Preparation of a binder composition based on vegetable fibers and mineral fillers
Patent Information
- Application Number
- ES2017805204T
- Authority / Receiving Office
- ES · ES
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2017-11-29
- Publication Date
- 2026-11-17
- Estimated Expiration
- 2037-11-29
AI Technical Summary
Existing paper and cardboard production methods rely on chemical agents like cationic polyacrylamides and starch to improve mechanical and optical properties, but there is a need for alternatives that reduce costs and maintain or enhance these properties without compromising mechanical integrity.
A binder composition comprising refined vegetable fibers and mineral fillers, produced through mechanical refining, which coats and integrates mineral fillers within a network of lignocellulosic fibers, enhancing mechanical properties and filler retention.
The binder composition improves mechanical properties and filler retention in paper and cardboard without altering their physical characteristics, allowing for increased mineral filler levels and reduced reliance on chemical additives.
Smart Images

Figure 00000013_0000 
Figure 00000013_0001
Abstract
Description
Composition of a binder based on vegetable fibers and mineral fillers, preparation and use thereof. Field of the invention The present invention relates to a binder composition whose components may be derived primarily from mixtures of recycled materials and / or industrial waste, or even any paper stream rich in mineral fillers and cellulose fines / fibers. This binder composition is formed primarily from mineral fillers and plant-based organic materials. Hereinafter, this mixture will be referred to as the "binder composition." The field of application of the present invention relates to the production of biomaterials, composite products, and products for the paper industry. In particular, it may involve the production of paper or cardboard. Description of the previous technique Paper products, such as paper and cardboard, are prepared from aqueous suspensions of lignocellulosic fibers. They can also be prepared from recycled fibers. In addition to lignocellulosic fibers, these products generally include mineral fillers. These fillers may originate from recycling streams, particularly recycled paper pulp. So-called "recycled" mineral fillers and so-called "natural" (non-recycled) mineral fillers are introduced into production lines to modify the properties of paper or cardboard, particularly their optical and / or surface properties. These fillers also make it possible to reduce the cost of the finished product. As an example, the so-called natural mineral fillers commonly used in the paper industry include calcium carbonate, kaolin, titanium dioxide, talc, and colloidal silica. However, even in terms of surface optical properties, while natural mineral fillers provide the desired properties, recycled mineral fillers often produce altered and sometimes undesirable optical effects. Regardless of their origin, all so-called natural or recycled fibers reduce the cost of paper or cardboard and influence its mechanical and optical properties. Furthermore, given the lack of chemical affinity between mineral fillers and lignocellulosic fibers, their deliberate or uncontrolled introduction, and depending on the method of introduction, generally requires the presence of other fixing and / or retention agents such as cationic polyacrylamides, and / or binding agents, such as starch, used to improve sheet strength and filler retention. Acrylamide-based polymers and their derivatives have also been developed to improve load retention while maintaining the inherent mechanical properties of paper or cardboard, such as tear resistance, internal cohesion, and burst strength, for example. Although these solutions are satisfactory relationships, there is still a need for alternatives, more particularly an alternative to polymers and / or starch, for use in the bulk or on the surface in order to improve the physical characteristics of paper, at a lower cost. In general terms, this is the problem that the present invention solves through the development of a binder composition. This binder composition makes it possible to partially or completely replace the use of strengthening agents in the dry state (starches, amphoteric polyacrylamides, carboxymethylcellulose, and guar gums). It also makes it possible to improve retention and mineral filler levels while minimizing losses in the mechanical properties of the paper or board. Disclosure of the invention The present invention relates to a binder composition consisting mainly of water, organic plant-based materials, and mineral fillers. More specifically, the present invention relates to a binder composition containing water, vegetable fibers, and mineral fillers, - the weight ratio between vegetable fibers and mineral fillers being between 99 / 1 and 2 / 98, advantageously between 95 / 5 and 15 / 85, and even more advantageously between 80 / 20 and 20 / 80, - the vegetable fibers and mineral fillers having been refined simultaneously. The present invention also relates to a method for producing this binder composition and its use in the production of paper or cardboard. Binder composition: The binding properties of the binder composition result from its preparation, and more specifically from the refining of plant-based organic materials (plant fibers) in the presence of mineral fillers. Refining involves mechanical compression and shearing. In general, refining allows for the fibrillation and / or cutting of the plant-based organic materials. Refining also increases the specific surface area and binding strength of the plant fibers. The presence of mineral fillers during refining makes it possible to fragment the refined plant fibers, but also to coat them at least partially with the refined vegetable fibers. Therefore, in the binder composition according to the invention, the mineral fillers are at least partially bonded to each other due to the formation of a network between the refined vegetable fibers. Once coated, the mineral fillers in the binder composition can be fixed to and / or embedded within a network of lignocellulosic fibers to produce paper or board. Their integration into this type of fibrous network, with its large specific surface area, makes it possible to improve the mechanical properties and / or softness of the paper or board, whereas adding mineral fillers using conventional methods deteriorates these properties. By "coated mineral fillers" in the binder composition, the inventors refer to mineral fillers that are at least partially integrated within the rows, preferably fully integrated. Therefore, the mineral fillers are at least partially covered or surrounded by the fibers. One of the specific characteristics of binder composition is related to increasing the level of mineral fillers without altering the physical properties of the paper or board. In fact, at least some of the mineral fillers present in paper or board come from the binder composition, in which the mineral fillers are at least partially coated with vegetable fibers. The increased specific surface area of the vegetable fibers makes it possible not only to fix the mineral fillers present during refining but also to improve the retention of mineral fillers in a paper or board production process. Consequently, a binder composition refers to a composition that fixes the mineral fillers without compromising the mechanical properties of the paper or board. Plant fibers are generally lignocellulosic fibers. They can be obtained from cellulose fibers derived from lignocellulosic materials, particularly wood (hardwood or softwood) and annual plants. They can also come from the recycling of cellulosic materials. The vegetable fibers in the binder composition have an average size advantageously ranging from 10 g to 700 g. The fiber size is more advantageously between 10 g and 500 g, even more advantageously from approximately 10 g to 400 g, and still more advantageously from approximately 100 g to 400 g. This is the average size of the fibers that have been refined in the presence of mineral fillers. According to another embodiment, the vegetable fibers in the binder composition can have an average size advantageously ranging from 10 g to 600 g, and more advantageously from approximately 100 g to 600 g. In general, fibers with a size of 10 g to 80 g are referred to as fines. Size refers to the largest dimension of plant fibers, for example, length. Typically, properties such as size (length, diameter, thickness) can be obtained from conventional methods and devices, for example a MorFi Fiber Morphology analyzer. The binder composition according to the invention is a fibrous composition. This contains refined fibers but may also contain fines (i.e., fibers ranging in size from 10 gm to 80 gm) and / or fibrillated fibers. In general, the refined fibers in the binder composition include: - fibers that have been cut, these fibers may or may not be fibrillated, - fine (10-80 gm), i.e., fibers that have been cut or fibrillated fibers that have been cut. However, the fiber content of the binder composition consists primarily of refined fibers. Refined fibers include both chopped and fibrillated fibers. The weight ratio of 99:1 to 2:98 of the binder composition refers to both refined fibers and refined fillers; therefore, it refers to both chopped and fibrillated fibers. According to a specific embodiment, the binder composition may have a total percentage of fines (fibers having a size of 10-80 gm) with a length preferably greater than 30%, more preferably greater than 50%, even more preferably between 60% and 90%, and even more preferably between 70% and 90%. These percentages can be obtained from conventional methods and instruments, for example, a MorFi Fiber Morphology Analyzer, the % of fines by length. Fibers are composed of layers of microfibrils. More specifically, a fiber consists of tens or hundreds of microfibrils (generally fewer than 500 microfibrils) arranged in layers connected by lignin and / or hemicellulose. Refined fibers typically have a diameter between 10 and 60 µm, preferably between 15 and 40 µm, and a length between 10 and 700 µm, more preferably between 100 and 600 µm. Fibrillated fibers are fibers that have fibrils emerging from a main fiber nucleus. Microfibrils result from the fibrillation of fibers. They are formed by aggregates of fibrils, generally fewer than 60 fibrils. For example, documents WO 2014 / 091212 and WO 2010 / 131016 refer to the formation of microfibrils. Nanofibrils, or primary fibrils, result from the fibrillation of microfibrils. They are formed by cellulose macromolecules that are linked by hydrogen bonds. For example, documents WO 2010 / 112519 and WO 2010 / 115785 refer to the formation of nanofibrils. Typically, nanocrystalline cellulose has a width of approximately 5 nm to 50 nm and a length of approximately 100 nm to 500 nm. Nanofibrillar cellulose has a width of approximately 20 nm to 50 nm and a length of approximately 500 nm to 2000 nm. Amorphous (elliptical) nanocellulose has an average diameter of approximately 50 nm to 300 nm. (See Chamberlain D., Paper Technology Summer 2017 Micro- and Nano-Cellulose Materials - An Overview). Refining allows the fibers to be cut. It also allows the fibers to swell. Refined fibers are therefore shorter and swollen. When fiber stripping occurs during refining, the size (diameter or thickness) of the resulting strips is not drastically reduced because swelling also occurs. These two phenomena actually cancel each other out. However, refining does increase the quantity of fibers smaller than 80 µm. In summary, the refining according to the invention stimulates the cutting of the fibers with respect to the fibrillation of the fibers. The binder composition according to the invention has a percentage of fibers having an average size of 335 pm or more, which is preferably 10% or less of the total amount of fibers within the binder composition, more preferably between 1% and 10%, and even more preferably between 1% and 5%. At the end of refining, vegetable fibers have a specific surface area advantageously included between 5 m2.g-1 and 200 m2.g-1, more advantageously between 10 m2.g-1 and 100 m2.g-1. The implemented plant fibers are advantageously obtained from paper and / or cardboard recycling channels. In the binder composition, the plant fibers (recycled or not) correspond to the portion of organic material obtained from the plant that can be burned when the previously dried binder composition is subjected to a temperature of 425 °C for a period of at least 2 hours. Therefore, the burned mass corresponds to the portion of plant fiber mass. Apart from vegetable fibers, the binder composition also includes mineral fillers. In general, the invention can be implemented with any type of conventional mineral fillers. This may include natural mineral fillers, i.e., fillers not obtained from recycling. However, mineral fillers are advantageously obtained from paper and / or cardboard recycling channels. Regardless of their origin, mineral fillers can be chosen in particular from the group comprising calcium carbonate, kaolin, titanium dioxide, talc, and mixtures thereof. In the binder composition, the mineral fillers have an average size advantageously centered around 1 µm to 100 µm, and more advantageously around 10 µm to 50 µm. They can also take the form of individual fillers and / or aggregates. The average size typically refers to the largest dimension, for example, the diameter of spherical fillers or aggregates. This is the size of the fillers after refining in the presence of vegetable fibers. In the binder composition, the mineral fillers, recycled or not, correspond to the part of the mineral material not burned when the binder composition, previously dried, is subjected to a temperature of 425 °C for a period of time of at least 2 hours. In the case of vegetable fillers and / or fibers obtained from recycling, in particular recycled paper or cardboard, the same combustion test at a temperature of 425 °C for at least 2 hours can be used to determine the amount of vegetable fillers and the amount of mineral fillers contained in the recycled materials. When mineral fillers and / or plant fibers are sourced from recycling channels, they can be obtained from recycled materials and / or industrial plant waste. They can also be obtained from wastewater treatment and / or other industrial waste. In general, these compositions consist primarily of mineral fillers and / or organic matter. Therefore, the binder composition may comprise: - water, - natural (non-recycled) plant fibers and / or recycled plant fibers, and - natural mineral fillers (not recycled) and / or recycled mineral fillers. The present invention therefore makes it possible to combine vegetable fibers (recycled and / or non-recycled) and mineral fillers (recycled and / or non-recycled) into a homogeneous composition. As already indicated, the binder composition has a weight ratio of vegetable fibers / mineral fillers between 99 / 1 and 2 / 98, advantageously between 95 / 5 and 15 / 85, advantageously between 80 / 20 and 20 / 80. Advantageously, it comprises from 5 to 500 g of the mixture of vegetable fibers and mineral fillers per liter of water, more advantageously 10 g to 100 g, and even more advantageously 20 g to 50 g. According to a particular embodiment, the binder composition may also comprise at least one additive, for example, a rheology modifier or an agent for improving mechanical properties. In the binder composition, the at least one additive advantageously represents between 0 and 50% by weight of the binder composition. When present, it is in quantities of at least one additive with respect to at least a non-zero weight percentage. However, apart from any impurities, the composition according to the invention advantageously consists of water, vegetable fibers (recycled or not), and mineral fillers (recycled or not). Any impurities may originate, in particular, from the fibrous slurry used to prepare the vegetable fibers of the binder composition. When present, the impurities preferably amount to less than 10% by weight of the binder composition, preferably less than 5% by weight, and more preferably less than 1% by weight. The amount of impurities can be measured according to conventional methods, for example, with a Somerville sieve having a standard mesh size of 0.15 mm. The impurities may include plastics...The binder composition according to the invention corresponds to a composition with a homogeneous distribution of its components in the volume, the refining making it possible to fragment the mineral fillers and, at least partially, coat them in the vegetable fibers. The binder composition has a Brookfield viscosity that preferably ranges from 500 cps to 20000 cps, more preferably from 800 cps to 12000 cps. The Brookfield viscosity of the binder composition can be measured using a Brookfield viscometer at 25 °C with an LV module. A person experienced in this task will be able to determine the appropriate module and speed (Brookfield viscometer, LV module) for the viscosity range to be measured. The Brookfield viscosity is preferably measured after 100 seconds at 100 rpm. The binder composition is generally thixotropic. In other words, its viscosity decreases after shearing and returns to its original viscosity or increases over time once shearing ceases. Method for preparing the binder composition: The present invention also relates to the method for preparing the binder composition. As already indicated, the properties of the binder composition result from the refining of vegetable fibers in the presence of mineral fillers. This method comprises the following stages: - preparing a suspension of vegetable fibers and mineral fillers in water, the weight ratio between the vegetable fibers and the mineral fillers being between 99 / 1 and 2 / 98, advantageously between 95 / 5 and 15 / 85, most advantageously between 80 / 20 and 20 / 80, - refine this suspension. Refining cannot be compared to a milling or fibrillation process. The applicants have compared a commercially available mixture resulting from the milling of cellulose and mineral fillers. Various experiments conducted by the applicants (see the "Examples" section below) show that milling the composition according to the invention provides improved strength properties. Without wishing to be bound by theory, the Applicants consider that these improvements are due to the fact that the refining stage increases the fiber cut. Unlike a milling stage, it does not stimulate fiber fibrillation, although some fibrillation may occur. Furthermore, fibrillation according to the invention provides a homogeneous size distribution, whereas fibrillation processes such as milling result in a diverse size distribution. Finally, unlike milling, refining according to the invention provides mineral fillers coated with or integrated within the refined fibers. Refining produces fibers that have been cut. Refined fibers consist primarily of fibers that have been shortened in length. Refining does not involve fibrillation, as its purpose is not to separate the fibers into microfibrils or nanofibrils. However, as already mentioned, some fibrillation can occur. In fact, small quantities of fibers may be partially or fully fibrillated. Additionally, refining can produce swollen fibers (the refining stage is carried out in the presence of water). Refining is generally performed between two parallel refiner discs with a fixed distance between them, typically between a rotating disc and a stationary disc.Refining can also be carried out using a series of parallel disc pairs, preferably a series of several disc pairs (26 pairs, for example), which can have the same inter-disc spacing or a decreasing inter-disc spacing. For example, these discs can be made of steel or stainless steel. Refiner discs typically consist of bars and grooves. A person experienced in this area will be able to select the appropriate discs that will stimulate shearing with respect to fiber fibrillation. Milling involves shearing / breaking and crushing of the fibers. The shearing / breaking in a milling process is significantly greater than in a refining process. More specifically, in a milling process, the fibers are subjected to abrasion as they are immobilized and pressed against a milling medium or a milling disc (discs with protruding milled pieces). As a result, the fibers are separated into individual fibers that are then crushed. On the other hand, refining peels and cuts the fibers. Fibrillation or nanofibrillation produces fibrils, that is, the separation of fibers into smaller fibrils. However, such a process does not necessarily involve a reduction in fiber length. Therefore, it differs from refining. Nanofibrils can be prepared by ultrafine milling. Typically, an ultrafine mill comprises ceramic discs separated by a distance that depends on the composition of the feed rows. The distance between the two discs changes during the milling process. As a result, the fibrillated fibers generally have a greater length than the refined fibers. Furthermore, according to the invention, the refining is preferably carried out in the absence of any grinding media such as beads, balls, or granules of any hard material such as ceramic or metal. Before refining, this method may also include a fractionation step and / or an enzymatic treatment step. Therefore, the method may comprise the following sequence: a) preparation of a suspension of vegetable fibers and mineral fillers in water, b) optionally, splitting of this suspension, c) optionally, enzymatic treatment of this suspension, d) refining of this suspension. a) Preparation of a suspension of vegetable fibers and mineral fillers in water The suspension of vegetable fibers and mineral fillers in water according to the invention can be prepared from recycled or non-recycled vegetable fibers and recycled or non-recycled mineral fillers. Therefore, it can be derived at least partially from recycled materials, for example, materials obtained from the recycling of paper or cardboard. Based on the nature of the recycled materials, non-recycled vegetable fibers and / or non-recycled mineral fillers can be added to achieve the desired vegetable fiber / mineral filler weight ratio. As previously stated, the plant fibers and / or mineral fillers may originate from recycled materials and / or industrial waste. For example, they may come from wastewater from papermaking, particularly from sewage treatment or sewage effluent, and / or other industrial waste, and / or a fast-flow filter cake from a paper machine. In general, the suspension of vegetable fibers (fibrous suspension) generally comprises 5 to 500 g of binder composition components per liter of water, more advantageously 10 to 100 g, and even more advantageously 20 to 50 g. Recycled materials are generally subjected to pre-treatments making it possible to isolate, during recycling processes, fractions enriched with recycled mineral fillers and vegetable fibers that have an average size generally less than 2000 gm. Consequently, in aqueous suspension, the vegetable fibers have an average size advantageously less than 5000 gm, more advantageously less than 2000 gm, more advantageously less than 1000 gm, and even more advantageously less than 800 gm. Any addition of mineral fillers can be carried out before and / or after the fractionation stage. It can also be carried out before and / or after the enzymatic processing stage. Therefore, the optional stages (fractionation and enzymatic treatment) can be performed in the absence of mineral fillers. Only the refining stage is necessarily carried out in the presence of vegetable fibers and mineral fillers. b) Optional installment plan The fractionation stage is optionally performed before refining, if applicable, before enzymatic treatment. The fractionation of the vegetable fiber suspension makes it possible to enrich the suspension with short vegetable fibers having an average size advantageously less than 2000 gm, more advantageously less than 1000 gm, and even more advantageously less than 800 gm, if applicable. That is, when the fiber suspension comprises mineral fillers, the fractionation can also enrich the suspension with mineral fillers. Therefore, compared to a fiber suspension not enriched by fractionation, the suspension enriched with short vegetable fibers and / or mineral fillers makes it possible to facilitate the coating of the mineral fillers and, consequently, the production of the binder composition with less energy. Fractionation can be performed using conventional techniques, in particular by sieving with slits and / or holes and / or hydrocyclone and / or thickener washer. At the end of the fractionation process, mineral fillers can be optionally added to the vegetable fiber suspension. Unfractionated vegetable fibers can also be added, these having an advantageous average size of less than 5000 g / cm². c) Optional enzymatic treatment According to a particular embodiment, the vegetable fibers can be subjected to enzymatic treatment before the refining stage. This treatment is advantageously performed after a fractionation stage. Therefore, according to a preferred embodiment, the method for preparing the binder composition comprises the following steps: - fractionation of a suspension of recycled or non-recycled fibers which may also include recycled or non-recycled mineral fillers, - optionally, add recycled or non-recycled mineral fillers and / or industrial waste to the resulting fractionation slurry, - enzymatic treatment of this suspension, - Optionally, add recycled or non-recycled mineral fillers and / or industrial waste to this suspension, - refine this suspension of vegetable fibers and mineral fillers. Enzymatic treatment can be carried out with or without the presence of mineral fillers. In fact, mineral fillers can be introduced before enzymatic treatment, or between enzymatic treatment and refining. Enzymatic treatment is advantageously carried out in the presence of a mixture of enzymes, and before refining. These enzymes are capable of breaking down at least one of the components of plant fibers, namely lignin, cellulose, and / or hemicellulose. In general, these enzymes can make plant fibers brittle by altering their components. The person with experience in the subject will know how to choose the appropriate enzymes as well as the treatment conditions based on the above. The enzyme activity can be stopped by exposing the suspension to steam. At the end of the enzymatic treatment, mineral fillers can optionally be added to the plant fiber suspension. Plant fibers that have not been enzymatically treated can also be added. d) Refining of vegetable fibers in the presence of mineral fillers As already mentioned, the refining of plant fibers is carried out in the presence of mineral fillers. This makes it possible to increase the specific surface area of the plant fibers and to at least partially coat the mineral fillers with the plant fibers. Advantageously, refining does not alter the concentration of the suspension in terms of vegetable fibers and mineral fillers. Therefore, the quantity of each component of the binder composition is advantageously determined just before refining. Refining is advantageously carried out after a fractionation stage and / or an enzymatic treatment stage. Before refining, mineral fillers are generally in the form of filler clumps. Furthermore, the mineral filler clumps obtained from recycling typically have a size, at the coarsest size value, ranging from 400 µm to 1000 µm, which is unsuitable for immediate use in paper production without negative consequences. In general, refining a fibrous suspension makes it possible to compress and shear the plant fibers. In this case, refining also makes it possible to reduce the size of the mineral fillers, particularly by breaking down the mineral filler aggregates. Simultaneous refining of the fibers and fillers also serves to coat, or integrate, the fillers at least partially with the fibers during the process of producing the binder composition. Refining makes it possible to fragment the mineral charges (or aggregates). At the end of refining, the recycled mineral charges (or aggregates) have generally experienced an increase by a factor of at least 1.5 to 30 with respect to their initial specific surface area, preferably at least 5 and possibly approximately 10. In other words, refining increases the specific surface area of the recycled mineral charges. Mineral fillers, refined and at least partially coated with vegetable fibers, then have an average size advantageously centered from approximately 1 pm to 100 pm, more advantageously from approximately 10 pm to 50 pm. Generally, the average size can be centered from approximately 1 pm to 10 pm. They can also take the form of unit fillers and / or groupings of unit fillers. Size refers to the largest dimension of the loads or groupings after the refining stage, for example the diameter for spherical loads or groupings. Therefore, this method is particularly suitable for the use of products obtained from recycled paper or cardboard, which until now might have been considered undesirable due to the potential presence of mineral fillers and fine cellulose elements. As already mentioned, at the end of refining, the refined fibers have an advantageous length-weighted average between 10 pm and 700 pm, most advantageously between 10 pm and 500 pm, and even more advantageously from approximately 100 pm to 400 pm. According to another embodiment, the vegetable fibers of the binder composition can have an advantageous length-weighted average between 100 pm and 600 pm, most advantageously from approximately 100 pm to 600 pm. In general, fibers with a size of 10 pm to 80 pm are referred to as fines. According to the knowledge of a person experienced in the subject, the length-weighted average length is preferably obtained from the following formula in which "n" is an individual fiber and "1" is the length of an individual fiber: Furthermore, at the end of the refining stage, the binder composition has a concentration that has a dry content (vegetable fibers + mineral fillers) advantageously between 5 and 500 g per liter of water, more advantageously from approximately 10 to 100 g per liter of water, and even more advantageously from 20 to 50 g per liter of water. As already mentioned, refining is generally carried out between two parallel refiner discs spaced at a fixed distance. According to a preferred embodiment of the invention, the aqueous suspension of vegetable fibers and mineral fillers to be refined is preferably passed between the discs one or more times. Refining is normally stopped after 10 to 80 passes through the refiner discs, more preferably 10 to 60 passes, and even more preferably 15 to 40 passes. The method according to the invention has a total energy input of between 200 and 2000 kW.h per ton of vegetable fibers and mineral fillers, more preferably between 300 and 900 kW.h per ton, even more preferably between 400 and 700 kW.h per ton. According to the invention, refining preferably refers to the development of the aqueous suspension of vegetable fibers and mineral fillers to be refined between refiner discs, for example, between two refiner discs. The indefinite development of the suspension is not necessary once the refining reaches a certain threshold. Furthermore, it does not occur during refining because most of the fibers are preferably never fibrillated. After the refining stage, the binder composition can be concentrated, for example, the water can be partially evaporated. Use of the binder composition: The present invention also relates to the use of the binder composition in a method for producing paper or cardboard, as well as a method for paper or cardboard. This binder composition can be used, for example, in methods for producing paper and / or cardboard, and / or for producing biomaterials and / or composite materials. In fact, it makes it possible to improve the bond between plant fibers, fix mineral fillers in the finished product, and contribute to the improvement of mechanical properties. When binder composition is used as an additive in a conventional paper or board production process, it is advantageously introduced into the diluted pulp, for example, in the feed box and / or a layered feed box. The amount of binder composition introduced then advantageously represents 0.5 to 10% by weight of the fiber suspension mass. The binder composition is also applied to paper or cardboard that has already been formed. This involves a surface treatment in which the binder composition is advantageously applied by spray bars and / or surface application, for example, in coating or sizing. This binder composition makes it possible to contribute to the mechanical properties of internal cohesion, tensile strength, burst strength, compressive strength, etc. and / or softness and / or reduced permeability and / or improved load retention, without hindering the drainage capacity process during paper or cardboard formation. Given its properties, the binder composition according to the invention can be used to prepare any type of paper or cardboard. Therefore, it can be incorporated into a specific layer of a laminate (lamination process for heterogeneous layers). Tania can be used to increase the amount of mineral fillers in printing and writing papers and / or sanitary or household papers (paper towels, tissues, toilet paper, napkins, etc.). The invention and its advantages will become more evident to someone with experience in the subject from the figures and examples that follow. Brief description of the figures Figure 1 shows the fiber length distribution of the binder composition according to the invention with respect to a composition obtained by milling (area-weighted fiber length). Figure 2 shows average fiber lengths of the binder composition according to the invention with respect to a composition obtained by milling. Examples The binder composition according to the invention (GP) has been compared to a composition resulting from the milling of fibers in the presence of mineral fillers (CE). 1 / Preparation of the composition according to the invention Vegetable fibers are treated as follows in the presence of mineral fillers: - Preparation of a cellulose pulp (Helico pulp extractor): 160 kg of vegetable fibers + 1300 liters of water at 63 °C for 15 minutes, - Enzymatic treatment in a bioreactor: or 30 minutes at 50 °C, or Filtration (Buchner) (% retention of C = 4.96%) , - Refined (40.6 cm (16 inches)) for 180 minutes, with an overall specific energy of 600 kWh per tonne of fibers and loads. Table 1 summarizes the different treatments carried out in order to prepare the compositions of GP0, GP2 and GP3 (softwood + simultaneously refined CaCÜ3). T l 1: niinrrrrlmiinrnl inv nin P P2 P . GP0, GP2, and GP3 have a mineral loading of 2.00, 18.60, and 45.40% by weight, respectively, with respect to the dry weight of the GP compositions. The amount of mineral loading corresponds to the ash content after treatment of the composition at 425 °C. 2 / Counter-example (CE) The composition according to the invention has been compared to a composition (CE) comprising fibers and mineral fillers that have been ground simultaneously. The composition of CE comprises softwood fibers and mineral fillers of CaC₅H₁₂O₅. It has an ash content of 53.6% by weight at 425°C. 3 / Properties of GP compositions with respect to EC The size distribution of GP (refined) compositions has been compared with the composition of CE resulting from a milling process. These analyses were performed using a MorFi instrument (Techpap). Only fibers and loads with a size of at least 80 pm were considered. According to the initial figure 1 (area-weighted fiber length), the GP0 composition has a narrow size distribution starting at approximately 174 pm. Less than 15% of GP0 fibers are 335 pm or larger. The composition according to the CE counter-example has 30% of its fibers being 335 pm or more. The size distribution of the GP composition is therefore definitely more homogeneous than that of the CE composition, as also demonstrated by the various length measurements (see Figure 2). Figure 2 shows the average fiber lengths of the binder composition according to the invention compared to a composition obtained by milling. The arithmetic mean fiber length (L(n)), the length-weighted mean fiber length (L(l)), and the area-weighted mean fiber length (L(w)) are calculated respectively according to the following formulas: 4 / Paper manufacturing involving compositions according to the invention and the composition of CE Paper sheets (90 g / m2) were formed using a dynamic sheet former. 5% by weight (dry weight) of a GP or CE composition (see "Composition Added" line in Table 2) was added to a paper pulp containing vegetable fibers (softwood) that had been refined to 250SR (see "Starting Pulp" line in Table 2). Additional mineral loads were added as shown in Table 2 in order to reach a total of 15% by weight (see lines "CaCÜ3 added" and "CaCÜ3 total" in Table 2). - Paper sheets prepared from GP compositions have higher filler retention than those from CE compositions (see the "Ash Retention" line). Refined fibers incorporating refined fillers (GP2 and GP3 compositions) also enhance the retention of added fillers. The filler content ranges from 5.1% (CE) to 11.9% (GP2). As shown in the examples for CE and GP0 (similar ash content), the amount of mineral fillers can dramatically change the properties of the paper sheet. In fact, GP0 provides an 8% improvement in the Tensile Strength (65.3 vs. 60.5), a 22% improvement in TEA (Tensile Energy Absorption; 0.263 vs. 0.215), and a 27% improvement in Scott Bond Strength (bonding strength, 490.4 vs. 385.9). In light of the foregoing, the composition according to the invention clearly provides improved properties compared to prior art compositions resulting from the milling of vegetable fibers in the presence of mineral fillers. It also improves filler retention.
Claims
CLAIMS 1. A binder composition containing water, vegetable fibers and mineral fillers, - vegetable fibers and mineral fillers having a weight ratio between 99 / 1 and 2 / 98, - the vegetable fibers and mineral fillers having been refined simultaneously, in which the refined fibers have an average size between 10 and 700 pm, and in which the refined fibers, at least partially, integrate the refined mineral fillers.
2. The binder composition according to claim 1, characterized in that the composition has a weight ratio of vegetable fibers / mineral fillers between 95 / 5 and 15 / 85, advantageously between 80 / 20 and 20 / 80.
3. The binder composition according to claim 1 or 2, characterized in that the composition is formed by water, vegetable fibers and mineral fillers.
4. The binder composition according to any one of claims 1 to 3, characterized in that the mineral fillers are selected from the group comprising calcium carbonate, kaolin, titanium dioxide, talc, and mixtures thereof.
5. The binder composition according to any one of claims 1 to 4, characterized in that the mineral fillers and / or vegetable fibers are obtained from recycled paper or cardboard channels.
6. The binder composition according to any one of claims 1 to 4, characterized in that the percentage of fibers having an average size of 335 pm or more is 10% or less of the total amount of fibers within the binder composition, preferably between 1% and 10%, more preferably between 1% and 5%.
7. A use of the composition according to any one of claims 1 to 6 in a process for producing paper or cardboard.
8. A method for preparing the composition according to any one of claims 1 to 6, comprising the following steps: - to prepare a suspension of vegetable fibers and mineral fillers in water, the weight ratio between the vegetable fibers and the mineral fillers being between 99 / 1 and 2 / 98, advantageously between 95 / 5 and 15 / 85, - refine this suspension.
9. The method according to claim 8, characterized in that the vegetable fibers are treated enzymatically before the refining stage.
10. The method according to claim 9, characterized in that mineral fillers are introduced prior to enzymatic treatment.
11. The method according to any one of claims 9 to 10, characterized in that mineral fillers are introduced between the enzymatic treatment and the refining.
12. The method according to any one of claims 9 to 11, characterized in that the method has a total energy input of between 200 and 2000 kWh per tonne of vegetable fibers and mineral fillers, preferably between 300 and 900 kWh per tonne, more preferably between 400 and 700 kWh per tonne.
13. The method according to any one of claims 8 to 12, characterized in that it comprises a fractionation stage prior to refining.
14. The method according to any one of claims 9 to 13, characterized in that it comprises a fractionation step followed by an enzymatic treatment step, prior to refining.