Abstract
Description
FIELD OF THE INVENTION:This invention relates to the field of mechanical engineeringParticularly, this invention relates to a mechanical setup for electropolishing.Specifically, this invention relates to a system for electropolishing ofdynamically tuned gyroscope.BACKGROUND OF THE INVENTION:Electropolishing (EP) is a non-conventional based polishing method that levelsand brightens a surface that is being electropolished by forming anelectrochemical cell.Electropolishing has found a multitude of applications in modern manufacturingsectors. Some of these applications include metal additive manufacturedcomponents, reactor vessels, heat exchangers, blenders, storage tanks, pipingand tubing, clean rooms, food and beverage processing equipment, medicalequipment, machined parts, and nuclear applications.Microscale removal of material from a top surface without changing its propertywith complex geometric features through electropolishing is perhaps one of themost effective applications of electrochemical cells.There are three significant aspects to this technology:- selection of electrolyte / s to generate required amount of polishing effect;- selection of cathode material / s; and- to fabricate a tool having a negative replica of a gyroscope's cruciformshaped thin flexural member.The selection of electrolytes is based on the low current density and viscosity ofthe electrolyte. After several trials and errors, the electrolyte is selected.Generally, a gyroscope is used in inertial sensors with gimbal flexures with acruciform shape and thin flexural. The fabrication of these cruciform-shapedthin flexures of thickness 100 μm is challenging by conventional machiningprocesses like milling, turning, etc. Therefore, non-conventional machiningprocesses like electrical discharge machining (EDM), laser beam machining(LBM), ultrasonic machining (USM) have been utilized for the fabrication ofcruciform-shaped thin flexures. However, EDM and LBM are thermoelectricprocesses that leave a recast layer on the surface, which has a tendency topropagate cracks. USM uses abrasive action, which elongates the grainboundary and changes the surface property of the parent material. Also, theseprocesses induce residual stress which reduces the performance of thegyroscope, which is the major disadvantage of these processes. Thus, a postpolishing technique is required to remove these defects. Due to complexgeometry in micron dimensions, conventional polishing methods fail to removethe defects formed during fabrication. Non-conventional polishing methods canbe applied. However, they have certain limitations of their own. Abrasive flowfinishing (AFF) directly contacts the surface and removes the recast layer.However, these abrasive particles elongate the grain boundary of the surfaceand deteriorate the surface property. Electrochemical grinding (ECG) and pulseelectrochemical mechanical polishing (PECMP) processes can polish the macrogeometry, but not miniature surfaces up to 50 nm (Ra). Shot peening andsandblasting are used to finish the complex geometry at the micron range.However, these processes plastically deform the surface. Plastic deformationinduces residual compressive stress in a peened surface, along with tensile stressin the interior. However, for better performance of the gyroscope, the gimbalflexures should not have any kind of stress at the surface.A uniform gap of 50 μm between the gyroscope's cruciform-shaped thinflexural member and the tool is kept for easy removal of gases evolved at anodeand cathode of the electrochemical setup. This gap helps to remove a recastlayer, from the surface, with better surface finish and reflectivity.The electrolyte characteristics such as concentration, temperature, and currentdensity affect process efficiency and surface finishing performance. Theelectrolyte concentration should be at its optimum level; Otherwise, the requiredamount of polishing effect at the gyroscope's surface will not be present. Theposition of the tool at the gyroscope's cruciform-shaped thin flexural memberalso affects the removal of the recast layer. The gap between the tool and thethin flexural member should be optimum such that the variation of the currentdensity during electropolishing should be minimal. The selection of toolmaterial such that it should be inert during electropolishing. After EP, the recastlayer is removed, and the thin flexural member is uniformly polished andimproved corrosion resistance.Therefore, there is a need for a setup that permits the control of theaforementioned requirements.OBJECTS OF THE INVENTION:An object of the invention is to provide a system for electropolishing ofdynamically tuned gyroscope.Another object of the invention is to provide a system for electropolishing ofdynamically tuned gyroscope fabricated by electrical discharge machining toremove the recast layer.SUMMARY OF THE INVENTION:According to this invention, there is provided a system for electropolishing ofdynamically tuned gyroscope.The current invention, disclosed herein, offers one possible solution to theissues of the prior art. The setup eliminates all manufacturing defects andpolishing defects created by conventional polishing processes and gives supersmooth uniform polishing surface with no recast layer to the gimbal flexures.Due to complex geometry, uniform removal of recast layer from thin flexures isvery strenuous. To ensure proper removal of recast layer with no damage to thebase surface, a tool is designed whose shape is the negative replica of thegyroscope's cruciform shaped thin flexural member (1). The gyroscope and thefabricated tool are kept in a container full of electrolyte. The complete setup (9)is used for electropolishing where the gyroscope will act as anode and the toolact as cathode. The anode is switched to positive and the cathode is switched tonegative terminals of the power supply. A magnetic stirrer is used to stir theelectrolyte to easily remove the gases evolved during EP. On applying thepower supply, the controlled anodic dissolution starts, which removes the recastlayer from the thin flexural without any damage to its base material. As the toolis inert, apart from completing the electrolytic cell, it does not influence theanodic dissolution. This setup gives uniform removal of recast layer andprovides highly polished and brighter surface with no surface defects.According to this invention, there is provided a system for electropolishing ofdynamically tuned gyroscope, said system comprising:- a gyroscope fabricated with said thin flexural members forming acruciform shape each flexural member spanning a diameter of saidgyroscope,- a tool, with its operative distal end shape, being a negative replica of saidcruciform shape, said tool having an operatively downward and distallyprotruding part being circumferential protrusions with depressions, asopenings between said protrusions, corresponding to receive operativedistal end portions of said cruciform shape flexural members of saidgyroscope;- said gyroscope shape being a positive replica of said tool'soperative distal end;- said gyroscope being co-axially aligned with said tool;- said gyroscope comprising a central gap, central to its thin flexuralmembers, configured to receive said operatively downward anddistally protruding part of said tool;- a gyroscope holder configured to:- hold said gyroscope such that its cruciform shaped thin flexuralmembers are operatively upside right for removal of its recastlayer;- hold said gyroscope's thin flexural members in a uniformly spacedapart distance from said tool; and- said tool, along with said gyroscope, being configured to be placed in aglass beaker filled with an electrolyte suited for electropolishing of saidgyroscope.In at least an embodiment, said tool being held by a tool holder, said tool beinga threaded tool connected to a threaded tool holder, said tool holder beingconnected to a computer numerical control (CNC) machine's Z-axis for up anddown movement.In at least an embodiment, said tool being held by a tool holder, said tool beinga threaded tool connected to a threaded tool holder, said tool holder beingconnected to a computer numerical control (CNC) machine's Z-axis for up anddown movement, in that, said Z-axis of said CNC machine providing aprovision of threaded grooves to accommodate said tool holder.In at least an embodiment, said tool being held by a tool holder, said tool holderbeing made of Perspex material such that said threaded tool can be attached tosaid threaded tool holder.In at least an embodiment, said tool being a copper tungsten tool.In at least an embodiment, said gyroscope material is maraging steel.In at least an embodiment, said gyroscope being ring-shaped, said gyroscopecomprising:- cruciform-shaped thin flexural members having horizontal thin flexuresspanning a first inner diameter of said gyroscope and vertical thinflexures spanning a second inner diameter of said gyroscope, saidhorizontal thin flexures being perpendicular to said vertical thin flexures;- a lateral circumferential gap between arms of said thin flexures in which adistally protruding part being a negative replica of said tool is received;and- an outwardly protruding shaft, located centrally in said gyroscope, saidshaft being placed, vertically, and being rigid.In at least an embodiment, a gap between said tool and said thin flexuralmember, of said gyroscope, is 50 μm.In at least an embodiment, said gyroscope's holder has a centre hole such thatsaid gyroscope is firmly fixed to it.In at least an embodiment, said gyroscope holder being made of Perspex sheetwith a central hole to accommodate said gyroscope, held vertically, over it.In at least an embodiment, said electrolyte being a composition of acetic acid(CH3COOH) and perchloric acid (HClO4) in a volumetric ratio of 3:1.In at least an embodiment, said system provisioning the selection of:- optimum potential to remove the recast layer from thin flexures withoutaffecting the surface property, in that, range of values of this optimumpotential varies from 4.7 V to 6.2 V;- optimum polishing time such that only recast layer is removed from thesurface and minimizes the anodic dissolution of base material, in that,range of values of this optimum polishing time varies from 120 sec to 480sec;- optimum temperature such that the anodic dissolution increases withoutmuch decrease in the viscosity of the electrolyte, in that, optimumpolishing temperature varies from 30 ºC to 90 ºC; and- optimum speed of magnetic stirrer such that the gas evolved during EPeasily removed and there should not be any turbulence due to stirrer, inthat, optimum magnetic stirrer speed varies from 200 rpm to 800 rpm.BRIEF DESCRIPTION OF THE ACCOMPANYING DRAWINGS:The accompanying drawings constitute a part of the description of theembodiments disclosed herein:Fig. 1 schematically illustrates the tool with its fixture, gyroscope with itsfixture, and comprehensive setup of the electropolishing process;Fig. 2 schematically illustrates the tool and the tool holder assembly unit;Fig. 3 schematically illustrates the tool with a threaded end whose shape is thenegative replica of the gyroscope's thin flexural member;Fig. 4 shows the tool holder arrangement having the provision to hold thethreaded tool, fixed to the CNC Z-axis with Allen bolts;Fig. 5 schematically illustrates the gyroscope with thin flexural and its assemblyunit with the glass beaker;Fig. 6 schematically illustrates the gyroscope's cruciform shaped with thinflexural;Fig. 7 shows the container which holds the electrolyte and the gyroscope holderduring EP; andFig. 8 shows the gyroscope and the tool, placed parallel with a uniform workinggap (8), for the electropolishing to takes place.DETAILED DESCRIPTION OF THE ACCOMPANYING DRAWINGS:According to this invention, there is provided a system for electropolishing ofdynamically tuned gyroscope.The present invention, disclosed herein, is in context to deliver a uniformlysmooth surface finish throughout the polishing of a gyroscope's cruciformshaped thin flexural member without any defects, recast layer, and / or residualstresses.Specifically, the present invention, disclosed herein, relates to anelectropolishing (EP) based finishing process, where cruciform shaped thinflexural members of dynamically tuned gyroscope is uniformly finished byusing a unique design of tool. This electropolishing setup with electrolyte,workpiece fixture, and tool fixture is small and economical.In at least an embodiment, the electropolishing setup consists of an electrolyticcell with anode as workpiece and tool as cathode, dipped in an electrolyte.The selection of electrolyte ensures a highly polished surface with no hazard tothe environment and operator.Design of the tool is such that the recast layer can be easily removed from thethin flexural member. The tool's shape is a negative replica of the gyroscope'scruciform shaped thin flexural member. The tool material selected for theelectropolishing should be inert to the chemicals.According to this invention, a unique tool design for electropolishing processto remove the recast in this specification.Fig. 1 schematically illustrates the tool (1) with its fixture, gyroscope (2) withits fixture, and comprehensive setup of the electropolishing process (9).In at least an embodiment, the invention discloses a unique arrangement for agyroscope's cruciform shaped thin flexural member polishing comprising: anelectropolishing setup with unique tool design and gyroscope fixture, removesthe recast layer without damaging the base material, no residual stresses andimproves the corrosion resistance and makes the surface hydrophilic andreflective; determining the electrolyte with optimum concentration, determiningthe tool material, selection of the optimum voltage for EP to get uniformpolished thin flexural with no recast layer; an optimum gap between the tooland thin flexural for uniform polishing with no pits; an optimum polishing timefor the removal of recast layer from the surface; an optimum temperature of theelectrolyte during EP and optimum magnetic stirrer speed for proper removal ofgas evolved during EP.A linear sweep voltammetry (LSV) (as shown in Figure 9) has been performedto determine constant current region. As per literatures, lower the currentdensity; better is electropolishing. This helps in determining an electrolyte withoptimum concentration. Table 1 presents variation of current density withvarying concentration of perchloric acid in acetic acid.Table 1 Current density for variation of electrolyte concentrationHowever, for Acetic acid: Perchloric acid in the ratio of 4:1, current density is50 mA / cm2, which takes large polishing time.Regarding the tool material, copper tungsten tool is selected as the tool materialas it has high thermal and electrical conductivity with less sensitive to thechemicals at low potential.Regarding the optimum voltage for electropolishing, the voltage correspondingto the constant current and near to breakdown potential, is most suitable forelectropolishing.The gap between the tool and thin flexural member leads to generation ofcurrent density. Larger the gap, smaller will be the current density as shown inTable 2. From simulation, it is observed that for larger gap, current density isnot uniform along the flexural members of gyroscope. Thus, smaller gap isconsidered for uniform current density. Due to experimental constraint, wecannot maintain the gap below 50 μm. Thus, 50 μm is selected as the optimumgap.Table 2 Current density for variation of Interelectrode gapThe polishing time is an important process parameter for the electropolishing.As polishing time increases, more amount of material is removed from thesurface. However, the workpiece in the present case, is an alloy, in whichdifferent element has different anodic dissolution rate. On increasing thepolishing time, surface roughness decreases. However, at higher polishing time,different alloying element starts anodic dissolution, creates pits, surfaceroughness increases. Thus, an optimum polishing time has to be selected forelectropolishing, so as to remove the recast layer. Table 3 shows the variation ofsurface roughness with polishing time.Table 3 Variation of surface roughness with polishing timeOn increasing the temperature of the electrolyte, conductivity of the electrolyteincreases. Thereby, increases the anodic dissolution. However, at higherelectrolyte temperature, the anodic dissolution becomes uncontrolled, leading toan increase in surface roughness. Thus, an optimum polishing temperature hasto be selected for electropolishing, so as to get uniform surface roughness. Table4 shows the variation of surface roughness with polishing temperature.Table 4 Variation of surface roughness with polishing temperatureThe magnetic stirrer helps in the removal of gases during electropolishing.These gas bubbles hinders the anodic dissolution process, thus need to beremoved for proper finishing of component. Table 5 shows the variation ofsurface roughness with magnetic stirrer speed.Table 5 Variation of surface roughness with magnetic stirrer speedThe workpiece fixture is used to hold the gyroscope (2) and the tool (1)attached to a tool holder (4).With the help of electrical discharge machining (EDM), the gyroscope (2) isfabricated with a thin flexural member in a cruciform shape, but the surfaceshave a recast layer, which deteriorates its property. An exact negative replica ofthe thin flexure (1) has been designed and developed such that the microndimension recast layer can be easily removed during electropolishing. Inpreferred embodiments, the gyroscope (2) material is maraging steel.In a least an embodiment, a setup is designed for electropolishing whichaccommodates the electrolyte, the tool (1), the tool holder (4), the gyroscope(2), and its holder (6).In a least an embodiment, tool head and tool holder (4) are provided withthreads such that the tool is fixed. The tool holder (4), along with the tool, isconnected to a computer numerical control (CNC) machine's Z-axis (3) for upand down movement with the help of Allen bolts (5).In a least an embodiment, the gyroscope's holder has a centre hole (6a) suchthat the gyroscope (2) is firmly fixed to it. The tool (1), along with thegyroscope (2), is placed in a glass beaker (7) filled with the electrolyte suitedfor the electropolishing of maraging steel (gyroscope's material).Fig. 2 schematically illustrates the tool (1) and its assembly to the Z-axis (3) of the computer numerical control (CNC) machine. The threaded tool (1) is connected to the tool holder (4), preferably, made of Perspex sheet. The tool holder (4) is attached to the Z-axis of CNC machine (3), preferably, with the help of Allen bolts (5).Fig. 3 shows the tool (1) whose shape is a negative replica of the gyroscope (2) to be fabricated. The tool's upper part has been threaded (1a) to be held firmly in the tool holder (4a). The tool (1) has a protruding part (1c) which protrudes in a gap between the gyroscope's flexure. The negative replica of the gyroscope flexural with horizontal flange and vertical flange is represented by tool (1d & 1e respectively) which, efficiently, removes the recast layer.Fig. 4 shows the tool holding arrangement in which the tool holder (4) isattached to the Z-axis of the CNC machine (3). The Z-axis of the CNC machine(3) has a provision of threaded grooves (3a) to accommodate the tool holder(4). The tool holder (4) is, preferably, made of Perspex material such that the threaded tool (1a) can be attached to the threaded tool holder (4a). The tool holder (4) has four throughout holes (4b), which is used to connect it with the CNC machine (3), preferably, with the help of Allen bolts (5).Fig. 5 shows the gyroscope (2) with the complete assembly unit. The gyroscope(2) is held in an operative vertical position and is placed in the gyroscopeholder. These two are, collectively, placed inside a glass beaker filled withelectrolyte for electropolishing.Fig. 6 shows the gyroscope cruciform shaped thin flexural members withuniform thickness. The horizontal and vertical thin flexures (2a & 2brespectively) are located perpendicular to each other. There is a gap betweenthin flexures (2c) in which the negative replica tool (1c) is placed. Duringelectropolishing, the gyroscope (2) is placed in the fixture especially designedfor it. The gyroscope cruciform (2) consists of an outwardly protruding shaft(2d) which is placed, vertically, in its fixture and is rigid.The thin flexure of the gyroscope is in the form of cruciform. There is agap between thin flexures (2c) in which the protruding part of the tool (1c) will be placed in the close vicinity of the gyroscope for uniform finishing of gyroscope.Fig. 7 shows the glass beaker (7) in which electrolyte is kept duringelectropolishing. The tool (1) along with the gyroscope (2) is dipped into the electrolyte. The glass beaker (7) is non-reactive with respect to the electrolyte and is transparent; thus, making it easy for monitoring during electropolishing. The gyroscope fixture (6) is, preferably, made of Perspex sheet with a central hole (6a) to accommodate the gyroscope (2), held vertically (2d), over it.The gyroscope has a protruding part (2d) which is used to place it atdesired location in the rockets, torpedoes, etc. This part does not requireelectropolishing. The target, of this invention, is to electropolish only the thin gimbal flexure of gyroscope (2a, 2b). The protruding part (2d) is used only to hold the gyroscope.Fig. 8 shows the schematic of the assembly for gyroscope (2) and the tool (1), which is made, preferably, of maraging steel and the copper tungsten,respectively. The tool is an exact negative replica of the gyroscope's cruciform shaped thin flexural members. The uniform gap (8) between the thin flexural and tool is maintained for the uniform removal of material duringelectropolishing. The tool protruding part (1c) will be placed in the gap between thin flexures of the gyroscope (2c).In at least an embodiment, the invention discloses a gyroscope's cruciformshaped thin flexural member polishing, further comprising an electropolishingsetup which consists of a glass beaker to hold the electrolyte, gyroscope fixture, tool holder, magnetic stirrer and temperature probe.In at least an embodiment, the invention discloses a gyroscope's cruciformshaped thin flexural member polishing, further comprising a fixture for holding the gyroscope such that the cruciform shape thin flexural is upside right for the removal of recast layer.In at least an embodiment, the invention discloses a gyroscope's cruciformshaped thin flexural member polishing, further comprising a tool whose shape is the negative replica of the cruciform shape thin flexural. The gap between the tool and thin flexural is uniformly maintained at 50 μm such that uniform removal of recast layer takes place from the thin flexural surface.In at least an embodiment, the invention discloses a gyroscope's cruciformshaped thin flexural member polishing, further comprising the selection ofacetic acid (CH3COOH) and perchloric acid (HClO4) in the volumetric ratio of3:1. This mixture is non-carcinogenic unlike sulfuric acid. It gives a supersmooth surface with improved corrosion resistance and reflectivity.In at least an embodiment, the invention discloses a gyroscope's cruciformshaped thin flexural member polishing, further comprising the selection ofcopper tungsten as a material for tool. Recommended tool material property for EP are high thermal and electrical conductivity. As copper tungsten have high thermal and electrical conductivity, it is selected as tool material.In at least an embodiment, the invention discloses a gyroscope's cruciformshaped thin flexural member polishing, further comprising the selection ofoptimum potential to remove the recast layer from thin flexures withoutaffecting the surface property.The range of values of this optimum potential varies from 4.7 V to 6.2 V.This potential is applied between the workpiece (gyroscope) and the fabricated tool. However, according to literatures, the voltage near the start of gas evolution region i.e., 6V, as shown in Fig. 9, is selected as the optimum potential value.In at least an embodiment, the invention discloses a gyroscope's cruciformshaped thin flexural member polishing, further comprising the selection ofoptimum polishing time such that only recast layer is removed from the surface and minimizes the anodic dissolution of base material.The range of values of this optimum polishing time varies from 120 secto 480 sec. The experimental comparative data is presented in Table 3.In at least an embodiment, the invention discloses a gyroscope's cruciformshaped thin flexural member polishing, further comprising the selection ofoptimum temperature such that the anodic dissolution increases without muchdecrease in the viscosity of the electrolyte.The range of values of this optimum polishing temperature varies from 30ºC to 90 ºC. The experimental comparative data is presented in Table 4.In at least an embodiment, the invention discloses a gyroscope's cruciformshaped thin flexural member polishing, further comprising the selection ofoptimum speed of magnetic stirrer such that the gas evolved during EP easilyremoved and there should not be any turbulence due to stirrer.The range of values of this optimum magnetic stirrer speed varies from200 rpm to 800 rpm. The experimental comparative data is presented in Table 5.The TECHNICAL ADVANCEMENT of this invention lies in providing asetup, for electropolishing, that eliminates all manufacturing defects andpolishing defects created by conventional polishing processes and gives supersmooth uniform polishing surface with no recast layer to the gimbal flexuresWhile this detailed description has disclosed certain specific embodiments for illustrative purposes, various modifications will be apparent to those skilled in the art which do not constitute departures from the spirit and scope of the invention as defined in the following claims, and it is to be distinctly understood that the foregoing descriptive matter is to be interpreted merely as illustrative of the invention and not as a limitation.
Claims
1. A system for electropolishing of dynamically tuned gyroscope, said system comprising: - a gyroscope (2) fabricated with said thin flexural members (2a, 2b) forming a cruciform shape each flexural member spanning a diameter of said gyroscope, - a tool (1), with its operative distal end shape, being a negative replica of said cruciform shape, said tool (1) having an operatively downward and distally protruding part (1c) being circumferential protrusions with depressions, as openings between said protrusions (1c), corresponding to receive operative distal end portions of said cruciform shape flexural members of said gyroscope; - said gyroscope (2) shape being a positive replica of said tool's (1) operative distal end; - said gyroscope (2) being co-axially aligned with said tool (2); - said gyroscope (2) comprising a central gap (2d), central to its thin flexural members (2a, 2b), configured to receive said operatively downward and distally protruding part (1b) of said tool (1); - a gyroscope holder (6) configured to: - hold said gyroscope (2) such that its cruciform shaped thin flexural members (2a, 2b) are operatively upside right for removal of its recast layer; - hold said gyroscope's (2) thin flexural members (2a, 2b) in a uniformly spaced apart distance from said tool (1); and - said tool (1), along with said gyroscope (2), being configured to be placed in a glass beaker (7) filled with an electrolyte suited for electropolishing of said gyroscope (2).
2. The system as claimed in claim 1 wherein, said tool (1) being held by a tool holder (4), said tool (1) being a threaded tool (1) connected to a threaded tool holder (4), said tool holder (4) being connected to a computer numerical control (CNC) machine's Z-axis (3) for up and down movement.
3. The system as claimed in claim 1 wherein, said tool (1) being held by a tool holder (4), said tool (1) being a threaded tool (1) connected to a threaded tool holder (4), said tool holder (4) being connected to a computer numerical control (CNC) machine's Z-axis (3) for up and down movement, in that, said Z-axis of said CNC machine (3) providing a provision of threaded grooves (3a) to accommodate said tool holder (4).
4. The system as claimed in claim 1 wherein, said tool (1) being held by a tool holder (4), said tool holder (4) being made of Perspex material such that said threaded tool (1a) can be attached to said threaded tool holder (4a).
5. The system as claimed in claim 1 wherein, said tool (1) being a copper tungsten tool.
6. The system as claimed in claim 1 wherein, said gyroscope (2) material is maraging steel.
7. The system as claimed in claim 1 wherein, said gyroscope (2) being ringshaped, said gyroscope (2) comprising: - cruciform-shaped thin flexural members having horizontal thin flexures (2a) spanning a first inner diameter of said gyroscope (2) and vertical thin flexures (2b) spanning a second inner diameter of said gyroscope, said horizontal thin flexures (2a) being perpendicular to said vertical thin flexures (2b); - a lateral circumferential gap (2c) between arms of said thin flexures (2a, 2b) in which a distally protruding part (1c) being a negative replica of said tool (1) is received; and - an outwardly protruding shaft (2d), located centrally in said gyroscope (2), said shaft (2d) being placed, vertically, and being rigid.
8. The system as claimed in claim 1 wherein, a gap between said tool (1) and said thin flexural member, of said gyroscope (2), is 50 μm.
9. The system as claimed in claim 1 wherein, said gyroscope's holder has a centre hole (6a) such that said gyroscope (2) is firmly fixed to it.10.The system as claimed in claim 1 wherein, said gyroscope holder (6) being made of Perspex sheet with a central hole (6a) to accommodate said gyroscope (2), held vertically (2d), over it.11.The system as claimed in claim 1 wherein, said electrolyte being a composition of acetic acid (CH3COOH) and perchloric acid (HClO4) in a volumetric ratio of 3:1.12.The system as claimed in claim 1 wherein, said system provisioning the selection of: - optimum potential to remove the recast layer from thin flexures without affecting the surface property, in that, range of values of this optimum potential varies from 4.7 V to 6.2 V; - optimum polishing time such that only recast layer is removed from the surface and minimizes the anodic dissolution of base material, in that, range of values of this optimum polishing time varies from 120 sec to 480 sec; - optimum temperature such that the anodic dissolution increases without much decrease in the viscosity of the electrolyte, in that, optimum polishing temperature varies from 30 ºC to 90 ºC; and - optimum speed of magnetic stirrer such that the gas evolved during EP easily removed and there should not be any turbulence due to stirrer, in that, optimum magnetic stirrer speed varies from 200 rpm to 800 rpm.