper hydroxide, antimony tin oxide, bismuth trioxide, and anthraquinone. Antimony trioxide and antimony tin oxide are particularly preferred. Antimony trioxide is especially preferred. The laser absorber, in particular antimony trioxide, can be used directly as a powder or in the form of basic mixtures. Preferred basic mixtures are those based on polyamide or those based on poly(butylene terephthalate), polyethylene, polypropylene, polyethylene-polypropylene copolymer, polyethylene grafted with maleic anhydride, and / or polypropylene grafted with maleic anhydride, with the polymers for the mixture being suitable. basic antimony trioxide, either individually or in a mixture. Antimony trioxide is preferably used in the form of a basic mixture based on polyamide 6. The laser absorber can be used individually or as a mixture of several laser absorbers. Laser absorbers can absorb laser light of a specific wavelength. In practice, this wavelength is typically between 157 nm and 10.6 pm. Examples of lasers operating at these wavelengths are described in WO2009 / 003976 A1. Nd:YAG lasers, which can achieve wavelengths of 1064, 532, 355, and 266 nm, and CO2 lasers are preferred. Component G) In one embodiment, the compositions according to the invention may contain as component G) in addition to melamine cyanurate (component D)) at least one flame retardant other than component D), preferably a halogen-free and / or phosphorus-free flame retardant. The preferred halogen-free and / or phosphorus-free flame retardants are nitrogen-containing flame retardants, used individually or in mixtures. The preferred nitrogen-containing flame retardants are the reaction products of trichlorotriazine, piperazine and morpholine according to CAS No. 1078142-02-5, in particular MCA PPM Triazin HF from MCA Technologies GmbH, Biel-Benken, Switzerland, and melamine condensation products such as Melem, Melam, Melon or higher condensation compounds of this type. Inorganic nitrogen-containing compounds, preferably ammonium salts, can also be used. In addition, salts of aliphatic and aromatic sulfonic acids and mineral flame retardant additives such as aluminum and / or magnesium hydroxide, hydrated Ca-Mg carbonates (e.g., document DE-A 4 236 122) can also be used. Synergists of flame retardants from the group of metallic compounds containing oxygen, nitrogen or sulfur are also taken into account, preferably zinc oxide, zinc borate, zinc stannate, zinc hydroxystannate, zinc sulfide, molybdenum oxide, magnesium oxide, magnesium carbonate, calcium carbonate, calcium oxide, titanium nitride, boron nitride, magnesium nitride, zinc nitride, zinc phosphate, calcium phosphate, calcium borate, magnesium borate or mixtures thereof. In an alternative embodiment, flame retardants containing halogen and / or phosphorus can be used as component G) however also (whenever necessary). The preferred halogen-containing flame retardants are commercially available organic halogen compounds, most preferably ethylene-1,2-bistetrabromophthalimide, decabromodiphenylethane, tetrabromobisphenol-A-epoxy oligomer, tetrabromobisphenol-A oligocarbonate, tetrachlorobisphenol-A oligocarbonate, pentabromobenzyl polyacrylate, brominated polystyrene, and brominated polyphenylene ethers, which can be used alone or in combination with synergists, particularly antimony trioxide or antimony pentoxide. Preferred phosphorus-containing flame retardants are red phosphorus, metal phosphinates, in particular aluminum phosphinate or zinc phosphinate, metal phosphonates, in particular aluminum phosphinate, calcium phosphonate or zinc phosphonate, derivatives of 9,10-dihydro-9-oxa-10-phosphaphenanthrene-10-oxides (DOPO derivatives), resorcinol-bis-(diphenyl phosphate), (RDP) including oligomers as well as bisphenol-A-bis-diphenyl phosphate (BDP) including oligomers, in addition to zinc bis(diethylphosphinate), aluminum tris(diethylphosphinate), melamine phosphate, melamine pyrophosphate, melamine polyphosphate, melamine-poly(aluminum phosphate), melamine-poly(zinc phosphate) or phenoxyphosphazene oligomers and mixtures thereof. Other flame retardants to be used as component G) are carbon-forming agents, especially preferably phenol-formaldehyde resins, polycarbonates, polyimides, polysulfones, polyethersulfones or polyetherketones as well as anti-drip agents, in particular tetrafluoroethylene polymers. Fire retardants can be added in pure form, as well as through basic mixtures or compacted materials. Component H) As component H), the compositions contain at least one other filler or reinforcing substance other than components B) and C). In this respect, mixtures of two or more different fillers and / or reinforcing substances may also be used, preferably based on talc, mica, silicate, quartz, wollastonite, kaolin, amorphous silicic acids, nanoscale minerals, especially montmorillonite or nano-boehmite, magnesium carbonate, chalk, feldspar, barium sulfate, and / or fiber-based fillers and / or reinforcing substances. Mineral particle fillers based on talc, mica, silicate, quartz, wollastonite, kaolin, amorphous silicic acids, magnesium carbonate, chalk, feldspar, and / or barium sulfate are preferably used. Mineral particle fillers based on talc, wollastonite, and / or kaolin are especially preferred. Needle-shaped mineral fillers are also preferably used. Needle-shaped mineral fillers, according to the invention, are defined as mineral fillers with a very pronounced needle-like character. Needle-shaped wollastonites are preferably mentioned. Preferably, the needle-shaped mineral filler has a length-to-diameter ratio in the range of 2:1 to 35:1, more preferably from 3:1 to 19:1, and particularly preferably in the range of 4:1 to 12:1. The average particle size of the needle-shaped mineral fillers is preferably less than 20 µm, more preferably less than 15 µm, and particularly preferably less than 10 µm, as determined using a CILAS granulometer. The fillers and / or reinforcing substances to be used as component H) are surface-modified in a preferred embodiment, preferably with a bonding agent or bonding agent system, most preferably silane-based. Pretreatment is not, however, strictly necessary. Silane compounds of general formula (I) already described above are also considered as bonding agents. For the finishing of component H) silane compounds are generally used in quantities of 0.05% to 2% by weight, preferably 0.25% to 1.5% by weight and in particular 0.5% to 1% by weight with respect to the mineral filler to obtain the surface coating. Also, the charges of component H) may exhibit, conditionally due to the processing to obtain the composition or to obtain the product from the composition or in the product, a d97 or d50 value smaller than the charges originally used. Component K) The additives to be used as component K) are antioxidants, UV stabilizers, gamma ray stabilizers, hydrolysis stabilizers, heat stabilizers, antistatic agents, emulsifiers, nucleating agents, softeners, processing aids, shock resistance modifiers, colorants, pigments, and elastomeric modifiers. The additives may be used alone, in mixtures, or as basic mixtures. Lowinox® HD 98, 3,3'-bis(3,5-di-tert-butyl-4-hydroxyphenyl)-N,N'-hexamethylenedipropionamide [CAS No. 23128-74-7], is preferably used as an antioxidant. Substituted resorcinols, salicylates, benzotriazoles and benzophenones are preferably used as UV stabilizers. The colorants used are preferably inorganic pigments, in particular ultramarine blue, iron oxide, zinc sulfide or carbon black, as well as organic pigments, preferably phthalocyanines, quinacridones, perylenes, and coloring substances, preferably nigrosin and anthraquinone. Stericly hindered phenols and / or phosphites, hydroquinones, aromatic secondary amines such as diphenylamines, substituted resorcinols, salicylates, benzotriazoles, and benzophenones, as well as representatives of these groups with different substitutions or mixtures thereof, are preferably used as heat stabilizers. Stericly hindered phenols, alone or in combination with phosphites, are particularly preferred, with N,N'-bis[3-(3',5'-di-tert-butyl-4'-hydroxyphenyl)propionyl]hexamethylenediamine (e.g., Irganox® 1098 from BASF SE, Ludwigshafen, Germany) [cAs No. 21328-74-7] being especially preferred. The nucleating agents used are preferably sodium or calcium phenylphosphinate, aluminum oxide or silicon oxide, and especially preferably talc [CAS No. 14807-96-6], this list being non-conclusive. Copolymers of at least one α-olefin with at least one methacrylic acid ester or acrylic acid ester of an aliphatic alcohol are preferably used as flow aids. Copolymers in which the α-olefin consists of ethene and / or propene and the methacrylic acid ester or acrylic acid ester as the alcohol component contains linear or branched alkyl groups with 6 to 20 carbon atoms are particularly preferred. (2-Ethyl)hexyl acrylate is especially preferred. Suitable copolymers according to the invention, used as flow aids, are characterized not only by their composition but also by their low molecular weight. Accordingly, for compositions that are to be protected against thermal degradation, The invention is particularly suitable for copolymers exhibiting a Melt Flow Index (MFI) measured at 190 °C and a 2.16 kg load of at least 100 g / 10 min, preferably at least 150 g / 10 min, and especially preferably at least 300 g / 10 min. The MFI is used to characterize the flow of a thermoplastic melt and is subject to ISO 1133 or ASTM D 1238. The MFI, or all indications relating to MFI in the context of the present invention, are obtained, measured, or determined uniformly according to ISO 1133 at 190 °C and a test weight of 2.16 kg. The softeners to be used as component K) are preferably dioctyl ester of phthalic acid, dibenzyl ester of phthalic acid, butylbenzyl ester of phthalic acid, hydrocarbon oils, N-(n-butyl)benzenesulfonamide. The elastomeric modifiers to be used as component K) preferably comprise, among others, one or more graft polymers of K.1 from 5% to 95% by weight, preferably from 30% to 90% by weight, of at least one vinyl monomer in K.2 from 95% to 5% by weight, preferably from 70% to 10% by weight of one or more grafting bases with glass transition temperatures < 10 °C, preferably < 0 °C, most preferably < - 20 °C. The K.2 grafting base generally has an average particle size (d50 value) of 0.05 to 10 pm, preferably 0.1 to 5 pm, most preferably 0.2 to 1 pm. The monomers for K.1 are preferably mixtures of K.1.1 from 50% to 99% by weight of vinyl aromatic compounds and / or core-substituted vinyl aromatic compounds, in particular styrene, α-methylstyrene, β-methylstyrene, β-chlorostyrene, and / or (C1-C8) alkyl esters of methacrylic acid, in particular methyl methacrylate, ethyl methacrylate and K.1.2 from 1% to 50% by weight of vinyl cyanides, in particular unsaturated nitriles such as acrylonitrile and methacrylonitrile and / or alkyl esters (CrCa) of (meth)acrylic acid, in particular methyl methacrylate, glycidyl methacrylate, n-butyl acrylate, t-butyl acrylate, and / or derivatives, in particular anhydrides and imides of unsaturated carboxylic acids, in particular maleic acid anhydride and N-phenyl-maleinimide. Preferred K.1.1 monomers are selected from at least one of the monomers styrene, a-methylstyrene and methyl methacrylate; preferred K.1.2 monomers are selected from at least one of the monomers acrylonitrile, maleic acid anhydride, glycidyl methacrylate and methyl methacrylate. The particularly preferred monomers are K.1.1 styrene and K.1.2 acrylonitrile. Certain K.2 grafting bases suitable for graft polymers to be used in elastomeric modifiers include, for example, diene rubbers, EPDM rubbers (ethylene / propylene-based rubbers with optional diene), acrylate rubbers, polyurethane, silicone, chloroprene, and ethylene / vinyl acetate. EPDM stands for ethylene-propylene-diene rubber. The preferred K.2 grafting bases are diene rubbers, in particular based on butadiene, isoprene etc. or mixtures of diene rubbers or copolymers of diene rubbers or their mixtures with other copolymerizable monomers, in particular according to K.1.1 and K.1.2), provided that the glass transition temperature of component K.2 is <10 °C, preferably < 0 °C, especially preferably < -10 °C. The particularly preferred K.2 grafting bases are ABS polymers (ABS in emulsion, bulk, and suspension), representing ABS acrylonitrile-butadiene-styrene, as described, for example, in DE-A 2 035 390 (= US-A 3 644 574) or DE-A 2 248 242 (= GB-A 1 409 275) or in Ullmann, Enzyklopadie der Technischen Chemie, Volume 19 (1980), page 280 et seq. The gel content of the K.2 grafting base is preferably at least 30% by weight, and especially preferably at least 40% by weight (measured in toluene). Elastomeric modifiers or graft polymers are prepared by radical polymerization, preferably by emulsion, suspension, solution or bulk polymerization, in particular by emulsion or bulk polymerization. Certain particularly suitable grafting rubbers are also ABS polymers prepared by redox initiation with an organic hydroperoxide initiator system and ascorbic acid according to US-A 4 937 285. Since in the grafting reaction the grafting monomers are grafted, as is known, not necessarily completely into the graft base, grafting polymers, according to the invention, are also understood to be those products obtained by (co)polymerization of the grafting monomers in the presence of the graft base and produced together in the processing. Equally suitable acrylate rubbers are based on K.2 graft bases, which are preferably polymers of acrylic acid alkyl esters, possibly with up to 40 wt% relative to K.2 of other ethylenically unsaturated polymerizable monomers. Preferred polymerizable acrylic acid esters include C1-C8 alkyl esters, preferably methyl, ethyl, butyl, n-octyl, and 2-ethylhexyl esters; haloalkyl esters, preferably C1-C8 haloalkyl esters, such as chloroethyl acrylate, glycidyl ester, and mixtures of these monomers. Graft polymers with butyl acrylate as the core and methyl methacrylates as the shell are particularly preferred, especially Paraloid® EXL2300, Dow Corning Corporation, Midland, Michigan, USA. For crosslinking, monomers with more than one polymerizable double bond can be copolymerized. Preferred examples of crosslinking monomers are esters of unsaturated monocarboxylic acids with 3 to 8 carbon atoms and unsaturated monohydroxylated alcohols with 3 to 12 carbon atoms, or saturated polyols with 2 to 4 OH groups and 2 to 20 carbon atoms, preferably ethylene glycol dimethacrylate, allyl methacrylate; multiple times unsaturated heterocyclic compounds, preferably trivinyl and trialyl cyanurate; polyfunctional vinyl compounds, preferably di- and trivinylbenzenes; however, trialyl phosphate and diallyl phthalate are also suitable. Certain preferred crosslinking monomers are allyl methacrylate, ethylene glycol dimethacrylate, diallyl phthalate, and heterocyclic compounds having at least 3 ethylenically unsaturated groups. Certain crosslinking monomers that are particularly preferred are the cyclic monomers trialyl cyanurate, trialyl isocyanurate, triacryloylhexahydro-s-triazine, and trialylbenzenes. The amount of crosslinked monomers preferably ranges from 0.02% to 5%, and in particular from 0.05% to 2% by weight, with respect to the K.2 graft base. In the case of cyclic crosslinking monomers with at least 3 ethylenically unsaturated groups, it is advantageous to limit the amount to below 1% by weight of the graft base K.2. Other preferred ethylenically unsaturated polymerizable monomers that, in addition to acrylic acid esters, may be used for the preparation of graft base K.2 are acrylonitrile, styrene, α-methylstyrene, acrylamides, vinyl-alkyl(C1-C6) ethers, methyl methacrylate, glycidyl methacrylate, and butadiene. The preferred acrylate rubbers for graft base K.2 are emulsion polymers with a gel content of at least 60% by weight. Other preferably suitable graft bases according to K.2 are silicone rubbers with active grafting sites, as described in documents DE-A 3 704 657 (= US 4 859 740), DE-A 3 704 655 (= US 4 861 831), DE-A 3 631 540 (= US 4 806 593) and DE A 3631 539 (= US 4 812 515). In addition to elastomeric modifiers based on graft polymers, elastomeric modifiers not based on graft polymers can also be used, provided they have glass transition temperatures < 10 °C, preferably < 0 °C, and especially preferably < -20 °C. These preferably include elastomers with a block copolymer structure, as well as thermoplastically meltable elastomers, in particular EPM, EPDM, and / or SEBS rubbers (EPM = ethylene-propylene copolymer, EPDM = ethylene-propylene-diene rubber, and SEBS = styrene-ethene-butene-styrene copolymer). The preferred subject of the invention is compositions containing A) from 5% to 92.89% by weight, preferably from 20% to 90% by weight, most preferably from 30% to 80% by weight of polyamide 6, B) from 5% to 80% by weight, preferably from 10% to 60% by weight, especially preferably from 15% to 50% by weight of a non-fiber-formed, non-foamed ground glass with a d90 determined by laser diffractometry in the range of 5 to 250 mm, preferably in the range of 10 to 150 mm, especially preferably in the range of 15 to 80 mm, most preferably in the range of 16 to 25 mm, and a length in the range of 0.01 to 0.5 mm, C) from 2% to 8% by weight, preferably from 3% to 7% by weight, most preferably from 4% to 6% by weight of long cut glass fibers with a starting length in the range of 1 to 50 mm, most preferably in the range of 1 to 10 mm, most preferably in the range of 2 to 7 mm, and D) from 0.1% to 40% by weight, preferably from 1% to 20% by weight of melamine cyanurate and G) from 0.01% to 60% by weight, preferably from 1% to 30% by weight, most preferably from 5% to 25% by weight, most preferably from 0.01% to 60% by weight of ethylene-bis-stearylamide, with the condition that the sum of all the percentages by weight always equals 100. The preferred subject of the invention is compositions containing A) from 5% to 92.89% by weight, preferably from 20% to 90% by weight, most preferably from 30% to 80% by weight of polyamide 66, B) from 5% to 80% by weight, preferably from 10% to 60% by weight, especially preferably from 15% to 50% by weight of a non-fiber-formed, non-foamed ground glass with a d90 determined by laser diffractometry in the range of 5 to 250 pm, preferably in the range of 10 to 150 pm, especially preferably in the range of 15 to 80 pm, most preferably in the range of 16 to 25 pm, and a length in the range of 0.01 to 0.5 mm, C) from 2% to 8% by weight, preferably from 3% to 7% by weight, most preferably from 4% to 6% by weight of long cut glass fibers with a starting length in the range of 1 to 50 mm, most preferably in the range of 1 to 10 mm, most preferably in the range of 2 to 7 mm, D) from 0.1% to 40% by weight, preferably from 1% to 20% by weight of melamine cyanurate, and G) from 0.01% to 60% by weight, preferably from 1% to 30% by weight, most preferably from 5% to 25% by weight, most preferably from 0.01% to 60% by weight of ethylene-bis-stearylamide, with the condition that the sum of all the percentages by weight always equals 100. The preferred subject of the invention is compositions containing A) from 5% to 92.88% by weight, preferably from 20% to 90% by weight, most preferably from 30% to 80% by weight of polyamide 6, B) from 5% to 80% by weight, preferably from 10% to 60% by weight, especially preferably from 15% to 50% by weight of a non-fiber-formed, non-foamed ground glass with a d90 determined by laser diffractometry in the range of 5 to 250 pm, preferably in the range of 10 to 150 pm, especially preferably in the range of 15 to 80 pm, most preferably in the range of 16 to 25 pm, and a length in the range of 0.01 to 0.5 mm, C) from 2% to 8% by weight, preferably from 3% to 7% by weight, most preferably from 4% to 6% by weight of long cut glass fibers with a starting length in the range of 1 to 50 mm, most preferably in the range of 1 to 10 mm, most preferably in the range of 2 to 7 mm, D) from 0.1% to 40% by weight, preferably from 1% to 20% by weight of melamine cyanurate, and G) from 0.01% to 60% by weight, preferably from 1% to 30% by weight, most preferably from 5% to 25% by weight, most preferably from 0.01% to 60% by weight of ethylene-bis-stearylamide, and K) from 0.01% to 20% by weight, preferably from 0.05% to 10% by weight, most preferably from 0.1% to 5% by weight of 3,3'-bis(3,5-di-tert-butyl-4-hydroxyphenyl)-N,N'-hexamethylenedipropionamide, provided that the sum of all the weight percentages always equals 100. The preferred subject of the invention is compositions containing A) from 5% to 92.88% by weight, preferably from 20% to 90% by weight, most preferably from 30% to 80% by weight of polyamide 66, B) from 5% to 80% by weight, preferably from 10% to 60% by weight, especially preferably from 15% to 50% by weight of a non-fiber-formed, non-foamed ground glass with a d90 determined by laser diffractometry in the range of 5 to 250 pm, preferably in the range of 10 to 150 pm, of especially preferably in the range of 15 to 80 pm, most preferably in the range of 16 to 25 pm, and a length in the range of 0.01 to 0.5 mm, C) from 2% to 8% by weight, preferably from 3% to 7% by weight, most preferably from 4% to 6% by weight of long cut glass fibers with a starting length in the range of 1 to 50 mm, most preferably in the range of 1 to 10 mm, most preferably in the range of 2 to 7 mm, D) from 0.1% to 40% by weight, preferably from 1% to 20% by weight of melamine cyanurate, G) from 0.01% to 60% by weight, preferably from 1% to 30% by weight, most preferably from 5% to 25% by weight, most preferably from 0.01% to 60% by weight of ethylene-bis-stearylamide, and K) from 0.01% to 20% by weight, preferably from 0.05% to 10% by weight, most preferably from 0.1% to 5% by weight of 3,3'-bis(3,5-di-tert-butyl-4-hydroxyphenyl)-N,N'-hexamethylenedipropionamide, provided that the sum of all the weight percentages always equals 100. Procedure The present invention further relates to a process for manufacturing products, preferably electrical construction parts, especially FI switches and line protection switches, most preferably line protection switches with rated currents >16 A, particularly preferably line protection switches with rated currents >32 A, by using compositions according to the invention in injection molding, including the special processes GIT (gas injection technique), WIT (water injection technique) and PIT (projectile injection technique), in extrusion processes, including in profile extrusion, or in blow molding. For the manufacture of these products, the individual components of the composition according to the invention are first mixed in at least one mixing tool, and this mixture, which is then in the form of a moldable mass, is fed through at least one outlet of the mixing tool either to direct processing, or discharged as a strand and, by means of a granulator, preferably a rotating blade-carrying cylinder, is cut into granules of the desired length to be available for further processing. Since most processors require plastic in granular form, granulation plays an increasingly important role. A basic distinction is made between hot and cold cutting. Depending on the processing method, different granule shapes result. Hot cutting yields granules containing the compositions according to the invention in pearl or lentil-like shapes, while cold cutting yields granules containing the compositions according to the invention in cylindrical or cube shapes. The compositions according to the invention in granular form are preferably obtained by cold cutting. The skillful practitioner is free to use various mixing tools suitable for achieving optimal mixing results with respect to the compositions to be used according to the invention. An extruder is a preferred mixing tool within the meaning of the present invention. Preferred extruders are single-screw or twin-screw extruders, as well as their respective subgroups, most preferably conventional single-screw extruders, efficient single-screw extruders, counter-rotating twin-screw extruders, or twin-screw extruders rotating in the same direction. These are known to the skillful practitioner from Technische Thermoplaste 4. Polyamide, ed.: G.W. Becker and D. Braun, Carl Hanser Verlag, 1998, pp. 311–314, as well as K.Brast, doctoral thesis "Verarbeitung von Langfaser-verstarkten Thermoplasten im direkten Plastifizier- / Pressverfahren", Rheinisch-Westfalische Technische Hochschule Aachen, 2001, p. 30 - 33. Starting with compositions in the form of moldable mass or granules according to the invention, the products according to the invention, preferably electrical or electronic products, are manufactured by means of forming processes. The preferred forming processes are injection molding or extrusion. The processes according to the invention for manufacturing products by extrusion or injection molding preferably operate at melt temperatures in the range of 230 °C to 330 °C, especially preferably at melt temperatures in the range of 250 °C to 300 °C and preferably additionally at pressures of no more than 2500 bar, especially preferably at pressures of no more than 2000 bar, very especially preferentially to pressures of no more than 1500 bar and in particular preferentially to pressures of no more than 750 bar. The injection molding process is characterized in that the composition to be used according to the invention, preferably in granular form, is melted (plasticized) in a heated cylindrical cavity and injected as injection material under pressure into a tempered cavity. After cooling (solidification) of the material, the injection-molded part is removed from the mold. In this respect, the following work steps are distinguished: 1. to plasticize / to melt 2. Injection phase (filling process) 3. Compression molding phase (due to thermal contraction during crystallization) 4. Unmold. An injection molding machine consists of a clamping unit, the injection unit, the drive, and the control system. The clamping unit includes fixed and movable clamping plates for the injection mold, a faceplate, and the actuator for the movable clamping plates (articulated lever mechanism or hydraulic clamping unit). An injection unit comprises the electrically heated cylinder, the screw drive (motor, gear), and the hydraulic system for moving the screw and the injection unit. The purpose of the injection unit is to melt, meter, inject, and compress (due to shrinkage) the composition to be used according to the invention, particularly in granular form. The problem of melt reflux inside the screw (leakage flow) is solved by means of check valves. The molten material is then injected into the mold, cooled, and the finished component is thus completed. This process always requires two injection mold halves. The following functional complexes are distinguished during injection molding: - riser system - morphogenic inserts - deaeration - mechanical and force absorption - demolding and motion transmission system - warm-up The special injection molding processes GIT (gas injection technique), WIT (water injection technique), and PIT (projectile injection technique) are specialized injection molding processes for manufacturing hollow parts. A key difference from conventional injection molding is a special working step towards the end of the injection mold filling phase or after a defined partial filling of the mold. In this process-specific working step, a processing medium is injected through a so-called injector into the molten core of the previously molded part to form a cavity. This medium is typically gas (usually nitrogen) in the case of GIT and water in the case of WIT. In the case of PIT, a projectile is injected into the molten core, thus forming a cavity. Unlike injection molding, extrusion uses an endless stream of molded plastic, in this case containing the composition according to the invention, in an extruder press, the extruder press being a machine for manufacturing thermoplastic molded parts. It differs - single screw extruder press and twin screw extruder press as well as their respective subgroups - conventional single-screw extrusion presses, efficient transport single-screw extrusion presses, - Twin-screw extrusion presses with opposite rotation and twin-screw extrusion presses that rotate in the same direction. Profiles, according to the present invention, are (construction) components that have an identical cross-section along their entire length. These can be manufactured using the profile extrusion process. The basic procedural steps of the profile extrusion process are: 1. To plasticize and facilitate the thermoplastic melt in an extruder press, 2. Extrude the thermoplastic molten material bead using a calibration sleeve that has the cross-section of the profile to be extruded, 3. Cool the extruded profile on a calibration table, 4. Subsequently transport the profile using an extraction system behind the calibration table, 5. Cut the previously endless profile in a cutting installation, 6. Collect the cut profiles on a collection table. A description of the extrusion of polyamide 6 and polyamide 66 profiles is given in Kunststoff-Handbuch 3 / 4, Polyamide, Carl Hanser Verlag, Munich 1998, pages 374-384. Blow molding processes within the meaning of the present invention are preferably conventional blow molding and extrusion, 3D blow molding and extrusion, suction blow molding process, and sequential coextrusion. The basic procedural steps of conventional blow molding and extrusion are, according to Thielen, Hartwig, Gust, "Blasformen von Kunststoffhohlkorpern", Carl Hanser Verlag, Munich 2006, pages 15 to 17: 1. To plasticize and facilitate the thermoplastic melt in an extruder press, 2. divert the molten mass in a downward perpendicular flow motion and mold a molten mass "preform" in the shape of a flexible tube, 3. surround the freely hanging preform with a mold that is generally made up of two halves, the blow molding mold, 4. Insert a blowing spike or one (possibly several) blowing needle(s), 5. Blow the plastic preform towards the cooled wall of the blow molding mold, where the plastic cools, hardens, and takes the final shape of the molded part. 6. Open the mold and remove the blow-molded piece. 7. Remove the separated "bubble residue" by squeezing at both ends of the blow-molded part. Further stages of processing may follow. Products with complex geometries and multi-axis curvatures can also be manufactured using blow molding and conventional extrusion. However, these processes result in products with a large proportion of excess material, separated by flattening, and exhibiting a weld bead in large areas. In 3D blow molding and extrusion, also known as 3D blow molding, a preform, its diameter adapted to the cross-section of the article using special devices, is deformed to avoid weld seams and to reduce the amount of material inserted. This preform is then manipulated and inserted directly into the blow molding cavity. The resulting compression edge is thus reduced to a minimum at the ends of the article (Thielen, Hartwig, Gust, "Blasformen von Kunststoffhohlkorpern", Carl Hanser Verlag, Munich 2006, pp. 117-122). In the suction blow molding process, also known as suction blowing, the preform is transported directly from the nozzle of the flexible tube head into the closed blow mold and is "suctioned" through the mold by means of an air stream. After the lower end of the preform exits the blow mold, it is separated by crushing the mold using closing elements above and below, and then undergoes the blowing and cooling process (Thielen, Hartwig, Gust, "Blasformen von Kunststoffhohlkorpern", Carl Hanser Verlag, Munich 2006, page 123). Use The objective of this application is also the use of the compositions according to the invention as moldable masses in injection molding, including the special procedures GIT (gas injection technique), WIT (water injection technique) and PIT (projectile injection technique), in the extrusion process, preferably in profile extrusion, in blow molding, especially preferably conventional blow molding and extrusion, 3D blow molding and extrusion process or blow molding and suction process to manufacture products therefrom according to the invention. The present invention also relates to the use of compositions according to the invention for the manufacture of products, preferably electrical components, and more preferably circuit breakers and line protection switches, and more preferably line protection switches with rated currents >16 A, and in particular preferably line protection switches with rated currents >32 A. A preferred objective of the invention is the use of compositions containing A) polyamide 6 or polyamide 66, B) non-fiber-formed and non-foamed ground glass with a d90 determined by laser diffractometry from 5 to 250 pm, preferably from 10 to 150 pm, most preferably from 15 to 80 pm, most preferably from 16 to 25 pm and a length in the range of 0.01 to 0.5 mm, C) long glass fibers cut to a starting length in the range of 1 to 50 mm, especially preferably in the range of 1 to 10 mm, and most preferably in the range of 2 to 7 mm, and D) melamine cyanurate for the manufacture of products for the electrical or electronic industry, preferably FI switches and line protection switches, especially preferably line protection switches with rated currents >16 A, in particular preferably line protection switches with rated currents >32 A. A particularly preferred objective of the invention is the use of compositions containing A) from 5% to 92.9% by weight, preferably from 20% to 90% by weight, most preferably from 30% to 80% by weight of polyamide 6 or polyamide 66, B) from 5% to 80% by weight, preferably from 10% to 60% by weight, especially preferably from 15% to 50% by weight of a non-fiber-formed, non-foamed ground glass with a d90 determined by laser diffractometry in the range of 5 to 250 pm, preferably in the range of 10 to 150 pm, especially preferably in the range of 15 to 80 pm, most preferably in the range of 16 to 25 pm, and a length in the range of 0.01 to 0.5 mm, C) from 2% to 8% by weight, preferably from 3% to 7% by weight, most preferably from 4% to 6% by weight of long cut glass fibers with a starting length in the range of 1 to 50 mm, most preferably in the range of 1 to 10 mm, most preferably in the range of 2 to 7 mm, and D) from 0.1% to 40% by weight, preferably from 1% to 20% by weight of melamine cyanurate, provided that the sum of all percentages by weight always equals 100, for the manufacture of products of the electrical or electronic industry, preferably FI switches and line protection switches, especially preferably line protection switches with rated currents >16 A, in particular preferably line protection switches with rated currents >32 A. Examples To verify the improvements described according to the invention, the corresponding plastic compositions were first produced by mixing. The individual components, as listed in Table 2, were mixed in a twin-screw extruder (ZSK 25 Compounder, Coperion Werner & Pfleiderer, Stuttgart, Germany) at temperatures between 240 and 280 °C, discharged as a strand, cooled to granulation capacity, and granulated. After drying (generally two days at 70 °C in a vacuum drying cabinet), the processing of the granulated at temperatures in the range of 240 °C to 280 °C to obtain standardized test specimens for the respective tests. Glow wire stability was determined by means of the GWFI (Glow-Wire Flammability-Index) glow wire test according to IEC 60695-2-12 on round plates with a diameter of 80 mm and a thickness of 0.75 mm. The Charpy impact resistance was determined according to ISO 179-1 eU on freshly injected test specimens of dimension 80 mm 10 mm 4 mm. Tensile strength, elongation at break and tensile modulus were determined according to ISO 527-1 / -2 on shoulder type 1A specimens (dimension 170 mm 10 mm 4 mm). Thermomolding stability was determined according to ISO 75-1,-2 with an applied bending stress of 1.8 MPa (HDT-A) on specimens of dimension 80 mm 10 mm 4 mm. The shrinkage in processing, in each case parallel and perpendicular to the injection direction, was determined according to ISO 294-4 on test specimens of dimension 60 mm 60 mm 2 mm at a mass temperature of 260 °C and a mold temperature of 80 °C at 600 bar compression. As a measure of isotropy, the strain was then calculated as the ratio of shrinkage during processing parallel to the injection direction to shrinkage during processing perpendicular to the injection direction. For isotropy values ​​above 0.8, materials with low strain can be considered to have this characteristic. Thus, for example, a commercially available polyamide 6 with 30% by weight of glass fibers exhibits a processing shrinkage of 0.3% / 0.7% [parallel / perpendicular], which then leads, according to the formula mentioned above, to an isotropy value of only 0.4 and thereby signifies a strong deformation. The particle size determination of the ground glass particles (component B) was performed using an optical laser procedure ("Eye Tech") from Ankersmid Ltd, Oosterhout, The Netherlands, in an "ACM-104 LiquidFlow (4x4 mm)" cell. The measurement time was approximately 900 s. The evaluation refers to the surface of the glass particles. The following were used in the trials: Component A): Polyamide 6 (Durethan® B26, Lanxess Deutschland GmbH, Koln, Germany) [CAS No. 25038-54-4] Component B): MF7900 from Lanxess Deutschland GmbH, Cologne, Germany. [a non-fiber-formed, non-foamed glass-based E containing approximately 0.1 wt% triethoxy(3-aminopropyl)silane finish B' with a d90 of 54 pm, a d50 of 14 pm, a d10 of 2.4 pm and an average particle size of 21 pm, in each case with respect to the particle surface]. Component C): CS 7997 chopped glass fiber from Lanxess Deutschland GmbH, Cologne, Germany [average fiber diameter 10 pm, average fiber length 4.5 mm, E glass] Component D): melamine cyanurate [cAs no. 37640-57-6] (Melapur® MC25, from BASF, Ludwigshafen, Germany) Component G): Ethylene-bis-stearylamide [CAS No. 110-30-5] as Loxiol® EBS from Emery Oleochemicals Component K): Lowinox® HD 98 - 50 D - TDS, 3,3'-bis(3,5-di-tert-butyl-4-hydroxyphenyl)-N,N'- Hexamethylenedipropionamide [CAS No. 23128-74-7] Table 2 A [%] 71.6 70.6 B [%] C [%] D [%] G [%] 0.2 0.2 K [%] 0.2 0.2 GWFI (0.75 mm) [°C] 960 960 HDTA [°C] CHARPY [kJ / m2] processing shrinkage (parallel) [%] 0.87 0.78 processing shrinkage (perpendicular) [%] 0.93 0.91 isotropy [parallel / perpendicular] 0.94 0.86 tensile strength [MPa] elongation at break [%] 2.8 2.9 tensile modulus [MPa] 4686 4885 The indications of the components in % by weight with respect to the total moldable mass. The examples in Table 2 show that examples 1 and 2 according to the invention in the incandescent filament test 5 also reached the maximum temperature of 960 °C in test specimens only 0.75 mm thick, in this respect they had with an isotropy above 0.8 a tendency to deformation very low and nevertheless exhibited thermoforming stabilities according to HDT A above 130 °C.

Claims

1. Compositions containing A) polyamide 6 or polyamide 66, B) non-fiber-formed, non-foamed ground glass with a d90 determined by laser diffractometry in the range of 5 to 250 mm, and a length in the range of 0.01 to 0.5 mm, C) long glass fibers cut with a starting length in the range of 1 to 50 mm, and D) melamine cyanurate.

2. Compositions according to claim 1, characterized in that they contain A) from 5% to 92.9% by weight of polyamide 6 or polyamide 66, B) from 5% to 80% by weight of a non-fiber-formed, non-foamed ground glass with a d90 determined by laser diffractometry in the range of 5 to 250 mm and a length in the range of 0.01 to 0.5 mm, C) from 2% to 8% by weight of long glass fibers cut with a starting length in the range of 1 to 50 mm, and D) from 0.1% to 40% by weight of melamine cyanurate, provided that the sum of all the weight percentages always equals 100.

3. Compositions according to claims 1 or 2, characterized in that component B) is further bonded with B'), at least one aminoalkyltryalkoxysilane, preferably in amounts from 0.01% to 1.5% by weight with respect to the amount of non-fibered, non-foamed ground glass.

4. Compositions according to any one of claims 1 to 3, characterized in that they contain, in addition to components A), B), C), D and E) or A), B), B'), C), D) and also E), from 0.01% to 5% by weight with respect to the total composition, at least one slip and / or release agent, the other components being reduced until the sum of all the percentages by weight is always 100. 5.Compositions according to any one of claims 1 to 4, characterized in that they contain in addition to components A) to E) or instead of E) also F) from 0.01% to 10% by weight with respect to the total composition of at least one laser absorber, preferably a laser absorber selected from the group of antimony trioxide, tin oxide, tin orthophosphate, barium titanate, aluminum oxide, copper hydroxyphosphate, copper orthophosphate, copper potassium diphosphate, copper hydroxide, antimony tin oxide, bismuth trioxide and anthraquinone, the other components being reduced until the sum of all the percentages by weight is always 100. 6.Compositions according to any one of claims 1 to 5, characterized in that they contain, in addition to components A) to F) or instead of E) and / or F) also G), from 0.01% to 60% by weight with respect to the total composition, at least another flame retardant other than melamine cyanurate, the other components being reduced until the sum of all the percentages by weight is always 100.

7. Compositions according to any one of claims 1 to 6, characterized in that they contain, in addition to components A) to G) or instead of E) and / or F) and / or G) also component H), from 0.01% to 50% by weight with respect to the total composition, at least a filler other than components B) and C), the other components being reduced until the sum of all the percentages by weight is always 100. 8.Compositions according to any one of claims 1 to 7, characterized in that they contain, in addition to components A) to H) or instead of components E) and / or F) and / or G) and / or H) also K), from 0.01% to 20% by weight with respect to the total composition, at least one other additive other than components D) to H), the other components being reduced until the sum of all the percentages by weight is always 100.

9. Compositions according to any one of claims 1 to 8, characterized in that the non-fiber-formed, non-foamed ground glass to be used as component B) is particle-shaped, non-cylindrical, and has a diameter-to-thickness ratio of less than 5, preferably less than 3, and especially preferably less than 2. 10.Compositions according to any one of claims 1 to 9, characterized in that the ground glass to be used as component B) has a density in the range of 2400 to 2700 kg / m3.

11. Compositions according to any one of claims 1 to 10, characterized in that the non-foamed, non-fiber-formed ground glass to be used as component B) does not exhibit the typical glass geometry for fiber-formed glass with a cylindrical or oval cross-section having a length-to-diameter ratio (L / D ratio) greater than 5.

12. Compositions according to any one of claims 1 to 11, characterized in that component B) is based on lime-sodium bicarbonate glass, borosilicate glass, or E-glass, preferably E-glass. 13.Compositions according to claims 1 to 12, characterized in that, as component B), 5 types of glass are used in which the K2O content is less than or equal to 2% by weight with respect to all the glass components.

14. Use of the compositions according to any one of claims 1 to 13 for the manufacture of products, preferably electrical construction parts, especially preferred FI switches and 10 line protection switches, most preferably line protection switches with rated currents > 16 A, particularly preferably line protection switches with rated currents > 32 A. 15.Method for manufacturing products, preferably electrical construction parts, especially FI switches and line protection switches, most preferably line protection switches with rated currents > 16 A, particularly preferably line protection switches with rated currents > 32 A, by using the compositions according to any one of claims 1 to 13 in injection molding, extrusion processes or blow molding.