A biomaterial-based composition and a method of preparation thereof
Patent Information
- Application Number
- IN202311065055
- Authority / Receiving Office
- IN · IN
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2023-09-27
- Publication Date
- 2026-10-27
- Estimated Expiration
- 2043-09-27
AI Technical Summary
Current bone cements used in orthopaedic surgeries, such as PMMA-based cements, face issues like generation of free radicals during polymerization, lack of adhesion to bone tissue, biofilm formation, and toxicity, leading to infections and poor mechanical qualities, along with limited biocompatibility and superoxide dismutase activity.
A biomaterial-based composition incorporating mangiferin (MG) into Bone Cement, with mangiferin loaded at concentrations of 5%, 7.5%, and 10%, which is extracted from mango tree bark and incorporated through free radical polymerization, enhancing superoxide dismutase activity and free radical scavenging capabilities while reducing cell toxicity and improving cell adhesion and viability.
The mangiferin-loaded Bone Cement composition demonstrates reduced free radical release, improved cell viability, and enhanced biocompatibility, acting as a potent free radical scavenger for prosthetic implants, thereby addressing the limitations of existing bone cements.
Abstract
Description
FIELD OF THE INVENTIONThe present invention relates to a biomaterial-based composition. More particularly, the present invention relates to a biomaterial-based composition and a method of preparing the same for prosthetic implants with superoxide dismutase activity and free radical scavenging behaviour.BACKGROUND OF THE INVENTIONBone Cement is a filler that is used in orthopaedic surgery to fill the gap or free space left between the bone and prosthetic implant. It is implanted in the form of a paste, having ability to solidify once implanted within the body. Bone Cement is provided herein as a two-component material. Bone Cement consists of a powder polymethyl methacrylate (PMMA) or methyl methacrylate (MMA) co-polymer beads or amorphous powder, radio-opacifier, initiator and a liquid, i.e., MMA monomer, stabilizer and inhibitor. It is prepared by mixing both the powder phase and the liquid phase. Bone Cement is one of the most common materials utilized as a prosthetic biomaterial in the medical industry. However, in spite of several advancements, Bone Cement shows failure in orthopaedic surgeries. The main reasons for failure are generation of free radicals during PMMA polymerization in situ, inability to anchor to bone tissues, unambiguity in drug loading and releasing behaviour and formation of biofilm over implants. Moreover, owing to inertness of PMMA, it is not adhesive to the bone tissue, which successively generates a gap that offers site for bacterial colonization and infections. PMMA-based bone cement consists of two phases, solid and liquid. In the solid phase, pre-polymerized PMMA particle is present along with benzoyl peroxide as an initiator, while the liquid phase consists of MMA monomer with N, N- dimethyl-p-toluidine as an activator. The generated benzoyl and benzoate free radicals during in situ polymerization at high exothermic temperature causes significant toxicity. These free radicals behave as an inflammatory mediator and shows cytotoxicity-induced cell death. These free radicals also induce lipid peroxidation and impairment in antioxidant enzyme activities and cause intraoperative morbidity and mortality. The oxidative stress induced by these free radicals causes cancer, osteoporosis and coronary heart diseases. CN107496413A discloses an application of mangiferin for promoting bone defect repair and solves the problems of short blood supply of the host micro-environment in a conventional bone repair mode, apoptosis of seed cells in an anaerobic environment, the poor ossifying effect wherein, using mangiferin for the protection of seed cell can help in promoting the endochondral ossification system for bone repair. Further, the drug-loading system in this document is nano controlled-release microballoon or mangiferin is carried on porous bone repairing support. The porous bone repairing support is decalcified / undecalcified bone matrix, or the artificial synthesized bone defect repair that is used for porous support materials. However, the porous bone repairing support, i.e., the decalcified / undecalcified bone matrix remove the calcium salts from the mineralized tissue using chemical solutions which hinders the process of bone repairing. CN114288296A discloses a pharmaceutical composition and application for preparation of anti-osteoporosis drugs, where the pharmaceutical composition can significantly reduce blood sugar level and can significantly improve the skull area and skull optical density of the zebra fish with diabetic osteoporosis, promoting bone formation related gene expression, as well as reduces the activity of tartarate-resistant acid phosphatase. Further, the cited document comprises of mangiferin, tetrahydro epiberberine, phellodendrine, magnoflorine, hydroxyl oxidized berberine, palmatine and berberine. However, this cited document does not disclose about the method for the improvement of alkaline phosphatase activity with respect to the anti-osteoporosis as well as the improvement of the skull area and skull optical density. IN3584 / KOLNP / 2015 discloses a medical composition of acrylic cement for augmenting bone tissue, where the composition relates to an injectable composition that sets upon mixing the liquid and the powder phase, the liquid phase containing unsaturated fatty acids or triglyceride oils. The reaction is initiated upon decomposing the peroxide in the powder phase by a chemical activator in the liquid phase rather than applying external heat, as is common in injectable Bone Cements. The free radicals can attack the double bonds in either the monomer or the unsaturated fatty acids forming an injectable acrylic cement that incorporates grafts or segments of fatty acids or triglyceride oils. However, the use of unsaturated fatty acids or triglyceride oils enhances the blood sugar level, causes cancer, inflammation, asthma, etc. Miyazaki et al., J Biomed Mater Res A. 2003 Dec 15;67(4):1417-23. doi: 10.1002 / jbm.a.20042, discloses bioactive polymethyl methacrylate (PMMA) bone cement prepared by modification with methacryloxy propyltrimethoxysilane and calcium chloride. Bone Cement consisting of polymethyl methacrylate (PMMA) powder and methyl methacrylate (MMA) liquid is used extensively for fixation of implants such as artificial hip joints with living bone. The citation discloses about bioactivity of the modified PMMA Bone Cement with alkoxysilane and calcium chloride. However, the limitation that this paper possess is that it provides modified bone cement composition by utilising inorganic materials that causes toxicity.Zheng et al., Materials & Design Volume 209, 1 November 2021, 109966 https: / / doi.org / 10.1016 / j.matdes.2021.109966, discloses a bioactive polymethyl methacrylate (PMMA) Bone Cement for prosthesis fixation in osteoporotic hip replacement surgery. The article discloses about the osteointegration ability of the PMMA cement by adding mineralized collagen (MC) to induce an efficient fixation between the modified cement surface and osteoporotic host bone. To simulate clinical hip replacement, prosthesis is fixed with either PMMA or PMMA-MC Bone Cement in osteoporotic cadaveric femurs. However, the osteoblast is affected by gravity, mechanical stress, calcitonin, parathyroid hormone etc. and the microgravity negatively influences the bone metabolism by affecting the normal functioning of the osteoblast.Mousa et al., Biomaterials 21 (2000) 2137 - 2146 discloses biological and mechanical properties of polymethyl methacrylate (PMMA)-based bioactive bone cements, where using small-diameter PMMA beads that improved the handling properties, mechanical properties and the bioactivity of the PMMA-based bioactive cement. However, no apparent advantage of adding irregular particles or PMMA flour to the powder is disclosed.Mori et al., Journal Of Materials Science: Materials in Medicine 1 6 (2 0 0 5) 713 - 718 discloses about the synthesis of bioactive polymethyl methacrylate (PMMA) bone cement via modification with methacryloxypropyltrimethoxysilane (MPS) and calcium acetate, where the effects of the kinds of PMMA powder on setting time, apatite formation and compressive strength were investigated in a simulated body fluid. However, the addition of a high content of bioactive powder into PMMA Bone Cement causes problems of limitation on its workability and mechanical properties. Shinzato et al., J Biomed Mater Res. 2000 Aug;51(2):258-72. doi: 10.1002 / (sici)1097-4636(200008)51:2<258::aid-jbm15>3.0.co;2-s. discloses a new bioactive Bone Cement consisting of polymethyl methacrylate (PMMA) as an organic matrix and bioactive glass beads as an inorganic filler that consists of MGO-CaO-SiO2-P2O5-CaF2 and glass. However, the paper fails to disclose effective ability of the composition to bond with bone.Although, the above-mentioned prior arts disclose about the polymethyl methacrylate (PMMA) Bone Cement, however, there are several limitations of the above-mentioned state of art such as poor mechanical qualities, lack of bone adhesiveness, use of inorganic materials, less biocompatibility, less superoxide dismutase activity and release of free radicles to the surrounding tissues of prosthetic implant that causes toxicity.Therefore, there is a need to develop a bioactive Bone Cement composition for prosthetic implant with superoxide dismutase activity and minimum toxicity that exhibits free radical scavenging activity as well as possesses better cell viability, cell adhesion and less haemolysis.OBJECT OF THE INVENTIONThe main object of the present invention is to provide a biomaterial-based composition for prosthetic implants. Another object of the present invention is to provide a method for preparing a biomaterial-based composition for prosthetic implants.Yet another object of the present invention is to provide a biomaterial-based composition with superoxide dismutase activity and reduction in free radical release.Yet another object of the present invention is to provide a biomaterial-based composition with less cell toxicity and free radical scavenging activity. Still another object of the present invention is to provide a biomaterial-based composition possessing less haemolysis, high concentration of cell adhesion, cell viability as well as provides stable biological and mechanical interface with bone.SUMMARY OF THE INVENTIONThe present invention relates to a biomaterial-based composition for prosthetic implants and a method of preparing the same having superoxide dismutase activity with less toxicity and high free radical scavenging behaviour with significant reduction in free radical release.In an embodiment, the present invention provides a biomaterial-based composition comprising of a glucosylxanthone and an orthopaedic filler in a defined ratio ranging from 5% to 10%. The glucosylxanthone is mangiferin (MG) and the orthopaedic filler is Bone Cement. Further, the mangiferin (MG) is loaded on the Bone Cement. In another embodiment, the present invention provides a method of preparing a biomaterial-based composition, comprising the steps of extraction of the mangiferin (MG) from a bark of a mango tree to obtain a powder that is incorporated with a Bone Cement by free radical polymerization to obtain a polymer of a mangiferin-based Bone Cement (MG-BC). The polymer of mangiferin-based Bone Cement (MG-BC) is placed in a mould to obtain mangiferin-loaded Bone Cement (MG-BC). In yet another embodiment of the present invention, the mangiferin (MG) is extracted from the bark of the mango tree (Mangifera indica) by collecting and drying the bark of the mango tree under the sunlight to obtain a dried bark that is crushed into very small pieces to form a coarse powder. The powder is extracted by soxhlet extraction for 16 hours with methanol at 50°C to form a solution that is cooled and filtered to obtain a solvent. The solvent is evaporated to form a solid sample that is air-dried to obtain a powder of mangiferin (MG). In still another embodiment of the present invention, the mangiferin-loaded Bone Cement (MG-BC) of concentration MG-BC-5%, MG-BC-7.5% and MG-BC-10% are prepared by following steps of taking a pre-defined amount of Bone Cement powder, adding 1 ml of Bone Cement liquid and mixing with a glass rod manually till a thickened mixture is obtained and (b) placing the thickened mixture obtained in step (a) in a mould for hardening to obtain a hardened mangiferin-loaded Bone Cement. Here, said predefined amount of Bone Cement powder is 1.9 g for MG-BC-5%, 1.85 g for MG-BC-7.5% and 1.8 g for MG-BC-10%.The present invention relates to a mangiferin-loaded Bone Cement composition for orthopaedic implants with superoxide dismutase and haemolytic activity, cell viability and adhesion properties. The mangiferin-loaded Bone Cement composition of the present invention is a potential free radical scavenger for prosthetic implants.The above objects and advantages of the present invention will become apparent from the hereinafter set forth brief description of the drawings, detailed description of the invention, and claims appended herewith.BRIEF DESCRIPTION OF THE DRAWINGAn understanding of a biomaterial-based composition for prosthetic implants of the present invention may be obtained by reference to the following drawings:Figure 1 shows a graphical representation of Fourier Transform Infrared (FT-IR) spectroscopy of isolated mangiferin (MG) in part (a) and a graphical representation of Ultraviolet (UV)-Visible spectroscopy of isolated mangiferin (MG) in part (b), according to an embodiment of the present invention.Figure 2 shows a pictorial representation of morphology of mangiferin (MG) through Scanning Electron Microscopy (SEM) at magnification of 10μm in part (a) and a pictorial representation of morphology of mangiferin (MG) through scanning electron microscopy (SEM) at magnification of 2μm in part (b), according to the present invention.Figure 3 shows a graphical representation of Fourier Transform Infrared (FT-IR) spectroscopy of polymethyl methacrylate (PMMA), mangiferin (MG) and mangiferin-loaded polymethyl methacrylate (MG-PMMA) incorporated by Fenton initiator method, according to the present invention.Figure 4 shows a graphical representation of Fourier Transform Infrared (FT-IR) spectroscopy of commercially available Bone Cement (BC) and mangiferin-loaded Bone Cement (MG-BC) with different compositions, according to the present invention.Figure 5 shows a graphical representation of thermogravimetric analysis (TGA) and differential thermogravimetric analysis (DTGA) of MG-BC-7.5% in part (a) and a graphical representation of X-ray diffraction (XRD) of MG-BC-7.5% and MG-BC-5% after removal from the rat in part (b), according to the present invention.Figure 6 shows a pictorial representation of Scanning Electron Microscopy (SEM) of pure Bone Cement in part (a); a pictorial representation of tablet composition of MG-BC-5% in part (b); a pictorial representation of tablet composition of MG-BC-7.5% in part (c); a pictorial representation of the tablet after removal from RAT of the tablet composition of MG-BC-5% (d) and a pictorial representation of the tablet after removal from rat of the tablet composition of MG-BC-7.5% (e), according to the present invention.Figure 7 shows pictorial representations of atomic force microscopy (AFM) of topography phase images of MG-BC-5% tablets in parts (a) and (c); and pictorial representations of 3D images of MG-BC-5% tablets in parts (b) and (d); and pictorial representations of topography phase images of MG-BC-7.5% tablets in parts (e) and (g); and pictorial representations of 3D images of MG-BC-7.5% tablets in parts (f) and (h), according to the present invention.Figure 8 shows a pictorial representation of fluorescence microscopy of: control in part (a); a pictorial representation of pure Bone Cement (BC) in part (b); a pictorial representation of MG-BC-5% in part (c); a pictorial representation of MG-BC-7.5% in part (d); a pictorial representation of MG-BC-10% in part (e); and a pictorial representation of MG-PMMA in part (f), according to the present invention.Figure 9 shows a graphical representation for cell viability of various bone cement tablets: control; pure Bone Cement (BC); various composition of mangiferin loaded Bone Cement (Mg-BC) and MG-PMMA tablets tested against L929 cells, according to the present invention.Figure 10(A) shows blood biocompatibility study illustrating: a pictorial representation of blood cells observed with microscope after haemolysis, illustrating a pictorial representation of control in part (a); a pictorial representation of bone cement in part (b); (c) a pictorial representation of MG-BC-5%; (c) a pictorial representation of MG-BC-7.5%; (d) a pictorial representation of MG-BC-10% in part (e); and a pictorial representation of MG-PMMA in part (f), according to the present invention. Figure 10(B) is a graphical representation of haemolysis activity of prepared tablets such as BC; MG-BC-5%; MG-BC-7.5%; MG-BC-10% and MG-PMMA in different time intervals with blood, according to the present invention.Figure 11 shows a graphical representation of measurement of superoxide dismutase level (SOD) in blood showing: pure bone cement, MG-PMMA, MG-BC-5%, MG-BC-7.5% and MG-BC-10% into rat body and the blood collected in 24-hour interval up to 9th day, according to an embodiment of the present invention.Figure 12 shows a graphical representation of powder of X-ray diffraction of isolated mangiferin (MG), according to the present invention.Figure 13 shows a graphical representation of Ultraviolet (UV)-Visible spectroscopy of PMMA, MG-PMMA and MG, according to the present invention.Figure 14 shows a graphical representation of Ultraviolet (UV)-Visible spectroscopy of BC, MG-BC-7.5%, MG-BC-5% and MG, according to the present invention.Figure 15 shows a schematic representation for the in vivo work and the proposed radical scavenging mechanism, according to an embodiment of the present invention.Figure 16 shows a schematic representation of scavenging of free radicals by MG, according to the present invention.Figure 17 shows a schematic representation for polymerization of commercial Bone Cement (BC) in part (a) and a schematic representation of MG-PMMA composition preparation in part (b), according to the present invention.DETAILED DESCRIPTION OF THE INVENTIONThe present invention will now be described hereinafter with reference to the accompanying drawings in which a preferred embodiment of the invention is shown. This invention may, however, be embodied in many different forms and should not be constructed as being limited to the embodiment set forth herein. Rather, the embodiment is provided so that this disclosure will be thorough, and will fully convey the scope of the invention to those skilled in the art.The present invention now will be described hereinafter with reference to the detailed description, in which some, but not all embodiments of the invention are indicated. Indeed, the invention may be embodied in many different forms and should not be construed as limited to the embodiments set forth herein; rather, these embodiments are provided so that this disclosure will satisfy applicable legal requirements. Like numbers refer to like elements throughout. The present invention is described fully herein with non-limiting embodiments and exemplary experimentation.The present invention relates to a biomaterial-based composition for prosthetic implants having free radical scavenging activity, possess cell viability, less cell toxicity and has stable biological and mechanical interface with bone and a method of preparing the same.In a preferred embodiment, the present invention provides a biomaterial-based composition comprising of a glucosylxanthone; and an orthopaedic filler in a defined ratio ranging from 5% to 10%; wherein, the glucosylxanthone is mangiferin (MG); the orthopaedic filler is Bone Cement; and the mangiferin (MG) is loaded on the bone cement. Here, the mangiferin (MG) is extracted from a bark of a mango tree (Mangifera indica). The composition is in the form of a tablet, capsule, semi-solid or powder, and is essentially in the form of a tablet. Further, the mangiferin (MG) is loaded on the Bone Cement in a concentration of 5%, 7.5% and 10%. The composition possess surface roughness of the mangiferin (MG) in a range of 10 nm to 18 nm and the Bone Cement in a range of 30 nm to 40 nm with a concentration of cell adhesion in a range of 5% to 10%. Additionally, the cell toxicity of the composition is in a range of 2% to 8% in a time period of 24 hours to 72 hours, possess superoxide dismutase (SOD) level and free radical release in a range from day 1 to day 9 for MG-5% of 1.394 to 0.113, for MG-7.5% of 1.578 to 0.173 and for MG-10% 1.410 to 0.220. The cell viability of the composition lies in the range of 98 to 92% for 24 to 72 hours, possess hemolysis ranging from 0.93 to 3.90 for MG-5%, 0.90 to 3.70 for MG-.5% and 0.89 to 4.57 for MG-10% for a time period of 1 hour to 24 hours. In another preferred embodiment, the present invention provides a method of preparing a biomaterial-based composition comprising the steps of: (a) extracting the mangiferin (MG) from a bark of a mango tree to obtain a powder; (b) incorporating the powder obtained in step (a) with a bone cement having concentration in a range of 5% - 10% by free radical polymerization to obtain a polymer of a mangiferin-based bone cement; and (c) placing the polymer of mangiferin-based bone cement (MG-BC) obtained in step (b) in a mould to obtain mangiferin-loaded bone cement (MG-BC).In yet another preferred embodiment of the present invention, the mangiferin (MG) is extracted from the bark of the mango tree through following steps: (a) collecting and drying the bark of the mango tree under the sunlight to obtain a dried bark; (b) crushing the dried bark obtained in step (a) into very small pieces to form a coarse powder; (c) extracting the coarse powder obtained in step (b) by soxhlet extraction for 16 hours with methanol at 50°C to obtain a solution; (d) cooling and filtering the solution obtained in step (c) to obtain a solvent; (e) evaporating the solvent of step (d) to obtain a solid sample; and (f) air-drying the solid sample obtained in step (e) to obtain a powder of glucoside (mangiferin).In still another preferred embodiment of the present invention, the mangiferin-loaded bone cement (MG-BC) of concentration MG-BC-5%, MG-BC-7.5% and MG-BC-10% are prepared by following steps: (a) taking a pre-defined amount of Bone Cement powder, adding 1 ml of Bone Cement liquid and mixing with a glass rod manually to obtain a thickened mixture; and (b) placing the thickened mixture obtained in step (a) in a mould for hardening to obtain a hardened mangiferin-loaded Bone Cement. Here, the predefined amount of Bone Cement powder is 1.9 g for MG-BC 5%, 1.85 g for MG-BC 7.5% and 1.8 g for MG-BC 10%.Referring to Figure 11, a graphical representation of superoxide dismutase level (SOD) in blood is illustrated in which the measurement of superoxide dismutase level (SOD) in blood is shown by placing the tablet of pure Bone Cement (BC), MG-PMMA, MG-BC-5%, MG-BC-7.5% and MG-BC-10% into rat body and the blood collected in 24-hours of interval up to ninth day.Referring to Figure 15, a scheme for the in vivo study and radical scavenging mechanism of mangiferin loaded bone cement of the present invention is represented.EXAMPLE 1MATERIALS AND METHODSMaterialsMethyl methacrylate (MMA) was purchased from Loba Chemie, Mumbai, India and was dried over anhydrous calcium hydride and distilled under reduced pressure. 2, 2'-Azobis (isobutyronitrile) (AIBN) (Spectrochem, Mumbai, India, 98%) was recrystallized from methanol. Tetrahydrofuran (THF) (Loba Chemie, Mumbai, India) was dried freshly over sodium metal and benzophenone. Hexane (CDH) was used as received. Commercially available distilled water was distilled twice from alkaline potassium permanganate solution in a glass distillation unit and middle fraction was used for further experiments.MethodsExtraction of mangiferin (MG):Mangiferin was extracted by modifying the method explained by Ghosal et al. The bark of the mango tree was collected from the premises of IIT (BHU), Varanasi, UP, India and dried under the sunlight and then crushed down into very small pieces. Further, this course powder was soxhlet for 16 hours with methanol at 50ºC. At this temperature, MG was completely dissolved in solvent. Dried and crushed plant material was soxhlet for 16 hours at 50°C with methanol. The solution was then cooled and filtered. The solvent was evaporated and then the solid sample was air-dried to acquire the powder.Preparation of MG incorporated BCCommercially available (Johnson & Johnson, Depuy CMW- 1) Bone Cement was used. The Bone Cement is a two-pack system of finely divided white powder and a colourless liquid. The powder is composed of PMMA and benzoyl peroxide to initiate the cement polymerization when the powder and liquid components are mixed. Barium sulphate was used as radio opaque agent. The liquid was composed of methyl methacrylate monomer (MMA), hydroquinone and stabilizer to prevent premature polymerization which may occur when the liquid is exposed to heat or light. Also, N, N-dimethyl-p-toluidine promotes cement polymerization. A schematic representation for polymerization of commercial Bone Cement (BC) is shown in part (a) of Figure 17 and a schematic representation for preparation of mangiferin-loaded Bone Cement (MG-PMMA) composition is shown in part (b) of Figure 17. Four major types of tablets were made using different combination of MG with BC and then they were placed in a mould to prepare tablets and taken out when hardened. Notation of these tablets are BC, MG-BC-5%, MG-BC-7.5% and MG-BC-10%.Preparation of MG incorporated PMMA:Further, Mg-PMMA polymerization has been performed. For polymerization 0.015 g of ferrous ammonium sulphate was taken in 100 mL of double distilled water (DDW) followed by 10 min of nitrogen flush. Monomer MMA and Mangiferin were then added, followed by 5 min of nitrogen flush again. Finally, the solution was corked after adding hydrogen peroxide and then it was kept in the dark overnight. Next day, the polymer composite was recovered by filtration followed by several washings with DDW. Then, 1.959 g of laboratory synthesized MG-PMMA polymer, fenton initiator, and 0.041 g of Benzoyl peroxide was mixed with glass rod manually. Then 1 mL of Bone Cement liquid was mixed with a glass rod till the mixture thickens. The purpose of synthesis of PMMA was that to compare the commercially available Bone Cement with laboratory synthesized MG-PMMA.Preparation of tablets with mangiferin:Different types of tablets are shown in Table 1 were made using different combinations of substances. Table 1: Composition of tablets prepared with mangiferinSymbols Tablets ConstituentsMG-PMMA Tablet 1 1.959 g of synthesized laboratory MG-PMMA powder polymer, obtained through aqueous polymerization of MMA in presence of mangiferin and fenton initiator, was taken and 0.041 g of benzoyl peroxide was mixed with glass rod manually. Then 1 ml of Bone Cement liquid was mixed with a glass rod till the mixture thickens.BC Tablet 2 2 g of bone cement powder and 1 ml of Bone Cement liquid were mixed with a glass rod manually till the mixture thickens.MG-BC-10% Tablet 3 1.8 g of Bone Cement powder was mixed with 0.2 g of mangiferin. 1 ml of Bone Cement liquid was mixed with a glass rod manually till the mixture thickens.MG-BC-7.5% Tablet 4 1.85 g of Bone Cement powder was mixed with 0.15 g of mangiferin. 1 ml of Bone Cement liquid was mixed with a glass rod manually till the mixture thickens.MG-BC-5% Tablet 5 1.9 g of Bone Cement powder was mixed with 0.1 g of mangiferin. 1 ml of Bone Cement liquid was mixed with a glass rod manually till the mixture thickens.Prior to tablet preparation, two types of polymers were made for the comparison purpose and examined the result comparably. One is MG-PMMA, a laboratory synthesized PMMA in the presence of MG and other is commercial Bone Cement (BC) i.e., is prepolymerized PMMA. Mangiferin was not added in the pure polymer sample that is commercial Bone Cement (BC). Different types of tablets were made using different combinations of substances and then they were placed in a mould to prepare tablets and taken out when hardened. Here, the sample were designated as follows: tablet 1 for MG-PMMA (synthesis of PMMA in presence of MG), tablet 2 for pure BC, tablet 3 for MG-BC-10%, tablet 4 for MG-BC-7.5% and tablet 5 for MG-BC-5%, respectively.EXAMPLE 2CHARACTERIZATIONFourier transform-infrared (FT-IR) spectra were recorded in a SHIMADZU 8400S FT-IR spectrophotometer. Powdered samples were mixed with dry potassium bromide (KBr) and made into the thin pellet form, for the analysis in wavenumber from 4000-400 cm-1 with a resolution of 4 cm-1 at room temperature. UV-visible absorption spectra of the samples were taken using Shimadzu UV- 17001 spectrophotometer in 200-1100 nm range. Morphology of mangiferin and mangiferin loaded bone cement before and collected after incorporation in rat were examined through ZEISS MA15 / 18 at different magnification stages. Crystalline behaviour of mangiferin was investigated using an X-Ray diffractometer (Rigaku Smart Lab 9kW) with a Cu-Ka source (? = 1.54 Å) with a step size of 0.02° and 2? between 5° and 70°. Thermal stability was studied in TGA-50, Shimadzu model. Approximately 10 MG of sample was heated at a rate of 20°C / minute with the PerkinElmer TGA. Surface roughness of prepared samples were measured through NTEGRA Prima (Russia) in semicontact mode with scan speed of 0.5 Hz.Characterization of mangiferin (MG):The structure of the powdered extract of MG was confirmed with FT-IR and UV-visible study. The crystallinity was confirmed with X-ray diffraction (XRD) and morphology of the powder was studied through scanning electron microscope (SEM). FT-IR spectra of isolated MG are shown in part (a) of Figure 1. A broad band appeared at 3363 cm-1 due to the presence of -OH, 2366cm-1 band appeared due to the -C-H stretching and 1497cm-1 appeared due to -CH-CH- bending. Additional bands appeared at 1665cm-1 for -C-O stretching, 1088 cm-1 for (C-O-C) and 1663cm-1 for (-C-O-C-) that confirmed for the MG. The UV-visible absorption spectra of the MG as shown in part (b) of Figure 1. The specific absorption band observed at 258 nm, 316 nm, and 366 nm for previous MG (for benzene ring). Absorption band appeared at 366 nm was due to the n?p* transition of anthracene present in MG. Additionally, Figure 2 displays the SEM images of MG with mesomorphic crystal structure. The crystal structure of MG as shown in Figure 12 was also studied through XRD. Crystalline peak appeared at 2? values of 10.6o, 12.2o, 13.9o, 16.4o, 17.3o, 18.2o, 20.1o, 21.2o, 22o, 23o, 24.5o and 27.4o due to the polymorphic crystal structure of MG. Characterization of pristine PMMA and MG-loaded PMMA: Figure 3 shows the FT-IR of PMMA and mangiferin incorporated PMMA. The characteristic intense bands observed at 2996 cm-1 (for symmetric stretching of CH2), 3100 cm-1 (for asymmetric stretching of CH3), 1731 cm-1 (C=O) and 1635 cm-1 (C=C). Additionally, bands appeared at 1485cm-1 (CH2 bending), 1447 cm-1 (C-H deformation of C-CH3), 1389 cm-1 (C-H bending), 1148 cm-1 (C-O-C symmetric) and 1064 cm-1 (asymmetric stretching) were confirmed for the PMMA. For MG-PMMA, the obtained bands at 3631 and 3549 cm-1 (-OH), 1337 and 1271cm-1 (-C-O) for MG, while 1734 cm-1 (C=O) was because of PMMA. All of the FT-IR bands partially confirmed that the MG has been successfully incorporated into the PMMA matrix. Likewise, in UV spectra PMMA show two intense absorption band below 400nm as shown in Figure 13. These strong absorption band appeared due to the electronic excitation within the carbonyl chromophores (C=O) present in the PMMA structure. The strongest absorption band appeared at 221nm due to the p?p* transition in the C=O system. There was another band observed at 281nm attributed to the n?p* transition, which is with less intensity compared to the p?p* transition of PMMA. In MG-PMMA system, a broad band observed between 280nm to 400nm due to the red shift. Preparation and characterization of Bone Cement (BC) and different compositions of MG-BC: DMPT and benzyl peroxide were acting as an activator and initiator respectively to form an intermediate complex. By releasing CO2, phenyl radicle has been formed and initiated the polymerization of MMA monomer. Figure 4 shows the FT-IR spectra of Bone Cement and various percentage of MG incorporated bone cement. The bands appeared at 2950 cm-1 (asymmetric stretching vibrations), 1726 cm-1 (carbonyl stretching) and 1141 cm-1 (O-CH3 stretching) were confirmed for Bone Cement. However, mangiferin loaded Bone Cement showed that the band obtained between the 3500 and 3000 cm-1 for -OH stretching only. Simultaneously, bands appeared at 1662 cm-1 was due to (C-O stretching) of mangiferin. Further, UV-spectra appeared between 200-600 nm and there was a cooperative transition of electrons in various energy bands (s, p and n), as shown in Figure 14. One absorbance band appeared at 220 nm in Bone Cement is due to the presence of carbonyl chromophore along with p?p* transition. For MG loaded in bone cement, the absorption band is shifted to 245 nm due to n? s* electronic transition. The thermal stability of MG-BC-7.5% was measured with temperature variation to investigate the weight loss percentage of material. Part (a) in Figure 5 shows the mass loss behaviour of MG-BC-7.5%, and their thermal degradation occurred in three stages. The ~4% weight loss occurred around 100°C, which was occurred due to the evaporation of surface water from the material. Afterwards, a second stage of weight loss was observed at 231°C for BC and mangiferin because both the material has almost same degradation temperature. A third stage of weight loss (~9.9%) corresponds to the degradation of DMPT and benzyl peroxide at 448°C. The DTGA curve of MG-BC-7.5% indicates the melting peak at 202°C for the first stage while 386°C for the second stage.Crystalline structure of MG was observed in powder XRD pattern as shown in Figure 12. Several crystalline peaks are observed at 2? ~10.7°; 12.4°; 13.8°; 16°; 18.8°; 20°; 21.2°; 22°; 23.3°; 24.8°; 25.2°; 28.6°; 29.4° and 31.9° which proves the high crystalline nature of MG. BC is an amorphous material and MG impregnation in BC provides overall crystallinity to the composite materials. The composite materials MG-BC-7.5% and MG-BC-5% tablets were recovered from nine days post treatment and undergone through the XRD analysis. The obtained results showed the reduced intensity of diffraction peaks of MG in MG-BC-7.5% at 2?~ 23°, 26.2°, 27.2°, 29.1°, 31.8°, 33.1°, 41.1° and 42.9° along with absence of some peaks compared to the pure MG as shown in part (b) of Figure 5. The compound MG contains two xanthone molecules bound to five molecules of crystalline water being stabilized by the formation of intermolecular hydrogen bonds. Figure 6 shows the morphology of pristine Bone Cement (BC) and MG incorporated Bone Cement analysed with SEM. The pure BC clay has globular structure in its morphology as shown in part (a) of Figure 6 while pure MG shows the rectangle type irregular shape at different magnification as shown in Figure 2. MG particles, in different composition, are first dispersed into cement phase and then added with liquid phase. Finally, MG embedded into Bone Cement matrix, which appeared as white specks into Bone Cement that medium uniformly distributed due to their crystalline structure. Before the incorporation of MG-BC-5% and MG-BC-7.5% tablets into rat body, both the tablets show globular structure with irregular shape of MG as it is shown in part (b) and part (c) of Figure 6, respectively. On physical mixing of MG with phospholipid, similar results were observed. Whereas, SEM images of BC-MG-5% as shown in part (d) of Figure 6 and MG-BC-7.5% as shown in part (e) of Figure 6 after incorporated into rat; both the tablets release MG as well as BC into the biological system. Consequently, their morphology is also changed as shown in Figure 6. From SEM images, it is observed that the MG has been successfully mixed with bone cement matrix and their release was also occurred inside the rat's body only. Similarly, Figure 7 shows AFM images of the mangiferin-loaded Bone Cement of the present invention. The roughness of MG-BC-5% and MG-BC-7.5% is clearly identified which is very important for biocompatibility. AFM topography phage and 3D images in part (b) and (d) of Figure 7 and in part (f) and (h) of Figure 7 for MG-BC-5% and MG-BC-7.5% are shown for different magnifications. For MG-BC-5% and MG-BC-7.5%, the average roughness values were calculated to be 18 nm and 40 nm, respectively. Their roughness results obtained from the profiles are also reported in Table 2. However, higher surface roughness supports the cell adhesion much more to the substrate. Table 2: Surface roughness Ra (μm) of different samples with different dimensionsSample Name 3μm 5μm 10μm 20μm DimensionMG-BC-5% 66.77 48.64 57.32 56.71 2D 56.99 75.03 58.34 40.32 3DMG-BC- 7.5% 51.95 51.27 62.13 70.29 2D 63.78 54.40 45.77 39.96 3DNote: BC: Bone Cement; MG: mangiferin.EXAMPLE 3In-vitro studiesHaemolysisErythrocyte activities of MG loaded and unloaded Bone Cement composites were verified with modified method. 50ml of whole blood was taken from a healthy human body and centrifuged at 3500 rpm for 5 minutes. Supernatant was removed and collected red blood cell (RBC) pallet was washed with PBS buffer thrice (pH 7.2). Thus, 50 mL of PBS buffer was added into RBCs pallet after multiple washing. PBS buffer and 1% Triton X-100 aqueous solution were used for negative and positive control samples, respectively. Loaded and unloaded Bone Cement tablets were mixed with RBC suspension for different time intervals at 37°C. After each incubation period, RBCs were centrifuged at 10,000 rpm for 5 minutes and supernatant was collected. Supernatant were assessed by optical absorption at 450nm. The haemolysis (%) of RBCs was calculated using the following equation:% haemolysis=(absorbance of sample-absorbance of negative solution) / (absorbance of positive-absorbance of negative solution) x100Cell culture studiesThe mouse mesenchymal stem cell line, C3H10 t1 / 2 (NCCS Pune, India), was cultured with Dulbecco's Modified Eagle's Medium (DMEM) with 10% foetal bovine serum (FBS) and 1% antibiotic-antimycotic solution at 37°C. Then 1 x 103 cells were seeded onto the material tablet for all the cells culture assays. The prepared tablets were washed with isopropanol for cleaning purpose. For surface sterilization, each specimen was washed thrice with PBS (phosphate buffered saline, pH-7.2) and kept in 70% alcohol for some time. Further, samples were exposed to UV light for 6-8 hours.Cell viabilityCytotoxicity of the prepared tablets were studied through previously reported modified method. Each well was seeded with 1 x103 cells in 200μL of medium and incubated at 37°C for 24 hours. After that, cell debris was removed and supernatant medium was replaced with fresh medium. Consequently, prepared various mangiferin loaded or unloaded bone cement and PMMA tablets were kept into each well and incubated for 1, 3 and 5 days distinctly. Afterward incubation, the supernatant was removed and 50μL of MTT solution at 0.5MG / mL in DMEM without FBS was added and incubated at 37°C for 4 hours in the dark. Then, 100μL of DMSO was added to solubilize the formazan. The number of viable cells were quantified by measuring the absorbance spectrophotometrically with a microplate reader (iMark, Biorad) at 570nm. The cell viability percentage has been calculated using the following equation:% of cell viability=(absorbance of test sample-absorbance of positive control) / (absorbance of negative control-absorbance of positive control)where, negative control = cells with medium alone, andpositive control = cells with medium and 5% DMSO.Fluorescence studiesCell proliferation of prepared tablets were studied through fluorescence microscopy. The cells (1x 104 per mL) were seeded in 24 well plate at 37°C for 24 hours. After that, cell debris was removed and supernatant was replaced with freshly prepared medium. Then, several MG loaded and unloaded Bone Cement and PMMA tablet were prepared and kept into each well and incubated for another 24 hours at 37°C. After that, samples were taken out and washed with 10 mM PBS thrice. Further, stained with acridine orange and ethidium bromide (Sigma, India) (100μgmL-1 each) and incubated at room temperature for 30 minutes in the dark. Images were acquired using a fluorescence microscope (Dewinter Technologies, India). Estimation of Blood SODThe blood samples were collected from rat each day continues up-to 9 days (stored in heparin) and were centrifuged at 2500 g at 2-8°C for 5-10 minutes. The plasma supernatant and the red blood cell pellet were removed. The erythrocytes were suspended in 4 volumes of ice-cold water and mixed thoroughly. After 5 minutes, the assay for superoxide dismutase (SOD) was carried out according to the described method with slight modifications. 1.20ml of sodium pyrophosphate buffer (pH 8.3, 0.052 M) with 0.1ml of 186μm phenazine methosulfate and 0.3ml of 30μm nitro blue tetrazolium was added in the above samples. Then 0.2ml NADH was added followed by addition of 3ml of ice-cold water. The solution was allowed to incubate at 30°C for 90 seconds. Then 1ml of glacial acetic acid was added. Afterwards, the reaction mixture was shaken vigorously with addition of 4mL butanol dropwise. Then the mixture was centrifuged (8000 RPM) for 10 minutes and the butanol layer was then extracted out. Colour intensity of the chromogen developed in the butanol layer was measured at 560nm in a spectrophotometer against butanol as blank.EXAMPLE 4In-vivo studiesThe in vivo study protocol was approved by Institute Animal Ethics Committee of Banaras Hindu University, clearance no. Dean / 2009-10 / 764. Middle aged (6-7 weeks) male Charles Foster rats (250-300 g) were taken from the Animal House, Institute of Medical Sciences, Banaras Hindu University, Varanasi, India. They were housed in different cages and were provided with Food Chow pellets and water ad libitum.Collection of blood samplesThe rats were anaesthetized intraperitoneally using pento barbitone (35 MGkg_1 body weight). Rats were distributed in three groups: Control (N=6), Sham control (N=6) and Experimental (N=6), where N is number of rats. The control group animals were kept as such during the experiment. The sham control group animals were just given the incision after anaesthetizing and their wound was sealed with sutures. The experimental group was given a small incision at the back of the neck and freshly prepared tablets were incorporated inside the skin and sealed with sutures and micropore. The blood samples were collected from each animal each day (after 24 hours) till ninth day and stored in microcentrifuge tubes containing heparin. Statistical AnalysisStatistical analysis was also accomplished from the mean of three independent data of independent experiment using GRAPH PAD PRISM for Windows. The results of experiments were taken as mean and standard deviation for the analysis. Two-way ANOVA followed by Bonferroni post-test predict the p value (<0.0001). Superoxide dismutase (SOD) activity on all the 9 days of test were calculated for the seven groups of rats.EXAMPLE 5Fluorescence analysis of apoptotic cellsFluorescence microscopy helped to identify the morphology observation of cells after any biomaterial exposed with biological cells or tissues. Orange stain cells show late apoptotic stage due to the presence of ethidium bromide in it, but have condensed cell with nuclei fragmentation. Whereas, viable necrotic orange cells have clear nuclear morphology but without condensed chromatin. It helped in identifying the cell death type either apoptosis or necrosis before proceeding to the in vivo study. Figure 8 shows the microscopic images after the incubation of different samples such as MG, PMMA, Bone Cement and MG-Bone Cement with L929 cells for 24 hours. The obtained results are very interesting, as a very less number of cells undergone apoptosis. However, it is crucial to measure the cells that recover later injury or advancement in necrosis stage because of the inflammatory response and cellular injury. The different features of the L929 cells after experience to the AO / EB dye is shown in Figure 8. Moreover, viable cells show regular nuclei with an actual good reticular shape with green stain in the nucleus and red / orange granules in the cytoplasm. Basically, acridine orange is a cell permeable dye that stains both the live and dead cells but ethidium bromide impermeable to normal cell or it stain cells which lost their membrane integrity due to some harsh reasons. Live cells seem consistently green in colour with BC-MG-5% and all cells are with normal morphology, whereas, cells in early apoptotic phase appeared with bright green dots in the nucleus because of the chromatin condensation process as shown in Figure 8.Cell viabilityCell viability is a measurement of live cells to determine the cytotoxicity of particular materials at different experimental conditions. Metabolic activity of cells provides the cell viability conditions that offer the cell death data through the loss of membrane integration of cells. The MTT assay is a colorimetric test for measuring the activity of enzymes that reduce 3-[4, 5- dimethylthiazol-2-yl]-2, 5 diphenyltetrazolium bromide (MTT) to formazan, giving a purple colour. Figure 9 illustrates the comparative cell viability results of BC, BC-MG and MG-PMMA composite materials by MTT assay. The obtained results revealed that the cytotoxicity of L929 cells was bare to MG-PMMA at 72 hours. All the composite materials exhibit very good viability except MG-PMMA. The composite materials BC, MG-BC-5%, MG-BC-7.5% and MG-BC-10% have more than 90% cell viability up to 72 hours. Among them, highest cell viability has been obtained (~95%) for BC-MG-7.5% at all the time interval. This result also supports the fluorescence microscopy results as shown in Figure 8.The destruction of red blood cells via the rupture of cell membranes with a release of haemoglobin is a primary and essential test to check the biocompatibility of an implant material before any biological test. The percentage value of haemoglobin signifies the number of RBCs, because cells encourage many reactions in it and ultimately release blood components. If any foreign material or synthetic or implant material is not safe for the biological purpose, then it will not behave very well with blood and cannot process further for a higher level. The haemoglobin level should not be more than 5% in any circumstances. Accordingly, haemolysis tests were performed for MG, MG-PMMA, bone cement, mangiferin incorporated bone cement 5, 7.5, and 10%. The outcome values after the incubation of all samples with blood is shown in part (B) of Figure 10. A 100% RBC rupture over the interaction with water (positive control) was observed, while the negative control showed 0% rupture of RBC. This experiment conducted in triplicate and their mean value represents the haemolysis absorbance. All the obtained results show good haemolysis activity and safe to use in biomedical applications. Further, haemolysed RBC images were taken from randomly picked haemolysed blood sample and were observed under the microscopy as shown in part (A) of Figure 10. The obtained images demonstrated that all biomaterial's compositions of BC-MG are safe and there is no RBC destructed in presence of BC-MG-5%; BC-MG-7.5% and BC-MG-10%.In-vivo result by drug elutionFigure 11 shows the superoxide dismutase (SOD) level in blood. It is revealed from the results that MG-BC-7.5% has the superior capacity to scavenge the free radicals generated by the bone cement. Several researchers have worked on antibiotic release from bone cement. The mechanism by which drugs are released from the bone cement has been in doubt. Some workers stated that the drug diffuses through the matrix of the cement, while others reported that it is released through the holes and pores in the cement. It is reported earlier, the initial release of antibiotics from the cement was mainly a surface phenomenon, while sustained release over several days was a bulk diffusion phenomenon. In the present invention, the same concept is predicted for the release of MG as shown in Figure 15 and Figure 16. Mangiferin elution followed two types of mechanisms. The first mechanism involved the dissolution of the drug particle within the surrounding medium. The other materials required the diffusion of the drug through the solid matrix, which is similar to the way of antibiotics released from the Bone Cement. Generally, a Bone Cement filler is essential to fill the gap between bones and implants, simultaneously, it generates free radical which creates hurdles to the surrounding tissue in the healing process. In this context, mangiferin loaded bone cement becomes a superior biomaterial as orthopaedic implants filler because mangiferin scavenges the free radicals liberated during prosthesis without effecting the Bone Cement properties. Mangiferin (MG) was loaded into Bone Cement (BC) during their polymerization reaction into three different wt% compositions. In-vitro results demonstrated better haemolysis, cell viability and adhesion properties as compared to the earlier reports. SOD assay has shown that BC-MG-7.5% composition showed protecting capacity in cells as positive control. Thus, BC-MG is a potent free radical scavenger for enhancement of therapeutic effects in orthopaedic surgery.For in vivo studies, the animals were divided into three groups and are analyzed: control, sham control, and experimental as shown in Figure 15. The experimental group rats were further divided into seven groups, i.e., BC (Bone Cement), MG-PMMA, MG-BC%, MG-BC-7.5%, and MG-BC% including control and sham control (SC) group. No treatment was given to the control group during whole experiments, whereas, sham control has been given incision on their neck after anesthesia, but no treatment provided to them and kept as such. All the animals were given specific treatment for continuous 9 days. The blood was collected from the animals at the interval of in 24 hours from the treatment up-to ninth day. Further, collected blood samples were subjected to SOD estimation assay. The data obtained was subjected to statistical analysis and was summarized as shown in Figure 11. Initially, the SOD levels of all biomaterials increased due to the injury caused by insertion in skin as shown in the scheme of the mechanism in Figure 16. Further, with treatment period, it decreased except for MG-PMMA up to sixth day of the treatment. Next, from the seventh day in BC-MG composition, the SOD level in blood is decreased. Mangiferin has the capacity to reduce SOD level caused by biomaterials and protects the cells from free radicle damage. Based on the experimental results, the mechanism of MG scavenging free radicles from the wound tissues is illustrated in Figure 16. The structure of catechol moiety and MG favours the iron chelation process in mitochondria. The MG-Fe(III) / Fe(II) coordinate complex acquire as additional superoxide dissimulating metal centre, which increase ?2 radicles. These free superoxide radicles are ultimately scavenged by metal catechol moiety.Therefore, the present invention relates to a modified bioactive bone cement as orthopaedic implant filler with improved superoxide dismutase activity, better haemolysis cell viability and adhesion properties by having mangiferin that scavenges the free radicals liberated during prosthesis without effecting the bone cement properties.Many modifications and other embodiments of the invention set forth herein will readily occur to one skilled in the art to which the invention pertain having the benefit of the teachings presented in the foregoing descriptions and the associated drawings. Therefore, it is to be understood that the invention is not to be limited to the specific embodiments disclosed and that modifications and other embodiments are intended to be included within the scope of the appended claims. Although specific terms are employed herein, they are used in a generic and descriptive sense only and not for the purposes of limitation.
Claims
1. A biomaterial-based composition, comprising of: a glucosylxanthone; and an orthopaedic filler in a defined ratio; wherein, said glucosylxanthone is mangiferin (MG); said orthopaedic filler is Bone Cement; said mangiferin (MG) is loaded on said Bone Cement; and said defined ratio is in a range of 5% to 10%.
2. The biomaterial-based composition as claimed in claim 1, wherein said mangiferin (MG) is extracted from bark of a mango plant (Mangifera Indica).
3. The biomaterial-based composition as claimed in claim 1, wherein said composition is in the form of a tablet, capsule, semi-solid or powder.
4. The biomaterial-based composition as claimed in claim 1, wherein said composition is essentially in the form of a tablet.
5. The biomaterial-based composition as claimed in claim 1, wherein said mangiferin (MG) is loaded on said Bone Cement in a concentration of 5%, 7.5% or 10%.
6. The biomaterial-based composition as claimed in claim 1, wherein said composition possess surface roughness of said mangiferin (MG) in a range of 10 nm to 18 nm and said Bone Cement in a range of 30 nm to 40 nm with a concentration of cell adhesion in a range of 5% to 10%.
7. The biomaterial-based composition as claimed in claim 1, wherein said composition possess cell toxicity in a range of 2% to 8% in a time period of 24 hours to 72 hours.
8. The biomaterial-based composition as claimed in claim 1, wherein said composition possess superoxide dismutase (SOD) level and free radical release in a range from day 1 to day 9 for MG-5% of 1.394 to 0.113, for MG-7.5% of 1.578 to 0.173 and for MG-10% 1.410 to 0.220.
9. The biomaterial-based composition as claimed in claim 1, wherein said composition possess cell viability ranging from 98 to 92% for 24 to 72 hours.
10. The biomaterial-based composition as claimed in claim 1, wherein said composition possess haemolysis ranging from 0.93 to 3.90 for MG-5%, 0.90 to 3.70 for MG-7.5% and 0.89 to 4.57 for MG-10% for a time period of 1 hour to 24 hours.
11. A method of preparing a biomaterial-based composition, comprising the steps of: a) extracting mangiferin (MG) from a bark of a mango tree to obtain a powder; b) incorporating said powder obtained in step (a) with a Bone Cement having concentration in a range of 5%-10% by free radical polymerization to obtain a polymer of a mangiferinbased Bone Cement (MG-BC); and c) placing said polymer of mangiferin-based Bone Cement (MG BC) obtained in step (b) in a mould to obtain mangiferin-loaded Bone Cement (MG-BC).
12. The method of preparing said biomaterial-based composition as claimed in claim 11, wherein said mangiferin (MG) is extracted from the bark of the mango tree through following steps: a) collecting and drying the bark of the mango tree under the sunlight to obtain a dried bark; b) crushing said dried bark as obtained in step (a) into very small pieces to form a coarse powder; c) extracting said coarse powder obtained in step (b) by soxhlet extraction for 16 hours with methanol at 50°C to form a solution; d) cooling and filtering said solution obtained in step (c) to obtain a solvent; e) evaporating said solvent obtained in step (d) to form a solid sample; and f) air-drying said solid sample obtained in step (e) to obtain a powder of mangiferin (MG).
13. The method of preparing said biomaterial-based composition as claimed in claim 11, wherein said mangiferin-loaded Bone Cement (MG-BC) of concentration MG-BC-5%, MG-BC-7.5% and MG-BC10% are prepared by following steps: a) taking a pre-defined amount of Bone Cement powder, adding 1 ml of Bone Cement liquid and mixing with a glass rod manually to obtain a thickened mixture; and b) placing the thickened mixture obtained in step (a) in a mould for hardening to obtain a hardened mangiferin-loaded Bone Cement.
14. The method as claimed in claim 11 and 13, wherein said predefined amount of Bone Cement powder is 1.9 g for MG-BC-5%, 1.85 g for MG-BC-7.5% and 1.8 g for MG-BC-10%.