Coated lightweight fabric, in particular for a spinnaker

IN607042BActive Publication Date: 2026-10-26PORCHER INDUSTRIES
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
IN202317023280
Authority / Receiving Office
IN · IN
Patent Type
Patents
Current Assignee / Owner
Priority Date
2020-10-05
Filing Date
2023-03-29
Publication Date
2026-10-26
Estimated Expiration
2041-10-04

AI Technical Summary

Technical Problem

Existing lightweight sail fabrics, such as those used in spinnakers, face issues with tear resistance, water absorption, hydrolysis resistance, stiffness, and durability, particularly when made from polyamide 6.6 or high tenacity polyester fibers, which lead to premature aging and aerodynamic performance degradation.

Method used

A lightweight fabric formed from high tenacity continuous polyester warp and weft yarns coated with crosslinked polyurethane, specifically a polycarbonate-based PU, which balances stiffness and elasticity to enhance tear resistance and hydrolysis resistance, allowing for durable decoration and improved aerodynamic performance.

Benefits of technology

The fabric achieves improved tear resistance, reduced water absorption, and enhanced hydrolysis resistance, enabling its use in lightweight sail applications while maintaining necessary flexibility and thermal stability for sublimation printing.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention relates to a fabric for lightweight nautical sails for sailboats and other surface vessels, such as spinnakers, asymmetric spinnakers, and gennakers, the fabric being formed from warp yarns and continuous weft yarns made of polyester and being coated on one or both faces with a crosslinked polymer, characterized in that the polyester is polyethylene terephthalate (PET) having a tenacity of 6 cN / dtex or more, in that the fabric has a density of between 20 and 50 yarns / cm in warp and weft, in that the polymer is a polyether-, polyester- or polycarbonate-based cross-linked polyurethane (PU), and in that said PU is derived from the cross-linking (1) of a one-component polyurethane elastomer having a modulus at 100% elongation of between 1 and 15 MPa, better still between 2 and 15 MPa, in particular between 6 and 15 MPa, according to standard DIN 53504, carried out in a solvent phase, and (2) by a cross-linking agent, with a proportion of dry cross-linking agent relative to dry elastomer of between 20% and 75% by weight, in particular between approximately 30 and approximately 75%. The coated fabric has a bias extension at 20 Lbs of between 10 and 30 1 / 100 inch.
Need to check novelty before this filing date? Find Prior Art

Description

The present invention relates to a lightweight fabric formed of continuous warpyarns and weft yarns, this fabric being coated on one and / or both of its two surfaceswith a polyurethane. The field of application for this lightweight fabric in particularincludes lightweight headsails, such as spinnakers, asymmetric spinnakers, andgennakers, for sailboats and other surface vessels. The invention also relates to afabric production method for producing this fabric.A spinnaker, upon being inflated by the wind, must have a very preciseaerodynamic form. The use of a stiff fabric is thus preferred in order to facilitateinflation and maintenance of the ideal shape and form. The stiffness of the fabrichas the downside in that fabrics so obtained are conducive to tearing under highstress, causing the spinnaker to break up or burst. Traditionally, the use of fabricsmade of Polyamide 6.6 based textile is preferred, given the shock absorbing abilitythereof attributable to the high elasticity and tenacity of polyamide 6.6. Howeverthis polyamide has certain drawbacks. Polyamide 6.6 is a hydrophilic polymerwhich provides the fibre with a propensity to absorb water. A spinnaker made froma polyamide 6.6 based fabric thus then has a tendency to become heavier and toage prematurely under the combined action of UV rays and hydrolysis. For theirpart, polyester based fabrics, that are less sensitive to water uptake, have provedin practice to be too stiff to be able to be used on sails such as spinnakers. Theuse of high tenacity polyester fibres, preferably polyethylene terephthalate fibres,supposed to provide even greater tear resistance, has not in practice resulted inuse thereof in spinnakers, the considerable stiffness of the sails thus producedrendering them prone to breaking up and bursting under high stresses.Another deficiency in fabrics for spinnakers is that they are not suitable forreceiving a durable decoration, in particular by modern printing techniques, afterthe sail has been fabricated.The objective of the present invention is to remedy the drawbacks of the prior art,by providing a fabric formed from polyester fibres that exhibits a tear resistance,and has a modulus and elasticity that enable use thereof in the production and useof lightweight headsails, such as spinnakers, asymmetric spinnakers, andgennakers, for sailboats and other surface vessels.Another objective of the invention is to provide such a fabric having lower waterabsorption, and exhibiting greater hydrolysis resistance, than the existing solutionsbased on polyamide fabric.Another objective of the invention is to provide a fabric that has high thermalstability which makes it possible for the fabric to be sublimation printed.Still other objectives will become apparent upon reading the description of theinvention.These and other objectives are achieved by a fabric formed from high tenacitycontinuous polyester warp and weft yarns. The fabric is coated on one or both ofits two surfaces with a crosslinked polyurethane (PU). The crosslinked PUaccording to the invention has the ability to compensate for the excessive stiffness(extremely high modulus) and the low elasticity of fabrics made of high tenacitypolyester fibres. Crosslinked polyurethane is flexible and is therefore durableagainst the mechanical stresses that the sail is subjected to during its useful life.Preferably, the polyurethane is a polyether-, polyester-, or polycarbonate basedPU. The preferred polyurethane is a polycarbonate based PU. According toanother preferred characteristic feature, the PU is obtained from a singlecomponent polyurethane elastomer. This elastomer is formed from polyolsegments (polyether, polyester or polycarbonate), isocyanate segments, and achain extender or hydroxylated crosslinking agent, as is known per se. Oneimportant preferred characteristic feature is that the elastomer has a modulus at100% elongation less than or equal to approximately 15 MPa, in particularcomprised between 1 and 15 MPa according to the standard DIN 53504. Moreadvantageously, this modulus is comprised between 2 and 15 MPa, in particularbetween 6 and 15 MPa, indeed more particularly between 6 and 10 MPa, typicallybetween 6 and 9.5 MPa, for example approximately 8 MPa, according to thestandard DIN 53504. Another important preferred characteristic feature is that theelastomer is in a mixture with a crosslinking agent (not to be confused with thecrosslinking agent used so as to form the elastomer), and that the proportion of drycrosslinking agent relative to the dry elastomer is between approximately 20% andapproximately 75%, better still between approximately 30% and approximately75% by weight, in particular between approximately 40% and approximately 75%by weight, in particular between approximately 50% and approximately 75% byweight (for example, approximately 67%). The crosslinking agent comprises inparticular an isocyanate, melamine, or a mixture of isocyanate and melamine. Thiscrosslinking agent makes it possible in particular to block all or part of the reactivefunctional groups (in particular NCO and alcohol) remaining on the elastomer, tocreate additional bonds or crosslinks, and to obtain the crosslinked PU forming thecoating of the fabric. The fabric according to the invention is intended for, orcapable of forming, the lightweight headsails, such as spinnakers, asymmetricspinnakers, and gennakers, for sailboats and other surface vessels.The invention relates in particular, to a fabric for lightweight nautical sails, such asspinnakers, asymmetric spinnakers, and gennakers, for sailboats and othersurface vessels the fabric being formed of continuous polyester warp and weftyarns and being coated on one or both of its two surfaces with a crosslinkedpolymer, characterised in that the polyester is poly(ethylene terephthalate) (PET);in that the fabric has a density of between 20 and 50 threads / cm, preferablybetween 25 and 50 threads / cm, in terms of warp and weft density; in that thepolymer is a crosslinked polyurethane (PU) that is polyether-, polyester-, orpolycarbonate based, preferably polycarbonate based; and in that this PU isderived from the crosslinking (1) of a single-component polyurethane elastomerhaving a modulus at 100% elongation less than or equal to approximately 15 MPa,in particular comprised between 1 and 15 MPa, in particular between 2 and 15MPa, more particularly still between 6 and 15 MPa, typically between 6 and 10MPa, for example between 6 and 9.5 MPa, for example approximately 8 MPaaccording to the standard DIN 53504, used in implementation in organic solventphase (in particular dissolved in a solvent); (2) by a crosslinking agent, based on aproportion of dry crosslinking agent relative to the dry elastomer of betweenapproximately 20% and approximately 75% by weight, better still betweenapproximately 30% and approximately 75% by weight, in particular betweenapproximately 40% and approximately 75% by weight, in particular betweenapproximately 50% and approximately 75% by weight.Advantageously, the coated fabric has an elongation in the bias direction under 20lbs, comprised between 10 and 30 hundredths of an inch, preferably between 14and 25 hundredths of an inch, according to the standard NF EN ISO 13934-1. Thecombination of the 100% elongation modulus of the PU and the proportion ofcrosslinking agent, each taken within the given intervals, provides the ability inparticular to obtain this elongation in the bias direction, making it possible toprovide the flexibility to the fabric that is necessary for the application but which byno means could have been anticipated given the intrinsic tenacity of the PET yarn.The high range of modulus values may in particular be favoured when theproportion of crosslinking agent is in the lower range of values, and vice versa.The rate of dry coating relative to the total dry fabric may be in particular greaterthan 5%, in particular between 5% and 30% by weight, in particular between 10%and 30% by weight, better still between 15% and 25% by weight. The rate of drycoating is the ratio by weight of dry coating (crosslinked PU) on the coated fabric;it is representative of the weight of the dried / crosslinked coating present on thefinal fabric. The rate of dry coating mentioned herein is understood to refer to thetotal rate of coating, either on one surface or on two surfaces, as the case may be.Preferably, the polyester is poly(ethylene terephthalate) or PET. PET is made upof repeating units of ethylene terephthalate; however, the scope of the inventionindeed also extends to variants comprising a minor amount of other units, forexample less than 10 mol%, in particular less than 5 mol% of other units, permolecular chain of the polyester (in order to form these other units the comonomersinclude, for example, isophthalic acid, naphthalene dicarboxylic acids, adipic acid,hydroxybenzoic acids, diethylene glycol, propylene glycol, trimellitic acid, andpentaerythritol).The polyester yarns are multifilament yarns. They are formed from multiplecontinuous filaments. According to one embodiment, the fabric comprises warpyarns and weft yarns which have a dtex of between 11 and 235 dtex, for examplebetween 22 and 110 dtex, in particular between 22 and 78 dtex, in particular witha DPF (decitex per filament) of between 1 and 4, preferably between 1.3 and 3.5.The tenacity of the PET yarns is in particular greater than or equal to 6 cN / dtex, inparticular between 6 and 7 cN / dtex. The elongation at break thereof is in particulargreater than or equal to 20%, in particular between 20 and 30%. The tenacity andelongation at break are measured according to the standard DIN EN ISO 2062.PET fibres or yarns having these characteristic features are commercially availableand / or can be produced to order.The polyester fibres optionally contain one or more additives, for example astabilising agent and / or an antistatic agent.One important preferred characteristic feature is that the bare fabric has a weftdensity of between 20 and 50 threads / cm, preferably between 25 and 50threads / cm, and a warp density of between 20 and 50 threads / cm, preferablybetween 25 and 50 threads / cm. Preferably, the yarn warp density is identical to theweft density. By way of a variant, the warp density may be different from the weftdensity, in particular with a 10 to 30% variation between warp and weft, with eitherthe warp or weft density having a higher value, preferably the warp density.In one embodiment, the fabric has a hybrid construction, making use of fibres oryarns with different counts between the warp and the weft. The fabric may thusthen include warp yarns and weft yarns which have a dtex (count) of between 11and 235 dtex, in particular between 22 and 110 dtex, in particular between 22 and78 dtex, with the warp yarns having a higher count than the weft yarns. By way ofa variant that is not preferred, it is the weft yarns that have a higher count. Theterm 'higher' in particular may be understood to indicate that the yarn count in onedirection is 1.5 or 2 to 5 times higher than the yarn count in the other direction.The weight of the coated fabric may in particular be between 25 and 130 g / m²,preferably between 30 and 120 g / m².The fabric of the present invention is characterised by stiffness in the bias direction.The bias is said to be the warp direction because it is measured along the directionat 45° to the warp yarns. This stiffness in the bias direction is expressed by theelongation in hundredths of inches, which is measured under a force of 20 pounds(Lbs, which is 89N) applied along the bias. This elongation characterises thestiffness of the fabric in the bias direction. The standard used is NF EN ISO 13934-1: test specimens measuring 76.2 mm in width and 300 mm in length are produced.The clamp jaws of the dynamometer are moved away from each other by 152.4mm and the measurement is performed at a speed of 50 mm / min. In the biasdirection, the test specimens are cut from the fabric according to these dimensions,by applying an angle of 45° relative to the warp direction of the fabric, then the twopieces of fabric are superimposed and subjected together to the effect of thedynamometer. The elongation in hundredths of inches in the warp and weftdirections is carried out according to the same standard, and in this case a singlepiece of fabric is used.The elongation in the bias direction of the coated fabric, under 20 lbs, in particularmay be between 10 and 30 hundredths of an inch, preferably between 14 and 25hundredths of an inch. This is the preferred target as established by the invention.The flexible polyurethane coating makes it possible to achieve this goal, despitethe fact that the PET yarns having high Young's modulus, generally between 3 andGPa, confer on the fabric high stiffness and low elasticity. A coated fabric with20 a bias elongation of less than 10 hundredths of an inch will be too stiff and wouldrisk bursting under high stress. A fabric with a bias elongation greater than 30hundredths of an inch will be too flexible or soft and will result in a sail, such as aspinnaker, having degraded aerodynamic performance.The Young's modulus or modulus of elasticity characterising polyester or PETfibres or yarns is the pascal constant which links the stress and the deformationgenerated by this stress when one is within the elastic range of the material. It isobtained by measuring the slope at the origin of the force=f(deformation) curve.The elongation at break is (L-L0) / L0*100, L being the length at break and L0 theinitial length of the sample.The modulus at 100% elongation as used to characterise the elastomer is nolonger the Young's modulus but an equivalent measured at 100% elongation.The fabric of the present invention is obtained by coating with polyurethane insolvent phase. The coating may have any one of the characteristic featuresmentioned below. Firstly, the fabric may be coated on one or both sides, preferablyit is coated on one side.A polyurethane includes a stiff part (isocyanate) and a flexible part (polyol). Theperson skilled in the art knows how to find the compromise between theisocyanate / polyol ratio and the nature of the components in order to obtain theelastomer of the desired stiffness, characterised by the modulus at 100%elongation. Preferably, the elastomer used in the coating is a single componentelastomer, the isocyanate having reacted with the polyol, then with the chainextender or the crosslinking agent, forming an elastomer generally still containingreactive functional groups such as NCO and alcohol. The person skilled in the artmay refer to the literature on the production of copolymers or elastomers obtainedfrom isocyanate, polyol, and chain extenders or crosslinking agent, in particular tothe These en Materiaux Polymeres et Composites [Thesis on Polymer Materialsand Composites] by Segolene Hibon, Institut National de Sciences AppliqueesINSA [National Institute of Applied Sciences) in Lyon, France, 2006.The coating composition is supplemented by a crosslinking agent, in particular anisocyanate or a melamine, or even a mixture of the two. The term "isocyanate" isunderstood to refer to both an isocyanate and a polyisocyanate, either alone or asa mixture with one or more other isocyanates and / or polyisocyanates. Unlessotherwise indicated, the term "isocyanate" should be understood herein asincluding the terms "isocyanate" and "polyisocyanate". Polyisocyanates arepreferred. As regards the melamine, it may in particular be melamine proper (1,3,5-triazine-2,4,6-triamine) or a compound or a resin containing melamine, for examplea melamine-formaldehyde resin.According to one embodiment, the proportion of dry crosslinking agent relative tothe dry elastomer is between approximately 20% and approximately 75% byweight, better still between approximately 30% and approximately 75% by weight,in particular between approximately 40% and approximately 75% by weight, inparticular between approximately 50% and approximately 75% by weight.According to one embodiment, the polyurethane (and the starting elastomer) ispolyether-based. In particular, the polyether-based polyurethane is linear orbranched and comprises a polyol part of the polyether type and an isocyanate part.According to one embodiment, the polyurethane (and the starting elastomer) ispolyester-based. In particular, the polyester-based polyurethane is linear orbranched and comprises a polyol part of the polyester type and an isocyanate part.According to another embodiment, the polyurethane (and the starting elastomer)is polycarbonate-based. In particular, the polycarbonate-based polyurethane islinear or branched and comprises a polyol part of the polycarbonate type and anisocyanate part. A polycarbonate-based polyurethane is used in the examples andconstitutes a particularly suitable embodiment.As regards the elastomer and the crosslinking agent, the isocyanate part ispreferably aliphatic, in fact aromatic isocyanates have the drawback of turningyellow over time, thereby making them less preferred, even though they can beused.In one embodiment, the lightweight fabric of the present invention is obtained bycoating with polyurethane in solvent phase. This fabric production method forproducing a coated fabric from the polyester fabric is another object of theinvention. The coating may have any one of the characteristic features mentionedbelow.The coating step is carried out by the techniques conventionally used in the coatingof textiles, such as direct coating. The term "direct coating" is understood to referto a direct deposition coating process, for example making use of a doctor blade,a cylinder, an air knife, a padder, using the Meyer rod (or Champion process).Another object of the invention is the use of a PU elastomer or a crosslinked PUcoating as defined herein, for the coating of a high tenacity PET fabric as definedherein. This coating is intended in particular to give the fabric the property orproperties described herein, in particular an elongation in the bias direction asdescribed herein. The coating also provides a level of porosity appropriate to theuse for which the fabric is intended. This use may result in the production methodthat follows, which is another object of the invention.The fabric production method for producing the coated fabric includes in particularthe following steps:(a) a polyester fabric according to the invention is provided;(b) one or both of the two surfaces of this fabric is / are coated making use of apolyurethane in solvent phase according to the invention, preferably from asingle-component elastomer dissolved in the solvent and in a mixture withthe crosslinking agent, as described herein, with a rate of coating inaccordance with the invention;(c) the fabric is heated until drying and crosslinking of the coating,(d) a coated fabric in accordance with the invention is obtained;(e) optionally, the fabric is printed, for example by sublimation, on one or bothof its two surfaces.The object of the invention relates in particular to a fabric production method forproducing the coated fabric in which:- a fabric is provided, the fabric made of poly(ethylene terephthalate) (PET)having a density of between 20 and 50 threads / cm, preferably between 25and 50 threads / cm, in terms of warp and weft density;- one or both of the two surfaces of this fabric is / are coated making use of amixture of: a single-component polyurethane elastomer having a modulusat 100% elongation as described above; a solvent for the elastomer; and acrosslinking agent; based on a proportion of dry crosslinking agent relativeto the dry elastomer as described above;- the fabric is heated until drying and crosslinking of the coating;- a coated fabric is obtained;- optionally, the fabric is printed, for example by sublimation, on one or bothof its two surfaces.This method is aimed at producing a fabric as described above and consequently,the characteristic features of the elements that are used in the production of thefabric and its coating are applicable to the method, to the selection of theseelements for use thereof in the method, without having to repeat them in thefollowing sections.In particular, the drying and crosslinking step comprises firstly the drying, forexample at a temperature of between approximately 90 and approximately 120°C,thereafter the crosslinking at a temperature of between approximately 140 andapproximately 210°C.In one embodiment, the method includes after the step of drying and crosslinkingone or more post-treatment step(s) that confer on the fabric anti-fouling and / orwater-repellent properties. The term "anti-fouling" treatment is understood to referto a treatment making use of anti-static and / or anti-tack products. The term "waterrepellent" treatment is understood to refer a treatment making use of fluorinatedresins with or without a crosslinking agent for the fluorinated resin, for example anisocyanate. The water-repellent treatment is followed by a drying / crosslinking step.In one embodiment, the post-treatment is applied by any method known to theperson skilled in the art and in particular by padding, coating, spraying or plasmatreatment. It is also possible to carry out a treatment with silicone in order toameliorate the slipperiness of the fabric.According to one embodiment, prior to coating, the fabric is calendered.Calendering crushes the fabric and spreads the yarns as well as the constituentfilaments, which contributes to closing the pores of the fabric and reducing theporosity thereof. According to one embodiment, the calendering is carried outbetween a tool, cylinder or calender roller and a counter plate. The surface of thefabric which has been subjected to the passing of the calendering tool, referred toas the "calendering surface", is smoothed as compared to the other surface.According to one method, the coating is effected on this calendering surface. Theadhesion of the polymer can be enhanced by first applying in advance a primertreatment to this smooth surface. It may be a physical treatment or a chemicaltreatment known as an adhesion treatment. It is for example a chemical treatmentproviding functional groups capable of reacting with the groups of the polymer inorder to form chemical bonds.According to another modality, the coating is effected on the other surface, whichis not smoothed. It should be understood that the rate of dry coating variesdepending on the surface concerned, this rate being higher on the non-smoothedsurface, which enables a person skilled in the art to adjust the quantity and theweight of the coating. It is also possible to coat both surfaces.According to another embodiment, the calendering is carried out between twotools, cylinders or calender rollers. Both surfaces of the fabric are smoothed. Oneor both of the two surfaces are subsequently coated, with or without an adhesiontreatment as described above.The calendering is preferably carried out at a temperature of betweenapproximately 150 and approximately 250°C, preferably between approximately180 and approximately 210°C. The calendering is preferably carried out with apressure ranging from approximately 150 to approximately 250 kg, preferablybetween approximately 180 and approximately 230 kg. The rotational speed of thecalender may be between approximately 1 and approximately 30 m / min, preferablybetween approximately 10 and approximately 20 m / min.The fabric of the present invention is obtained by coating with polyurethanedissolved in a solvent. In particular, the coating contains the single-componentelastomer (formed in particular from isocyanate, polyol and the chain extender orthe crosslinking agent), in solution in the solvent. The film forms naturally duringthe evaporation of the solvent. The solvent is an organic solvent and may inparticular be selected from the group constituted of aromatic solvents, alcohols,ketones, esters, dimethylformamide, and n-methylpyrolidone. In one particularembodiment, the solvent is selected from the group constituted of toluene, xylene,isopropanol, butanol, 1-methoxypropan-2-ol, methyl ethyl ketone, acetone,butanone, ethyl acetate, dimethylformamide, n-methylpyrolidone, and a mixture ofat least two of the afore-mentioned. For example, a mixture of toluene andisopropanol.In one embodiment, the solvent-phase polyurethane may be characterised by itsconcentration of between 20% and 50% by weight of non-crosslinked PU, inparticular a single-component elastomer, relative to the PU and solvent mixture. Inone embodiment, this solvent-phase polyurethane, in particular the elastomer insolution in the solvent, may be characterised by a viscosity of less than 100,000mPa.s at 23°C, preferably between 5,000 and 60,000 mPa.s at 23°C (according tothe standard DIN EN ISO / A3).Consequently, in one embodiment, the lightweight fabric of the present inventionis obtained or can be obtained by coating with polyurethane, preferably a singlecomponent polyurethane elastomer, in solvent phase.The fabric coating composition of the present invention may in addition includeadditives. The said additives may be any additive commonly used in fabric coatingcompositions. They are in particular selected from the group constituted ofviscosity modifiers, UV stabilisers, dyes, dispersants, and surfactants. Accordingto one embodiment, the coating comprises an anti-UV agent.The coated fabrics described herein are found to be capable of being printed bythe so-called sublimation printing technique. According to one aspect of theinvention, this coated fabric is coloured, printed or decorated by a sublimationtechnique. This latter may in particular be implemented by printing a pattern on asubstrate (transfer substrate) with one or more dyes which can be sublimated athigh temperature. The substrate is thereafter applied in contact with the coatedfabric, then hot calendered, for example at approximately 200°C and underpressure. The dyes pass into the gas phase and are transferred into the coating,and / or to the surface and / or to the fibre. The polyester PET remains stable at thistemperature.Spinnakers (standard or asymmetric) and gennakers are inflatable wind sails,which typically include three angular peaks, commonly referred to as head orhalyard point, clew point, and tack point. These sails are obtained by assemblingfabric widths, in particular several radial widths which open out from each angularvertex, each radial width being obtained beforehand in the form of a planar fabriccutting, cut according to the geometric needs of the width to be obtained.The object of the invention thus relates to an article such as a headsail for sailboatsand other surface vessels, for example a spinnaker, asymmetric spinnaker, andgennaker, which comprises a coated fabric according to the invention or is madefrom one or more fabric(s) or fabric width(s) coated according to the invention. Inparticular, the article may comprise multiple fabrics or fabric widths according tothe invention, assembled so as to form the article in question. In one embodiment,the nautical sail bears a pattern that is sublimation printed. In particular the nauticalsail bears a pattern formed with dye within the PU coating and / or on the surface orwithin the PET yarns.The object of the invention thus also relates to the said fabric widths cut from afabric according to the invention.The invention will now be described with the aid of examples corresponding to thepreferred embodiments, these being provided by way of illustration withouthowever any limitation whatsoever.Example:Example 1: This example compares the impact of a polyurethane coating onconventional polyamide 6.6 fabrics coated with PU (Control) and high tenacitypolyethylene terephthalate (PET) fabrics coated on one surface with a PUaccording to the invention.PA6.6 is a conventional polyamide fabric in the spinnaker industry, with a PUcoating obtained from PU elastomer having a 100% elongation modulus of 32.4and melamine formaldehyde crosslinking agent. The proportion of dry crosslinkingagent relative to the dry elastomer is 104%. The PU is used in a 50 / 50 mixture oftoluene and isopropanol.The PET has a PU coating obtained from PU elastomer having a 100% elongationmodulus of 8, and melamine formaldehyde crosslinker. The proportion of drycrosslinking agent relative to the dry elastomer is 66.9%. The PU is used in a 50 / 50mixture of toluene and isopropanol.The tenacity of PET is 6.8 cN / dtex. The elongation at break is 24.6%.The coating is effected by using a doctor blade, and is followed by a step of dryingat 100°C, and then a step of crosslinking at 170°C. The speed is 27 m / min.[Table 1][Table 2]The fabric of the invention from Example 1 made of 33 dtex yarns is taken andcompared with counter-examples 1 and 2, which differ therefrom by combinationsof the modulus of the PU and proportion of crosslinking agent which are outsidethe limits of the invention.[Table 3]Methods and measurements used in the application (characteristic featuresof the invention and examples):NF EN ISO 2062 - Determination of the breaking strength and elongation at breakof individual yarns making use of a constant rate of elongation test apparatus, usingMethod A of the standard.Breaking force (unit centiNewton - cN): maximum force developed to break thesample during a tensile test leading to breakageElongation at break (%): increase in the length of the sample measured at breakingof the latterTenacity (cN / tex): quotient of the breaking force expressed in cN by the lineardensity of the yarn expressed in dtex (1 tex = 1 g per 1000 m of yarn length).The test makes it possible to measure the force and the elongation at break of thesample, characteristic variables of the yarn.The yarn is placed between two fixing clamps, spaced apart by 500 mm. Theapparatus (Dynamometer) then moves the clamps away from each other at aconstant displacement speed of 500 mm / min and measures the applied forcecontinuously. The force required to break the yarn is measured as well as theincrease in length of the yarn upon breaking.The mean breaking strength and mean elongation at break are the two data itemscharacterised by this test. The tenacity is calculated based on dividing the breakingforce by the linear density.The modulus at 100% elongation of the single-component polyurethane elastomeris measured according to the standard DIN 53504. The modulus is defined in 3.4of the standard "Spannungswerte". The measurement is carried out on testspecimens that are dumbbell-shaped (Schulterstab) of type S2, however with a barlength lS of 55 mm and a thickness of 200 μm. The equipment used is adynamometer. The dumbbell specimen is placed in the fixing clamps, spaced apartby a length L0 with the minimum possible pre-tension. The clamps are then movedaway from each other at a constant speed of 400 mm / min and the dynamometermeasures the force applied as a function of the elongation. The modulus or stressat 100% elongation in MPa is the force ratio measured at 100% elongation on theinitial section of the specimen. This is described in paragraph 9.4 Spannungswerteof the standard DIN 53504.The elongations of the fabric are measured according to the standard NF EN ISO13934-1, as described in the general description. The lesser elongation in thedirection of the warp and weft yarns due to the polyester nature is compensatedby a greater elongation in the bias (measured herein in the warp direction). Thiselongation in the bias effectively serves to compensate for the excessive rigidity ofthe PET and enables avoiding the risks of breaking and bursting under highstresses. The mechanical performance results are equivalent or indeed evensuperior, this consequently leads to a polyester fabric that is suitable for use inspinnaker production.The absorption of water by the coated fabric of Example 1 was measuredaccording to the standard Tappi 441 om-90. One measurement was performed onthe new coated fabric, with another performed post aging. The measurement isexpressed in percentage. The equipment consists of a square rubber substrateand a metal ring clad at its base with a rubber gasket. The sample is placed on thesquare substrate and the metal ring is placed on the sample. A clamping device isused to make the system watertight. A certain quantity of water (100 ml) is placedin the ring, in contact with the sample for a determined time (1 minute). When thetime has elapsed, the water is removed from the cylindrical ring, the water residueremaining on the surface of the sample is removed by using a cylinder as describedin the standard, via a to-and-fro movement of this cylinder over the sample placedbetween two blotters, without applying pressure. The percentage of waterabsorbed is determined by calculating the difference in weight before and after thecontact with water.For the aging, the fabric is placed for 4 hours in a 'Cocotte Minute' pressure cookerwith salted water (30 g / l) at operating temperature and pressure. Subsequently 1hour of treatment is applied by floating the fabric in open air and at high speed, thefabric being fixed to a mill-type assembly (4 blade assembly, the fabric being fixedto the end of one of the blades).It is thus demonstrated that the fabric according to the invention undergoespractically no unfavourable evolution in terms of its water absorption after aging.This level of resistance to water uptake is another surprising positive result.

Claims

1. A fabric for lightweight nautical sails, such as spinnakers, asymmetric spinnakers, and gennakers, for sailboats and other surface vessels, the fabric being formed of continuous polyester warp and weft yarns and being coated on one or both of its two surfaces with a crosslinked polymer, characterised in that the polyester is poly(ethylene terephthalate) (PET); in that the PET has a tenacity greater than or equal to 6 cN / dtex, in particular between 6 and 7 cN / dtex; in that the fabric has a density of between 20 and 50 threads / cm, preferably between 25 and 50 threads / cm, in terms of warp and weft density; in that the polymer is a crosslinked polyurethane (PU) that is polyether-, polyester-, or polycarbonate based; and in that this PU is derived from the crosslinking (1) of a single-component polyurethane elastomer having a modulus at 100% elongation comprised between 1 and MPa, more advantageously comprised between 2 and 15 MPa, in particular between 6 and 15 MPa, indeed more particularly between 6 and MPa, typically between 6 and 9.5 MPa, according to the standard DIN 53504, used in implementation in solvent phase; (2) by a crosslinking agent, based on a proportion of dry crosslinking agent relative to the dry elastomer of between 20% and 75 % by weight, in particular between 30% and 75% by weight, in particular between approximately 50% and approximately 75% by weight.

2. A fabric according to claim 1, characterised in that the coated fabric has an elongation in the bias direction under 20 lbs, comprised between 10 and 30 hundredths of an inch, preferably between 14 and 25 hundredths of an inch, measured on test specimens measuring 76.2 mm in width and 300 mm in length according to the standard NF EN ISO 13934-1.

3. A fabric according to claim 1 or 2, characterised in that the fabric comprises warp yarns and weft yarns which have a count of between 11 and 235 dtex, in particular between 22 and 110 dtex, more particularly between 22 and 78 dtex, with a DPF (decitex per filament) of between 1 and 4, preferably between 1.3 and 3.5.

4. A fabric according to any one of the preceding claims, characterised in that the PET has an elongation at break greater than or equal to 20%, in particular between 20 and 30%, according to the standard DIN EN ISO 2062.

5. A fabric according to any one of the preceding claims, characterised in that the rate of dry coating of crosslinked PU relative to the total dry fabric is greater than 5% by weight, in particular between 5% and 30% by weight, preferably between 10% and 30% by weight, better still between 15% and 25% by weight.

6. A fabric according to any one of the preceding claims, characterised in that the weight of the coated fabric is between 25 and 130 g / m², preferably between 30 and 120 g / m².

7. A fabric according to any one of the preceding claims, characterised in that the crosslinking agent of the elastomer is an isocyanate, a polyisocyanate, melamine, a compound comprising melamine, or a mixture of isocyanate and melamine.

8. A fabric according to any one of the preceding claims, characterised in that the isocyanates or polyisocyanates, and / or the crosslinking agent are aliphatic.

9. A lightweight nautical sail, in particular a spinnaker, asymmetric spinnaker, or gennaker, comprising a fabric according to any one of claims 1 to 8, or formed by the assembling of multiple fabrics according to any one of claims 1 to 8.

10. A lightweight nautical sail according to claim 9, characterised in that it bears a pattern that is sublimation printed.

11. A fabric production method for producing the coated fabric according to any one of claims 1 to 8, that includes the following steps: - a fabric is provided, the fabric made of poly(ethylene terephthalate) (PET) having a density of between 20 and 50 threads / cm, preferably between 25 and 50 threads / cm, in terms of warp and weft density; and the PET has a tenacity greater than or equal to 6 cN / dtex, in particular between 6 and 7 cN / dtex; - one or both of the two surfaces of this fabric is / are coated making use of a mixture of: a single-component polyurethane elastomer having a modulus at 100% elongation less than or equal to approximately 15 MPa, in particular comprised between 1 and 15 MPa, better still between 2 and 15 MPa, in particular between 6 and 15 MPa, in particular between 6 and 10 MPa, typically between 6 and 9.5 MPa, according to the standard DIN 53504; a solvent for the elastomer; and a crosslinking agent; based on a proportion of dry crosslinking agent relative to the dry elastomer of between approximately 20% and approximately 75% by weight, in particular between approximately 30% and approximately 75% by weight, in particular between approximately 50% and approximately 75% by weight; - the fabric is heated until drying and crosslinking of the coating; - a coated fabric is obtained; - optionally, the fabric is printed, for example by sublimation, on one or both of its two surfaces.