Fluoride-free hydrothermal synthesis of ti-CHA zeolite via interzeolitic conversion of titanated zeolite
Patent Information
- Application Number
- IN202511097503
- Authority / Receiving Office
- IN · IN
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2025-10-09
- Publication Date
- 2026-10-23
- Estimated Expiration
- 2045-10-09
AI Technical Summary
Existing methods for synthesizing Ti-CHA zeolites rely on hazardous chemicals like HF, limiting thermal stability, scalability, and environmental sustainability, and introduce metal nanoparticles into the framework, affecting performance.
A fluoride-free hydrothermal synthetic protocol using interzeolitic conversion of TS-1 zeolite with organic precursors, enhancing structural properties and thermal stability, and achieving uniform particle size distribution.
The protocol produces Ti-SSZ-13 zeolites with high thermal stability, uniform particle size, and improved catalytic efficiency, suitable for high-temperature reactions with extended catalyst lifetime.
Abstract
Description
TECHNICAL FIELD OF THE INVENTIONThe present invention relates to zeolites and a process for their preparation, moreparticularly, to fluoride-free titanium-substituted chabazite (Ti-CHA) zeolite andthe process for its fluoride-free hydrothermal synthesis via interzeolitic conversionof titanated zeolite (TS-1).BACKGROUND OF THE INVENTIONZeolites are inorganic crystalline porous materials that have been extensively usedas molecular sieves in the past few decades. Their applications include petroleumrefining (Fluidised catalytic cracking, hydrocracking, isomerisation),environmental pollutants removal (NOx conversion), wastewater treatment (watersoftening, removal of phosphates), gas adsorbents, agriculture (soil conditioners),biotechnology and medicine and many more. Being responsible for more than 30%of worldwide gasoline production, they have been the soul of numerous refineryoperations. Owing to a plethora of industrial applications, the global consumptionof zeolite amounts to ca. 250000 metric tons per year. The wide industrial usage ofthese catalysts is due to their high hydrothermal stability, acid strength and flexiblemolecular structure, which allows high product selectivity for specific applications.Zeolites typically consist of TO4 octahedra, where T denotes Si4+, Al3+ or any othertetravalent or trivalent cation, with a suitable size, which can be easily mould intothe tetrahedral coordination in the zeolite framework. This flexibility in structureallows for tuning of properties via heteroatom doping or isomorphous substitutionof various zeolite frameworks for specific applications. The research centred onisomorphous substitution of zeolite frameworks exploded when Ti was successfullyincorporated into the MFI framework, leading to the discovery of TitaniumSilicalite-1 (TS-1) zeolite. Following this, excluding Al3+ , a plethora of T-atomshave been explored for different zeolite frameworks, including but not limited toB3+, Fe3+, Ga3+, Ti4+, Ge4+, Sn4+, Zr4+, Hf4+ and Mo6+. Among these metals, Tisubstitution has garnered significant attention owing to its high selectivity forhigher hydrocarbons in selective oxidation reactions using H2O2 as an oxidant. Thevariability of Ti incorporation ranges from chabazite framework for photocatalyticapplications to MWW and BEA zeolites for olefin epoxidation reactions.Among various zeolites, SSZ-13 with Chabazite (CHA) framework has beenextensively investigated due to its myriad of applications, including but not limitedto selective catalytic reduction (SCR) of NOx, Methanol to hydrocarbon (MTH),and amination (e.g., methylamines). The SSZ-13 zeolite framework typicallyconsists of 4-membered, 6-membered and 8-membered rings (MR) with narrowpore openings of about 3.8 A x3.8 A, a large ellipsoidal cavity size of 6.7 A x10 A,and a framework density of 15.1T / 1000 A3. The synthesis of SSZ 13 was firstreported by Zones in 1985 with the help of N,N,N-trimethyl-1-adamantylammonium hydroxide (TMAdaOH) as an organic structure directingagent (OSDA) using hydrothermal synthesis protocol. Since then, SSZ-13 has beendirectly synthesized using numerous OSDA and indirectly synthesized usinginterzeolitic transformation methods.Owing to its narrow pore opening, it has been investigated for CO2 separation fromflue gas, natural gas and biogas. However, Al-containing SSZ-13 zeolites have atendency to absorb water from humid gases, resulting in dealumination of zeoliteframeworks, which leads to the collapse of the structure. Consequently, the collapseof the zeolite structure leads to a decline in catalytic performance and shorterlifetime of the catalyst. Therefore, several attempts have been made to increase thehydrophobicity of SSZ-13 zeolites by reducing Al content in the zeolite byisomorphous substitution of T-atoms in the zeolite framework. Previousinvestigations indicate a significant increase in lifetime of SSZ-13 zeolites for CO2separation upon incorporation of Ti in the framework. This directed the researchersto discover new and economically viable methods for the synthesis of Ti-SSZ-13with high Ti content.Previously, Ti-CHA (Ti-SSZ-13) was synthesized using long hydrothermaltreatment methods, interzeolitic transformation methods or by post-synthetic Tiincorporation into the CHA framework. In most synthetic protocols, TMAdaOHhas been used as OSDA while hydrofluoric (HF) acid has been used as mineralisingagent and structure directing agent. However, the use of HF in any industrialprocess is not encouraged due to its hazardous and carcinogenic nature. This callsfor the development of a fluoride-free synthetic protocol that results in Ti-SSZ-13with high structural stability.Moreover, the synthesis of Ti-SSZ-13 using direct hydrothermal methods is highlytime consuming with a complex mechanism. This challenge can be effectivelyaddressed by using indirect synthetic protocols such as interzeolitic conversion,wherein a parent zeolite framework can be converted into the desired daughterzeolite framework. Interzeolitic transformation also results in daughter zeolites withenhanced structural properties and simpler formation mechanisms. Severalinterzeolitic transformations have been attempted in the past to synthesize variouszeolite frameworks including CHA framework. This strategy can be easilyexpanded for the synthesis of isomorphously substituted zeolite as well.The existing literature highlights the direct hydrothermal synthesis of Ti-SSZ-13using fluoride ion as SDA and mineralising agent. The previous synthesis methodsinclude TMAdaOH as OSDA, HF as mineralising agent, Al2O3 as aluminum sourceand a suitable organic precursor of silica and titanium followed by the hydrothermaltreatment at high temperature for a few days. In further investigations, TiO2 wasused as a Ti source instead of an organic Ti precursor to increase the Tiincorporation into the CHA framework. In a couple of studies, the secondarygrowth method was employed for synthesis via seed crystals of Ti-CHA zeolite.The secondary growth method was used to construct a Ti-CHA membrane forCO2 / CH4 separation studies on porous alumina support. The growth of Ti-CHAmembrane was investigated as a function of the size of seed crystals and the amountof seed in the precursor solution. Another study indicates the indirect synthesis ofTi-SSZ-13 via post synthetic treatment of the SSZ-13 crystals. The Ti atoms wereisomorphously substituted in the CHA framework via ion exchange treatment ofthe as synthesized CHA zeolite. Another route to indirect synthesis of Ti-SSZ-13was taken through interzeolitic conversion of Ti-Faujasite zeolite (FAU) frameworkto Ti-CHA framework. The interzeolitic conversion of low-density FAUframework into high density CHA framework is thermodynamically feasible andresults in shorter synthesis time.Moreover, in the existing literature, Ti-SSZ-13, synthesized using HF, was foundto exhibit thermal stability limited to 1000°C.Therefore, all the existing direct or indirect processes involve the usage of fluorideion in the form of HF or other fluoride precursors (example: (NH4)2TiF6) for theproduction of smooth Ti-SSZ-13 crystals with limited or poor thermal stability. Insummary, while numerous methods have been developed for synthesizing Ti-CHAzeolites, the common reliance on hazardous chemicals such as HF and the use ofion-exchange processes that introduce metal nanoparticles into the frameworkremain significant drawbacks. These issues limit the thermal stability, scalability,environmental sustainability, and performance of the zeolites, underscoring theneed for new, more efficient, and environmentally friendly approaches to thesynthesis of Ti-CHA zeolites for industrial applications.Therefore, despite these developments, there is a need for fluoride-free Ti-CHAzeolite and its synthesis that overcomes one or more of the technical problems asset forth above.OBJECTIVES OF THE INVENTIONAn objective of the present invention is to provide a fluoride-free Ti-CHA(Titanium-Chabazite) zeolite.Another objective of the present invention is to provide a process for synthesizingfluoride-free Titanium-Chabazite (Ti-CHA) zeolite.Yet another objective of the present invention is to provide an economically viableand scalable solution to the synthesis of Ti-CHA zeolite particles, which can beemployed for various catalytic applications, including gas and liquid phasereactions.Another objective of the present invention is to provide a fluoride-freehydrothermal synthetic protocol which allows one to produce Ti-SSZ-13 crystalsusing organic precursors, additionally, enhancing the structural properties of thematerial.Still, another objective of the present invention is to carry out indirect synthesis ofhighly crystalline Ti-SSZ-13 zeolite by facilitating interzeolitic transformation ofTS-1 zeolite (density= 17.9 T atom / 1000 A3), which is a relatively high-densityframework as compared to Ti-SSZ-13 (density= 15.1 T atom / 1000 A3).Another objective of the present invention is to provide synthesis of Ti-SSZ-13without any form of fluoride ion.Yet another objective of the present invention is the formation of Ti-SSZ-13particles with uniform particle size, which aids in improving the catalytic efficiencyStill, another objective of the present invention is to synthesize Ti-SSZ-13 with highthermal stability, which can be conveniently used for high temperature reactionswith delayed deactivation time.Still, another objective of the present invention is to synthesize stacked plateletsspheroidal particles of Ti-SSZ-13 zeolites.SUMMARY OF THE INVENTIONAn aspect of the present invention relates to a fluoride-free titanium-chabazite (TiCHA) zeolite characterized by a CHA framework having an X-ray diffractioncharacteristic peak at 2θ is 9.5°, 14.0°, 16.1°, 17.8°, 20.7, having titanium atoms attetrahedral framework positions in an amount of at least 10% of the total titaniumcontent, a tetrahedral to octahedral titanium ratio in the range of 0.15 to 4.79, a Si / Timolar ratio in the range of 37 to 83, a Si / Al molar ratio in the range of 11 to 15, anda particle size distribution or a crystal size in the range of 1.2 μm to 8.0 μm.Another aspect of the present invention relates to a process for synthesizingfluoride-free titanium-chabazite (Ti-CHA) zeolite. The process comprisingpreparing a titanium silicalite-1 (TS-1) precursor mixture comprising a siliconsource, a titanium source, water, and an organic structure directing agent (OSDA),aging the TS-1 precursor mixture at room temperature, subjecting the aged TS-1precursor mixture to hydrothermal treatment to obtain TS-1 zeolite having a MobilFive (MFI) framework, calcining the TS-1 zeolite to remove the organic structuredirecting agent (OSDA) and moisture, preparing a Ti-CHA precursor reactionmixture by combining the calcined TS-1 zeolite with an aluminum source, anorganic structure directing agent (OSDA), and an alkaline source, aging the TiCHA precursor reaction mixture at room temperature; and subjecting the aged TiCHA precursor reaction mixture to hydrothermal interzeolitic conversion to obtaintitanium-substituted chabazite (Ti-CHA) zeolite.These and other features, aspects, and advantages of the present subject matter willbecome better understood with reference to the following description. Thissummary is provided to introduce a selection of concepts in a simplified form. Thissummary is not intended to identify key features or essential features of the claimedsubject matter, nor is intended to be used to limit the scope of the claimed subjectmatter.BRIEF DESCRIPTION OF ACCOMPANYING DRAWINGSThe above and other features, aspects, and advantages of the subject matter will bebetter understood with regard to the following description and accompanyingdrawings, where:Figure 1A illustrates the field emission scanning electron microscopy (FESEM)image of TS-1 zeolite (named as TS-1_A) synthesized using tetrabutyl orthotitanate(TBOT) as the titanium source, showing ellipsoidal morphology with an averageparticle size of about 320 nm.Figure 1B illustrates the FESEM image of TS-1 zeolite (named as TS-1_B)synthesized using titanium tetraisopropoxide (TTIP) as the titanium source,showing ellipsoidal morphology with an average particle size of about 270 nm.Figure 1C illustrates the X-ray diffraction (XRD) patterns of TS-1_A and TS-1_Bsamples, confirming the formation of the MFI framework by comparison with thereference pattern from the IZA (International Zeolite Association) database.Figure 1D illustrates the N2 adsorption-desorption isotherms of TS-1_A and TS1_B, confirming the microporous characteristics of the synthesized zeolite.Figure 2 illustrates the X-ray diffraction (XRD) patterns of Ti-CHA zeolites (TiCHA_A, Ti-CHA_B, Ti-CHA_AA and Ti-CHA_BB) obtained by interzeolitictransformation of TS-1 (TS-1_A and TS-1_B), confirming the complete phaseconversion to CHA framework. The peak at 6.5° indicates the presence of a layeredtitanate phase.Figure 3A illustrates the FESEM micrograph of Ti-CHA_A synthesized from TS1_A, showing a bimodal particle size distribution.Figure 3B illustrates the FESEM micrograph of Ti-CHA_B synthesized from TS1_B, showing a bimodal particle size distribution.Figure 3C illustrates the FESEM micrograph of Ti-CHA_AA obtained by addingan additional TBOT solution to the growth solution, showing uniform cuboidalmorphology with particle size ~2.75 μm.Figure 3D illustrates the FESEM micrograph of Ti-CHA_BB obtained by addingan additional TTIP solution to the growth solution, showing uniform cuboidalmorphology with particle size ~4.97 μm.Figure 4 illustrates the X-ray photoelectron spectra (XPS) of Ti-CHA zeolites (TiCHA_A, Ti-CHA_B, Ti-CHA_AA and Ti-CHA_BB), confirming Ti incorporationin the CHA framework and distinguishing tetrahedral and octahedral Ti species fordifferent synthesis protocols.Figure 5A illustrates the XRD patterns of Ti-SSZ-13 zeolite (a type of Ti-CHA)calcined at various temperatures, showing high structural stability up to 1100°C,which shows higher thermal stability than the current reported state of the art.Figure 5B illustrates the XRD patterns of Al-SSZ-13 zeolite calcined at 550°C and1100°C, showing framework collapse at high temperature.Figure 5C illustrates the XRD patterns of Ti-CHA zeolite synthesized in thepresence of fluoride media.DETAILED DESCRIPTIONThe following description, with reference to the accompanying drawings, isprovided to facilitate an understanding of various embodiments of the presentinvention. It is to be understood, however, that the invention is not limited to thespecific embodiments described herein, which may be varied in form and detailwithout departing from the scope or spirit of the disclosure. The terminology usedherein is intended solely for the purpose of description and should not be regardedas limiting. Unless otherwise indicated, the singular forms "a," "an," and "the" shallbe understood to include plural referents. Similarly, the term "comprising," and itsgrammatical variations, shall be interpreted to mean "including but not limited to,"and does not exclude the presence of additional elements or steps. All technical andscientific terms used in this invention have the same meaning as commonlyunderstood by one of ordinary skill in the relevant art. The individual embodimentsdescribed and illustrated herein may include features that are combinable withfeatures from other embodiments, and such combinations are also intended to bewithin the scope of the present invention. Those skilled in the art will recognize thatmodifications, substitutions, and variations may be made to the compounds,compositions, and methods described without departing from the broader inventiveconcepts. It is intended that such variations and equivalents are encompassed withinthe scope of the present invention.In the present invention, titanium source 1 refers to tetrabutyl orthotitanate (TBOT),while titanium source 2 refers to titanium tetraisopropoxide (TTIP). Protocol 1refers to the process where calcined TS-1 is directly converted into Ti-CHA, givingproducts Ti-CHA_A (from TBOT) and Ti-CHA_B (from TTIP). Protocol 2 refersto the process where an additional titanium precursor is introduced during theconversion step, giving products Ti-CHA_AA (from TBOT) and Ti-CHA_BB(from TTIP).Conventionally, Ti-CHA was synthesized using long hydrothermal treatmentmethods, interzeolitic transformation methods or by post-synthetic Ti incorporationinto the CHA framework. In most synthetic protocols, TMAdaOH has been used asOSDA while hydrofluoric (HF) acid has been used as mineralising agent andstructure directing agent. However, the use of HF in any industrial process is notencouraged due to its hazardous and carcinogenic nature. This calls for thedevelopment of a fluoride-free synthetic protocol that results in Ti-SSZ-13 withhigh structural stability.In an aspect, the present invention relates to a fluoride-free titanium-chabazite (TiCHA) zeolite characterized by:a) a CHA framework having an X-ray diffraction characteristic peak at2θ is 9.5°, 14.0°, 16.1°, 17.8°, 20.7.b) having titanium atoms at tetrahedral framework positions in anamount of at least 10% of the total titanium content;c) a tetrahedral to octahedral titanium ratio in the range of 0.15 to 4.79;d) a Si / Ti molar ratio in the range of 37 to 83;e) a Si / Al molar ratio in the range of 11 to 15; andf) a particle size distribution or a crystal size in the range of 1.2 μm to8.0 μm.In an embodiment, titanium-chabazite (Ti-CHA) zeolite is Ti-SSZ-13 zeolite.In an embodiment, the amount of titanium in the tetrahedral position is 77.51%. Inanother embodiment, the amount of titanium in the tetrahedral position is 82.73%.In yet another embodiment, the amount of titanium in the tetrahedral position is35.85%. In still another embodiment, the amount of titanium in the tetrahedralposition is 13.08%. In an embodiment, the rest of the amount of titanium is in theoctahedral position.In an embodiment, the tetrahedral to octahedral titanium ratio is 0.15. In anotherembodiment, the tetrahedral to octahedral titanium ratio is 0.56. In yet anotherembodiment, the tetrahedral to octahedral titanium ratio is 3.45. In still anotherembodiment, the tetrahedral to octahedral titanium ratio is 4.79.In an embodiment, the silicon to titanium (Si / Ti) ratio is 37.42. In anotherembodiment, the silicon to titanium (Si / Ti) ratio is 39.95. In yet anotherembodiment, the silicon to titanium (Si / Ti) ratio is 82.56. In still anotherembodiment, the silicon to titanium (Si / Ti) ratio is 55.46.In an embodiment, the silicon to aluminium (Si / Ai) ratio is 11.73. In anotherembodiment, the silicon to aluminium (Si / Ai) ratio is 12.17. In yet anotherembodiment, the silicon to aluminium (Si / Ai) ratio is 13.20. In still anotherembodiment, the silicon to aluminium (Si / Ai) ratio is 14.50.The Ti-SSZ-13 zeolite is used for multifarious heterogeneous catalytic applications,including:Shape selective oxidation catalysis. For example, oxidation of methanol to methylformate can be effectively carried out using tuneable Ti-CHA. The tuneable poresize of Ti-CHA facilitates high product selectivity and higher conversion due tosynergistic effect of Ti-O-Si bonds.Selective Catalytic Reduction (SCR) of NOx. The current technology iseffectively utilized to reduce NOx emissions from the exhaust gas pipes ofautomobiles. The high thermal stability of these catalysts can enable better NOxreduction and increase the lifetime of the catalyst. Moreover, it will aid in reducingthe pollutant concentration in the earth's atmosphere.Flue gas treatment. The Ti-SSZ-13 is used for the separation of CO2 / CH4 presentin the flue gases from various industries. The increased hydrophobicity due to thehigh introduction of Ti atoms in the CHA framework delays the catalyst decay, thusincreasing the overall lifetime of catalyst. This facilitates air purification andreduces the risks posed by flue gases to the environment.In another aspect, the present invention focuses on the development of a fluoridefree synthetic protocol for the construction of Ti-SSZ-13 (CHA framework) fromTS-1 zeolite via interzeolitic transformation. The synthetic protocol was furthertweaked to obtain uniform size distribution of zeolite particles. This results in anovel experimental procedure that can be conveniently scaled up at industrial levelfor the synthesis of Ti-SSZ-13 zeolite for various catalytic applications.The present invention offers an economically viable and scalable solution to thesynthesis of Ti-CHA zeolite particles, which can be employed for various catalyticapplications, including gas and liquid phase reactions. The present inventionprovides a fluoride-free hydrothermal synthetic protocol or process which allowsone to produce Ti-SSZ-13 crystals using organic precursors, additionally enhancingthe structural properties of the material. The invention includes the indirectsynthesis of highly crystalline Ti-SSZ-13 zeolite by facilitating interzeolitictransformation of TS-1 zeolite (density= 17.9 T atom / 1000 A3), which is a relativelyhigh-density framework as compared to Ti-SSZ-13 (density= 15.1 T atom / 1000A3). The present invention involves the formation of Ti-SSZ-13 particles with auniform particle size, which aids in improving the catalytic efficiency of thematerial. The catalyst synthesized in the present invention displays high thermalstability, which can be conveniently used for high-temperature reactions with adelayed deactivation time. The process provides highly crystalline Ti-CHA (TiSSZ-13) with uniform particle size distribution, high titanium incorporation, andsuperior thermal stability.The process for synthesizing fluoride-free titanium-chabazite (Ti-CHA) zeolitecomprising:a. preparing a titanium silicalite-1 (TS-1) precursor mixturecomprising a silicon source, a titanium source, water, and anorganic structure directing agent (OSDA);b. aging the TS-1 precursor mixture at room temperature;c. subjecting the aged TS-1 precursor mixture to hydrothermaltreatment to obtain TS-1 zeolite having a Mobil Five (MFI)framework;d. calcining the TS-1 zeolite to remove the organic structuredirecting agent (OSDA) and moisture;e. preparing a Ti-CHA precursor reaction mixture bycombining the calcined TS-1 zeolite with an aluminumsource, an organic structure directing agent (OSDA), and analkaline source;f. aging the Ti-CHA precursor reaction mixture at roomtemperature; andg. subjecting the aged Ti-CHA precursor reaction mixture tohydrothermal interzeolitic conversion to obtain titaniumsubstituted chabazite (Ti-CHA) zeolite.The process is detailed as follows:Step a): Preparing a titanium silicalite-1 (TS-1) precursor mixture comprising asilicon source, a titanium source, water, and an organic structure directing agent(OSDA).In an embodiment, the silicon source is selected from tetraethyl orthosilicate(TEOS), fumed silica (FS), or silica gel (SG), and the titanium source is selectedfrom tetrabutyl orthotitanate (TBOT), titanium tetraisopropoxide (TTIP), titaniumdioxide, or titanium tetrachloride. In an embodiment, the OSDA istetrapropylammonium hydroxide (TPAOH).In an embodiment, the silicon source is tetraethyl orthosilicate (TEOS), and thetitanium source is tetrabutyl orthotitanate (TBOT), in the presence oftetrapropylammonium hydroxide (TPAOH) as OSDA. In this case, the productobtained after hydrothermal treatment is designated TS-1_A.In another embodiment, the silicon source is tetraethyl orthosilicate (TEOS), andthe titanium source is titanium tetraisopropoxide (TTIP), with TPAOH as OSDA.In this case, the product obtained is designated TS-1_B.In further embodiments, the titanium source is titanium dioxide or titaniumtetrachloride, resulting in corresponding TS-1 variants.In a preferred embodiment, the TS-1_A precursor mixture has a molar compositionof 1SiO2: 0.025TiO2: 0.2TPAOH: 14H2O.In an embodiment, Step a) ensures the controlled incorporation of titanium into theMFI framework, which is the required precursor for subsequent interzeoliticconversion.The FESEM images of the synthesized TS-1 zeolites are shown in Figures 1A and1B, corresponding to TBOT and TTIP as titanium sources, respectively. The XRDpattern confirming the MFI framework of TS-1 is illustrated in Figure 1C, and themicroporous characteristics are shown by the adsorption-desorption isotherms inFigure 1D.Step: b) Aging the TS-1 precursor mixture at room temperature.In an embodiment, the aging is carried out for 8 to 24 hours at room temperatureprior to hydrothermal synthesis. In a preferred embodiment, the TS-1_A and TS1_B precursor mixtures are aged for 12 hours before hydrothermal treatment.Step b promotes gel reorganization and ensures uniform nucleation duringhydrothermal synthesis, which directly impacts crystal size and morphology.Step c) Subjecting the aged TS-1 precursor mixture to hydrothermal treatment toobtain TS-1 zeolite having a Mobil Five (MFI) framework.In one embodiment, the hydrothermal treatment is carried out at 150 to 200°C for12 to 48 hours. In a preferred embodiment, the precursor mixtures for TS-1_A andTS-1_B are treated at 170°C for 24 hours to yield crystalline MFI frameworkzeolites. In a specific embodiment, the hydrothermal treatment is carried out in a100 ml Teflon-lined stainless-steel autoclave.Step c transforms the precursor mixture into crystalline TS-1 zeolite with MFIframework, which serves as the essential parent structure for CHA conversion.Step d) Calcining the TS-1 zeolite to remove the organic structure directing agent(OSDA) and moisture.In an embodiment, the calcination of the TS-1 zeolite is performed at a temperaturefrom 500°C to 600°C for 4 to 8 hours. In a preferred embodiment, TS-1 zeolite iscalcined at 550°C for 6 hours at a heating rate of 0.0167 K / s.Step d eliminates organic residues and water, yielding an activated TS-1 zeoliteframework that can undergo interzeolitic conversion efficiently.Step e) Preparing a Ti-CHA precursor reaction mixture by combining the calcinedTS-1 zeolite with an aluminum source, an organic structure directing agent(OSDA), and an alkaline source.In an embodiment, the aluminum source is aluminum hydroxide. In an embodiment,the alkaline source is sodium hydroxide. In an embodiment, the OSDA is N, N, Ntrimethyl-1-adamantylammonium hydroxide (TMAdaOH). In an embodiment, theprecursor mixture prepared using calcined TS-1_A yielded Ti-CHA_A, while themixture prepared using calcined TS-1_B yielded Ti-CHA_B.In a specific embodiment, the precursor mixture for synthesized Ti-CHA has thefollowing molar composition ranges:Table1: Molar composition of synthesized TCHA_A and TCHA_B mentioned inExample 3.Step e) provides the chemical environment necessary for CHA frameworkformation, introducing aluminum for framework balance and TMAdaOH as thestructure directing agent.Step f) Aging the Ti-CHA precursor reaction mixture at room temperature.In an embodiment, the aging of the Ti-CHA precursor reaction mixture is carriedout for about 4 hours at room temperature. In a preferred embodiment, the precursormixtures for Ti-CHA_A and Ti-CHA_B are aged for 4 hours. In an embodiment,the hydrothermal interzeolitic conversion is carried out at 150 to 200°C for 4 to 7days.Step f ensures homogeneous mixing and nucleation prior to hydrothermalconversion, which improves particle size uniformity.Step g) Subjecting the aged Ti-CHA precursor reaction mixture to hydrothermalinterzeolitic conversion to obtain Ti-CHA zeolite.In one embodiment, the hydrothermal interzeolitic conversion is carried out at 150to 200°C for a period of 4 to 7 days. In a specific embodiment, Ti-CHA_A and TiCHA_B were synthesized by hydrothermal treatment at 170°C for 4-7 days.Step g converts the MFI framework into CHA framework, yielding Ti-CHAzeolites with tunable morphology and enhanced titanium incorporation. This stepalso determines thermal stability and catalytic efficiency.In another embodiment, additional titanium precursors (TBOT or TTIP) wereintroduced into the mother liquor, leading to the formation of Ti-CHA_AA and TiCHA_BB, respectively, which exhibited modified morphology and higheroctahedral Ti content.The phase conversion from MFI to CHA framework is confirmed by the XRDpatterns in Figure 2. The morphology of Ti-CHA_A, Ti-CHA_B, Ti-CHA_AA, andTi-CHA_BB is shown in Figures 3A-3D. The framework incorporation of titaniumis confirmed by XPS data in Figure 4, while the enhanced thermal stability of TiCHA compared to Al-SSZ-13 is demonstrated in Figures 5A and 5B.In one embodiment, the Ti-CHA zeolite synthesized by this process is Ti-SSZ-13.EXAMPLESThe following examples are given by way of illustration of the present disclosureand should not be construed to limit the scope of the present disclosure. It is to beunderstood that both the foregoing general description and the following detaileddescription are exemplary and explanatory only and are intended to provide furtherexplanation of the subject matter.Example 1: Synthesis of TS-1_A zeolite using various Silicon sources inaccordance with the present inventionAn aqueous solution containing 19.38 ml of Deionized water (Type -I, 18.2 MOcm-1, MilliQ) and 12.70 g of tetrapropylammonium hydroxide) TPAOH was mixedwith 1.065 g of tetratbutyl orthotitanate (TBOT). The solution was then stirred atroom temperature for sufficient time to allow complete dissolution of allingredients, followed by dropwise addition of 26.04 g TEOS (Tetraethylorthosilicate). The newly formed solution was kept under stirring conditions foraging for 12 h at room temperature. The resultant solution, termed as 'motherliquor' has the molar composition 1SiO2:0.025TiO2:0. 2TPAOH:14H2O. After theaging process, the mother liquor was transferred to a 100 ml Teflon liner placedinside the stainless-steel acid digestion vessel / autoclave. The autoclave was heatedat 170°C for at least 1 day. Then, the autoclave was quenched to room temperaturein cold water. The solid product was washed with DI water using centrifugation,followed by drying at 80°C overnight. The final solid sample was analyzed usingthe powder X-ray diffraction method depicted in Figure 1C (red curve). Thediffractogram illustrates the formation of the pure TS-1 (MFI framework) phase(compared with the reference pattern of MFI taken from the IZA website). Scanningelectron microscopy (SEM) was used to visualize the morphology of the formedparticle, which revealed the formation of typical ellipsoidal shape highlyagglomerated bulk particles depicted in Figure 1A. Analysis of textural propertieswas carried out using N2 adsorption-desorption analysis, which furnished typicalType-I isothermal corresponding to microporous sample (depicted in Figure 1D,red curve). The average particle size was obtained to be 320 nm, which wascalculated using SEM image and Image J software, considering at least 100 bulkparticles. The TS-1 obtained in example 1 was named as TS-1_A, in which (TBOTas Ti-source) was used.Example 2: Synthesis of TS-1_B zeolite using various Titanium sources inaccordance with the present inventionSimilarly, for the synthesis of TS-1_B (TTIP as Ti-source), 15.50 ml of Deionizedwater (Type -I, 18.2 MO cm-1, MilliQ), an aqueous solution containing 19.38 mlof Deionized water (Type -I, 18.2 MO cm-1, MilliQ) and 12.70 g of TPAOH wasmixed with 1.065 g of tetratbutyl orthotitanate. Then, 20.83 g of Tetraethylorthosilicate, was added dropwise to the existing solution. The solution was thenstirred at room temperature for sufficient time to allow complete dissolution of allingredients. The liquid solution termed as 'mother liquor' has the molarcomposition of 1SiO2:0.025TiO2:0. 2TPAOH:14H2O. After aging, the liquor wastransferred to a 100 ml Teflon liner, which was placed inside the stainless steel theacid digestion vessel / autoclave. The autoclave was heated at 170°C for at least 1day. The final solid sample was analyzed using the powder X-ray diffractionmethod depicted in Figure 1B (blue curve). The diffractogram illustrates theformation of the pure TS-1 (MFI framework) phase (compared with the referencepattern of MFI taken from the IZA website). Scanning electron microscopy (SEM)was used to visualize the morphology of the formed particle, which revealed theformation of a typical ellipsoidal shape, highly agglomerated bulk particles depictedin Figure 1B. Analysis of textural properties was carried out using N2 adsorptiondesorption analysis, which furnished typical Type-I isothermal corresponding tomicroporous sample (depicted in Figure 1D, blue curve). The average particle sizewas obtained to be 320 nm for TS-1_A and 270nm for TS-1_B, which wascalculated using SEM image and Image J software, considering at least 100 bulkparticles. The TS-1 obtained in example 2 was named as TS-1_B, in which (TTIPas Ti-source) was used.Example 3: Synthesis of Ti-CHA_A and Ti-CHA_B zeolites using TS-1_A andTS-1_B, respectively in accordance with the present invention (Protocol 1)The synthesized TS-1_A and TS-1_B in Examples 1 & 2 were first calcined at 550°C for 6h at 0.0167 K / s to remove the organic structure-directing agent (TPAOH)and moisture. For the synthesis of Ti-CHA_A zeolite, 4.40 ml of Deionized water(Type I, 18.2 MO cm-1, MilliQ), 0.040g of sodium hydroxide and 1.124 g ofTrimethyladamantylammonium Hydroxide (TMAdOH) were mixed for 15 minutesto allow complete dissolution of all ingredients. Further, 30 mg of aluminiumhydroxide was added, followed by 400mg of TS-1_A or TS-1_B for Ti-CHA_Aand Ti-CHA_B, respectively. The newly formed solution was kept under stirringfor atleast 4h for aging at room temperature. The solution has molar compositionmentioned in Table 1. After aging, the mother liquor was transferred to a 25 mlTeflon liner, which was placed inside the stainless-steel acid digestionvessel / autoclave. The autoclave was heated at 170°C for 4-7 days. The final solidproduct was washed thoroughly with DI water using centrifugation, followed bydrying at 80°C overnight. The solid sample was analyzed using the powder X-raydiffraction method depicted in Figure 2 (red curve and green curve for Ti-CHA_Aand Ti-CHA_B, respectively). The diffractogram shows the formation of the pureCHA phase (compared with the reference pattern of the CHA phase (depicted bythe black curve) taken from the IZA website). While the SEM image depicted inFigure 3A and 3B revealed bimodal distribution of crystals (size shown in Table 2).Subsequent quantitative analysis via XPS has elucidated that the tetrahedral Ti unitsin the compounds TCHA_A and TCHA_B are present in proportions of 77.51%and 82.73%, respectively (from Figure 4 and Table 3).Table 2. The table shows the variation in Si / Ti and Si / Al ratio with change in Tisource and synthetic protocol. The Energy Dispersive X-ray spectroscopy hasconfirmed the presence of Ti atoms in the SSZ-13 crystals. The amount of Alremains in similar range in all the samples showing no significant effect of syntheticprotocol and Ti source. The second synthesis method results in a lower Si / Ti ratio,suggesting higher Ti incorporation in the CHA framework. The particle size wasmeasured using ImageJ software for at least 100 particles.Table 2:Table 3:The table enlists the varying amount of Ti in tetrahedral and octahedral positions ascalculated from the XPS spectrum.Example 4: Synthesis of Ti-CHA_AA and Ti-CHA_BB using an additionalorganic Ti source in accordance with the present invention (Protocol 2)In example 3, synthesis mother liquor, additional Ti-source TBOT and TTIP, wereadded in the mother liquor of Ti-CHA_A and Ti-CHA_B to form Ti-CHA_AA andTi-CHA_BB. In 6 ml mother liquor, 1.67 wt. % of TBOT and equivalent moles ofTTIP were added to the growth solution to synthesis to Ti-CHA_AA and TiCHA_BB. The remaining process is similar to example 3. The solid sample wasanalyzed using the powder X-ray diffraction method depicted in Figure 2C (bluecurve and magenta curve for Ti-CHA_AA and Ti_CHA_BB, respectively). Thediffractogram shows the formation of the pure CHA phase (compared with thereference pattern of the CHA phase (depicted by the black curve) taken from theIZA website). The SEM images depicted in Figures 3C and 3D revealed the uniformcubical morphology of synthesized crystals. From SEM images and Image Jsoftware Ti-CHA_AA have average particle dimension of 2.75±0.26 μm while forTi-CHA_BB is 4.97±0.26 μm. Further, upon the introduction of an additionaltitanium source to the mother liquor, there is a notable predominance ofoctahedrally coordinated Ti in the resultant compounds TCHA_AA andTCHA_BB, with their respective concentrations being 64.15% and 86.92%. Thereis a reduction in tetrahedrally coordinated Ti in the resultant compoundsTCHA_AA and TCHA_BB, with their respective concentrations being 35.85% and13.08% (From figure 4 and Table 3). The synthesized Ti-CHA (Ti-SSZ-13) as perexamples 3 and 4 of the present invention are evaluated for thermal stability asillustrated in Figure 5A.Example 5: Synthesis of Al-SSZ-13 zeolite (Comparative example)In Example 5, 15 g of solution with molar composition 20TMAdaOH: 7.5Na2O:2.5Al2O3: 100SiO2: 4400 H2O. In a Polypropylene bottle, 0.100 g of NaOH wasadded to 9.517g of DI water. After that, 2.811g TMAdaOH (trimethyladmantlyhydroxide) was added, and the resulting mixture was stirred. 0.075g of Aluminiumhydroxide was added, followed by 2.498g of LUDOX AS-40, and the mixture wasleft at room temperature for 2h while stirring. Then, the solution was transferred toa 25 ml Teflon-lined stainless-steel autoclave at 170°C for 4-7 days in dynamicconditions (30 rpm) in an oven. The synthesized Ai-SSZ-13, as per example 5, isevaluated for thermal stability as illustrated in Figure 5B.TECHNICAL EFFECTS:The thermal stability of the Ti-SSZ-13 (examples 3 and 4) is evaluated using XRDand compared with that of conventional Al-SSZ-13 (example 5), as illustrated inFigures 5A and 5B. The XRD patterns presented in Figure 5A clearly demonstratethat the Ti-SSZ-13 zeolite exhibits significantly enhanced thermal stabilitycompared to conventional Al-SSZ-13, illustrated in Figure 5B. As shown in Figure5A, Ti-SSZ-13 retains the characteristic diffraction peaks of the CHA frameworkeven after calcination at temperatures as high as 1100°C for 10 hours, indicatingthe preservation of crystallinity and structural integrity. In contrast, Figure 5Breveals that Al-SSZ-13 undergoes substantial structural degradation at 1100°C,evidenced by the disappearance of distinct peaks and the emergence of a broad,amorphous halo. This direct comparison confirms that titanium incorporation intothe zeolite framework imparts a stabilizing effect that prevents amorphization andcollapse of the microporous structure under extreme thermal conditions. Thetechnical effect of this structural robustness is critical for catalytic applications thatrequire prolonged operation at high temperatures, as it ensures retention offramework integrity, microporosity, and potential active sites, ultimately leading toimproved catalyst durability, process flexibility, and operational lifespan.The technical results as per Examples 3-4 of the present invention are comparedwith Example 5 and are tabulated as below:Table 4:Although the subject matter has been described in considerable detail with referenceto certain preferred embodiments thereof, other embodiments are possible. As such,the spirit and scope of the subject matter should not be limited to the description ofthe preferred embodiment contained therein.
Claims
1. A fluoride-free titanium-chabazite (Ti-CHA) zeolite characterized by: a) a CHA framework having an X-ray diffraction characteristic peak at 2θ is 9.5°, 14.0°, 16.1°, 17.8°, and 20.7; b) having titanium atoms at tetrahedral framework positions in an amount of at least 10% of the total titanium content; c) a tetrahedral to octahedral titanium ratio in the range of 0.15 to 4.79; d) a Si / Ti molar ratio in the range of 37 to 83; e) a Si / Al molar ratio in the range of 11 to 15; and f) a particle size distribution or a crystal size in the range of 1.2 μm to 8.0 μm.
2. The fluoride-free titanium-chabazite (Ti-CHA) as claimed in claim 1, having thermal stability up to 1100°C.
3. A process for synthesizing fluoride-free titanium-chabazite (Ti-CHA) zeolite, comprising: a. preparing a titanium silicalite-1 (TS-1) precursor mixture comprising a silicon source, a titanium source, water, and an organic structure directing agent (OSDA); b. aging the TS-1 precursor mixture at room temperature; c. subjecting the aged TS-1 precursor mixture to hydrothermal treatment to obtain TS-1 zeolite having a Mobil Five (MFI) framework; d. calcining the TS-1 zeolite to remove the organic structure directing agent (OSDA) and moisture; e. preparing a Ti-CHA precursor reaction mixture by combining the calcined TS-1 zeolite with an aluminum source, an organic structure directing agent (OSDA), and an alkaline source; f. aging the Ti-CHA precursor reaction mixture at room temperature; and g. subjecting the aged Ti-CHA precursor reaction mixture to hydrothermal interzeolitic conversion to obtain titaniumsubstituted chabazite (Ti-CHA) zeolite.
4. The process as claimed in claim 3, wherein the silicon source is selected from tetraethyl orthosilicate (TEOS), fumed silica (FS), or silica gel (SG), and the titanium source is selected from tetrabutyl orthotitanate (TBOT), titanium tetraisopropoxide (TTIP), titanium dioxide, or titanium tetrachloride.
5. The process as claimed in claim 3, wherein the organic structure directing agent (OSDA) is tetrapropylammonium hydroxide (TPAOH) in the titanium silicalite-1 (TS-1) precursor mixture and the organic structure directing agent (OSDA) is N,N,N-trimethyl-1-adamantylammonium hydroxide (TMAdaOH) in the Ti-CHA precursor reaction mixture.
6. The process as claimed in claim 3, wherein the aging of the TS-1 precursor mixture is carried out for 8 to 24 hours at room temperature prior to hydrothermal synthesis.
7. The process as claimed in claim 3, wherein the hydrothermal treatment of the TS-1 zeolite is carried out at 150 to 200°C for 12 to 48 hours.
8. The process as claimed in claim 3, wherein the calcination of the TS-1 zeolite is performed at a temperature from 500°C to 600°C for 4 to 8 hours.
9. The process as claimed in claim 3, wherein the aging of the Ti-CHA precursor reaction mixture is carried out for about 4 hours at room temperature, and the hydrothermal interzeolitic conversion is carried out at 150 to 200°C for 4 to 7 days.
10. The process as claimed in claim 3, wherein the aluminum source is aluminum hydroxide, the alkaline source is sodium hydroxide, and the titanium-chabazite (Ti-CHA) zeolite is Ti-SSZ-13.