Method for Developing and Characterising Core Layer for Sweat Pad from Musa Paradisiaca Waste
Patent Information
- Application Number
- IN202441023792
- Authority / Receiving Office
- IN · IN
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2024-03-26
- Publication Date
- 2026-08-03
- Estimated Expiration
- 2044-03-26
AI Technical Summary
Existing sweat pads for hyperhidrosis often rely on synthetic materials that are not environmentally friendly and may irritate the skin, with complex development methods and high polymer usage.
Development of an ultra-absorbent core layer using fibers extracted from banana flower bracts, blended with wood pulp fibers, processed through a wet-laying technique to create a nonwoven web with enhanced absorbency and eco-friendliness.
The absorbent core layer demonstrates superior sweat and blood absorption capacity, improved comfort, and sustainability, outperforming commercial sweat pads in tests, while being cost-effective and biodegradable.
Abstract
Description
FIELD OF THE INVENTIONThe present invention relates to the field of personal hygiene and healthcare products, specifically focusing on the development and characterization of an ultra-absorbent core layer for sweat pads. The core layer is derived from agricultural waste materials, particularly the flower bracts of Musa paradisiaca (banana). The invention addresses the issue of hyperhidrosis, a condition characterized by excessive sweating, by providing an eco-friendly solution in the form of sweat pads with enhanced liquid absorption properties. BACKGROUND OF THE INVENTIONHyperhidrosis, or excessive sweating, is a prevalent medical condition that significantly impacts individuals' daily lives. Traditional solutions often involve the use of synthetic materials that may not be environmentally friendly. One of the prior art EP3544557 Al, titled "Absorbent Article Comprising Natural Fibres" discloses an absorbent article that incorporates natural fibers, including those derived from plants, to enhance the absorbency and comfort of the product. The application emphasizes the use of natural fibers to improve the ecological footprint of absorbent articles by reducing reliance on synthetic materials.One of the prior art US 5079004, titled "Absorbent Article with High Concentration of Hydrogel Particles," discloses an absorbent article that incorporates a high concentration of hydrogel particles to enhance the absorbency of the product. This patent focuses on improving the liquid retention capacity of absorbent articles by using superabsorbent polymers to manage bodily fluids efficiently.One of the prior art CN105996246 A, titled "Absorbent Material and Method for Preparing Same," discloses an absorbent material comprising natural fibers, specifically focusing on the preparation method that enhances the material's 35 absorbency and liquid retention properties. The application details the use of plant-based fibers to create an absorbent material that is both effective and environmentally friendly.One of the prior art EP 3845084 Al, titled "Absorbent Article Comprising 40 Biodegradable Fibers," discloses an absorbent article that includes biodegradable fibers derived from natural sources. This application focuses on creating eco-friendly absorbent products by incorporating biodegradable materials, aiming to reduce environmental impact while maintaining high absorbency and comfort.45 Yet another prior art One of the prior art W02007 / 026794, titled "Absorbent Structure and Method of Making the Same," discloses an absorbent structure designed to improve liquid absorption and distribution in hygiene products. This application highlights the use of layered absorbent materials, which enhance the efficiency and capacity of liquid retention, making the structure suitable for use in 50 various absorbent articles.However, the existing solutions rely on non-biodegradable polymers, skin-irritating materials, a higher number of polymers, and complex development methods for sweat pads. The present invention has addressed these limitations by initiating the 55 extraction of fibers from banana flower bracts to develop an absorbent core layer for sweat pads.OBJECTIVES OF THE INVENTION1. The primary object of the present invention is to develop and characterise 60 core layer for Sweat Pad from Musa Paradisiaca waste.2. Another object of the present invention is to extract fibres from banana flower bracts manually after drying and combing, blending them with woodpulp fibres, and utilizing wet-laying technique to develop absorbent core layer for sweat pad application.A further object of the present invention is to develop a cost-effective and eco-friendly absorbent core layer for sweat absorption application. A further object of the present invention is to blend fibre by working on different proportions of banana fibre and wood pulp fibre blends to achieve an integrated structure that maximizes absorbency and comfort. It is an object of the present invention to develop a method that offers superior absorption properties and also contributes to sustainability by repurposing agricultural waste.SUMMARY OF THE INVENTION It will be understood that this disclosure is not limited to the particular systems and methodologies described, as there can be multiple possible embodiments of the present disclosure which are not expressly illustrated in the present disclosure. It is also to be understood that the terminology used in the description is for the purpose of describing the particular versions or embodiments only, and is not intended to 80 limit the scope of the present disclosure.To achieve the objects, the present invention relates to a method for developing and characterising core layer for sweat pad from musa paradisiaca waste. It is one aspect of the present invention to extract the fibres from banana flower bract waste by drying the bracts for 4 days and peeling by combing process. 85 It is another aspect of the present invention to characterize the extracted banana flower fibres for their fundamental properties such as FTIR, SEM, XRD, fibre density, fibre burning identification test, water absorbency, moisture regain and content analysis.It is one aspect of the present invention which involves blending the banana flower 90 fibres with wood pulp(WP) in different weight ratio.It is another aspect of the present invention to develop wet laid nonwoven webs by using 75:25, 50:50, 25:75 combinations of banana flower and wood pulp fibres. It is further aspect of the present invention where the sweat and blood absorbency, contact angle measurement of wet laid samples and absorbent core layer of95 commercial sweat pad are analyzed and the presence of OH groups and pores / hollow structure of fibre in wet laid sample increase the liquid absorbency, thereby improving sweat and blood absorbency.Hence the present invention utilizes a sustainable approach to develop absorbent core for sweat pad application using banana flower fibres from banana bract waste. 100 Additionally, it is ecofriendly, biodegradable and cost effective compared to the commercial sweat pad's absorbent core layer.BRIEF DESCRIPTION OF DRAWINGS:The embodiment of the present invention is illustrated with the help of 105 accompanying drawings.Figure 1 illustrates the wet laying processFigure 2 illustrates the flowchart of preparation and characterization of web Figure 3 illustrates the graph of FTIR spectra of fibreFigure 4 illustrates the graph indicating the XRD pattern of banana flower fibre 110 Figure 5 illustrates the SEM analysis of fibreFigure 6 illustrates the absorption capacity of test samples and commercial sweat pad in artificial sweat and blood solutionFigure 7 illustrates contact angle measurement of three wet laid webs and commercial sample using distilled waterDETAILED DESCRIPTION OF INVENTION:The following detailed description illustrates by way of example and not by way of limitations. Embodiments of the present disclosure will be described more fully hereinafter with reference to the accompanying drawings in which like numerals 120 represent like elements throughout the several figures, and in which example embodiments are shown.With reference to figure 1, the process of extracting and processing banana fibre to create nonwoven fabrics involves: Raw banana flower bracts are collected (101) 125 and subjected to combing and manual peeling to extract the fibres (102). Theseextracted banana flower fibres are then mixed with wood pulp (103) in varying proportions (e.g., 75:25, 50:50, 25:75). The mixed fibres are dispersed in water and stirred using a magnetic stirrer (104) to form a homogeneous slurry. This slurry is then poured into a wet-lay container (105), where the water is drained, allowing the 130 fibres to settle and form a nonwoven web. The formed web is pressed and dried at a suitable temperature (e.g., 60°C) to remove residual moisture (106). The final product is a nonwoven fabric (107) composed of a blend of banana fibre and wood pulp, which can be used for various applications such as absorbent core layers.135 With reference to figure 2, illustrates fiber extraction, the process of nonwoven web formation from the fiber stage to testing stage.Extraction of Banana Flowers fibre:Banana flowers are collected. 140 Bract Removal: The banana bracts are removed from the flowers.Drying: The bracts are dried at room temperature to reduce moisture content. Combing and Peeling: The fibres are extracted from the bracts using a combination of combing and manual peeling. Cleaning: The extracted fibres are cleaned thoroughly. 145 Sorting and Storage: The fibres are sorted and stored for further processing.Web Formation:Wet laying using banana flowers fibre and wood pulp in ratio of 25:75, 50:50, 75:25:The extracted banana flowers fibres are mixed with wood pulp in different ratios 150 (25:75, 50:50, 75:25) and then dispersed in water to form a slurry. This slurry is then poured into a wet-lay container, where the water is drained, allowing the fibres to settle and form nonwoven webs.Web Formation: The slurry is poured into a wet-lay container, and the water is drained to form a nonwoven web. 155 Pressing and Drying: The web is pressed and dried at 60°C for 30 minutes.Applications: Wet-laid Absorbent Core Layer: The nonwoven web is used as acore layer in absorbent products like diapers, sweat pad and sanitary napkins.Characterization of banana flower fibre and the Core Layer:The core layer's absorbency is tested by immersing samples in artificial sweat at room temperature, with weight measurements taken at regular intervals to calculate the percentage of sweat absorption. Contact angle measurements are conducted using an Optical Tensiometer to determine the surface wettability of the core layer. The extracted banana fiber (BF) is characterized using Fourier Transform Infrared Spectroscopy (FTIR), Scanning Electron Microscopy (SEM), X-ray Diffraction (XRD), fiber density, burning test, moisture regain and moisture content analysis, determination of water absorbency of Banana fibre. The FTIR spectrum of the extracted fibre is shown in Figure 3. The presence of the C-0 stretching of alcohol in cellulose, lignin, and hemicelluloses is evidenced by the peak at 1032 cm-1. This peak indicates the presence of these components in the fibre. The peak at 1631 cm-1 corresponds to the C=C stretching of alkenes found in lignin, confirming the presence of lignin in the fibre. Finally, the peak at 3336 cm-1 indicates the OH stretching of hydrogen-175 bonded alcohol, further supporting the presence of cellulose, lignin, and hemicelluloses in the fibre. These findings suggest that the extracted fibre is primarily composed of cellulose, lignin, and hemicelluloses, which are common components of plant fibres.With reference to figure 4, the X-ray diffraction pattern of the fibre is given. Peaks 180 observed at approximately 20 = 16 and 22 are attributed to the cellulose (110) and (002) indicating the presence of cellulose in the fibre. The broad peak (002) observed in banana flower fibre confirmed that microcrystalline polymer due to small crystallites as like in the cotton fibre.With reference to figure 5, Scanning electron microscopy (SEM) images are185 acquired for the fibre extracted from banana flower bract. The longitudinal andcross sectional view of the fibre are given in Figure 5 (a) and (b) where figure 5 (a)represents the longitudinal view of SEM analysis of BF fibre and 5 (b) represents Cross-sectional view of SEM analysis of fibre. In the longitudinal view of the fibre surfaces, the measured fibre diameter is approximately 90.03 μm. In the cross-190 sectional view, the raw fibre exhibits a porous structure, and the measured pore diameter is approximately 25.84 μm. The cross sectional view of fibre shows finer hollow / porous structure, which may enhance the absorption property of the fibre.Determination of Fibre DensityThe density column is prepared per ASTM D3 800-99 standards. Banana flower 195 bract fibre is introduced into the density column in the form of a small ball. The fibre exhibited floatability within the volume range of 30 ml to 40 ml. The determined density of the banana flower bract fibre is found to be 1.37 g / cc.Burning Test200 The combustion of the fibre when exposed to an open flame emitted an odour similar to burning paper. The resulting ash showed a powdery consistency and a grey colour. The burning characteristic of the banana flower fibre is identical to burning behaviour of cellulosic fibres.205 Determination of Moisture Content and Moisture RegainThe moisture content and moisture regain of the BF fibre are given in Table 1. This test is conducted as per the gravimetric principle. The moisture content and moisture regain of the banana flower's bract fibre is high due to the presence of porous structure and hydrophilic functional groups(OH) which are confirmed by 210 SEM and FTIR analysis. The moisture regains value of the fibre is more than other existing cellulosic fibres (Hearle & Morton 2008).Table 1: Moisture content and moisture regain of the fibreSAMPLE MOISTURE CONTENT (%) MOISTURE REGAIN (%)Banana flower bract fibre 13.6 15.87(The test is carried out as per gravimetric method)Determination of Water AbsorbencyAs per the standard ASTM D 570, about 0.03 g of fibre is immersed in distilled water for 10-minute time intervals within 1 hour at room temperature. After every 10 minutes, samples are taken out from test liquid and hung for 5 minutes. Then weight of the sample is determined using a precise digital weighing balanc to 220 calculate the water absorption percentage (Abul Shahid et al. 2021). The fibre exhibited absorption capacity about 1200% due to the presence of multi-capillary tubes, pores, and high lignin content (higher OH group), as revealed in FTIR and SEM analyses. The absorbency of test sample is determined by using below formula.225 Water Absorption (%) = [(wet weight - dry weight) / (dry weight)] * 100Determination of Sweat and Blood Absorbency of Wet-laid sample The absorption capacity of the wet-laid non- woven webs and commercial sweat pad in artificial sweat and blood solution is given in Figure 6 (a) and (b). The 230 artificial sweat is prepared as per standard with a pH of 6.5 is formulated in accordance with the European standard EN1811. The formulation involved the meticulous blending of specific components in deionized water, including 0.1 wt% urea, 0.5 wt% sodium chloride (NaCl), and 0.1 wt.% lactic acid. The synthetic blood is prepared as per the standard ASTM F1670 standard. 235 With reference to figure 6, Figure 6 (a) and 6 (b) shows sweat absorption capacity of the wet-laid non-woven webs in artificial sweat and blood solution. In figure 6(a), the absorption capacity of 75:25, 50:50, 25:75, and commercial sweat pad sample is found to be approximately 1148%, 1044%, 846%, and 740%, respectively. The 75:25 sample showed 9.6%, 26.2%, and 35.5% higher absorption 240 percentage than other samples. Figure 6(b) showed the absorption capacity of test samples and commercial sweat pad in synthetic blood solution. Meanwhile the 75:25 sample showed 32%, 61% and 59.9% higher absorption capacity in blood solution than 50:50, 25:75 and commercial sweat pad. This is due to the increase in the higher ratio of banana flower bract fibre, which has a higher OH group and245 hollow pores. Moreover, the high ionic concentration of blood solution reduces swelling by influencing the osmotic pressure within the matrix. As a result, when blood is used as the test solution, thus samples showed less absorption capacity than sweat solution. Therefore, the wet-laid sample with 75:25 sample exhibited its potential usage for absorbent core in sweat pad application.250 With reference to figure 7, Contact angle measurement is conducted on three wet laid webs and commercial sample using distilled water. Figure 7(a) shows the lowest contact angle of 8°, indicating a higher surface wettability characteristic of 75:25 sample compared to the other samples and absorbent core of commercial sweat pad. Figure 7 (b), shows contact angle of 9.6°, indicating a surface wettability 255 characteristic of 50:50 sample. Figure 7 (c), shows the contact angle values around 10.2°, showing a relatively lower surface wettability. The slight difference in contact angle values of test samples is due to variation in weight ratio of banana flower fibre and wood pulp fibre. The test results clearly showed that as the proportion of increases the angle value decreased respectively. Figure 7 (d) shows 260 the contact angle measurement of commercial sweat pad. The surface pores and hydrophilic groups would be the reason for higher wettability properties of wet laid samples than commercial sweat pad (121°).The present invention addresses the challenges posed by hyperhidrosis, offering a promising solution through the development of underarm sweat pads and also used 265 in many other applications. The utilization of the absorbent core layer, derived from Musa paradisiaca waste materials, particularly banana flower bracts, proves an innovative and eco-friendly approach. The multi-stage process, encompassing material collection, processing, and core design, has resulted in a highly efficient absorbent core, validated through comprehensive testing. The FTIR, XRD, SEM, 270 burning test, fibre density, moisture regain and moisture content assessments provided a detailed understanding of the physical and chemical properties of the banana flower bract fibre (banana flower fibre). Comparative tests with commercial sweat pads highlighted the potential advantages of the newly developed wet laid webs. The 75:25 wet-laid sample showed superior performance in artificial sweat and 275 blood absorbency and contact angle measurements, suggesting its suitability forunderarm sweat pad applications. Beyond addressing hyperhidrosis, the present invention contributes to the broader development of eco-friendly materials with diverse applications in healthcare and personal hygiene products.
Claims
1. A method of developing an absorbent core layer, comprising: removing banana bracts from the collected banana flowers (101); extracting fibres from the dried banana bracts using a combination of combing and manual peeling (102); drying the removed banana bracts at room temperature; cleaning the extracted fibres thoroughly; sorting and storing the cleaned fibres; cutting the fibres into short lengths; mixing the cut fibres with wood pulp in various ratios of 75:25, 50:50, 25:75 (103); dispersing the fibre-wood pulp mixture in water and stirring it to form a slurry (104); pouring the slurry into a wet-lay container (105); draining the water from the wet-lay container to form a nonwoven web; pressing the nonwoven web; drying the pressed nonwoven web at a suitable temperature of 60°c (106); the fundamental characteristics of banana flower fibre were analysed; developing wet laid webs for sweat pads; testing their absorbency with respect to bio-liquids such as sweat, blood (synthetic); and performing the liquid contact angle test.
2. The method of developing an absorbent core layer as claimed in claim 1, wherein the absorbent core layer from banana flower bracts, being an agricultural waste 3. An absorbent core layer used in sweat pads, characterized by, high absorbency, sustainability, biodegradability and enhanced performance, wherein the core layer is environmental friendly and alternative to synthetic fibres.