Selective depolymerisation of polyamide 6 to produce caprolactam from mixtures of caprolactam-containing polymers and polyurethane-containing polymers, in particular polyurethane block copolymers

IN595050BActive Publication Date: 2026-07-10BASF SE
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
IN202327042913
Authority / Receiving Office
IN · IN
Patent Type
Patents
Current Assignee / Owner
Priority Date
2020-12-17
Filing Date
2023-06-27
Publication Date
2026-07-10
Estimated Expiration
2041-12-14

AI Technical Summary

Technical Problem

Current recycling processes for textiles containing caprolactam-containing polymers and polyurethane-containing polymers, such as spandex, face challenges due to the difficulty in economically and environmentally acceptable recycling, as they require costly and complex solvent-based separation processes, which contaminate caprolactam and pose environmental concerns.

Method used

A process involving depolymerization of mixtures in the presence of 0.05% to 5% by weight of a base at temperatures of 250°C to 350°C and pressures of 5 to 700 mbar, allowing for the selective separation of caprolactam in a gaseous form without prior separation of the polymers, thereby avoiding solvent-based processes.

Benefits of technology

This process enables the selective depolymerization of PA6 from mixtures with polyurethane-containing polymers, resulting in caprolactam with minimal contamination by polyurethane decomposition products, achieving high purity and reducing environmental impact.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

Method for obtaining caprolactam from mixtures of caprolactam-containing polymers and polyurethane-containing polymers, in particular polyurethane block copolymers, by depolymerisation, characterised in that the depolymerisation of the mixture is carried out in the presence of 0.05 to 5 wt.% of a base, at a temperature of 250 to 350°C, at a pressure of 5 to 700 mbar, with the caprolactam being obtained in gas form.
Need to check novelty before this filing date? Find Prior Art

Description

The present invention relates to a process for obtaining caprolactam from mixturesof caprolactam-containing polymers and polyurethane-containing polymers, in particular polyurethane block copolymers, in particular spandex, by depolymerization.The recovery of caprolactam from caprolactam-containing polymers is an importanteconomic concern, especially against the background of ever scarcer resources.Thus for example US 5,233,021 discloses a recycling process of polymeric materialfrom carpets and other multicomponent structures by supercritical fluid extraction.Also, polymer wastes composed of polyamide (nylon 6) are cleaved in a processunder high pressure and using superheated steam and acid (WO 96 / 18613).Caprolactam is also obtainable from mixtures comprising polymeric or thermoplastic molding materials by depolymerization at elevated temperatures in the presence of a base under reduced pressure or in the presence of water (WO 96 / 18614).WO96 / 18612 discloses a process for basic depolymerization of polyamide-containing starting materials under reduced pressure. The resulting caprolactam is withdrawn from the process via the vacuum and sent for further use.None of these processes employ materials comprising caprolactam-containing polymers and polyurethane-containing polymers.However, textile recycling is an important issue in the recycling industry and isfocusing the attention of textile manufacturers to reduce the immense resources required for textile production.Fabrics comprising polyamide fibers (usually caprolactam-containing polymers(PA6)) and polyurethane-containing polymers, in particular polyurethane block copolymers such as for example spandex, are employed in many garments and industrial applications to improve product properties.To produce the polyurethane block copolymers simple linear polyurethanes areformed for example by the diisocyanate polyaddition process. The production of apolyurethane from butylene glycol and hexamethylene diisocyanate for example iswell-suited for fiber production. To form the elastomeric polyurethane block copolymer, a segmented polyurethane, a large part of the glycol is replaced by long-chainpolyether- or polyester-based dihydroxy compounds (macrodiols) having terminalOH groups in the polyaddition reaction.Fabrics made of polyamide fibers (preferably polyamide 6) and polyurethane blockcopolymers can generally vary in the content of spandex relative to the polyamidefiber content. Typical contents are 5-25% by weight of spandex and 95-75% byweight of polyamide.Since polyurethane-containing polymers, particularly spandex, and polyamide polymers have very different chemical properties and production techniques, the fabrics and garments comprising both polymers are very difficult to recycle in an economical and environmentally acceptable manner.The depolymerization in the process disclosed in WO96 / 18612 for example is performed at temperatures at which polyurethanes show thermal instability. The use ofPU (polyurethane)-containing polymers with polyamides, for example PA6 (polyamide 6) / spandex (polyurethane block copolymer) fibers, mixtures of PA6 fibersand spandex fibers or else PA6 fibers coated with polyurethane-containing polymers, in this process can cause the obtained caprolactam to become contaminatedsince the PU (polyurethane) decomposes under the process conditions and the decomposition products are likewise withdrawn via the vacuum.Many known processes are therefore based on the use of solvents for separatingpolyurethane-containing polymers, for example spandex fibers, or polyamide fibersfrom fabrics and garments.To dissolve spandex from an elastomeric fabric, strong polar solvents such as dimethylacetamide (DMAc) or dimethylformamide (DMF) for example are used.They dissolve spandex, leaving behind the polyamide undissolved for separaterecycling. Formic acid and sulfuric acid in turn can dissolve the polyamide and thusseparate spandex for recycling.Gong et al. (Textile Research Journal 0(00) 1-10) examined for example the recycling of PA6 and polyurethane (PU) from mixed PA6 / PU wastes. A solvent (DMF)was employed to selectively dissolve the polyurethane. Filtration afforded pure PA6which can subsequently be sent for recycling after further purification steps.The recycling of PA6 / spandex wastes was also described by Wang et al. (Composites Part B 77 (2015) 232-237). In the disclosed process the spandex was removedby washing with a solvent at high temperatures before the PA6 can be recycled.WO 2013 / 032408 discloses a process for recycling polyamide from elastic fiberscomprising PA6 and spandex. The multi-stage process consists of a controlled thermal decomposition of the spandex proportion which, in a subsequent step, is thendissolved by a suitable solvent (for example ethanol, DMAc, DMF). Separation ofthe solvent makes it possible to obtain polyamide which may be sent for recyclingin a further step.However, common to all known processes is that a costly and complex separationof the polyamide and polyurethane compounds must be performed before the polycaprolactone (PA 6) can be recycled. In addition, a great disadvantage of thesesolvent-based separation processes is the amount of the solvent required and environmental problems potentially resulting therefrom.It is accordingly an object of the present invention to provide a process for obtaining caprolactam from mixtures of caprolactam-containing polymers and polyurethane-containing polymers, in particular polyurethane block copolymers, for example spandex, which does not have the abovementioned disadvantages and allowsdirect selective separation of caprolactam from these mixtures comprising polyurethane-containing polymers without prior separation of the mixtures.It is especially an object of the present invention to provide a process which entirelyavoids solvent-based separation processes.This object has now been achieved by a process for obtaining caprolactam frommixtures of caprolactam-containing polymers and polyurethane-containing polymers by depolymerization of the mixture in the presence of 0.05% to 5% by weightof a base at a temperature of 250°C to 350°C and a pressure of 5 to 700 mbar,wherein the caprolactam is obtained in gaseous form.The object has further been achieved by a process for obtaining caprolactam froma mixture of caprolactam-containing polymers with polyurethane-containing polymers by depolymerization, comprising the steps of:(A) heating the mixture to a temperature of 220°C to 300°C to obtain a melt,(B) adding a base before, during or after step (A),(C) charging the melt into at least one depolymerization reactor,(D) heating the mixture to a temperature of 250°C to 350°C to obtain gaseous caprolactam,(E) discharging the gaseous caprolactam from the depolymerization reactor to leavebehind a residue.The process is preferably performed at a pressure of 5 to 700 mbar.It has surprisingly been found that the process according to the invention makes itpossible to selectively depolymerize PA6 from a mixture comprising polyamide 6and polyurethane-containing polymers - in particular spandex (polyurethane blockcopolymers). The resulting caprolactam is separated via the vacuum and is contaminated only to a small extent, if at all, by decomposition products of polyurethane(PU). To a small extent is to be understood as meaning that the resulting caprolactam comprises 0% to 5% by weight of decomposition products of polyurethane(PU), preferably 0% to 3.5% by weight, particularly preferably 0% to 3% by weight,very particularly preferably 0% to 1% by weight, of decomposition products of polyurethane (PU).Definitions:Spandex: The term "spandex" or "elastane" refers to an elastomeric polyurethaneblock copolymer comprising at least 85% by weight of segmented polyurethanesbased on polyethers, polyesters and / or polycarbonates. Spandex is a segmentedpolymer that exhibits superior stretch and elastic resilience through alternating stiffand flexible segments. The urethane forms stiff, stretched sections that attach longitudinally to one another and ensure the cohesion of the fibers through establishment of secondary bonding forces. By contrast, rubber-like polyalcohols blocks(about 40 to 50 monomer units each) are severely balled up but may easily bestretched. This combination of stiff and elastic blocks achieves exceptionally highextensibility. Spandex is used very widely and is sold as an elastomeric fiber underthat name or under the names elastane (preferred in Europe) or under trade names,such as Lycra (Invista) and ELASPAN (Invista). Typical examples of spandex fibers are described for example in US 4,973,647, EP 0343985, US 6,639,041 (all duPont) and WO03 / 010216.As used herein, the term "elastomeric fabric" refers to any desired fabric containingdifferent sections of spandex fibers and different sections of other synthetic fibersand the term "elastomeric garments" relates to any government which contains different sections of spandex fibers and different sections of other synthetic fibers.The term "polyamide fibers" refers to polyamide fibers, in particular polyamide 6(PA6, polycaprolactam), copolymers, any desired combination thereof or any desired combination thereof with other polyamides.The term "block copolymer" refers to copolymers made up of at least two differentcomonomers A and B, wherein these are in the form of longer sequences or blocks(for example -AAAAAAAAABBBBBBBBBBBB-).A polyurethane block copolymer according to the present invention has a mass fraction of at least 85% polyurethane."Polyurethane-containing polymers" in the context of the present invention refersto polyurethane copolymers (copolymers) and / or polyurethane block copolymers(copolymers with (segmented) polyurethanes), wherein polyurethane block copolymers are particularly preferred.In contrast to polyamides, in particular PA6 (polyamide 6), spandex has a markedlylower heat stability. "Recycling of Polyurethane Foams 2018, page 33" disclosesthe heat stability of polyurethanes at different temperatures. Decomposition of thePU segments commences at temperatures as low as between 200-250°C. Polyamides show no thermal decomposition in these temperature ranges (Pashaei et al.;Chemical Industry and Chemical Engineering Quarterly 17(2):141-151).Despite the low heat stability of spandex fibers the process according to the invention makes it possible to selectively obtain caprolactam from mixtures comprisingpolyurethane-containing polymers, in particular polyurethane block copolymers.According to the invention caprolactam is obtained from mixtures of caprolactamcontaining polymers and polyurethane-containing polymers by depolymerization,wherein the depolymerization of the mixture is performed in the presence of 0.05%to 5% by weight of a base, based on the amount of caprolactam-containing polymers, at a temperature of 250°C to 350°C and a pressure of 5 to 700 mbar andwherein the caprolactam is obtained in gaseous form.The mixtures comprise 75% to 99.9% by weight of caprolactam-containing polymers and 0.1% to 25% by weight of polyurethane-containing polymers, preferably75% to 98% by weight, of caprolactam-containing polymers and 2% to 25% byweight of polyurethane-containing polymers, particularly preferably 75% to 95%by weight of caprolactam-containing polymers and 5% to 25% by weight of polyurethane-containing polymers, very particularly preferably 80-95% by weight ofcaprolactam-containing polymers and 5% to 20% by weight of polyurethane-con25 taining polymers, especially preferably 80% to 98% by weight of caprolactam-containing polymers and 2% to 20% by weight of polyurethane-containing polymers,based on the mass of caprolactam-containing polymers and polyurethane-containing polymers in the mixture.All economically relevant polycaprolactams may be converted into caprolactam bythe process according to the invention, for example also polycaprolactams producedin the presence of mono- or dicarboxylic acids or amines acting as chain regulators,such as acetic acid, propionic acid, benzoic acid, C4-C10-alkanedicarboxylic acidssuch as adipic acid, pimelic acid, suberic acid, azelaic acid, sebacic acid, undecanedioic acid, dodecanedioic acid and mixtures thereof, C5-C8-cycloalkanedicarboxylic acids such as cyclopentane-1,3-dicarboxylic acid, cyclohexane-1,4-di-carboxylic acid and mixtures thereof, benzenedicarboxylic and naphthalenedicarboxylicacids which may bear up to two sulfonic acid groups, wherein this is to be understood as also including the corresponding alkali metal salts, and whose carboxylicacid groups are nonadjacent, such as terephthalic acid, isophthalic acid, naphthalene-2,6-dicarboxylic acid, 5-sulphoisophthalic acid and the sodium and lithiumsalts thereof, and mixtures thereof, and 1,4-piperazine-di(C1-C6-alkanedicarboxylic acids) such as 1,4-piperazinediacetic acid, 1,4-piperazinedipropionic acid, 1,4-piperazinedibutanoic acid, 1,4-piperazinedipentanoic acid, 1,4-piperazinedihexanoic acid.Corresponding copolyamides are known to those skilled in the art and are producible by processes described for example in WO 93 / 25736, DE-A 14 95 198 and DEA 25 58 480.The depolymerization is particularly preferably performed in the presence of 0.05%to 3% by weight of a base, based on the amount of caprolactam-containing polymers.It is very particularly preferably performed in the presence of 0.6% to 2.8% byweight of a base, based on the amount of caprolactam-containing polymers.According to the invention the base employed is selected from the group consistingof alkali metal oxide, alkali metal hydroxide, alkali metal carbonate, alkali metalalkoxide, alkaline earth metal oxide, alkali metal hydroxide and alkaline earth metalcarbonate, such as sodium oxide, potassium oxide, magnesium oxide, calcium oxide, sodium hydroxide, potassium hydroxide, calcium hydroxide, sodium carbonate, potassium carbonate, sodium methoxide, calcium carbonate and magnesium carbonate.The base is particularly preferably a compound selected from the group of: alkalimetal oxide, alkali metal hydroxide, alkali metal carbonate, preferably potassiumhydroxide.According to the invention the depolymerization is carried out in at least one depolymerization reactor, preferably in precisely one depolymerization reactor.In the context of the present invention a depolymerization reactor is to be understood as meaning a horizontal or vertical depolymerization reactor having a mixingand / or conveying means, for example a screw conveyor which is provided alongthe longitudinal axis of the reactor in its interior, for example a kneader reactor ora stirred tank reactor, wherein a horizontal kneader reactor is particularly preferred.According to the invention there may be precisely one depolymerization reactor butit may also be preferable to use at least two depolymerization reactors one behindthe other (in series). It may also be preferable to use at least 2 depolymerizationreactors in parallel.In the case of the at least 2 reactors the resulting caprolactam is preferably combined.In the present invention it is particularly preferable when the water content of themixture during the depolymerization is not more than 5% by weight, preferably notmore than 1% by weight, particularly preferably not more than 0.3% by weight,based on the total mixture.The depolymerization by the process according to the invention is preferably performed at a temperature of 270°C to 350°C. The depolymerization is particularlypreferably performed at a temperature of 280°C to 320°C. The depolymerizationis performed at a pressure of 5 to 700 mbar, preferably 8 to 200 mbar, particularlypreferably at a pressure of 10 to 100 mbar.The residence time in each of the depolymerization reactors is 10 to 300 minutes,preferably from 20 to 200 minutes, in the case of a continuous process.In a further particularly preferred embodiment the process for obtaining caprolactam from a mixture of caprolactam-containing polymers with polyurethane-containing polymers, in particular polyurethane block copolymers, by depolymerization comprises the steps of:(A) heating the mixture to a temperature of 220°C to 300°Cto obtain a melt (S),(B) adding a base before, during or after step (A),(C) charging the melt (S) into at least one depolymerization reactor,(D) heating the melt (S) to a temperature of 250°C to 350°C to obtain gaseous caprolactam (C),(E) discharging the gaseous caprolactam (C) from the depolymerization reactor toleave behind a residue.The corresponding mixture to be depolymerized may be melted in conventionalmelting apparatuses. This is preferably done in an extruder at a temperature of220°C to 300°C, preferably of 230°C to 290°C, to obtain the melt (S). The extruderis, for example, a compounding extruder for plastics processing, preferably a twinscrew extruder.In a preferred embodiment the base is supplied to the melt (S) during step (A). Thisis preferably done in the extruder. Addition in the depolymerization reactor is alsopossible.In a further preferred embodiment the water present is removed from the melt (S)before the depolymerization by subjecting the melt (S) to a reduced pressure of 5to 700 mbar, preferably 8 to 200 mbar, particularly preferably 10 to 100 mbar.This may be done in the extruder and / or the depolymerization reactor.The melt (S) is brought to a temperature of 250°C to 350°C, preferably a temperature of 270°C to 350°C, in at least one depolymerization reactor. Depolymerizationat a temperature of 280°C to 320°C is particularly preferred.The depolymerization is performed at a pressure of 5 to 700 mbar, preferably 8 to200 mbar, particularly preferably at a pressure of 10 to 100 mbar.The water content of the melt (S) during the depolymerization is not more than 5%by weight, preferably not more than 0.3% by weight, particularly preferably notmore than 0.01% by weight, based on the total mixture.The obtained caprolactam is generally continuously discharged from the at leastone depolymerization reactor. When using more than one depolymerization reactorthe resulting caprolactam is preferably combined from all reactors.The purification of the caprolactam obtained according to the invention may beperformed by a conventional process. Examples of purification processes includefor example an acidic or basic distillation such as disclosed in EP0670308 for example.The caprolactam obtained by the process according to the invention has a high purity of 85% to 100% by weight, preferably of 90% to 100% by weight, especiallypreferably 95% to 100% by weight and particularly preferably of 97% to 100% byweight. The caprolactam obtained by the process according to the invention generally has a purity of 90% to 95% by weight.The caprolactam obtained by the process according to the invention comprises 0%to 5% by weight of decomposition products of polyurethane (PU), preferably 0%to 3.5% by weight, particularly preferably 0% to 3% by weight, very particularlypreferably 0% to 1% by weight.The caprolactam obtained by the process according to the invention may be reusedfor producing polycaprolactam or corresponding copolymers and polymer mixtures.This polycaprolactam produced from caprolactam obtained by the process according to the invention or corresponding copolymers and polymer mixtures are advantageously suitable for use for automotive applications and for producing moldingsfor electrical and electronic components, especially also in the high-temperaturerange.A specific embodiment is that of shaped articles in the form of or as part of a component part for the automotive sector, especially selected from cylinder head covers,engine covers, housings for charge air coolers, charge air cooler valves, intakepipes, intake manifolds, connectors, gears, fan impellers, cooling water tanks, housings or housing parts for heat exchangers, coolant coolers, charge air coolers, thermostats, water pumps, heating elements, securing parts or as a constituent of batterysystems for electromobility.Possible uses in automobile interiors are for dashboards, steering-column switches,seat components, headrests, center consoles, gearbox components and door modules, and possible uses in automobile exteriors are for A, B, C, or D pillar covers,spoilers, door handles, exterior mirror components, windshield wiper components,windshield wiper protective housings, decorative grilles, cover strips, roof rails,window frames, sunroof frames, antenna covers, front and rear lights, engine hoods,cylinder head covers, intake pipes, windshield wipers, and exterior bodywork parts.A further specific embodiment is that of shaped bodies as such or as part of anelectrical or electronic passive or active component, of a printed circuit board, ofpart of a printed circuit board, of a housing constituent, of a film, or of a wire, moreparticularly in the form of or as part of a switch, of a plug, of a bushing, of a distributor, of a relay, of a resistor, of a capacitor, of a winding or of a winding body,of a lamp, of a diode, of an LED, of a transistor, of a connector, of a regulator, ofan integrated circuit (IC), of a processor, of a controller, of a memory elementand / or of a sensor.This polycaprolactam or corresponding copolymers and polymer mixtures are further especially suitable for use in lead free soldering, for production of plug connectors, microswitches, microbuttons and semiconductor components, especiallyreflector housings of light-emitting diodes (LEDs).A specific embodiment is that of shaped articles as securing elements for electricalor electronic components, such as spacers, bolts, fillets, push-in guides, screws andnuts.Especially preferred is a molding in the form of or as part of a socket, of a plugconnector, of a plug or of a bushing. The molding preferably includes functionalelements which require mechanical toughness. Examples of such functional elements are film hinges, snap-in hooks and spring tongues.Possible uses of the polyamides of the invention for the kitchen and household sector are for production of components for kitchen machines, for example fryers,clothes irons, knobs, and also applications in the garden and leisure sector, for example components for irrigation systems or garden equipment and door handles.This polycaprolactam or corresponding copolymers and polymer mixtures produced from the caprolactam obtained by the process according to the invention aremoreover advantageously suitable for use in injection molding and extrusion applications, for example in the field of film extrusion and fiber and monofilament production. In the packaging sector the polyamides according to the invention may beemployed for example in monolayer or multilayer blown films, cast films (monoor multilayer), biaxially stretched films (BoPA), laminated films or in extrusioncoatings. Typical fields of application are in the field of foodstuffs packaging aspackaging films, bags or lidding films, for example for packaging meat, poultry,seafood, cheese or coffee. Other preferred fields of application are in medical packaging for packaging syringes and surgical instruments for example, in containersfor packaging cosmetics or in multilayer containers for solvent-containing productssuch as paints, coatings or plant protection products. Further possible applicationsin the field of film extrusion may be found in agricultural films, VARTM films,bubble wrap or general technical films.This polycaprolactam or corresponding copolymers and polymer mixtures are alsopreferentially suitable for producing monofilaments used in fishing lines, fishingnets, offshore fishing lines and ropes. For the possible applications ofmonofilaments include inter alia tennis strings, climbing ropes, bristles and brushes,artificial grass, filaments for 3D printing, grass trimmers, zippers, hook-and-loopfasteners and paper machine clothing.In the field of fiber production this polycaprolactam or corresponding copolymersand polymer blends are preferentially suitable for producing industrial fibers, textilefibers or BCF yarns (carpet fibers). The applications include inter alia fibers forproduction of airbags, ropes, tire cords, textiles, tights, jackets, trousers, carpets,etc.Further suitable applications include the extrusion of semifinished products andthus the production of rods, sheets and pipes, from which a series of further components may be fabricated. These include inter alia sliding elements, spindle nuts,chain conveyors, plain bearings, rollers, wheels, transmissions, gears, rolls, ringgears, screws and spring dampers.Other possible applications include for example pipes, hoses, pipe conduits, cablesheathings, sockets, switches, cable ties, fan wheels etc.The process according to the invention accordingly allows recycling of textilesconsisting both polyamide 6 and polyurethane-containing polymers, in particularspandex, in just a few steps without preceding separation of the components. Theprocess according to the invention allows selective polyamide 6 depolymerizationto afford caprolactam in the presence of polyurethane-containing polymers such asin particular spandex without costly pretreatment to separate the polymers. The obtained caprolactam also has a high purity.MethodsGC method for purity determination of caprolactamTable :Dimethyl adipate (Sigma Aldrich, >99%) is used as internal standard for quantification of caprolactam. A calibration series with pure caprolactam (BASF pure lactam, 99%) was also prepared.Sample preparation:20 mg of internal standard (dimethyl adipate, Sigma Aldrich, > 99%) and 0.1-0.6 gof caprolactam are dissolved in 3-6 ml of isopropanol (Fisher Scientific, >99.8%).The solution is diluted 1:1 with acetone (BASF, pure) and left to stand at roomtemperature for 30 min. The sample is subsequently measured.ExamplesExample 1 (according to the invention)Depolymerization of a PA6 (polyamide 6) / polyurethane block copolymer mixture:An 80:20 PA6 / polyurethane block copolymer mixture (textile from INDITEX / Nextil) (402 g) was admixed with 2% KOH (Bernd Kraft, ultrapure potassium hydroxide pellets) (8 g) and melted in a TCF 2.5 twin-screw kneader (LIST TechnologyAG, Switzerland). A vacuum of 80-100 mbar abs. was then established and at aninternal temperature of 300°C the PA6 in the mixture was depolymerized over 2.5h. The caprolactam formed was withdrawn overhead in gaseous form and then condensed at 74°C. The resulting caprolactam melt was cooled to obtain solid caprolactam. 290 g of caprolactam (90% based on PA6 content of starting mixture) were obtained. The product was analyzed by gas chromatography and had a purity of90% by weight.Examples 2 and 3 (comparative examples) Table :Example 2 was carried out analogously to the inventive example. Ultramid B36was used instead of the 80:20 PA6 / polyurethane block copolymer mixture.Example 3In a twin-screw compounding extruder 15 kg / h of a mixture of Ultramid B3WG6and 2% KOH (Bernd Kraft, ultrapure potassium hydroxide pellets) based on thetotal amount (200 g of KOH per 10 kg of Ultramid B3WG6) were melted at 245°Cand supplied to a CKR 25 C twin-screw kneader reactor with discharge screw (LISTTechnology AG, Switzerland). At a temperature of 271°C and a vacuum of 35 mbarabsolute the obtained polyamide 6 was depolymerized (residence time about 1 h).The caprolactam formed was withdrawn overhead in gaseous form and then condensed at 89°C. The resulting caprolactam melt was cooled to obtain solid caprolactam. The inert constituents, KOH and residual amounts of polyamide 6 wereconveyed continuously via a discharge screw into a collecting vessel which waslikewise under vacuum. 9.68 kg / h of caprolactam (94% based on the PA6 contentof the starting mixture) were obtained. The product was analyzed by gas chromatography and had a purity of 95-97% by weight.Example 4 (inventive)Depolymerization of a PA6 (polyamide 6) / polyurethane block copolymer mixturein a continuous process:In a twin-screw compounding extruder 13 kg / h of a mixture of a PA6 / spandex mixture (80:20) and 2% KOH (Bernd Kraft, ultrapure potassium hydroxide pellets)based on the total amount (200 g of KOH per 10 kg of PA6 / spandex) were meltedat 245°C and supplied to a CKR 25 C twin-screw kneader reactor with dischargescrew (LIST Technology AG, Switzerland).At a temperature of 300°C and a vacuum of 60 mbar absolute the obtained polyamide 6 was depolymerized (residence time about 1 h). The caprolactam formed waswithdrawn overhead in gaseous form and then condensed at 130°C. The resultingcaprolactam melt was cooled to obtain solid caprolactam. The remaining constituents, KOH and residual amounts of polyamide 6 were conveyed continuously outof the kneader reactor via a discharge screw into a collecting vessel which was likewise under vacuum. 9.4 kg / h of caprolactam (94% based on the PA6 content of thestarting mixture) were obtained. The product was analyzed by gas chromatographyand had a purity of 87-88% by weight.

Claims

1. A process for obtaining caprolactam from mixtures of caprolactam-containing polymers and polyurethane-containing polymers, in particular polyure thane block copolymers, by depolymerization, wherein the depolymerization of the mixture is performed in the presence of 0.05% to 5% by weight of a base at a temperature of 250°C to 350°C and a pressure of 5 to 700 mbar and wherein the caprolactam is obtained in gaseous form.

2. The process according to claim 1, wherein the depolymerization of the mixture is performed in the presence of 0.05% to 3% by weight of a base.

3. The process according to claim 1 and / or 2, wherein the depolymerization is performed at a temperature of 270°C to 350°C.

4. The process according to any of claims 1 to 3, wherein the depolymerization is performed at a pressure of 8 to 200 mbar, preferably at a pressure of 10 to 100 mbar.

5. The process according to any of claims 1 to 4, wherein the water content of the mixture during the depolymerization is not more than 5% by weight, preferably not more than 0.3% by weight, particularly preferably not more than 0.01% by weight.

6. The process according to any of claims 1 to 5, wherein the base is a compound selected from the group of: alkali metal oxide, alkali metal hydroxide, alkali metal carbonate.

7. The process according to any of claims 1 to 6, wherein the process is performed in a depolymerization reactor.

8. A process for obtaining caprolactam from a mixture of caprolactam-containing polymers with polyurethane-containing polymers, in particular polyurethane block copolymers, by depolymerization, comprising the steps of: (A) heating the mixture to a temperature of 220°C to 300°C to obtain a melt (S), (B) adding a base before, during or after step (A), (C) charging the melt (S) into at least one depolymerization reactor, (D) heating the melt (S) to a temperature of 250°C to 350°C to obtain gaseous caprolactam (C), (E) discharging the gaseous caprolactam from the depolymerization reactor to leave behind a residue.

9. The process according to claim 8, wherein the water content of the mixture in step (C) is not more than 5% by weight, preferably 0.3% by weight, particularly preferably 0.01% by weight.

10. The process according to either of claims 8 and / or 9, wherein the pressure in step (D) is 5 to 700 mbar, preferaby 10 to 100 mbar.

11. A caprolactam produced by a process according to any of claims 1 to 10.

12. The use of the caprolactam according to claim 11 for producing polyca prolactam- and / or caprolactam-containing copolymers and / or polymer mixtures.

13. The use of the caprolactam according to claim 11 for producing fibers, in particular textile fibers.