Copper-doped lithium cobalt oxide precursor, positive electrode material, method of preparation and use thereof

ES3010560B2Pending Publication Date: 2026-11-19GUANGDONG BRUNP RECYCLING TECH CO LTD +1
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
ES2023090231
Authority / Receiving Office
ES · ES
Patent Type
Patents
Current Assignee / Owner
Priority Date
2022-06-27
Filing Date
2022-09-20
Publication Date
2026-11-19
Estimated Expiration
2042-09-20

AI Technical Summary

Technical Problem

Existing lithium cobalt oxide (LCO) materials exhibit poor charge and discharge cycles and inadequate high-temperature energy storage performance, limiting their discharge capacity improvement when traditional doping and coating methods are used.

Method used

A copper-doped lithium cobalt oxide precursor is prepared through a hydrothermal reaction of a soluble copper cobalt salt, urea, and a carbon source, followed by solid-liquid separation and calcination with a lithium source to form a copper-doped positive electrode material.

Benefits of technology

The copper-doped positive electrode material demonstrates improved discharge capacity exceeding 219.4 mAh/g and capacity retention rate of 84.6% after 600 cycles, enhancing structural stability and lithium ion transfer under high voltage.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000018_0000
    Figure 00000018_0000
  • Figure 00000019_0000
    Figure 00000019_0000
Patent Text Reader

Abstract

The present invention discloses a copper-doped lithium cobalt oxide precursor, a positive electrode material, and a method for preparing and using the same, comprising the following steps: (1) mixing a solution of soluble copper cobalt salt, urea, and a carbon source to carry out a hydrothermal reaction to obtain a mixed solution; (2) subjecting the mixed solution obtained in step (1) to solid-liquid separation, washing, and drying the resulting solid product to obtain the copper-doped lithium cobalt oxide precursor. The positive electrode material prepared from the copper-doped lithium cobalt oxide precursor has good cycle performance and good discharge capacity.
Need to check novelty before this filing date? Find Prior Art

Description

Copper-doped lithium cobalt oxide precursor, positive electrode material, method of preparation and use thereof Field This disclosure relates to the field of positive electrode materials for lithium batteries, and in particular to a copper-doped lithium cobalt oxide precursor, a positive electrode material, a method of preparation, and its use. Background Lithium cobalt oxide (LCO) is an early positive electrode material used in commercial lithium-ion batteries, primarily for mobile phones, laptops, and other portable electronic devices. LCO is characterized by its wide voltage range, ease of synthesis, and rapid charging and discharging. However, existing LCO materials exhibit several limitations at high voltages due to their inherent structure, including poor charge and discharge cycles and inadequate high-temperature energy storage performance.When traditional doping and coating methods are used to modify lithium cobalt oxide materials, the improvement in the discharge capacity of the lithium cobalt oxide materials is limited, which cannot meet the increasingly higher requirements of the lithium battery industry. Brief description of the invention The present invention aims to solve at least one of the technical problems existing in the prior art. Therefore, the present invention provides a copper-doped lithium cobalt oxide precursor, a positive electrode material, a method for preparing and using the same, and the positive electrode material prepared from the copper-doped lithium cobalt oxide precursor has good cycling performance and good discharge capacity. The aforementioned technical purpose of the present invention is achieved through the following technical solutions: The present invention provides a method for preparing a copper-doped lithium cobalt oxide precursor, comprising the following steps: (1) mixing a solution of soluble copper cobalt salt, urea and carbon source to perform a hydrothermal reaction to obtain a mixed solution; (2) subject the mixed solution obtained in step (1) to solid-liquid separation, wash and dry the resulting solid product to obtain the copper-doped lithium cobalt oxide precursor. Preferably, the total concentration of metal ions in the soluble copper cobalt salt solution is 0.01-1.5 mol / L, and the molar ratio of the cobalt element to the copper element is 10: (0.01-2). Furthermore, preferably, the total concentration of metal ions in the soluble copper cobalt salt solution is 0.05-1.0 mol / L, and the molar ratio of the cobalt element to the copper element is 10: (0.01-1). Preferably, the concentration of urea is 0.1-5.0 mol / L. In addition, preferably, the concentration of urea is 0.2-4.0 mol / L. Preferably, the molar amount of the carbon source is 1.5-6 times that of the copper element. In addition, preferably, the molar amount of the carbon source is 2-4 times greater than that of the copper element. Preferably, the carbon source is at least one selected from the group consisting of glucose, fructose, galactose, lactose, and maltose. Preferably, the temperature of the hydrothermal reaction in step (1) is 100-200 °C, and the reaction time is 1-10 h. Furthermore, preferably, the temperature of the hydrothermal reaction in step (1) is 120-160 °C, and the duration of the reaction is 4-8 h. Preferably, the soluble copper cobalt salt solution is prepared from a soluble salt, and the soluble salt is at least one selected from the group consisting of sulfate salt and chloride salt. Preferably, the washing method in step (2) is to wash the obtained product with ethanol first, and then with water. Preferably, the drying method in step (2) is to dry the obtained product at 60-150 °C for 1-10 hours. Additionally, preferably, the drying method in step (2) is to dry the obtained product at 80-120 °C for 2-4 hours. Preferably, the mixing method in step (1) is to first add the soluble copper cobalt salt solution into a hydrothermal reaction kettle with an additional amount of 3 / 5-4 / 5 of the reaction kettle volume, and then add the urea and carbon source into the hydrothermal reaction kettle. Preferably, during the hydrothermal reaction, the stirring speed in the reaction kettle is 100-500 rpm. Additionally, preferably, during the hydrothermal reaction, the stirring speed in the reaction kettle is 100-200 rpm. A copper-doped lithium cobalt oxide precursor, prepared by the method mentioned above. A method for preparing a positive electrode material, comprising the following steps: mixing the aforementioned lithium cobalt oxide precursor with a lithium source, and then calcining the resulting mixture to obtain the positive electrode material. Preferably, the lithium source is at least one selected from the group consisting of lithium carbonate and lithium hydroxide. Preferably, the calcination method is to first heat the material under the protection of an inert gas with a heating rate of 3-15 °C / min and a heating gradient from room temperature to 600-900 °C, then introduce an oxidizing gas instead, and maintain it at 600-900 °C for 10-20 h. Furthermore, preferably, the calcination method is to first heat the material under the protection of an inert gas with a heating rate of 5-10 °C / min and a heating gradient from ambient temperature to 700-850 °C, then introduce an oxidizing gas instead, and maintain it at 700-850 °C for 12-18 h, where ambient temperature refers to 25 °C. Preferably, a method for preparing a positive electrode material, comprising the following steps: (1) according to the molar ratio of the element cobalt to the element copper of 10: (0.01-1) , select soluble salts as raw material to prepare a mixed salt solution with a total metal ion concentration of 0.05-1.0 mol / L, wherein the soluble salt is at least one selected from the group consisting of sulfate salt and chloride salt; (2) add the mixed salt solution from step (1) into a hydrothermal reaction kettle with an additional amount of 3 / 5-4 / 5 of the reaction kettle volume; (3) add urea to the reaction kettle with a concentration of 0.2-4.0 mol / L; (4) add a carbon source to the reaction kettle with a molar amount 2-4 times that of the copper element; the carbon source is at least one selected from the group consisting of glucose, fructose, galactose, lactose and maltose; (5) seal the reaction kettle, heat and stir the mixture at a heating temperature of 120-160 °C and a stirring speed of 100-200 r / min to react for 4-8 h; (6) After the reaction is complete, subject the reaction mixture to solid-liquid separation, wash the resulting solid product with ethanol first, then with pure water, and then dry the washed product at 80-120 °C for 2-4 hours to obtain a copper-doped lithium cobalt oxide precursor; (7) In accordance with the molar ratio of the element cobalt to the element lithium of 1: (1, 2 1, 4) , mix the precursor material with at least one of lithium carbonate and lithium hydroxide, then heat the mixture under an inert gas with a heating rate of 5-10 °C / min and a heating gradient from room temperature to 700-850 °C, then introduce air or oxygen instead, maintain the temperature for 12-18 h, then pulverize and sieve the resulting mixture, and remove iron from the mixture to obtain a copper-doped lithium cobalt oxide positive electrode material. The present invention provides a positive electrode material, which is prepared by the method mentioned above. Preferably, the discharge capacity of the positive electrode material is not less than 219 mAh / g, for example, 219.4 mAh / g. Preferably, the capacity retention rate after 600 cycles of the positive electrode material is not less than 84%, e.g., 84.6%. The present invention provides for the use of the aforementioned positive electrode material in the lithium-ion battery. The beneficial effects of the present invention are: In the present invention, a mixed copper-cobalt salt, urea, and carbon source are subjected to a hydrothermal reaction in a reaction kettle to obtain a copper-doped lithium cobalt oxide precursor, which is then mixed and calcined with a lithium source to prepare a copper-doped positive electrode material. Since the copper-doped lithium cobalt oxide precursor is doped with copper, when prepared as a positive electrode material, the discharge capacity and cycle stability of the positive electrode material under high voltage can be further improved, such that the discharge capacity of the positive electrode material exceeds 219.4 mAh / g, and the capacity retention rate after 600 cycles exceeds 84.6%. The reaction principle is as follows: During the hydrothermal reaction: CO (NH2) 2+H2O^2NH3+CO2 NH3^H2O^NH4++OH- CO2+H2OCO32-+2H+ Co2++ (1-0, 5y) CO32-+yOH-^ Co (OH) y (CO3) 1-0.5y, where y <2. Copper ions complex with urea and react with a carbon source (such as glucose) in a redox reaction: {Cu[CO (NH2) 2M2++CH2OH (CHOH) 4CHO^CH2OH (CHOH) 4COOH+Cu2O+2H2O+4CO (NH2) 2 CH2OH (CHOH) 4COOH+NH3^H2O^CH2OH (CHOH) 4COONH4+H2O. During the hydrothermal reaction, cuprous oxide precipitates through the redox reaction between copper ions and carbohydrates, while divalent cobalt ions precipitate as basic cobalt carbonate, resulting in a mixed precipitate of cuprous oxide and basic cobalt carbonate. Compared to cupric oxide, when cuprous oxide and a lithium source are calcined to prepare lithium cuprate, a lower temperature is required, and pure lithium cuprate can be obtained. Therefore, in the subsequent high-temperature calcination of the positive electrode material, cuprous oxide is more conducive to lithium cuprate formation than divalent copper. In the high-temperature calcination stage, the initial heating in an inert atmosphere melts the lithium source, preventing the oxidation of the cuprous oxide. Then, when air / oxygen is subsequently introduced, the reaction proceeds as follows: 4Co (OH) and (CO3) 1-0, 5y+4LiOH+O2^4UCoO2+ (2+2y) H2O+ (4-2y) CO2 2Cu2O+8LiOH+O2*4L¡2CuO2+4H2O. The positive electrode material of lithium cuprate (Li2CuO2) is a lithium-rich positive electrode material, which has a higher theoretical specific capacity and theoretical energy density than other positive electrode materials, and can provide prelithiation capacity for the material obtained from the lithium cobalt oxide positive electrode, further improving the discharge capacity of the positive electrode material. Furthermore, the lithium cuprate structure contains [CuO4] chains arranged in a co-superior manner, forming a tetrahedron with a copper atom at its center. This structure is relatively stable under high voltage and provides a channel for lithium ion transfer. During charging and discharging, lithium ions can enter and exit the [CuO4] structures through the interconnected spaces, ensuring both structural stability and the normal charging and discharging of the positive electrode material. Brief description of the drawings FIGURE 1 is the SEM image of the copper-doped lithium cobalt oxide precursor prepared in Example 1 of the present invention. FIGURE 2 is the SEM image of the positive electrode material prepared in Example 1 of the present invention. Detailed description of the invention The present invention will be further described below with reference to specific examples. Example 1: A method for preparing a copper-doped lithium cobalt oxide precursor, comprising the following steps: (1) In accordance with the molar ratio of the element cobalt to the element copper of 10:0.5, cobalt sulfate and copper sulfate were selected respectively as raw materials to prepare a mixed salt solution with a total metal ion concentration of 0.5 mol / L; (2) the mixed salt solution in step (1) was added to a hydrothermal reaction kettle with an additional amount of 3 / 5 of the reaction kettle volume; (3) Urea was added to the reaction kettle with a concentration of 2.0 mol / L; (4) Glucose was added to the reaction kettle with a molar amount 3 times that of the copper element; (5) The reaction kettle was sealed, then the mixture was heated and stirred at a heating temperature of 140 °C and a stirring speed of 150 rpm to react for 6 hours; (6) After the reaction was completed, the reaction mixture was subjected to solid-liquid separation, the solid product obtained was washed first with ethanol, then with pure water, and then the washed product was dried at 100 °C for 3 hours to obtain a copper-doped lithium cobalt oxide precursor. A copper-doped lithium cobalt oxide precursor was prepared using the method mentioned above, and the SEM image of the copper-doped lithium cobalt oxide precursor is shown in FIGURE 1. A method for preparing a positive electrode material, comprising the following steps: according to the molar ratio of the element cobalt to the element lithium of 1:1, 3, the copper-doped lithium cobalt oxide precursor and lithium hydroxide were mixed, the mixture was heated under an inert gas with a heating rate of 10 °C / min and a heating gradient from room temperature to 850 °C, then air was introduced instead, the temperature was maintained for 15 h, and then the resulting mixture was crushed, sieved and iron removed to obtain a copper-doped lithium cobalt oxide positive electrode material. A positive electrode material was prepared by the method mentioned above, and the SEM image of the positive electrode material is shown in FIGURE 2. Example 2: A method for preparing a copper-doped lithium cobalt oxide precursor, comprising the following steps: (1) In accordance with the molar ratio of the element cobalt to the element copper of 10:1, cobalt chloride and copper chloride were selected respectively as raw materials to prepare a mixed salt solution with a total metal ion concentration of 1.0 mol / L; (2) the mixed salt solution in step (1) was added to a hydrothermal reaction kettle with an additional amount of 4 / 5 of the reaction kettle volume; (3) Urea was added to the reaction kettle with a concentration of 4.0 mol / L; (4) Fructose was added to the reaction kettle with a molar amount 4 times that of the copper element; (5) The reaction kettle was sealed, then the mixture was heated and stirred at a heating temperature of 160 °C and a stirring speed of 200 rpm to react for 4 hours; (6) After the reaction was completed, the reaction mixture was subjected to solid-liquid separation, the solid product obtained was washed first with ethanol, then with pure water, and then the washed product was dried at 120 °C for 2 h to obtain a copper-doped lithium cobalt oxide precursor. A copper-doped lithium cobalt oxide precursor was prepared using the method mentioned above. A method for preparing a positive electrode material, comprising the following steps: according to the molar ratio of the element cobalt to the element lithium of 1:1, 4, the copper-doped lithium cobalt oxide precursor and lithium carbonate were mixed, the mixture was heated under an inert gas with a heating rate of 5 °C / min and a heating gradient from room temperature to 850 °C, then oxygen gas was introduced instead, the temperature was maintained for 12 h, and then the resulting mixture was crushed, sieved and iron removed to obtain a copper-doped lithium cobalt oxide positive electrode material. A positive electrode material was prepared using the method mentioned above. Example 3: A method for preparing a copper-doped lithium cobalt oxide precursor, comprising the following steps: (1) In accordance with the molar ratio of the element cobalt to the element copper of 10:0.01, cobalt sulfate and copper sulfate were selected respectively as raw materials to prepare a mixed salts solution with a total metal ion concentration of 0.05 mol / L; (2) the mixed salt solution in step (1) was added to a hydrothermal reaction kettle with an additional amount of 3 / 5 of the reaction kettle volume; (3) Urea was added to the reaction kettle with a concentration of 0.2 mol / L; (4) Galactose was added to the reaction kettle at a molar amount of 2 times that of the copper element; (5) The reaction kettle was sealed, then the mixture was heated and stirred at a heating temperature of 120 °C and a stirring speed of 100 rpm to react for 8 h; (6) After the reaction was completed, the reaction mixture was subjected to solid-liquid separation, the solid product obtained was washed first with ethanol, then with pure water, and then the washed product was dried at 80 °C for 4 h to obtain a copper-doped lithium cobalt oxide precursor. A copper-doped lithium cobalt oxide precursor was prepared using the method mentioned above. A method for preparing a positive electrode material, comprising the following steps: according to the molar ratio of the element cobalt to the element lithium of 1:1, 2, the copper-doped lithium cobalt oxide precursor and lithium carbonate were mixed, the mixture was heated under an inert gas with a heating rate of 8 °C / min and a heating radiant from room temperature to 700 °C, then oxygen gas was introduced instead, the temperature was maintained for 18 h, and then the resulting mixture was crushed, sieved and iron removed to obtain a copper-doped lithium cobalt oxide positive electrode material. A positive electrode material was prepared using the method mentioned above. Comparative Example 1: (Compared to Example 1, no carbon source was added, and the other steps and parameters were exactly the same as Example 1) A method for preparing a copper-doped lithium cobalt oxide precursor, comprising the following steps: (1) In accordance with the molar ratio of the element cobalt to the element copper of 10:0.5, cobalt sulfate and copper sulfate were selected respectively as raw materials to prepare a mixed salt solution with a total metal ion concentration of 0.5 mol / L; (2) the mixed salt solution in step (1) was added to a hydrothermal reaction kettle with an additional amount of 3 / 5 of the reaction kettle volume; (3) Urea was added to the reaction kettle with a concentration of 2.0 mol / L; (4) The reaction kettle was sealed, then the mixture was heated and stirred at a heating temperature of 140 °C and a stirring speed of 150 rpm to react for 6 hours; (5) After the reaction was completed, the reaction mixture was subjected to solid-liquid separation, the solid product obtained was washed first with ethanol, then with pure water, and then the washed product was dried at 100 °C for 3 h to obtain a copper-doped lithium cobalt oxide precursor. A copper-doped lithium cobalt oxide precursor was prepared using the method mentioned above. A method for preparing a positive electrode material, comprising the following steps: according to the molar ratio of the element cobalt to the element lithium of 1:1, 3, the copper-doped lithium cobalt oxide precursor and lithium hydroxide were mixed, the mixture was heated under an inert gas with a heating rate of 10 °C / min and a heating gradient from room temperature to 850 °C, then air was introduced instead, the temperature was maintained for 15 h, and then the resulting mixture was crushed, sieved and iron removed to obtain a copper-doped lithium cobalt oxide positive electrode material. A positive electrode material was prepared using the method mentioned above. Comparative Example 2: (Compared to example 2, no carbon source was added, and the other steps and parameters were exactly the same as example 2) A method for preparing a copper-doped lithium cobalt oxide precursor, comprising the following steps: (1) In accordance with the molar ratio of the element cobalt to the element copper of 10:1, cobalt chloride and copper chloride were selected respectively as raw materials to prepare a mixed salt solution with a total metal ion concentration of 1.0 mol / L; (2) the mixed salt solution in step (1) was added to a hydrothermal reaction kettle with an additional amount of 4 / 5 of the reaction kettle volume; (3) Urea was added to the reaction kettle with a concentration of 4.0 mol / L; (4) The reaction kettle was sealed, then the mixture was heated and stirred at a heating temperature of 160 °C and a stirring speed of 200 rpm to react for 4 h; (5) After the reaction was completed, the reaction mixture was subjected to solid-liquid separation, the solid product obtained was washed first with ethanol, then with pure water, and then the washed product was dried at 120 °C for 2 h to obtain a copper-doped lithium cobalt oxide precursor. A copper-doped lithium cobalt oxide precursor was prepared using the method described above. A method for preparing a positive electrode material, comprising the following steps: according to the molar ratio of the element cobalt to the element lithium of 1:1, 4, the copper-doped lithium cobalt oxide precursor and lithium carbonate were mixed, the mixture was heated under an inert gas with a heating rate of 5 °C / min and a heating gradient from room temperature to 850 °C, then oxygen gas was introduced instead, the temperature was maintained for 12 h, and then the resulting mixture was crushed, sieved and iron removed to obtain a copper-doped lithium cobalt oxide positive electrode material. Comparative Example 3: (Compared to example 3, no carbon source was added, and the other steps and parameters were exactly the same as example 3) A method for preparing a copper-doped lithium cobalt oxide precursor, comprising the following steps: (1) In accordance with the molar ratio of the element cobalt to the element copper of 10:0.01, cobalt sulfate and copper sulfate were selected respectively as raw materials to prepare a mixed salts solution with a total metal ion concentration of 0.05 mol / L; (2) the mixed salt solution in step (1) was added to a hydrothermal reaction kettle with an additional amount of 3 / 5 of the reaction kettle volume; (3) Urea was added to the reaction kettle with a concentration of 0.2 mol / L; (4) The reaction kettle was sealed, then the mixture was heated and stirred at a heating temperature of 120 °C and a stirring speed of 100 rpm to react for 8 h; (5) After the reaction was completed, the reaction mixture was subjected to solid-liquid separation, the solid product obtained was washed first with ethanol, then with pure water, and then the washed product was dried at 80 °C for 4 h to obtain a copper-doped lithium cobalt oxide precursor. A copper-doped lithium cobalt oxide precursor was prepared using the method mentioned above. A method for preparing a positive electrode material, comprising the following steps: according to the molar ratio of the element cobalt to the element lithium of 1:1, 2, the copper-doped lithium cobalt oxide precursor and lithium carbonate were mixed, the mixture was heated under an inert gas with a heating rate of 8 °C / min and a heating gradient from room temperature to 700 °C, then oxygen gas was introduced instead, the temperature was maintained for 18 h, and then the resulting mixture was crushed, sieved and iron removed to obtain a copper-doped lithium cobalt oxide positive electrode material. A positive electrode material was prepared using the method mentioned above. Example test: The positive electrode materials obtained in Examples 1-3 and Comparative Examples 1-3 were used as active materials, acetylene black as the conductive agent, and PVDF as the binding agent. The active materials, conductive agent, and binding agent were weighed in a 92:4:4 ratio, mixed with a certain amount of NMP organic solvent, and stirred. The resulting mixture was coated with aluminum foil to make a positive electrode sheet, and a sheet of lithium metal was used as the negative electrode. A CR2430 button cell battery was made in a glove box filled with argon gas. The electrical performance test was carried out on the CT2001A Blue Electricity Test System. Test conditions: 3, 0-4, 48 V, current density 1 C = 180 mAh / g, test temperature 25 ± 1 °C. The test results are shown in Table 1 below. Table 1: Battery electrical performance test results Table 1 shows that the positive electrode materials prepared from the copper-doped lithium cobalt oxide precursors using the method of the present invention exhibited good discharge capacity and cycle stability, with a discharge capacity exceeding 219.4 mAh / g and a capacity retention rate exceeding 84.6% after 600 cycles. Furthermore, comparing Example 1 with Comparative Example 1, Example 2 with Comparative Example 2, and Example 3 with Comparative Example 3, respectively, reveals that when no carbon source was added to the hydrothermal reaction during the preparation of the copper-doped lithium cobalt oxide precursor, the cycle stability and discharge capacity of the final positive electrode material decreased. The examples mentioned above are preferred embodiments of the present invention, but the embodiments of the present invention are not limited to the examples mentioned above, and any other changes, modifications, substitutions, combinations, and simplifications made without departing from the spirit and principle of the present invention must be equivalent replacements, which are included within the scope of protection of the present invention.

Claims

1. A method for preparing a copper-doped lithium cobalt oxide precursor, comprising the following steps: (1) mixing a soluble copper cobalt salt solution, urea, and a carbon source to carry out a hydrothermal reaction to obtain a mixed solution; (2) subjecting the mixed solution obtained in step (1) to solid-liquid separation, washing, and drying the resulting solid product to obtain the copper-doped lithium cobalt oxide precursor.

2. The method for preparing a copper-doped lithium cobalt oxide precursor according to claim 1, wherein the total concentration of metal ions in the soluble copper cobalt salt solution is 0.01–1.5 mol / L, and the molar ratio of cobalt to copper is 10:(0.0–2).

3. The method for preparing a copper-doped lithium cobalt oxide precursor according to claim 1, wherein the urea concentration is 0.1-5.0 mol / l. 4.The method for preparing a copper-doped lithium cobalt oxide precursor according to claim 2, wherein the molar amount of the carbon source is 1.5-6 times that of the copper element.

5. The method for preparing a copper-doped lithium cobalt oxide precursor according to claim 1, wherein the temperature of the hydrothermal reaction in step (1) is 100-200 °C, and the reaction time is 1-10 h.

6. A copper-doped lithium cobalt oxide precursor, prepared by the method according to any one of claims 1-5.

7. A method for preparing a positive electrode material, comprising the following steps: mixing the lithium cobalt oxide precursor according to claim 6 with a lithium source, and then calcining the resulting mixture to obtain the positive electrode material. 8.The method for preparing a positive electrode material according to claim 7, wherein the calcination method is to first heat the material under the protection of an inert gas at a heating rate of 3-15 °C / min and a heating gradient from ambient temperature to 600-900 °C, then introduce an oxidizing gas instead, and maintain it at 600-900 °C for 10-20 h.

9. A positive electrode material, prepared by the method according to any of claims 7-8.

10. Use of the positive electrode material according to claim 9 in a lithium-ion battery.

Citation Information

Patent Citations

  • Preparation method and application of flower-shaped composite material formed by carbon plates in which cobaltosic oxide is embedded in hollow nano sphere mode

    CN106058174A

  • Hollow spherical particle negative electrode material with openings and preparation method and application thereof

    CN114242960A

  • Carbon coated electrode active material for secondary battery, and fabrication methode for preparing the same

    KR101617836B1