Preparation method for lithium iron phosphate

IN595001BActive Publication Date: 2026-07-10SVOLT ENERGY TECHNOLOGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
IN202317028280
Authority / Receiving Office
IN · IN
Patent Type
Patents
Current Assignee / Owner
Priority Date
2021-05-12
Filing Date
2023-04-18
Publication Date
2026-07-10
Estimated Expiration
2042-04-06

AI Technical Summary

Technical Problem

The existing methods for synthesizing lithium iron phosphate result in lower purity due to impurity phases and irregular particle sizes, which affect the electrochemical performance and energy efficiency.

Method used

A method involving a hydrothermal reaction with a pH buffering agent containing a carboxylate radical, along with a surfactant and carbon source, to control pH and inhibit impurity phase formation, followed by sequential sintering to achieve stable and conductive lithium iron phosphate.

Benefits of technology

This method improves the purity and yield of lithium iron phosphate, enhances its electrical conductivity, and simplifies the production process, leading to better electrochemical performance and reduced energy consumption.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The present invention provides a preparation method for lithium iron phosphate. The preparation method comprises: step S1, mixing an iron source, a phosphorus source and a pH buffer agent to obtain a mixed solution; step S2, subjecting the mixed solution to a hydrothermal reaction to obtain an iron phosphate precursor; and step S3, mixing and sintering the iron phosphate precursor, a lithium source and a carbon source to obtain lithium iron phosphate, wherein the pH buffer agent comprises a compound containing a carboxylate radical. The pH buffer agent containing a carboxylate radical can not only have a complexation function, but also have an extremely significant pH buffering effect, and is crucial for controlling the stability of the whole reaction system, such that the final lithium iron phosphate is in a single phase, and has stable product performance, good fluidity and high conductivity; furthermore, the lithium iron phosphate is used as a positive electrode material to make a battery have excellent electrical properties such as conductivity and rate capability. Moreover, the preparation process is simple, saves energy, and reduces the reaction cost.
Need to check novelty before this filing date? Find Prior Art

Description

Technical FieldThe present disclosure relates to the technical field of synthesis of lithium ironphosphate, and in particular to a method for preparing lithium iron phosphate.BackgroundAs a chemical raw material, iron phosphate has wide application. It plays animportant role in the field of lithium-ion battery materials because of its uniqueelectrochemical performance. In the field of battery materials, iron phosphate hasbecome an ideal electrode material for an electric vehicle battery since it can bedirectly used as an intercalated electrode of a lithium-ion battery, has high thermalstability and good electrochemical cycling performance.Currently, a traditional process employs ammonium dihydrogen phosphate,ferrous oxalate and lithium carbonate to synthesize lithium iron phosphate throughphysically mixing and calcining at a high temperature. Although these methodshave already achieved mass production in the early stage, they are graduallyreplaced by other methods since a product has a particle size which is not easy tocontrol, uneven distribution and irregular morphology.In fact, there are many processes for synthesizing iron phosphate. In modernindustrial production, iron phosphate is generally prepared by employing aprecipitation method with ferric sulfate or other soluble iron salts as an ironsource, phosphoric acid or a phosphate as a phosphorus source, and NaOH as apH regulator. In the preparation process, heating is generally required, and thenthe iron phosphate is used as a precursor and added with lithium carbonate forhigh-temperature synthesis of lithium iron phosphate.Y. Huang kept ferrous sulfate, phosphoric acid and hydrogen peroxide as rawmaterials at a temperature of 80°C in a water bath with a pH in the range of 1-2for 12 hours to obtain iron phosphate, and then used lithium hydroxide as alithium source to prepare a material of lithium iron phosphate with a high rateperformance. However, in actual production, the process has strict requirementson the control of the pH value, which generally needs to be controlled between1.6-2.0, since an impurity of Fe(OH)3 may precipitate when the pH value is toohigh while it will lead to incomplete precipitation of Fe3+ when the pH value is toolow. However, such pH adjustment often leads to generation of a local impurityphase of iron hydroxide due to the too strong alkalinity of NaOH or ammoniumhydroxide. Thereafter, it needs to keep the impurity phase at a high temperaturefor a relatively longer period of time before most of the impurity phase is removed,but there is still a little residue of it, which not only wastes energy, but also affectsthe ratio of phosphorus to iron in the lithium iron phosphate, thereby reducing thepurity and electrochemical performance of the lithium iron phosphate.SummaryA main objective of the present disclosure is to provide a method for preparinglithium iron phosphate, so as to solve the problem of relatively lower purity of alithium iron phosphate material in the prior art.In order to achieve the aforementioned objective, according to one aspect of thepresent disclosure, provided is a method for preparing lithium iron phosphate,which includes: step S1. mixing an iron source, a phosphorus source and a pHbuffering agent to obtain a mixed solution; step S2. subjecting the mixed solutionto a hydrothermal reaction to obtain an iron phosphate precursor; and step S3.mixing the iron phosphate precursor, the lithium source and the carbon source,and sintering that to obtain the lithium iron phosphate, wherein the pH bufferingagent includes a compound containing a carboxylate radical.Further, a molar ratio of the aforementioned pH buffering agent to iron ions in theaforementioned iron source is 0.005-0.05:1.Further, the aforementioned pH buffering agent is selected from any one or moreof chloroacetic acid, ammonium acetate and potassium hydrogen phthalate.Further, a pH value of the aforementioned mixed solution is 2.3-4.8.Further, the aforementioned mixed solution further includes a surfactant, and thestep S1 includes: mixing the iron source and the phosphorus source to obtain afirst solution; and adding the surfactant and the pH buffering agent into the firstsolution to obtain a mixed solution.Further, a ratio of the mass of the aforementioned surfactant to the volume of theaforementioned first solution is 0.1-5 g: 1 L.Further, the surfactant is sodium dodecyl benzene sulfonate and / or sodiumdodecyl sulfate.Further, a pH value of the mixed solution is controlled to be 2.3-4.8 in the processof the aforementioned hydrothermal reaction.Further, a temperature of the aforementioned hydrothermal reaction is 50-90°C.Further, a time of the aforementioned hydrothermal reaction is 5-12 h.Further, stirring is carried out in the process of the hydrothermal reaction.Further, a speed of the aforementioned stirring is 1,000-2,000 r / min.Further, a molar ratio of the aforementioned iron source to the aforementionediron phosphate precursor is 1-1.08:1.Further, the aforementioned iron source is selected from any one or more of ferricsulfate, ferric nitrate and ferric chloride.Further, a process of the aforementioned sintering includes a first section ofsintering and a second section of sintering that are conducted sequentially,wherein a temperature of the first section of sintering is 300-500°C.Further, a time of the aforementioned first section of sintering is 3-6 h.Further, a temperature of the aforementioned second section of sintering is700-750°C.Further, a time of the aforementioned second section of sintering is 8-15 h.Further, the iron phosphate precursor is dried before the first section of sintering.Further, a molar ratio of the aforementioned lithium source to the aforementionedphosphorus source is 1.02-1.06:1.Further, the aforementioned phosphorus source is selected from any one or moreof phosphoric acid, ammonium dihydrogen phosphate and sodium dihydrogenphosphate.Further, the aforementioned lithium source is lithium carbonate and / or lithiumhydroxide.Further, the aforementioned carbon source is 10-25wt% of the total amount of theiron phosphate precursor, the lithium source and the carbon source.Further, the aforementioned carbon source is selected from any one or more ofglucose, fructose and maltose.By applying the technical solution of the present disclosure, the pH bufferingagent containing the carboxylate radical can not only act for complexation, butalso have an extremely significant pH buffering effect, which is critical forcontrolling the stability of the whole reaction system. On one hand, the pHbuffering agent can be complexed with the iron ions in the mixed solution,thereby greatly inhibiting early precipitation of the iron ions in the form of ferrichydroxide, and in turn reducing the content of the impurity phase of ferrichydroxide in the iron phosphate precursor. On the other hand, the pH bufferingagent is used instead of strong alkaline substances such as sodium hydroxide tomake the mixed solution reach a certain pH value, which avoids the generation ofthe local impurity phase of ferric hydroxide caused by too strong alkalinity ofNaOH or ammonium hydroxide, thereby making the lithium iron phosphateobtained after sintering has a simplified phase, a stable product performance, goodflowability and narrow particle size distribution, and finally not only improvingthe purity of the lithium iron phosphate, but also improving the yield thereof.Moreover, the carbon source is converted into a reductive substance such ascarbon, CO and the like in the process of the sintering, which can not only inhibitoccurrence of an oxidative side reaction in the process of the sintering as much aspossible, but also make the carbon included therein partially doped in the lithiumiron phosphate and partially cladded on the surface of the lithium iron phosphate,thereby improving the conductivity of the lithium iron phosphate, and in turnimproving its electrical conductivity. Further, use of the lithium iron phosphate asa positive electrode material makes a battery have excellent electricalperformances such as conductivity and rate capability. In addition, theaforementioned preparation process is simple, energy-saving, and reduces thereaction cost.Detailed Description of the EmbodimentsIt should be noted that the examples in the present application and the features inthe examples can be combined with each other without conflict. The presentdisclosure will be described in detail below with reference to examples.As analyzed in the Background, due to the generation of the local impurity phaseof ferric hydroxide caused by too strong alkalinity of NaOH or ammoniumhydroxide, thereafter it needs to keep the impurity phase at a high temperature fora relatively longer period of time before most of the impurity phase is removed,but there is still a little residue of it, thereby leading to the problem of relativelylower of the prepared lithium iron phosphate in the prior art. In order to solve thisproblem, the present disclosure provides a method for preparing lithium ironphosphate.In a typical embodiment of the present application, provided is a method forpreparing lithium iron phosphate, which includes: step S1. mixing an iron source,a phosphorus source and a pH buffering agent to obtain a mixed solution; step S2.subjecting the mixed solution to a hydrothermal reaction to obtain an ironphosphate precursor; and step S3. mixing the iron phosphate precursor, the lithiumsource and the carbon source, and sintering that to obtain the lithium ironphosphate, wherein the pH buffering agent includes a compound containing acarboxylate radical.The pH buffering agent containing the carboxylate radical can not only act forcomplexation, but also have an extremely significant pH buffering effect, which iscritical for controlling the stability of the whole reaction system. On one hand, thepH buffering agent can be complexed with the iron ions in the mixed solution,thereby greatly inhibiting early precipitation of the iron ions in the form of ferrichydroxide, and in turn reducing the content of the impurity phase of ferrichydroxide in the iron phosphate precursor. On the other hand, the pH bufferingagent is used instead of strong alkaline substances such as sodium hydroxide tomake the mixed solution reach a certain pH value, which avoids the generation ofthe local impurity phase of ferric hydroxide caused by too strong alkalinity ofNaOH or ammonium hydroxide, thereby making the lithium iron phosphateobtained after sintering has a simplified phase, a stable product performance, goodflowability and narrow particle size distribution, and finally not only improvingthe purity of the lithium iron phosphate, but also improving the yield thereof.Moreover, the carbon source is converted into a reductive substance such ascarbon, CO and the like in the process of the sintering, which can not only inhibitoccurrence of an oxidative side reaction in the process of the sintering as much aspossible, but also make the carbon included therein partially doped in the lithiumiron phosphate and partially cladded on the surface of the lithium iron phosphate,thereby improving the conductivity of the lithium iron phosphate, and in turnimproving its electrical conductivity. Further, use of the lithium iron phosphate asa positive electrode material makes a battery have excellent electricalperformances such as conductivity and rate capability. In addition, theaforementioned preparation process is simple, energy-saving, and reduces thereaction cost.In an embodiment of the present application, a molar ratio of the aforementionedpH buffering agent to iron ions in the aforementioned iron source is 0.005-0.05:1.The aforementioned pH buffering agent includes a hydrophilic carboxylate radical,so that it has a relatively better dispersibility in an aqueous phase, thereby beingmore conducive to the coordination between the carboxylate radical of it and theiron ions. Moreover, controlling the molar ratio of the pH buffering agent to theiron ions in the iron source within the aforementioned range is conducive toreducing the precipitation of the iron ions as much as possible, and is also helpfulto control the overall pH value of the mixed solution, so as to reduce the contentof the impurity phase of ferric hydroxide to minimum synergistically.In order to improve the dispersibility of the pH buffering agent in the aqueousphase as much as possible and thus improve the stability of the whole reactionsystem, it is preferred that the pH buffering agent has a small molecular weight,and it is further preferred that the pH buffering agent is selected from any one ormore of chloroacetic acid, ammonium acetate and potassium hydrogen phthalate.Of course, other pH buffering agents can also be selected by those skilled in theart according to actual needs, which will not be described here anymore.In some embodiments of the present application, a pH value of theaforementioned mixed solution is 2.3-4.8, thereby being conducive to improvingthe stability of the iron ions in the mixed solution as much as possible, andreducing the difficulty of pH adjustment in the process of the coprecipitationreaction.In an embodiment of the present application, the aforementioned mixed solutionfurther includes a surfactant, and the step S1 includes: mixing the iron source andthe phosphorus source to obtain a first solution; and adding the surfactant and thepH buffering agent into the first solution to obtain a mixed solution, whereinpreferably a ratio of the mass of the surfactant to the volume of the first solution is0.1-5 g:1 L, and further preferably, the surfactant is sodium dodecyl benzenesulfonate and / or sodium dodecyl sulfate.The surfactant is helpful to control the magnitude of the subsequent particle sizeof the lithium iron phosphate. In order to obtain the lithium iron phosphate with auniform particle size as much as possible, the aforementioned surfactant ispreferred. Of course, other surfactants can also be selected by those skilled in theart according to the actual situation, which will not be described here anymore.In order to improve the efficiency of the aforementioned hydrothermal reaction asmuch as possible and shorten the time of the hydrothermal reaction, preferably inthe process of the aforementioned hydrothermal reaction the pH value of themixed solution is controlled to be 2.3-4.8, preferably the temperature of thehydrothermal reaction is 50-90°C, preferably the time of the hydrothermalreaction is 5-12 h, preferably stirring is conducted in the process of thehydrothermal reaction, and preferably the speed of the stirring is 1,000-2,000r / min. The stirring is conducive to obtaining the lithium iron phosphate with auniform size.In order to have a more appropriate ratio between iron and phosphorus and thelike elements and thus to obtain the lithium iron phosphate with a more stablecomposition synergistically, preferably a molar ratio of the aforementioned ironsource to the aforementioned iron phosphate precursor is 1-1.08:1, and preferablythe iron source is selected from any one or more of ferric sulfate, ferric nitrate andferric chloride.In order to improve the mutual synergistic effect among the iron phosphateprecursor, the lithium source and the carbon source and enable the formed lithiumiron phosphate to have stable and excellent performances, preferably a process ofthe aforementioned sintering includes a first section of sintering and a secondsection of sintering that are conducted sequentially, wherein a temperature of thefirst section of sintering is 300-500°C, and preferably a time of the first section ofsintering is 3-6 h; preferably a temperature of the second section of sintering is700-750°C, and preferably a time of the second section of sintering is 8-15 h.Among them, the first section of sintering at a lower temperature can removesmall molecular substances such as water, carbon dioxide, carbon monoxide andthe like after decomposition of the carbon source, so as to reduce the influence ofthese small molecular substances on the crystallinity of the lithium iron phosphateduring the second section of sintering (at a higher temperature) as much aspossible. In order to reduce the influence of the moisture in the doped ironphosphate precursor on the sintering process, preferably the iron phosphateprecursor is dried before the first section of sintering, and preferably a temperatureof the drying is 200°C.In an embodiment of the present application, a molar ratio of the aforementionedlithium source to the aforementioned phosphorus source is 1.02-1.06:1, preferablythe phosphorus source is selected from any one or more of phosphoric acid,ammonium dihydrogen phosphate and sodium dihydrogen phosphate, andpreferably the lithium source is lithium carbonate and / or lithium hydroxide.The aforementioned ratio of the lithium source to the phosphorus source and theirrespective categories are more helpful to control the ratio of lithium to phosphorusin a composite and more stable lithium iron phosphate molecule.The carbon source generates a conductive carbon substance in the sinteringprocess. In order to further improve the decomposition efficiency of the carbonsource and thus improve the conductivity of the lithium iron phosphate more fully,preferably the aforementioned carbon source is 10-25wt% of the total amount ofthe iron phosphate precursor, the lithium source and the carbon source, andpreferably the carbon source is selected from any one or more of glucose, fructoseand maltose.The beneficial effects of the present application will be illustrated hereafter withreference to specific examples and comparative examples.Example 11.05 parts of ferric trichloride and 1 part of phosphoric acid were weighedaccording to a ratio of 1.05:1 to prepare a first solution in which the molarconcentration of ferric trichloride was 5 mol / L. Then, chloroacetic acid (the ratioof the mass of chloroacetic acid to the volume of the first solution was 2 g:1 L),ammonium acetate (the ratio of the mass of ammonium acetate to the volume ofthe first solution was 2 g:1 L) and sodium dodecyl benzene sulfonate (the ratio ofthe mass of sodium dodecyl benzene sulfonate to the volume of the first solutionwas 0.5 g:1 L) were weighed and added into the first solution, and potassiumhydrogen phthalate was weighed and added into the first solution to prepare a 0.04mol / L solution of the potassium hydrogen phthalate, and then the pH of thesystem was adjusted to 3.5 with sodium hydroxide (0.5 mol / L) and hydrochloricacid (0.5 mol / L), so as to obtain a mixed solution.Then the mixed solution was heated to 70°C, and the materials were allowed toreact through a hydrothermal reaction at a controlled rotation speed of 1,500 r / min.A temperature continuously controlled at 70°C, a pH value of the mixed solutioncontrolled to be 3.5 in the process of the hydrothermal reaction for a time of 8hours. The product was centrifuged, dehydrated and washed for three times. Themoisture content of a wet material was controlled to be 25-35%, and then this wetmaterial was placed into a bowl and dried at 180°C for 48 h to obtain a 3.5-microndisk-type precursor with a thickness of about 100 nm as an iron phosphateprecursor. The iron phosphate precursor was added with lithium hydroxide (withthe molar ratio of lithium hydroxide to phosphoric acid of 1.02:1) and glucose(which was 20wt% of the total amount of the iron phosphate precursor, lithiumhydroxide and glucose), subjected to ball milling with ethanol as a dispersant for 2h, mixed fully, subjected to a first section of sintering at a temperature of 350°Cunder the protection of nitrogen for 5 hours, and then heated to 700°C andcontinued to be subjected to a second section of sintering for 15 hours, Thenobtained 1.029 parts of lithium iron phosphate, and it could be seen upon analysisthat the ratio of iron to phosphorus in this material was 1.01:1.Example 21.03 parts of ferric nitrate and 1 part of phosphoric acid were weighed accordingto a ratio of 1.03:1 to prepare a first solution in which the molar concentration offerric trichloride was 5 mol / L. Then, chloroacetic acid (the ratio of the mass ofchloroacetic acid to the volume of the first solution was 3 g:1 L), ammoniumacetate (the ratio of the mass of ammonium acetate to the volume of the firstsolution was 4 g:1 L) and sodium dodecyl benzene sulfonate (the ratio of the massof sodium dodecyl benzene sulfonate to the volume of the first solution was 1 g:1L) were weighed and added into the first solution, and potassium hydrogenphthalate was weighed and added into the first solution to prepare a 0.04 mol / Lsolution of the potassium hydrogen phthalate, and then the pH of the system wasadjusted to 2.8 with sodium hydroxide (0.5 mol / L) and hydrochloric acid (0.5mol / L), so as to obtain a mixed solution.Then the mixed solution was heated to 90°C, and the materials were allowed toreact through a hydrothermal reaction at a controlled rotation speed of 2000 r / min,a temperature continuously controlled at 70°C, a pH value of the mixed solutioncontrolled to be 2.8 in the process of the hydrothermal reaction for a time of 6hours. The product was centrifuged, dehydrated and washed for three times. Themoisture content of a wet material was controlled to be 25-35%, and then this wetmaterial was placed into a bowl and dried at 180°C for 48 h to obtain a 2-microndisk-type precursor with a thickness of about 100 nm as an iron phosphateprecursor. The iron phosphate precursor was added with lithium hydroxide (withthe molar ratio of lithium hydroxide to phosphoric acid of 1.03:1) and glucose(which was 25wt% of the total amount of the iron phosphate precursor, lithiumhydroxide and glucose), subjected to ball milling with ethanol as a dispersant for 2h, mixed fully, subjected to a first section of sintering at a temperature of 380°Cunder the protection of nitrogen for 5 hours, and then heated to 750°C andcontinued to be subjected to a second section of sintering for 12 hours. Thenobtained 1.004 parts of lithium iron phosphate, and it could be seen upon analysisthat the ratio of iron to phosphorus in this material was 0.995:1.Example 31.01 parts of ferric trichloride and 1 part of phosphoric acid were weighedaccording to a ratio of 1.01:1 to prepare a first solution in which the molarconcentration of ferric trichloride was 5 mol / L, Then, chloroacetic acid (the ratioof the mass of chloroacetic acid to the volume of the first solution was 5 g:1 L),ammonium acetate (the ratio of the mass of ammonium acetate to the volume ofthe first solution was 10 g:1 L) and sodium dodecyl benzene sulfonate (the ratio ofthe mass of sodium dodecyl benzene sulfonate to the volume of the first solutionwas 1.5 g:1 L) were weighed and added into the first solution, and then the pH ofthe system was adjusted to 4.5 with sodium hydroxide (0.5 mol / L) andhydrochloric acid (0.5 mol / L), so as to obtain a mixed solution.Then the mixed solution was heated to 50°C, and the materials were allowed toreact through a hydrothermal reaction at a controlled rotation speed of 1800 r / min,a temperature continuously controlled at 50°C, a pH value of the mixed solutioncontrolled to be 3.5 in the process of the hydrothermal reaction for a time of 7hours. The product was centrifuged, dehydrated and washed for three times. Themoisture content of a wet material was controlled to be 25-35%, and then this wetmaterial was placed into a bowl and dried at 180°C for 48 h to obtain a 4-microndisk-type precursor with a thickness of about 150 nm as an iron phosphateprecursor. The iron phosphate precursor was added with lithium hydroxide (withthe molar ratio of lithium hydroxide to phosphoric acid of 1.02:1) and glucose(which was 15wt% of the total amount of the iron phosphate precursor, lithiumhydroxide and glucose), subjected to ball milling with ethanol as a dispersant for 2h, mixed fully, subjected to a first section of sintering at a temperature of 400°Cunder the protection of nitrogen for 3 hours, and then heated to 720°C andcontinued to be subjected to a second section of sintering for 12 hours. Thenobtained 0.9877 parts of lithium iron phosphate, and it could be seen uponanalysis that the ratio of iron to phosphorus in this material was 0.99:1.Example 4The difference between Example 4 and Example 1 was that,the molar ratio of the total molar weight of chloroacetic acid, ammoniumacetate and potassium hydrogen phthalate to that of the iron ions in ferrictrichloride was 0.05:1, and finally obtained 1.030 parts of the lithium ironphosphate.Example 5The difference between Example 5 and Example 1 was that,the molar ratio of the total molar weight of chloroacetic acid, ammoniumacetate and potassium hydrogen phthalate to that of the iron ions in ferrictrichloride was 0.005:1, and finally obtained 1.0322 parts of the lithium ironphosphate.Example 6The difference between Example 6 and Example 1 was that,the molar ratio of the total molar weight of chloroacetic acid, ammoniumacetate and potassium hydrogen phthalate to that of the iron ions in ferrictrichloride was 0.004:1, and finally obtained 1.0070 parts of the lithium ironphosphate.Example 7The difference between Example 7 and Example 1 was that,the molar ratio of the total molar weight of chloroacetic acid, ammoniumacetate and potassium hydrogen phthalate to that of the iron ions in ferrictrichloride was 0.08:1, and finally obtained 1.0080 parts of the lithium ironphosphate.Example 8The difference between Example 8 and Example 1 was that,the pH value of the mixed solution was 2.3, the pH value of the mixedsolution was controlled to be 2.3 in the process of the hydrothermal reaction, andfinally obtained 1.0301 parts of the lithium iron phosphate.Example 9The difference between Example 9 and Example 1 was that,the pH value of the mixed solution was 4.8, the pH value of the mixedsolution was controlled to be 4.8 in the process of the hydrothermal reaction, andfinally obtained 1.0343 parts of the lithium iron phosphate.Example 10The difference between Example 10 and Example 1 was that,the pH value of the mixed solution was 1.5, the pH value of the mixedsolution was controlled to be 1.5 in the process of the hydrothermal reaction, andfinally obtained 1.0028 parts of the lithium iron phosphate.Example 11The difference between Example 11 and Example 1 was that,the ratio of the mass of sodium dodecyl benzene sulfonate to the volume ofthe first solution was 0.1 g:1 L, and finally obtained 1.0301 parts of the lithiumiron phosphate.Example 12The difference between Example 12 and Example 1 was that,the ratio of the mass of sodium dodecyl benzene sulfonate to the volume ofthe first solution was 5 g:1 L, and finally obtained 1.0353 parts of the lithium ironphosphate.Example 13The difference between Example 13 and Example 1 was that,no sodium dodecyl benzene sulfonate was added, and finally obtained 1.0038parts of the lithium iron phosphate.Comparative Example 1The difference between Comparative Example 1 and Example 1 was that,A sodium hydroxide solution was used instead of chloroacetic acid,ammonium acetate and potassium hydrogen phthalate to adjust the reactionsystem to react under the condition of a pH value of 1.5. The ratio of an impurityphase in the produced product was relatively large. After three times of washingwith a weak acid, the ratio of iron to phosphorus could only reach 1.03:1, and thecapacity was as low as 132 mAh / g.The lithium iron phosphates prepared by the aforementioned Examples 1 to 13and Comparative Example 1 were tested respectively for purities and yields,which were listed in Table 1.Table 1The lithium iron phosphates prepared in the aforementioned Examples 1 to 13 andComparative Example 1 were respectively prepared into positive electrode sheets,and then each of the positive electrode sheets was assembled with a lithium metalnegative electrode and a electrolyte solution of 1mol / L LiPF6 / EC + DMC + DEC(1:1:1) to form a button battery. The button battery was tested for its dischargecapacity and cycling capacity retention rate at a condition of 1C, and the testresults were shown in Table 2.Table 2From the aforementioned description, it can be seen that the aforementionedembodiments of the present disclosure achieve the following technical effects:The pH buffering agent containing the carboxylate radical can not only act forcomplexation, but also have an extremely significant pH buffering effect, which iscritical for controlling the stability of the whole reaction system. On one hand, thepH buffering agent can be complexed with the iron ions in the mixed solution,thereby greatly inhibiting early precipitation of the iron ions in the form of ferrichydroxide, and in turn reducing the content of the impurity phase of ferrichydroxide in the iron phosphate precursor. On the other hand, the pH bufferingagent is used instead of strong alkaline substances such as sodium hydroxide tomake the mixed solution reach a certain pH value, which avoids the generation ofthe local impurity phase of ferric hydroxide caused by too strong alkalinity ofNaOH or ammonium hydroxide, thereby making the lithium iron phosphateobtained after sintering has a simplified phase, a stable product performance, goodflowability and narrow particle size distribution, and finally not only improvingthe purity of the lithium iron phosphate, but also improving the yield thereof.Moreover, the carbon source is converted into a reductive substance such ascarbon, CO and the like in the process of the sintering, which can not only inhibitoccurrence of an oxidative side reaction in the process of the sintering as much aspossible, but also make the carbon included therein partially doped in the lithiumiron phosphate and partially cladded on the surface of the lithium iron phosphate,thereby improving the conductivity of the lithium iron phosphate, and in turnimproving its conductivity. Further, use of the lithium iron phosphate as anpositive electrode material makes a battery have excellent electrical performancessuch as conductivity and rate capability. In addition, the aforementionedpreparation process is simple, energy-saving, and reduces the reaction cost.

Claims

1. A method for preparing lithium iron phosphate, comprising: step S1, mixing an iron source, a phosphorus source and a pH buffering agent to obtain a mixed solution; step S2, subjecting the mixed solution to a hydrothermal reaction to obtain an iron phosphate precursor; and step S3, mixing the iron phosphate precursor, a lithium source and a carbon source, and sintering it to obtain the lithium iron phosphate, wherein the pH buffering agent comprises a compound containing a carboxylate radical.

2. The preparation method according to claim 1, wherein a molar ratio of the pH buffering agent to the iron ions in the iron source is 0.005-0.05:1.

3. The preparation method according to claim 1 or 2, wherein the pH buffering agent is selected from any one or more of chloroacetic acid, ammonium acetate and potassium hydrogen phthalate.

4. The preparation method according to claim 1 or 2, wherein a pH value of the mixed solution is 2.3-4.8.

5. The preparation method according to claim 1 or 2, wherein the mixed solution further comprises a surfactant, and the step S1 comprises: mixing the iron source and the phosphorus source to obtain a first solution; adding the surfactant and the pH buffering agent into the first solution to obtain the mixed solution, wherein a ratio of the mass of the surfactant to the volume of the first solution is 0.1-5 g:1 L, and the surfactant is sodium dodecyl benzene sulfonate and / or sodium dodecyl sulfate.

6. The preparation method according to claim 1 or 2, wherein the pH value of the mixed solution is controlled to be 2.3-4.8 in the process of the hydrothermal reaction, a temperature of the hydrothermal reaction is 50-90°C, and a time of the hydrothermal reaction is 5-12 h.

7. The preparation method according to claim 1, wherein a molar ratio of the iron source to the iron phosphate precursor is 1-1.08:1.

8. The preparation method according to claim 1, wherein a process of the sintering comprises a first section of sintering and a second section of sintering that are conducted sequentially, wherein a temperature of the first section of sintering is 300-500°C, and a time of the first section of sintering is 3-6 h; and a temperature of the second section of sintering is 700-750°C, and a time of the second section of sintering is 8-15 h.

9. The preparation method according to claim 1, wherein a molar ratio of the lithium source to the phosphorus source is 1.02-1.06:1.

10. The preparation method according to claim 1, wherein the carbon source is 10-25wt% of the total amount of the iron phosphate precursor, the lithium source and the carbon source.