Amorphous alloy strip and preparation method therefor

IN604684BActive Publication Date: 2026-09-30AT&M AMORPHOUS TECH CO LTD +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
IN202327028877
Authority / Receiving Office
IN · IN
Patent Type
Patents
Current Assignee / Owner
Priority Date
2021-04-25
Filing Date
2023-04-20
Publication Date
2026-09-30

AI Technical Summary

Technical Problem

Current methods struggle to produce wide and thick iron-based amorphous alloy strips stably due to insufficient cooling capacity, leading to embrittlement and crystallization, as the critical cooling rate requirements are not met, especially for strips with a thickness of 30μm and above and a width of 80mm.

Method used

The solution involves optimizing the cooling roller sleeve's thermal conductivity and maximum usable thickness, balancing these parameters with the strip's thickness to achieve the necessary cooling rate, using a range of thermal conductivity (80-350 W/m·K) and maximum thickness (4-20 mm) to ensure stable production of strips with a width of ≥80mm and thickness of ≥30μm, incorporating specific alloy compositions like Fe with additives for enhanced properties.

Benefits of technology

This approach allows for the stable manufacturing of wide and thick iron-based amorphous strips with improved toughness, magnetic properties, and reduced production costs, ensuring sufficient cooling capacity and structural integrity.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

The present invention provides an amorphous alloy strip and a preparation method therefor. The width of the amorphous alloy strip is =80 mm, the thickness thereof is =30 µm, and the toughness value thereof is <4.0. The amorphous alloy strip is obtained by cooling an alloy liquid by means of a cooling roller. The cooling roller comprises a roller sleeve. The thermal conductivity of the roller sleeve, the maximum usable thickness of the roller sleeve, and the thickness of the amorphous alloy strip have the following relationship: a requirement on the cooling capacity of the cooling roller during preparation of a strip is achieved by means of optimized fitting among the thickness of the strip, the thermal conductivity of the roller sleeve, and the maximum usable thickness of the roller sleeve, to thereby prepare a strip having a width of =80 mm and a thickness of =30 µm.
Need to check novelty before this filing date? Find Prior Art

Description

Technical FieldThe present invention belongs to the technical field of alloy preparation, andparticularly relates to an amorphous alloy strip and a preparation method therefor.BackgroundAmorphous alloy is a category of soft magnetic material developed in recentyears. Compared with conventional soft magnetic materials such as,electrotechnical steel and ferrite, amorphous alloy has higher magneticconductivity and lower AC power loss. Therefore, amorphous alloy has beenwidely applied to the iron core of magnetic components and devices such as,transformers, inductors, transducers and motor stators.Amorphous alloy strip is generally manufactured by the technology of planeflow; and the method is as follows: a certain proportion of raw materials aremolten into molten alloy with a smelting furnace, and then the molten alloy ispoured into a nozzle ladle provided with a slit nozzle at the bottom; the moltenalloy in the nozzle ladle flows out of the nozzle and is spread out on the outercircumferential surface of the copper-alloy cooling roller with high-speed rotationbelow the nozzle to form a molten pond having a certain size between the surfaceof the cooling roller and the bottom surface of the nozzle; the molten alloy isquickly drawn out and cooled rapidly, and meanwhile, the molten alloy in thenozzle slit is continuously supplemented to the molten pond, thus formingcontinuous thin strip with an amorphous structure. The thin strip is closelyadhered to the outer surface of the cooling roller and rotates with the coolingroller at a high speed, and is peeled off by a high pressure gas or a mechanicaldevice in a proper position of the outer circumferential surface of the coolingroller, and finally wound into coils by a coiling device.During the manufacturing process of amorphous strips, the rapidsolidification of molten alloy is the essential condition for the strip formed bycooling to have an amorphous structure. For common amorphous alloy strips inthe prior art, the cooling rate of the molten alloy should be up to 105°C / sec abovewhen a solid amorphous strip is formed nearby the glass transition temperature Tg,and the temperature (stripping temperature) of the amorphous strip should belower than about 200°C when peeling off from the surface of the cooling roller.Moreover, different amorphous materials have different requirements on thecooling rate. If the actual cooling rate of the molten alloy or strip is below therequirement, the strip suffers structural relaxation and even crystallization due toinsufficient cooling, thus resulting in serious embrittlement of the strip andseriously worsened properties.During the manufacturing process of the amorphous strip, the rapidsolidification of the molten alloy and the cooling process of the strip arecompleted on the outer surface of the cooling roller. The cooling roller isgenerally assembled by two components of a ring-shaped cooling roller sleeveand a cylindrical roll core; an annular channel is formed between the roller sleeveand the roll core, and cooling water which flows at a high speed is put to thechannel. During the manufacturing process of the amorphous strip, the heatcontained in the molten alloy must flow through the molten pond, the interfacebetween the molten alloy and the outer surface of the roller sleeve, the rollersleeve having a certain thickness, and the interface between the inner surface ofthe roller sleeve and the cooling water successively, and finally passes to theflowing cooling water. The heat-conducting property of the cooling roller sleevedetermines the cooling capacity of the cooling system to a great extent, which thusplays a decisive role to the formation of an amorphous strip. To achieve the rapidsolidification of the molten alloy, copper alloy with high heat-conducting propertygenerally serves as the material of a cooling roller sleeve in the prior art, forexample, chromium-zirconium copper, beryllium bronze, Ni-Si bronze and thelike.In the amorphous alloy strips, the iron-based amorphous strip has beenapplied most extensively; the iron-based amorphous strip has the majoradvantages of low costs, high saturation magnetic induction, and capable of beingapplied to the iron core of various transformer components and devices.Generally, the iron-based amorphous strip having a thickness of about 25 μm anda width of 100-300 mm can be manufactured in the prior art.With the technical progress and intensive market competition of thetransformer industry, there is an urgent need for the wide and thick iron-basedamorphous strip (thickness: 30μm above and width: 80 mm above). For example,during the manufacturing process of a transformer core, the use of thick strip willreduce the workload of iron core machining and improve the productionefficiency, and can further reduce fragments caused by the broken strip, which isbeneficial to improving the reliability of the components and devices.However, it is always a difficult to produce a wide and thick iron-basedamorphous strip stably. Nickel-based or cobalt-based amorphous alloy has a lowercritical cooling rate and thus, is processed into a thick strip more easily, forexample, nickel-based amorphous alloy soldering foils having a thickness of 50μm above can be produced in the prior art. However, the critical cooling rate ofthe iron-based amorphous alloy is higher than that of the nickel-based amorphousalloy, when the wide iron-based amorphous alloy strip having a thickness of30μm above is manufactured, the heat contained in the thick strip increasesobviously compared with the common thin strip and the thermal load borne by thecooling roller sleeve increases obviously therewith; moreover, the coolingcapacity of the cooling roller sleeve used in the prior art has been not enough toensure that the cooling rate of the molten alloy and strip is higher than the criticalcooling rate, which will cause the obvious embrittlement of the manufactured stripand even occurrence of obvious crystallization. Therefore, it is difficult tomanufacture a wide and thick iron-based amorphous alloy stably. There is norelevant solution proposed in the prior art.For example, methods for manufacturing a thick amorphous alloy strip with aplurality of nozzles are respectively disclosed in Chinese patents CN107442750Band CN204486736U as well as in Japanese patent JP3280778B2, namely, themolten alloy flows out of multiple adjacent (front and back) nozzles at the sametime, and the molten alloy flowing out of each nozzle or solidified strip is boundto form a thick strip. The technical key point to manufacturing a thick amorphousalloy strip is not how to form the thick strip, but how to ensure enough coolingcapacity of the equipment and the formation of an amorphous structure from thematerial during the manufacturing process.US patent US4537239 discloses a cooling roller for manufacturing anamorphous strip; the material is beryllium-copper alloy; diameter is about 380mm and the thickness of the roller sleeve is about 6.35 mm. Such a roller sleevehas too small diameter, and the fitting time between the strip and the roller surfaceis very short; therefore, the thickness of the roller sleeve must be kept very thin toensure the cooling capacity. Thereby, the wide amorphous alloy strip having athickness of greater than 26 μm cannot be manufactured stably.Chinese patent application CN110976794A discloses a method formanufacturing an iron-based amorphous alloy strip; the iron-based amorphousalloy strip having a thickness capable of reaching 40 μm can be achieved byimproving the cooling capacity of the cooling system; and it is prompted that thecooling capacity of the roller sleeve may be improved by a process of thinning theroller sleeve to 20 mm from 30 mm above in thickness. However, the coolingcapacity of the roller sleeve is not only related to the thickness thereof, but alsodepends on the thermal conductivity thereof. Moreover, the present invention doesnot relate to the thermal conductivity of the roller sleeve used; therefore, it is lackof practical guiding significance for the selection of the parameters of the coolingroller sleeve.Non-patent literature (Guo Qian, Yan Mi. Thermal Analysis for CoolingRolls in Planar-flow Melt Spinning, Rare Metal Materials and Engineering, 2015,No.8 of Vol.44, 2048-2052) performs simulated calculation on the temperaturefield of cooling rolls during the manufacturing process of the amorphous alloystrip; a copper alloy with a thermal conductivity of 180 W / m·K serves as thematerial of the cooling rolls to obtain the optimal size of the cooling rolls duringthe manufacturing process of the iron-based amorphous alloy strip having athickness of 30μm and a width of 220 mm, namely, the roller sleeve has athickness of 10 mm and a diameter of 1200 mm. However, there is no option onthe cooling roller sleeve of the amorphous alloy strip having a thickness of 30μmabove proposed in the literature.To sum up, the prior art provides some technical solutions on themanufacture of thick amorphous alloy strips from the aspects of amorphousmaterial components and forming process of the thick strip, but does not provideany supporting measure for the core problems of thick strip manufacturing,namely, cooling rate of the molten alloy and strip. Even though some attempts onthe improvement of the cooling capacity are implemented in some prior arts, thereis no method for manufacturing a thick amorphous alloy strip having a width of80 mm above and thickness of 30μm above and having good toughness.SummaryDirected to the above problems, the present invention provides an amorphousalloy strip and a preparation method thereof. A requirement of the cooling rolleron the cooling capacity of the molten alloy during preparation of a strip isachieved by means of fitting among the thickness of the strip, the thermalconductivity of the roller sleeve, and the maximum usable thickness of the rollersleeve, thereby preparing a strip having a width of ≥80 mm and a thickness of≥30μm.To achieve the above objectives, the present invention adopts the followingtechnical solutions:an amorphous alloy strip is provided, and the amorphous alloy strip has awidth of ≥80 mm, a thickness of ≥30 μm, and a toughness value of <4.0.Preferably, the amorphous alloy strip consists of: any one or more of Ti, Zr,Hf, V, Nb, Ta, Cr, Mo, W, Mn, Cu, Ag, Au, Zn, Al or Sn having a total content of0-20 at%, any one or more of Si, B, P or C having a total content of 15-30 at%,one or two of Co or Ni having a total content of 0-20 at%, and the balance is Fe.Preferably, the amorphous alloy strip is obtained by cooling a molten alloy bymeans of a cooling roller; the cooling roller includes a roller sleeve; a thermalconductivity and a maximum usable thickness of the roller sleeve, and thethickness of the amorphous alloy strip have the following relationship:δλd = k maxwhere λ is the thermal conductivity of the roller sleeve with a unit of W / m·K;dmax is the maximum usable thickness of the roller sleeve with a unit of mm;δis an average thickness of the amorphous alloy strip with a unit of μm;k has a value range of 1-2 mm3K / W; the optimization of k may be incombination with properties, width and process parameters of the amorphousalloy strip; the parameters include the molten alloy temperature, linear surfacevelocity of the cooling roller, space between nozzles, molten alloy pressure at thenozzles, protection parameters of the molten pond, flow rate and temperature ofthe cooling water.A method for preparing the amorphous alloy strip is provided, and themethod is as follows: the amorphous alloy strip is prepared by the rapidsolidification process of plane flow; the method includes steps of heating to meltraw materials of the amorphous alloy strip into a molten alloy, and spraying themolten alloy onto the surface of the cooling roller for cooling.Preferably, the molten alloy has a temperature of 1250-1450°C; the coolingroller has a linear velocity of surface rotation of 15-30 m / s and a surfacetemperature of 70-150°C; the amorphous alloy strip has a temperature of 120-200°Cwhen peeling off from the surface of the cooling roller; the molten alloy issprayed onto the surface of the cooling roller at a static pressure of 20-60 kPa anda width of a nozzle slit of 0.4-1.0 mm.Preferably, the molten alloy has a temperature of 1300-1400°C.Preferably, the molten alloy is sprayed onto the surface of the cooling rollerat a static pressure of 25-50 kPa.Preferably, the cooling roller has a surface temperature of 90-120°C.Preferably, the amorphous alloy strip has a temperature of 140-180°C whenpeeling off from the surface of the cooling roller.Preferably, the λ has a value of 80-350 W / m·K; and the dmax has a value of4-20 mm.Preferably, the dmax has a value of 4-20 mm; and the λ has a value of 100-300W / m·K.In the iron-based amorphous alloy of the present invention, Fe is the mostimportant element to provide ferromagnetic property for the material. Comparedwith Co or Ni, Fe has the highest atomic magnetic moment and thus, can enablethe alloy to have the strongest saturation magnetic induction in all the amorphousalloys. To obtain certain special properties, e.g., increased induced magneticanisotropy, Fe may be partially substituted by Co and / or Ni at a low substitutionratio, being not greater than 20 at%, otherwise the saturation magnetic inductionof the material will be reduced obviously.Any one or more of Ti, Zr, Hf, V, Nb, Ta, Cr, Mo, W, Mn, Cu, Ag, Au, Zn, Alor Sn may be added in the iron-based amorphous alloy of the present invention insmall amount, which is aimed at improving the thermal stability, corrosionresistance or mechanical properties of the alloy, or enabling the alloy to have thecapacity of forming a nanocrystal structure in the subsequent thermal treatment.The total amount of these elements added should be not greater than 20 at%,otherwise the saturation magnetic induction of the material will be reducedobviously.Si, B, P and C in the iron-based amorphous alloy of the present inventionareindispensable elements capable of making alloy forming an amorphousstructure during rapid solidification, and also called amorphous elements orvitrified elements. To achieve better amorphous forming ability, two or more ofthe elements should be added at the same time. The total content of these elementsis within 15-30 at%; too high or too low content will drop the amorphous formingability of alloy.The present invention has the following beneficial effects: the thickness andwidth of the strip determine the thermal load capable of being borne by the rollersleeve; the thermal conductivity and thickness of the roller sleeve must be selectedreasonably, thus achieving enough high cooling rate under such a condition.Therefore, the thickness of the strip, the thermal conductivity of the roller sleeveand the maximum usable thickness of the roller sleeve are mutually balanced andaffected; stable manufacturing of the wide and thick iron-based amorphous stripcan be achieved only when there exists an optimal fitting range among the threevariables. The present invention provides a method for manufacturing a wide andthick iron-based amorphous strip having a thickness of 30 μm or above and awidth of 80 mm or above. According to the specific requirements of differentcomponents and specifications of iron-based amorphous strips on the coolingcapacity, strip property, production costs and the like, parameters such as materialand thickness of the roller sleeve are selected reasonably such that the rollersleeve has the overall characteristics simultaneously, such as satisfactoryheat-conducting property, good heat resistance and anti-fatigue property, goodconsistency of performance of the roller sleeve and lower manufacturing costs ofthe roller sleeve. The wide and thick iron-based amorphous strip manufactured bysuch a roller sleeve can guarantee satisfactory electromagnetic properties, goodconsistency and low costs.Other features and advantages of the present invention will be set forth in thefollowing description, and will partially become apparent from the description, orunderstood via implementing the present invention. Objectives and otheradvantages of the present invention can be achieved and obtained by the structuresindicated in the description, claims and accompanying drawings.Brief Description Of The DrawingsTo describe the examples of the present invention or the technical solutionsin the prior art more clearly, the accompanying drawings described in theexamples or the prior art will be introduced simply one by one below. Apparently,the accompanying drawings described below are some examples in the presentinvention. A person skilled in the art can further obtain other drawings based onthese accompanying drawings without any inventive effort.FIG. 1 is a diagram showing a relationship among the thermal conductivityof a roller sleeve, the maximum usable thickness of the roller sleeve and thethickness of a strip in the present invention.Detailed Description Of EmbodimentsTo make the objectives, technical solutions and advantages of the examplesof the present invention clearer, the technical solutions in the examples of thepresent invention will now be described clearly and fully hereinafter withreference to the accompanying drawings in the examples of the present invention.Apparently, the examples described herein are merely a portion of theembodiments of the present invention, but are not all the embodiments of thepresent invention. Based on the examples of the present invention, all the otherexamples obtained by a person skilled in the art without any inventive effort shallfall within the protection scope of the present invention.Example 1:An amorphous alloy strip is provided; the amorphous alloy strip has a thickness of171 mm and a width of 32μm; the alloy component of the amorphous alloy strip isFe78Si9B13 (where 78, 9, 13, and other subscript figures indicate the molarpercentage of the corresponding element).A method for preparing the amorphous alloy strip is provided herein; in themethod, the amorphous alloy strip is prepared by the rapid solidification processof plane flow. The process includes steps of heating to melt raw materials of theamorphous alloy strip into a molten alloy, and spraying the molten alloy onto thesurface of the cooling roller for cooling. The amorphous alloy strip has a width of171 mm and a thickness of 32μm; the molten alloy has a temperature of 1370°C;the cooling roller has a linear velocity of surface rotation of 22 m / s and has asurface temperature of 70°C; the amorphous alloy strip has a temperature of 120°Cwhen peeling off from the surface of the cooling roller; the molten alloy issprayed onto the surface of the cooling roller at a static pressure of 35 kPa; thenozzle slit has a width of 0.8 mm; the cooling roller contains a roller sleeve; theroller sleeve has a thermal conductivity of 104 W / m·K, a thickness of 5.0 mm,and an inner diameter of 600 mm; the roller sleeve is made of Cu-Be alloy.Example 2:The example has the process and conditions the same as those in Example 1,but differs from Example 1 in that the thickness of the roller sleeve is 3.2 mm, thewidth of the strip is 213 mm and the thickness of the strip is 32μm.Example 3:An amorphous alloy strip is provided; the amorphous alloy strip has a thickness of143mm and a width of 38μm; the alloy component of the amorphous alloy strip isFe78Si9B13 (where 78, 9, 13, and other subscript figures indicate the molarpercentage of the corresponding element).A method for preparing the amorphous alloy strip is provided herein; in themethod, the amorphous alloy strip is prepared by the rapid solidification processof plane flow. The process includes steps of heating to melt raw materials of theamorphous alloy strip into a molten alloy, and spraying the molten alloy onto thesurface of the cooling roller for cooling. The amorphous alloy strip has a width of143 mm and a thickness of 38μm; the molten alloy has a temperature of 1390°C;the cooling roller has a linear velocity of surface rotation of 20 m / s and has asurface temperature of 150°C; the amorphous alloy strip has a temperature of 200°Cwhen peeled off from the surface of the cooling roller; the molten alloy is sprayedonto the surface of the cooling roller at a static pressure of 45 kPa; the nozzle slithas a width of 0.6 mm; the cooling roller contains a roller sleeve; the roller sleevehas a thermal conductivity of 346 W / m·K, a thickness of 17.0 mm and an innerdiameter of 1200 mm.Example 4:The example has the process and conditions the same as those in Example 3,but differs from Example 1 in that the thickness of the strip is 11.8mm, the widthof the strip is 142 mm and the thickness of the strip is 38μm.Example 5:An amorphous alloy strip is provided herein; the amorphous alloy strip has athickness of 143 mm and a width of 38μm; the alloy component of the amorphousalloy strip is Fe82Si4B13C1 (where the subscript figures indicate the molarpercentage of the corresponding element, the same below).A method for preparing the amorphous alloy strip is provided herein; in themethod, the amorphous alloy strip is prepared by the rapid solidification processof plane flow. The process includes steps of heating to melt raw materials of theamorphous alloy strip into a molten alloy, and spraying the molten alloy onto thesurface of the cooling roller for cooling. The amorphous alloy strip has a width of85 mm and a thickness of 48μm; the molten alloy has a temperature of 1380°C;the cooling roller has a linear velocity of surface rotation of 21 m / s and has asurface temperature of 80°C; the amorphous alloy strip has a temperature of 130°Cwhen peeled off from the surface of the cooling roller; the molten alloy is sprayedonto the surface of the cooling roller at a static pressure of 55 kPa; the nozzle slithas a width of 0.7 mm; the cooling roller contains a roller sleeve; the roller sleevehas a thermal conductivity of 82 W / m·K, a thickness of 48.0 mm and an innerdiameter of 600 mm.Example 6:An amorphous alloy strip is provided herein; the amorphous alloy strip has athickness of 100 mm and a width of 41μm; the alloy component of the amorphousalloy strip is Fe83Si3B11C1P2 (where the subscript figures indicate the molarpercentage of the corresponding element).A method for preparing the amorphous alloy strip is provided herein; in themethod, the amorphous alloy strip is prepared by the rapid solidification processof plane flow. The process includes steps of heating to melt raw materials of theamorphous alloy strip into a molten alloy, and spraying the molten alloy onto thesurface of the cooling roller for cooling. The amorphous alloy strip has a width of100 mm and a thickness of 41μm; the molten alloy has a temperature of 1365°C;the cooling roller has a linear velocity of surface rotation of 22 m / s and has asurface temperature of 90°C; the amorphous alloy strip has a temperature of 140°Cwhen peeled off from the surface of the cooling roller; the molten alloy is sprayedonto the surface of the cooling roller at a static pressure of 52 kPa; the nozzle slithas a width of 0.7 mm; the cooling roller contains a roller sleeve; the roller sleevehas a thermal conductivity of 180 W / m·K, a thickness of 7.5 mm and an innerdiameter of 600 mm.Example 7:The example has the process and conditions the same as those in Example 6,but differs from Example 6 in that the thickness of the strip is 4.5mm, the width ofthe strip is 284mm and the thickness is 41μm.Example 8:An amorphous alloy strip is provided herein; the amorphous alloy strip has athickness of 85 mm and a width of 49μm; the alloy component of the amorphousalloy strip is Fe60Co18Ta2Si8B12 (where the subscript figures indicate the molarpercentage of the corresponding element).A method for preparing the amorphous alloy strip is provided herein; in themethod, the amorphous alloy strip is prepared by the rapid solidification processof plane flow. The process includes steps of heating to melt raw materials of theamorphous alloy strip into a molten alloy, and spraying the molten alloy onto thesurface of the cooling roller for cooling. The amorphous alloy strip has a width of85 mm and a thickness of 49μm; the molten alloy has a temperature of 1360°C;the cooling roller has a linear velocity of surface rotation of 20m / s and has asurface temperature of 100°C; the amorphous alloy strip has a temperature of 160°Cwhen peeled off from the surface of the cooling roller; the molten alloy is sprayedonto the surface of the cooling roller at a static pressure of 55 kPa; the nozzle slithas a width of 0.7 mm; the cooling roller contains a roller sleeve; the roller sleevehas a thermal conductivity of 200 W / m·K, a thickness of 11.2 mm and an innerdiameter of 1600 mm.Example 9:The example has the process and conditions the same as those in Example 8,but differs from Example 8 in that the thickness of the strip is 5.7 mm, the widthof the strip is 85 mm and the thickness of the strip is 49μm.Comparative Example 1:An amorphous alloy strip is provided herein; the amorphous alloy strip has athickness of 170 mm and a width of 32μm; the alloy component of the amorphousalloy strip is Fe82Si4B13C1 (where the subscript figures indicate the molarpercentage of the corresponding element).A method for preparing the amorphous alloy strip is provided herein; in themethod, the amorphous alloy strip is prepared by the rapid solidification processof plane flow. The process includes steps of heating to melt raw materials of theamorphous alloy strip into a molten alloy, and spraying the molten alloy onto thesurface of the cooling roller for cooling. The amorphous alloy strip has a width of170 mm and a thickness of 32μm; the molten alloy has a temperature of 1380°C;the cooling roller has a linear velocity of surface rotation of 20m / s and has asurface temperature of 70°C; the amorphous alloy strip has a temperature of 120°Cwhen peeled off from the surface of the cooling roller; the molten alloy is sprayedonto the surface of the cooling roller at a static pressure of 45 kPa; the nozzle slithas a width of 0.6 mm; the cooling roller contains a roller sleeve; the roller sleevehas a thermal conductivity of 104 W / m·K, a thickness of 6.5 mm and an innerdiameter of 600 mm.Comparative Example 2:An amorphous alloy strip is provided herein; the amorphous alloy strip has athickness of 143 mm and a width of 31μm; the alloy component of the amorphousalloy strip is Fe82Si4B13C1 (where the subscript figures indicate the molarpercentage of the corresponding element, the same below).A method for preparing the amorphous alloy strip is provided herein; in themethod, the amorphous alloy strip is prepared by the rapid solidification processof plane flow. The process includes steps of heating to melt raw materials of theamorphous alloy strip into a molten alloy, and spraying the molten alloy onto thesurface of the cooling roller for cooling. The amorphous alloy strip has a width of143 mm and a thickness of 31μm; the molten alloy has a temperature of 1380°C;the cooling roller has a linear velocity of surface rotation of 21 m / s and has asurface temperature of 70°C; the amorphous alloy strip has a temperature of 120°Cwhen peeled off from the surface of the cooling roller; the molten alloy is sprayedonto the surface of the cooling roller at a static pressure of 55 kPa; the nozzle slithas a width of 0.7 mm; the cooling roller contains a roller sleeve; the roller sleevehas a thermal conductivity of 346 W / m·K, a thickness of 22.8 mm and an innerdiameter of 1200 mm.Comparative Example 3:An amorphous alloy strip is provided herein; the amorphous alloy strip has athickness of 100 mm and a width of 41μm; the alloy component of the amorphousalloy strip is Fe83Si3B11C1P2 (where the subscript figures indicate the molarpercentage of the corresponding element, the same below).A method for preparing the amorphous alloy strip is provided herein; in themethod, the amorphous alloy strip is prepared by the rapid solidification processof plane flow. The process includes steps of heating to melt raw materials of theamorphous alloy strip into a molten alloy, and spraying the molten alloy onto thesurface of the cooling roller for cooling. The amorphous alloy strip has a width of100 mm and a thickness of 41μm; the molten alloy has a temperature of 1365°C;the cooling roller has a linear velocity of surface rotation of 22 m / s and has asurface temperature of 70°C; the amorphous alloy strip has a temperature of 120°Cwhen peeled off from the surface of the cooling roller; the molten alloy is sprayedonto the surface of the cooling roller at a static pressure of 52 kPa; the nozzle slithas a width of 0.7 mm; the cooling roller contains a roller sleeve; the roller sleevehas a thermal conductivity of 180 W / m·K, a thickness of 11mm and an innerdiameter of 800mm.Comparative Example 4:An amorphous alloy strip is provided herein; the amorphous alloy strip has athickness of 85 mm and a width of 49μm; the alloy component of the amorphousalloy strip is Fe83Si3B11C1P2.A method for preparing the amorphous alloy strip is provided herein; in themethod, the amorphous alloy strip is prepared by the rapid solidification processof plane flow. The process includes steps of heating to melt raw materials of theamorphous alloy strip into a molten alloy, and spraying the molten alloy onto thesurface of the cooling roller for cooling. The amorphous alloy strip has a width of85 mm and a thickness of 49μm; the molten alloy has a temperature of 1365°C;the cooling roller has a linear velocity of surface rotation of 21 m / s and has asurface temperature of 70°C; the amorphous alloy strip has a temperature of 120°Cwhen peeled off from the surface of the cooling roller; the molten alloy is sprayedonto the surface of the cooling roller at a static pressure of 46 kPa; the nozzle slithas a width of 0.6mm; the cooling roller contains a roller sleeve; the roller sleevehas a thermal conductivity of 220 W / m·K, a thickness of 13.6mm and an innerdiameter of 1600 mm.To verify the technical effects of the present invention, the inventor designedcooling roller sleeves having combinations of key parameters such as differentthermal conductivity, different thickness and different inner diameters. As acontrol, roller sleeve parameters inconformity to the scope of the presentinvention were tested separately as the Comparative Examples. Processparameters in Examples 1-9 and Comparative Examples 1-4 are shown in Table 1;parameters of the cooling roller sleeve, measured data of average thickness,toughness value, lamination coefficient and magnetic property of the strip in eachexample and comparative example are shown in Table 2; the width, thickness,lamination coefficient and magnetic property of the strip are measured by themethod of national standard GB / T 19345.1-2017; the toughness value of the stripis measured by IEC 60404-8-11, namely, the International ElectrotechnicalCommission (IEC) standard.Table 1 Process parameters used in the manufacturing of the stripTable 2 Parameters of the cooling roller sleeve and measured data of the strippropertyAs can be seen, when the technical solution provided by the presentinvention is applied (namely, the thermal conductivity and the thickness of theroller sleeve are located within the shaded area in FIG. 1), the manufactured wideand thick iron-based amorphous alloy strip has a good toughness value, alamination coefficient of ≥0.86, a saturation magnetic induction Bs of ≥1.50 T, acoercive force Hc of ≤2.0 A / m, a specific total loss Pc(50 Hz, 1.3 T) of ≤0.15W / kgc and thus, is capable of achieving the objectives of the present invention;when the technical solution of the present invention is not applied (namely, thethermal conductivity and the thickness of the roller sleeve are located above theshaded area in FIG. 1), the manufactured wide and thick iron-based amorphousalloy strip has obviously weakened toughness.When the wide and thick iron-based amorphous strip having a thickness of30μm above and a width of 80 mm above is manufactured, the maximum usablethickness of the cooling roller sleeve is closely related to the thermal conductivityof the roller sleeve. When roller sleeve is made of a high-thermal conductivitytexture, the maximum thickness of the roller sleeve may be increased properly;when the roller sleeve is made of a low-thermal conductivity texture, themaximum thickness of the roller sleeve must be thinned, or the strip will sufferembrittlement even crystallization due to insufficient cooling. Based on thepresent invention, when the thermal conductivity of the roller sleeve texture usedis improved to 350 W / m·K from 80 W / m·K, the maximum usable thickness of theroller sleeve may be increased to 18 mm from 5 mm.When the wide and thick iron-based amorphous strip having a thickness of30μm above and a width of 80 mm above is manufactured, the relationshipbetween the maximum usable thickness of the roller sleeve and the thermalconductivity of the roller sleeve can be visually shown by the linear segment ABin FIG. 1. The linear segment AB has two aspects of meanings: firstly, if thethermal conductivity of the roller sleeve is determined in advance, the maximumusable thickness of the roller sleeve must be below the maximum usable thicknessvalue of the roller sleeve corresponding to the thermal conductivity on the linearsegment AB, or the cooling capacity may not be ensured; secondly, if themaximum thickness of the roller sleeve is determined in advance, the thermalconductivity of the roller sleeve material must be above the thermal conductivityvalue of the roller sleeve corresponding to the maximum thickness on the linearsegment AB, or the cooling capacity may not be ensured, either. That is to say, thelinear segment AB actually shows the upper limit of the maximum usablethickness of the roller sleeve at a constant thermal conductivity of the roller sleeve,and the lower limit of the thermal conductivity of the roller sleeve at a constantmaximum thickness of the roller sleeve.On the premise of a constant thermal conductivity of the roller sleeve, themaximum usable thickness of the roller sleeve is further related to the thickness ofthe manufactured strip. The thicker the manufactured strip is, the larger thethermal load capable of being borne by the roller sleeve is, and at this time, themaximum thickness of the roller sleeve must be further thinned. Similarly, on thepremise of a constant maximum thickness of the roller sleeve, the thermalconductivity of the roller sleeve material must be further enhanced when a thickerstrip is manufactured. In this way, the preferable range of "thermal conductivity ofroller sleeve-maximum usable thickness of roller sleeve" will be located belowthe linear segment AB in FIG. 1 on the condition of different strip thickness.Therefore, when the wide and thick iron-based amorphous strip having athickness of 30μm above and a width of 80 mm above is manufactured, theoptimal thermal conductivity range and the actual usable thickness range of theroller sleeve are located within the scope of the polygon ABCD of the shaded areain FIG. 1, where coordinates in each point are A (80, 4), B (350, 20), C (80, 2),and D (350, 2).The diameter of the cooling roller sleeve is mainly selected according to theprocess equipment conditions. The diameter of the cooling rollerhas certainimpact on the cooling capacity of the cooling roller system, but has smaller degreeof impact relative to the thermal conductivity and thickness of the roller sleeve.The suitable range of the inner diameter of the roller sleeve is 400-1600 mmaccording to the present invention. More preferably, the optimal range of the innerdiameter of the roller sleeve is 500-1200 mm.The roller sleeve belongs to the category of consumable materials, after eachproduction of the strip, roller surface turning needs to be performed to remove thethermal fatigue layer on the surface thereof; therefore, the actual thickness of theroller sleeve is gradually thinned during the whole service life. When the rollersleeve is thinned to a certain extent, a new roller sleeve must be replaced. Toreduce the production costs, it is always desirable that the initial thickness of thenew roller sleeve is as large as possible. However, the maximum thickness of theroller sleeve is determined while the cooling capacity thereof must be guaranteedat the same time according to the present invention. Therefore, the initialthickness of the roller sleeve may be determined by the following two ways inactual production: one is to limit the initial thickness of the new roller sleevewithin the maximum usable thickness directly, and accordingly, the new rollersleeve may be directly used to produce the wide and thick iron-based amorphousstrip. Another way is to intentionally make the initial thickness of the new rollersleeve greater than the maximum usable thickness in the manufacturing of thewide and thick iron-based amorphous strip. The roller sleeve is only used toproduce a thinner amorphous strip or an amorphous strip with lower requirementson the cooling rate when the actual thickness of the roller sleeve is greater thanthe maximum usable thickness; when the thickness of the roller sleeve isconsumed below the maximum usable thickness in the manufacturing of the wideand thick iron-based amorphous strip, the manufacturing of the wide and thickiron-based amorphous strip is initiated. That is to say, during the purchasing ormanufacturing process of a new roller sleeve, it is feasible to limit the initialthickness of the roller sleeve below the maximum usable thickness, or to make theinitial thickness of the new roller sleeve greater than the maximum usablethickness.Even though the present invention is described specifically with reference tothe preceding examples, it is understood that a person skilled in the art can stillamend the technical solutions recorded in the preceding examples, or makeequivalent substitutions on a portion of the technical features thereof. Moreover,these amendments or substitutions of the corresponding technical solution shallfall within the spirit and scope of the technical solution in the examples of thepresent invention.

Claims

1. An amorphous alloy strip, wherein the amorphous alloy strip has a width of ≥80 mm, a thickness of ≥30 μm, and a toughness value of <4.0.

2. The amorphous alloy strip according to claim 1, wherein the amorphous alloy strip consists of: any one or more of Ti, Zr, Hf, V, Nb, Ta, Cr, Mo, W, Mn, Cu, Ag, Au, Zn, Al or Sn having a total content of 0-20 at%, any one or more of Si, B, P or C having a total content of 15-30 at%, one or two of Co or Ni having a total content of 0-20 at%, and the balance is Fe.

3. The amorphous alloy strip according to claim 1 or 2, wherein the amorphous alloy strip is obtained by cooling a molten alloy by means of a cooling roller; the cooling roller comprises a roller sleeve; a thermal conductivity and a maximum usable thickness of the roller sleeve, and the thickness of the amorphous alloy strip have the following relationship: δ d k λ = max wherein λ is the thermal conductivity of the roller sleeve with a unit of W / m·K; dmax is the maximum usable thickness of the roller sleeve with a unit of mm; δis an average thickness of the amorphous alloy strip with a unit of μm; k has a value range of 1-2 mm3K / W.

4. A method for preparing the amorphous alloy strip of claim 3, wherein the method comprises steps of heating to melt raw materials of the amorphous alloy strip into a molten alloy, and spraying the molten alloy onto the surface of the cooling roller for cooling.

5. The method for preparing the amorphous alloy strip according to claim 4, wherein the molten alloy has a temperature of 1250-1450°C; the cooling roller has a linear velocity of surface rotation of 15-30 m / s and a surface temperature of 70-150 C; the amorphous alloy strip has a temperature of 120-200°C when peeling off from the surface of the cooling roller; the- molten alloy is sprayed onto the surface of the cooling roller at a static pressure of 20-60 kPa and a width of a nozzle slit of 0.4-1.0 mm.

6. The method for preparing the amorphous alloy strip according to claim 4, wherein the molten alloy has a temperature of 1300-1400°C.

7. The method for preparing the amorphous alloy strip according to claim 4, wherein the molten alloy is sprayed onto the surface of the cooling roller at a static pressure of 25-50 kPa.

8. The method for preparing the amorphous alloy strip according to claim 4, wherein the cooling roller has a surface temperature of 90-120°C.

9. The method for preparing the amorphous alloy strip according to claim 4, wherein the amorphous alloy strip has a temperature of 140-180°C when peeling off from the surface of the cooling roller10. The method for preparing the amorphous alloy strip according to claim 4, wherein the X has a value of 80-350 W / m-K and the dmm has a value of 4-20 mm.

11. The method for preparing the amorphous alloy strip according to claim 4, wherein the dma}i has a value of 4-20 mm and the X has a value of 100-300 W / m-K.