Nanocomposite material for photocatalytic dye degradation and hydrogen generation coupled with benzyl alcohol conversion
Patent Information
- Application Number
- IN202411046444
- Authority / Receiving Office
- IN · IN
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2024-06-17
- Publication Date
- 2026-07-16
- Estimated Expiration
- 2044-06-17
AI Technical Summary
Current photocatalytic technologies for water splitting and dye degradation face inefficiencies in hydrogen generation and dye degradation rates, with rapid electron-hole recombination and low visible light utilization, necessitating the development of highly active nanocomposite materials that can also facilitate organic transformations like benzyl alcohol oxidation.
A ternary nanocomposite of BiOI/g-C3N4/MoS2 synthesized via in-situ precipitation, enhancing photocatalytic activity for amaranth dye degradation, hydrogen generation, and benzyl alcohol conversion to benzaldehyde, with improved stability and efficiency compared to conventional catalysts.
The BiOI/g-C3N4/MoS2 nanocomposite demonstrates superior amaranth dye degradation efficiency and remarkable hydrogen generation coupled with selective benzyl alcohol oxidation, maintaining stability across multiple cycles and optimizing reaction conditions for enhanced performance.
Abstract
Description
FIELD OF INVENTIONThe present invention relates to the field of nanocomposites. More particularly itpertains to nanocomposite material for photocatalytic degradation of dye andhydrogen generation coupled with benzyl alcohol conversion. It relates to enhancedphotocatalytic activity of BiOI / g-C3N4 / MoS2 nanocomposite towards amaranth dyedegradation and hydrogen generation incorporated with benzyl alcohol conversion.BACKGROUND OF THE INVENTIONIn recent decades, the world has focused on water and energy concerns. The primarydrivers of the current water pollution and energy crises are population growth andeconomic development. The release of untreated industrial wastewater has resultedin ecological consequences and posed a threat to human health. It is imperative todiscover effective, rapid, and cost-effective methods for treating dyes. In order tomitigate the environmental impact of pollutants, a range of methods, includingadsorption, electrocatalysis, and biodegradation, are employed for the treatment ofthese pollutants. In addition, nearly 80 % of the world's energy supply is dependenton fossil fuels. The energy consumption rate reached 15 TW in 2008, and it hasbeen estimated that this pace will nearly double by 2050 due to the expanding globalpopulation and output. The non-renewable nature of fossil fuels and theirproduction of CO2, a major contributor to global warming, constitute a worldwideenergy crisis that must be addressed immediately.Photocatalytic technology is being used to effectively remove hazardous chemicalsand pathogens from water and air medium and to produce hydrogen gas via a watersplitting process. This technology primarily utilizes solar energy, a sustainableenergy supply, considerably decreases environmental issues and providesnumerous significant advantages over traditional catalytic processes that involvetime-consuming stages, high pressure, and temperature. However, simultaneousproduction of oxygen and H2 is hazardous for the power plant and further increasesthe end product cost due to the need for an extra gas separation step. To tackle thisproblem, most reports take the strategy of using hole sacrifice agents to increase H2production, such as methanol, triethanolamine, sodium sulfite / sodium sulfate, etc.Nevertheless, the utilization of sacrifice agents not only causes a waste of solarenergy in oxidation half-reaction, but also increases the reaction cost and producesunwanted pollutants in liquid. Thus, it is meaningful to utilize the photogeneratedholes to drive useful organic transformations, such as the synthesis of aldehydes byselective oxidation of the corresponding alcohols, instead of the consumption ofsacrificial agent in the photocatalytic system, which will enhance the H2 productionactivity and simultaneously yield value-added chemicals.Hence, the utilization of photocatalytic decomposition technology for hydrogengeneration is seen as a promising solution to address the energy crisis and mitigateenvironmental pollution. Unfortunately, the efficiency of using sunlight tocatalytically decompose water for hydrogen generation is currently quite low.There is a significant disparity between this efficiency and the level required forindustrialization. Consequently, the development of a highly active photocatalyst iscrucial in order to overcome this challenging situation.(https: / / www.sciencedirect.com / science / article / pii / S0147651321012720)(https: / / www.sciencedirect.com / topics / engineering / photocatalytic-hydrogenproduction)(https: / / pubs.rsc.org / en / content / articlelanding / 2024 / ra / d4ra01307g#!divAbstrac)Creating linked photocatalysts or heterojunctions can enhance the efficiency andperformance of a photocatalyst. Several semiconductor photocatalysts, includingzinc oxide, TiO2, ZnS, CdS, Bi2O3, MXene and ferric oxide, have been developedand studied for the degradation of dyes. However, the degradation process istypically slow due to the rapid recombination of electron-hole pairs and the lowutilization of visible light. Thus, there was an immense need for development ofsuch nanocomposite materials, which aids in degradation of dye, generation ofhydrogen, and simultaneously facilitating the oxidation of alcohols toaldehydes.(https: / / www.sciencedirect.com / science / article / pii / S2666386422003769)Drawbacks of Existing Raw materials:Two major problems that humanity faces in the current era are water contaminationand energy shortages. Both of these problems have major ramifications regardingthe environment, human health, and the long-term survival. The previousdrawbacks might include factors such as feasibility, cost-effectiveness, scalability,or limitations in the available technology and materials.Also, the efficiency of using sunlight to catalytically decompose water for hydrogenproduction is currently lacking. There exists a significant disparity between theefficiency achieved and the ability to implement this process on an industrial scale.Consequently, the development of a highly active photocatalyst is crucial in orderto overcome this current predicament. Over the past forty years, there has beensignificant research on catalysts for semiconductor photocatalytic water splitting.This area of study has attracted a lot of attention, and numerous materials have beenidentified for their ability to use light to break down water and generate hydrogen.Innovative Approach by Inventors:The inventors have developed a novel nanocomposite photocatalyst with enhancedcapabilities for degrading amaranth dye, generating hydrogen, and facilitating theoxidation of benzyl alcohol, likely with applications in environmental remediationand clean energy production.The development of the described nanocomposite catalyst represents an innovativeapproach to catalyst design. By leveraging advances in materials science andnanotechnology, the process achieves superior performance compared toconventional catalysts.Prior art PatentsPatent Application No. US11717810B1 discloses "Nanocomposite photocatalyst andmethod of degrading organic pollutant therewith"This above disclosure pertains to a nanocomposite photocatalyst consisting of a carbonnanomaterial, metal oxide nanoparticles, and noble metal nanoparticles. It also includes aprocess for creating the nanocomposite photocatalyst and a method for degrading anorganic dye.Present invention involves a ternary nanocomposite of BiOI / g-C3N4 / MoS2 produced usinga straightforward in-situ precipitation method, whereas the nanocomposite photocatalystdisclosed in aforementioned patent comprises amorphous carbon and graphitic carbon andmetal oxide, thus present invention differs from above cited patent.Patent Application No. 202241077079 discloses "NIR dye sensitized nanocomposite ofnanographene oxide for simultaneous effluent degradation and hydrogen generation"The above invention discloses a nanocomposite that absorbs near-infrared (NIR) light overa broad range in the absorption spectrum and can catalyze both effluent dye degradationand hydrogen creation when exposed to visible light. The NIR-sensitizing nanocompositeVJ-Q2 / r-NGOT / Pt is created through the reaction of VJ-Q2-dye and a core-shellnanostructure of r-NGOT under visible light exposure.The above patent used a VJ-Q2 / r-NGOT / Pt nanocomposite for simultaneous waste waterdegradation and hydrogen generation, while the current invention uses a ternarynanocomposite of BiOI / g-C3N4 / MoS2, thus both the inventions are different.Patent Application No. US10773247B2 discloses "Hollow porous carbon nitridenanospheres composite loaded with AgBr nanoparticles, preparation method thereof,and its application in dye degradation.The above patent reveals a composite material consisting of hollow porous carbon nitridenanospheres filled with AgBr nanoparticles, along with the process of synthesis and its usein dye degradation. The carbon nitride nanocomposite exhibits effective photocatalyticproperties for dye degradation when combined with silver bromide. It offers benefits suchas simple raw material synthesis, stability, and reusability.The above mentioned invention utilizes a porous carbon nitride nanospheres filled withAgBr nanoparticles for photocatalytic degradation of azo dyes whereas the presentinvention discloses ternary BiOI / g-C3N4 / MoS2 nanocomposite for amaranth dyedegradation, hydrogen generation and conversion of benzyl alcohol to benzaldehyde, thusboth the inventions are different.Non-patent literatureMin Wang, Peng Ju, Jiajia Li, Yun Zhao, Xiuxun Han and Zhaomin Hao; Facilesynthesis of MoS2 / g-C3N4 / GO ternary heterojunction with enhanced photocatalyticactivity for water splitting; ACS Sustainable Chemistry & Engineering, 15 August2017, Vol. 5, No. 9, PP 7878-7886The above publication consist of MoS2 / g-C3N4 / graphene oxide (GO) as an effectivephotocatalyst for hydrogen production through solar energy utilization. The combinationof MoS2 and g-C3N4 quantum dots boosts their redox activity in water splitting. This workpresents a new and easy method for creating an effective composite photocatalyst withmany components for energy conversion.The present invention uses a ternary nanocomposite made of BiOI / g-C3N4 / MoS2 tobreakdown amaranth dye, generate hydrogen, and catalyze the conversion of benzylalcohol to benzaldehyde to eliminate water pollutants. While the above invention used aMoS2 / g-C3N4 / graphene oxide nanocomposite solely for hydrogen production with solarenergy. Thus both inventions are different.Mohamed Benaissa, Nadir Abbas, Saleh Al Arni, et.al; BiVO3 / g-C3N4 S-schemeheterojunction nanocomposite photocatalyst for hydrogen production and amaranthdye removal; optical materials, 2021, Vol. 118, No. 9, PP 111237Above cited research article discloses a BiVO3 / g-C3N4 heterojunction containingnanoparticles to degrade amaranth dye through photocatalysis and produce a significantquantity of hydrogen gas.However, the present invention utilizes a ternary nanocomposite consisting of BiOI / g-C3N4 / MoS2 to degrade amaranth dye, produce hydrogen, and catalyze the transformationof benzyl alcohol into benzaldehyde. The present invention employs a distinctnanocomposite that yields a higher rate of amaranth dye degradation compared to themethod disclosed in above mentioned patent. The present invention involves hydrogengeneration coupled with conversion of benzyl alcohol to benzaldehyde, which is notdisclosed in the above invention. Thus, the two inventions are different.Junsheng Li, Li Guan, Liming Jiang, Meiyan Xu, Jiahui Li, Jinlong Zuo, Chong Tan,and Zhi Xia; Construction of 2D / 3D g-C3N4 / BiOI photocatalysts with p-nheterojunction and their performance in photocatalytic degradation of amaranthdye; ACS Omega, 2024, Vol. 9, PP 361-370The above cited article discloses g-C3N4 / BiOI photocatalysts with a distinctivenanomicrosphere structure created by a three-step process that included heatpolycondensation, hydrothermal treatment, and hybrid techniques, utilizing melamine,bismuth nitrate, and potassium iodide as initial substances. The photocatalyst wasthoroughly examined and its effectiveness in degrading amaranth (AR) throughphotocatalysis under different lighting circumstances was studied.The present invention uses a ternary nanocomposite made of BiOI / g-C3N4 / MoS2 to degradeamaranth dye, generate hydrogen, and catalyze the conversion of benzyl alcohol tobenzaldehyde. The current innovation involves adding MoS2 to the nanocomposite toimprove dye degradation, produce hydrogen efficiently, and catalyze the conversion ofbenzyl alcohol to benzaldehyde, a process not covered in the previous work. Therefore, thetwo inventions are distinct.Maria J. Lima, Pedro B. Tavares, Adrian M.T. Silva, Claudia G. Silva, Joaquim L.Faria; Selective photocatalytic oxidation of benzyl alcohol to benzaldehyde by usingmetal-loaded g-C3N4 photocatalysts; Catalysis Today, Published online on 01 June2017, Vol. 287, PP 70-77.The above publication discloses graphitized-carbon nitride (g-C3N4) as photocatalyst forthe selective synthesis of benzaldehyde from benzyl alcohol.The present discovery uses a ternary nanocomposite made of BiOI / g C3N4 / MoS2 to breakdown amaranth dye, generate hydrogen, and catalyze the conversion of benzyl alcohol tobenzaldehyde. The two inventions vary in the substitute replacements used in thenanocomposite g C3N4. The above invention utilized only g-C3N4, while the current oneuses BiOI / MoS2.OBJECT OF THE PRESENT INVENTIONThe main object of the present invention is to disclose a ternary BiOI / g-C3N4 / MoS2nanocomposite synthesized by facile in-situ precipitation method.Another object of the present invention is to disclose the photocatalytic applicationsof this nanocomposite in direct solar light irradiation for amaranth dye degradationand hydrogen generation simultaneously oxidation of benzyl alcohol (BA) intobenzaldehyde (BAL).One more object of the present invention is to disclose a ternary BiOI / g-C3N4 / MoS2nanocomposite which has outstanding stability throughout five cycles.Yet another object of the present invention is to disclose a ternary BiOI / g-C3N4 / MoS2 nanocomposite which can demonstrated remarkable H2 generationcoupled with selective oxidation of BA into BAL.SUMMARY OF THE INVENTIONThe present invention discloses a ternary BiOI / g-C3N4 / MoS2 nanocompositesynthesized by facile in-situ precipitation method. The photocatalytic applicationsof this nanocomposite were evaluated in direct solar light irradiation for amaranthdye degradation and hydrogen generation simultaneously oxidation of BA intoBAL. Nanocomposite demonstrated superior degradation efficiency for amaranthdye after introducing only 2.5% MoS2, in comparison to bare g-C3N4, BiOI andMoS2. Furthermore, throughout five cycles, this invention showed outstandingstability of composite. Additionally, as-synthesized material demonstratedremarkable H2 generation coupled with selective oxidation of BA into BAL.BRIEF DESCRIPTION OF THE DRAWINGSFigure 1: XRD spectrum of (a) bare BiOI, g-C3N4, BC nanocomposites, (b) bareMoS2 and BCM nanocomposites.Figure 2: FTIR spectrum of as-prepared materials.Figure 3: FESEM images of (a-c) bare BiOI, (d-f) bare g-C3N4, and (g-i) BCM-2.5nanocomposite.Figure 4: (a-c) HRTEM images, and (d) SAED pattern of BCM-2.5 nanocompositeFigure 5: XPS spectrum of BCM-2.5: (a) full survey, (a) Bi 4f, (c) O 1s, (d) I 3d,(e) C 1s, (f) N 1s, (g) Mo 3d, and (h) S 2p.Figure 6: N2 physisorption isotherms of as-prepared materials and BJH pore sizedistribution (inset) of BCM-2.5 nanocomposite.Figure 7: (a) Effect of pH, (b) photocatalyst dose and (c) initial drug concentrationon the degradation of amaranth dye.Figure 8: Photolysis, photocatalysis, and adsorption comparison using BCM-2.5nanocomposite.Figure 9: Comparison of degradation of amaranth dye over different photocatalystsunder optimized conditionsFigure 10: Recyclability study of BCM-2.5 nanocomposite for amaranth dyedegradationFigure 11: Effect of photocatalyst dose on photocatalytic H2 generation coupledwith BA oxidation: (a) H2 generation rate, (b) BA conversion and BAL selectivityafter 4 h irradiation under natural solar light.Figure 12: Photocatalytic (a) H2 generation, and (b) BA conversion efficienciesover different photocatalysts.Figure 13: Role of different scavengers in the (a) amaranth dye degradation, and(b) H2 generation coupled with BA oxidation.Figure 14: (a) PL spectrum and (b) EIS curves of as-prepared materialsFigure 15: (a) UV-Vis DRS spectra and (b) Tauc plots of as-prepared materials. (c,d) UV-Vis DRS spectra and Tauc plot of bare MoS2.Figure 16: Mott-Schottky plots of (a) bare BiOI, and (b) bare g-C3N4, and (c) bareMoS2 at 1000 Hz frequency.Figure 17: Plausible mechanism for photocatalytic amaranth dye degradation andH2 generation coupled with BA oxidation over BCM-2.5 nanocomposite.DETAILED DESCRIPTION OF THE INVENTIONThe present invention discloses a ternary BiOI / g-C3N4 / MoS2 nanocompositesynthesized by facile in-situ precipitation method. It has photocatalytic applicationsin direct solar light irradiation for amaranth dye degradation and hydrogengeneration along with simultaneous oxidation of benzyl alcohol (BA) intobenzaldehyde (BAL). The same has an outstanding stability throughout five cycles.Procurement of chemicals- For synthesis, bismuth nitrate pentahydrate(Bi(NO3)3.5H2O, 98%) was procured from Loba Chemie Pvt. Ltd., India. Furtherpotassium iodide (KI, ≥ 99%), ammonium heptamolybdate tetrahydrate((NH4)6Mo7O24.4H2O, ≥ 99%), thiourea (CH4N2S, 99%), triethanolamine (TEOA,C6H15NO3, ≥ 97%), hydrochloric acid (HCl, 36.5-38%), isopropanol (IPA, C3H8O,99%), formic acid (FA, HCOOH, ≥ 98-100%), sodium chloride (NaCl, ≥ 99%), p-benzoquinone (p-BQ, C6H4O2, ≥ 98%), sodium hydroxide pellets (NaOH, ≥ 97%)and amaranth dye were obtained from Merck, India. Benzyl alcohol (BA, C7H8O,99%) and benzaldehyde (BAL, C7H7O, ≥ 99%) were purchased from S D fine-chemPvt. Ltd., India. Melamine (99%) was procured from Sigma Aldrich, USA.Ethylene glycol (C2H6O2, 99%) was purchased from SRL Pvt. Ltd., India andethanol (C2H6O, 99%) from Changshu Hongsheng Fine Chemical, China.Synthesis of BiOI- BiOI is synthesized using simple facile precipitation method.Typically, 1.4552 g Bi(NO3)2.5H2O and 0.4980 g KI is dissolved into 20 mLethylene glycol separately and vigorous stirred until completely mixed. Further,KI solution is added dropwise into the solution of Bi (NO3)2.5H2O with continuousstirring. Afterward, added double distilled water drop wise until orange precipitateof BiOI was found. Then, these orange precipitates were washed with ethanol andwater mixture and dried at 60°C.Synthesis of g-C3N4- Direct heating of melamine was used for the synthesis of g-C3N4 in a muffle furnace. Specific amount of melamine was added to an aluminacrucible that was sealed with a lid and heated at 520 °C for 4 h with heating rate of2°C / min. The as obtained bulk product was properly shredded using a mortar andpestle and further, ultrasonicated for 2 h in ethanol-water mixture (1:1). Lastly,yellow powder precipitates corresponding to g-C3N4 were obtained.Synthesis of MoS2-The synthesis of MoS2 was carried out through hydrothermalmethod. Briefly, 1.5 g of (NH4)6Mo7O24.4H2O and 3.0 g of CH4N2S were dissolvedindividually into 50 mL of double-distilled water. After stirring for 30 min, thereaction mixture was put into a Teflon-lined stainless-steel autoclave and heatedto 240°C for 24 h in a muffle furnace. The obtained precipitate was gently washedmultiple times with an ethanol-water solution, then dried overnight at 60 °C in hotair oven.Synthesis of BiOI / g-C3N4 and BiOI / g-C3N4 / MoS2 composite- BiOI / g-C3N4composite synthesized using simple facile precipitation method. Typically, 0.5432g Bi(NO3)2.5H2O dissolved into 20 mL ethylene glycol and vigorous stirred untilcompletely mixed. In the solution of Bi(NO3)2.5H2O added with 0.4 g of as-synthesized g-C3N4 with molar ratio of 1:1 (BiOI / g-C3N4 (1:1)=BC-11) undermagnetic stirring. Further, KI was dissolved into 10 ml double distilled water andadded dropwise into the above mixture solution with continuous vigorous stirring.Afterwards, obtained precipitate was washed with ethanol and water mixture anddried at 60 °C. Similarly, BiOI / g-C3N4 (1:2)=BC-12, and BiOI / g-C3N4 (2:1)=B-C21 were synthesized. The ternary BiOI / g-C3N4 / MoS2 composite was synthesizedby similar method with addition of MoS2 by x wt.% (x = 1, 2.5, 5), labelled asBiOI / g-C3N4 / 1%MoS2 (BCM-1), BiOI / g-C3N4 / 2.5%MoS2 (BCM-2.5), andBiOI / g-C3N4 / 5%MoS2 (BCM-5).Characterization of synthesized nanocomposite- The prepared nanocompositefurther undergoes characterization studies to determine crystalline, morphological,optical, photoluminescent, and electrochemical properties. The following analysiswere done to determine various characteristics:XRD Analysis: Diffraction peak for g-C3N4 (Fig. 1(a)) at 12.93º and 27.40° werederived from tri-s-triazine ring unit (100) and interlayer stacking of aromaticsegments (002) respectively; Diffraction peaks of BiOI were present along with onelower intensity of g-C3N4 peak. The lower intensity of g-C3N4 might be due togrowth of BiOI on the surface of g-C3N4 and covered the (002) facet. Further, thediffraction peaks (Fig. 1(b)) centered at 14.10°, 33.21°, 39.54°, and 58.79° werecorresponding to (002), (101), (103), and (110) planes of MoS2 hexagonal phaserespectively. The XRD pattern of BCM-2.5 (Fig. 1(b)) exhibited the analogousdiffraction peaks of BiOI and one peak of g-C3N4. However, no peak of MoS2 wasobserved in BCM-2.5 nanocomposite that might be due to lower amount of MoS2.Further, the average crystallite size of BiOI, g-C3N4, and BCM-2.5 nanocompositewas found to be 25.09 nm, 4.64 nm, and 20.60 nm, respectively. It is clearlyobserved that the crystallite size of BCM-2.5 nanocomposite decreased, since, alower crystallite size could contribute to in a greater surface area, and this would beadvantageous for improving the nanocomposite's photocatalytic efficiency.FTIR (Fourier transform infrared) Analysis: As per Fig. 2, BiOI showedcharacteristics peaks at 616.72 cm-1 and 480.26 cm-1 referred to bending andstretching vibration mode of Bi-O bond. In FTIR spectra of g-C3N4, the bandspositioned in the range of 1650-1240 cm-1 and at 809.36 cm-1 were induced bystretching vibrations of C-N / C=N groups in heterocyclic system and breathingmode of tri-s-triazine ring unit, respectively. The characteristic bands in the rangeof 3500-3000 cm-1 and at 1618.06 cm-1 were associated with stretching (υ-OH) andbending (δ-OH) mode of -OH group, presumably arise from surface adsorbedwater. The BC-11 nanocomposite demonstrated the characteristics bands of bothBiOI and g-C3N4. Further, the FTIR spectra of BCM nanocomposites revealed thatthe intensity of 616.72 cm-1 increased with increasing MoS2 amount that verifiedthe interaction of MoS2 with BiOI and g-C3N4.FESEM (Field emission scanning electron microscopy) analysis: FESEMimages of BiOI (Fig. 3(a-c)) discloses flower like microspheres morphologyconsisting of vertically aligned nanosheets. Fig 3(d-f) showed compressed layeredirregular sheets morphology of g-C3N4. Fig. 3(g-i) show FESEM images of the as-prepared BCM-2.5 nanocomposite, revealing that BiOI and MoS2 flowersincorporated on the surface of different sized g-C3N4 sheets. In BCM-2.5nanocomposite, MoS2 exhibited the flower-like morphology comprisingnanosheets with the bending edges, whereas, BiOI nanosheets were verticallyaligned. The BiOI flowers were crumpled into distinct nanosheets and g-C3N4larger sheets collapsed into smaller different sized sheets in BCM-2.5nanocomposite, potentially as a result of nanocomposite formation. This revealedthe robust interaction between BiOI, g-C3N4, and MoS2 in nanocomposite, whichmay aid in boosting the rate of charge transfer.HRTEM (High resolution transmission electron microscopy) analysis:HRTEM images (Fig 4(a-c)) confirmed flower-like morphology of BiOI and MoS2incorporated over g-C3N4 sheets. The HRTEM data Fig. 4(a-c) comparable withFESEM imageries, showed a distinct interaction between BiOI, MoS2 and g-C3N4.Furthermore, the lattice fringes seen in Fig. 5(c) exhibited values of 0.265 nm and0.302 nm, which corresponded to the (101) plane of MoS2 and (102) plane of BiOI,respectively, compatible with XRD results. Fig. 4(d) showed the contours of thedotted circular diffraction rings in the BCM-2.5 SAED signal, indicating thenanocomposite's polycrystalline structure. This, confirm successful synthesis ofnanocomposite.XPS (X-ray photoelectron spectroscopy) analysis: Fig. 5(a) displayed the fullsurvey spectrum of nanocomposite, which exhibited the elemental peaks for Bi 4f,O 1s, I 3d, C 1s, N 1s, Mo 3d, and S 2p. In deconvoluted Bi 4f spectra (Fig. 5(b)),two peaks located at 165.00 eV and 159.66 eV that corresponded to Bi3+ 4f5 / 2 andBi3+ 4f7 / 2, respectively, attributed to the +3 oxidation state of Bi. Moreover, twoextra satellite peaks were also observed at 162.94 eV and 157.67 eV correspondingto Bi 0 metallic. The peaks of O 1s spectra (Fig. 5(c)) centered at 532.86 eV and530.44 eV were corresponding to surface-active oxygen and Bi-O, respectively.Fig. 5(d) demonstrated the I 3d spectra, which displayed the binding energiespositioned at 631.06 eV and 619.56 eV associated to I-1 3d3 / 2 and I-1 3d5 / 2,respectively, revealed the -1 oxidation state of I. The C 1s spectra shown in Fig.5(e) illustrate peaks at 288.67 eV and 285.36 eV consistent with N=C-N in N-containing aromatic ring and C-C bond, respectively. The deconvoluted N 1sspectra (Fig. 5(f)) exhibited two peaks at 400.87 eV and 399.06 eV correspondingto C-N-H and N-C3 groups, respectively. Fig. 5(g) showed the Mo 3d spectrum withthe doublet of Mo4+ 3d3 / 2 and Mo4+ 3d5 / 2 positioned at 232.73 eV and 229.63 eV,respectively, ascribed to +4 oxidation state of Mo. There is also a small peakobserved at 226.49 eV for S 2s. The S spectra in Fig. 5(h) revealed two peaks in 2pregion, with corresponding energies of 165.00 / 162.96 eV for S2- 2p1 / 2 and159.66 / 157.67 eV for S2- 2p3 / 2, indicating the presence of -2 oxidation state of S.These results revealed that the BCM-2.5 nanocomposite was successfullysynthesized and existence of interaction between materials.BET Analysis: From Fig. 6, it was concluded that all the samples exhibited typeIV hysteresis with H3 loop, demonstrating the mesoporous nature of materials. BETanalysis showed that the specific surface area of BC-11, BC-12, BC-21, BCM-1,BCM-2.5, and BCM-5 nanocomposite was higher than the bare BiOI and g-C3N4and the obtained results were summarized in Table 1.Table 1: Surface characteristics of as-prepared materialsFrom table 1 above, it was clearly observed that the surface area of binary BCnanocomposite increased as the amount of g-C3N4 increased. While, surface areawas decreased as g-C3N4 amount increased, which could be agglomeration of g-C3N4 sheets. Further, the surface area of BCM nanocomposites increased as theamount of MoS2 increased (BCM-2.5), could be because the distribution of MoS2flowers with BC-11 nanocomposite. However, increase in the MoS2 amount (B-CM5) in B C-11 nanocomposite, the surface area decreased, which could be the resultof excess amount of MoS2 flowers that accumulated and agglomerated over time.Additionally, the BJH pore size distribution of the BCM-2.5 nanocomposite wasdisplayed in the inset of Fig. 6, and found that it possessed higher pore volume(0.175 cc / g) with pore diameter of 3.635 nm. Thus, the higher surface area and porevolume can provide more active sites, which is significantly enhanced thephotocatalytic activity of catalyst.Estimation of photocatalytic amaranth dye degradation in aqueous phaseBatch studies were carried out to examine the photocatalytic activity of as-synthesized materials toward amaranth dye degradation under natural solar lightirradiations. For photocatalytic evaluation, specific amount of photocatalyst wasdispersed in 100 mL of dye solution (10 mg / L). To achieve adsorption-desorptionequilibrium between the photocatalyst an, the reaction mixture was kept in the darkfor 30 min. Later, the reaction solution was exposed in solar light irradiation and2.5 mL of reaction sample was collected at specific time interval. The collectedsamples were passed through 0.45 μm syringe filter and recorded UV-Vis spectrumusing UV-Vis spectrophotometer.Quantification of photocatalytic H2 generation and conversion of BA into BALThe photocatalytic H2 generation coupled with BA oxidation through water-splitting experiments was carried out in borosilicate round bottom reactor undernatural solar light irradiation. Typically, specific amount of photocatalyst wasdispersed in 25 mL BA aqueous solution. Before conducting photocatalytic studies,the reactor was sealed with septum and purged with N2 to eliminate dissolvedoxygen. Thereafter, the reaction mixture was irradiated under solar light for 4 hwith continuously stirring. The generated H2 was quantified using gaschromatography (GC, 5Å sieve column, Ar as carrier gas) equipped with thermalconductivity detector (TCD). Further, for the BA conversion quantification, thereaction mixture centrifuged and injected into high performance liquidchromatography.Investigation of photocatalytic activityAmaranth dye degradation under solar light irradiationThrough a series of studies, various variables such as the pH of the amaranth dyesolution, catalyst dose, and dye initial concentration were investigated over B-CM2.5, in order to achieve the required optimal conditions. The pH was achieved bymaking multiple solutions (4, 6, 8, and 10) and figuring out the percentage of dyethat degraded at each pH while maintaining consistent values for the otherparameters (catalyst dose of 0.25 g / L and dye concentration of 10 mg / L). As pHincrease from 4 to 6, degradation efficiency increased from 87.53% to 96.02%, asshown in Fig. 7(a). Further, the efficiency of degradation decreased after pH 6(6.30% at pH 8 and 7.97% at pH 10). Consequently, under sun light irradiation, themaximum degrading efficacy was reached at pH 6 in 40 min. Therefore, pH 6 ofthe dye solution was determined to be the optimum pH level for carrying out morestudies.Afterwards, the optimal BCM-2.5 dosage was determined by conductingexperiments with different doses under solar light irradiation. Fig. 7(b) illustrate theeffect of dose with the variation from 0.15 g / L to 0.35 g / L for the photocatalyticamaranth dye degradation (pH of 6 and dye concentration of 10 mg / L). It isobserved that there was a considerable enhancement in photocatalytic efficacy from59.77% to 96.02% upon increasing the photocatalyst dose from 0.15 g / L to 0.25g / L. This could be explained by the increased surface-active sites of photocatalystbeing accessible to degrading processes. However, a slight decrease in thedegradation efficiency (87.66%) was seen with an additional increase inphotocatalyst dose (0.35 g / L). This can be explained by the fact that turbidity growswith an increase in BCM-2.5 concentration, which obstructs light penetration. Thus,the optimized dose for the amaranth dye degradation of BCM-2.5 was found to be0.25 g / L.The next key parameter i.e. the effect of initial dye concentration on the degradationof amaranth dye was examined. Fig. 7 (c) revealed that the 10 mg / L exhibitedmaximum degradation efficiency (96.02%) towards amaranth dye in 40 min undersolar light irradiation (pH of 6 and photocatalyst dose of 0.25 g / L). Whereas, as dyeconcentration increased, the degradation efficiency (77.55% at 20 mg / L and58.94% at 30 mg / L) dropped. The observed decline in photocatalytic efficacy wasattributed to lower capacity of light to penetrate the solution as dye moleculesconcentration increased. Consequently, the dye concentration of 10 mg / L wasobserved to be optimal.Furthermore, to verify superiority of nanocomposite, adsorption and photolysiswere compared. Amaranth dye molecules exhibited extremely modest self-photolysis (1.21%), as seen in Fig. 8, demonstrating the dye's resilience to solarlight. Another study was also conducted to determine the amount of dye adsorbedover the surface of BCM-2.5 in a dark environment. The results showed that BCM-2.5 had absorbed 3.73% of amaranth dye in 40 min under optimized conditions. Itfinds that the BCM-2.5 nanocomposite has excellent photocatalytic activity.After that, under optimal conditions, studies were carried out to validate the potencyof BCM-2.5 in comparison to BiOI, g-C3N4, MoS2, BC-21, BC-11, BC-12, BCM1, and B-CM-5. As indicated in Fig. 9, the photocatalytic efficiencies of the bareBiOI, g-C3N4, and MoS2 were determined to be 20.31, 27.0, and 18.90% in 40 min,respectively. For the BC-21, BC-11, and BC-12 nanocomposites, the degradationefficiency was obtained to be 27.38, 50.26, and 41.52%, respectively. The enhancedactivity of binary nanocomposite was observed when BiOI interact with g-C3N4 inmolar ratio of 1:1 (BC-11), due to the sufficient charge separation pathway ofphotogenerated charge carriers with tuneable band gap. Further, the photocatalyticperformance of BC-11 nanocomposite was improved after addition of MoS2amount. The BCM-1, BCM-2.5, and BCM-5 showed the 71.72, 96.02, and 83.04%degradation efficiency, respectively. However, as an increase in MoS2 on thesurface of BC-11, the photocatalytic activity first increased considerably and thengradually decreased, attributed to the large amount of MoS2 could be prevent thelight absorbing capacity and also shield the surface of BC-11 nanocomposite fromphotocatalytic reaction. This demonstrated that the BCM-2.5 nanocompositeexhibited superior photocatalytic activity towards amaranth dye degradation.Reusability and stability of BCM-2.5 nanocompositeFig. 10 shows a recyclability analysis of the BCM-2.5 nanocomposite for amaranthdye degradation in appropriate experimental circumstances to assess photocatalyststability and durability. To achieve this, a number of cycles were carried out toexamine the recyclable nature of BCM-2.5 for the amaranth degradation process.After 5 cycles, amaranth dye photocatalytic effectiveness dropped from 96.02% to87.66%. Suggesting that BCM-2.5 is a stable and efficient photocatalyst fordegrading organic contaminants.H2 generation coupled with BA selective oxidation under solar light irradiationIn addition to amaranth dye degradation, the nanocomposite was also studied forphotocatalytic H2 generation and BA selective oxidation in presence of solar lightirradiation. As seen in Fig. 11, the effect of photocatalyst dose was investigated forthe H2 generation coupled with selective oxidation of BA. The H2 generation rateinitially increased at 1.0 g / L (1.2522 mmolg-1h-1) of photocatalyst dosage (Fig.11(a)), with 40.07% conversion of BA and 99.40% selectivity of BAL (Fig. 11(b)).This could be caused by increased in active sites on the catalyst surface forphotocatalytic activity. Further, decreased as the dose increased (1.4 g / L), whichcould have been caused by the reaction mixture becoming more turbid, whichdispersed the light irradiation and reduced the system's ability to absorb light. Thus,1.0 g / L was found to be the optimum photocatalyst dosage.Subsequently, experiments were conducted to verify the efficacy of BCM-2.5against BiOI, g-C3N4, MoS2, BC-21, BC-11, BC-12, BCM-1, and BCM-5 with 1.0g / L dosage of photocatalyst. Fig. 12 displayed the rate of H2 generation, theconversion of BA to BAL, and the selectivity for BAL in the presence of differentphotocatalysts. The bare BiOI (0.1138 mmolg-1h-1), g-C3N4 (0.3128 mmolg-1h-1), and MoS2 (0.1956 mmolg-1h-1) were shown lower H2 generation rate (Fig. 12(a))with the conversion efficiencies 31.63% (37.36% selectivity), 19.43% (27.87%selectivity), and 30.37% (33.22% selectivity) of BA (Fig. 12(b)), respectively.Further, the H2 generation rate for the BC-21, BC-11, and BC-12 nanocompositeswere observed to be 0.6116 mmolg-1h-1, 0.9122 mmolg-1h-1, and 0.7590 mmolg-1h-1and 38.67% (79.78% selectivity), 35.54% (85.15% selectivity), and 36.65%(81.36% selectivity) of BA conversion efficiency, respectively. Further, theinclusion of MoS2 increased the BC-11 nanocomposite's photocatalytic efficiency.For the BCM-1, BCM-2.5, and BCM-5, the corresponding H2 generation rate was0.9632 mmolg-1h-1, 1.2522 mmolg-1h-1, and 1.1244 mmolg-1h-1and 37.57%(98.19% selectivity), 40.07% (99.4% selectivity), and 37.31% (99.07% selectivity)BA conversion efficiency, respectively. Whereas, the amount of MoS2 on the BC-11 surface increased, the photocatalytic activity first increased significantly andthen progressively decreased. This is likely because the large amount of MoS2 canboth prevent the BC-11 nanocomposite's surface from being exposed tophotocatalytic reactions and also shield it from light absorption. This revealed thatthe BCM-2.5 nanocomposite showed more proficient photocatalytic activity.Scavenger studyAs illustrated in Fig. 13(a), the inhibitory effect of scavengers NaCl (for h+), FA(for e-), IPA (for -OH radicals), and p-BQ (for -O2- radicals) on the degradation ofamaranth dye was investigated, the results indicated that the degradation efficiencywas 94.91%, 95.24%, 84.40%, and 12.41%, respectively. The obtained resultsdemonstrated a considerable drop in the degradation efficiency in the presence ofp-BQ, suggesting that -O2- played a significant role in the photocatalytic activity,while e-, h+ and -OH contributed a minor role. In addition, the contribution of activespecies to the photocatalytic H2 generation and BA oxidation was also investigatedby introducing FA, IPA, and TEOA as equivalent scavengers of e-, -OH, and h+,respectively. As seen in Fig. 13(b), the H2 generation rate significantly decreasedwhen FA (0.2069 mmolg-1 h-1) was added to the reaction system. This result isconsistent with the observation that H2 is generate via an electron-driven protonreduction process. However, the rate of BA conversion decreased when TEOA(12.24%) was added, and it slightly decreased in presence of IPA. This suggeststhat h+ had important part in the oxidation of BA, whereas -OH had a minorfunction.PL studyThe PL emission spectrum is the result of charge carrier recombination on thesurface of photocatalyst. Fig. 14(a) depicted the PL spectra of as-preparedphotocatalyst under the excitation wavelength of 280 nm. In contrast to BiOI, g-C3N4, MoS2 and binary nanocomposite, the ternary hybrid material of BCM-2.5was found to have a weaker PL intensity. This suggests that composite contributesto the effective electron-hole pair separation, potentially accounting for the higherphotocatalytic activity of the BCM-2.5 nanocomposite.EIS studyTo further comprehend the charge transfer nature and recombination potential ofphotoinduced charge carriers in the photocatalyst, electrochemical analysis (EIS)was also carried out. Fig. 14(b) illustrated the EIS Nyquist plot of BCM-2.5nanocomposite showed a significantly reduced arc radius as compared to bare andbinary materials. This suggests that photogenerated charge carriers in BCM-2.5 aremore efficiently segregated and transferred.UV-Vis DRS analysisUV-Vis DRS was used to analyze the optical properties and band values of the as-prepared materials. The characteristic band edges of BiOI and g-C3N4 were foundat approximately 680 nm and 455 nm, respectively, as shown in Fig. 15(a),demonstrating the superior ability to absorb visible light. On the other hand, MoS2absorbed a wider spectrum (Fig. 15(c)). Further, after the interaction of BiOI andg-C3N4, the absorption region of g-C3N4 shift towards more visible region.Additionally, as the amount of MoS2 in the BC-11 nanocomposite increased, theabsorption shifted a bit toward the lower visible range, while remained higher thang-C3N4 visible region. In next, their optical bandgaps were calculated using theKubelka-Munk function (Fig. 15(b)) by linearly extrapolating the Tauc plot, asgiven below equation:Equationwhereas, photon energy, absorption coefficient, proportionality constant, and bandgap energy are represented by the symbols hv, α, A, and Eg, respectively. For directand indirect semiconductors, the values of 'n' are 2 and 0.5, respectively. The Egvalue of BiOI, g-C3N4, and MoS2 (Fig. 15(d)) was measured to be 1.75 eV, 2.80eV, and 2.10 eV, respectively. For the BC-21, BC-11, BC-12, BCM-1, BCM-2.5,and BCM-5, the Eg value was found to be 1.71 eV, 1.80 eV, 1.78 eV, 1.93 eV, 2.02eV, and 2.29 eV, respectively. The observed data clearly showed that the Eg of thenanocomposite material is less than that of bare g-C3N4. Consequently, a reductionin the energy band to promote the creation of electron-hole pairs and easy passageacross the nanocomposites interface, leading to a marked improvement in thephotodegradation performance of the as-prepared material.Mott-Schottky analysisMott-Schottky plots were also used to examine the band structure andsemiconductor type of BiOI, g-C3N4, and MoS2. As illustrated in Fig. 20, BiOI, g-C3N4, and MoS2 possess positive slopes, demonstrating the distinctivecharacteristic of n-type semiconductors. The BiOI (Fig. 16(a)), g-C3N4 (Fig. 16(b)),and MoS2 (Fig. 16(c)) were found to have flat band potentials (Efb) of +0.477 eV, -1.371 eV, and -0.373 eV (vs Ag / AgCl), respectively. As a result, using the formulaENHE = ESCE + 0.24 eV, the Efb of BiOI, g-C3N4, and MoS2 vs NHE was calculatedto be +0.717 eV, -1.131 eV, and -0.133 eV, respectively. Since the conduction bandedge potential (ECB) of n-type semiconductors is -0.1 eV with respect to Efb, thus,the ECB of BiOI, g-C3N4, and MoS2 were determined to be +0.617 eV, -1.231 eV,and -0.233 eV, respectively. The valence band edge potential (EVB) of BiOI, g-C3N4, and MoS2 was also determined by applying the formula EVB = ECB + Eg,based on the assessed Eg values using the Tauc plot (Fig. 15(b)), which were foundto be +2.367 eV, +1.569 eV, and +1.867 eV, respectively.Plausible mechanism for the photocatalytic activityFollowing that, the electron transport process between BiOI, g-C3N4, and MoS2 wasexamined in in depth, taking into consideration of previously discussed results.These findings implied that photocatalytic activity was carried out by the dual Sscheme pathway that has been postulated. The specific alignment of the energyband edges for BiOI, g-C3N4, and MoS2 was shown in Fig. 17. Given that thematerials are n-type semiconductors, therefore, their respective CB bands andFermi levels (Ef) are near together. Since BiOI and MoS2 (MoS2 and g-C3N4) arenear to other, spontaneous electron flow from MoS2 to BiOI (g-C3N4 to MoS2) willpersist until the Ef reach equilibrium. During this process, BiOI (MoS2) gainselectrons that create a negative charge layer, while MoS2 (g-C3N4) loses electronsand accumulates a positive charge layer. This creates an internal electric field at thecontact that is directed from MoS2 to BiOI (g-C3N4 to MoS2). In the meantime, theband edges will bend, this is noticeable since the band edge of BiOI (MoS2) bendsdownward whereas the band edge of MoS2 (g-C3N4) bends upward. Further,exposure of BCM-2.5 to natural solar light irradiation activated all BiOI, g-C3N4,and MoS2, which aided in the production of photogenerated charge carriers.Through the S-scheme, the electrons that had accumulated in the BiOI CB weremoved to the MoS2 VB, leaving the holes in BiOI. Next, gathered electrons fromthe VB of MoS2 were excited into CB of it and further transferred into VB of g-C3N4, also used for the generation of H2. Furthermore, g-C3N4 VB electrons wereexcited into CB of it and reacted with adsorbed H+ions to form H2 and O2 to produce -O2-, which contributed to amaranth dye degradation. Simultaneously, thephotogenerated holesin the VB of BiOI produce -OH radicals through the oxidationof OHions could be involved in amaranth dye degradation. This is because theirVB potential is higher than the reduction potential of -OH radicals (-OH / H2O =+2.40 eV, -OH / OH- = +1.99 eV). Also, the holes directly contributed in theoxidation of BA.From the above, it can be concluded that the present invention is better in efficacydue to synergistic effect of three ingredients taken together in the form of singlenanocomposite material.The technological advancement of the described process over existing products orprocesses:Synergistic Nanocomposite: The incorporation of BiOI, g-C3N4, and MoS2 into asingle nanocomposite structure offers synergistic effects not present in traditionalcatalysts. This synergistic effect can lead to enhanced catalytic activity due toimproved charge separation, increased surface area, and enhanced light absorption.Enhanced Photocatalytic Activity: The described process demonstrates superiorphotocatalytic activity compared to traditional catalysts. This enhanced activityresults in faster degradation of pollutants such as amaranth dye, more efficienthydrogen generation, and higher conversion rates of benzyl alcohol.Multifunctionality: Unlike many existing processes that focus on a singleapplication, the described process multiple environmental and industrial challenges,including dye degradation, hydrogen generation, and benzyl alcohol conversion,making it more versatile and valuable.Improved Efficiency and Selectivity: The nanocomposite catalyst likely offersimproved efficiency and selectivity in the target reactions. This can lead to higheryields of desired products, reduced energy consumption, and minimized wastecompared to conventional methods.Tailored Reaction Conditions: The process may allow for precise control andoptimization of reaction conditions such as photocatalyst dose, dye concentration,and pH. This tailored approach optimizes the performance of the catalyst, leadingto superior outcomes compared to one-size-fits-all approaches used in existingprocesses.Environmental Impact: The described process utilizes environmentally friendlymaterials, reduces energy consumption, it represents a significant technologicaladvancement aligned with sustainability goals.Potential for Scalability: The process can be scaled up efficiently and cost-effectively, it holds a significant advantage over existing methods that may strugglewith scalability issues. This scalability ensures broader applicability and economicviability of the technology.An inventive approach step lies in the unique combination and configuration ofthese materials to achieve enhanced photo catalytic performance for the specifiedapplications, setting it apart from conventional approaches in the field.The industrial use is evident since the current invention is a formulation designedto remove pollutants from waste water. Water pollutants are widespread issue,therefore a formulation that is extremely effective, easy to access, and has lowadverse effects will be appealing.
Claims
1. A nanocomposite material for amaranth dye degradation, hydrogen generation coupled with oxidation of benzyl alcohol into benzaldehyde wherein the same is BiOI / g-C3N4 / MoS2 i.e., Bismuth oxyiodide / graphitic carbon nitride / molybdenum disulfide.
2. The nanocomposite material as claimed in claim 1 wherein the same has an average crystalline size of 20.60 nm.
3. The nanocomposite material as claimed in claim 1 wherein the same has surface area of 16.861 m2 / g, pore volume of 0.173 cc / g and pore diameter of 3.635 nm.
4. The nanocomposite material as claimed in claim 1 wherein the same possesses flower-like morphology of BiOI and MoS2 incorporated over gC3N4 sheets.
5. The nanocomposite material as claimed in claim 1 wherein 0.25 g / L nanocomposite material degrade 96.02% amaranth dye at pH 6 in 40 minutes under solar radiations.
6. The nanocomposite material as claimed in claim 1 wherein the same adsorb 3 % of amaranth dye in 40 minutes under dark conditions.
7. The nanocomposite material as claimed in claim 1 wherein the same corresponds to 1.2522 mmolg-1 h-1 hydrogen generation rate coupled with 40.04% conversion of benzyl alcohol (BA) and 99.40% selectivity of benzaldehyde (BAL).
8. The nanocomposite material as claimed in claim 1 wherein the same is stable after 5 repetitive amaranth dye degradation cycles.
9. The process for synthesis of the nanocomposite material as claimed in claim 1 is facile precipitation method, wherein the same consists of following steps: - synthesis of BiOI by dissolving 1.4552g Bi(NO3)2.5H2O and 0.4980g KI into 20mL ethylene glycol by vigorous stirring followed by addition of KI dropwise to solution of Bi(NO3)2.5H2O and adding distilled water to obtain orange crystals of BiOI, washing with ethanol and water mixture and dried at 60°C; - synthesis of g-C3N4 by adding melamine to alumina crucible and heating at 520°C for 4 hours with heating rate of 2o C / min, followed by shredding the obtained product and ultrasonication for 2 hours in 1:1 ethanol-water mixture to obtain yellow precipitates of g-C3N4; - synthesis of MoS2 by dissolving 1.5g (NH4)6Mo7O24.H2O and 3.0g CH4N2S into 50mL double distilled water with continuous stirring followed by autoclaving the mixture in Teflon lined stainless steel autoclave at 240°C for 24 hours in muffle furnace; - dissolving 0.5432 g Bi(NO3)2.5H2O into 20 mL ethylene glycol and vigorous stirring for complete mixing; - adding 0.4 g of as-synthesized g-C3N4 with molar ratio of 1:1 (BiOI / gC3N4 (1:1)=BC-11) under magnetic stirring to Bi(NO3)2.5H2O solution. - dissolving KI into 10 ml double distilled water and adding dropwise into the above mixture solution with continuous vigorous stirring. - washing the obtained precipitate with ethanol and water mixture and dried at 60°C. - similarly, BiOI / g-C3N4 (1:2)=BC-12, and BiOI / g-C3N4 (2:1)=BC-21 were synthesized. - addition of MoS2 by x wt.% (x = 1, 2.5, 5) to BiOI / g-C3N4 to produce ternary BiOI / g-C3N4 / MoS2.