Abstract

This invention relates to a method for forming a heat-treatable aluminum alloy sheet into a target shape component, and the aluminum alloy component formed by the method. The method includes: (a) heating the aluminum alloy sheet to an alloy solution heat treatment (SHT) temperature or above, and maintaining this temperature until the SHT is completed; (b) continuously transferring the heated sheet to a die to be stamped into the target shape, and subjecting the formed component to in-die quenching; (c) continuously transferring the quenched component and subjecting it to pre-aging treatment; and (d) subjecting the pre-aging treated component to a second aging treatment to obtain the target shape component that meets strength requirements.
Need to check novelty before this filing date? Find Prior Art

Description

1. Description of a Continuous Pre-Aging Method for Hot Forming Alloy Sheets Technical Field This invention relates to a method for forming heat-treatable alloy sheets into parts of a desired shape. The invention also relates to alloy parts formed by this method. The alloy may be an aluminum alloy. Background Art In automotive applications, using monolithic body parts instead of multi-part assemblies helps reduce weight and cost while improving structural integrity. A widely adopted method is to use a set of dies to form a single sheet of metal into a desired geometry through stamping. However, the complexity of formable parts is inherently limited by the formability of the sheet metal. If the metal has poor plastic deformation capacity, it may crack during forming; conversely, if the ductility is too high, it may fail to maintain the required shape or mechanical strength due to insufficient work hardening capacity. To address these issues, the Hot Form and Quench (HFQ®) process (WO2010 / 032002A1 or CN102216484A), also known as Direct Hot Form and Quench (HFQ®), was developed. This process improves formability and enables the creation of more complex shapes from a single sheet metal. The process involves heating the aluminum alloy to the SHT temperature, rapidly transferring it to a cold-forming tool for forming, and simultaneously quenching the tool to create a supersaturated solid solution microstructure. The formed part is then artificially aged to achieve the T6 condition, which exhibits optimal strength due to precipitate formation. The indirect HFQ® process (as disclosed in US2022 / 0341015A1 or CN114867885A) employs a two-step forming process: first, the sheet metal is cold-formed to approximately 90-95% of its final shape, followed by solution heat treatment (SHT), and finally hot forming and quenching.20 Compared to conventional hot forming, this method reduces energy consumption by more than 40%, eliminates the need for complex mold heating and cooling systems, and allows the same mold to be reused for both cold forming and quenching. The indirect HFQ® process typically requires several hours (usually 6 to 12 hours) of aging treatment after forming to achieve the desired mechanical properties. Furthermore, this process benefits from the strain hardening effect of the O-temper alloy state, thereby reducing subsequent strengthening steps and increasing yield strength.25 While conventional aging processes offer these advantages, they require several hours to complete. Both the aluminum alloy HFQ® and indirect HFQ® forming processes require rapid mold cooling to ensure that the cooling rate is higher than the critical quenching rate, which places high demands on mold cooling.Furthermore, the need to transport formed parts between aging steps increases energy consumption and logistics costs. While indirect hot forming methods can reduce some energy costs, their coarsened microstructure grains result in lower mechanical properties compared to direct HFQ®. Therefore, there is an urgent need to develop a technical solution that can quickly complete the aging process of parts and reduce the need for mold cooling, thereby improving the production efficiency of hot-formed aluminum alloy parts, reducing energy consumption and enterprise production costs, and extending the service life of molds under thermal cycling. This invention provides a rapid strengthening and stamping process suitable for 2xxx, 6xxx, and 7xxx series heat-treatable aluminum alloy sheets, characterized by completing a continuous pre-aging stage within 10 minutes after hot forming and in-mold quenching. This process includes solution heat treatment (SHT) of the sheet metal, rapid transfer, stamping in a forming die, in-die quenching to 20–300°C, followed by rapid or continuous transfer to a pre-aging furnace (holding for 1–20 minutes) for continuous rapid pre-aging at 50–250°C. Final strengthening is achieved through short-duration secondary aging or automotive painting baking cycles. Compared to traditional thermoforming and aging processes, this process allows parts to be demolded at relatively high temperatures, significantly reducing die holding time and improving production efficiency. Furthermore, this process reduces die cooling intensity and complexity, mitigates die thermal fatigue, and extends die life. Pre-aging treatment achieves 60%–75% of T6 strength in less than 20 minutes, significantly shortening aging time and part delivery cycle. Simultaneously, utilizing waste heat and simplifying the online process reduces energy, labor, and logistics costs. This process achieves satisfactory T6 mechanical properties, high dimensional and surface quality, and is suitable for continuous industrial stamping production. This invention can be directly applied to the manufacture of high-strength aluminum alloy parts, particularly structural or collision-related components in the automotive industry. This method is especially suitable for mass production of body-in-white components because it reduces processing time, minimizes mold wear, and can be seamlessly integrated with painting and baking processes. Overall, this invention provides an integrated, efficient, low-cost, and industrially scalable solution for manufacturing high-strength aluminum alloy parts with excellent dimensional stability and mechanical properties. In one aspect, this invention provides a method for forming alloy sheet into a component of a desired shape. In this aspect, the sheet, blank, or component may be an aluminum alloy, such as a heat-treatable aluminum alloy.In this aspect, the sheet metal, blank, or component may be a magnesium alloy or titanium alloy, such as a heat-treatable magnesium alloy or titanium alloy. Further, the sheet metal is an aluminum alloy sheet that can be heat-treatable at 25°C. For example, the aluminum alloy is a 2xxx series, 6xxx series, or 7xxx series aluminum alloy. More specifically, the aluminum alloy is AA6016, AA6082, or AA7075 aluminum alloy. For example, the aluminum alloy is AA6016 aluminum alloy. The blank as the sheet metal can come from various states, such as O, F, W, T4, T6. HK 30137558 A 3 In this aspect of the invention, the target shape component may be an automotive industry component, an aerospace component, a railway industry component, a marine industry component, or a consumer electronics product or housing component, such as a monocoque body component. In the foregoing, the present invention relates to a method for forming an alloy sheet into a component of a target shape, the method comprising: (a) heating the alloy sheet to an alloy solution heat treatment (SHT) temperature or above, and maintaining the temperature until the SHT is completed; (b) continuously transferring the heated sheet into a mold and stamping it into the target shape, and subjecting the formed component to in-mold quenching; (c) continuously transferring the quenched component and subjecting it to pre-aging treatment; and (d) subjecting the pre-aging treated component to a second aging treatment to obtain the component of the target shape. The obtained component of the target shape meets strength requirements. The sheet or component may be an aluminum alloy, such as a heat-treatable aluminum alloy, such as the aluminum alloy described above. The SHT temperature in step (a) is 470°C to 550°C, for example 520°C to 540°C, such as 470°C, 480°C, 490°C, 500°C, 510°C, 520°C, 530°C, 540°C, or 550°C. In step (a) 10, the alloy sheet is heated to the alloy solution heat treatment (SHT) temperature or above to perform a complete solution heat treatment to form a supersaturated solid solution (SSSS). Therefore, the alloy sheet can be heated to the alloy solution heat treatment (SHT) temperature of 470°C to 550°C or higher. In this step, the solution heat treatment is performed in a furnace. The alloy sheet billet is heated in a furnace to a temperature range of 470°C to 550°C for a complete solution heat treatment to form a supersaturated solid solution. For example, the time spent holding the SHT temperature until the SHT is completed is less than 30 minutes, less than 15-25 minutes, less than 25 minutes, less than 20 minutes, for example, 5 seconds to 25 minutes, for example, 15 seconds to 20 minutes. For example, for materials in the W state, the sheet needs to be held for approximately 15 to 60 seconds to allow the alloying elements to completely dissolve into the aluminum matrix.For materials in the F / O state, the holding time at SHT temperature needs to be extended to 1 to 20 minutes. Immediately after this step, the sheet or blank should be quickly transferred to the hot stamping press to prevent premature precipitation of the strengthening phase, which would otherwise affect subsequent forming and heat treatment. In step (b), the heated sheet is continuously transferred to the mold for a dwell time of less than 1 minute, for example, less than 50 seconds, less than 40 seconds, less than 30 seconds, less than 25 seconds, less than 20 seconds, less than 15 seconds, less than 10 seconds, less than 5 seconds, less than 1 second, for example, 0 seconds, 1 second, 2 seconds, 3 seconds, 4 seconds, 5 seconds, 6 seconds, 7 seconds, 8 seconds, 9 seconds, or 10 seconds. This transfer step transfers the SHT-completed sheet to the stamping process. In step (b), the formed part is quenched in the mold to a temperature above 20°C, for example, 20°C to 300°C, or 25°C to 60°C to 180°C, for example, 20°C, 30°C, 40°C, 50°C, 60°C, 70°C, 80°C, 90°C, 100°C, 110°C, 120°C, 130°C, 140°C, 150°C, 160°C, 170°C, 180°C, 190°C, 200°C, 210°C, 220°C, 230°C, 240°C, 250°C, 260°C, 270°C, 280°C, 290°C, or 300°C, for example, 20°C, 60°C, 100°C, 150°C, or 170°C. Step (b) is preferably performed in the mold. HK 30137558 A 4 Therefore, in this step, the heated sheet metal is stamped into the target shape and the formed part is quenched to a temperature above 20°C, preferably in a die. In this step, the sheet metal or blank is rapidly transferred to a cold forming die for rapid pressing, followed by in-die quenching at a rate exceeding the alloy's specific critical cooling rate, thereby preventing premature precipitation, maintaining the SSSS microstructure, and minimizing springback. In this step, the stamping of the heated sheet metal can be completed on a press. In this step, 5 the heated sheet metal blank is rapidly transferred to a die and formed into the target shape (e.g., a pre-set complex shape); subsequently, quenching is performed to cool the formed part to a temperature range of 20°C to 300°C. This effectively maintains the supersaturated microstructure of the part and minimizes springback after forming. It is preferable to use an active cooling die for immediate quenching after forming to avoid common forming defects.When the final temperature of in-mold quenching (part ejection temperature) is controlled at a relatively high level (optimally 60–180°C), the mold cooling requirement is reduced, and early ejection can significantly shorten the stamping cycle time. There are several methods to improve the quench rate of in-mold quenching, such as directly injecting air, water, or a mixture of air and water into the gap between the part and the mold or into the vents on the mold, which can further shorten the stamping cycle time. For example, to further increase production speed, additional external cooling can be used during in-mold quenching, including injecting air jet cooling, water mist spraying, or a mixed air-water cooling solution into the mold cavity, vents, or the gap between the part and the mold surface to accelerate cooling. In step (c), the dwell time for the continuous transfer of the quenched part is less than 20 minutes and less than 10 minutes, for example, 1 minute to 10 minutes, such as 0 seconds, 10 seconds, 20 seconds, 30 seconds, 1 minute, 2 minutes, 3 minutes, 4 minutes, 5 minutes, 6 minutes, 7 minutes, 8 minutes, 9 minutes, 10 minutes, 11 minutes, 12 minutes, 13 minutes, 14 minutes, 15 minutes, 16 minutes, 17 minutes, 18 minutes, 19 minutes, or 20 minutes. Furthermore, the pre-aging treatment of the quenched component in step (c) 20 is performed at temperatures ranging from 50°C to 250°C, such as 50°C, 60°C, 70°C, 80°C, 90°C, 100°C, 110°C, 120°C, 130°C, 140°C, 150°C, 160°C, 170°C, 180°C, 190°C, 200°C, 210°C, 220°C, 230°C, 240°C, 250°C, such as 50°C, 120°C, 150°C, 170°C, 200°C, or 250°C. Furthermore, in step (c), the pre-aging treatment of the quenched component is performed within a time frame of less than 20 minutes, for example less than 10 minutes, for example 1 minute to 20 minutes, for example 30 seconds, 1 minute, 225 minutes, 3 minutes, 4 minutes, 5 minutes, 6 minutes, 7 minutes, 8 minutes, 9 minutes, 10 minutes, 11 minutes, 12 minutes, 13 minutes, 14 minutes, 15 minutes, 16 minutes, 17 minutes, 18 minutes, 19 minutes, or 20 minutes. In step (c), the pre-aging treatment enables the component to achieve a partial T6 temper strength or T6 mechanical properties.In step (c), the pre-aging treatment brings the HK 30137558 A 5 component to less than 90% of its (full) T6 temper strength or T6 mechanical properties, for example, 50% to 90%, 60% to 80%, 60% to 75%, or 50%, 55%, 60%, 65%, 70%, 75%, 80%, or 85%. Therefore, in this step, the quenched component is rapidly transferred within a dwell time of less than 10 minutes and pre-aged at 50°C to 250°C for less than 20 minutes. Specifically, in step (c), the quenched component is continuously transferred to the pre-aging treatment (e.g., a pre-aging furnace) within 10 minutes, and pre-aging is performed at a temperature range of 50°C to 250°C and held for 1 to 20 minutes. After stamping, the formed component is immediately transferred to the pre-aging furnace (the dwell time from ejection from the mold to entry into the furnace does not exceed 10 minutes). The pre-aging furnace can be integrated at the end of the production line and continuous, rapid pre-aging can be achieved using a roller hearth furnace, box furnace, or resistance heating equipment. Furthermore, various heating methods can be employed, including current heating, box resistance furnaces, roller hearth furnaces, and other conventional industrial heating equipment. All these methods enable rapid pre-aging treatment while maintaining process continuity. Immediate transfer is preferred to fully utilize the residual heat of the component. The pre-aging temperature range is 50–250°C, and the holding time is 1–20 minutes. This step utilizes the residual heat of the component to promote precipitate nucleation. This rapid pre-aging treatment allows the component to reach 60–75% of its T6 temper strength in a short time and effectively accelerates the nucleation of strengthening precipitates in the aluminum alloy, which is advantageous for secondary aging treatment. Optionally, the method of the present invention may include a transfer step between step (c) and step (d), transferring the pre-aged component to the secondary aging treatment without heat treatment. In this respect, the transfer may not require continuous transfer. For example, the transfer step includes packaging and transportation. In step (d), the second aging treatment is performed at a temperature of 150°C to 250°C, for example, 150°C to 220°C, such as 150°C, 160°C, 170°C, 180°C, 190°C, 200°C, 210°C, 220°C, 230°C, 240°C, or 250°C, such as 150°C, 180°C, 220°C, or 250°C.In step (d), the second aging treatment is performed for 10 to 60 minutes, for example, 10, 20, 30, 40, 50, or 60 minutes. In this step, the component is placed in a second aging furnace to complete the final aging treatment to achieve the desired mechanical properties. For example, the second aging of the component is performed at a temperature range of 150°C to 250°C for 10–60 minutes to achieve the required full T6 temper strength or full T6 mechanical properties, thus completing the entire heat treatment cycle of the aluminum alloy hot forming process. This step can be performed in the original equipment manufacturer's (OEM) factory. For example, in the automotive industry, this step can be part of a paint baking process. For example, the secondary aging treatment can be a paint baking aging treatment in an automotive paint shop, whereby the component achieves full T6 properties. Alternatively, other short-time heat strengthening methods, such as infrared heating or low-temperature convection heating, can also be used. These alternatives can be flexibly adapted to different HK 30137558 A 6 production lines while still achieving the expected full target mechanical properties. Therefore, the second aging treatment in step (d) can be completed in a shorter time, thereby greatly shortening the entire process flow. Using this two-step aging treatment scheme (short pre-aging + secondary aging), the total heat treatment time is reduced from 6-18 hours to less than 1.33 hours. In this invention, "continuous" in "continuous transfer" means that the sheet or part is transferred directly and quickly from the previous processing step, scene, or processing device in the method of this invention to the next processing step, scene, or processing device. Transfer is, for example, from SHT to stamping, or from quenching to pre-aging. Continuous transfer can be achieved by robotic arm transfer or manual transfer. Continuous transfer can shorten the overall time of the method of this invention while ensuring the overall mechanical properties of the final product. "Dwell time" refers to the time required for continuous transfer of the sheet or part. For example, in step (b), the dwell time for continuous transfer is less than 30 seconds or less than 10 seconds. For example, the dwell time during continuous transfer in step (c) is less than 20 minutes, less than 10 minutes, or 1 to 10 minutes. Continuous transfer of the part after in-mold quenching is one of the keys to achieving the effects of this invention. Furthermore, those skilled in the art will understand that the heated sheet metal in step (b) should be continuously transferred to the mold.In one aspect, the present invention relates to a method for forming a heat-treatable aluminum alloy sheet into a component of a target shape, the method comprising: (a) heating the alloy sheet to an alloy solution heat treatment (SHT) temperature or above and holding the temperature until the SHT is completed, the SHT temperature being 470°C to 550°C; (b) continuously transferring and stamping the heated sheet into the target shape, and quenching the formed component to a temperature above 20°C, preferably the stamping and quenching being performed in a die; (c) continuously transferring the quenched component for a dwell time of less than 20 minutes and performing a pre-aging treatment, the pre-aging treatment being performed at a temperature of 50°C to 250°C for less than 20 minutes; and (d) subjecting the pre-aged component to a second aging treatment at a temperature of 150°C to 250°C for 10 minutes to 60 minutes to obtain the component of the target shape. The sheet or component may be an aluminum alloy, such as a heat-treatable aluminum alloy, such as the aforementioned Aluminum 20 alloy. In step (c), the pre-aging treatment brings the part to 50% to 90%, for example 60% to 80%, or for example 60% to 75%, of the full T6 temper strength or T6 mechanical properties required for use. In step (d), the second aging treatment brings the resulting target-shaped part to the full T6 temper strength or full T6 mechanical properties required for use. In one aspect, the present invention relates to an aluminum alloy part formed by the method of the present invention. The part may be an automotive part, aerospace part, railway part, marine part, or consumer electronics or housing part. Therefore, the method of the present invention is applicable to the pre-forming treatment of a variety of solution-heat-treatable alloys, including aluminum alloys such as 6016, 6082, and 7075. It is particularly suitable for the manufacture of complex parts in the automotive and aerospace industries, improving production efficiency, reducing energy consumption, and ensuring part quality. HK 30137558 A 7 Brief Description of the Drawings Figure 1 shows the overall continuous rapid pre-aging hot forming process. For quenching end temperatures (>20℃), the transfer should be performed as quickly as possible. For room temperature (20℃), the dwell time before pre-aging should preferably not exceed 10 minutes. For continuous rapid pre-aging paths (rapid transfer), path A indicates that the quenching end temperature is equal to the pre-aging temperature, path B indicates that the quenching end temperature is higher than the pre-aging temperature, and path C indicates that the quenching end temperature is lower than the pre-aging temperature. Figure 2 shows a schematic diagram of the continuous rapid pre-aging thermoforming process.The process includes the following steps: Step (a) Furnace SHT: The sheet metal billet is heated in a furnace to 470–550°C for complete solution heat treatment, forming a supersaturated solid solution. The billet is then rapidly transferred (transfer*) to a hot stamping press to avoid premature precipitation. Step (b) Press-Hot Stamping and In-Die Quenching: The billet is rapidly fed into a hot stamping die for forming, followed by in-die quenching to 20–300°C. Actively cooled dies ensure that the cooling rate exceeds the alloy's critical cooling rate, thus preserving the supersaturated microstructure and minimizing springback. Step (c) Continuous Low-Temperature Fast Pre-Ageing: After quenching, the formed part is immediately (with a dwell time not exceeding 10 minutes) transferred to a pre-aging furnace using residual heat. Pre-aging, performed at temperatures of 50℃–250℃ for 1–20 minutes, accelerates the nucleation of precipitates, achieving 15-60%–75% of the T6 temper strength. Packaging and Transportation: Pre-aged parts are packaged and transported to the final aging step without intermediate heat treatment. Step (d) Second Ageing: Parts undergo final aging at 150–220℃ for 10–60 minutes to achieve full T6 mechanical properties, thus completing the heat treatment cycle. Figure 3 shows the mechanical properties of 6016 aluminum alloy after pre-aging (PA) + second aging (PB): (a) properties at different quenching end temperatures (20℃, 100℃, 150℃, and 170℃); (b) properties after second aging under different pre-aging conditions at the same quenching end temperature (60℃). PB (paint bake process) refers to simulating the painting and baking process of the parts. Figure 4 shows the final mechanical properties of the parts (6016 aluminum alloy) after different dwell times: to ensure mechanical properties, the transfer dwell time from in-mold quenching to the low-temperature pre-aging furnace should not exceed 10 minutes (0.167 hours). PB25 (paint bake process) refers to the simulated painting and baking process of the parts. Detailed Embodiments The embodiments of the method of the present invention for forming parts from 6016 aluminum alloy sheets into the target shape are described below with reference to Figures 1 to 4. HK 30137558 A 8 Embodiments In general, as shown in Figure 1, the overall process flow of the continuous low-temperature rapid pre-aging thermoforming technology includes solution heat treatment, hot stamping, in-mold quenching, continuous low-temperature pre-aging, and final aging.Specifically, the process first heats the aluminum alloy sheet to a set solution heat treatment temperature to form a supersaturated solid solution; then, the sheet is formed into a preset shape by hot stamping, followed by in-mold quenching to ensure the stability of the supersaturated structure and minimize springback. Subsequently, the part is immediately transferred to a low-temperature pre-aging furnace to fully utilize the residual heat to complete rapid pre-aging; finally, a final aging treatment is performed to obtain the desired mechanical properties. The routes A / B / C shown in Figure 1 are defined as follows: A: Quenching end temperature equal to pre-aging temperature; B: Quenching end temperature higher than pre-aging temperature; and C: Quenching end temperature lower than pre-aging temperature. Specifically, as shown in Figure 2, the process of forming complex parts from heat-treatable 6016 aluminum alloy sheet includes 10 steps: Step (a): Solution heat treatment. The 6016 aluminum alloy sheet is heated to or above its solution heat treatment (SHT) temperature, typically between 520°C and 540°C. For W-state materials, the sheet metal needs to be held at the temperature for approximately 15 to 60 seconds to allow the alloying elements to completely dissolve into the aluminum matrix. For F / O-state materials, the holding time at the SHT temperature needs to be extended to 1 to 20 minutes. Step (b): Hot forming and in-mold hardening. The heated billet is transferred to a cooled die set, where it is formed into the desired complex shape while being hardened in-mold to form a supersaturated solid solution microstructure, thereby ensuring dimensional accuracy and minimizing springback. The formed part is then ejected from the die at a temperature of 20°C to 250°C. In a preferred embodiment, the part is removed at a higher temperature of 60°C to 250°C to retain the residual heat generated during forming and hardening for subsequent pre-aging treatment. There are several methods to increase the hardening rate of in-mold hardening, for example, by directly injecting air, water, or a mixture of air and water into the gap between the part and the die or into the vent holes on the die, which can further shorten the stamping cycle time. Step (c): Rapid transfer to a pre-aging furnace. The formed parts undergo continuous pre-aging treatment in the furnace at a controlled temperature of approximately 150°C for 5 minutes. 25 In the automotive industry, parts are not packaged and then transported to a separate aging furnace; instead, they are directly transferred by an automated robotic system to an online continuous rapid pre-aging furnace integrated at the end of the forming line. This furnace can be a roller hearth furnace or a segmented furnace with multiple heating zones, configured to maintain precise temperature control and enable continuous production. For manual production lines (HK 30137558 A 9), the initial temperature of the parts during pre-aging is very low, close to room temperature; to maintain the continuity of pre-aging, the transfer dwell time should not exceed 10 minutes.Step (d): Secondary Aging After pre-aging, the component undergoes a second aging treatment (250℃ × 20 minutes) to complete precipitation hardening and achieve the full T6 mechanical properties required for stringent use. For automotive applications, the pre-aged component can be packaged and shipped to the OEM factory, where the second aging can be easily integrated into the paint baking process. All uniaxial test standards used in the experiments followed the ASTM E8 / E8M standard test method for tensile testing of metallic materials. More specifically, following steps (a) to (d) above, as shown in Figure 3(a), different quenching temperatures of 20℃, 100℃, 150℃, and 170℃ were used, followed by a 5-minute pre-aging treatment at 150℃, and then a 20-minute secondary aging treatment at 180℃ (simulating the paint baking process (PB)) at different temperatures. After pre-aging and secondary aging treatment of 6016 aluminum alloy, the mechanical properties of the target-shaped component were tested. Furthermore, following steps (a) to (d) above, as shown in Figure 3(b), a quenching temperature of 60°C was used, and pre-aging treatments were performed under various conditions (5 minutes at 120°C, 5 minutes at 150°C, 10 minutes at 150°C, 5 minutes at 170°C, 10 minutes at 170°C, 3 minutes at 200°C, and 5 minutes at 200°C). After pre-aging and secondary aging treatments for 15 minutes, the mechanical properties of the target-shaped component were tested. The results in Figure 3(a) show that good consistency in mechanical properties was ultimately achieved after different continuous pre-aging temperatures (i.e., the end temperature of in-mold quenching) plus a second aging (180°C × 20 minutes). Increasing the continuous pre-aging temperature to 170°C did not adversely affect the final mechanical properties of the component, indicating that the selected continuous pre-aging temperature range is reliable and feasible. Higher pre-aging temperatures (above 250°C) are detrimental to post-forming processing, such as trimming and CNC machining, because the hardness and strength of the pre-aged part are only 85-95% of the T6 properties, and mechanical properties (such as strength and ductility) may decrease. Lower temperatures (below 250°C) and shorter pre-aging times can be performed over a wider temperature range (50-250°C), which is beneficial for industrial environments. Figure 3(b) shows that, at the same pre-aging temperature, the secondary aging process enables the part to meet the required mechanical property indicators. Rapid transfer and continuous pre-aging of the quenched part significantly improves the strength, bringing it to approximately 60% to 75% of the T6 temper strength. The final step (d) completes the aging process, ensuring the part achieves full T6 mechanical properties.Furthermore, following steps (a) to (d) above, as shown in Figure 4, the final mechanical properties of 6016 aluminum alloy parts quenched to 20°C and subjected to pre-aging and secondary aging treatments (simulating the painting and baking process (PB) of the parts) were tested for different pre-aging transfer dwell times (0, 10 minutes, 1 hour, 4 hours, 8 hours, 22 hours). As shown in Figure 4, to ensure stable mechanical properties, the transfer dwell time from the completion of stamping quenching to the low-temperature pre-aging furnace should not exceed 10 minutes (0.167 hours). Figure 4 also shows that the time for the parts to enter the pre-aging furnace after quenching should be controlled within 1 hour; to obtain the best mechanical properties, this transfer time is preferably limited to within 10 minutes. Using the T6 tempering strength as a reference, the performance requirements are clearly defined: the mechanical properties of the parts should be better than or equal to the T6 tempering strength. The dashed lines in the figure represent the minimum yield strength (YS) and ultimate tensile strength (UTS) of the T6 tempered strength. This demonstrates the superior technical effects achieved by the method of this invention. For example, production efficiency is improved; parts can be ejected at relatively high temperatures (20–250°C) without the need for prolonged temperature maintenance within the mold as in traditional processes, nor for slow cooling below 250–300°C, thus significantly shortening the stamping cycle and increasing output. Chip thermal load is reduced and lifespan extended; reduced cooling intensity decreases mold thermal cycling and fatigue, simplifies cooling channel design, and extends mold lifespan. Heat treatment time is significantly shortened; only 1–20 minutes of pre-aging treatment is required to achieve 60–75% of the T6 strength, and the final performance can be obtained through a short secondary aging treatment or a painting and baking cycle. The total heat treatment time is reduced from 6–18 hours to approximately 0.16–1.33 hours. Energy saving and reduced logistics costs are achieved by directly utilizing the residual heat of the molded parts for pre-aging treatment (e.g., in cases of robotic arm transfer). The integrated online pre-aging equipment reduces intermediate transportation and storage, thereby lowering labor and logistics costs. Stable mechanical properties and dimensional accuracy are ensured; controlled quenching guarantees supersaturated solid solutions, while optimized quenching end temperature minimizes springback and guarantees dimensional stability. In summary, the method of this invention achieves satisfactory T6 grade mechanical properties, improves production efficiency, reduces energy consumption, extends mold life, shortens manufacturing cycles, and reduces overall production costs.20 HK 30137558 A 1 Claim 1. A method for forming a heat-treatable aluminum alloy sheet into a component of a target shape, the method comprising: (a) heating the sheet to an alloy solution heat treatment (SHT) temperature or above and maintaining the temperature until the SHT is completed; (b) continuously transferring the heated sheet into a mold and stamping it into the target shape, and subjecting the formed component to in-mold quenching; (c) continuously transferring the quenched component and subjecting it to pre-aging treatment; and (d) subjecting the pre-aging treated component to a second aging treatment to obtain the component of the target shape. 2. The method of claim 1, wherein the heat-treatable aluminum alloy sheet is selected from 2xxx, 6xxx, or 7xxx series aluminum alloy sheets, such as AA6016, AA6082, or AA7075 aluminum alloy sheets, such as AA6016 aluminum alloy sheet; wherein the target shape component is an automotive component, aerospace component, railway component, marine component, or consumer electronics component or housing component, such as a unibody component; and / or wherein the second aging treatment is a paint baking process, such as an automotive paint baking process, such as an OEM automotive paint baking process. 3. The method of any of the preceding claims, wherein the SHT temperature in step (a) is 470°C to 550°C, for example, 520°C to 540°C. 4. The method of any of the preceding claims, wherein the residence time of continuously transferring the heated sheet material into the mold in step (b) is less than 10 seconds; and / or the quenching of the formed part in the mold to a temperature above 20°C, for example, a temperature from 20°C to 300°C, for example, a temperature from 60°C to 180°C, for example, 20°C, 60°C, 100°C, 150°C, or 170°C, in step (b). 5. The method of any of the preceding claims, wherein the residence time of continuously transferring the quenched part in step (c) is less than 20 minutes, for example, less than 10 minutes, for example, 1 minute to 10 minutes. 6. The method of any of the preceding claims, wherein the pre-aging treatment of the quenched part in step (c) is performed at a temperature of 50°C to 250°C, for example, 50°C, 120°C, 150°C, 170°C, 200°C, or 250°C. 7. The method of any of the preceding claims, wherein the pre-aging treatment of the quenched component in step (c) is performed in less than 20 minutes, for example less than 10 minutes, for example from 1 minute to 20 minutes.HK 30137558 A 2 8. The method of any of the preceding claims, wherein the second aging treatment in step (d) is performed at a temperature of 150°C to 250°C, for example 150°C to 220°C, for example 150°C, 180°C, 220°C or 250°C. 9. The method of any of the preceding claims, wherein the second aging treatment in step (d) is performed within 10 minutes to 60 minutes, for example 10 minutes, 20 minutes or 60 minutes. 10. An aluminum alloy component formed by the method of any of claims 1-9, preferably the component being an automotive component, aerospace component, railway component, marine component, or consumer electronics component or housing component, such as a unibody component. HK 30137558 A HK 30137558 A HK 30137558 A.