Method for fabricating flexible and self-supporting PANI / PVDF composite films for energy storage devices
Patent Information
- Application Number
- IN202541132544
- Authority / Receiving Office
- IN · IN
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2025-12-27
- Publication Date
- 2026-10-09
- Estimated Expiration
- 2045-12-27
AI Technical Summary
Existing flexible energy storage devices face challenges in achieving high areal capacitance, energy density, and long-term cycling stability due to reliance on binders and current collectors, which limit mechanical flexibility and scalability, and lack uniform nanostructures for improved electrochemical performance.
A method for preparing a binder-free, self-supporting PANI/PVDF composite film through oxidative polymerization of an aniline monomer and ammonium peroxydisulfate, followed by dispersion in a polar aprotic solvent and vacuum filtration, resulting in a uniform distribution of PANI within PVDF, forming a predominantly electroactive β-phase for enhanced mechanical robustness and electrochemical activity.
The composite film exhibits high specific capacitance, energy density, and power density with efficient surface-controlled charge storage, maintaining capacitance under mechanical deformation, and demonstrating excellent cycling stability, making it suitable for flexible and wearable supercapacitors.
Abstract
Description
FIELD OF THE INVENTION
[0001] The present invention is related to polymer-based composite films for supercapacitors moreparticularly using an aniline monomer and an ammonium peroxydisulfate (APS).BACKGROUND
[0002] Flexible energy storage devices have evolved from substrate-supported PANI, graphene,CNT, and metal oxide-polymer electrodes, which often suffer from poor mechanical flexibility,cracking, and limited cycle stability. Early PANI-based and nanocomposite films improvedconductivity and capacitance but relied on binders, current collectors, or substrates, limitingrobustness and scalability. Efforts to control polymer phases and achieve uniform nanostructuresenhanced electrochemical performance but often compromised mechanical integrity. Devices alsofaced challenges in maintaining performance under repeated bending or deformation. Achievinghigh areal capacitance, energy density, and long-term cycling stability simultaneously remaineddifficult. Therefore, there is a continuing need for flexible, mechanically robust, andelectrochemically efficient materials for wearable energy storage applications.
[0003] The existing invention discloses a polyaniline (PANI)-MIL-101 metal-organic framework(MOF) nanocomposite flexible supercapacitor and a method for its preparation. MIL-101 isselected for its excellent acid resistance and chemical stability. The preparation method involves:synthesizing the PANI / MIL-101 composite material; dispersing the composite in N-methyl-2-pyrrolidone (NMP) with acetylene black and polyvinylidene fluoride (PVDF, e.g., Kynar) to forma homogeneous slurry; coating the slurry onto carbon cloth to form flexible electrodes; andassembling a symmetric supercapacitor by stacking two electrodes with a gel electrolyte separatedby a diaphragm, followed by encapsulation. The resulting electrode exhibits a specific capacitanceof up to 1197 F / g. The flexible supercapacitor demonstrates excellent mechanical stability,retaining 90% of its capacitance after 10,000 cycles and showing only 10% decay after 1000bending cycles. Four connected devices can power a 1.8 V red LED. The supercapacitor combineshigh electrochemical performance with mechanical flexibility, showing strong potential forapplications in flexible electronics and wearable energy storage devices.
[0004] Furthermore, the other invention discloses an asymmetric supercapacitor comprising apositive electrode with a current collector and a first active material selected from layered doublehydroxides, lithium metal oxides, metal sulphides, phosphate-based compounds, activated carbon,graphite, or combinations thereof. The negative electrode comprises a carbonaceous material,metal, metal oxide, metal nitride, metal sulphide, or conductive polymer, optionally supported bya current collector. The device employs a solid or aqueous electrolyte and includes a separatorplate. The electrodes can be nanostructured, and the supercapacitor exhibits high electrochemicalperformance, mechanical stability, and flexibility. The positive and negative electrodes mayincorporate conductive polymers, binders, or coatings, and are fabricated with controlledthicknesses to optimize capacitance and energy density. The supercapacitor demonstrates excellentcycling stability, high specific capacitance, and practical utility in flexible electronic devices andenergy storage applications.
[0005] The existing inventions have limitations: lack free-standing, self-supporting structures.They do not control the polymer phase, leaving PVDF in a mixed or inactive form, and rely onconventional slurry coating methods, resulting in less uniform and mechanically weaker films.Mechanical flexibility and stability under bending are only qualitatively addressed, with noquantitative evaluation. Electrochemical performance is reported mainly by gravimetriccapacitance, without detailed analysis of surface-controlled charge storage, energy density, orpower density. Device assembly requires current collectors or additional supports, limitingscalability and flexibility. Hence, the present invention provides a free-standing, binder-freePANI / PVDF films with PVDF β-phase, uniform nanostructure, high mechanical robustness, andquantified electrochemical performance, overcoming these limitations.SUMMARY
[0006] A method for preparing a flexible, free-standing, binder-free polyaniline / polyvinylidenefluoride (PANI / PVDF) composite film for use as an electrochemically active electrode in flexibleand wearable supercapacitors.
[0007] Polyaniline is synthesized by oxidative polymerization of an aniline monomer in an acidicmedium using ammonium peroxydisulfate, followed by washing to obtain a neutral PANI clay.
[0008] The neutralized PANI is uniformly dispersed in a polar aprotic solvent, while PVDF isseparately dissolved to form a homogeneous solution. The PANI dispersion is then combined withthe PVDF solution at controlled weight ratios ranging from 60:40 to 80:20.
[0009] The resulting composition is vacuum-filtered through a microporous nylon membrane anddried under compression. This process yields a crack-free, self-supporting composite film withoutthe need for additional binders or current collectors.
[0010] Structural and chemical characterization confirms uniform distribution of PANI within thePVDF matrix and predominant formation of the electroactive β-phase of PVDF. The resultingcomposite films exhibit excellent mechanical flexibility, robustness, and enhanced electrochemicalactivity.
[0011] When used as electrodes in symmetric supercapacitor devices with a PVA-H2SO4 gelelectrolyte, the films demonstrate high specific capacitance, energy density, and power density.
[0012] The electrodes show efficient charge-discharge behavior dominated by surface-controlledmechanisms. Additionally, the devices retain good capacitance over repeated cycling and undermechanical bending.
[0013] Consequently, the present invention provides a scalable and efficient approach forfabricating high-performance flexible electrodes.OBJECTIVES OF THE INVENTION
[0014] The main objective of the proposed invention is to develop a simple, scalable, and binderfree method for fabricating a flexible, free-standing polyaniline / polyvinylidene fluoride compositefilm with high mechanical robustness and electrochemical activity.
[0015] Another objective is to combine the pseudocapacitive properties of polyaniline with theflexibility and electroactive β-phase characteristics of PVDF to obtain a durable electrode suitablefor flexible and wearable supercapacitor applications.DETAILED DESCRIPTION OF THE INVENTION:
[0016] A method for preparing a flexible, free-standing polyaniline / polyvinylidene fluoride(PANI / PVDF) composite film has been proposed in the present invention and to the resultingcomposite films, which are particularly useful as mechanically robust and electrochemically activeelectrodes for flexible and wearable supercapacitor applications. The invention provides a binderfree, self-supporting polymer composite electrode that combines the high pseudocapacitiveperformance of polyaniline with the mechanical flexibility, chemical stability, and electroactive βphase characteristics of PVDF.
[0017] The proposed invention comprises step-1: an acidic medium, an aniline monomer, anammonium peroxydisulfate (APS), a methanol, a polar aprotic solvent, a polyvinylidene fluoride(PVDF) polymer and a nylon membrane. Step-2: the acidic medium or hydrochloric acid of 1M isdiluted using deionised water at a temperature of 0-5 °C. The aniline monomer of 4.6mL isprotonated in 1M of the diluted acidic medium using the ammonium peroxydisulfate (APS) of 5.9g as an oxidant to form the polyaniline (PANI) clay. The polyaniline (PANI) clay is washed withthe methanol and deionized water until a neutral pH is achieved, ensuring the removal of unreactedspecies and residual acid.
[0018] The neutralized polyaniline (PANI) clay of 0.8g / mL is dispersed in the polar aprotic solventpreferably dimethyl sulfoxide (DMSO) of 3mL with magnetic and ultrasonicated for 2 hours whichpromotes deagglomeration of PANI particles and enhances dispersion stability to form apolyaniline (PANI) dispersion. This step ensures uniform distribution of electroactive PANI withinthe polymer matrix in the final composite film. Step-3: the polyvinylidene fluoride (PVDF)polymer of 200mg is dissolved in the polar aprotic solvent of 5mL at 60°C for 2 hours to form apolyvinylidene fluoride (PVDF) solution.
[0019] Step-4: the polyaniline (PANI) dispersion in step-2 is added to the polyvinylidene fluoride(PVDF) solution under continuous stirring for 30 minutes to form a composition. The relativeweight ratio of PANI to PVDF is adjusted between 60:40 and 80:20 (w / w), resulting in compositefilms designated as 64Pp, 73Pp, and 82Pp, respectively. It has been observed that composite filmswithin this composition range exhibit optimal mechanical integrity and electrochemicalperformance while avoiding surface cracking. The composition is then subjected to vacuumfiltration through a microporous membrane, preferably a nylon membrane having a pore size ofapproximately 0.22 μm.
[0020] Vacuum filtration is continued for a period of about 1 to 1.5 hours, during which a uniform,free-standing composite film is formed on the membrane surface. The filtered composition is driedunder compression at 60°C for 6 hours to form the polyaniline / polyvinylidene fluoride(PANI / PVDF) composite film. Drying under compression enhances interfacial adhesion betweenPANI and PVDF, improves mechanical robustness, and yields a crack-free, flexible, and selfsupporting composite film without the need for additional binders or current collectors. Structuraland chemical characterization of the composite film reveals that PVDF predominantly exists in itselectroactive β-phase, as confirmed by X-ray diffraction (XRD) analysis.
[0021] Fourier transform infrared spectroscopy (FTIR) further confirms the presence ofcharacteristic absorption bands corresponding to the β-phase of PVDF, indicating that theprocessing method promotes electroactive phase formation. Scanning electron microscopy andelemental color mapping demonstrate that aggregated PANI nanospheres are uniformly distributedwithin the PVDF matrix, with homogeneous distribution of carbon, nitrogen, oxygen, fluorine, andsulfur throughout the film. The free-standing composite films prepared according to the inventionexhibit excellent electrochemical properties when employed as electrodes in symmetricsupercapacitor configurations.
[0022] In a representative embodiment, the 82Pp composite film exhibits a specific capacitance ofapproximately 347.72 F / cm2 at a scan rate of 10 mV / s. The films demonstrate a predominantlysurface-controlled, non-Faradaic charge storage mechanism, indicating efficient active surfaceutilization and rapid charge-discharge kinetics. The composite films further exhibit high energydensity, reaching approximately 52.24 mWh / cm2, and a power density of about 1099.78 mW / cm2.For device fabrication, the free-standing composite film is used directly as both the anode andcathode in a symmetric supercapacitor assembly.
[0023] A polyvinyl alcohol-sulfuric acid (PVA-H2SO4) gel electrolyte is employed, with GradeB59501 filter paper serving as a flexible separator and substrate. The assembled device showsexcellent cycling stability, retaining at least 64.3% of its initial capacitance after 500 cyclicvoltammetry cycles. Additionally, the device maintains stable electrochemical performance undermechanical deformation, including bending angles of 0°, 90°, 120°, and 150°, demonstrating itssuitability for flexible and wearable energy storage applications. Accordingly, the presentinvention provides a scalable, reproducible, and efficient method for fabricating flexible, freestanding PANI / PVDF composite films with superior mechanical flexibility, electrochemicalperformance, and long-term stability, making them highly suitable for next-generation flexible andwearable supercapacitor devices.
Claims
1. A method for preparing a flexible, free-standing polyaniline / polyvinylidene fluoride (PANI / PVDF) composite film, comprising: step-1: an acidic medium; an aniline monomer; an ammonium peroxydisulfate (APS); a methanol; a polar aprotic solvent; a polyvinylidene fluoride (PVDF) polymer; a nylon membrane; step-2: the acidic medium of 1M is diluted using deionised water at a temperature of 0-5 °C; the aniline monomer of 4.6mL is protonated in 1M of the diluted acidic medium using the ammonium peroxydisulfate (APS) as an oxidant to form the polyaniline (PANI) clay; the polyaniline (PANI) clay is washed with the methanol and deionized water until a neutral pH is achieved; the neutralized polyaniline (PANI) clay of 0.8g / mL is dispersed in the polar aprotic solvent of 3mL with magnetic stirring and ultrasonicated for 2 hours to form a polyaniline (PANI) dispersion; step-3: the polyvinylidene fluoride (PVDF) polymer of 200mg is dissolved in the polar aprotic solvent of 5mL at 60°C for 2 hours to form a polyvinylidene fluoride (PVDF) solution; step-4: the polyaniline (PANI) dispersion in step-2 is added to the polyvinylidene fluoride (PVDF) solution in step-3 under continuous stirring for 30 minutes to form a composition; the composition is vaccum filtered through the 0.22μm of nylon membrane for 1 hour; and the filtered composition is dried under compression at 60°C for 6 hours to form the polyaniline / polyvinylidene fluoride (PANI / PVDF) composite film.
2. The method as claimed in claim 1, wherein the acidic medium in step-1 is a hydrochloric acid.
3. The method as claimed in claim 1, wherein the ammonium peroxydisulfate (APS) is used in an amount of 5.9 g.
4. The method as claimed in claim 1, wherein the polar aprotic solvent in step-1 is a dimethyl sulfoxide (DMSO).