Indigenous diaphragm and non-noble bi-functional catalysts based alkaline wastewaters electrolyzer
Patent Information
- Application Number
- IN202441052211
- Authority / Receiving Office
- IN · IN
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2024-07-08
- Publication Date
- 2026-08-10
- Estimated Expiration
- 2044-07-08
AI Technical Summary
Current methods for green hydrogen production, such as steam methane reforming, contribute significantly to CO2 emissions, and the use of seawater in electrolysis is hindered by salt-related challenges, while traditional wastewater treatment is inefficient, necessitating a cost-effective and sustainable approach for hydrogen production from wastewater.
A zero-gap alkaline electrolyzer system using transition metal nanoparticles encapsulated in carbonaceous structures as bifunctional catalysts and a chitosan-based diaphragm membrane with hexagonal boron nitride, which prevents gas crossover and enhances ion transport and selectivity, facilitating efficient hydrogen and oxygen production from wastewater.
The system achieves high-purity gas production with improved efficiency and reduced freshwater consumption, addressing the challenges of salt in seawater and inefficiencies in traditional wastewater treatment, while being cost-effective and environmentally friendly.
Abstract
Description
FIELD OF INVENTIONThe present invention relates to advancements in the field of hydrogen production, fromwastewater, employing electrolyzers. Particularly the present invention relates toemploying electrolyzers. More particularly the present invention relates to zero gapalkaline electrolyzer system including an anode, cathode, a indigenous diaphragmmembrane and an electrolyte.BACKGROUND OF THE INVENTIONGlobal energy demand is expected to double by 2050 and triple by the end of the 21stcentury. Given the severe pollution caused by conventional fossil fuel usage, it is essentialto explore renewable energy sources. Despite the intermittent nature of sustainablenatural resources, storing energy in molecular bonds like hydrogen has advantages overelectrochemical storage methods such as Li-ion batteries, which suffer from self-discharge during storage. Hydrogen is considered a promising energy carrier for futuresocio-economic development. However, its current predominant production method,utilizing fossil fuels, contributes to approximately 830 million tons of CO2 emissionsannually. Steam methane reforming (SME) is the prevalent method for gray hydrogenproduction (48%), emitting at least 6.6 tons of CO2 per 1 ton of H2. To meet internationalcarbon neutrality goals, there is an urgent need to boost the market for green hydrogenproduction.To overcome the challenge of green hydrogen production, methods like water electrolysisare being considered as an attractive alternative to fossil-fuel-based techniques. However,a major obstacle to widespread adoption of green hydrogen production is the need forultrapure water, which puts pressure on freshwater resources. Efforts have been made toexplore alternative water sources, such as seawater electrolysis. But the presence of saltsin seawater poses challenges, leading to the generation of harmful chlorine gas andcorrosion of catalyst and support materials. Water-related issues in many countries are hindering the development of greenhydrogen infrastructure. To address this, utilizing treated wastewater has been identifiedas an effective strategy. Significant waste in agricultural, domestic, and industrial sectorsnecessitates efficient wastewater treatment methods. Traditional methods are oftenineffective, while the organic matter in wastewater, with a potential energy content of17.8 kJ g-1 COD, can be a valuable resource. Biological H2 production offers numerousbenefits in contrast to photoelectrochemical or thermochemical processes, given itsminimal energy demands and cost-effective nature. Among the array of wastewater bio-treatment technologies, the bioelectrochemical method stands out as an effectiveapproach for producing harmless wastewater and utilizing resources efficiently.Green hydrogen production from wastewater has significant potential for development.Industries such as distilleries and wastewater treatment plants can use water recycling tocreate green hydrogen and oxygen. Distilleries are looking to replace fossil fuels in boilerswith green hydrogen and sell any excess green hydrogen produced from these processeson the market. The involvement of the wastewater industry in this eco-friendlyproduction process is crucial for meeting decarbonization targets. Given the challengesposed by global warming and climate change due to high greenhouse gas emissions, it isessential to develop low-carbon, clean, and sustainable energy sources for achievingcarbon neutrality.Wastewater treatment processes also result in significant CO2-equivalent emissions.Additionally, an estimated 5.5 billion liters of pure water are required to produce 3million tons of H2, equivalent to the annual water consumption of 1.6 million people.Simultaneous degradation and hydrogen production during wastewater treatmentprovide an opportunity to reduce freshwater consumption and address water shortagesin hydrogen production through water splitting.Efforts are being made to explore more cost-effective and cleaner methods for hydrogenproduction, and water treatment is proving to be a promising source of green hydrogenthat is attracting increasing interest. Water electrolysis is a suitable, dependable, andscalable solution for converting renewable electricity into the chemical energy of greenhydrogen. The proton exchange membrane water electrolyzer (PEMWE), solid oxideelectrolysis cell (SOEC), alkaline water electrolyzer (AWE), and anion exchangemembrane water electrolyzer (AEMWE) are the main technologies for this purpose.SOEC is suitable for industrial settings with readily available high-temperature streams.The cost of PEMWE is significantly influenced by membrane material expenses, whileAEMWE faces maintenance costs due to membrane stability issues.Alkaline water electrolysis is a promising method for energy conversion. Developingtransition metal-based electrocatalyst materials with low overpotential and fast kineticsis crucial for improving efficiency and reducing costs. Industrial wastewater is a viablesolution for sustainable green hydrogen production, providing an environmentallyfriendly alternative to conventional methods. However, wastewater contains variousions, salts, impurities, and microbes, which can pose risks for the corrosion of electrolyzercomponents such as the anode, cathode, and diaphragm. Nevertheless, it also presentsan opportunity for innovative solutions in electrolyzer design and operation.To address these challenges, the inventors have developed a method for producinghydrogen and oxygen from wastewater. The system features a zero-gap alkalineelectrolyzer with non-noble catalysts (Ni-NCNT, NiFe-NCNT, and NiFe-ECNT)composed of transition metal nanoparticles encapsulated within carbonaceousstructures, specifically nitrogen-doped carbon nanotubes (NCNT) and etched carbonnanotubes (ECNT), which function as bifunctional catalysts. These catalysts are appliedto carbon cloth substrates, serving as both the anode and cathode components.Additionally, the invention incorporates a chitosan-based indigenous diaphragmmembrane as a separator. This membrane is fabricated using a straightforward castingtechnique, resulting in the production of high-purity gases at the anode and cathode,thereby enhancing the overall efficiency and efficacy of the hydrogen production process.SUMMARY OF THE INVENTIONThe present invention discloses an electrolyzer system for the production of hydrogenand oxygen from wastewater. More particularly the present invention relates to a zero-gap alkaline water electrolyzer that comprises an anode, cathode, an indigenousdiaphragm membrane and an electrolyte. The anode and the cathode are prepared byusing a catalyst comprising transition metal nanoparticles encapsulated in carbonaceousstructures. The indigenous diaphragm membrane is chitosan-based indigenousdiaphragm membrane that is dispersed with hexagonal boron nitride (HBN) and aged inCu2+ solution.Further the present invention relates to a method for preparing the chitosan-basedindigenous diaphragm membrane. The HBN coated chitosan-based indigenousdiaphragm membrane of the present invention configured as a separator between theanode and cathode prevents crossover and permeation of hydrogen and oxygen gases.The indigenous diaphragm membrane enhances ion transport and provides improvedselectivity for the evolved gases during electrolysis.BRIEF DESCRIPTION OF THE DRAWINGSIn order that the invention may be readily understood and put into practical effect,reference will now be made to exemplary embodiments as illustrated with reference tothe accompanying figures. The figures together with a detailed description below, areincorporated in and form part of the specification, and serve to further illustrate theembodiments and explain various principles and advantages, in accordance with thepresent invention where:Figure 1 illustrates zero-gap alkaline electrolyzer.Figure 2 illustrates components of zero-gap alkaline electrolyzer.Figure 3 illustrates the setup for hydrogen production from industrial wastewater.Figure 4 illustrates (a) X-Ray diffractogram of the catalysts; (b) X-Ray diffractogram ofchitosan-based diaphragm membranes.Figure 5 illustrates Raman spectra of the catalysts.Figure 6 illustrates (a and b) illustrates SEM image of Ni NCNT, (c) elemental mappingof Ni NCNTFigure 7 illustrates (a and b) SEM image of NiFe NCNT and (c) elemental mapping ofNiFe NCNTFigure 8 illustrates (a, b) SEM image of NiFe ECNT; and (c) Elemental mapping of NiFeECNTFigure 9 illustrates SEM image of Chitosan based diaphragm membranes.Figure 10 illustrates (a) OER polarization curve of the catalysts in 3 M KOH + Industrialwastewater; (b) HER polarization curve of the catalysts in 3 M KOH + Industrialwastewater; and (c) Tafel plot of the catalysts in OER; d. Tafel plot of the catalysts in HERFigure 11 illustrates long term stability test of the catalysts at 10 mA / cm2 in 3 M KOH +Industrial wastewater.Figure 12 illustrates electrochemical performance of the catalysts in 3 M KOH + IndustrialWastewater.Figure 13 illustrates electrochemical performance of Ni NCNT with different diaphragmmembranes.Figure 14 illustrates chlorine test to confirm absence of chlorine evolution.DETAILED DESCRIPTION OF THE INVENTIONAt the very outset of the detailed description, it may be understood that the ensuingdescription only illustrates a particular form of this invention. However, such a particularform is only an exemplary embodiment, and without intending to imply any limitationon the scope of this invention. Accordingly, the description is to be understood as anexemplary embodiment and teaching of invention and not intended to be takenrestrictively.Unless defined otherwise, technical, and scientific terms used herein have the samemeaning as commonly understood by one of the ordinary skills in the art to which thisinvention belongs. Further, unless otherwise required by context, singular terms shallinclude pluralities and plural terms shall include the singular.As used herein, the terms "comprise," "comprising," or any other variations thereof, areintended to cover a non-exclusive inclusion, such that a method that comprises a list ofacts does not include only those acts but may include other acts not expressly listed orinherent to such method. In other words, one or more acts in a method proceeded by"comprises… a" does not, without more constraints, preclude the existence of other actsor additional acts.As used herein, "zero-gap" implies that the distance between the anode and cathode isnear to zero. This minimizes the resistance of the overall cell significantly. The zero-gapconfiguration is achieved by sandwiching the cellulose-based material or a syntheticpolymer-based material between the bifunctional anode and cathode in a separatorelectrode assembly.As used herein, electrode means cathode and anode.As used herein, the term "fabricated" refers to the construction or assembly of a zero-gapalkaline electrolyzer, typically through a manufacturing process. To fabricate somethingin this context entails creating or assembling the essential components required for theoperation of the electrolyzer. This process encompasses various steps such as designing,engineering, and manufacturing electrodes, separator membranes, and other necessaryparts, and subsequently assembling them into a fully functional electrolyzer system.Therefore, a "fabricated zero-gap alkaline electrolyzer" denotes an electrolyzer that hasbeen constructed or manufactured specifically for operation with zero gap between theelectrodes. Such electrolyzers likely utilize advanced materials and manufacturingtechniques to achieve high efficiency and reliability.As used herein, the term "OER "refers to Oxygen evolution reaction .As used herein, the term "HER" refers to Hydrogen evolution reaction.As used herein, the term "SHE" refers to Standard hydrogen electrode.Where a range of values is provided, it is understood that each intervening value, to thetenth of the unit of the lower limit unless the context clearly dictates otherwise, betweenthe upper and lower limit of that range and any other stated or intervening value in thatstated range, is encompassed within the methods. The upper and lower limits of thesesmaller ranges may independently be included in the smaller ranges and are alsoencompassed within the methods, subject to any specifically excluded limit in the statedrange. Where the stated range includes one or both of the limits, ranges excluding eitheror both of those included limits are also included in the methods.Certain ranges are presented herein with numerical values being preceded by the term"about." The term "about" is used herein to provide literal support for the exact numberthat it precedes, as well as a number that is near to or approximately the number that theterm precedes. In determining whether a number is near to or approximately aspecifically recited number, the near or approximating unrecited number may be anumber which, in the context in which it is presented, provides the substantial equivalentof the specifically recited number.The articles "a" and "an" are used herein to refer to one or to more than one (i.e., to at leastone) of the grammatical object of the article. By way of example, "an element" means oneelement or more than one element.Any discussion of documents, methods, acts, materials, equipment, and the like that hasbeen included in this specification is solely for the purpose of providing a context for theinvention. It is not to be taken as an admission that any or all of these matters form a partof the prior art base or were common general knowledge in the field relevant to theinvention as it existed anywhere before the priority date of this application.The present invention relates to an electrolyzer system for the production of hydrogenand oxygen from wastewater, the electrolyzer system comprising an anode, a cathode,an indigenous diaphragm membrane and an electrolyte.In one of the embodiments the electrolyzer system is used in the field of hydrogenproduction, particularly from wastewater. The electrolyzer system enable the efficientgeneration of hydrogen and oxygen from treated wastewater, marking a significant leapforward in sustainable hydrogen production technologies.The present invention particularly relates to a zero-gap alkaline water electrolyzerassembly comprising of membrane electrode assembly, graphitic conducting blocks withserpentine flow fields for flow of electrolyte, stainless-steel plates for connecting powersupply.In yet another embodiment the membrane electrode assembly is prepared by configuringtogether the anode, cathode, and the indigenous diaphragm as separator membrane.In a wastewater electrolyzer, both the anode and cathode play integral roles in theelectrolysis process. The anode, serving as the positively charged electrode, initiatesoxidation reactions essential for breaking down organic pollutants and contaminantspresent in the wastewater. This oxidation process leads to the conversion of pollutantsinto simpler compounds or ions, while also facilitating the production of oxygen gas.Conversely, the cathode, functioning as the negatively charged electrode, facilitatesreduction reactions. Here, water molecules are reduced to produce hydrogen gas, aidingin the removal of excess hydrogen ions from the solution and maintaining electricalneutrality. Together, these complementary processes at the anode and cathode contributeto the effective treatment and purification of wastewater.In one of the embodiments the anode and the cathode are prepared by using a catalystcomprising transition metal nanoparticles encapsulated in carbonaceous structures.The catalyst comprising transition metal nanoparticles encapsulated in carbonaceousstructures, serves as bifunctional catalyst material for anode and cathode.The carbonaceous structures include nitrogen-doped carbon nanotubes (NCNT) andetched carbon nanotubes (ECNT).In one of the embodiments the catalysts are selected from Ni- NCNT (Nickel Nitrogen-Doped Carbon Nanotubes) and Ni Fe -NCNT (Nickel-Iron Nitrogen-Doped CarbonNanotubes).In one of the embodiments the anode and cathode are coated with the catalyst on a carbonsubstrate.In one of the preferable embodiments the carbon substrate is a carbon cloth.In yet another embodiment the carbon substrate is selected from carbon paper, graphitefelt, carbon cloth, carbon mesh, microporous carbon coated carbon cloth orpolytetrafluoroethylene coated carbon cloth.The anode and cathode are coated with the catalyst on a carbon cloth substrate to enhancenon-corrosive properties in wastewater.The anode and / or cathode are prepared using catalysts coated on non-corrosive carboncloth of desired dimensions.The active area of both the anode and cathode measures 6.25cm2 / L.In yet another embodiment the active area of both the anode and cathode measures 1 to100 square centimeters per liter (cm² / L).In yet another embodiment when active area increases, consequently the production ofH2 also increases.The anode and / or cathode is formed by coating the bifunctional catalyst material on acarbon substrate. Any coating technique, as known to or appreciated by any personskilled in art may be used. Thus, by way of example, the coating is brush coating andspray coating.The amount of the catalyst material to be applied on carbon substrate to prepare a cathodeand anode is 1mg / cm2 .In one of the embodiments the indigenous diaphragm membrane is a chitosan-baseddiaphragm membrane that is dispersed with hexagonal boron nitride (HBN) and aged inCu2+ solution.The aging of HBN-coated chitosan indigenous diaphragm membranes in Cu+2 solutionenhances the metal ion separation properties. It improves selectivity by potentiallymodifying the membrane's surface chemistry, enabling more effective binding of copperions while allowing other ions to pass through. It enhances the interaction between thechitosan material and copper ions, thereby increasing resistance to degradation fromexposure to water or chemicals. Moreover, it boosts adsorption capacity by providingmore time for copper ions to interact with the membrane material, potentially leading tohigher efficiency in copper ion removal. Additionally, aging in Cu+2 solution may altersurface properties like charge and hydrophilicity / hydrophobicity, influencingmembrane performance in metal ion separation processes. This alteration reducesfouling, creating a more resistant surface or enhancing the membrane's ability to repelunwanted substances. The aging in Cu+2 solution offers a cost-effective approach forenhancing membrane performance compared to developing entirely new materials ortechnologies.In yet another embodiment the HBN-coated chitosan indigenous diaphragm membraneis configured as a separator between the anode and cathode to prevent crossover andpermeation of hydrogen and oxygen gases.In an embodiment electrolyzer system comprises of an electrolyte. Electrolytes serve vitalroles in wastewater electrolyzers, primarily by enhancing the electrical conductivitywithin the solution. When treating wastewater, which often contains various impuritiesand ions, electrolytes like sodium chloride or sulfuric acid are added to augment ionconcentration and, consequently, conductivity. This elevated conductivity enhances thetransmission of electrical current, facilitating more efficient electrolysis. Additionally,electrolytes aid in ion exchange during electrolysis, promoting the breakdown of watermolecules into hydrogen and oxygen gases. They also play a crucial role in protectingelectrodes from corrosion or degradation, potentially forming a protective layer.Furthermore, electrolytes can help regulate the pH of the electrolyte solution, ensuringoptimal conditions for electrolysis.In yet another embodiment the electrolyte used is an alkaline solution comprisespotassium hydroxide (KOH) and / or sodium hydroxide (NaOH).In a preferable embodiment the electrolyte comprises of treated wastewater by addingKOH, preferably by adding 3 M KOH.In yet another embodiment sodium hydroxide (NaOH) serves as an alternativeelectrolyte and is almost interchangeable with potassium hydroxide (KOH). These twocompounds, NaOH and KOH, are the most chemically similar among hydroxides. Inalkaline water electrolysis, KOH is typically preferred over NaOH to avoid corrosionissues from acidic electrolytes. This preference stems from the higher conductivity ofKOH compared to NaOH. KOH solutions are about 5% more conductive than NaOHsolutions at equivalent molar concentrations. For instance, KOH exhibits a maximumspecific conductivity of 950 mS cm-1 at 50°C with a 30 wt.% solution, whereas NaOHreaches 650 mS cm-1 under similar conditions with a 20 wt.% solution.KOH is recognized as a stronger base compared to NaOH, attributed partly to the weakerK-O bond due to the larger size of potassium (K) compared to sodium (Na), resulting ina more facile release of hydroxide ions (OH-). This characteristic is supported by theionization energy values, with sodium requiring more energy (495.8 kJ / mol) to ionizecompared to potassium (418.8 kJ / mol). Consequently, potassium is more electro-positive / reactive than sodium, enhancing the propensity of KOH to lose OH- ions andthus exhibiting stronger basic properties than NaOH.In one of the embodiments the chitosan-based indigenous diaphragm membrane isfabricated by dissolving chitosan powder in acetic acid, adding HBN, casting the solutionon a petri dish, and aging in Cu2+ solutionThe method of preparing HBN-dispersed Chitosan-based indigenous diaphragmmembranes involve several sequential steps:i. dissolving chitosan powder in acetic acid at room temperature. Thechitosan is stirred overnight to achieve a homogeneous and transparentsolution.ii. adding 1 wt.% HBN to the chitosan solution obtained in step (i). Themixture is then cast onto a petri dish and left to air dry, resulting in theformation of a chitosan membrane with dispersed HBN.iii. subjecting the indigenous diaphragm membrane obtained from step (ii)to further aging in a Cu2+ saturated sodium hydroxide (NaOH) solution(Na2Cu (OH)4) (sodium tetrahydroxycuprate (II) ) for a duration of 4days. After aging, the membrane is washed with deionized water toremove any excess sodium hydroxide (NaOH), and then dried at roomtemperature.The HBN-dispersed Chitosan-based indigenous diaphragm membrane is obtainedthrough the previously described process. The aging process in a Cu2+ solution serves toenhance the metal ion separation properties of the separator membrane.In yet another embodiment, the present invention provides a method for preparing non-noble catalysts (Ni-NCNT, NiFe-NCNT, and NiFe-ECNT), which involves the followingsteps:For Ni-NCNT:i. Melamine is dissolved in ethanol, and NiCl3 is added to the solution. The mixture isstirred continuously overnight at 400 rpm to achieve homogeneity.ii. The mixture from step (i) is heated to 800°C to evaporate the solvent, leaving behind aresidue.iii. The collected residue is then heated in a tube furnace under a nitrogen atmosphere ata flow rate of 20 ml / min. The temperature is ramped up to 700°C at a rate of 5°C / minand maintained for two hours.iv. The product obtained from step (iii) is cooled to yield the final product, Ni-NCNT.Similarly, for NiFe-NCNT:The same procedure as described above is followed, with the addition of Ni(NO3)2 andFe(NO3)2 as precursors in step (i).For NiFe-ECNT:i. Fe(NO3)2 and CNT are mixed using a mortar and pestle, then heated in a box furnaceunder an air atmosphere at 400°C with a ramp rate of 5°C / min for two hours.ii. The product from step (i) is refluxed in concentrated HNO3 at 120°C for 24 hours.iii. The residue from step (ii) is washed several times with deionized water and dried at60°C to obtain ECNT.iv. NiCl3, Fe(NO3)2, and ECNT are mixed using a mortar and pestle, loaded into analumina boat, and heated in a tube furnace under a nitrogen environment at 700°C witha ramp rate of 5°C / min for two hours.v. The mixture from step (iv) is cooled to ambient temperature to yield NiFe-ECNT.In yet another embodiment the method of production of the electrolyzer system forhydrogen production comprises the following steps:i. synthesizing, the catalysts by dissolving melamine in ethanol, adding nickel andiron nitrates, stirring, evaporating the solvent, and heating in a nitrogenenvironment;ii. coating, the anode and the cathode with the synthesized catalyst on a carbon clothsubstrate;iii. fabricating, a chitosan-based indigenous diaphragm membrane by dissolvingchitosan powder in acetic acid, adding hBN, casting the solution on a petri dish,drying, and aging in Cu2+ solution; andiv. assembling the electrolyzer system with the prepared anode, cathode, andindigenous diaphragm membrane.In yet another embodiment the wastewater, can be selected from industries, agriculture,hospitals, sewage, and seawater.The electrolyzer system operates at a voltage of 2.55 V, achieving a current density of 669mA / cm² with the HBN-coated chitosan indigenous diaphragm and 785 mA / cm² withthe chitosan indigenous diaphragm membrane without HBN coating.In yet another embodiment increasing the voltage directly increases the current densitysince voltage and current density are directly proportional to each other.Certain specific aspects and embodiments of the present application will be explained ingreater detail with reference to the following examples, which are provided only forpurposes of illustration and should not be construed as limiting the scope of theapplication in any manner. While particular aspects of the present invention have beenillustrated and described, it would be obvious to those skilled in the art that various otherchanges and modifications can be made without departing from the spirit and scope ofthe invention. It is therefore intended to cover in the appended claims all such changesand modifications that are within the scope of this invention.EXAMPLESThe following examples are for the purpose of illustration of the invention and are notintended in any way to limit the scope of the invention.Experimental Details:Synthesis of non-noble catalyst:Example 1:Synthesis of Ni Fe -NCNT and Ni -NCNTNickel (II) nitrate (Ni(NO3)2) and iron(II) nitrate (Fe(NO3)2) were utilized as precursors,while melamine served as a carbon and nitrogen source. Initially, melamine wasdissolved in 10 ml of ethanol. Subsequently, a predetermined amount of Ni(NO3)2 (1g)and Fe(NO3)2 (1g) were gently added to this solution under continuous stirring. Theresulting mixture was stirred overnight at 400 rpm to achieve homogeneity. Followingthis, the mixture was heated to 80°C to facilitate solvent evaporation. The residueobtained after evaporation was collected and subjected to further treatment in a tubefurnace under a nitrogen environment (N2 flow rate of 20 ml / min) at 700°C, with a ramprate of 5°C / min, for two hours. After completion of the heating process, the material wasallowed to cool to ambient temperature and subsequently ground to produce the finalproduct, denoted as Ni Fe-NCNT. A similar procedure was employed to synthesize Ni-NCNT, omitting the use of Fe(NO3)2.Example 2:Synthesis of Nickel Iron - Electrospun Carbon Nanotubes (Ni Fe-ECNT):The synthesis process begins with the preparation of ECNT. Initially, 0.5 grams ofFe(NO3)2 were mixed with 0.4 grams of carbon nanotubes (CNT) using a mortar andpestle. The resulting mixture was then heated in a box furnace in an air atmosphere at400°C, with a ramp rate of 5°C / min, for two hours. Subsequently, the collected sampleunderwent acid treatment using concentrated HNO3 at 120°C for 24 hours employing areflux method. The residue obtained after acid treatment was washed multiple times withdeionized (DI) water and dried at 60°C. The resulting product was termed ECNT.The second step involved the preparation of Ni Fe-ECNT. A mixture comprising NiCl3,Fe(NO3)2, and ECNT was thoroughly mixed using a mortar and pestle. This mixture wasthen loaded into an alumina boat and heated in a tube furnace under a nitrogenenvironment (N2 flow rate of 20 ml / min) at 700°C, with a ramp rate of 5°C / min, for twohours. After completion of the heating process, the material was allowed to cool toambient temperature before being ground into a finished product.Synthesis of HBN dispersed Chitosan-based diaphragm membranesExample 3:To synthesize the chitosan-based diaphragm membranes, initially, 1 gram of chitosanpowder was dissolved in 200 milliliters of 4 wt.% acetic acid solution at roomtemperature. The solution was stirred overnight to achieve a homogeneous andtransparent chitosan solution. Subsequently, 1 wt.% hexagonal boron nitride (HBN) wasadded to the solution. The resulting mixture was then cast onto a petri dish and allowedto dry in the air, resulting in the formation of a chitosan membrane.To further enhance the properties of the diaphragm membrane, it underwent an agingprocess in a 2 wt.% Cu2+ saturated NaOH solution (Na2Cu(OH)4) for a duration of 4days. Following the aging process, the membrane was washed with deionized water toremove excess NaOH and then dried at room temperature.Preparation of working electrodeExample 4:To fabricate the working electrode, a catalyst ink was prepared by dispersing 10milligrams (mg) of catalyst in a hybrid solvent consisting of 90 microliters (μL) ofdeionized water, 50 microliters (μL) of ethyl alcohol, and 10 microliters (μL) of 5 wt.%Nafion solution. The mixture underwent ultrasonication treatment for 20 minutes toensure proper dispersion. Subsequently, the ink was coated onto a carbon cloth substratemeasuring 1 centimeter (cm) by 1 centimeter (cm). The coated substrate was then driedat 60°C until fully dry.Example 5:Preparation of anode and cathodeTo fabricate the anode and cathode, catalyst ink was prepared by dispersing 15milligrams of catalyst in a hybrid solvent consisting of 3 millilitres (mL) of ethyl alcoholand 90 microliters of 5 wt.% Nafion solution. The resulting mixture underwentultrasonication treatment for 20 minutes to ensure proper dispersion. Subsequently, theink was coated onto carbon cloth substrates measuring 2.5 centimetres by 2.5 centimetres.The coated substrates were then dried at 60°C until fully dry.Electrochemical Testing:Example 6:The electrochemical performance of Ni NCNT for industrial wastewater splitting wasevaluated using a Biologic SP-300 potentiostat. The working electrode underwentpreparation and testing in a three-electrode setup employing Ag / AgCl and platinumwire as reference and counter electrodes, respectively. The electrolyte consisted of 3 MKOH in industrial wastewater. Prior to measuring polarization curves, the electrodeswere subjected to 15 cycles of cyclic voltammetry (CV) to attain stable polarization.The OER and HER polarization curves were determined through linear sweepvoltammetry (LSV) with a scan rate of 5 mV / s, with 100% iR correction applied viasoftware in potentistatic electrochemical impedance mode.To assess the catalyst's durability, two-electrode measurements were conducted viachronopotentiometry at a current density of 10 mA / cm². These measurements occurredin an electrolyte composed of 3 M KOH mixed with industrial wastewater at roomtemperature, following CV activation.Assembly of zero-gap alkaline electrolyzerFirstly, a membrane electrode assembly was fabricated by pressing together the anode,cathode, and the prepared indigenous diaphragm serving as the separator membrane(refer to Fig. 1). Following this, a zero-gap alkaline electrolyzer was assembled. Thisassembly included the fabricated membrane electrode assembly, graphitic conductingblocks featuring serpentine flow fields for electrolyte flow, and stainless-steel plates forconnecting to the power supply.A schematic illustration of the setup for hydrogen production from industrial wastewateris shown in figure 1 and schematic illustration of the components of zero-gap alkalineelectrolyzer is shown in figure 2.The catalysts performance underwent testing within the setup illustrated in Figure 2,which included an assembled zero-gap alkaline electrolyzer, a peristaltic pump(MICLINS INDIA), and a DC power supply unit (Aplab). The electrolyte, consisting of 3M KOH and industrial wastewater, was circulated through the zero-gap alkalineelectrolyzer using the peristaltic pump. The DC power supply was responsible forproviding the necessary potential across the electrolyzer terminals.Material Characterization:The phase composition of the synthesized samples was analyzed using X-Ray diffraction(Rigaku Supermini flex) with a Cu Kα radiation source (λ = 1.5406 Å). Raman spectra andmorphology were acquired utilizing a Raman spectrometer (Horiba XPLORA-MV2000),while scanning electron microscopy (Apreo S) was employed for further characterizationof the samples' morphology.Analysis:The X-Ray Diffractograms of the three catalysts are presented in Fig. 3a. All catalystsexhibit peaks at 25.93° attributable to carbon (ICDD Reference No. 98-001-7125).Moreover, Ni NCNT displays peaks at 44.41°, 51.77°, and 76.21° corresponding to (111),(002), and (022) planes of Ni (ICDD Reference No. 98-012-3812). In addition, thediffractogram of NiFe NCNT reveals peaks at 35.9°, 43.94°, and 51.24° associated withFeNi3 (ICDD Reference No. 98-007-3210). The diffractogram of NiFe ECNT indicatespeaks at 36.91° and 62.75°, indicating the presence of iron (ICDD Reference No. 98-007-1820), and at 43.44°, attributed to FeNi (ICDD Reference No. 98-006-0276). Furthermore,the X-Ray diffractogram of the Chitosan diaphragm membrane exhibits peakscorresponding to chitosan, HBN, and NaOH, which may be attributed to aging in NaOHsolution (Fig. 3b).The Raman spectra (Fig. 4) of the catalysts reveal characteristic vibrations of the D and Gbands at approximately 1350 cm^-1 and 1580 cm^-1, respectively. These bandscorrespond to the defects and amorphousness of carbon atoms, and the tangentialoscillations and vibrations of sp^2-hybridized carbon atoms, as documented [2,3].Typically, the intensity ratio of the D and G bands (ID / IG) is considered a crucialparameter for evaluating the degree of structural disorder in carbon materials. A higherID / IG ratio signifies a greater degree of defects in the carbon materials [4].Specifically, Ni NCNT exhibits an ID / IG ratio of 0.9, NiFe NCNT shows a ratio of 1.04,and NiFe ECNT displays a ratio of 0.81.Figures 5a and 5b present the SEM images of Ni NCNT, illustrating an encapsulatedstructure where Ni particles are confined within N-doped carbon nanotubes, along withsmall-sized Ni particles adorning the N-doped carbon nanotubes. Elemental mapping ofthe catalyst reveals a uniform distribution of Ni on the N-doped carbon nanotubes (Fig.5c). Transitioning to NiFe NCNT, SEM images (Fig. 6a and 6b) exhibit Ni and Fe particlesdecorating N-doped carbon nanotubes, with elemental mapping indicating ahomogeneous distribution of both metals (Fig. 6c). NiFe ECNT displays a ruggedmorphology with evenly dispersed Ni and Fe nanoparticles, alongside carbon nanotubeson the surface (Fig. 7). Finally, the SEM image of the chitosan diaphragm membrane agedin Cu2+ saturated solution and coated with Cu2+ displays a morphological alteration,resulting in a rough surface post-HBN coating on the chitosan aged in Cu2+ solution (Fig.8).Electrochemical data:The electrochemical performance of the synthesized catalysts for industrial wastewatersplitting was meticulously evaluated, focusing on their activity in both the oxygenevolution reaction (OER) and hydrogen evolution reaction (HER) within a solutioncomposed of 3 M KOH + Industrial wastewater. Figures 9a and 9b illustrate thepolarization curves of OER and HER, respectively. The Ni NCNT catalyst exhibited anoverpotential (η10) of 410.13 mV to achieve a current density of 10 mA / cm², showcasingsuperior performance compared to NiFe NCNT with an η10 of 519.19 mV and NiFeECNT displaying the lowest η10 of 382.41 mV among the three catalysts in OER (Fig. 9a).Conversely, in HER (Fig. 9b), Ni NCNT demonstrated a significantly lower overpotential(η10) of 86.15 mV at 10 mA / cm², while NiFe NCNT and NiFe ECNT displayedoverpotentials of 149.49 mV and 135.32 mV, respectively.The, Tafel slope analysis was employed to assess the kinetic performance of the catalysts,with smaller Tafel slopes indicating better catalytic kinetics and higher catalytic activity.The Tafel slope, calculated from the Tafel equation: η=a+blog(j) ,(where b denotes Tafel slope, j denotes current density, and η denotes overpotential)In OER (Fig. 9c), NiFe ECNT exhibited the lowest Tafel slope of 92.47 mV / dec among thecatalysts, while Ni NCNT and NiFe NCNT displayed Tafel slopes of 120.78 mV / dec and115.09 mV / dec, respectively. Conversely, in HER (Fig. 9d), NiFe NCNT demonstratedsuperior kinetics with a smaller Tafel slope of 156.59 mV / dec, whereas Ni NCNT andNiFe ECNT exhibited Tafel slopes of 251.56 mV / dec and 215.93 mV / dec, respectively.The overall industrial wastewater splitting performance of the catalysts was investigatedutilizing a two-electrode configuration employing bifunctional catalysts in 3 M KOH +Industrial wastewater. The same catalyst served as both the anode and cathode.Chronopotentiometry studies were conducted at a current density of 10 mA / cm² for 30hours. Figure 10 illustrates the, NiFe ECNT achieved the lowest cell potential of 1.81 V at10 mA / cm², whereas Ni NCNT and NiFe NCNT exhibited cell potentials of 2.45 V and1.93 V, respectively. Importantly, all catalysts demonstrated excellent stability in theelectrolyte.Further enhancing the study, a zero-gap cell was constructed based on the optimizedelectrochemical performance of the catalysts in both three-electrode and two-electrodeconfigurations. Utilizing 3 M KOH + Industrial wastewater electrolyte, the cell circulatedthe electrolyte via a peristaltic pump while a DC power supply provided the necessarypotential across the terminals. Figure 11 demonstrated the performance of the catalystswith a butter sheet diaphragm membrane.At a cell voltage of 2V, NiFe ECNT achieved the highest current density of 318.08mA / cm², while Ni NCNT and NiFe NCNT exhibited current densities of 164.32 mA / cm²and 100.8 mA / cm², respectively. Additionally, the performance of the prepareddiaphragm membranes was evaluated using Ni NCNT as a bifunctional catalyst (Figure12). Interestingly, at a voltage of 2.55 V, Ni NCNT demonstrated a current density of 785mA / cm² with a chitosan (aged in Cu2+) diaphragm membrane, whereas with an HBN-coated chitosan (aged in Cu2+) diaphragm membrane, a current density of 669 mA / cm²was achieved.While a slightly lower current density was obtained with the diaphragm membranecoated with HBN, the HBN coating effectively prevented the crossover of oxygen andhydrogen gas, resulting in high-purity gas at both the anode and cathode. A chlorine testconducted post the electrochemical test for Ni NCNT indicated no evolution of chlorine(Figure 13).Thus, it is evident that the specially designed diaphragm enhances ion transport andprovides improved selectivity for the evolved gases in electrolysis process. A zero-gapalkaline electrolyzer is constructed using the developed anode, cathode, and HBN-coatedchitosan-based diaphragm membranes as separators. The catalyst Ni NCNTdemonstrates a current density of 669 mA / cm2 at 2.55 V when paired with the HBN-coated chitosan diaphragm membrane treated with Cu2+. Additionally, a higher currentdensity of 785 mA / cm2 is achieved with the chitosan diaphragm membrane withoutHBN coating. The absence of hypochlorite and chlorine indicates the possibility ofgenerating green hydrogen from industrial wastewater without encountering theconstraints observed in alternative media, such as seawater.Therefore, the non-noble catalysts and separator membranes developed in this inventionwork together to enhance electrochemical performance, providing a sustainableapproach to hydrogen production from industrial wastewater. Additionally, thesecatalysts and diaphragm membranes have the potential to be applied to the productionof hydrogen and oxygen from various sources of industrial wastewater across differentindustries.While preferred aspects have been shown and described, it is to be understood thatvarious further modifications and additional configurations will be apparent to thoseskilled in the art. It is intended that the specific embodiments and configurationsdisclosed herein are illustrative of the preferred nature of the invention and should notbe interpreted as limitations on the scope of the invention.
Claims
1. An electrolyzer system for the production of hydrogen and oxygen from wastewater, the electrolyzer system comprising: an anode, a cathode, an indigenous diaphragm membrane and an electrolyte, wherein the anode and the cathode are prepared by using a catalyst comprising transition metal nanoparticles encapsulated in carbonaceous structures, wherein the indigenous diaphragm membrane is chitosan-based indigenous diaphragm membrane that is dispersed with hexagonal boron nitride (HBN) and aged in Cu2+ solution.
2. The electrolyzer system as claimed in claim 1, wherein the catalysts are selected from Ni- NCNT (Nickel Nitrogen-Doped Carbon Nanotubes) and Ni Fe -NCNT (Nickel-Iron Nitrogen-Doped Carbon Nanotubes).
3. The electrolyzer system as claimed in claim 1, wherein the anode and cathode are coated with the catalyst on a carbon cloth substrate.
4. The electrolyzer system as claimed in claim 1, wherein the HBN-coated chitosan indigenous diaphragm membrane is configured as a separator between the anode and cathode.
5. The electrolyzer system as claimed in claim 1, wherein the electrolyte used is an alkaline solution comprises potassium hydroxide (KOH), and / or sodium hydroxide (NaOH) .
6. The electrolyzer system as claimed in claim 1, wherein the chitosan-based indigenous diaphragm membrane is fabricated by dissolving chitosan powder in acetic acid, adding HBN, casting the solution on a petri dish, and aging in Cu2+ solution.
7. A method of production of the electrolyzer system for hydrogen production as defined in claim 1, the method comprising: synthesizing, the catalysts by dissolving melamine in ethanol, adding nickel and iron nitrates, stirring, evaporating the solvent, and heating in a nitrogen environment; coating, the anode and the cathode with the synthesized catalyst on a carbon cloth substrate; fabricating, a chitosan-based indigenous diaphragm membrane by dissolving chitosan powder in acetic acid, adding HBN, casting the solution on a petri dish, drying, and aging in Cu2+ solution; and assembling the electrolyzer system with the prepared anode, cathode, and indigenous diaphragm membrane.
8. The electrolyzer system, as claimed in claim 1, utilized for the production of hydrogen from wastewater, wherein the wastewater can be selected from industries, agriculture, hospitals, sewage, and seawater.