Method for manufacturing wall panel
Patent Information
- Application Number
- IN202217053974
- Authority / Receiving Office
- IN · IN
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2020-08-05
- Filing Date
- 2022-09-21
- Publication Date
- 2026-10-23
- Estimated Expiration
- 2041-06-03
AI Technical Summary
The existing methods for manufacturing wall panels for prefabricated baths using solid dry joint fillers face challenges in achieving high formation accuracy and water-stopping performance due to the need for expensive, high-accuracy machinery and materials, leading to increased costs and labor, while also risking water intrusion if the formation accuracy is low.
A manufacturing method that uses an inexpensive oblong metal plate material with a large angle tolerance at the corners, which is machined into a predetermined shape with press working, including bending and cutting steps to improve the external dimension accuracy and water-stopping performance, allowing for the use of a solid dry joint filler to prevent water intrusion.
This method enables the production of wall panels with extremely high formation accuracy and improved water-stopping performance, reducing construction time and costs by using a less expensive material and simplifying the construction process while maintaining effective water prevention.
Abstract
Description
Technical FieldThe present invention relates to a method for manufacturing wall panels and, moreparticularly, to a method for manufacturing wall panels configuring a wall section of aprefabricated bath.Background ArtConcerning wall panels configuring a wall section of a prefabricated bath, techniquesconcerning the structure of the wall panels and a method for manufacturing the wall panelsare disclosed in PTL 1 (JP-A-2003-033837), PTL 2 (JP-A-2004-150253), and the like.Citation ListPatent LiteraturePTL 1: JP-A-2003-033837PTL 2: JP-A-2004-150253Summary of InventionTechnical ProblemThe wall panels illustrated above are disposed in parallel to and spaced a gap havinga predetermined dimension from each other in the wall section of the prefabricated bath andare used in a state in which a joint filler is fit in the gap to thereby cause water-stopping action.If a liquid resin material having hardenability is used as the joint filler, even if fluctuationoccurs in the shape and the dimension of the gap because formation accuracy of an externaldimension of the wall panels is low, it is possible to fill the gap and prevent intrusion of waterinto a wall (a rear side opposite to an interior side). However, a problem occurs in that laborand time are required to construct the joint filler made of the liquid resin material and a workperiod and cost increase.Therefore, the wall panels described in PTLs 1 and 2 have a configuration in whicha solid dry joint filler formed using a resin material is used, whereby it is attempted to achievefacilitation of construction work and achieve a reduction in a work period and a cost reduction.On the other hand, since the dry joint filler is used, when the formation accuracy of theexternal dimension of the wall panels is low even a little, a problem occurs in that a waterstop in the gap in which the joint filler is fit cannot be completely performed and waterintrudes into the wall.The wall panels described above are manufactured by forming an oblong metal platematerial into a predetermined shape with press working. Therefore, if an oblong platematerial, an error (an angle tolerance) of which at a formation time (a cutting time) insquareness at four corners is set as small as possible, is used as a raw material, it is alsopossible to improve the formation accuracy of the external dimension of the wall panelsformed by the press working. However, to prepare such a raw material, an expensiveapparatus having high machining accuracy is necessary. Work and the like for measuring amaterial after the machining and reducing an error are also necessary. As a result, a problemoccurs in that the price of the plate material used as the raw material rises.Solution to ProblemThe present invention has been devised in view of the above circumstances and anobject of the present invention is to, concerning wall panels that are disposed in parallel toand spaced a gap having a predetermined dimension from each other in a wall section of aprefabricated bath and are used in a state in which a solid dry joint filler is fit in the gap tothereby cause water-stopping action, realize a manufacturing method that enables aninexpensive oblong plate material, an angle tolerance of which at a formation time (a cuttingtime) in squareness at four corners is set relatively large, to be used as a raw material and iscapable of improving formation accuracy of an external dimension at the time of formationof the wall panels by press working to be extremely high, dramatically improve water20stopping performance in the gap in which the dry joint filler is fit, and achieve a reduction ina work period and a cost reduction through facilitation of construction work.As an embodiment, the problems described above are solved by solving meansdisclosed below.A disclosed method for manufacturing wall panels is a method for manufacturingwall panels formed by a machining step of machining a plate material made of a metalmaterial, to one surface of which a sheet made of a resin material is stuck, into apredetermined shape while line-conveying the plate material, disposed in parallel to andspaced a gap having a predetermined dimension from each other in a wall section of aprefabricated bath, and used in a state in which a solid dry joint filler is fit in the gap to therebycause water-stopping action, the machining step including: an A1 step of preparing the platematerial having an oblong shape, an angle tolerance of 0.5° or less of which that occurs at acutting time is included in squareness at four corners; a B1 step of, after the A1 step, forming,at a first corner portion where a first short side and a first long side cross in the plate material,a cutout section including a first reference line serving as a reference position in bending theplate material along a bending line parallel to the first long side; a B2 step of forming, at thefirst corner portion, a cutout section including a second reference line serving as a referenceposition in bending the plate material along a bending line parallel to the first short side; a B3step of forming, at a second corner portion where a second short side and the first long sidecross in the plate material, a cutout section including a third reference line serving as areference position in bending the plate material along the bending line parallel to the first longside; a C1 step of, after the B1 step, the B2 step, and the B3 step, bumping the secondreference line against a bumping section and bending the plate material with press workingin a position parallel to and separated a predetermined dimension from the second referenceline to form a first bent surface; a C2 step of bumping the first bent surface against a bumpingsection and bending the plate material with the press working in a position parallel to andseparated a predetermined dimension from the first bent surface to form a second bent surface;a D1 step of, after the C1 step and the C2 step, rotating the plate material 90° in an in-planedirection; an E1 step of, after the D1 step, bumping the first reference line and the thirdreference line against bumping sections respectively corresponding thereto and bending theplate material with the press working in a position parallel to and separated a predetermineddimension from the first reference line and the third reference line to form a third bent surface;and an E2 step of bumping the third bent surface against a bumping section and bending theplate material with the press working in a position parallel to and separated a predetermineddistance from the third bent surface to form a fourth bent surface. The D1 step includes aprocess for rotating the plate material 90° with an error of 1° or less such that the first cornerportion faces a start point side in a line conveying direction. The E1 step includes a processfor, when bumping the first reference line and the third reference line against the bumpingsections respectively corresponding thereto, retracting the plate material toward the start pointside in the line conveying direction to thereby perform the bumping and bending the platematerial along a bending line parallel to the first long side and a second long side in a positioncloser to the second long side than the first long side.Advantageous Effects of InventionAccording to the present invention, it is possible to, concerning a method formanufacturing wall panels that are disposed in parallel to and spaced a gap having apredetermined dimension from each other in a wall section of a prefabricated bath and areused in a state in which a joint filler is fit in the gap to thereby cause water-stopping action,use, as a raw material, an inexpensive oblong plate material, an angle tolerance of which insquareness at four corners is set relatively large and manufacture wall panels havingextremely high formation accuracy of an external dimension. Consequently, in aconfiguration in which not liquid resin but a solid dry joint filler is used as a joint filler, it ispossible to dramatically improve water-stopping performance in a gap in which the dry jointfiller is fit. Therefore, when a wall section is configured, facilitation of construction workis achieved and it is possible to achieve a reduction in a work period and a cost reduction.Brief Description of DrawingsFig. 1 is a schematic diagram (a front surface side perspective view) showing anexample of a wall panel according to an embodiment of the present invention.Fig. 2 is a schematic diagram (a rear surface side perspective view) showing theexample of the wall panel according to the embodiment of the present invention.Fig. 3 is a III-III line sectional view in Fig. 1.Fig. 4 is a IV-IV line sectional view in Fig. 1.Fig. 5 is a schematic diagram (a plan view) of a corner joiner that couples wall panelsaccording to the embodiment.Fig. 6 is a schematic diagram (a plan view) of a flat joiner that couples wall panelsaccording to the embodiment.Fig. 7 is a schematic diagram (a perspective view) of a dry joint filler fit in a gapformed between the wall panels according to the embodiment disposed in parallel.Fig. 8 is an explanatory diagram for explaining a method for configuring a wallsection of a prefabricated bath using the wall panels according to the embodiment.Fig. 9 is an explanatory diagram for explaining a method for configuring the wallsection of the prefabricated bath using the wall panels according to the embodiment.Fig. 10 is an explanatory diagram for explaining the method for configuring the wallsection of the prefabricated bath using the wall panels according to the embodiment.Fig. 11 is a schematic diagram (a schematic configuration diagram in a plane view)showing an example of a manufacturing apparatus that manufactures the wall panelsaccording to the embodiment.Figs. 12A to 12C are schematic diagrams (plan views emphasizing a shape) of a rawmaterial used in manufacturing the wall panels according to the embodiment.Fig. 13 is a schematic diagram (a plan view) showing a machining example (a shapeexample) of the raw material in a halfway process of a method for manufacturing the wallpanels according to the embodiment.Fig. 14 is an A part enlarged diagram in Fig. 13.Fig. 15 is a B part enlarged diagram in Fig. 13.Fig. 16 is a schematic diagram (a plan view) of a first press mold included in themanufacturing apparatus that manufactures the wall panels according to the embodiment.Fig. 17 is a schematic diagram (a plan view) of a second press mold included in themanufacturing apparatus that manufactures the wall panels according to the embodiment.Description of EmbodimentsWall panels manufactured by a manufacturing method according to an embodimentare formed by a machining step of machining a plate material made of a metal material, toone surface of which a sheet made of a resin material is stuck, into a predetermined shapewhile line-conveying the plate material, disposed in parallel to and spaced a gap having apredetermined dimension from each other in a wall section of a prefabricated bath, and usedin a state in which a solid dry joint filler is fit in the gap to thereby cause water-stoppingaction. The embodiment of the present invention is explained in detail below with referenceto the drawings. Note that, in all figures for explaining the embodiment, members havingthe same functions are denoted by the same reference numerals and signs. Repeatedexplanation of the members is sometimes omitted.(Wall panel)First, a configuration example of a wall panel 30 according to this embodiment isexplained. Fig. 1 is a perspective view of a front surface side (an interior side of aprefabricated bath) of the wall panel 30. Fig. 2 is a perspective view of a rear surface side(an exterior side of the prefabricated bath) of the wall panel 30. Fig. 3 is a III-III linesectional view in Fig. 1. Fig. 4 is a IV-IV line sectional view in Fig. 1. As an example, thewall panel 30 is formed with a long side dimension of approximately 1000 mm to 2300 mmand a short side dimension of approximately 300 mm to 1200 mm but is not limited to this.The drawings such as Fig. 1 are not displayed in strict scales with respect to actual dimensions.As a material for manufacturing the wall panel 30, as an example, a rectangular(substantially oblong) plate material (explained in detail below) made of a metal material (forexample, galvanized steel having thickness of approximately 0.5 mm), that is, a steel plate(so called "decorated steel plate") 10, to one surface of which a sheet (so-called "decoratedsheet") 39 made of a resin material (for example, polyester resin having thickness ofapproximately 0.1 mm) is stuck (hereinafter, sometimes simply referred to as "raw material")is used. Wall surface design of the prefabricated bath can be changed by changing designof the sheet 39. It is possible to provide a wide variety of variations (that is, a sheet 39sticking surface is the surface of the wall panel 30). As explained in detail below, the wallpanel 30, a wall surface configuration section of which has an oblong shape in a plane view,is manufactured by, using the raw material 10, after machining four corners into apredetermined shape with press working (cutting), machining four sides into a predeterminedshape with press working (bending). Note that the configuration of the raw material 10 isnot limited to the example described above.As a configuration example of the wall panel 30, the wall panel 30 includes a bentsection 31 having a U-shape in section (more accurately, a square bracket shape) as shown inFig. 3 by being bent at 90° to a rear surface side and subsequently bent at 90° to the rearsurface side in a position closer to a first short side 15 of the raw material 10. The wall panel30 includes a bent section 32 having an L shape in section as shown in Fig. 3 by being bentat 90° to a front surface side and subsequently bent at 90° to the rear surface side in a positioncloser to a second short side 16 of the raw material 10. On the other hand, the wall panel 30includes bent sections 33 and 34 having a triangular shape in section as shown in Fig. 4 bybeing bent at 90° to the rear surface side, subsequently bent at 120° to the rear surface side,and subsequently bent at 90° to the rear surface side respectively in a position closer to a firstlong side 17 and a position closer to a second long side 18 of the raw material 10. However,the wall panel 30 is not limited to this configuration.(Joiners)Subsequently, a configuration example of joiners 40, 50 that couple wall panels 30according to this embodiment is explained. Fig. 5 is a plan view of a corner joiner 40disposed at a corner portion of the prefabricated bath. Fig. 6 is a plan view of a flat joiner50 disposed in a side portion (an intermediate portion) of the prefabricated bath.The corner joiner 40 is formed by machining an oblong plate material made of ametal material (for example, galvanized steel) into a predetermined shape with bending. Asshown in Fig. 5, the corner joiner 40 includes bent sections 41, 42 having a triangular shapein section formed by being bent respectively at end portions (that is, long side portions) in thelatitudinal direction of the plate material. The corner joiner 40 has a configuration in whicha space between the bent sections 41, 42 is formed as an opening section 44 and the inside ofthe corner joiner 40 is formed as a hollow section 46.The flat joiner 50 is formed by machining an oblong plate material made of a metalmaterial (for example, galvanized steel) into a predetermined shape with bending. As shownin Fig. 6, the flat joiner 50 includes bent sections 51, 52 having a triangular shape in sectionformed by being bent respectively at ends portions (that is, long side portions) in thelatitudinal direction of the plate material. The flat joiner 50 has a configuration in which aspace between the bent sections 51, 52 is formed as an opening section 54 and the inside ofthe flat joiner 50 is formed as a hollow section 56.(Method of use)A method for configuring a wall section of the prefabricated bath using the wallpanels 30 according to this embodiment is explained. Schematically, the wall panels 30 aredisposed to extend along the whole outer peripheral edge of a floor section 62 (as an example,a shallow box-like floor pan) 62 together with the corner joiner 40 and the flat joiner 50,which are components for coupling, to configure the wall section of the prefabricated bath.Note that block members 66 to 69 made of a resin material are fit in the upper end portionsand the lower end portions of the corner joiner 40 and the flat joiner 50. The method isexplained below in detail.First, as shown in Fig. 8, one wall panel 30 (30A) is erected at the outer edge portionof the floor section 62 in one corner vicinity position (adjacent position) of the floor section62 formed in a rectangular shape. At this time, a bent surface 31b (a first bent surface) ofthe bent section 31 of the wall panel 30 (30A) and a under-wall gasket 64 provided on acontact surface 62a at the outer edge portion of the floor section 62 come into contact (closecontact). Water intrusion prevention is achieved. Note that, as an example of the underwallgasket 64, a publicly-known waterproof tape made of a resin material or the like is used.Subsequently, the corner joiner 40 is erected in a predetermined position (a cornerposition adjacent to the wall panel 30 (30A)) of the floor section 62. Specifically, after thecorner joiner 40 is attached to the wall panel 30 (30A), the lower end portion of the cornerjoiner 40 is fit in the block member 67 disposed on the floor section 62, whereby the cornerjoiner 40 and the wall panel 30 are erected while being positioned in predetermined positions.When the corner joiner 40 is attached to the wall panel 30 (30A), the bent section 33of the wall panel 30 (30A) is inserted into the hollow section 46 from the opening section 44of the corner joiner 40 and locked to the bent section 42. At this time, a bent surface 33a (asecond locking surface) of the bent section 33 and a bent surface 42a (a second supportingsurface) of the bent section 42 come into contact.Subsequently, one wall panel 30 (30B) is erected at the outer edge portion of the wallsection 62. When the one wall panel 30 (30B) is erected, the bent section 34 of the wallpanel 30 (30B) is inserted into the hollow section 46 from the opening section 44 of the cornerjoiner 40 to be locked to the bent section 41. At this time, a bent surface 34a (a first lockingsurface) of the bent section 34 and a bent surface 41a (a first supporting surface) of the bentsection 41 come into contact. Note that, as in the case of the wall panel 30 (30A), the bentsurface 31b (the first bent surface) of the bent section 31 of the wall panel 30 (30B) and theunder-wall gasket 64 provided on the contact surface 62a at the outer edge portion of the floorsection 62 come into contact (close contact). Water intrusion prevention is achieved.Subsequently, as shown in Fig. 9, the block member 66 is attached to the upper endportion of the corner joiner 40. The block member 66 is provided with protrusion-likeinsertion sections (not shown) respectively inserted into the bent section 33 (specifically, ahollow section 33d) of the wall panel 30 (30A) and the bent section 34 (specifically, a hollowsection 34d) of the wall panel 30 (30B). The insertion sections are inserted into the bentsection 33 (the hollow section 33d) and the bent section 34 (the hollow section 34d), wherebythe block member 66 can be prevented from coming off. The wall panel 30 (30A) and thecorner joiner 40 can be surely fixed in a state in which the bent surface 33a (the second lockingsurface) of the wall panel 30 (30A) is in contact with the bent surface 42a (the secondsupporting surface) of the bent section 42 of the corner joiner 40 and the wall panel 30 (30B)and the corner joiner 40 can be surely fixed in a state in which the bent surface 34a (the firstlocking surface) of the wall panel 30 (30B) is in contact with the bent surface 41a (the firstsupporting surface) of the bent section 41 of the corner joiner 40. However, theconfiguration of the block member 66 is not limited to the example described above.Subsequently, the flat joiner 50 is erected in a predetermined position (anintermediate position adjacent to the wall panel 30B) of the floor section 62. Specifically,after the flat joiner 50 is attached to the wall panel 30B, the lower end portion of the flat joiner50 is fit in the block member 69 disposed on the floor section 62, whereby the flat joiner 50and the wall panel 30 are erected while being positioned in predetermined positions.When the flat joiner 50 is attached to the wall panel 30 (30B), the bent section 33 ofthe wall panel 30 (30B) is inserted into the hollow section 56 from the opening section 54 ofthe flat joiner 50 to be locked to the bent section 52. At this time, the bent surface 33a (thesecond locking surface) of the bent section 33 and a bent surface 52a (a fourth supportingsurface) of the bent section 52 come into contact.Subsequently, as shown in Fig. 10, the block member 68 (68A) is attached to theupper end portion of the flat joiner 50. The block member 68 (68A) is provided with aprotrusion-like insertion section (not shown) inserted into the bent section 33 (specifically,the hollow section 33d) of the wall panel 30 (30B). The insertion section is inserted into thebent section 33 (the hollow section 33d), whereby the block member 68 (68A) can beprevented from coming off. The wall panel 30 (30B) and the flat joiner 50 can be surelyfixed in a state in which the bent surface 33a (the second locking surface) of the wall panel30 (30B) is in contact with the bent surface 52a (the fourth supporting surface) of the bentsection 52 of the flat joiner 50. However, the configuration of the block member 68 (68A)is not limited to the example described above.Subsequently, one wall panel 30 (30C) is erected at the outer edge portion of thefloor section 62. When one wall panel 30 (30C) is erected, the bent section 34 of the wallpanel 30 (30C) is inserted into the hollow section 56 from the opening section 54 of the flatjoiner 50 to be locked to the bent section 51. At this time, the bent surface 34a (the firstlocking surface) of the bent section 34 and a bent surface 51a (a third supporting surface) ofthe bent section 51 come into contact. Note that, as in the case of the wall panels 30A, 30B,the bent surface 31b (the first bent surface) of the bent section 31 of the wall panel 30C andthe under-wall gasket 64 provided on the contact surface 62a at the outer edge portion of thefloor section 62 come into contact (close contact). Water intrusion prevention is achieved.Subsequently, the block member 68 (68B) is attached to the upper end portion of theflat joiner 50. The block member 68 (68B) is provided with a protrusion-like insertionsection (not shown) inserted into the bent section 34 (specifically, the hollow section 34d) ofthe wall panel 30 (30C). The insertion section is inserted into the bent section 34 (the hollowsection 34d), whereby the block member 68 (68B) can be prevented from coming off. Thewall panel 30 (30C) and the flat joiner 50 can be surely fixed in a state in which the bentsurface 34a (the first locking surface) of the wall panel 30 (30C) is in contact with the bentsurface 51a (the third supporting surface) of the bent section 51 of the flat joiner 50.However, the configuration of the block member 68 (68B) is not limited to the exampledescribed above.Subsequently, according to design specifications (here, a horizontal directiondimension of the wall section) of the prefabricated bath, a process for attaching the cornerjoiner 40 to the wall panel 30C and terminating the wall surface or attaching the flat joiner 50to extend the wall surface is carried out. Note that, irrespective of whether the corner joiner40 or the flat joiner 50 is attached, a method for attaching the corner joiner 40 or the flat joiner50 is the same as the respective cases explained above. Therefore, repeated explanation isomitted.By sequentially assembling the wall panel 30, the corner joiner 40, and the flat joiner50 in this way, the wall section can be formed to extend along the whole outer peripheral edgeof the floor section 62. When the wall section is formed, the wall panel 30, the corner joiner40, and the flat joiner 50 pull against each other to be integrated. It is possible to easily formthe wall surface of the prefabricated bath without providing a special member. Note that, atthis time, the bent surfaces 34a (the first locking surface) and 33a (the second locking surface)of the wall panel 30 and the bent surfaces 41a (the first supporting surface) and 42a (thesecond supporting surface) of the corner joiner 40 and the bent surfaces 51a (the thirdsupporting surface) and 52a (the fourth supporting surface) of the flat joiner 50 correspondingto the bent surfaces 34a (the first locking surface) and 33a (the second locking surface) of thewall panel 30 are elastically locked.Incidentally, a gap is formed between the wall panels 30 locked by the corner joiner40 and disposed in parallel, more specifically, between the bent section 33 of one wall panel30 (30A) inserted into the hollow section 46 from the opening section 44 and the bent section34 of the other wall panel 30 (30B). Therefore, a process for fitting a dry joint filler 60shown in Fig. 7 in the gap and closing the gap to prevent intrusion of water is carried out.As an example, the dry joint filler 60 is formed in an elastically deformable solid shape usinga resin material. That is, the dry joint filler 60 is configured to bring the rear surface (thesurface on the exterior side) of a base 60a into elastic contact with the surface of the wallpanel 30 and bring projected sections 60b into elastic contact with the bent section 33 (here,a fourth bent surface 33c) and the bent section 34 (here, a third bent surface 34c) of the wallpanel 30 to thereby cause water-stopping action for the gap (action of preventing waterintrusion into the wall). However, the configuration of the dry joint filler 60 is not limitedto the example described above.Similarly, a gap is formed between the wall panels 30 locked by the flat joiner 50and disposed in parallel, more specifically, between the bent section 33 of one wall panel 30(30B) inserted into the hollow section 56 from the opening section 54 and the bent section 34of the other wall panel 30 (30C). Therefore, a process for fitting the dry joint filler 60 shownin Fig. 7 in the gap and closing the gap to prevent intrusion of water is carried out. Asexplained above, the dry joint filler 60 is formed in the elastically deformable solid shapeusing the resin material. That is, the dry joint filler 60 is configured to bring the rear surface(the surface on the exterior side) of the base 60a into elastic contact with the surface of thewall panel 30 and bring the projected sections 60b into elastic contact with the bent section33 (here, the fourth bent surface 33c) and the bent section 34 (here, the third bent surface 34c)of the wall panel 30 to thereby cause water-stopping action for the gap (action of preventingwater intrusion into the wall). However, the configuration of the dry joint filler 60 is notlimited to the example described above. The dry joint filler may be configured differentlyfor a corner and for a side portion (an intermediate portion) (not shown).The wall section of the prefabricated bath is configured through these processes.As explained above, if the liquid resin material having hardenability is used as thejoint filler, even if fluctuation occurs in the shape and the dimension of the gap becauseformation accuracy of the external dimension of the wall panel 30 is low, it is possible to fillthe gap and prevent intrusion of water into the wall (the rear side opposite to the interior side).However, a problem occurs in that labor and time are required to construct the joint fillermade of the liquid resin material and a work period and cost increase. Therefore, in thisembodiment, facilitation of construction work is achieved (see Fig. 8 to Fig. 10) and areduction in a work period and a cost reduction are enabled by using the solid dry joint filler60 formed using the resin material shown in Fig. 7.However, since the solid dry joint filler is used, a problem occurs in that, as theformation accuracy of the external dimension of the wall panel 30 is lower, the water-stoppingaction for the gap in which the joint filler is fit is not obtained and water intrudes into the wall.Specifically, intrusion of water into the wall (the rear side opposite to the interior side) couldoccur when squareness of the bent surface 33c (the fourth bent surface) of the bent section 33and squareness of the bent surface 34c (the third bent surface) of the bent section 34 withrespect to the bent surface 31b (the first bent surface) of the bent section 31 are inaccurate.That is, when the bent surface 31b (the first bent surface) is brought into contact (closecontact) with the floor section 62 (here, the under-wall gasket 64 provided on the contactsurface 62a) and the wall panel 30 is erected, if the squareness is inaccurate, the bent surface33c (the fourth bent surface) and the bent surface 34c (the third bent surface) of the wall panel30 are disposed to deviate (tilt) from the vertical direction. Therefore, the gap between thebent surface (here, the fourth bent surface 33c) of one wall panel 30 and the bent surface (here,the third bent surface 34c) of the other wall panel 30 is distorted in a trapezoidal shape or thelike, a void is formed between the bent surfaces (the fourth bent surface 33c and the third bentsurface 34c) when the solid dry joint filler 60 is fit in the gap, and intrusion of water occurs.Conversely, when it is attempted to hold the bent surface (here, the fourth bent surface 33c)of one wall panel 30 and the bent surface (here, the third bent surface 34c) of the other wallpanel 30 in parallel along the vertical direction, a void is formed between the bent surface 31b(the first bent surface) of the wall panel 30 and the floor section 62 (here, the under-wallgasket 64 provided on the contact surface 62a) and intrusion of water occurs.The wall panel 30 described above is manufactured to be formed in a predeterminedshape by press-working the oblong raw material 10 (the decorated steel plate described above).Therefore, if press working by an outer shape reference is performed using, as the rawmaterial 10, an oblong plate material, an error (an angle tolerance) of which at a formationtime (a cutting time) in squareness at four corners is set as small as possible, it is also possibleto improve formation accuracy of the external dimension of the wall panel 30 to be formed.However, to prepare such a raw material 10, an expensive apparatus having high machiningaccuracy is necessary. Work and the like for measuring a material after the machining andreducing an error are also necessary. As a result, a problem occurs in that the price of theplate material used as the raw material 10 rises.Therefore, the present inventor has devised the following manufacturing method thatenables an inexpensive oblong plate material, an angle tolerance of which at a formation time(a cutting time) in squareness at four corners is set relatively large, to be used as the rawmaterial 10 and is capable of improving formation accuracy of an external dimension at thetime of formation of the wall panel 30 by press working to be extremely high.(Manufacturing method)Subsequently, a method for manufacturing the wall panels 30 according to thisembodiment is explained. The manufacturing method includes main steps described belowfor manufacturing the wall panel 30 having a predetermined shape by cutting and bending theraw material 10 while line-conveying the raw material 10. A manufacturing apparatus 100that performs machining in one line is used for the manufacturing. An explanatory diagram(a schematic configuration diagram in a plane view) of the manufacturing apparatus 100 isshown in Fig. 11. Note that an arrow X in the figure indicates a line conveying direction.An oblong plate material (the decorated steel plate described above) is used as theraw material 10. About the shape "oblong", ideally, all angles at four corners are 90° (±0°).However, in reality, an error (in this application, referred to as "angle tolerance") is includedin the angles at the four corners at a formation time (a cutting time) (that is, not only ageometrically defined oblong but also a substantial oblong is included in the oblong). Ingeneral, as the angle tolerance is smaller, a material price is higher and, as the angle toleranceis larger, the material price is lower.With the manufacturing method according to this embodiment, since themanufacturing method includes a characteristic configuration (steps) explained below, aninexpensive oblong plate material, an angle tolerance of which at a formation time (a cuttingtime) in squareness at four corners is set relatively large, can be used as the raw material 10.If examples of the raw material 10 are clearly emphasized and illustrated, raw materialshaving shapes like a rhombus raw material 10 (10A) shown in Fig. 12A, a trapezoidal rawmaterial 10 (10B) shown in Fig. 12B, and a raw material 10 (10C) including a camber shownin Fig. 12C can also be used (the figures are figures in which the shapes are emphasized forexplanation and are not reduced figures of actual shapes). As in these examples, an oblongplate material in which a relatively large angle tolerance is allowed in squareness at fourcorners, specifically, an oblong plate material having an angle tolerance of ±0.5° or less withrespect to a right angle (90°) in angles at four corners (an angle θ1 of a first corner portion11, an angle θ2 of a second corner portion 12, an angle θ3 of a third corner portion 13, andan angle θ4 of a fourth corner portion 14) can be used as the raw material 10. The wall panel30 having high outer shape accuracy can be manufactured. This is explained in detail below.First, a step of preparing an oblong plate material (in which the angle tolerancedescribed above is allowed) to be the raw material 10 and carrying the oblong plate materialonto a line is carried out (an A1 step). As an example, a method for placing, from a stocker102 in which a plurality of the plate materials are stacked and stored, the plate materials onthe line (here, on a start end portion 104) one by one in predetermined tact using a conveyingapparatus (not shown) such as a feeder can be adopted. Note that a conveying apparatus(not shown) such as a belt conveyor is mainly used for line conveyance of the raw material10 thereafter. As an example, the plate material is conveyed with the first short side 15 as ahead up to a rotating and moving unit 110 (explained below) and is conveyed with the secondlong side 18 side as a head from the rotating and moving unit 110. However, the step is notlimited to this configuration.Subsequently, B1, B2, and B3 steps are carried out in a corner cutting unit 106 afterthe A1 step. As an example, the corner cutting unit 106 includes a first press mold 160 anda second press mold 170 for cutting (explained in detail below). A shape example (in a planeview) of the raw material 10 formed by carrying out the B1, B2, and B3 steps is shown in Fig.13, Fig. 14 (an A part enlarged view), and Fig. 15 (a B part enlarged view).First, as the B1 step, a step of forming, using the first press mold 160, at the firstcorner portion 11 where the first short side 15 and the first long side 17 cross in the rawmaterial 10, with press working (cutting), a cutout section 24 including a first reference line21 serving as a reference position in bending the raw material 10 along a bending line parallelto the first long side 17 is carried out. Note that "parallel" in this application is meant notto be limited to geometrically defined "parallel" and is meant to indicate that a defineddirection extends along a target direction.As the B2 step, a step of forming, using the second press mold 170, at the first cornerportion 11, with press working (cutting), a cutout section 25 including a second reference line22 serving as a reference position in bending the raw material 10 along a bending line parallelto the first short side 15 is carried out.As the B3 step, a step of forming, using the second press mold 170, at the secondcorner portion 12 where the second short side 16 and the first long side 17 cross in the rawmaterial 10, with press working (cutting), a cutout section 26 including a third reference line23 serving as a reference position in bending the raw material 10 along the bending lineparallel to the first long side 17 is carried out.Note that the B1, B2, and B3 steps are carried out in this order in this embodiment.However, the B1, B2, and B3 steps are not limited to this. The B1, B2, and B3 steps canalso be carried out, for example, in the order of the B2, B1, and B3 steps. Alternatively, thefirst press mold and the second press mold can also be configured as one mold (not shown)and the B1 and B2 steps can also be simultaneously carried out as one step.Subsequently, C1 and C2 steps are carried out in a short side machining unit 108after the B1, B2, and B3 steps. As an example, the short side machining unit 108 includesa press mold 130 for bending, bumping sections 132, 136 that set a reference position inperforming positioning of the raw material 10, and positioning devices 134, 138 that grip andprecisely move the raw material 10 from the reference position and perform the positioning.Note that the bumping section 132 advances and retracts in the left-right direction with respectto the line conveying direction and has a bumping surface on a start end side in the lineconveying direction. The bumping section 136 advances and retracts in the up-downdirection with respect to the line conveying direction and has a bumping surface on the startend side in the line conveying direction. However, the short side machining unit 108 is notlimited to this configuration.First, as the C1 step, the reference line 22 of the raw material 10 is bumped againstthe bumping section 132 and a reference position in performing positioning of a press workingposition in the raw material 10 is set. Subsequently, a step of bending the raw material 10with press working and forming the first bent surface 31b in a predetermined position wherebending is performed in the raw material 10 (specifically, a position parallel to and separateda predetermined dimension from the second reference line 22) is carried out. In thisembodiment, since an end portion closer to the first short side 15 in the raw material 10 isbent twice to form the bent section 31 including a bent surface 31a and the bent surface 31b(the first bent surface), two positions are set as the predetermined position. Therefore, anoperation for moving the raw material 10 in the same direction as the line conveying directionwith the positioning devices 134, performing positioning such that the predetermined positioncoincides with a press working position in the press mold 130, and performing press working(bending) is performed twice (that is, two rounds). Note that "parallel" in this applicationis meant to indicate geometrically defined "parallel" but include a tolerance due to machiningor the like.As the C2 step, the first bent surface 31b of the raw material 10 is bumped againstthe bumping section 136 and a reference position in positioning a press working position inthe raw material 10 is set. Subsequently, a step of bending the raw material 10 with pressworking to form a second bent surface 32b in a predetermined position where bending isperformed in the raw material 10 (specifically, a position parallel to and separated apredetermined dimension from the first bent surface 31b) is carried out. In this embodiment,since an end portion closer to the second short side 16 in the raw material 10 is bent twice toform the bent section 32 including a bent surface 32a and the bent surface 32b (the secondbent surface), two positions are set as the predetermined position. Therefore, an operationfor moving the raw material 10 in the opposite direction of the line conveying direction withthe positioning devices 138, performing positioning such that the predetermined positioncoincides with a press working position in the press mold 130, and performing press working(bending) is performed twice (that is, two rounds).Note that, as a modification, a press model that performs the press working in the C1step and a press mold that performs the press working in the C2 step may be configured bydifferent two molds (not shown).Subsequently, a D1 step is carried out in the rotating and moving unit 110 after theC1 and C2 steps. As an example, the rotating and moving unit 110 includes a rotating andmoving device (not shown) that rotates and moves the raw material 10 to change the directionof the line conveyance. As the D1 step, a step of rotating the raw material 10 90° in the in30plane direction is carried out.Subsequently, an E1 step is carried out in a long side machining unit 112 (112A) afterthe D1 step. An E2 step is carried out in the long side machining unit 112 (112B). As anexample, the long side machining unit 112 (112A) includes a press mold 140 for bending,bumping sections 142 (142A, 142B) that set a reference position in positioning the rawmaterial 10, and positioning devices 144 that push and precisely move the raw material 10from the reference position and perform positioning. Note that, in this embodiment, thepositioning devices 144 include mechanisms for moving the bumping sections 142. Thebumping sections 142 are configured to come into contact with the raw material 10 (that is,while keeping a bumped state) and push the raw material 10. The bumping sections 142advance and retract in the up-down direction with respect to the line conveying direction andhave bumping surfaces on a terminal end side in the line conveying direction. However, thelong side machining unit 112 (112A) is not limited to this configuration.On the other hand, the long side machining unit 112 (112B) includes a press mold146 for bending, bumping sections 148 (148A, 148B) that set a reference position inpositioning the raw material 10, positioning devices 150 that push and precisely move the rawmaterial 10 from the reference position and perform positioning. Note that, in thisembodiment, the positioning devices 150 include mechanisms for moving the bumpingsections 148. The bumping sections 148 are configured to come into contact with the rawmaterial 10 (that is, while keeping a bumped state) and push the raw material 10. Thebumping sections 148 advance and retract in the up-down direction with respect to the lineconveying direction and have bumping surfaces on a start end side in the line conveyingdirection. However, the long side machining unit 112 (112B) is not limited to thisconfiguration.First, as the E1 step, the first reference line 21 and the third reference line 23 of theraw material 10 are respectively bumped against the bumping sections 142 correspondingthereto (specifically, the first reference line 21 is bumped against the bumping section 142Aand the third reference line 23 is bumped against the bumping section 142B) and a referenceposition in positioning a press working position in the raw material 10 is set. Subsequently,a step of bending the raw material 10 with press working to form the third bent surface 34cin a predetermined position where bending is performed in the raw material 10 (specifically,a position parallel to and separated a predetermined dimension from the first reference line21 and the third reference line 23) is carried out. In this embodiment, since an end portioncloser to the second long side 18 in the raw material 10 is bent three times to form the bentsection 34 including the bent surface 34a (the first locking surface), a bent surface 34b, andthe bent surface 34c (the third bend surface), three positions are set as the predeterminedposition. Therefore, an operation for moving the raw material 10 in the same direction asthe line conveying direction with the positioning devices 144, performing positioning suchthat the predetermined position coincides with a press working position in the press mold 140,and performing press working (bending) is performed three times (that is, three rounds).As the E2 step, the third bent surface 34c of the raw material 10 is bumped againstthe bumping sections 148 (148A, 148B) and a reference position in positioning a pressworking position in the raw material 10 is set. Subsequently, a step of bending the rawmaterial 10 with press working to form the fourth bent surface 33c in a predetermined positionwhere bending is performed in the raw material 10 (specifically, a position parallel to andseparated a predetermined dimension from the third bent surface 34c) is carried out. In thisembodiment, since an end portion closer to the first long side 17 in the raw material 10 is bentthree times to form the bent section 33 including the bent surface 33a (the second lockingsurface), a bent surface 33b, and the bent surface 33c (the fourth bent surface), three positionsare set as the predetermined position. Therefore, an operation for moving the raw material10 in the opposite direction of the line conveying direction with the positioning devices 150,performing positioning such that the predetermined position coincides with a press workingposition in the press mold 146, and performing press working (bending) is performed threetimes (that is, three rounds).With the method for manufacturing the wall panels 30 according to this embodiment,since the manufacturing method includes the main steps closely linked to one another, thefollowing marked effects can be obtained. Specifically, a plate material having lowmachining accuracy (that is, outer shape accuracy), for example, an oblong plate material inwhich an angle tolerance of 0.5° or less that occurs at a cutting time is included in squarenessat four corners can be used as the raw material 10. Therefore, it is possible to achieve areduction in material expenses. Further, even if such a plate material having low accuracyis used, it is possible to manufacture the oblong wall panel 30 in which a tolerance (amachining error) in squareness between short side bent surfaces (here, the first bent surface31b and the second bent surface 32b) and long side bent surfaces (here, the third bent surface34c and the fourth bent surface 33c) (that is, squareness at four corners) is extremely small.Therefore, it is possible to obtain high water-stopping action (water intrusionpreventing action) simply by disposing the wall panels 30 in parallel to and spaced a gaphaving a predetermined dimension from each other in the wall section of the prefabricatedbath and fitting the solid dry joint filler 60 in the gap. That is, since it is unnecessary toperform work for filling the gap with a liquid joint filler and stopping water, it is possible toperform setting work for the wall section simply and in a short time and achieve a reductionin site work expenses.Subsequently, the first press mold 160 and the second press mold 170 used incarrying out the B1, B2, and B3 steps explained above are explained in detail. Fig. 16 is aplan view (a schematic diagram) of the first press mold 160. Fig. 17 is a plan view (aschematic diagram) of the second press mold 170.The first press mold 160 according to this embodiment includes a first edge surface162 as an edge surface that forms the first reference line 21. On the other hand, the secondpress mold 170 according to this embodiment includes a second edge surface 172 as an edgesurface that forms the second reference line 22 and includes a third edge surface 174 as anedge surface that forms the third reference line 23. The second edge surface 172 of thesecond press mold 170 is configured to be formed at 90° with an angle tolerance of 0.05° orless with respect to the first edge surface 162 of the first press mold 160. The third edgesurface 174 of the second press mold 170 is configured to be formed at 90° with an angletolerance of 0.05° or less with respect to the second edge surface 172.Therefore, the B1 step according to this embodiment explained above includes aprocess in which the first edge surface 162 forms the first reference line 21 with press working(cutting) using the first press mold 160.The B2 step according to this embodiment explained above includes a process inwhich, after the raw material 10 is line-conveyed in parallel to the first reference line 21formed in the B1 step with an error (here, an error (a deviation amount) in an angle direction(a rotating direction) in the in-plane direction of the raw material 10 that occurs during theconveyance) of 0.03° or less, the second edge surface 172 forms the second reference line 22with press working (cutting) using the second press mold 170. That is, the second referenceline 22 is machined to be formed at 90° with an angle tolerance of 0.05° or less with respectto the first reference line 21.By including the processes explained above, it is possible to obtain the followingmarked effects. Specifically, a bending width on a short side to be the floor side of the wallsection at a setting time (here, a width dimension in the latitudinal direction (the short sidedirection) of the first bent surface 31b) can be optionally set. That is, many types of wallpanels 30 having different outer shapes (here, width dimensions described above) can bemanufactured in one line. Since the raw material 10 can be cut into a shape having anextremely small tolerance (machining error) in squareness between the first reference line 21and the second reference line 22, it is possible to manufacture the oblong wall panel 30 havingan extremely small tolerance (machining error) in squareness between a short side bentsurface (here, the first bent surface 31b) and long side bent surfaces (here, the third bentsurface 34c and the fourth bent surface 33c). Therefore, when the wall section is configured,it is possible to obtain high water-stopping action simply by fitting the dry joint filler 60 inthe gap of the wall panels 30 disposed in parallel.Further, the B3 step according to this embodiment explained above includes aprocess in which, after the raw material 10 is line-conveyed in parallel to the first referenceline 21 formed by the B1 step with an error (here, an error (a deviation amount) in an angledirection (a rotating direction) in the in-plane direction of the raw material 10 that occursduring the conveyance) of 0.03° or less, the raw material 10 is moved in parallel to the secondreference line 22 formed by the B2 step with an error (here, an error (a deviation amount) inan angle direction (a rotating direction) in the in-plane direction of the raw material 10 thatoccurs during the conveyance) of 0.03° or less and the third edge surface 174 forms the thirdreference line 23 with press working (cutting) using the second press mold 170. At this time,the third reference line 23 is machined to be formed in parallel to the first reference line 21with a tolerance (here, a separation dimension error) of 0.5 mm or less (more preferably, 0.2mm or less).By including the processes explained above, it is possible to obtain the followingmarked effects. Specifically, since the raw material 10 can be cut into a shape having anextremely small tolerance (machining error) in parallelism between the first reference line 21and the third reference line 23, it is possible to manufacture the oblong wall panel 30 havingan extremely small tolerance (machining error) in squareness between a short side bentsurface (here, the first bent surface 31b) and long side bent surfaces (here, the third bentsurface 34c and the fourth bent surface 33c). Therefore, when the wall section is configured,it is possible to obtain high water-stopping action simply by fitting the dry joint filler 60 inthe gap between the wall panels 30 disposed in parallel.Further, the D1 step according to this embodiment explained above includes aprocess for rotating the raw material 10 90° with an error (here, an error (a deviation amount)in an angle direction (a rotating direction) in the in-plane direction of the raw material 10 thatoccurs during rotation and movement) of 1° or less such that the first corner portion 11 facesthe start end side in the line conveying direction.The E1 step according to this embodiment explained above includes a process for,when bumping the first reference line 21 and the third reference line 23 respectively againstthe bumping sections 142A, 142B corresponding thereto, performing the bumping byretracting the raw material 10 toward the start end side in the line conveying direction andbending the raw material 10 along a bending line parallel to the first long side 17 and thesecond long side 18 in a position closer to the second long side 18 than the first long side 17.By including the processes explained above, it is possible to obtain the followingmarked effects. Specifically, the first corner section 11 used as a reference position withhigh accuracy (in particular, accuracy of squareness of the first reference line 21 and thesecond reference line 22) can be located in a side portion on the left or the right in the lineconveying direction (is set in the right side portion in the line conveying direction in thisembodiment but may be set in the left side portion). That is, when the raw material 10 ismachined, the bumping section 132 against which the second reference line 22 is bumped andthe bumping section 142 (142A) against which the first reference line 21 is bumped can bealigned and disposed in the side portion on the left or the right in the line conveying direction(here, the right side portion in the line conveying direction). Therefore, it is possible toimprove adjustment accuracy in adjusting bumping surfaces of the two bumping sections 132,142 (142A) to be parallel to each other.In a state in which the first reference line 21 and the third reference line 23 providedon the first long side 17 side are bumped against the bumping sections 142A, 142B, bybending the raw material 10 in a position closer to the second long side 18 than the first longside 17, the first reference line 21 and the third reference line 23 formed at high accuracy canbe used as a reference for positioning and a moving distance in moving the raw material 10to a press position can be set as small as possible. Therefore, it is possible to form anexternal dimension of the wall panel 30 at high accuracy.In this way, it is possible to manufacture the oblong wall panel 30 having anextremely small tolerance (machining error) in squareness between a short side bent surface(here, the first bent surface 31b) and long side bent surfaces (here, the third bent surface 34cand the fourth bent surface 33c). Therefore, when the wall section is configured, it ispossible to obtain high water-stopping action simply by fitting the dry joint filler 60 in thegap between the wall panels 30 disposed in parallel.A great technical significance (specifically, simplification and a reduction in cost ofthe manufacturing apparatus 100) is accomplished in that use of a rotating and movingapparatus in which an error of rotation and movement is large (accuracy is low) in the rotatingand moving unit 110 can be allowed in realizing the action effects described above, that is, inimproving machining accuracy (shape accuracy) of the wall panel 30.Note that, after the E2 step, necessary steps are carried out if necessary. As anexample, F1 and F2 steps for forming a corner portion of the raw material 10 into apredetermined shape with press working are carried out in a corner machining unit 114 (114A,114B). Subsequently, a G1 step of placing, on a terminal end section 116, the wall panel 30in a state in which the machining of the raw material 10 in the manufacturing apparatus 100ends and the raw material 10 is formed in a predetermined shape is carried out. Subsequently,an H1 step of conveying the wall panels 30 one by one from the line (here, the terminal endportion 116) into a stocker 118 using a conveying apparatus (not shown) such as a feeder andstacking and storing the wall panels 30 is caried out. However, steps carried out if necessaryare not limited to these steps. Other additional machining may be performed following theF2 step. Note that, in that case, a necessary mechanism may be provided in themanufacturing apparatus 100 to perform additional machining of the wall panel 30.Alternatively, additional machining may be performed after the wall panel 30 is conveyed(transferred) to another manufacturing apparatus (not shown).As explained above, with the method for manufacturing the wall panels according tothe present invention, it is possible to use, as a raw material, an inexpensive oblong platematerial, an angle tolerance of which in squareness at four corners is set relatively large, andmanufacture a wall panel having extremely high formation accuracy of an external dimension.Consequently, in a configuration in which not liquid resin but a solid dry joint filler is usedas a joint filler, it is possible to dramatically improve water-stopping performance in a gap inwhich the joint filler is fit. Therefore, when a wall section of a prefabricated bath isconfigured, facilitation of construction work is achieved and it is possible to achieve areduction in a work period and a cost reduction.Note that the present invention is not limited to the embodiment explained above andvarious changes are possible in a range not departing from the present invention. The wallpanel is suitably used when the wall section of the prefabricated bath is configured.However, it goes without saying that the wall panel can also be used when a wall section ofother than the wall section of the prefabricated bath is configured.
Claims
1. A method for manufacturing wall panels formed by a machining step of machining a plate material made of a metal material, to one surface of which a sheet made of a resin material is stuck, into a predetermined shape while line-conveying the plate material, disposed in parallel to and spaced a gap having a predetermined dimension from each other in a wall section of a prefabricated bath, and used in a state in which a solid dry joint filler is fit in the gap to thereby cause water-stopping action, the machining step including: an A1 step of preparing the plate material having an oblong shape, an angle tolerance of 0.5° or less of which that occurs at a cutting time is included in squareness at four corners; a B1 step of, after the A1 step, forming, at a first corner portion where a first short side and a first long side cross in the plate material, a cutout section including a first reference line serving as a reference position in bending the plate material along a bending line parallel to the first long side; a B2 step of forming, at the first corner portion, a cutout section including a second reference line serving as a reference position in bending the plate material along a bending line parallel to the first short side; a B3 step of forming, at a second corner portion where a second short side and the first long side cross in the plate material, a cutout section including a third reference line serving as a reference position in bending the plate material along the bending line parallel to the first long side; a C1 step of, after the B1 step, the B2 step, and the B3 step, bumping the second reference line against a bumping section and bending the plate material with press working in a position parallel to and separated a predetermined dimension from the second reference line to form a first bent surface; a C2 step of bumping the first bent surface against a bumping section and bending the plate material with the press working in a position parallel to and separated a predetermined dimension from the first bent surface to form a second bent surface; a D1 step of, after the C1 step and the C2 step, rotating the plate material 90° in an in-plane direction; an E1 step of, after the D1 step, bumping the first reference line and the third reference line against bumping sections respectively corresponding thereto and bending the plate material with the press working in a position parallel to and separated a predetermined dimension from the first reference line and the third reference line to form a third bent surface; and an E2 step of bumping the third bent surface against a bumping section and bending the plate material with the press working in a position parallel to and separated a predetermined dimension from the third bent surface to form a fourth bent surface, wherein the D1 step includes a process for rotating the plate material 90° with an error of 1° or less such that the first corner portion faces a start point side in a line conveying direction, and the E1 step includes a process for, when bumping the first reference line and the third reference line against the bumping sections respectively corresponding thereto, retracting the plate material toward the start point side in the line conveying direction to thereby perform the bumping and bending the plate material along a bending line parallel to the first long side and a second long side in a position closer to the second long side than the first long side.
2. A method for manufacturing wall panels formed by a machining step of machining a plate material made of a metal material, to one surface of which a sheet made of a resin material is stuck, into a predetermined shape while line-conveying the plate material, disposed in parallel to and spaced a gap having a predetermined dimension from each other in a wall section of a prefabricated bath, and used in a state in which a solid dry joint filler is fit in the gap to thereby cause water-stopping action, the machining step including: an A1 step of preparing the plate material having an oblong shape, an angle tolerance of 0.5° or less of which that occurs at a cutting time is included in squareness at four corners; a B1 step of, after the A1 step, forming, at a first corner portion where a first short side and a first long side cross in the plate material, a cutout section including a first reference line serving as a reference position in bending the plate material along a bending line parallel to the first long side; a B2 step of forming, at the first corner portion, a cutout section including a second reference line serving as a reference position in bending the plate material along a bending line parallel to the first short side; a B3 step of forming, at a second corner portion where a second short side and the first long side cross in the plate material, a cutout section including a third reference line serving as a reference position in bending the plate material along the bending line parallel to the first long side; a C1 step of, after the B1 step, the B2 step, and the B3 step, bumping the second reference line against a bumping section and bending the plate material with press working in a position parallel to and separated a predetermined dimension from the second reference line to form a first bent surface; a C2 step of bumping the first bent surface against a bumping section and bending the plate material with the press working in a position parallel to and separated a predetermined dimension from the first bent surface to form a second bent surface; a D1 step of, after the C1 step and the C2 step, rotating the plate material 90° in an in-plane direction; an E1 step of, after the D1 step, bumping the first reference line and the third reference line against bumping sections respectively corresponding thereto and bending the plate material with the press working in a position parallel to and separated a predetermined dimension from the first reference line and the third reference line to form a third bent surface; and an E2 step of bumping the third bent surface against a bumping section and bending the plate material with the press working in a position parallel to and separated a predetermined dimension from the third bent surface to form a fourth bent surface, wherein the B1 step includes a process for forming the cutout section with the press working using a first press mold including a first edge surface as an edge surface that forms the first reference line, and the B2 step includes a process for, after line-conveying the plate material in parallel to the first reference line formed by the B1 step with an error of 0.03° or less, forming the cutout section with the press working using a second press mold including, as an edge surface that forms the second reference line, a second edge surface formed at 90° with respect to the first edge surface with an angle tolerance of 0.05° or less.
3. The method for manufacturing the wall panels according to claim 2, wherein the B3 step includes a process for, after line-conveying the plate material in parallel to the first reference line formed by the B1 step with an error of 0.03° or less, moving the plate material in parallel to the second reference line formed by the B2 step with an error of 0.03° or less and forming the cutout section with the press working using the second press mold including, as an edge surface that forms the third reference line, a third edge surface formed at 90° with respect to the second edge surface with an angle tolerance of 0.05° or less.