AI Technical Summary
The existing methods for producing artificial aggregates from waste materials face challenges in achieving uniform water absorption, environmental sustainability, and cost-effectiveness, particularly in reducing the environmental impact of quarrying and conserving natural resources.
A method involving the crushing and sieving of construction debris, mixing with fly ash and binders like sodium hydroxide and sodium silicate, and compressing using a cut-blade mechanism to form angular-shaped aggregates, followed by optimal curing techniques such as hot water curing, to produce lightweight, high-strength aggregates with low bulk density and specific gravity.
This approach results in durable, cost-effective, and environmentally friendly artificial aggregates suitable for various construction applications, reducing the need for natural aggregates and enhancing resource efficiency while minimizing environmental impact.
Abstract
Description
TECHNICAL FIELD OF INVENTIONThe present invention is related to the field of civil engineering. Morespecifically, it relates to a method for producing artificial aggregates from wastematerials.BACKGROUND OF THE INVENTIONThe background information herein below relates to the present disclosure butis not necessarily prior art.Prior studies on artificial aggregates have looked at a variety of topics tocomprehend and maximize their qualities for a range of building uses. To create highperformance and sustainable concrete, studies have investigated a variety of rawmaterials, including industrial by-products like fly ash, slag, and recycled concrete.Scholars have investigated the impact of several activation techniques, such aspolymer-based approaches or alkali activation, on the mechanical strength, durability,and thermal characteristics of these varieties of concrete.Studies on particle size, curing conditions, and mixing ratios influence thefinal properties of artificial aggregates, claim Shahane et al. Hasan et al. state thatresearchers have evaluated the life cycle analysis and overall sustainability of usingwaste materials in aggregate manufacturing, with a focus on the environmentalconsequences of this practice. By expanding on this collection of information,scientists hope to aid in the creation of novel, environmentally friendly buildingmaterials that can lessen dependency on conventional natural aggregates.EP2013152A1 relates to a method for producing an artificial lightweightaggregate containing bottom ash, and more particularly to a method for producing anartificial lightweight aggregate containing bottom ash, the method comprises the stepsof mixing 100 parts by weight of clay and 10-100 parts by weight of bottom ash toobtain a mixture; extrusion-molding the mixture by using an extruder and cutting theextrusion-molded mixture to form a molded article; drying the molded article by usinga rotary drier; and Sintering the dried article at 1050-1150 °C for 15-45 minutes toproduce the artificial lightweight aggregate. The lightweight aggregate according tothe present invention is produced by mixing bottom ash that did not satisfy a desiredphysical property of an aggregate with clay and dust in an optimum mixture ratio, sothat the problem that there is a great deviation in water absorptions of a lightweightaggregates that are mass produced using existing fly ash was solved so as to reduce adeviation in water absorptions depending on a change in the amount of raw materialadded during mass production, thereby making it possible to produce an artificiallightweight aggregate having uniform water absorption. In addition, bottom ash thatwas difficult to dispose is disposed in a large quantity and thus the cost required forinstallation of an ash pond is reduced and the bottom ash is recycled so that theproduced artificial lightweight aggregate is economically efficient. Also, it is possibleto solve environment-related problems.OBJECTIVE OF THE INVENTIONThe primary objective of the present invention is to provide a method forproducing artificial aggregates from waste materials.Yet another objective of the invention is to evaluate the impact of variousbinders (sodium hydroxide and sodium silicate) on the physical and mechanicalproperties of the aggregates.Yet another objective of the invention is to analyze the influence of differentcuring methods (hot water curing, water curing, room temperature, and humiditycuring) on the aggregates' strength and durability.Yet another objective of the invention is to determine the optimal curingtechniques and durations to achieve the best performance in artificial angularaggregates.Yet another objective of the invention is to develop a sustainable, costeffective method for producing high-strength artificial aggregates from wastematerials, reducing environmental impact and conserving natural resources.SUMMARY OF THE INVENTIONAccordingly the following invention provides a method for producingartificial aggregates from waste materials. The method involves crushing and sievingconstruction debris, mixing it with fly ash and binders such as sodium hydroxide andsodium silicate, and compressing the mixture using a cut-blade mechanism to formangular-shaped aggregates. The aggregates are then cured using optimal methods likehot water curing or water curing.This process results in lightweight, high-strength aggregates with low bulkdensity and specific gravity. The invention offers a sustainable alternative to naturalaggregates, reducing the environmental impact of quarrying and utilizing wastematerials effectively.Additionally, incorporating glass powder enhances the strength of theaggregates. These artificial aggregates are suitable for various constructionapplications, contributing to resource efficiency and environmental preservation. Theinnovative cut-blade mechanism and optimized curing techniques ensure theproduction of durable, cost-effective construction materials.BRIEF DESCRIPTION OF DRAWING:Figure 1 of Sheet 1 illustrates the flowchart of the present invention.Figure 2 of Sheet 1 illustrates the composition of glass powder.Figure 3 (a) of Sheet 2 illustrates the loss angle abrasion value test.Figure 3 (b) of Sheet 2 illustrates the impact value test.Figure 3 (c) of Sheet 2 illustrates the specific gravity test.Figure 3 (d) of Sheet 2 illustrates the water absorption test.Figure 4 (a) of Sheet 3 illustrates the loss angle abrasion value test.Figure 4 (b) of Sheet 3 illustrates the impact value test.Figure 4 (c) of Sheet 3 illustrates the specific gravity test.Figure 4 (d) of Sheet 3 illustrates the water absorption test.Figure 5 of Sheet 4 illustrates the comparison of Natural Aggregate & artificialaggregate test results.DETAILED DESCRIPTION OF THE INVENTIONAs used in the description herein and throughout the claims that follow, themeaning of "a," "an," and "the" includes plural reference unless the contextclearly dictates otherwise. Also, as used in the description herein, the meaning of "in"includes "in" and "on" unless the context clearly dictates otherwise.The present invention relates to a method for producing artificial aggregatesfrom waste materials. An environmentally friendly alternative to conventionalbuilding materials is provided by artificial aggregates made from fly ash andconstruction demolition trash using a cut-blade mechanism. Fly ash, a by-product ofburning coal, is combined with building demolition debris, which usually consists ofbricks, concrete, and other materials, to make these aggregates.After the demolition trash has been crushed and sieved to the proper particlesizes, fly ash and a binder, such as sodium hydroxide and sodium silicate, are added tothe mixture. To create angular artificial aggregates, this mixture is then compressedand allowed to cure. There are several benefits to using fly ash and buildingdemolition trash to make artificial aggregates.First off, it lessens the need for natural aggregates, which reduces the negativeeffects of quarrying on the environment and aids in the conservation of naturalresources. It also gives two kinds of waste materials a sustainable home instead ofadding them to landfills or requiring energy-intensive disposal techniques. Artificialaggregates can also have qualities similar to those of natural aggregates, whichqualifies them for use in a variety of building applications.Moreover, by lowering the carbon footprint associated with cementmanufacturing, adding fly ash to the production process improves the aggregates'sustainability. As an additional cementitious ingredient, fly ash decreases the quantityof cement used while simultaneously enhancing the strength and longevity of theaggregates.All things considered, artificial aggregates made from fly ash and debris frombuilding demolitions present a viable option for environmentally friendly buildingmethods. These aggregates support environmental preservation and encourageresource efficiency by recycling trash and lowering dependency on natural resources.Crushing and sieving construction demolition debris to obtain particles ofdesired sizes, mixing the sieved debris with fly ash, adding a binder comprisingsodium hydroxide and sodium silicate to the mixture of fly ash and debris,compressing the mixture using a cut-blade mechanism to form angular-shapedaggregates, and curing the formed aggregates using optimal methods selected fromhot water curing, water curing, room temperature curing, and humidity curing toachieve high strength and durability.Fly ash, building demolition waste, and alkali activators are used to produceeasily, affordably, and sustainably angular-shaped, high-strength artificial aggregates.Artificial aggregates' engineering properties are greatly influenced by the curingtemperature, duration, and process. The optimal technique for creating artificialaggregate has been discovered to be hot water curing and water curing, as determinedby the unconfined compressive strength result.It is also shown that brittle failure manifests in the later stages of curing timeand plastic failure develops in the early stages of curing time when the curing durationis extended from 28 days to 60 days. The room temperature and humidity curingtechniques resulted in a much smaller improvement in the properties of the artificialaggregates compared to the hot water curing strategy.However, when it comes to quick curing methods, hot water curing and watercuring can be better options. Artificial green coarse aggregate, which is utilized in allkinds of building activities, has an average particle size of 10 to 20 mm aftermanufacture. It has been found that artificial angular coarse aggregate has a low bulkdensity and specific gravity, indicating that it is porous and lightweight.Class C Fly-ashThe tested percentage of fly ash is shown in Figure 1. Generally, as per theprevious study, there is no need for alkali activators when using class C fly ash.However, for making artificial coarse aggregate, sodium hydroxide, and sodiumsilicate should be used to obtain early strength.Table 1 shows the tested chemical composition of class C fly ash:Construction demolition debrisThe building dismantling industry significantly contributes to global wastegeneration, with dismantled building materials waste estimated to constitute asubstantial portion of total waste in many countries. However, it also offers anopportunity for resource recovery and recycling. Many components of dismantledbuilding materials waste can be effectively recycled and reused.Table 2 shows the properties of construction demolition debris:Glass powderThe glass powder is collected from construction demolition waste. For theresearch work, three types of glass are collected: clear glass, colored glass & stitchingglass. The tested compound obtained from all three glasses should be nearly the same.In this research, artificial aggregates were developed from waste materialssuch as GBFS, bentonite, glass powder, and construction demolition debris. Thecomposition and properties of these materials were analyzed. A mix design for theartificial aggregate was then formulated using a trial-and-error approach, guided by IScodes. Various trial mixes were prepared. If the first trial met all strength criteria, nofurther trials were necessary.However, if the strength criteria, when compared to natural aggregate, werenot met, subsequent trials were conducted. The mixes were prepared using a concretemixer drum. Unlike previous studies that used the palletization method, whichproduces rounded aggregates with poor interlocking properties, this method involvedmodifications to the concrete mixer drum to produce angular aggregates. Afterproduction, tests such as the abrasion test, impact test, water absorption test, andspecific gravity test were conducted on the aggregates.Experimental DataTrial Mix-1Trial Mix-2Trial Mix-3The abrasion value for natural coarse aggregates is found to be 8.35%, whilethe abrasion value for artificial green aggregates from trial mix-1 with different foursamples is found to be 20.6 %, 28.18 % 16.6 % & 13.2 % respectively. The impactvalue for natural coarse aggregates is found to be 7.3 %, while the impact value forartificial green aggregates from trial mix-1 with different four samples is found to be14 %, 22 %, 11.5 % & 9.6 % respectively.The water absorption value for natural coarse aggregates is found out to be1.86 %, while the water absorption value for artificial green aggregates from trialmix-1 with different four samples is found out to be 7%, 6.4%, 1.96% & 4.2%respectively. The specific gravity for natural coarse aggregates is found to be 2.81 %,while the specific gravity for artificial green aggregates from trial mix-1 with differentfour samples is found to be 1.9, 2.1, 2.6 & 2.7 respectively.The abrasion value for trial mix-2 with different three combinations is foundto be 15.4%, 20.64% & 9.6% respectively. The impact value for trial mix-2 withdifferent three combinations is found to be 10.5 %, 18.2% & 8.1% respectively. Thewater absorption for trial mix-2 with different three combinations is found to be 5.6%,3.8% & 2.2 % respectively. The specific gravity for trial mix-2 with different threecombinations is found to be 2.4, 2.61 & 2.76 respectively.The abrasion value for trial mix-3 with different three combinations is foundto be 9.4%, 7.9% & 9% respectively. The impact value for trial mix-3 with differentthree combinations is found out to be 8%, 6.8% & 7.6% respectively. The waterabsorption for trial mix-3 with different three combinations is found out to be 2.2%,1.98% & 2.1% respectively.The specific gravity for trial mix-3 with different three combinations is foundout to be 2.75, 2.2 & 2.5 respectively. The average particle size in the coarseaggregate is represented by an index value in the fineness modulus of coarseaggregates. Sieve analysis is used to ascertain it using standard sieves. The finenessmodule of artificial green aggregate is found to be 7.4.Construction demolition debris is first crushed and sieved to obtain particles ofthe desired size. A mixture is then prepared by combining 70% of the sieved debriswith 20% fly ash, 20% glass powder, and 6% cement. A binder, composed of 2%sodium hydroxide and 2% sodium silicate, is added to the mixture of fly ash anddebris. The resulting mixture is compressed using a cut-blade mechanism to formangular-shaped aggregates. These aggregates are cured for 28 days using hot watercuring, enhancing their strength and durability.It has proven to be quite difficult to acquire appropriate rocks for buildingprojects like cement roads in the changing geography of Asia, especially in India. Asa result, natural aggregates are in low supply. Because of this, the construction sectoris experiencing an increase in demand for artificial coarse aggregates. Studying howto make these artificial aggregates stronger and more stable will help close asignificant knowledge gap.It has also been observed that most studies that have studied round artificialaggregates employing the palletisation process have neglected to optimize sodiumhydroxide, sodium silicate, and other parameters required for the creation of artificialaggregates. Some disadvantages of this strategy are that it requires more monitoring,more equipment, uses more energy, and is not repeatable. Its round form also reducesthe interlocking effect.A novel technique for creating angular artificial aggregates utilizing a cutblade mechanism is suggested to overcome these restrictions. The goal of thisinvention is to create artificial aggregate from all waste resources, including alkaliactivators, fly ash, and leftover concrete from demolished structures.While various embodiments of the present disclosure have been illustrated anddescribed herein, it will be clear that the disclosure is not limited to theseembodiments only. Numerous modifications, changes, variations, substitutions, andequivalents will be apparent to those skilled in the art, without departing from thespirit and scope of the disclosure, as described in the claims.
Claims
1. A method for producing artificial aggregates from waste materials, consisting of following steps; a) Crushing and sieving construction demolition debris to obtain particles of a desired size; b) Mixing 70 % of the sieved demolition debris with 20 % of fly ash, 20 % of glass powder, and 6 % of cement; c) Adding a binder composed of 2 % of sodium hydroxide and 2 % of sodium silicate to the mixture of fly ash and demolition debris; d) Compressing the resulting mixture using a cut-blade mechanism to form angular-shaped aggregates; and e) Curing the formed aggregates for 28 days using hot water curing to achieve high strength and durability.