Modified iron phosphate precursor, modified lithium iron phosphate and method of preparation thereof
Patent Information
- Application Number
- ES2023090206
- Authority / Receiving Office
- ES · ES
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2022-05-26
- Filing Date
- 2023-03-20
- Publication Date
- 2026-11-19
- Estimated Expiration
- 2043-03-20
AI Technical Summary
The conductivity of lithium-ion batteries using lithium iron phosphate as the positive electrode material is poor, limiting their application and industrialization due to the structural limitations of lithium iron phosphate.
A modified iron phosphate precursor is prepared by dissolving a soluble ferric salt in a niobium diselenide suspension, reacting with a phosphoric acid source, and then mixing with a lithium source and carbon source to form a modified lithium iron phosphate, which is doped with niobium diselenide to enhance conductivity.
The modified lithium iron phosphate exhibits improved conductivity, with resistivity reduced to less than 186 Ω·m, and increased lithium intercalation, enhancing first charging efficiency and structural stability.
Smart Images

Figure 00000017_0000
Abstract
Description
Modified iron phosphate precursor, modified lithium iron phosphate and method of preparation thereof Field of invention This disclosure relates to the field of battery materials, and in particular to a modified iron phosphate precursor, a modified lithium iron phosphate, and a method for preparing them. Background of the invention The problem of energy scarcity and environmental issues is becoming increasingly severe. The petrochemical energy used at this stage will also be used in the future. To maintain the sustainable development of human society, energy and the environment are two critical problems that must be addressed in the 21st century. The development of clean and renewable energy is one of the most crucial technologies for the future global economy. As a high-performance secondary green battery, the lithium-ion battery has advantages such as high voltage, high energy density, low self-discharge rate, wide operating temperature range, long cycle life, environmental friendliness, no memory effect, and high-current charge and discharge capacity, making it the most promising energy battery in the coming years.However, one of the bottlenecks restricting the large-scale industrialization of lithium-ion batteries is the positive electrode material. Given that lithium-ion batteries must have the aforementioned stability, price and resource issues are also significant factors that cannot be ignored. Lithium iron phosphate is an electrode material for lithium-ion batteries, with the chemical formula LiFePO4 (LFP for short). It is primarily used in various lithium-ion batteries. Due to its advantages such as low cost, non-polluting properties, abundant resources, and good thermal stability, lithium iron phosphate has become one of the most promising positive electrode materials today and is a focus of research, production, and development in the field of energy storage lithium-ion batteries. However, due to the limitations of the structure of lithium iron phosphate itself, the conductivity of lithium-ion batteries that use lithium iron phosphate as the positive electrode material is poor, which greatly limits their application. Brief description of the invention The present disclosure aims to address at least one of the technical problems existing in the prior art. For this reason, this disclosure provides a modified iron phosphate precursor, a modified lithium iron phosphate, and a method for preparing the same. The modified iron phosphate precursor provided herein can effectively absorb a lithium source, thereby significantly improving the conductivity of the lithium iron phosphate. In order to resolve the aforementioned technical problems, this disclosure offers the following technical solutions: In the first aspect, a modified iron phosphate precursor is provided. The modified iron phosphate precursor is prepared by dissolving the soluble ferric salt in a niobium diselenide suspension and reacting the mixture with a phosphoric acid source. In the niobium diselenide suspension of this disclosure, the niobium diselenide can be uniformly and stably dispersed in the suspension; specifically, a dispersant or dispersion solution can be added during the preparation of the suspension to stably suspend the niobium diselenide. In this disclosure, the soluble ferric salt is the ferric salt commonly used in the technique, preferably at least one of ferric sulfate and ferric nitrate; the source of phosphoric acid is at least one of phosphoric acid and ammonium phosphate. Preferably, after adding the phosphoric acid source, the pH of the niobium diselenide suspension is 1.8-2.2, more preferably 2.0-2.2. Preferably, after adding the phosphoric acid source, the mixture is heated to 60-80 °C to react for 2-4 h; more preferably, it is heated to 70-80 °C to react for 2-3 h. In this disclosure, ferric ions are first uniformly distributed in the niobium diselenide dispersion system and then added with a phosphoric acid source to synthesize an iron phosphate precursor in situ, resulting in an iron phosphate uniformly doped with niobium diselenide. Due to the metallic nature of niobium diselenide, it exhibits excellent superconductivity, with a resistivity of approximately 3.5 x 10⁻⁴ Ω·cm. Doping lithium iron phosphate with niobium diselenide in the amount described herein can significantly improve the conductivity of the lithium iron phosphate, reducing its resistivity to less than 186 Ω·m, without affecting its structural stability. Furthermore, in the modified iron phosphate precursor, the molar ratio of the soluble ferric salt to niobium diselenide is 1:0.05-0.15, preferably 1:0.1-0.15; The molar ratio of the element phosphorus in the phosphoric acid source to the element iron in the soluble ferric salt is 1.4-1.6:1, preferably 1.5-1.6:1. Additionally, the niobium diselenide suspension is prepared by adding niobium diselenide to a dispersion solution for dispersion. In the process of preparing the niobium diselenide suspension, the stirring and wetting and / or ultrasonication method can be used to accelerate the dissolution rate of the niobium diselenide or to dissolve it completely. Preferably, in the present disclosure, the niobium diselenide suspension is obtained by adding the niobium diselenide to a dispersion solution, stirring and wetting, and then by ultrasonic dispersion. The dispersion solution is an aqueous solution of polyvinylpyrrolidone; preferably, the concentration of polyvinylpyrrolidone in the dispersion solution is 0.4% by weight - 1% by weight, more preferably 0.8% by weight - 1% by weight. The solid content of the niobium diselenide suspension is 0.1% - 0.5%; preferably 0.3% - 0.5%. Preferably, the stirring condition is stirring at a rotation speed of 100-200 rpm for 10-15 minutes, and the ultrasonic condition is dispersing by ultrasound at 15-20 KHz for 10-20 minutes. More preferably, the stirring condition is stirring at a rotation speed of 150-200 rpm for 10-12 minutes, and the ultrasonic condition is dispersing by ultrasound at 16-20 KHz for 10-15 minutes. In a second aspect, a modified lithium iron phosphate is provided, wherein the modified lithium iron phosphate comprises a lithium source and the modified iron phosphate precursor according to the first aspect. The lithium from the lithium carbonate will intercalate into the iron phosphate network to form a modified lithium iron phosphate. In this disclosure, since the diffusion barrier of niobium diselenide to lithium is small, lithium can be adsorbed onto the surface of the niobium diselenide, thus increasing the amount of lithium intercalated in the positive electrode material. This allows for the pre-supplementation of lithium during the synthesis process of the positive electrode material. Furthermore, if an excess of lithium is stored in the positive electrode material, it can be released during the first charging process. The lithium ions disintercalated by the positive electrode can be retained to a greater extent, thus improving the first charging efficiency. In addition, the lithium source is lithium carbonate, lithium hydroxide, lithium acetate or lithium bromide; preferably lithium hydroxide or lithium carbonate. In a third aspect, a method is provided for preparing the modified lithium iron phosphate according to the second aspect, the method comprising the following steps: mix a lithium source, a carbon source and the modified iron phosphate precursor under a protective atmosphere, and sinter the mixture to obtain the modified lithium iron phosphate. In this disclosure, the protective atmosphere is a nitrogen atmosphere or an argon atmosphere. Furthermore, the molar ratio of the modified iron phosphate precursor, the lithium source, and the carbon source is 1:1, 1-1, 2:0, 1-0, 3; preferably 1:1, 1-1, 2:0, 2-0, 3. In addition, the carbon source is at least one of glucose, lactose, and sucrose; the sintering temperature is 550-650 °C, preferably 600-650 °C; the sintering duration is 6-8 h, preferably 6-7 h. As a preferred technical solution, the method for preparing the modified lithium iron phosphate of this disclosure comprises the following steps: 51. Preparation of the niobium diselenide suspension: Add the niobium diselenide to a dispersion solution, stir and wet, and then ultrasonically disperse the mixture uniformly to obtain a niobium diselenide suspension with a solid content of 0.1% - 0.5%; wherein the dispersion solution is a deionized aqueous solution of polyvinylpyrrolidone, and the concentration of polyvinylpyrrolidone is 0.4% by weight - 1% by weight; 52. Preparation of modified iron phosphate precursor: Add a soluble ferric salt to the niobium diselenide suspension of S1, stir the mixture to dissolve, and add the phosphoric acid source while stirring, control the mixture to a pH of 1.8-2.2, and heat to 60-80 °C to react for 2-4 h to synthesize iron phosphate in situ, perform solid-liquid separation to obtain the modified iron phosphate precursor, wherein preferably, sodium hydroxide or hydrochloric acid is used to adjust the pH in this step; 53. Preparation of modified lithium iron phosphate: In a nitrogen atmosphere or an inert atmosphere, mix the S2 modified iron phosphate precursor, a lithium source and a carbon source, and sinter the mixture to obtain the modified lithium iron phosphate, wherein preferably, the inert atmosphere is an argon atmosphere. In a fourth aspect, a lithium battery is provided, the lithium battery comprising the modified lithium iron phosphate according to the second aspect. Compared to the previous technique, the present disclosure has at least the following beneficial effects: (1) In the modified method for preparing lithium iron phosphate described herein, ferric ions are first uniformly distributed in the niobium diselenide dispersion system, and then phosphoric acid is added to synthesize an iron phosphate precursor in situ, so that a ferric phosphate uniformly doped with niobium diselenide can be obtained, and a lithium iron phosphate uniformly doped with niobium diselenide is obtained. Due to the metallic nature of niobium diselenide, it has excellent superconductivity, and its resistivity is approximately 3.5 x 10⁻⁴ Ω·cm.Doping lithium iron phosphate with niobium diselenide in an amount according to the present disclosure can significantly improve the conductivity of lithium iron phosphate, so that the resistivity of lithium iron phosphate is less than 186 Q^m, and the structural stability of lithium iron phosphate would not be affected. (2) In the modified lithium iron phosphate preparation method described herein, since the diffusion barrier of niobium diselenide to lithium is small, during the sintering process, lithium can be adsorbed onto the surface of the niobium diselenide, thus increasing the amount of lithium intercalated in the positive electrode material. This allows for the pre-supplementation of lithium, thereby achieving pre-supplementation during the synthesis of the positive electrode material. Furthermore, if an excess amount of lithium is stored in the positive electrode material, this excess lithium can be released during the first charging process. The lithium ions disintercalated by the positive electrode can be retained to a greater extent, thus improving the first charging efficiency. (3) In the method for preparing the modified lithium iron phosphate of the present disclosure, due to the high surface energy of the niobium diselenide particles, the particles are prone to agglomeration, resulting in sedimentation. In the present disclosure, the niobium diselenide can be added to the dispersion solution containing polyvinylpyrrolidone for dispersion. This effectively reduces the surface energy of the niobium diselenide, thus maintaining a stable dispersion state.On the other hand, the stability of niobium diselenide in air is poor, but polyvinylpyrrolidone has film-forming properties, which can create a protective surface encapsulation effect on niobium diselenide, improving its stability. The polyvinylpyrrolidone can then be removed in the subsequent sintering process. Furthermore, polyvinylpyrrolidone is reducible, which can further enhance the reduction effect of ferric iron. Additionally, polyvinylpyrrolidone can promote the uniform distribution of ferric ions in the dispersion system, thus improving the uniformity of doping of niobium diselenide in the positive electrode material. Brief description of the drawings FIGURE 1 is an SEM image of the modified lithium iron phosphate from Example 1 of this disclosure. Detailed description of the invention This disclosure will be described later together with specific embodiments, in which the raw materials used in the examples and comparative examples can be obtained through commercially available channels, and are used in parallel experiments. Example 1: The present example provides a modified lithium iron phosphate; the method for preparing the modified lithium iron phosphate comprises the following steps: S1. Preparation of the niobium diselenide suspension: Niobium diselenide was added to a dispersion solution, and the mixture was stirred and moistened (stirred at 100 rpm for 15 minutes) and then ultrasonically dispersed uniformly (ultrasonicated at 15 KHz for 20 minutes) to obtain a niobium diselenide suspension with a solid content of 0.1%; wherein the dispersion solution was a deionized aqueous solution of polyvinylpyrrolidone, and the concentration of polyvinylpyrrolidone was 0.4% by weight; 52. Preparation of modified iron phosphate precursor: Ferric sulfate was added to the niobium diselenide suspension prepared by S1, so that the molar ratio of ferric sulfate to niobium diselenide was 1:0.05. The mixture was stirred and dissolved, and phosphoric acid was added while stirring so that the molar ratio of phosphorus:iron = 1.4:1. The mixture was controlled at a pH of 1.8 (the pH was adjusted with sodium hydroxide or hydrochloric acid), and heated to 60 °C to react for 4 h to synthesize iron phosphate in situ. The resulting product was subjected to solid-liquid separation to obtain the modified precursor of iron phosphate. 53. Preparation of modified lithium iron phosphate: In a nitrogen atmosphere, the S2-modified iron phosphate precursor, lithium carbonate, and sucrose were mixed, such that the molar ratio of the modified iron phosphate precursor, lithium carbonate, and sucrose was 1:1, 1:0, 1. The mixture was sintered at 550 °C for 8 h to obtain the modified lithium iron phosphate. The scanning electron microscope image of the appearance of the modified lithium iron phosphate particles prepared in Example 1 is shown in FIGURE 1. Example 2: The present example provides a modified lithium iron phosphate; the method for preparing the modified lithium iron phosphate comprises the following steps: 51. Preparation of the niobium diselenide suspension: Niobium diselenide was added to a dispersion solution, and the mixture was stirred and moistened (stirred at 200 rpm for 10 minutes) and then ultrasonically dispersed uniformly (ultrasonicated at 20 KHz for 10 minutes) to obtain a niobium diselenide suspension with a solid content of 0.3%; wherein the dispersion solution was a deionized aqueous solution of polyvinylpyrrolidone, and the concentration of polyvinylpyrrolidone was 0.8% by weight; 52. Preparation of modified iron phosphate precursor: Ferric nitrate was added to the niobium diselenide suspension prepared by S1, so that the molar ratio of ferric nitrate to niobium diselenide was 1:0.1. The mixture was stirred and dissolved, and phosphoric acid was added while stirring so that the molar ratio of phosphorus:iron = 1.5:1. The mixture was controlled at a pH of 2.2 (the pH was adjusted with sodium hydroxide or hydrochloric acid), and heated to 70 °C to react for 3 h to synthesize iron phosphate in situ. The resulting product was subjected to solid-liquid separation to obtain the modified precursor of iron phosphate. S3. Preparation of modified lithium iron phosphate: In a nitrogen atmosphere, the S2-modified iron phosphate precursor, lithium carbonate, and sucrose were mixed, such that the molar ratio of the modified iron phosphate precursor, lithium carbonate, and sucrose was 1:1, 1:0, 2. The mixture was sintered at 650 °C for 6 h to obtain the modified lithium iron phosphate. Example 3: The present example provides a modified lithium iron phosphate; the method for preparing the modified lithium iron phosphate comprises the following steps: 51. Preparation of the niobium diselenide suspension: Niobium diselenide was added to a dispersion solution, and the mixture was stirred and moistened (stirred at 150 rpm for 12 minutes) and then ultrasonically dispersed uniformly (ultrasonicated at 16 KHz for 15 minutes) to obtain a niobium diselenide suspension with a solid content of 0.5%; wherein the dispersion solution was a deionized aqueous solution of polyvinylpyrrolidone, and the concentration of polyvinylpyrrolidone was 1% by weight; 52. Preparation of modified iron phosphate precursor: Ferric sulfate was added to the niobium diselenide suspension prepared by S1, so that the molar ratio of ferric sulfate to niobium diselenide was 1:0.15. The mixture was stirred and dissolved, and ammonium phosphate was added while stirring so that the molar ratio of phosphorus:iron = 1.6:1. The mixture was controlled at a pH of 2.0 (the pH was adjusted with sodium hydroxide or hydrochloric acid), and heated to 80 °C to react for 2 h to synthesize iron phosphate in situ. The resulting product was subjected to solid-liquid separation to obtain the modified precursor of iron phosphate. S3. Preparation of modified lithium iron phosphate: In a nitrogen atmosphere, the S2-modified iron phosphate precursor, lithium carbonate, and sucrose were mixed, such that the molar ratio of the modified iron phosphate precursor, lithium carbonate, and sucrose was 1:1, 2:0, 3. The mixture was sintered at 650 °C for 6 h to obtain the modified lithium iron phosphate. Example 4: The present example provides a modified lithium iron phosphate; the method for preparing the modified lithium iron phosphate comprises the following steps: 51. Preparation of the niobium diselenide suspension: Niobium diselenide was added to deionized water, and the mixture was stirred and moistened (stirred at 150 rpm for 12 minutes) and then ultrasonically dispersed evenly (ultrasonically dispersed at 16 KHz for 15 minutes) to obtain a niobium diselenide suspension with a solid content of 0.5%; 52. Preparation of modified iron phosphate precursor: Ferric sulfate was added to the niobium diselenide suspension prepared by S1, so that the molar ratio of ferric sulfate to niobium diselenide was 1:0.15. The mixture was stirred and dissolved, and ammonium phosphate was added while stirring so that the molar ratio of phosphorus:iron = 1.6:1. The mixture was controlled at a pH of 2.0 (the pH was adjusted with sodium hydroxide or hydrochloric acid), and heated to 80 °C to react for 2 h to synthesize iron phosphate in situ. The resulting product was subjected to solid-liquid separation to obtain the modified precursor of iron phosphate. 53. Preparation of modified lithium iron phosphate: In a nitrogen atmosphere, the S2-modified iron phosphate precursor, lithium carbonate, and sucrose were mixed, such that the molar ratio of the modified iron phosphate precursor, lithium carbonate, and sucrose was 1:1, 2:0, 3. The mixture was sintered at 650 °C for 6 h to obtain the modified lithium iron phosphate. Comparative example 1: (In comparison to example 3, no niobium diselenide was doped) In the present comparative example, a modified lithium iron phosphate is provided; the method for preparing the lithium iron phosphate comprises the following steps: 51. Preparation of an aqueous solution of polyvinylpyrrolidone; A deionized aqueous solution of polyvinylpyrrolidone with a concentration of 1% by weight was prepared, which was stirred at 150 rpm for 12 minutes and then dispersed by ultrasound at 16 KHz for 15 minutes; 52. Preparation of iron phosphate precursor: Ferric sulfate was added to the aqueous polyvinylpyrrolidone solution of S1, and the mixture was stirred to dissolve. Ammonium phosphate was then added while stirring, resulting in a phosphorus:iron molar ratio of 1.6:1. The mixture was controlled at a pH of 2.0 (adjusted with sodium hydroxide or hydrochloric acid) and heated to 80 °C for 2 h to synthesize iron phosphate in situ. The resulting product was subjected to solid-liquid separation to obtain the iron phosphate precursor. 53. Preparation of lithium iron phosphate: In a nitrogen atmosphere, the iron phosphate precursor S1, lithium carbonate, and sucrose were mixed, such that the molar ratio of iron phosphate precursor, lithium carbonate, and sucrose was 1:1, 2:0, 3. The mixture was sintered at 650 °C for 6 h to obtain lithium iron phosphate. Comparative example 2: (Differs from example 3 in that the niobium diselenide doping method was different, and the doping was done at the sintering stage) In the present comparative example, a modified lithium iron phosphate is provided; the method for preparing the lithium iron phosphate comprises the following steps: 51. Preparation of an aqueous solution of polyvinylpyrrolidone; A deionized aqueous solution of polyvinylpyrrolidone with a concentration of 1% by weight was prepared, which was stirred at 150 rpm for 12 minutes and then dispersed by ultrasound at 16 KHz for 15 minutes; 52. Preparation of iron phosphate precursor: Ferric sulfate was added to the aqueous polyvinylpyrrolidone solution of S1, and the mixture was stirred to dissolve. Ammonium phosphate was then added while stirring, resulting in a phosphorus:iron molar ratio of 1.6:1. The mixture was controlled at a pH of 2.0 (adjusted with sodium hydroxide or hydrochloric acid) and heated to 80 °C for 2 h to synthesize iron phosphate in situ. The resulting product was subjected to solid-liquid separation to obtain the iron phosphate precursor. 53. Preparation of modified lithium iron phosphate: In a nitrogen atmosphere, the iron phosphate precursor from S1, niobium diselenide, lithium carbonate, and sucrose were mixed such that the molar ratio of iron phosphate precursor, lithium carbonate, and sucrose was 1:1, 2:0, 3, wherein the amount of niobium diselenide added was the same as in Example 3. The mixture was sintered at 650 °C for 6 h to obtain the modified lithium iron phosphate. Example test: The lithium iron phosphate or modified lithium iron phosphate obtained in Examples 1-4 and Comparative Examples 1-2 was used as the positive electrode material. Acetylene black was used as the conducting agent, and PVDF as the binding agent. A certain amount of NMP organic solvent was added. The mixture was stirred to obtain an electrode mixture. The resulting electrode mixture was coated with aluminum foil and dried to make a positive electrode sheet. The negative electrode was a lithium metal sheet. The diaphragm was a Celgard2400 polypropylene porous membrane. The solvent in the electrolyte was a solution composed of EC, DMC, and EMC in a 1:1:1 mass ratio, and the solute was LiPFe with a concentration of 1.0 mol / L. The 2023-type button cell battery was assembled in a glove box.The resistivity of the prepared positive electrode sheet was tested using a four-probe resistivity tester, and the first efficiency test was performed on the battery. The capacity retention rate of 100 cycles at 0.2 C was tested within the cutoff voltage range of 2.2–4.3 V. The test results are shown in Table 1. Table 1: Performance test results: Analysis of the results: It can be seen in Table 1 that the modified lithium iron phosphate of the present disclosure has a relatively good electrical conductivity, capacity retention rate and first efficiency, and the resistivity of the positive electrode sheet is less than 186 Q^m, and the capacity retention rate of 100 cycles at 0.2 C is above 92.5%, and its first efficiency is above 93.19%. Comparing Example 3 with Comparative Example 1, it can be seen that the resistivity of the positive electrode sheet of the modified lithium iron phosphate prepared in Example 3 is significantly reduced, the conductivity is effectively improved, and the capacity retention rate and first efficiency are also enhanced. This indicates that the method of the present disclosure modifies the precursor by doping niobium diselenide into the lithium iron phosphate positive electrode material precursor, and then prepares the positive electrode material using the modified iron phosphate precursor. This can effectively improve the conductivity of the positive electrode material while ensuring that the positive electrode material has better structural stability. Furthermore, the positive electrode material can be pre-supplemented with lithium to improve first efficiency.Comparing Example 3 with Comparative Example 2, it can be seen that in Comparative Example 2, since the niobium diselenide is doped during the sintering stage of the positive electrode material, the doping effect is poor, resulting in decreased conductivity, capacitance retention rate, and first efficiency of the positive electrode material. Comparing Example 3 with Example 4, it can be seen that using an aqueous polyvinylpyrrolidone solution to disperse the niobium diselenide provides a better doping effect and further improves the conductivity, capacitance retention rate, and first efficiency of the positive electrode material. The examples mentioned above are the preferred embodiments of this disclosure, but the embodiments of this disclosure are not limited by the examples mentioned above, and any other changes, modifications, substitutions, combinations, and simplifications made without departing from the spirit and principle of this disclosure shall be equivalent means of replacement, all of them included within the scope of protection of this disclosure.
Claims
1. A modified iron phosphate precursor, wherein the modified iron phosphate precursor is prepared by dissolving a soluble ferric salt in a niobium diselenide suspension and reacting the mixture with a phosphoric acid source.
2. The modified iron phosphate precursor according to claim 1, wherein in the modified iron phosphate precursor, the molar ratio of the soluble ferric salt to niobium diselenide is 1:0.05–0.15, preferably 1:0.1–0.15; the molar ratio of phosphorus in the phosphoric acid source to iron in the soluble ferric salt is 1.4–1.6:1, preferably 1.5–1.6:
1.
3. The modified iron phosphate precursor according to claim 1, wherein the niobium diselenide suspension is prepared by adding niobium diselenide to a dispersion solution. 4.The modified iron phosphate precursor according to claim 1 or 2, wherein the soluble ferric salt is at least one of ferric sulfate and ferric nitrate; the phosphoric acid source is at least one of phosphoric acid and ammonium phosphate.
5. A modified lithium iron phosphate, characterized in that the modified lithium iron phosphate comprises a lithium source and the modified iron phosphate precursor according to any one of claims 1-4.
6. The modified lithium iron phosphate according to claim 5, wherein the lithium source is lithium carbonate, lithium hydroxide, lithium acetate, or lithium bromide; preferably lithium hydroxide or lithium carbonate. 7.A method for preparing modified lithium iron phosphate according to any one of claims 5-6, wherein the method comprises the following steps: mixing a lithium source, a carbon source, and the modified iron phosphate precursor in a protective atmosphere, and sintering the mixture to obtain the modified lithium iron phosphate.
8. The method according to claim 7, wherein the molar ratio of the modified iron phosphate precursor, the lithium source, and the carbon source is 1:1, 1:1, 2:0, 1:0, 3; preferably 1:1, 1:1, 2:0, 2:0, 3.
9. The method according to claim 7 or 8, wherein the carbon source is at least one of glucose, lactose, and sucrose; the sintering temperature is 550-650 °C, preferably 600-650 °C; The duration of sintering is 6-8 h, preferably 6-7 h. 10.A lithium battery, wherein the lithium battery comprises modified lithium iron phosphate according to any of claims 5-6.
Citation Information
Patent Citations
Method for preparing high-density spherical lithium iron phosphate for lithium ion power battery
CN101519199A
Doped lithium manganese iron phosphate-carbon composite material and preparation method thereof
CN113148969A
Lithium iron phosphate with high conductivity and high compaction density and preparation method thereof
CN113562712A