A conductive nanocomposition for wound management and a method of preparation thereof
Patent Information
- Application Number
- IN202411081983
- Authority / Receiving Office
- IN · IN
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2024-10-28
- Publication Date
- 2026-10-22
- Estimated Expiration
- 2044-10-28
AI Technical Summary
Existing conductive hydrogels for wound management are complex, costly, and lack biocompatibility and antimicrobial properties, making them unsuitable for scalable production and effective wound healing, particularly in diabetic wounds.
A biocompatible conductive hydrogel is developed using bovine serum albumin (BSA) and graphene oxide (GO) reduced with ascorbic acid, which imparts conductivity and antibacterial properties, suitable for wound management.
The hydrogel effectively manages diabetic wounds in 8-12 days with enhanced mechanical strength, electrical conductivity, and antibacterial properties, promoting rapid wound healing.
Abstract
Description
FIELD OF THE INVENTION The present invention relates to the field of wound management. More particularly, the present invention relates to the biocompatible and conductive nanocomposition for management of wound exhibiting anti-bacterial properties and is prepared by the reduction of serum albumin (BSA) protein and graphene oxide (GO)-based hydrogel through ascorbic acid.BACKGROUND OF THE INVENTIONWound management helps in healing of wounds by providing a suitable environment and depends on several factors such as size, depth and severity of wound. Wound management promotes the smooth transition of wound through four different stages of wound healing that includes hemostasis, inflammation, proliferation and remodeling. Various parameters including age, infection, stress, diabetes, alcohol intake, smoking, and nutrition plays an important role in wound healing.Diabetic wound is a complicated case due to severe nerve damage and poor blood circulation in Diabetes Milletus patients that leads to development of deep wounds and chronic ulcers. Furthermore, high blood sugar levels and compromised immune system promotes the growth of bacteria leading to infection that worsen the process of wound healing. Available treatment includes antibacterial dressing, sugar control, surgical debridement and oxygen therapy that are accompanied with drawbacks like lengthy and painful procedures, and involves the use of hazardous materials and expensive process. In order to combat this, numerous materials are being tested for wound management such as biodegradable and natural polymers along with naturally occurring and cost effective substances with properties that manage wounds. In this regard, conductive hydrogels deserve a mention as normal skin cell's conductivity is impaired in cases of wound.EP0934593B1 reveals an electrically conductive adhesive hydrogel of cationic acrylate polymer formed by free radical polymerization in the presence of water by ultra-violet curing with initiator and multi-functional cross-linking agent. However, the hydrogel disclosed in the cited invention utilizes multiple components and hence increasing the cost of the product.US20080207779A1 discloses a precipitate-free electrically conductive hydrogel comprising N,N-Dimethylaminoethyl acrylate dimethyl sulfate quaternary, dimethyl amino ethyl methacrylate, acrylamido methyl propane sulfonic acid as monomer; one initiator; cross-linking agent; and an organic solvent. However, the cited invention employs methylene-bis-acrylamide as cross linking agent that is not biocompatible and hence limiting the use of hydrogel to non-biological applications.EP3619272 reveals an electrically conductive antifouling coating comprising a mixture of carbon nanotube or graphene and a proteinaceous material. The cited invention states that the composition upon functionalization can be used in biological fluid and tissues on living organism such as implant or diagnostic probe. However, the biological assessment of the composition with respect to biocompatibility, antimicrobial properties are not provided in the cited invention.In view of the above mentioned citations, it is evident that conductive hydrogels are extensively prepared and assessed for their adhesive properties, however these are not evaluated for their biological applications especially in terms of biocompatibility, biodegradability, and antimicrobial potential. Additionally, the preparation method is complex and require multiple components as initiator and cross linking agents.Therefore, there is a need of developing a conductive hydrogel using biocompatible materials that possess biocompatibility and antimicrobial potential with none or limited side effects and is prepared in a cost-effective and time-efficient manner for scalable production. OBJECT OF THE INVENTION The main object of the present invention is to provide a conductive nanocomposition of a hydrogel for wound management.Another object of the present invention is to provide a bovine serum albumin (BSA) and graphene oxide (GO)-based hydrogel. Yet another object of the present invention is to provide a bovine serum albumin (BSA)-based hydrogel incorporated with graphene oxide (GO) to impart electrical properties to hydrogel. Yet another object of the present invention is to provide a method of preparation of bovine serum albumin (BSA) and graphene oxide (GO)-based conductive hydrogel (r(GO / BSA)).Still another object of the present invention is to provide a conductive hydrogel exhibiting antibacterial properties and is biocompatible. SUMMARY OF THE INVENTIONThe present invention relates to a conductive nanocomposition for wound management and a method of preparation thereof. The combination of bovine serum albumin (BSA) and graphene oxide (GO) is subsequently reduced with ascorbic acid to tune the electrical properties of graphene oxide thereby imparting conductivity to the hydrogel. The conductive hydrogel is biocompatible and exhibits the management of the diabetic wound in a span of 8 - 12 days.In an embodiment, the present invention provides a conductive nanocomposition for wound management comprising of a bovine serum albumin and a graphene oxide whereby Bovine Serum Albumin (BSA) is in a concentration range of 15% to 20% (w / v) and graphene oxide is in a concentration range of 0.1 to 1% (w / v)). The nanocomposition is in the form of a hydrogel that is further is reduced in presence of a reducing agent. In another embodiment, the present invention provides a method of preparation of conductive nanocomposition in the form of hydrogel comprising the steps of dissolving 250 to 350 mg / ml of BSA powder in deionized (Di) water to form a solution of BSA and dissolving 5 to 10 mg of graphene oxide powder in 1-2 ml DI water to form a dispersion of Graphene oxide (GO). 150 - 250 mg / ml of the solution of BSA was taken along with the dispersion of graphene oxide in the range of 0.1 to 1% (w / v) to form a sample of GO-BSA which is incubated in a pre-heated hot air oven at 80°C for 30 minutes followed by cooling the sample at room temperature to prepare a dried sample of GO-BSA that is treated with a reducing agent at a predetermined temperature of 37°C for a predefined time period of 24 hours followed by washing 3 to 5 times with DI water to form a hydrogel. In yet another embodiment, the present invention provides a method of preparation of dispersion of graphene oxide. 1 - 2 g of graphite is mixed with with 150 - 200 mL of concentrated sulphuric acid (H2SO4) and 1.3 - 1.6 g of sodium nitrate (NaNO3) for 15 - 20 minutes in a three-neck flask under constant magnetic stirring while maintaining temperature in a range of 3 to 5°C to form a mixture. 4 - 6 g of potassium permanganate (KMnO4) is added slowly to mixture over a period of 25 - 30 minutes under continuous stirring to form a dark green paste that is further diluted with 180 - 250 mL of deionized (DI) water followed by adding hydrogen peroxide (H2O2) dropwise to produce a dark brown mixture. The dark brown mixture is washed with hydrogen chloride (HCl) and DI water followed by sonication and centrifugation to form a KMnO4 and metal ions free sediment that is further air-dried for 4 to 5 hours to obtain graphite oxide powder. 10 to 15 mg of powder of graphite oxide is dispersed in 1 to 2 DI water followed by sonicating in a water bath to obtain a dispersion of graphene oxide.The present invention relates to the preparation of a biocompatible and antibacterial protein-based conductive hydrogel incorporated with graphene oxide for the management of rapid chronic diabetic wounds aided by combating of the bacterial infection.The above objects and advantages of the present invention will become apparent from the hereinafter set forth brief description of the drawings, detailed description of the invention, and claims appended herewith.BRIEF DESCRIPTION OF THE DRAWINGSAn understanding of the conductive nanocomposition for wound management and a method of preparation thereof of the present invention may be obtained by reference to the following drawings:Figure 1 is a graphical representation of UV / visible (UV / Vis) spectra of graphene oxide (GO) in part (a); a graphical representation of X-ray Diffraction (XRD) spectra of graphene oxide in part (b); a graphical representation of Raman spectra of graphene oxide in part (c); a graphical representation of size distribution of graphene oxide suspension in part (d); a pictorial representation of scanning electron microscopic (SEM) image of graphene oxide in part (e); and a pictorial representation of transmission electron microscopic (TEM) image of graphene oxide in part (f), according to the present invention.Figure 1 is a pictorial representation of BSA protein hydrogels with varying concentration of GO (0, 0.1, 0.5, 1.0% GO (w / v)) in part (a); a pictorial representation of partial reduction of (GO / BSA)0.5 hydrogel by ascorbic acid in part (b); a graphical representation of raman spectra of (GO / BSA)0.5 compared to its reduced forms in part (c); a graphical represenatation of comparative plot of ID / IG ratio for different duration of reduction in part (d); a pictorial representation of SEM images of cross-sectional area of hydrogels of BSA in part (e); a pictorial representation of SEM images of crosssectional area of hydrogels of r(GO / BSA)0.1 in part (f); a pictorial representation of SEM images of crosssectional area of hydrogels of r(GO / BSA)0.5 in part (g); a pictorial representation of SEM images of crosssectional area of hydrogels of r(GO / BSA)1.0 in part (h); a graphical representation of pore distribution of BSA in part (i); a graphical representation of pore distribution of r(GO / BSA)0.1 in part (j); a graphical representation of pore distribution of r(GO / BSA)0.5 in part (k); and a graphical representation of pore distribution of r(GO / BSA)1.0 in part (l), according to the present invention.Figure 2 is a graphical representation of: the amplitude sweep of hydrogels comprised of various concentrations of GO in part (a); the frequency sweep of hydrogels comprised of various concentrations of GO in part (b); the viscosity versus shear rate plot of hydrogels comprised of various concentrations of GO in part (c); the compressive test of hydrogels comprised of various concentrations of GO showcasing relation between stroke and force in part (d); the cyclic compressive test for r(GO / BSA)1.0 hydrogel in part (e); the swelling ratio of hydrogels comprised of various concentrations of GO in part (f); the water remaining ratio of hydrogels comprised of various concentrations of GO in part (g); two probe conductivity measurement of hydrogels comprised of various concentrations of GO in part (h); electrochemical impedance spectroscopy (EIS) measurement of conductivity for hydrogels comprised of various concentrations of GO in part (i), according to the present invention.Figure 4 is a pictorial representation of antibacterial properties of effect of BSA hydrogel in (i), r(GO / BSA) hydrogel (ii), ampicillin (iii), and GO / BSA hydrogel (iv) on gram-positive (S. aureus) and gram-negative (E. coli) bacteria inoculated in agar plates in part (a); a graphical representation of the optical density recorded for S. aureus and E. coli bacteria solutions exposed to BSA, GO / BSA and r(GO / BSA) hydrogels compared with control group in part (b); a graphical representation of cell viability of NIH 3T3 fibroblast cells exposed to various dose concentrations of BSA hydrogel, GO / BSA hydrogel, and r(GO / BSA) hydrogel in part (c), according to the present invention.Figure 5 is a pictorial representation of macroscopic images taken on day 0, 3, 7, 10, and 16 showcasing the wound closing process for control, BSA hydrogel, and r(GO / BSA) hydrogel in part (a); a pictorial representation of histopathological anatomy of wound tissue after the wound healing in part (b); weight and blood glucose levels information for rats of three groups is represented in tabulated form in part (c); and a graphical representation of the wound closure speed for three different groups in part (d), according to an embodiment of the present invention.DETAILED DESCRIPTION OF THE INVENTION The present invention will now be described hereinafter with reference to the accompanying drawings in which a preferred embodiment of the invention is shown. This invention may, however, be embodied in many different forms and should not be construed as being limited to the embodiment set forth herein. Rather, the embodiment is provided so that this disclosure will be thorough, and will fully convey the scope of the invention to those skilled in the art.The present invention now will be described hereinafter with reference to the detailed description, in which some, but not all embodiments of the invention are indicated. Indeed, the invention may be embodied in many different forms and should not be construed as limited to the embodiments set forth herein; rather, these embodiments are provided so that this disclosure will satisfy applicable legal requirements. Like numbers refer to like elements throughout. The present invention is described fully herein with non-limiting embodiments and exemplary experimentation. The present invention relates to a nanocomposition for wound management and a method of preparation thereof. The combination of Bovine serum albumin (BSA) and graphene oxide (GO) is subsequently reduced with ascorbic acid to impart conductivity to the hydrogel. The conductive hydrogel is biocompatible and exhibits the management of the diabetic wound in a time span of 8 to 12 days.In a preferred embodiment, the present invention provides a conductive nanocomposition for wound management comprising of a protein; and a carbon-based nanomaterial; wherein, said protein is Bovine Serum Albumin (BSA) in a concentration range of 15% to 20% (w / v); said carbon-based nanomaterial is graphene oxide in a concentration range of 0.1 to 1% (w / v); said nanocomposition is in form of a hydrogel; and said hydrogel is reduced in presence of a reducing agent. The reducing agent is ascorbic acid in a concentration range of 1.5 to 2 mg / ml.Here, said hydrogel is of pore size ranging from 21 to 28 μm and swells in a range of 300-400%. The hydrogel exhibits storage modulus in a range of 130 to 150 Pa and sustains 4.5 to 5x103 MPa of compressive stress with 50% deformation. The hydrogel exhibits conductivity in a range of 4.7 Sm-1 at 1 MHz frequency.Further, said hydrogel exhibits zone of inhibition in a range of 18 - 27.52 mm against E. coli and in a range of 25.6- 31.95 mm against S. aureus and cell viability in a range of 74-77% in NIH3T3 fibroblast cells. The hydrogel manages wound in a time span of 8 to 12 days.In another preferred embodiment, the present invention provides a method of preparation of conductive nanocomposition in the form of hydrogel comprising the steps of: a) dissolving 250 to 350 mg / ml of BSA powder in deionized (DI) water to form a solution of BSA; b) dissolving 5 to 10 mg of graphene oxide powder in 1 to 2 ml DI water to form a dispersion of Graphene oxide (GO); c) taking 150 - 250 mg / ml of said solution of bovine serum albumin (BSA) obtained in step (a) with said dispersion of graphene oxide obtained in step (b) in the range of 0.1 to 1% (w / v) to form a sample of GO-BSA; d) incubating said sample of GO-BSA obtained in step (c) in a preheated hot air oven at 80°C for 30 minutes followed by cooling the sample at room temperature to prepare a dried sample of GO-BSA; and e) treating said dried sample of GO-BSA obtained in step (d) with a reducing agent at a predetermined temperature of 37°C for a predefined time period of 24 hours followed by washing 3 to 5 times with DI water to form a hydrogel.In yet another preferred embodiment, the present invention provides a method of preparing dispersion of graphene oxide by the steps of i) mixing 1 - 2 g of graphite with 150 - 200 mL of concentrated sulphuric acid (H2SO4) and 1.3 - 1.6 g of sodium nitrate (NaNO3) for 15 - 20 minutes in a three-neck flask under constant magnetic stirring while maintaining temperature in a range of 3 to 5°C to form a mixture; ii) adding 4 to 6 g of potassium permanganate (KMnO4) slowly to said mixture obtained in step (i) over a period of 25 - 35 minutes under continuous stirring to form a dark green paste; iii) diluting said dark green paste obtained in step (ii) with 180 - 250 mL of deionized (DI) water followed by adding hydrogen peroxide (H2O2) dropwise to produce a dark brown mixture; iv) filtering said dark brown mixture obtained in step (iii) followed by washing with hydrogen chloride (HCl) and DI water to form a neutral mixture; v) removing KMnO4 and metal ions from said neutral mixture obtained in step (iv) through sonication and centrifugation to form a sediment; vi) subjecting said sediment obtained in step (v) to air drying for 4 to 5 hours to obtain graphite oxide powder; and vii) dispersing 10 to 15 mg of said powder of graphite oxide obtained in step (vi) in 1 to 2 of DI water followed by sonicating in a water bath to obtain a dispersion of graphene oxide.Referring to Figure 5, a pictorial representation of macroscopic images taken on day 0, 3, 7, 10, and 16 showcasing the wound closing process for control, BSA hydrogel, and r(GO / BSA) hydrogel in part (a); a pictorial representation of histopathological anatomy of wound tissue after the wound healing in part (b); weight and blood glucose levels information for rats of three groups is represented in tabulated form in part (c); and a graphical representation of the wound closure speed for three different groups is in part (d), is depicted.EXAMPLE 1 For Experimentation DetailsMaterialsBovine Serum Albumin (BSA), graphite, sulfuric acid (H2SO4, 98%), sodium nitrate (NaNO3), potassium permanganate (KMnO4), hydrochloric acid (HCl, 30%), Hydrogen peroxide (H2O2, 30%), and L-ascorbic acid were purchased from Sigma-Aldrich. Streptozotocin (STZ) and citrate buffer were purchased from Sigma-Aldrich. Dimethyl sulfoxide anhydrous (DMSO) and Fetal Bovine Serum (FBS) were procured from SRL. LB broth and nutrient agar media were purchased from HiMedia laboratories. NIH-3T3 cell line was procured from NCCS Pune. Deionized (DI) water (> 18MO) was used to prepare all aqueous solutions. All the reagents were used as such without further purification.Synthesis and characterization of Graphene oxide Graphene oxide was prepared by modified hummer's method, using graphite as precursor. Briefly, in a three-neck flask, 1 g of graphite was mixed with 150 mL of concentrated H2SO4 and 1.5 g of NaNO3 for 15 min under constant magnetic stirring while maintaining temperature under 5°C, followed by slow addition of 6g of KMnO4 to the mixture over a period of 30 minutes under continuous stirring until the mixture turned into a dark green paste. The prepared mixture was diluted with 180 mL of DI water and accompanied by dropwise addition of H2O2. The resulting dark brown mixture was filtered and washed with HCl and DI water until the neutral pH was achieved. The mixture was further sonicated and centrifuged to remove excess KMnO4 and metal ions. The sediment was air-dried overnight to obtain graphite oxide. Finally, the obtained powder was dispersed in DI water and sonicated in a water bath to obtain graphene oxide dispersion. The optical absorbance of the prepared graphene oxide (GO) was recorded using an Eppendorf biospectrometer in the wavelength range of 200-800 nm. To obtain detailed crystallographic information, X-ray diffraction technique analysis was performed using a Rigaku Miniflex 600 with a Cu-ka radiation source. Raman spectroscopy was conducted to analyze the structural defects of GO. DLS measurements were performed using Malvern Panalytical Zetasizer pro to examine the hydrodynamic size distribution and polydispersity index (PDI) of graphene oxide. The surface morphology of GO samples was examined using a scanning electron microscope (NovananoSEM), which provided detailed images of surface features. Furthermore, transmission electron microscopy (Tecnai G2 20 TWIN) was utilized to investigate the morphology at a higher resolution. Graphene oxide was exfoliated from graphite using modified hummer's method. The absorption spectra of the GO dispersion (in DI water), as presented in part (a) of Figure 1 exhibited a characteristic peak at 230 nm which is associated with p -p* transitions of the aromatic C = C bonds in the GO structure. A broad shoulder was also observed at 305 nm which is attributed to n- p* transitions of C = O bonds. These features are distinct to the GO spectra indicating successful synthesis of graphene oxide. X-ray diffraction (XRD) spectra, as presented in part (b) of Figure 1 revealed a prominent sharp peak at 2θ = 10.63° which is attributed to the (001) plane of GO, indicating an interlayer spacing of 8.2 Å. The significant increase in d-spacing compared to pristine graphite (3.4 Å) is due to the incorporation of oxygen-containing functional groups such as hydroxyl, epoxy, and carboxyl groups. The spectra also showcased a smaller peak at 42.8°, which is attributed to the (100) plane of graphene oxide. The presence of a small peak at 2θ = 20.5° is attributed to the (002) plane of graphite, indicating the presence of unoxidized graphitic particles alongside.Raman spectroscopy is an important tool for characterizing the structural properties of graphene oxide. As presented in part (c) of Figure 1, the Raman spectra of graphene oxide exhibited two bands. The D band centered at 1348 cm-1 is attributed to the defects and disorders present in the graphene lattice and is a characteristic feature of graphene oxide, whereas G band is associated with the in-plane stretching vibrations of sp2 carbon atoms present in graphene lattice and it is found to be centered around 1580 cm-1. The high ID / IG ratio (~ 1.05) indicated significant structural disorder created by incorporation of oxygen groups in the graphene lattice. The size distribution analysis of the graphene oxide dispersion in DI water as performed by dynamic light scattering is provided in part (d) of Figure 1. The plot revealed a uniformity in the GO dispersion, with the hydrodynamic radius centered around 150 nm. Next, SEM image of the prepared GO showcased two-dimensional morphology with wrinkled and curved texture, as shown in part (e) of Figure 1. The morphological information was complimented by the TEM images which revealed layers of GO stacked onto one another with the typical wrinkled morphology, as shown in part (f) of Figure 1. The extensive chemical and morphological analysis confirmed the successful synthesis of graphene oxide, which was further employed in the fabrication of composite hydrogel.EXAMPLE 2 Synthesis and characterization of r(GO / BSA) hydrogelLyophilized BSA powder was dissolved in DI water at 300 mg / ml concentration. A stock solution of 10 mg / ml Graphene oxide was prepared in DI water. Next, an assortment of samples of 200 mg / ml BSA was prepared in petri dishes with varying concentrations of GO (namely 0.1, 0.5, and 1% (w / v)). The petri dishes were incubated in a hot air oven preheated at 80°C for 30 minutes. After incubation, the obtained GO / BSA hydrogels were placed in ambient condition to bring them to room temperature. A control hydrogel was also prepared, where instead of GO, equivalent amount of DI was added to maintain a constant concentration. Eventually, GO / BSA hydrogels were chemically reduced to r(GO / BSA) by incubation in a 2 mg mL-1 ascorbic acid solution at 37 °C for 24 h. The hydrogels were washed several times by DI water and stored at 4°C for further application. For further reference, the hydrogels are named BSA for control, (GO / BSA)x and r(GO / BSA)x hydrogel respectively, where x represents the concentration of GO in the sample hydrogel.The porosity and cross-sectional surface morphology of the hydrogels were investigated using an EVO MA15 / 18 scanning electron microscope. Pore distribution data were analyzed and tabulated using ImageJ software. The rheological properties of the prepared hydrogels were measured using a parallel plate geometry setup in an Anton paar MCR 72 Rheometer. Initially, the linear viscoelastic range (LVR) was determined by applying a constant frequency of 10 rad / s. Subsequently, a frequency sweep was performed across a range of 0.1 rad / s to 10 rad / s at a constant strain in LVR to determine the storage and loss modulus, G' and G" respectively. Additionally, the shear thinning behavior was investigated in shear rate range of 0.1 - 100 s-1. The mechanical strength of prepared hydrogels was studied through compression tests performed on a texture analyzer (Shimadzu, Japan) with a maximum load capacity of 500 N. For these tests, the hydrogels were cut in cylindrical shape with a diameter of 10mm and a height of 5mm. The compression measurements were carried out at a constant speed of 1 mm / min. Additionally, cyclic compression tests were performed by subjecting hydrogels to 50% deformation over three cycles. The swelling ratio and water retention property of prepared hydrogels were investigated. The lyophilized samples were first soaked in DI water for 24 hours to allow them to reach equilibrium swelling. Then, the samples were carefully removed from the water and superficial water was removed by using kimwipes. The swollen samples were then weighed.The swelling ratio, S was calculated using the equation 1,S=(wt-w0) / w0 (1)where, w0 and wt are the weight of dry and swollen hydrogel samples, respectively.Water retaining ratio (WRR) was also calculated for all hydrogels. The swollen hydrogels were periodically weighed over a time period of 15 days at an interval of 2 days. Each measurement was conducted in triplicate for all hydrogel samples.Conductivity measurements were performed using a digital multimeter (FLUKE 287 true rms multimeter). The hydrogel samples were cut in cuboid shapes with fixed length and cross-section area. Triplicate readings for resistance were measured at the end points of each sample and averaged. The conductivity, s, was computed using the following relation having equation 2:ρ=L / (R.A) (2)where, R is the measured resistance, L and A are length and cross-sectional area of sample. To measure the ionic conductivity of the prepared hydrogels, electrochemical impedance spectra were recorded by applying an alternate sinusoidal potential of 10 mV in the frequency range of 1-105 Hz using a computer-assisted MULTI AUTOLAB M204 (Metrohm Autolab) system. The disc shaped samples of 10 mm diameter and 5mm thickness were prepared, and placed between two parallel silver electrodes. The morphological and mechanical properties of hydrogels play an integral role in the therapeutical effects of diabetic wound dressing. To optimize these properties, various tests were conducted to evaluate the effect of different concentrations of graphene oxide while maintaining a constant concentration of BSA. Four hydrogel samples were prepared with GO concentrations of 0, 0.1, 0.5, and 1.0 % (w / v) in 20% (w / v) BSA solution, as shown in part (a) of Figure 2. A mild reduction of the GO / BSA hydrogels was carried out by dipping the samples in 2 mgml-1 ascorbic acid solution at 37°C for 24 hours. The treatment changed the color of hydrogel from light brown to black, as shown in part (b) of Figure 2, indicating that the reduction was successful. To understand the effect and extent of reduction, Raman spectra were recorded for (GO / BSA)0.5 samples incubated in ascorbic acid solution for 0, 12, 24, and 36 hours as presented in, as shown in part (c) of Figure 2. All recorded spectrum exhibit two distinct peaks corresponding to D and G band, centered around 1350 cm-1 and 1580 cm-1 respectively. The presence of the D band is attributed to defects and disorder in the otherwise pristine sp2-bonded graphene structure, indicating the extent of oxidation. As the incubation period increased from 0 to 36 hours, the intensity of D band decreased, suggesting a reduction of sp3 bonds and partial restoration of graphene structure. A comparative analysis of ID / IG ratio, as shown in part (d) of Figure 2 clearly indicates that the hydrogels incubated in ascorbic acid for longer durations exhibit reduced defects, revealing the successful reduction reaction. Surface morphology and porosityAfter the validation of reduction, the morphology of all hydrogels were investigated using scanning electron microscope, as presented in part (e-h) of Figure 2. The microscopic images of hydrogel's cross-sectional area exhibited interconnected porous structure. The 3D porous structure is typical of heat-induced gelation of BSA protein. As the concentration of graphene oxide in the matrix increased, the pore size of the hydrogel decreased significantly. The statistical analysis using imageJ software showcased decrement in pore size with increment in GO concentration, as depicted in part (i-l) of Figure 2. Evidently, the average pore size decreased from 75 μm in control hydrogel to 28 μm in r(GO / BSA)1.0. The decrease in pore size is attributed to the supramolecular interaction between graphene oxide sheets and BSA hydrogel, leading to stronger crosslinking density and thus reduced pore size. Notably, increase in the pore density is a desirable property suitable for enhanced water encapsulation.Rheological propertiesA wound dressing applied on the wounded area is often subjected to variable tension as the body moves around. Therefore, an efficient wound dressing must have acceptable structural, mechanical and biological strength so that it conform to such tensions. These properties were analyzed by performing rheological studies of the prepared hydrogels. First and foremost, to find the linear viscoelastic range (LVR), amplitude test was performed for all the samples at a constant frequency of 1 rads-1. The amplitude was varied in range of 0.1 to 150% shear strain, as shown in part (a) of Figure 3. The storage modulus was found to be greater than the loss modulus in all cases, indicating the elastic nature of hydrogel. Both the storage and loss modulus were constant till 35% shear strain which depicts the LVR region that is an important parameter for the application as a wound dressing. A certain increase in storage modulus and the shift of breaking point towards higher values of shear strain with increasing GO content point towards enhanced crosslinking density of hydrogel due to incorporation of graphene oxide. Next, frequency sweep was carried out with amplitude kept fixed at 10% (within LVR region). The storage and loss modulus were plotted against angular frequency, as shown in part (b) of Figure 3. Here again, an increase in the storage modulus with increasing GO content is witnessed; control hydrogel showcasing a G' of 80 Pa, whereas r(GO / BSA)1.0 having storage modulus of 150 Pa. G' remained dominant over G" across frequency range of 0.1-20 rad s-1 which indicated that the hydrogels were stable and behaved as viscoelastic solid. Furthermore, both G' and G" were nearly constant in the entire frequency range, thereby showcasing stability over long-term storage due to stable cross-linked network. In addition, hydrogel viscosity behavior with changing shear rate was also recorded, as depicted in part (c) of Figure 3. The constant negative slope of viscosity vs shear rate plot revealed the shear thinning nature of hydrogel, which is a crucial property for fabricating extrusion-based wound dressings. The increase in viscosity with increasing GO content again confirmed hypothesis that GO was playing a pivotal role in enhancing the crosslinking density of BSA hydrogel. Compression TestA wound dressing is required to have good compressive strength, hence mechanical strength of hydrogels was recorded by conducting the compression test. All the hydrogels were cut in cylindrical shape of height 4 mm. As depicted in part (d) of Figure 3, compared to control hydrogel, the composite hydrogel showcased increased mechanical strength. The r(GO / BSA)1.0 hydrogel could sustain ~ 5x103 MPa of compressive stress upon 50% deformation compared to only ~ 103 MPa sustained by control hydrogel. The five-fold increase in compressive strength of composite hydrogel is attributed to enhanced crosslinking density and supramolecular interaction between BSA and graphene oxide. Additionally, the cyclic compression test was performed to assess the shape memory of r(GO / BSA)1.0 hydrogel. As witnessed in the part (e) of Figure 3, after first cycle of compression, the composite hydrogel exhibited only 11% decline in sustained force for 50% deformation. Only 3% decline was noticed in the subsequent cycle indicating that the prepared composite hydrogel possesses considerable shape memory. The test confirms the excellent mechanical strength of hydrogel owing to the non-covalent interaction between BSA and graphene oxide.Swelling ratio and water remaining ratioThe encapsulated water plays a crucial role in maintaining the optimum moisture levels at wound site, reducing the chances of infection and thereby escalating the wound healing process. Hence, swelling ratio of the hydrogels was calculated. As presented in part (f) of Figure 3, the swelling ratio of BSA hydrogel showcased significant enhancement with incorporation of graphene oxide. Evidently, the BSA hydrogel showcased a swelling ratio of 200% which is owed to three-dimensional cross-linked structure of BSA. r(GO / BSA)0.1 and r(GO / BSA)0.5 -demonstrated an increased swelling ratio of 300% and 400%, respectively. The enhanced water encapsulation is attributable to the highly hydrophilic nature of GO owing to the oxygen rich surface functionalities. However, further increase in GO content as witnessed in case of r(GO / BSA)1.0 witnessed a slight decrease in swelling ratio. It is inferred from the observation that the pore size plays critical role in water holding capacity of hydrogel, and decrease in pore size beyond a certain point lead to reduced swelling. Next, water remaining ratio of a hydrogel was assessed as it provides crucial information regarding proposed wound dressing. Rapid water loss lead to premature degradation of the hydrogel that impede the healing process. As demonstrated in part (g) of Figure 3, the incorporation of GO significantly enhances the water retention properties of the hydrogel. With increasing concentrations of GO, the hydrogels exhibit an improved capacity to retain water over extended periods. Conductivity testAs reported by various groups, conductivity play a significant role in wound healing process. The skin possess own conductive pathways for conveying bioelectrical signals across cell. At the wound site, these pathways get disrupted impeding the signal transmission, which probably impede or delay wound healing process. Conductive hydrogels help in forming these pathways, which potentially escalate the healing process. The electrical and ionic conductivities of composite hydrogels are tuned by varying the amount of graphene oxide incorporated inside hydrogel matrix. The electric conductivity was measured by using digital multimeter using the relation having equation 3,ρ=L / (R*a) (3)where, L, R, and a are the length, resistance and cross-sectional area of the hydrogel sample. As shown in part (h) of Figure 3, the control hydrogel showcased high resistance. Compared to control hydrogel, r(GO / BSA) hydrogels demonstrated significant increase in conductivity with increasing concentration of GO within the hydrogel. The observed increase in conductivity is attributed to several factors, the primary factor being the partial reduction of surface GO which restored some of the conjugated p-electron systems of graphene. Furthermore, graphene oxide create strong interfacial interactions with the protein matrix, potentially facilitating better charge transfer. Next, the ionic conductivity of the hydrogels was measured by applying an AC signal, the conductivity increased with increasing frequency for all samples, as depicted in the part (i) of Figure 3. The increase in graphene oxide content significantly enhanced the ionic conductivity of hydrogel. While r(GO / BSA)0.1 sample demonstrated little improvement compared to the control hydrogel, further increase in GO concentration resulted in substantially enhanced conductivity values. Specifically, the conductivity for BSA hydrogel was measured to be 2.7 Sm-1, which increased to 4.7 Sm-1 for r(GO / BSA)1.0, both measured at 1MHz frequency. The significant enhancement in conductivity is attributed to two reasons; first, reduced graphene oxide at the surface facilitates better charge transfer at the interface and second, graphene oxide is highly hydrophilic which lead to improved water encapsulation, which in turn enhances the ionic conductivity of composite hydrogels. The extensive characterization of the prepared hydrogel samples is conducted for understanding the effect of GO in BSA hydrogel. All the hydrogels exhibited similar rheological properties, and were characterized as viscoelastic materials. The viscosity of the hydrogels increased with higher GO concentrations. Compressive test results indicate that the incorporation of graphene oxide into the BSA matrix does impart greater mechanical strength to the hydrogels. It also influenced the morphology of the BSA hydrogel by making the pores more uniform and compact, thus increasing the swelling ratio. However, swelling ratio reached a saturation after 0.5% GO (w / v) and decreased beyond this concentration. The conductivity of the composite hydrogel increased with increasing GO concentration. The results favor the composite hydrogel over BSA hydrogel in terms of morphological, mechanical, and electrical properties. For wound dressing application, water retention is crucial for maintaining optimum moisture at the wound site, adsorbing wound exudates, and providing ionic conductivity. Also, it was witnessed that the conductivity of r(GO / BSA)0.5 and r(GO / BSA)1.0 are comparable. Therefore, for further biological studies, the r(GO / BSA)0.5 hydrogel, which showcased greatest water swelling was selected. All subsequent tests and studies were performed using the r(GO / BSA)0.5 hydrogel. Thus, to avoid the confusion, the subscript indicating GO concentration is dropped from here on and r(GO / BSA) is used for hydrogel containing 0.5% GO, unless mentioned otherwise. EXAMPLE 3Antibacterial activity assayThe antibacterial efficacy of the r(GO / BSA) composite hydrogel were evaluated against Gram-positive (S. aureus) and Gram-negative (E. coli) bacteria using the agar disc diffusion method and kinetic growth inhibition studies. Overnight cultures of E. coli and S. aureus were grown in Luria-Bertani (LB) medium and incubated at 37°C. These cultures were then diluted to an optical density (OD) of 0.6 (at 600 nm) and treated with various concentrations of the rGO-BSA hydrogel. As a positive control, ampicillin was used. The treated cultures were incubated at 37°C, and the optical density was measured after 24 hours using a microplate reader.For the agar disc diffusion assay, 200 μL of each bacterial culture (OD 0.6) was evenly spread onto the agar plates. Whatman filter paper discs (6 mm in diameter) were soaked in 1 mg / mL hydrogel solutions and placed on the plates. Additionally, disc soaked in ampicillin solution served as positive control. The plates were incubated at 37°C for 24 hours. The inhibition zones around the discs were measured to determine antibacterial efficacy.The antibacterial efficacy of BSA hydrogel, GO / BSA hydrogel, and r(GO / BSA) hydrogel was evaluated and compared it to the antibiotic ampicillin formulation against both gram-positive (Staphylococcus aureus) and gram-negative (Escherichia coli) bacteria. The bacterial growth in solutions having BSA, GO / BSA and r(GO / BSA) formulations was examined by measuring the optical density at 600nm and compared to control solution, as shown in part (b) of Figure 4. It was witnessed that the BSA hydrogel has negligible effect on bacterial growth, and the solution showcased OD similar to the control group. Bacterial solution exposed to r(GO / BSA) hydrogel exhibited significantly lower OD value compared to GO / BSA hydrogel. The agar disc diffusion method was used to measure the inhibition zones for different samples. BSA hydrogel (i) did not show any inhibitory behavior against either of the bacteria strain, which confirmed the lack of antibacterial properties. Sample (iii) showed the characteristic inhibition rings of ampicillin antibiotic. The inhibition zones against E. coli and S. aureus are shown in part (a) of Figure 4. The measured inhibition zones against E. coli, for ampicillin, GO / BSA, and r(GO / BSA) were 29.36 mm, 18 mm and 27.52 mm. The inhibition zones against S. aureus were measured to be 32.13 mm, 25.6 mm, and 31.95 mm respectively. It was noted that in both the bacteria cases, r(GO / BSA) performed considerably well in inhibiting bacteria growth compared to (GO / BSA) hydrogel. Moreover, it demonstrated comparable efficacy to the antibiotic ampicillin. The results from the OD test and agar disc diffusion indicate that the incorporation of GO into BSA hydrogel significantly enhances the antimicrobial properties owing to the strong anti-bacterial properties of graphene oxide. Also, the partial reduction of GO on the hydrogel surface further elevated the antibacterial efficacy of composite hydrogel. The results indicate that the prepared composite hydrogel also serve as effective antibacterial agent in the hydrogel, which potentially boost the wound healing process. EXAMPLE 4In vitro studyThe biocompatibility of BSA, GO / BSA, and r(GO-BSA) hydrogel formulations was examined using the NIH-3T3 cell line and assessed via the MTT assay. NIH-3T3 embryonic mouse fibroblast cells were seeded in 96-well plates at a density of 1x104 cells per well in 100 μL of complete medium and incubated for 24 hours. Post incubation, the cells were treated with three concentrations (5 μL / mL, 10 μL / mL, and 20 μL / mL) of each formulation for 24, 48, and 72 hours to assess the time-dependent effects of the formulation on cell viability. Following treatment, the medium was replaced with 100μL of MTT solution (0.5 mg mL-1), and the cells were incubated for an additional 4 hours at 37°C in a 5% CO2 atmosphere to allow the yellow MTT tetrazolium salt to be reduced by viable cells to purple formazan crystals. Then, the MTT solution was carefully removed and 100 μL of DMSO:MeOH (1:1) solution was added to dissolve the formazan crystals. The absorbance of the resulting-coloured solution was measured at 570 nm using a multiplate reader.The cell viability was calculated by the following equation 4: % cell viability=AS / AC *100 (4)where, AS and AC represents the absorbance of treated sample and control at 570 nm, respectively.The biocompatibility of biomedical materials is paramount for their successful application in medical treatments. The MTT colorimetric assay was employed to estimate the effect of hydrogels (specifically, BSA hydrogel, (GO / BSA) hydrogel and r(GO / BSA) hydrogel) on the viability of NIH-3T3 fibroblast cells. Cell viability was measured at multiple time points, with a focus on 72-hour mark for assessing any long-term effects of hydrogel on cell health in part (c) of Figure 4. A time-dependent decrease in cell viability was observed across all hydrogel formulations. There was an initial increase in cell viability, suggesting a favorable interaction between hydrogel and cells. However, at higher doses, cell viability decreased. After 72 hours, a reduction in cell viability by approximately 20-25% was noted. Despite the decrement, all hydrogel formulations maintained relatively high cell viability rates (74-77%) even at the highest concentration. The observed cell viability test indicates a dose-dependent response to hydrogels. Nonetheless, the cell viability levels remained above 70%, which is indicative of low toxicity and acceptable biocompatibility. The high cell viability also indicates that hydrogels do not significantly impair fibroblast mitochondrial function and is applicable in biomedical applications.EXAMPLE 5In vivo studyRat model was used to conduct the in-vivo assessment of composite hydrogel. Rats were acclimatized under standard condition with free access to commercial pellet food and water. Diabetes was induced in rats using streptozotocin (STZ) injection at a 60 mg / kg body weight dose dissolved in a 0.1 M citrate buffer (pH 4.5). To confirm the successful induction of diabetes, blood glucose levels were monitored three days post STZ injection. Blood samples were obtained via tail vein sampling. Only those rats with fasting blood glucose levels above 250 mg / dL were considered diabetic and included in study. On the 8th day post-STZ injection, a full-thickness excisional wound was created on the rats' back and disinfected with 70% ethanol. Diabetic animals were divided into three groups: (1) negative control (no treatment), (2) BSA hydrogel-treated wounds, and (3) r(GO / BSA) composite hydrogel-treated rats. Treatments were applied topically every other day until the complete wound healing was observed. Throughout the experimental period, blood glucose levels and body weight were measured regularly to monitor the health status of rats. At the experiment's conclusion, rats were fasted overnight to stabilize the metabolic rate. Subsequently, the animals were sacrificed as per the guidelines of ethics committee and wound tissues were excised for histopathological analysis. To evaluate the efficacy of prepared composite hydrogel, dressing of BSA hydrogel, and r(GO / BSA) hydrogel were applied to diabetic wound in rats. A negative control (no treatment) was also evaluated for comparison. The wound areas were measured at 0, 3, 7, 10, 16 days after wound creation. The residual wound area for three groups and corresponding change with time are summarized in part (a) of Figure 5. For the negative control (with no treatment), the wound closed gradually albeit very slowly. There was significant wound size on day 16. In the experimental groups, all groups showed good healing speed. Compared to BSA hydrogel, the wound closed much faster when treated with composite hydrogel. On day 10, the wound in composite hydrogel group were almost healed, whereas the group with BSA hydrogel treatment showed considerable wound size. By day 16, wounds were completely sealed off in composite hydrogel treated group. The speed of wound closure in all three groups is revealed in part (d) of Figure 5. It is noted that r(GO / BSA) hydrogel showed escalated wound healing compared to the control groups. Histological analysis shown in part (b) of Figure 5, revealed a fully integrated new epidermis in the hydrogel-treated groups, with the r(GO / BSA) hydrogel-treated group showing advanced healing and thicker granulation tissue. From the above wound closure results, it is noted that the BSA based hydrogel showed positive efficacy towards diabetic wound healing owing to highly porous structure and high swelling ratio of BSA. The incorporation of graphene oxide in BSA hydrogel matrix and partial reduction helped in escalating the re-epithelialization process, which resulted in considerably faster wound healing in r(GO / BSA) hydrogel-treated group. The faster healing response by composite hydrogel is attributed to the conductive nature of hydrogel, which helps in transmitting endogenic bioelectrical signals to the wound. The bioelectrical signals thereby activate the electro-stimuli responsive cells, which result in accelerated wound healing. The study indicates that protein-based conductive hydrogels is employed as dressing material for treating diabetic wounds. Therefore, the present invention reveals the preparation of composite r(GO / BSA) conductive hydrogel dressings for treating diabetic wounds. The composite hydrogel exhibits excellent mechanical strength, electrical conductivity and antibacterial properties. The conductive nature of composite hydrogel facilitates enhanced electrical simulation that accelerates the wound management. Many modifications and other embodiments of the invention set forth herein will readily occur to one skilled in the art to which the invention pertain having the benefit of the teachings presented in the foregoing descriptions and the associated drawings. Therefore, it is to be understood that the invention is not to be limited to the specific embodiments disclosed and that modifications and other embodiments are intended to be included within the scope of the appended claims. Although specific terms are employed herein, they are used in a generic and descriptive sense only and not for purposes of limitation.
Claims
1. A conductive nanocomposition for wound management comprising of: a protein; and a carbon-based nanomaterial; wherein, said protein is Bovine Serum Albumin (BSA) in a concentration range of 15% to 20% (w / v); said carbon-based nanomaterial is graphene oxide in a concentration range of 0.1 to 1% (w / v); said conductive nanocomposition is in the form of a hydrogel; and said hydrogel is reduced in the presence of a reducing agent.
2. The conductive nanocomposition as claimed in claim 1, wherein said reducing agent is ascorbic acid in a concentration range of 1.5 to 2 mg / ml.
3. The conductive nanocomposition as claimed in claim 1, wherein said hydrogel is of pore size ranging from 21 to 28 μm.
4. The conductive nanocomposition as claimed in claim 1, wherein said hydrogel exhibits storage modulus in a range of 130 to 150 Pa.
5. The conductive nanocomposition as claimed in claim 1, wherein said hydrogel sustains 4.5 to 5x103 MPa of compressive stress with 50% deformation.
6. The conductive nanocomposition as claimed in claim 1, wherein said hydrogel swells in a range of 300-400%.
7. The conductive nanocomposition as claimed in claim 1, wherein said hydrogel exhibits conductivity in a range of 4.7 to 5 Sm-1 at 1 MHz frequency.
8. The conductive nanocomposition as claimed in claim 1, wherein said hydrogel exhibits zone of inhibition in a range of 18 - 27.52 mm against E. coli and in a range of 25.6- 31.95 mm against S. aureus.
9. The conductive nanocomposition as claimed in claim 1, wherein said hydrogel exhibits cell viability in a range of 74-77% in NIH3T3 fibroblast cells.
10. The conductive nanocomposition as claimed in claim 1, wherein said hydrogel manages wound in a time span of 8 to 12 days.
11. A method of preparation of a conductive nanocomposition in the form of hydrogel comprising the steps of : a) dissolving 250 to 350 mg / ml of BSA powder in deionized (DI) water to form a solution of BSA; b) dissolving 5 to 10 mg of graphene oxide powder in 1-2 ml DI water to form a dispersion of graphene oxide (GO); c) taking 150 - 250 mg / ml of said solution BSA obtained in step (a) with said dispersion of graphene oxide obtained in step (b) in the range of 0.1 to 1% (w / v) to form a sample of GO-BSA; d) incubating said sample of GO-BSA obtained in step (c) in a preheated hot air oven at 80°C for 30 minutes followed by cooling the sample at room temperature to prepare a dried sample of GO-BSA; and e) treating said dried sample of GO-BSA obtained in step (d) with a reducing agent at a predetermined temperature of 37°C for a predefined time period of 24 hours followed by washing 3 to 5 times with DI water to form a hydrogel.
12. The method of preparation as claimed in claim 12, wherein said dispersion of graphene oxide is prepared by the steps of: i) mixing 1 - 2 g of graphite with 150 - 200 mL of concentrated sulphuric acid (H2SO4) and 1.3 - 1.6 g of sodium nitrate (NaNO3) for 15 - 20 minutes in a three-neck flask under constant magnetic stirring while maintaining temperature in a range of 3 to 5°C to form a mixture; ii) adding 4 to 6 g of potassium permanganate (KMnO4) slowly to said mixture obtained in step (i) over a period of 25 - 35 minutes under continuous stirring to form a dark green paste; iii) diluting said dark green paste obtained in step (ii) with 180 - 250 mL of deionized (DI) water followed by adding hydrogen peroxide (H2O2) dropwise to produce a dark brown mixture; iv) filtering said dark brown mixture obtained in step (iii) followed by washing with hydrogen chloride (HCl) and DI water to form a neutral mixture; v) removing KMnO4 and metal ions from said neutral mixture obtained in step (iv) through sonication and centrifugation to form a sediment; vi) subjecting said sediment obtained in step (v) to air drying for 4 to 5 hours to obtain graphite oxide powder; and vii) dispersing 10 to 15 mg of said powder of graphite oxide obtained in step (vi) in 1 to 2 mL of DI water followed by sonicating in a water bath to obtain a dispersion of graphene oxide.